Semiconductor element and manufacturing method thereof
By integrating shallow trench isolation and deep trench isolation in semiconductor components, the problem of isolation between high-voltage zone and low-voltage zone is solved, ensuring the depth of deep trench and improving the voltage control capability, and solving the reduction of component size The problem of post-leakage current and breakdown voltage.
Patent Information
- Application Number
- CN202310614242.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-08
- Filing Date
- 2023-05-29
- Publication Date
- 2024-11-08
AI Technical Summary
The integration of existing high-voltage components and fin structures has difficulties in controlling leakage current and breakdown voltages. Especially when the component size is reduced, the process of existing planar field effect transistor components has faced the limit and is difficult to meet the high voltage zone and low voltage. Requirements for isolation in the area.
A method of integrating shallow trench isolation in low pressure zone and deep trench isolation in high pressure zone is adopted, and deep trench isolation in low pressure zone is etched into a low pressure zone through multiple fin structures, and a deep trench has different sides in high pressure zone. Deep grooves with wall slope, filled with insulating layer for isolation.
Effectively ensure the design depth of deep trench isolation, improve the breakdown voltage control capability and leakage current management in high-voltage zones, reduce the energy band reduction effect and short channel effect of small-sized components, and enhance the gate to carrier Channel control capability.
Smart Images

Figure CN118919533A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing deep trench isolation, and in particular to a method for manufacturing deep trench isolation in a high voltage area and a medium voltage area of a semiconductor element and a structure of the deep trench isolation. Background Art
[0002] With the current semiconductor technology level, the industry has been able to integrate control circuits, memory, low-voltage operating circuits, and high-voltage operating circuits and components on a single chip, thereby reducing costs and improving operating performance. Among them, high-voltage components such as vertical double-diffusion metal-oxide-semiconductor (VDMOS), insulated gate bipolar transistor (IGBT) and lateral-diffusion metal-oxide-semiconductor (LDMOS) are more commonly used because of their better switching efficiency. As known to those familiar with the art, the aforementioned high-voltage components are often required to withstand a higher breakdown voltage and operate at a lower resistance.
[0003] In addition, as the size of components continues to shrink, the development of existing planar field effect transistor components has faced the limit of manufacturing process. In order to overcome the limitation of manufacturing process, it has become the current mainstream development trend to replace planar transistor components with non-planar field effect transistor components, such as fin field effect transistor (Fin FET) components. Since the three-dimensional structure of the fin field effect transistor component can increase the contact area between the gate and the fin structure, the gate can further increase the control of the carrier channel region, thereby reducing the drain induced barrier lowering (DIBL) effect faced by small-sized components and suppressing the short channel effect (SCE). Furthermore, since the fin field effect transistor component has a wider channel width at the same gate length, it can obtain double the drain drive current. Even more, the threshold voltage of the transistor component can be regulated by adjusting the work function of the gate.
[0004] However, as the size of components continues to shrink, there are still many challenges in integrating the existing high-voltage components with the fin structure, such as the control of leakage current and breakdown voltage, etc. Therefore, how to improve the existing high-voltage component architecture is an important issue today. Summary of the invention
[0005] In view of this, the present invention provides a manufacturing method for integrating shallow trench isolation in a low voltage region and deep trench isolation in a high voltage region, and can ensure that the manufactured deep trench isolation can meet the designed depth.
[0006] According to a preferred embodiment of the present invention, a semiconductor element includes a substrate, the substrate includes a high-voltage area and a low-voltage area, a first deep trench isolation is arranged in the high-voltage area, wherein the first deep trench isolation includes a first deep trench arranged in the substrate and a first insulating layer filling the first deep trench, wherein the first deep trench includes a first side wall and a second side wall, the first side wall faces the second side wall, the first side wall is only composed of a first plane and a second plane, the edge of the first plane is connected to the edge of the second plane, the slope of the first plane is different from the slope of the second plane, and a shallow trench isolation is arranged in the low-voltage area, wherein the shallow trench isolation includes a trench arranged on the substrate and a second insulating layer filling the trench, wherein the depth of the shallow trench isolation is less than the depth of the first deep trench isolation.
[0007] According to another preferred embodiment of the present invention, a method for manufacturing a semiconductor element includes, first providing a substrate, the substrate is divided into a high-voltage area and a low-voltage area, wherein a plurality of fin-like structures are arranged in the low-voltage area and the fin-like structures protrude from a first surface of the substrate, and then performing a first etching process, the first etching process includes completely removing at least one fin structure in the fin-like structures and etching the substrate in the high-voltage area to form a first groove in the high-voltage area, after the first etching process, performing a second etching process, wherein the second etching process includes etching the substrate located at the bottom of the first groove to extend a second groove from the bottom of the first groove, the first groove and the second groove together constitute a deep groove, wherein the deep groove includes a first sidewall and a second sidewall, the first sidewall faces the second sidewall, the first sidewall is only composed of a first plane and a second plane, the edge of the first plane is connected to the edge of the second plane, the slope of the first plane is different from the slope of the second plane, after the second etching process, performing a third etching process, wherein the third etching process includes truncating at least one fin structure in the fin-like structure, and finally forming an insulating material to fill the deep groove.
[0008] In order to make the above-mentioned objectives, features and advantages of the present invention more clearly understood, the following is a detailed description of the preferred embodiments and the accompanying drawings. However, the following preferred embodiments and drawings are only for reference and explanation, and are not intended to limit the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figures 1 to 8 A schematic diagram of a method for manufacturing a semiconductor device according to a preferred embodiment of the present invention;
[0010] Fig. 9A An enlarged schematic diagram of deep trench isolation according to a preferred embodiment of the present invention;
[0011] Fig. 9B It is an enlarged schematic diagram of deep trench isolation according to another preferred embodiment of the present invention.
[0012] Explanation of symbols
[0013] 10: Base
[0014] 10a: Surface
[0015] 10b: Surface
[0016] 10c: Surface
[0017] 10d: First surface
[0018] 10e: Third surface
[0019] 10f: Second surface
[0020] 12: Fin structure
[0021] 14a: pad silicon oxide layer
[0022] 14b: pad silicon nitride layer
[0023] 14c: Silicon oxide mask layer
[0024] 16a: organic dielectric layer
[0025] 16b: Patterned mask
[0026] 18a: first groove
[0027] 18b: Second groove
[0028] 19: Photoresist layer
[0029] 20a: Third groove
[0030] 20b: Fourth groove
[0031] 22a: first deep groove
[0032] 22b: Second deep groove
[0033] 24a: organic dielectric layer
[0034] 24b: Patterned mask layer
[0035] 26: Insulation layer
[0036] 28: Groove
[0037] 30a: first gate dielectric layer
[0038] 30b: third gate dielectric layer
[0039] 30c: second gate dielectric layer
[0040] 32a: first gate electrode
[0041] 32b: third gate electrode
[0042] 32c: second gate electrode
[0043] 100:Semiconductor components
[0044] 200:Semiconductor components
[0045] A: Angle
[0046] E: Angle
[0047] B1: Turning Point
[0048] B2: Turning Point
[0049] B3: Turning Point
[0050] B4: Turning Point
[0051] D1: First deep trench isolation
[0052] D2: Second deep trench isolation
[0053] D3: Shallow Trench Isolation
[0054] E1: The first etching process
[0055] E2: Second Etching Process
[0056] E3: The third etching process
[0057] HV: High Voltage Area
[0058] LV: Low Pressure Area
[0059] MV: Medium Voltage Zone
[0060] P1: First plane
[0061] P2: Second plane
[0062] P3: The third plane
[0063] P4: The fourth plane
[0064] P5: First plane
[0065] P6: Second plane
[0066] P7: The third plane
[0067] P8: The fourth plane
[0068] S1: First side wall
[0069] S2: Second side wall
[0070] S3: First side wall
[0071] S4: Second side wall
[0072] T1: High voltage transistor
[0073] T2: Medium voltage transistor
[0074] T3: Fin transistor DETAILED DESCRIPTION
[0075] Figures 1 to 8 A method for manufacturing a semiconductor device according to a preferred embodiment of the present invention is shown. Fig. 9A FIG. 1 is an enlarged schematic diagram of deep trench isolation according to a preferred embodiment of the present invention. Fig. 9B FIG. 1 is an enlarged schematic diagram of deep trench isolation according to another preferred embodiment of the present invention.
[0076] like Figure 1 As shown, a substrate 10 is provided, and the substrate 10 is divided into a high-pressure area HV, a medium-pressure area MV and a low-pressure area LV, wherein a plurality of fin-like structures 12 are arranged in the low-pressure area LV and all the fin-like structures 12 protrude from a surface 10a of the substrate 10, the substrate 10 in the medium-pressure area MV has a surface 10b, and the substrate 10 in the high-pressure area HV has a surface 10c, the surface 10a is lower than the surface 10b, and the surface 10b is lower than the surface 10c. A pad silicon oxide layer 14a, a pad silicon nitride layer 14b and a silicon oxide mask layer 14c are sequentially covered on the surface 10a, the surface 10b and the surface 10c from bottom to top, an organic dielectric layer (ODL) 16a is filled between each fin structure 12 and covers the high voltage area HV, the medium voltage area MV and the low voltage area LV, a patterned mask 16b covers the organic dielectric layer 16a, and at least one position of the fin structure 12 to be removed is defined on the patterned mask 16b corresponding to the low voltage area LV, and at least one predetermined position of deep trench isolation is defined on the patterned mask 16b corresponding to the medium voltage area MV and the high voltage area HV.
[0077] like Figure 2As shown, a first etching process E1 is performed. The first etching process E1 includes completely removing at least one fin structure 12 and etching the substrate 10 in the high voltage region HV and the medium voltage region MV to form a first trench 18a in the high voltage region HV and a second trench 18b in the medium voltage region MV. In detail, the first etching process E1 is performed with a patterned mask 16b (see Figure 1 ) is used as a mask to first transfer the pattern on the patterned mask 16b to the pad silicon oxide layer 14a, the pad silicon nitride layer 14b and the silicon oxide mask layer 14c, and then use the pad silicon oxide layer 14a, the pad silicon nitride layer 14b and the silicon oxide mask layer 14c as masks to etch the substrate 10 and remove the fin structure 12. Since the removal of the fin structure 12 and the formation of the first trench 18a and the second trench 18b are both completed in the first etching process E1, the depth of the first trench 18a and the depth of the second trench 18b will be the same as the height of the removed fin structure 12.
[0078] like Figure 3 As shown, a photoresist layer 19 is formed to cover the low voltage region LV so that the medium voltage region MV and the high voltage region HV are exposed by the photoresist 19, and then a second etching process E2 is performed. The second etching process E2 and the first etching process E1 use the same mask, for example, the pad silicon oxide layer 14a, the pad silicon nitride layer 14b and the silicon oxide mask layer 14c are used as masks. The second etching process E2 includes etching the substrate 10 at the bottom of the first trench 18a to extend a third trench 20a from the bottom of the first trench 18a and includes etching The substrate 10 at the bottom of the second groove 18b is engraved to extend a fourth groove 20b from the bottom of the second groove 18b. The third groove 20a and the fourth groove 20b have the same depth. The first groove 18a and the third groove 20a in the high pressure area together constitute a first deep groove 22a. The depth of the first groove 18a is between 1000 angstroms and 1400 angstroms. The depth of the third groove 20a is between 1000 angstroms and 1400 angstroms. The second groove 18b and the fourth groove 20b in the medium pressure area MV together constitute a second deep groove 22b.
[0079] Since the first deep trench 22a and the second deep trench 22b are both completed by the first etching process E1 and the second etching process E2, the profiles of the two are the same. Fig. 9A Schematic diagram of deep trench isolation according to a preferred embodiment of the present invention, deep trench isolation D1 is formed by filling the first deep trench 22a with an insulating layer, and deep trench isolation D2 is formed by filling the second deep trench 22b with an insulating layer. Fig. 9AAs shown, the first deep trench 22a includes a first sidewall S1 and a second sidewall S2, the first sidewall S1 faces the second sidewall S2, the first sidewall S1 is only composed of a first plane P1 and a second plane P2, the edge of the first plane P1 is connected to the edge of the second plane P2, the slope of the first plane P1 is different from the slope of the second plane P2, that is, the first sidewall S1 has only one turning point (bend) B1, the second sidewall S2 and the first sidewall S1 are symmetrical structures, so the second sidewall S2 also has only one turning point B2. The second deep trench 22b also includes a first sidewall S3 and a second sidewall S4 and a first plane P5 and a second plane P6, and also has the characteristics that the slope of the first plane P5 is different from the slope of the second plane P6, the first sidewall S3 has only one turning point B3, and the second sidewall S4 also has only one turning point B4.
[0080] Please also see Figure 2 and Figure 3 Because the first deep trench 22a and the second deep trench 22b are made by the first etching process E1 and the second etching process E2, etching residues will be produced in the first etching process E1 and attached to the sidewalls of the first trench 18a and the second trench 18b. Therefore, although the first etching process E1 and the second etching process E2 use the same mask, the etching residues will cause the sidewall slope of the trench in the second etching process E2 to be different from the sidewall slope of the trench in the first etching process, thus generating a turning point. Fig. 9A According to different etching conditions, the slope of the first plane P1 / P5 and the slope of the second plane P2 / P6 vary differently. For example, Fig. 9A In FIG. 1 , because of the change in slope, the angle A between the first plane P1 and the second plane P2 is greater than 180 degrees, and the angle E between the first plane P5 and the second plane P6 is greater than 180 degrees. Fig. 9B As shown, due to the change in slope, the angle A between the first plane P1 and the second plane P2 is less than 180 degrees and greater than 90 degrees, and the angle E between the first plane P5 and the second plane P6 is less than 180 degrees and greater than 90 degrees.
[0081] like Figure 4 As shown, the photoresist 19 is removed, and then an organic dielectric layer 24a is formed to fill between the fin structures 12, as well as to fill the first deep trench 22a and the second deep trench 22b, and to cover the pad silicon oxide layer 14a, the pad silicon nitride layer 14b and the silicon oxide mask layer 14c, and then a patterned mask layer 24b is formed to cover the organic dielectric layer 24a, and the patterned mask layer 24b exposes part of the low voltage area LV. In detail, the patterned mask layer 24b defines the position of the fin structure 12 that will be truncated later, and the patterned mask layer 24b completely covers the medium voltage area MV and the high voltage area HV.
[0082] like Figure 5 As shown, a third etching process E3 is performed using the patterned mask layer 24b as a mask, wherein the third etching process E3 includes cutting off at least one of the fin structures 12. Figure 6 As shown, the organic dielectric layer 24a and the patterned mask layer 24b are removed, and then an insulating layer 26 is formed to completely cover the high voltage area HV, the medium voltage area MV and the low voltage area LV. The insulating layer 26 is filled in the first deep trench 22a, the second deep trench 22b and the fin structure 12, and then the upper surface of the insulating layer 26 is ground with the pad silicon nitride 14b as a stop layer until it is flush with the upper surface of the pad silicon nitride layer 14b. At this point, the semiconductor element 100 of the present invention has been completed, and the semiconductor element 100 can be used to form high voltage transistors, medium voltage transistors and fin transistors later.
[0083] Continue Figure 6 The production process, such as Figure 7 As shown, the pad silicon nitride layer 14b and the insulating layer 26 are polished until the pad silicon nitride layer 14b is completely removed. Figure 8 As shown, after several semiconductor manufacturing processes, a high voltage transistor T1 is formed in the high voltage region HV, a medium voltage transistor T2 is formed in the medium voltage region MV, and a fin transistor T3 is formed in the low voltage region LV. At this time, the first deep trench 22a in the high voltage region HV and the insulating layer 26 in the first deep trench 22a serve as a first deep trench isolation D1, and the second deep trench 22b in the medium voltage region MV and the insulating layer 26 in the second deep trench 22b serve as a second deep trench isolation D2. The trenches 28 between the fin structures 12 and the insulating layer 26 in the trenches 28 constitute a shallow trench isolation D3.
[0084] Figure 8 A semiconductor device 200 is shown according to a preferred embodiment of the present invention. The semiconductor device 200 includes a substrate 10, the substrate 10 includes a high voltage region HV, a medium voltage region MV and a low voltage region LV, a first deep trench isolation D1 is arranged in the high voltage region HV, a second deep trench isolation D2 is arranged in the medium voltage region MV, the second deep trench isolation D2 and the first deep trench isolation D1 have the same depth, and a shallow trench isolation D3 is arranged in the low voltage region LV, the depth of the shallow trench isolation D3 is less than the depth of the first deep trench isolation D1. The first deep trench isolation D1 includes a first deep trench 22a arranged in the substrate 10 and an insulating layer 26 filling the first deep trench 22a, the second deep trench isolation D2 includes a second deep trench 22b arranged in the substrate 10 and an insulating layer 26 filling the second deep trench 22b, and the shallow trench isolation D3 includes a trench 28 arranged on the substrate 10 and an insulating layer 26 filling the trench 28.
[0085] A high-voltage transistor T1 is arranged in the high-voltage region HV, wherein the high-voltage transistor T1 includes a first gate dielectric layer 30a arranged on a first surface 10d of the substrate 10 and located on one side of the first deep trench isolation D1 and contacting the first deep trench isolation D1. In the present embodiment, there are two first deep trench isolations D1, and the two first deep trench isolations D1 are respectively on both sides of the first gate dielectric layer 30a, sandwiching the first gate dielectric layer 30a therebetween. A first gate electrode 32a is arranged on the first gate dielectric layer 30a, and the substrate 10 on the side of the first deep trench isolation D1 that does not contact the first gate dielectric layer 30a serves as the source / drain doping region of the high-voltage transistor T1. A medium voltage transistor T2 is disposed in the medium voltage region MV, and two second deep trench isolations D2 define an active region in the medium voltage region MV, wherein the medium voltage transistor T2 is located on the active region in the medium voltage region MV, and the medium voltage transistor MV includes a third gate dielectric layer 30b disposed on a third surface 10e of the substrate 10 and a third gate electrode 32b disposed on the third gate dielectric layer 30b. A fin transistor T3 is disposed in the low voltage region LV, wherein the fin transistor T3 includes at least one fin structure 12 protruding from a second surface 10f of the substrate 10. In the present embodiment, two fin structures 12 are taken as an example, a second gate electrode 32c is disposed across the fin structure 12 and a second gate dielectric layer 30c is disposed between the fin structure 12 and the second gate electrode 32c, and the shallow trench isolation D3 is located on one side of the fin structure 12 or between adjacent fin structures 12.
[0086] Furthermore, the distance between the first surface 30a and the bottom of the substrate 10 is greater than the distance between the second surface 10f and the bottom of the substrate 10, and the distance between the third surface 10e and the bottom of the substrate 10 is greater than the distance between the second surface 10f and the bottom of the substrate.
[0087] As mentioned above, the manufacturing process of the first deep trench isolation D1 and the second deep trench isolation D2 is the same, so they have the same structure. Fig. 9AThe first deep trench isolation D1 includes a first deep trench 22a disposed in the substrate 10 and an insulating layer 26 filling the first deep trench 22a, wherein the first deep trench 22a includes a first side wall S1 and a second side wall S2, the first side wall S1 faces the second side wall S2, the first side wall S1 and the second side wall S2 are symmetrical, the first side wall S1 is composed of only a first plane P1 and a second plane P2, the edge of the first plane P1 is connected to the edge of the second plane P2, the slope of the first plane P1 is different from the slope of the second plane P2, the second side wall S2 is composed of only a third plane P3 and a fourth plane P4, the edge of the third plane P3 is connected to the edge of the fourth plane P4, and the slope of the third plane P3 is different from the slope of the fourth plane P4. In addition, the first side wall P1 has only one turning point B1, and the second side wall P2 has only one turning point B2. According to a preferred embodiment of the present invention, the insulating layer 26 is preferably silicon oxide. In addition, the first plane P1 and the second plane P2 contact the insulating layer 26. Fig. 9A In the example, the angle between the first plane P1 and the second plane P2 is greater than 180 degrees.
[0088] Since the first deep trench isolation D1 and the second deep trench isolation D2 have the same structure, the second deep trench isolation D2 also has a first side wall S3, a second side wall S4, a first plane P5, a second plane P6, a third plane P7 and a fourth plane P8, and the slope of the first plane P5 is different from the slope of the second plane P6, the slope of the third plane P7 is different from the slope of the fourth plane P8, the first side wall S3 has only one turning point B3, the second side wall S4 has only one turning point B4, and the angle E between the first plane P56 and the second plane P6 is greater than 180 degrees.
[0089] Furthermore, according to another preferred embodiment of the present invention, Fig. 9B As shown, depending on changes in manufacturing process parameters, the angle A and the angle E can also be less than 180 degrees and greater than 90 degrees.
[0090] The present invention uses a first etching process to simultaneously remove the fin structure and the upper half of the deep trench, and then uses a second etching process to continuously form the lower half of the deep trench, and finally forms an insulating layer to simultaneously fill the deep trench in the high-voltage area, the deep trench in the medium-voltage area, and the shallow trench in the low-voltage area, and grinds the insulating layer in the high-voltage area, the medium-voltage area, and the low-voltage area. In this way, it can ensure that the deep trench has sufficient depth, and can also combine the manufacturing processes of transistors in the high-voltage area, the medium-voltage area, and the low-voltage area.
[0091] The above descriptions are only preferred embodiments of the present invention. All equivalent changes and modifications made according to the claims of the present invention should fall within the scope of the present invention.
Claims
1. A semiconductor device comprising: the base, which contains areas of high and low pressure; A first deep trench isolation is disposed in the high voltage region, wherein the first deep trench isolation comprises: A first deep trench is disposed in the substrate, wherein the first deep trench comprises a first sidewall and a second sidewall, the first sidewall faces the second sidewall, the first sidewall is only composed of a first plane and a second plane, an edge of the first plane is connected to an edge of the second plane, and a slope of the first plane is different from a slope of the second plane; as well as A first insulating layer filling the first deep trench; A shallow trench isolation is disposed in the low voltage region, wherein the shallow trench isolation comprises: A groove is disposed on the substrate; as well as A second insulating layer is filled into the trench, wherein the depth of the shallow trench isolation is less than the depth of the first deep trench isolation. 2 . The semiconductor device as claimed in claim 1 , wherein the second sidewall of the first deep trench consists only of a third plane and a fourth plane, an edge of the third plane connects to an edge of the fourth plane, and a slope of the third plane is different from a slope of the fourth plane. 3 . The semiconductor device as claimed in claim 1 , wherein the first plane and the second plane contact the first insulating layer, and an angle between the first plane and the second plane is greater than 180 degrees. 4 . The semiconductor device as claimed in claim 1 , wherein the first plane and the second plane contact the first insulating layer, and an angle between the first plane and the second plane is less than 180 degrees and greater than 90 degrees.
5. The semiconductor device according to claim 1, further comprising: a medium pressure zone, disposed on the base; A second deep trench isolation is disposed in the medium voltage region, wherein the second deep trench isolation comprises: a second deep trench disposed in the substrate, wherein the second deep trench comprises a third sidewall and a fourth sidewall, the third sidewall faces the fourth sidewall, the third sidewall is only composed of a fifth plane and a sixth plane, an edge of the fifth plane is connected to an edge of the sixth plane, and a slope of the fifth plane is different from a slope of the sixth plane; and A third insulating layer is filled into the second deep trench, wherein the second deep trench isolation has the same depth as the first deep trench isolation.
6. The semiconductor device according to claim 5, further comprising: A high-voltage transistor is disposed in the high-voltage region, wherein the high-voltage transistor comprises: A first gate dielectric layer is disposed on the first surface of the substrate and is located on one side of the first deep trench isolation and contacts the first deep trench isolation; A first gate electrode is disposed on the first gate dielectric layer; A fin-shaped transistor is disposed in the low-voltage region, wherein the fin-shaped transistor comprises: A fin-shaped structure protrudes from the second surface of the substrate; A second gate electrode is disposed across the fin structure; and A second gate dielectric layer is disposed between the fin structure and the second gate electrode; A medium voltage transistor is disposed in the medium voltage region, wherein the medium voltage transistor comprises: A third gate dielectric layer is disposed on a third surface of the substrate; and The third gate electrode is disposed on the third gate dielectric layer. 7 . The semiconductor device as claimed in claim 6 , wherein a distance between the first surface and a bottom of the substrate is greater than a distance between the second surface and the bottom of the substrate. 8 . The semiconductor device as claimed in claim 1 , wherein the first sidewall has only a first turning point, and the second sidewall has only a second turning point.
9. A method for manufacturing a semiconductor device, comprising: Providing a substrate, wherein the substrate is divided into a high-pressure area and a low-pressure area, wherein a plurality of fin-shaped structures are disposed in the low-pressure area and the fin-shaped structures protrude from a first surface of the substrate; Performing a first etching process, the first etching process comprising completely removing at least one of the fin structures and etching the substrate of the high voltage region to form a first trench in the high voltage region; After the first etching process, a second etching process is performed, wherein the second etching process includes etching the substrate at the bottom of the first trench to extend a second trench from the bottom of the first trench, the first trench and the second trench together form a deep trench, wherein the deep trench includes a first sidewall and a second sidewall, the first sidewall faces the second sidewall, the first sidewall is only composed of a first plane and a second plane, the edge of the first plane is connected to the edge of the second plane, and the slope of the first plane is different from the slope of the second plane; After the second etching process, performing a third etching process, wherein the third etching process includes cutting off at least one fin structure among the fin structures; as well as An insulating layer is formed to fill the deep trench. 10 . The method for manufacturing a semiconductor device as claimed in claim 9 , wherein the first plane and the second plane contact the insulating layer, and an angle between the first plane and the second plane is greater than 180 degrees. 11 . The method for manufacturing a semiconductor element as claimed in claim 9 , wherein the first plane and the second plane contact the insulating layer, and an angle between the first plane and the second plane is less than 180 degrees and greater than 90 degrees. 12 . The method for manufacturing a semiconductor device as claimed in claim 9 , wherein the first sidewall has only a first turning point, and the second sidewall has only a second turning point. 13 . The method for manufacturing a semiconductor device as claimed in claim 9 , wherein a depth of the first trench is between 1000 angstroms and 1400 angstroms, and a depth of the second trench is between 1000 angstroms and 1400 angstroms.
14. A method for manufacturing a semiconductor device as claimed in claim 9, wherein the second sidewall of the deep trench consists only of a third plane and a fourth plane, an edge of the third plane connects to an edge of the fourth plane, and a slope of the third plane is different from a slope of the fourth plane. 15 . The method for manufacturing a semiconductor device as claimed in claim 9 , wherein a trench is disposed between each of the fin-shaped structures, and a depth of the deep trench is greater than a depth of the trench. 16 . The method for manufacturing a semiconductor device as claimed in claim 9 , further comprising forming a photoresist to cover the low voltage area before performing the second etching process.