Shield gate trench MOSFET and power device

By introducing a dual-trench layout and oxide layer into the shielded gate trench MOSFET, an additional conductive channel is solved, and the balance problem between high breakdown voltage and low on-resistance in the prior art is achieved, lower on-conductance Impedance and higher efficiency.

CN118919571APending Publication Date: 2024-11-08HUNAN HONGAN MICROELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411269214.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The prior art is difficult to achieve both high breakdown voltage and low on-resistance in power MOSFET devices, and it is difficult to balance the two.

Method used

The shielded gate trench MOSFET structure adopts a dual-trench layout, which forms two conductive channels to enhance the device by adding a shallow trench into a traditional deep trench and setting an oxide layer and a gate polysilicon layer within the shallow trench. on-resistance performance.

Benefits of technology

While maintaining a high breakdown voltage, the device's on-impedance is significantly reduced, the device's efficiency and performance is improved, and the same on-impedance specification can be achieved in smaller component sizes, reducing switching losses and improving reliability sex.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919571A_ABST
    Figure CN118919571A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to a shield gate trench MOSFET (Metal-Oxide-Semiconductor Field Effect Transistor) and a power device. The shield gate trench MOSFET comprises a substrate, an epitaxial layer, a first trench, a second trench, an oxide layer, a source polycrystalline silicon layer and a gate polycrystalline silicon layer, wherein an epitaxial layer is arranged on one side of the substrate; the first groove and the second groove are formed in the epitaxial layer; the oxide layer and the grid polycrystalline silicon layer are arranged in the second groove, and the grid polycrystalline silicon layer is arranged on the oxide layer; wherein an active region and a well region are respectively formed in one end, far away from the substrate, of the epitaxial layer, and the well region is arranged on one side, close to the substrate, of the source region; and the second groove passes through the source region and the well region and extends to the surface of one side, close to the substrate, of the well region. According to the embodiment, the first groove and the second groove are arranged, so that the conduction impedance of the device is reduced, and the efficiency and the performance of the device are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a shielded gate trench MOSFET and a power device. Background Art

[0002] With the growth of demand for electronic consumer products, the demand for power MOSFET devices is increasing, such as disk drives, automotive electronics, power devices, etc. Trench MOSFET (Trench MOS) is widely used in the field of low-voltage power due to its high device integration, low on-resistance, low gate-drain charge density, and large current capacity, thus having low switching losses and fast switching speed.

[0003] However, the prior art does not have an obvious technical solution that can enable a power MOSFET device to simultaneously obtain a high breakdown voltage and a low on-resistance, and achieve a balance between the high breakdown voltage and the low on-resistance. Summary of the invention

[0004] Therefore, in order to overcome at least some of the defects and shortcomings of the above prior art, an embodiment of the present invention proposes a shielded gate trench MOSFET, which can reduce the on-resistance of the shielded gate trench MOSFET, thereby improving the efficiency and performance of the device.

[0005] On the one hand, a shielded gate trench MOSFET proposed in an embodiment of the present invention comprises: a substrate, an epitaxial layer, a first trench, a second trench, an oxide layer, a source polysilicon layer and a gate polysilicon layer; wherein an epitaxial layer is provided on one side of the substrate; the first trench and the second trench are formed in the epitaxial layer, the first trench and the second trench are spaced apart, and the first trench and the second trench extend along the thickness direction of the epitaxial layer; the oxide layer, the source polysilicon layer and the gate polysilicon layer are provided in the first trench, wherein the oxide layer The source polysilicon layer is wrapped by a layer to isolate the source polysilicon layer from the gate polysilicon layer and the epitaxial layer; the oxide layer and the gate polysilicon layer are arranged in the second trench, and the gate polysilicon layer is arranged on the oxide layer; wherein an active region and a well region are respectively formed in one end of the epitaxial layer away from the substrate, and the well region is arranged on a side of the source region close to the substrate; the first trench passes through the source region and the well region, and the second trench passes through the source region and the well region, wherein the depth of the first trench is greater than the depth of the second trench.

[0006] In one embodiment of the present invention, the shielded gate trench MOSFET also includes a surface metal layer, the surface metal layer is arranged on a side of the epitaxial layer away from the substrate, and a contact hole is formed in the epitaxial layer; the contact hole is located between the first trench and the second trench, and the contact hole is filled with the surface metal layer.

[0007] In one embodiment of the present invention, the depth of the contact hole is 0.2-0.5 micrometers, and the width of the contact hole is 0.05-0.5 micrometers.

[0008] In one embodiment of the present invention, a height of the gate polysilicon layer away from the surface of the substrate is lower than a height of the epitaxial layer away from the surface of the substrate.

[0009] In one embodiment of the present invention, a distance between a surface of the epitaxial layer away from the substrate and a surface of the gate polysilicon layer away from the substrate is 500-1500 angstroms.

[0010] In one embodiment of the present invention, the gate polysilicon layer in the first trench corresponds to the gate polysilicon layer in the second trench, and the gate polysilicon layer in the first trench has the same height as the gate polysilicon layer in the second trench.

[0011] In one embodiment of the present invention, the depth of the second groove is 0.2-1.5 microns.

[0012] In one embodiment of the present invention, the width of the second groove is 0.1-2 microns.

[0013] In one embodiment of the present invention, the depth of the first groove is 2-10 microns.

[0014] On the other hand, an embodiment of the present invention provides a power device, including: the shielded gate trench MOSFET as described above.

[0015] As can be seen from the above, the above technical features of the present invention can have the following beneficial effects: the present application sets a first trench and a second trench, the first trench passes through the source region and the well region and extends to the vicinity of the substrate, and the second trench passes through the source region and the well region and extends to the surface of the well region on one side close to the substrate, that is, the depth of the first trench exceeds the depth of the second trench. When a voltage is applied to the gate electrode of the device, the gate polysilicon layer in the first trench and the gate polysilicon layer in the second trench simultaneously reach the MOSFET turn-on voltage. The trench sidewall near the gate polysilicon layer in the first trench forms a conductive channel, and the trench sidewall near the gate polysilicon layer in the second trench also forms a conductive channel. Therefore, when the gate electrode voltage is applied, the conductive channel density doubles when the device is turned on, thereby achieving the purpose of reducing the channel resistance of the shielded gate trench MOSFET, thereby reducing the on-resistance of the device and improving the efficiency and performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.

[0017] Figure 1 A schematic structural diagram of a shielded gate trench MOSFET provided in the first embodiment of the present invention.

[0018] Figure 2a-2f A flowchart of a method for manufacturing a shielded gate trench MOSFET provided in accordance with a second embodiment of the present invention.

[0019]

Description of the accompanying drawings

[0020] 10: shielded gate trench MOSFET; 100: substrate; 101: epitaxial layer: 102: source region; 103: well region; 111: first trench; 112: second trench; 120: oxide layer; 121: silicon nitride; 130: source polysilicon layer; 140: gate polysilicon layer; 150: contact hole; 160: surface metal layer. DETAILED DESCRIPTION

[0021] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] Power MOSFET has high input impedance, small drive current, fast switching speed, good high temperature characteristics, etc. Its advantages are widely used in the field of power electronics. High breakdown voltage, large current, and low on-resistance are the most critical indicators of power MOSFET. The breakdown voltage and on-resistance are related. In the MOSFET design process, high breakdown voltage and low on-resistance cannot be obtained at the same time, and a balance needs to be struck between the two.

[0023] In order to obtain a higher breakdown voltage and lower on-resistance as much as possible, a new type of split-gate structure MOSFET device came into being. Compared with the ordinary trench MOSFET structure, its main feature is the addition of a deep trench split gate short-circuited with the source, and then the lateral electric field between the split gates is used to improve the device's withstand voltage.

[0024] Currently, SGT (Shield Gate Trench) devices are a new type of shielded gate trench MOSFET structure. They adopt the charge balance principle to alleviate the contradiction between the device breakdown voltage and on-resistance. The optimization of breakdown voltage and on-resistance is mainly based on the improvement of process capabilities. For example, trench etching process and polycrystalline filling process with higher aspect ratio make the unit cell intercept of the device smaller, thereby optimizing the on-resistance.

[0025] [First embodiment]

[0026] In order to further reduce the on-resistance and make the device performance more superior, the present application proposes a shielded gate trench MOSFET device with a double trench layout, which is different from the traditional SGT structure in that, Figure 1 As shown, the shielded gate trench MOSFET device proposed in the present application adds a shallow trench (i.e., the second trench) between the two existing deep trenches (i.e., the first trench), and an oxide layer (e.g., a gate oxide layer) and gate polysilicon are arranged in the shallow trench. Since the added shallow trench occupies the position of the contact hole in the original SGT device structure, the contact hole of the device structure in the present application is changed from one to two, which are respectively placed on both sides of the shallow trench.

[0027] like Figure 1 As shown, an embodiment of the present invention provides a shielded gate trench MOSFET 10. The shielded gate trench MOSFET 10 includes, for example: a substrate 100, an epitaxial layer 101, a first trench 111, a second trench 112, an oxide layer 120, a source polysilicon layer 130, and a gate polysilicon layer 140;

[0028] An epitaxial layer 101 is disposed on one side of the substrate 100 ; the first trench 111 and the second trench 112 are formed in the epitaxial layer 101 .

[0029] The substrate 100 is, for example, a substrate sheet, which is the basis for manufacturing a shielded gate trench MOSFET, and other subsequent components such as an epitaxial layer 101 need to be grown on the substrate 100. The substrate sheet can be, for example, a wafer made of semiconductor single crystal material, which is an important step in semiconductor manufacturing and lays the foundation for subsequent circuit etching.

[0030] The first trench 111 is formed in the epitaxial layer 101, and then source polysilicon is deposited in the first trench 111, and the source polysilicon is etched back in the first trench 111 to form a source polysilicon layer 130, that is, the source polysilicon is etched back in the first trench 111 to form a source polysilicon layer 130, and then an isolation oxide layer is deposited, and then the second trench 112 is etched.

[0031] The first groove 111 and the second groove 112 can be formed, for example, by etching on the epitaxial layer 101, and the first groove 111 and the second groove 112 are spaced apart from each other, and the first groove 111 and the second groove 112 extend along the thickness direction of the epitaxial layer 101; the oxide layer 120, the source polysilicon layer 130 and the gate polysilicon layer 140 are arranged in the first groove 111, wherein the oxide layer 120 wraps the source polysilicon layer 130 to isolate the source polysilicon layer 130 from the gate polysilicon layer 140 and the epitaxial layer 101, that is, the upper part (including the top), both sides and the lower part (including the bottom) of the source polysilicon layer 130 all have the oxide layer 120.

[0032] The oxide layer 120 and the gate polysilicon layer 140 are disposed in the second trench 112, and the gate polysilicon layer 140 is disposed on the oxide layer 120. The source region 102 and the well region 103 are respectively formed in one end of the epitaxial layer 101 away from the substrate 100, and the well region 103 is disposed on a side of the source region 102 close to the substrate 100; the first trench 111 passes through the source region 102 and the well region 103, and the second trench 112 passes through the source region 102 and the well region 103, wherein the depth of the first trench 111 is greater than the depth of the second trench 112.

[0033] It is only necessary to grow or deposit a gate oxide layer in the second trench 112 , then deposit gate polysilicon, and then etch back the gate polysilicon to form a gate polysilicon layer 140 in the second trench 112 .

[0034] The shielded gate trench MOSFET 10 also includes a well region (P-body) 103 and a source region (N+Plus) 102, wherein the well region 103 and the source region 102 are both located in the epitaxial layer 101, the source region 102 is close to the side of the epitaxial layer 101 away from the substrate 100, and the well region 103 is arranged on the side of the source region 102 close to the substrate, that is, the well region 103 is arranged below the source region 102.

[0035] In this embodiment, by providing the first trench 111 and the second trench 112, the gate polysilicon in the first trench 111 and the gate polysilicon in the second trench 112 are at the same potential, and the gate electrode of the shielded gate trench MOSFET 10 is interconnected with the gate polysilicon layer 140 in the first trench 111 and the gate polysilicon layer 140 in the second trench 112 respectively. When a voltage is applied to the gate electrode of the shielded gate trench MOSFET 10, the gate polysilicon layer 140 in the first trench 111 and the gate polysilicon layer 140 in the second trench 112 will reach the gate electrode voltage at the same time. The first trench sidewall near the gate polysilicon layer 140 in the first trench 111 forms a conductive channel, and the second trench sidewall near the gate polysilicon layer 140 in the second trench 112 also forms a conductive channel. Therefore, when the gate electrode voltage is applied, the conductive channel density doubles when the shielded gate trench MOSFET is turned on, thereby achieving the purpose of reducing the channel resistance of the shielded gate trench MOSFET.

[0036] Furthermore, the shielded gate trench MOSFET 10 further includes a surface metal layer 160, a contact hole 150 is formed in the epitaxial layer 101; the contact hole 150 is located between the first trench 111 and the second trench 112, the surface metal layer 160 is arranged on a side of the epitaxial layer 101 away from the substrate 100, and the surface metal layer 160 is filled in the contact hole 150. The surface metal layer 160 is, for example, a single layer of aluminum alloy, and the contact hole 150 is filled with metal tungsten and interconnected with the surface metal layer 160, so as to realize electrical connection between the surface metal layer 160 and the gate polysilicon layer 140 and the source polysilicon layer 130.

[0037] The surface metal layer 160 can be formed into a MOSFET device with a complete structure through the existing SGT device process. The depth of the contact hole is 0.2-0.5 microns, and the width of the contact hole is 0.05-0.5 microns.

[0038] Furthermore, the height of the gate polysilicon layer 140 away from the surface of the substrate 100 (that is, the upper surface of the gate polysilicon layer 140) is lower than the height of the epitaxial layer 101 away from the surface of the substrate (that is, the upper surface of the epitaxial layer 101), that is, the height of the gate polysilicon layer 140 formed by etching back in the first trench 111 and the second trench 112 is lower than the height of the epitaxial layer 101, or the height of the gate polysilicon layer 140 formed by etching back in the first trench 111 and the second trench 112 is lower than the height of the silicon plane, which is the height of the epitaxial layer 101 after the epitaxial layer 101 is grown on the substrate 100. After the epitaxial layer 101 undergoes processes such as oxidation and etching, the height of the epitaxial layer 101 will be reduced.

[0039] Specifically, the distance between the surface of the epitaxial layer 101 away from the substrate 100 and the surface of the gate polysilicon layer 140 away from the substrate 100 is 500-1500 angstroms.

[0040] Furthermore, the gate polysilicon layer 140 in the first trench 111 corresponds to the gate polysilicon layer 140 in the second trench 112 , and the gate polysilicon layer 140 in the first trench 111 and the gate polysilicon layer 140 in the second trench 112 have the same height. Of course, the height of the gate polysilicon layer 140 in the first groove 111 and the gate polysilicon layer 140 in the second groove 112 may also be basically the same. Considering the actual manufacturing and production conditions, there may be a slight difference in height between the two, but the difference is not large, so the height of the gate polysilicon layer 140 in the first groove 111 and the gate polysilicon layer 140 in the second groove 112 are basically the same. The purpose of setting the height of the gate polysilicon layer 140 in the first groove 111 and the gate polysilicon layer 140 in the second groove 112 to be basically the same is to make the gate polysilicon layer 140 in the first groove 111 and the gate polysilicon layer 140 in the second groove 112 have the same potential, and the conductive channel density is doubled when the device is turned on, thereby achieving the purpose of reducing the channel resistance of the shielded gate trench MOSFET.

[0041] In a preferred embodiment of the present application, the depth range of the first groove 111 is 2 microns to 10 microns. The depth range of the second groove 112 is 0.2 microns to 1.5 microns. By limiting the depth range of the first groove 111 and the second groove 112, this embodiment can ensure that the side walls of the first groove 111 and the second groove 112 are not damaged during subsequent steps, thereby further ensuring the performance of the device. At the same time, by limiting the depth range of the second groove 112 and the depth range of the first groove, and the depth of the second groove 112 is less than the depth of the first groove 111, it can be ensured that the height of the gate polysilicon layer 140 obtained by etching back in the first groove 111 is consistent with that of the gate polysilicon layer 140 obtained by etching back in the second groove 112, thereby further reducing the channel resistance to achieve lower on-resistance.

[0042] Furthermore, the width of the second groove 112 is 0.1-2 microns. By limiting the width of the second groove 112 and the width of the contact hole 150 , the width range of the second groove 112 and the contact hole 150 will not exceed the spacing formed between the two first grooves 111 .

[0043] Furthermore, the breakdown voltage of the shielded gate trench MOSFET 10 is 30-200 volts. By performing simulation experiments on the device of the present application and the SGT device of the prior art, the simulation results shown in Table 1 are obtained:

[0044]

[0045] Table 1

[0046] As can be seen from Table 1 above, the existing SGT structure and the present application both use the same epitaxial material, and the device breakdown voltage remains unchanged at 68 volts when the first trench parameters remain unchanged. However, due to the introduction of the second trench in the device structure of the present application, the device has a lower resistance when it is on and performs better, and the RSP is reduced by about 10.3% compared with the original traditional structure. That is, the device of the present application can achieve a lower on-resistance under the same breakdown voltage.

[0047] By setting a second groove 112 between the two first grooves 111, the device of the present application can further reduce the on-resistance while keeping the breakdown voltage unchanged, compared with the existing SGT device. At the same time, the device of the present application can use a smaller component size to achieve the same on-resistance specification as the SGT device in the prior art, and can obtain better other dynamic parameters to achieve lower switching losses, so as to further improve the reliability of the device.

[0048] [Second embodiment]

[0049] like Figure 2a-2fAs shown, this embodiment provides a manufacturing process of a shielded gate trench MOSFET. The specific structure of the shielded gate trench MOSFET can refer to the shielded gate trench MOSFET described in the first embodiment above, and the details are not repeated here.

[0050] Specifically, Figure 2a As shown, an epitaxial layer 101 is grown on a substrate 100, and an oxide layer-silicon nitride-oxide layer is deposited on the epitaxial layer 101 to form a hard mask. This structure is the basis for generating a shielded gate trench MOSFET and is a basic condition for ensuring the performance of MOSFET devices. The thickness of the epitaxial layer 101 is determined according to the withstand voltage between the drain and source. A structure of an oxide layer-silicon nitride-oxide layer of a certain thickness is deposited on the upper surface of the epitaxial layer to form a hard mask, thereby protecting the non-groove area on the epitaxial layer 101 when forming the groove.

[0051] Then, the epitaxial layer 101 is trench-etched, and a structure of an oxide layer 120-silicon nitride 121-oxide layer 120 is first deposited to form a hard mask, for example, Figure 2a The structure of the oxide layer 120 and the silicon nitride 121 shown is that the epitaxial layer 101 is etched on the hard mask using a trench mask to obtain a first trench 111, and the depth of the first trench ranges from 2 microns to 10 microns.

[0052] Secondly, if Figure 2b As shown, a field oxide layer (i.e., oxide layer 120) is grown on the surface of the first trench 111 and the epitaxial layer 101 as a field dielectric layer. Then, source polysilicon is filled in the field dielectric layer and the source polysilicon is etched back. First, the field dielectric layer in the first trench 111 is filled with source polysilicon, and the source polysilicon is etched back to obtain a source polysilicon with a suitable height, and a source polysilicon layer 130 is formed, so that the height of the source polysilicon layer 130 is less than the depth of the first trench 111.

[0053] like Figure 2c As shown, the device with the source polysilicon layer 130 is then subjected to HDPCVD (high-density plasma chemical vapor deposition) method to deposit an oxide layer to obtain an oxide layer 120 for isolation.

[0054] like Figure 2d As shown, the second trench 112 is etched again to remove part of the isolation oxide layer, and then a gate oxide layer 120 is grown on the isolation oxide layer in the first trench 111 , and a gate oxide layer is grown on the isolation oxide layer in the second trench 112 .

[0055] like Figure 2eAs shown, gate polysilicon is deposited on the gate oxide layer, and a gate polysilicon layer 140 containing gate polysilicon is obtained by back etching, and the distance between the upper surface of the gate polysilicon layer 140 and the silicon plane of the epitaxial layer 101 (that is, the upper surface of the epitaxial layer 101 before etching) is 500-1500 angstroms, so as to form the gate polysilicon layer 140 in the first trench 111 and the second trench 112.

[0056] like Figure 2f As shown, this process is the same as the rest of the manufacturing process of the SGT device in the prior art, and a MOSFET device with a complete structure is finally formed through this process.

[0057] The present application reduces the variability of the process and only adds one etching process step for the second trench 112, that is, further reducing the on-resistance with minimal process variation. The optimization of the on-component of the shielded gate trench MOSFET 10 is simpler.

[0058] [Third embodiment]

[0059] In this embodiment, the power device includes the shielded gate trench MOSFET described in the first embodiment above, and the power device is, for example, a low voltage to medium voltage power MOSFET, a high efficiency DC-DC converter, a synchronous rectification controller, etc.

[0060] The specific effects of the power device may be as described in the first embodiment above, and will not be described in detail here.

[0061] In addition, it can be understood that the aforementioned embodiments are only exemplary descriptions of the present invention. Under the premise that the technical features do not conflict, the structures do not contradict, and the purpose of the present invention is not violated, the technical solutions of the various embodiments can be arbitrarily combined and used in combination.

[0062] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A shielded gate trench MOSFET (10), It is characterized in that include: A substrate (100), an epitaxial layer (101), a first trench (111), a second trench (112), an oxide layer (120), a source polysilicon layer (130) and a gate polysilicon layer (140); An epitaxial layer (101) is provided on one side of the substrate (100); the first trench (111) and the second trench (112) are formed in the epitaxial layer (101); the first trench (111) and the second trench (112) are arranged at intervals; the first trench (111) and the second trench (112) extend along the thickness direction of the epitaxial layer (101); the oxide layer (120), the source layer (121) and the substrate (100) are provided in the first trench (111); The source polysilicon layer (130) and the gate polysilicon layer (140) are provided in the second trench (112), wherein the oxide layer (120) wraps the source polysilicon layer (130) to isolate the source polysilicon layer (130) from the gate polysilicon layer (140) and the epitaxial layer (101); the oxide layer (120) and the gate polysilicon layer (140) are provided in the second trench (112), and the gate polysilicon layer (140) is provided on the oxide layer (120); An active region (102) and a well region (103) are respectively formed in one end of the epitaxial layer (101) away from the substrate (100), and the well region (103) is arranged on a side of the source region (102) close to the substrate (100); the first trench (111) passes through the source region (102) and the well region (103), and the second trench (112) passes through the source region (102) and the well region (103), and the depth of the first trench (111) is greater than the depth of the second trench (112).

2. The shielded gate trench MOSFET (10) according to claim 1, It is characterized in that The shielded gate trench MOSFET (10) further comprises a surface metal layer (160), the surface metal layer (160) being arranged on a side of the epitaxial layer (101) away from the substrate (100), a contact hole (150) being formed in the epitaxial layer (101); the contact hole (150) being located between the first trench (111) and the second trench (112), the contact hole (150) being filled with the surface metal layer (160).

3. The shielded gate trench MOSFET (10) according to claim 2, It is characterized in that The depth of the contact hole (150) is 0.2-0.5 micrometers, and the width of the contact hole (150) is 0.05-0.5 micrometers.

4. The shielded gate trench MOSFET (10) according to claim 1, It is characterized in that The height of the gate polysilicon layer (140) away from the surface of the substrate (100) is lower than the height of the epitaxial layer (101) away from the surface of the substrate (100).

5. The shielded gate trench MOSFET (10) according to claim 4, It is characterized in that The distance between the surface of the epitaxial layer (101) away from the substrate (100) and the surface of the gate polysilicon layer (140) away from the substrate (100) is 500-1500 angstroms.

6. The shielded gate trench MOSFET (10) according to claim 5, It is characterized in that The gate polysilicon layer (140) in the first trench (111) corresponds to the gate polysilicon layer (140) in the second trench (112), and the gate polysilicon layer (140) in the first trench (111) and the gate polysilicon layer (140) in the second trench (112) have the same height.

7. The shielded gate trench MOSFET (10) according to any one of claims 1 to 6, It is characterized in that The depth of the second groove (112) is 0.2-1.5 microns.

8. The shielded gate trench MOSFET (10) according to claim 7, It is characterized in that The width of the second groove (112) is 0.1-2 microns.

9. The shielded gate trench MOSFET (10) according to claim 7, It is characterized in that The depth of the first groove (111) is 2-10 microns.

10. A power device, It is characterized in that include: A shielded gate trench MOSFET as claimed in any one of claims 1 to 9.