Optical fiber sealing structure in high vacuum environment and forming process thereof

By adopting the dual welding process of high-temperature and low-temperature solder in the optical fiber sealing structure, the problems of unstable fiber sealing and insufficient connection strength in the prior art are solved, and stable sealing and high-quality welding effects are achieved in a high vacuum environment.

CN118915252APending Publication Date: 2024-11-08HEFEI JUNENG ELECTRO PHYSICS HIGH-TECH DEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411066320.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-05
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing optical fiber sealing technology has unstable sealing effect in high vacuum environments and insufficient connection strength, making it difficult to meet the performance requirements in high vacuum environments.

Method used

High-temperature brazing is used for nickel tubes and austenitic stainless steel cavity, and then vacuum brazing of copper-plated fibers and nickel tubes is used for vacuum brazing. Combined with the dual welding process of high-temperature and low-temperature brazing, the sealing structure is ensured and the stability of the sealing structure is ensured. strength.

Benefits of technology

It achieves stable sealing in a high vacuum environment, low extreme vacuum degree, high brazing quality, firm fiber sealing, able to withstand large tension and vibration, and has a long service life, and is suitable for various high vacuum occasions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118915252A_ABST
    Figure CN118915252A_ABST
Patent Text Reader

Abstract

The invention discloses an optical fiber sealing structure in a high vacuum environment and a forming process thereof, the optical fiber sealing structure comprises an optical fiber sealed in a metal tube, and the metal tube is welded in a metal cavity; the metal tube is a nickel tube, the optical fiber is a copper-plated optical fiber, the metal cavity is an austenitic stainless steel cavity, the austenitic stainless steel cavity and the nickel tube are subjected to vacuum brazing by adopting high-temperature brazing filler metal, then the nickel tube and the copper-plated optical fiber are subjected to vacuum brazing by adopting low-temperature brazing filler metal, and the brazing temperature of the high-temperature brazing filler metal is higher than that of the low-temperature brazing filler metal by more than 100 DEG C; the forming process comprises the steps of vacuum brazing and the like. The optical fiber sealing device is compact in structure, small in size, low in vapor pressure, capable of achieving very high ultimate vacuum, high in brazing success rate, stable in brazing quality, firm in optical fiber sealing, capable of bearing large tension and vibration tests, long in service life and capable of being widely applied to various high-vacuum sealing occasions, the quality and the yield of the optical fiber sealing structure are improved through optimization of the forming technology, and the production cost is reduced. And the production cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an optical fiber sealing structure, in particular to an optical fiber sealing structure in a high vacuum environment and a molding process thereof. Background Art

[0002] In the prior art, the most common process for sealing optical fibers is to seal the optical fibers in a metal tube using low-temperature glass solder, and then solder the metal tube to the metal cavity of a laser or detector to lead out the optical fiber.

[0003] As the operating parameters of various large scientific devices such as tokamaks become higher and higher, the vacuum requirements for each subsystem are also increased. Therefore, it is sometimes necessary to vacuum seal the optical fiber when it is led out from the inside of the device. However, the optical fiber sealing method in the above-mentioned prior art has the defects of unstable sealing effect and low connection strength, which makes it difficult to meet the performance requirements in a high vacuum environment. Summary of the invention

[0004] In order to overcome the problems existing in the above optical fiber sealing technology, the purpose of the present invention is to provide an optical fiber sealing structure in a high vacuum environment in a first aspect.

[0005] The invention discloses an optical fiber sealing structure in a high vacuum environment, comprising an optical fiber sealed in a metal tube, wherein the metal tube is welded in a metal cavity; the metal tube is a nickel tube, the optical fiber is a copper-plated optical fiber, and the metal cavity is an austenitic stainless steel cavity. The austenitic stainless steel cavity and the nickel tube are first vacuum brazed with a high-temperature brazing material, and then the nickel tube and the copper-plated optical fiber are vacuum brazed with a low-temperature brazing material. The brazing temperature of the high-temperature brazing material is more than 100°C higher than that of the low-temperature brazing material.

[0006] The second aspect provides a molding process that can effectively ensure the molding quality of the optical fiber sealing structure in the above-mentioned high vacuum environment.

[0007] A molding process for an optical fiber sealing structure in a high vacuum environment, used for manufacturing an optical fiber sealing structure in a high vacuum environment, comprises the following steps: (1) Prepare nickel tube, copper-plated optical fiber and austenitic stainless steel cavity; (2) Insert the nickel tube vertically into the opening of the austenitic stainless steel cavity; (3) Place the high-temperature solder into the high-temperature solder placement groove at the opening of the austenitic stainless steel cavity; (4) Use high temperature brazing filler metal to vacuum braze the nickel tube and austenitic stainless steel cavity; (5) Insert the copper-plated optical fiber vertically into the nickel tube; (6) Place the low-temperature solder into the low-temperature solder placement tank of the nickel tube; (7) Use low-temperature solder to vacuum braze the copper-plated optical fiber and nickel tube.

[0008] The present invention has a compact structure, small size, low vapor pressure, can achieve a very high ultimate vacuum, and at the same time has a high brazing success rate, stable brazing quality, firm optical fiber sealing, can withstand large tension and vibration tests, has a long service life, and can be widely used in various high vacuum sealing occasions.

[0009] The process of the present invention not only reduces the difficulty of processing and assembling, but also has the advantage of stable quality of the optical fiber sealing structure.

[0010] Other features and advantages of the present invention will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0012] Figure 1 Schematic diagram of the structure of the optical fiber sealing structure in a high vacuum environment in this embodiment; Figure 2 This is a schematic diagram of the vacuum brazing structure of the austenitic stainless steel cavity and the nickel tube in this embodiment; Figure 3 This is a schematic diagram of the vacuum brazing structure of the nickel tube and the copper-plated optical fiber in this embodiment; Figure 4 Schematic diagram of the vacuum brazing structure of the optical fiber sealing structure in a high vacuum environment in this embodiment. DETAILED DESCRIPTION

[0013] The preferred embodiments of the present invention are described in detail below in conjunction with the accompanying drawings so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention. Example 1

[0014] The present embodiment provides an optical fiber sealing structure in a high vacuum environment, including an optical fiber sealed in a metal tube, the metal tube is welded in a metal cavity, in order to solve the technical problems described in the background technology, see Figure 1In this embodiment, a nickel tube 1 is used as a metal tube, a copper-plated optical fiber 2 is used as an optical fiber, and an austenitic stainless steel cavity 3 is used as a metal cavity. After vacuum brazing the austenitic stainless steel cavity 3 and the nickel tube 1 with a high-temperature brazing material, the nickel tube 1 and the copper-plated optical fiber 2 are vacuum brazed with a low-temperature brazing material. The brazing temperature of the high-temperature brazing material is more than 100°C higher than the brazing temperature of the low-temperature brazing material.

[0015] According to the brazing structure of austenitic stainless steel cavity-nickel tube-copper-plated optical fiber mentioned above, the brazing of austenitic stainless steel and nickel can generally withstand a high temperature of 1000°C (martensitic and ferritic stainless steels are not suitable for this brazing method), while the temperature withstood by copper-plated optical fibers is basically below 600°C, so high-temperature brazing alloys are selected above 800°C, such as high-copper-based brazing alloys (liquidus 900~1000°C), Au65Cu35 (liquidus 950°C), Au80Ni20 (liquidus 960°C), Ag72Cu28 (liquidus 730°C) and the like.

[0016] Low temperature brazing materials can be selected from Au80Sn20 (liquidus 280℃), Au97Si3 (liquidus 360℃), Au88Ge12 (liquidus 353℃), Au76In24 (liquidus 460℃), etc. The brazing temperature should be about 50℃ higher than the liquidus. Since the workpiece is small, the brazing time can be within 2-10 minutes.

[0017] The above are some of the available solders. In actual use, other solders can also be selected according to the temperature zone of use. Note that in high vacuum environments, metals with high vapor pressure, such as zinc and aluminum, should be avoided as solders. In situations with radiation requirements, activated metals such as silver should be avoided as solders.

[0018] This embodiment is sealed by vacuum brazing. Compared with the existing optical fiber feedthrough, it has the advantages of high vacuum sealing level, high temperature resistance, low vapor pressure, reliable sealing, pure vacuum brazing environment, few weld inclusions, high batch production success rate, and more stable quality. Therefore, it has a wider range of use places and can withstand greater impact and vibration, thereby meeting the use requirements of various large scientific devices. The brazing temperature of high-temperature brazing material is more than 100°C higher than that of low-temperature brazing material, which can ensure that the second brazing will not affect the welding quality of the first brazing.

[0019] See also Figure 2 and Figure 3 Since the optical fiber is generally long, the clearance between the inner diameter d2 of the nickel tube 1 and the outer diameter D2 of the copper-plated optical fiber 2 should be controlled within 0.05~0.1mm, and the fitting depth should not be less than 20mm. If the fitting clearance is enlarged, the fitting depth can be lengthened, which can not only ensure a better siphon effect during soldering, but also make assembly easier.

[0020] A low-temperature solder placement groove 4 (inner diameter d3 and depth L3) is provided on the inner wall of the nickel tube 1. The low-temperature solder contained should be more than twice the solder required by the placement groove to ensure that the copper-plated optical fiber 2 and the nickel tube 1 can be fully combined to ensure sealing and bonding strength.

[0021] Since the nickel tube 1 is shorter and has better processing performance, the fitting clearance between the outer diameter d1 of the nickel tube 1 and the opening D1 of the austenitic stainless steel cavity 3 should be as small as possible, controlled within 0.02-0.05 mm, and the assembly fitting depth should not be less than 3 mm.

[0022] In this embodiment, the nickel tube 1 is inserted into the opening D1 of the austenitic stainless steel cavity 3, and a high-temperature solder placement groove 5 (inner diameter d1 and depth L1) is provided on the inner wall of the opening D1. The high-temperature solder contained should be more than twice the solder required by the placement groove, which can ensure that the brazing strength between the nickel tube 1 and the austenitic stainless steel cavity 3 is higher than the brazing strength of the optical fiber. Example 2

[0023] A molding process for an optical fiber sealing structure in a high vacuum environment, used for manufacturing an optical fiber sealing structure in a high vacuum environment, combined with Figure 4 , including the following steps: (1) Prepare a nickel tube 1, a copper-plated optical fiber 2 and an austenitic stainless steel cavity 3; (2) Insert the nickel tube 1 vertically into the opening D1 of the austenitic stainless steel cavity 3; (3) Place the high-temperature solder into the high-temperature solder placement groove 5 of the opening D1 of the austenitic stainless steel cavity 3; (4) Use high-temperature brazing material to vacuum braze the nickel tube 1 and the austenitic stainless steel cavity 3 (at point A); (5) Insert the copper-plated optical fiber 2 vertically into the nickel tube 1; (6) Place low-temperature solder into the low-temperature solder placement groove 4 of the nickel tube 1; (7) Use low-temperature solder to vacuum braze the copper-plated optical fiber 2 and the nickel tube 1 (at B).

[0024] The above process reduces the difficulty of processing the sealing structure and improves the success rate of processing the sealing structure. At the same time, since metal materials are used for vacuum welding at various locations, by selecting appropriate materials, reducing the vapor pressure, and brazing under a high vacuum environment, bubbles and oxides can be avoided during welding, and air inclusion can be avoided during use, thereby achieving a very high vacuum degree and avoiding adverse effects on the host device in the later stage. The vacuum brazing has high welding strength and stable quality, and also improves the reliability of the optical fiber sealing structure.

[0025] The reason why steps (2) and (5) are inserted vertically is that since the location where the solder is placed is small and the surrounding assembly space is also small, vertical placement can effectively reduce the difficulty of assembly and solder placement. It is also beneficial for the solder to evenly infiltrate and fill the weld after melting, thereby improving the welding success rate.

[0026] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.

Claims

1. An optical fiber sealing structure in a high vacuum environment, comprising an optical fiber sealed in a metal tube, the metal tube being welded in a metal cavity, characterized in that: The metal tube is a nickel tube, the optical fiber is a copper-plated optical fiber, and the metal cavity is an austenitic stainless steel cavity. The austenitic stainless steel cavity and the nickel tube are first vacuum brazed using a high-temperature brazing material, and then the nickel tube and the copper-plated optical fiber are vacuum brazed using a low-temperature brazing material. The brazing temperature of the high-temperature brazing material is more than 100°C higher than the brazing temperature of the low-temperature brazing material.

2. The optical fiber sealing structure in a high vacuum environment according to claim 1, characterized in that: The high temperature solder is a high copper-based solder, Au65Cu35 solder, Au80Ni20 solder or Ag72Cu28 solder.

3. The optical fiber sealing structure in a high vacuum environment according to claim 1, characterized in that: The low-temperature solder is Au80Sn20 solder, Au97Si3 solder, Au88Ge12 solder or Au76In24 solder.

4. The optical fiber sealing structure in a high vacuum environment according to claim 1, 2 or 3, characterized in that: The matching clearance between the inner diameter of the nickel tube and the outer diameter of the copper-plated optical fiber is within 0.05-0.1 mm, and the matching depth is not less than 20 mm.

5. The optical fiber sealing structure in a high vacuum environment according to claim 1, 2 or 3, characterized in that: A low-temperature solder placement groove is provided in the nickel tube, and the low-temperature solder exceeds the solder required by the low-temperature solder placement groove by more than two times.

6. The optical fiber sealing structure in a high vacuum environment according to claim 1, 2 or 3, characterized in that: The fitting clearance between the outer diameter of the nickel tube and the austenitic stainless steel cavity is within 0.02-0.05 mm, and the assembly fitting depth is not less than 3 mm.

7. The optical fiber sealing structure in a high vacuum environment according to claim 4, characterized in that: A high-temperature solder placement groove is provided in the austenitic stainless steel cavity, and the high-temperature solder contained is more than twice the solder required by the high-temperature solder placement groove.

8. A molding process for an optical fiber sealing structure in a high vacuum environment, used for manufacturing an optical fiber sealing structure in a high vacuum environment as claimed in any one of claims 1 to 7, characterized in that: The following steps are involved: (1) Prepare nickel tube, copper-plated optical fiber and austenitic stainless steel cavity; (2) Insert the nickel tube vertically into the opening of the austenitic stainless steel cavity; (3) Place the high-temperature solder into the high-temperature solder placement groove at the opening of the austenitic stainless steel cavity; (4) Use high temperature brazing filler metal to vacuum braze the nickel tube and austenitic stainless steel cavity; (5) Insert the copper-plated optical fiber vertically into the nickel tube; (6) Place the low-temperature solder into the low-temperature solder placement tank of the nickel tube; (7) Use low-temperature solder to vacuum braze the copper-plated optical fiber and nickel tube.