Display device including light emitting element

In the manufacturing process of the inorganic light emitting diode, mask pattern and laminated etching technology are used to ensure that the side surface of the light emitting element is flat, solving the problem of disconnection when connected to the contact electrode, and improving the reliability of the element.

CN118919625APending Publication Date: 2024-11-08SAMSUNG DISPLAY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410986285.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2018-06-11
Filing Date
2019-05-20
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing inorganic light-emitting diodes are prone to unsmoothing side surfaces during separation, resulting in open circuit failures when in contact with the contact electrode.

Method used

By forming a mask pattern and an open area on the substrate, a conductive semiconductor layer and an active material layer are laminated, the element rod is etched and separated from the substrate by an insulating film, ensuring that the side surface is flat and avoiding disconnection of contact electrode material.

Benefits of technology

The flat side surface separation of the light emitting element is achieved, preventing the contact electrode material from being disconnected, and improving the reliability of the light emitting element and the stability of the display device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919625A_ABST
    Figure CN118919625A_ABST
Patent Text Reader

Abstract

The invention relates to a display device including a light emitting element. The display device includes a base substrate, a first electrode and a second electrode spaced apart from each other, a first contact electrode on an upper surface of the first electrode, a second contact electrode on an upper surface of the second electrode, and at least one light emitting element in a region where the first electrode and the second electrode are spaced apart from each other. Wherein both side surfaces of the light-emitting element, which are in contact with the first contact electrode and the second contact electrode, have a flat shape so as to be parallel to a surface perpendicular to the base substrate, and wherein one of the two side surfaces of the light-emitting element, which is separated from the substrate on which the light-emitting element is pre-formed, has a surface roughness of 8 nm Ra to 12 nm Ra.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to and the benefit of Korean Patent Application No. 10-2018-0066819 filed on June 11, 2018, in the Korean Intellectual Property Office, the disclosure of which is incorporated herein in its entirety by reference. Technical Field

[0003] Aspects of embodiments of the present invention relate to a method of manufacturing a light emitting element, and a display device including the light emitting element. Background Art

[0004] As multimedia has developed, the importance of display devices has increased. Therefore, various types of display devices, such as organic light emitting displays and liquid crystal displays (LCDs), have been used.

[0005] A display device for displaying an image includes a display panel, such as an organic light emitting display panel or a liquid crystal display panel. In the display panel, the organic light emitting display panel includes an organic light emitting element, such as a light emitting diode (LED). The light emitting diode (LED) includes an organic light emitting diode (OLED) using an organic material as a fluorescent material and an inorganic light emitting diode using an inorganic material as a fluorescent material.

[0006] Organic light emitting diodes (OLEDs) using organic materials as fluorescent materials of light emitting elements have the advantages of simple manufacturing process and flexible display elements. However, it is known that organic materials are susceptible to high temperature driving environment and have relatively low blue light efficiency.

[0007] In contrast, inorganic light-emitting diodes using inorganic semiconductors as fluorescent materials have advantages in that they are durable even in high temperature environments and have higher blue light efficiency than organic light-emitting diodes (OLEDs). In addition, a migration method using a dielectrophoresis (DEP) method has been developed in the manufacturing process that has been pointed out as having limitations on conventional inorganic light-emitting diodes. Therefore, research on inorganic light-emitting diodes having superior durability and efficiency compared to organic light-emitting diodes is continuing.

[0008] Inorganic light emitting diodes can be manufactured by growing a semiconductor layer doped with n-type or p-type impurities and an inorganic fluorescent material layer on a substrate, forming rods with a specific shape, and then separating the rods. However, when a physical method is used to separate light emitting elements, there is a problem that the light emitting elements may be separated so that their longitudinal side surfaces are not smooth. When one side surface of a light emitting element is rough or has an uneven shape or roughness, there may be a problem of an open circuit failure when the light emitting element contacts the contact electrode. Summary of the invention

[0009] According to an aspect of an embodiment of the present invention, a light-emitting element having a flat end connected to a contact electrode and a method for manufacturing the light-emitting element are provided. According to another aspect of an embodiment of the present invention, a light-emitting element having a smooth side surface, a method for manufacturing the light-emitting element and a display device including the light-emitting element are provided.

[0010] According to another aspect of an embodiment of the present invention, there is provided a display device including a light emitting element, in which a problem of disconnection or open failure of an electrode material occurring when the light emitting element is connected to a contact electrode can be eliminated.

[0011] However, aspects of the present invention are not limited to those set forth herein. The above and other aspects of the present invention will become more apparent to those of ordinary skill in the art to which the present invention pertains by referring to the detailed description of the present invention given below.

[0012] According to one or more exemplary embodiments of the present disclosure, a method for manufacturing a light-emitting element includes: preparing a lower plate including a substrate and a first sub-conductive semiconductor layer located on the substrate; forming a first mask layer including a mask pattern and an opening area, wherein the mask pattern is located on at least a portion of the lower plate to be spaced apart from each other, and the mask patterns are spaced apart from each other in the opening area; stacking a first conductive semiconductor layer, an active material layer, and a second conductive semiconductor layer on the first mask layer to form an element stack; etching the element stack in a vertical direction to form an element rod; and removing the mask pattern to separate the element rod from the lower plate.

[0013] In an exemplary embodiment, forming the element stack includes: growing semiconductor crystals of the first sub-conductive semiconductor layer in a vertical direction in opening regions of a mask pattern spaced apart from each other; growing semiconductor crystals in a horizontal direction on a mask pattern of the first mask layer; and fusing grains of the semiconductor crystals on the mask pattern.

[0014] In an exemplary embodiment, forming an element rod includes: forming a second mask layer on the element stack, the second mask layer including a hard mask layer and a nanopattern layer, in which nanopatterns are spaced apart from each other on the hard mask layer; vertically etching areas where the nanopatterns are spaced apart from each other to form holes; and removing the second mask layer.

[0015] In an exemplary embodiment, the method of manufacturing a light emitting element further includes forming an electrode material layer between the element stack and the hard mask layer.

[0016] In an exemplary embodiment, forming the light emitting element includes: forming an insulating film on a side surface of an element rod; and dissolving the mask pattern to separate the element rod provided with the insulating film from a lower plate.

[0017] In an exemplary embodiment, the light emitting element includes a separation surface at which the element rod is separated from the lower plate, and the separation surface is substantially flat and parallel to the upper surface of the second conductive semiconductor layer.

[0018] In an exemplary embodiment, the separation surface of the light emitting element has a surface roughness of 8 nm Ra to 12 nm Ra.

[0019] In an exemplary embodiment, the mask pattern includes a silicon oxide (SiO x ), silicon nitride (SiN x ), silicon oxynitride (SiO x N y ), at least one of ITO, ZnO, IGO, graphene and graphene oxide.

[0020] In an exemplary embodiment, the mask pattern has a structure in which at least one layer is stacked, an insulating material layer including an insulating material is located on a surface contacting a lower plate, and a conductive material layer including a conductive material is located on the insulating material layer.

[0021] In an exemplary embodiment, while the mask pattern is formed, a conductive material layer is attached to the light emitting element to form an electrode layer.

[0022] In an exemplary embodiment, in the first mask layer, the opening in the opening region has a circular cross-sectional structure.

[0023] In an exemplary embodiment, in the first mask layer, the mask patterns are located between one side of the lower plate and the other side thereof facing the one side, and are arranged to be spaced apart from each other in a second direction perpendicular to the first direction to form openings in the opening area, wherein the mask patterns are connected in the first direction.

[0024] In an exemplary embodiment, in the first mask layer, a ratio of a length of the mask pattern measured in the second direction to a length of the opening measured in the second direction is 3:1 to 5:1.

[0025] According to one or more exemplary embodiments of the present disclosure, a display device includes a base substrate, a first electrode and a second electrode, a first contact electrode, a second contact electrode, and at least one light-emitting element, wherein the first electrode and the second electrode are spaced apart from each other; the first contact electrode is located on an upper surface of the first electrode; the second contact electrode is located on an upper surface of the second electrode; at least one light-emitting element is located in a region where the first electrode and the second electrode are spaced apart from each other, wherein two side surfaces of the light-emitting element in contact with the first contact electrode and the second contact electrode have a flat shape so as to be parallel to a surface perpendicular to the base substrate.

[0026] In an exemplary embodiment, the light emitting element includes an n-type semiconductor layer, an active layer, a p-type semiconductor layer, and an insulating film, wherein the active layer is located on the n-type semiconductor layer to emit light in a specific band; the p-type semiconductor layer is located on the active layer; the insulating film surrounds the side surfaces of the n-type semiconductor layer, the p-type semiconductor layer, and the active layer, wherein the length measured in the direction in which the n-type semiconductor layer and the p-type semiconductor layer are stacked is longer than the spacing length between the first electrode and the second electrode.

[0027] In an exemplary embodiment, a contact surface between the light emitting element and the first contact electrode or the second contact electrode includes at least one surface perpendicular to the base substrate.

[0028] In an exemplary embodiment, the display device further includes at least one passivation layer on an outer surface of the insulating film of the light emitting element. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] The above and other aspects and features of the present invention will become more apparent through a more detailed description of some exemplary embodiments of the present invention with reference to the accompanying drawings, in which:

[0030] Figure 1 is a cross-sectional view of a pixel of a display device according to an embodiment;

[0031] Figure 2 is a schematic diagram of a light emitting element according to an embodiment;

[0032] Figure 3 It is along Figure 2 A cross-sectional view taken along line II';

[0033] Figure 4 and Figure 6 is a schematic diagram of a light emitting element according to another embodiment, and Figure 5 It is along Figure 4 A cross-sectional view taken along line II-II';

[0034] Figure 7 yes Figure 1 An enlarged view of area "A";

[0035] Figures 8 to 20 are views sequentially showing a method of manufacturing a light emitting element according to an embodiment;

[0036] Fig.21 and 22 is an enlarged view showing a separation surface of a first light emitting element and a second light emitting element according to an embodiment;

[0037] Figure 23 to Figure 26 is a plan view of a lower plate on which a first mask layer is formed according to an embodiment; and

[0038] Fig. 27 is a cross-sectional view of a lower plate having a first mask layer formed thereon according to another embodiment. DETAILED DESCRIPTION

[0039] The present invention will now be described more fully herein with reference to the accompanying drawings, in which some exemplary embodiments of the present invention are shown. However, the present invention may be implemented in different forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, these embodiments are provided so that the present disclosure will be complete and complete, and will fully convey the scope of the present invention to those skilled in the art.

[0040] It will be understood that when a layer is referred to as being 'on' another layer or another substrate, it may be directly on another layer or another substrate, or one or more intervening layers may also be present. Throughout the specification, the same reference numerals refer to the same components.

[0041] It should be understood that although the terms "first", "second", etc. may be used herein to describe various elements, these elements should not be limited by these terms. These terms are used to distinguish one element from another element. For example, without departing from the teachings of the present invention, the "first" element discussed below may be referred to as the "second" element. Similarly, the "second" element may also be referred to as the "first" element.

[0042] Herein, embodiments of the present invention will be described with reference to the accompanying drawings.

[0043] Figure 1 is a cross-sectional view of a pixel of a display device according to an embodiment.

[0044] The display device according to the embodiment may include a pixel PX. The pixel PX emits light of a specific wavelength band and is provided in a display unit of the display device to display a series of information to be provided to a user. Figure 1 A case where the display device includes one pixel PX is shown, but the present invention is not limited thereto, and it should be understood that the display device includes a plurality of pixels PX.

[0045] The pixel PX may include a plurality of light emitting elements 300 and may emit light of different wavelengths. For example, the light emitting element 300 may emit light of a blue wavelength, a green wavelength, and a red wavelength, and therefore, the pixel PX may be implemented as a pixel emitting blue light, green light, and red light. However, the present invention is not limited thereto. In some cases, all the light emitting elements 300 emit light of the same color band, so that the pixel PX emits light of the same color (e.g., blue). In addition, a light emitting element 300 emitting light of different color bands may be provided in one pixel PX to emit light of different colors, for example, white light.

[0046] The pixel PX includes a base substrate 100, a plurality of electrodes 210 and 220 disposed on the base substrate 100, contact electrodes 230 and 240 disposed on the respective electrodes 210 and 220, and a plurality of light emitting elements 300 connected to the respective contact electrodes 230 and 240. The unit pixel PX may further include an outer partition wall 500 to distinguish the unit pixel PX from each adjacent pixel PX. Herein, the pixel PX will be described in more detail.

[0047] The pixel PX includes a base substrate 100 and a first electrode 210 and a second electrode 220 disposed on the base substrate 100 to face each other. Reflective partition walls 211 and 221 may be disposed on the base substrate 100. The first electrode 210 and the second electrode 220 may be disposed on the reflective partition walls 211 and 221, respectively, to cover the reflective partition walls 211 and 221. The reflective partition walls 211 and 221 may be formed of an organic material such as polyimide, but the present invention is not limited thereto.

[0048] The light emitting element 300 may be disposed between the first electrode 210 and the second electrode 220 which are spaced apart from each other. Figure 1 2 shows that the first electrode 210 and the second electrode 220 are directly disposed on the base substrate 100, but the present invention is not limited thereto, and other layers or other structures may be disposed between the base substrate 100 and the first electrode 210 and the second electrode 220. For example, a buffer layer, a thin film transistor, etc. may be disposed on the base substrate 100, and the first electrode 210 and the second electrode 220 may be disposed on the buffer layer, the thin film transistor, etc.

[0049] The base substrate 100 may support structures disposed thereon, for example, reflective partition walls 211 and 221, the first and second electrodes 210 and 220, the light emitting element 300, and the outer partition wall 500. The base substrate 100 may be any one of a glass substrate, a quartz substrate, a sapphire substrate, a plastic substrate, and a flexible polymer film, but is not limited thereto.

[0050] The first electrode 210 and the second electrode 220 may be disposed on the base substrate 100 to be spaced apart from each other and to face each other. The first electrode 210 and the second electrode 220 may receive an electrical signal applied from a first electrode line 250 and a second electrode line (not shown). The applied electrical signal is transmitted to the light emitting element 300 disposed between the first electrode 210 and the second electrode 220 to allow the light emitting element 300 to emit light.

[0051] The first electrode 210 may be electrically connected to the first electrode line 250 extending in one direction to receive an electrical signal from the first electrode line 250. The second electrode 220 may be electrically connected to the second electrode line (not shown) extending in a direction perpendicular to the direction in which the first electrode line 250 is disposed to receive an electrical signal from the second electrode line (not shown).

[0052] In an embodiment, the first electrode 210 and the second electrode 220 may be spaced apart from each other by a distance (e.g., a predetermined distance), and the distance may be shorter than the length of the light emitting element 300. When the length of the light emitting element 300 is shorter than the distance between the first electrode 210 and the second electrode 220, the light emitting element 300 may not receive an electrical signal applied from the first electrode line 250 and the second electrode line (not shown) because the light emitting element 300 does not make contact with the electrodes.

[0053] The first electrode 210 and the second electrode 220 may include reflective partition wall layers 210_1 and 220_1 formed on the reflective partition walls 211 and 221 and reflective partition wall electrode layers 210_2 and 220_2 formed on the reflective partition wall layers 210_1 and 220_1 , respectively.

[0054] The reflective partition wall layers 210_1 and 220_1 may reflect light emitted from the light emitting element 300 to transmit the light toward the outside of the display device. The light emitted from the light emitting element 300 is emitted in all directions and has no directivity. The light directed to the reflective partition wall layers 210_1 and 220_1 may be reflected and transmitted toward the outside of the display device, for example, toward the upper side of the reflective partition wall layers 210_1 and 220_1. Therefore, the light emitted from the light emitting element 300 may be concentrated in one direction to improve light efficiency. The reflective partition wall layers 210_1 and 220_1 may include a material having a high reflectivity to reflect the light emitted from the light emitting element 300. For example, the reflective partition wall layers 210_1 and 220_1 may include a material such as silver (Ag), but the present invention is not limited thereto.

[0055] The reflective partition wall electrode layers 210_2 and 220_2 may be formed on the reflective partition wall layers 210_1 and 220_1 and may be connected to the first electrode line 250 and the second electrode line (not shown). The reflective partition wall electrode layers 210_2 and 220_2 may transmit an electrical signal applied to the first electrode line 250 and the second electrode line (not shown) to the contact electrodes 230 and 240. The reflective partition wall electrode layers 210_2 and 220_2 may include a transparent conductive material. For example, the reflective partition wall electrode layers 210_2 and 220_2 may include a material such as ITO, IZO, or IGO, but the present invention is not limited thereto.

[0056] In an embodiment, if Figure 1As shown in , the first electrode 210 , the second electrode 220 , the light emitting element 300 , the first contact electrode 230 , and the second contact electrode 240 may be covered by a plurality of insulating material layers 410 , 420 , and 430 .

[0057] In an embodiment, in order to protect the reflective partition wall electrode layers 210_2 and 220_2, the first insulating material layer 410 may be disposed between the first electrode 210 and the second electrode 220. Figure 1 As shown in FIG. 1 , the first insulating material layer 410 may be disposed between the first electrode 210 and the second electrode 220, and the light emitting element 300 may be aligned on the first insulating material layer 410. The first insulating material layer 410 may include silicon oxide (SiO x ), silicon nitride (SiN x ), silicon oxynitride (SiO x N y ), aluminum oxide (Al 2 O 3 ) or aluminum nitride (AlN), but the present invention is not limited thereto. The first insulating material layer 410 protects the reflective partition wall electrode layers 210_2 and 220_2 of the first electrode 210 and the second electrode 220, and can prevent the semiconductor layers 310 and 320 of the light emitting element 300 from directly contacting other substrates, thereby preventing or substantially preventing damage to the light emitting element 300.

[0058] In order to transmit the electrical signal applied from the first electrode line 250 and the second electrode line (not shown), the first contact electrode 230 and the second contact electrode 240 may be disposed on the upper surface of the reflective partition wall electrode layer 210_2 and 220_2. The first contact electrode 230 and the second contact electrode 240 may be connected to the first semiconductor layer 310 and the second semiconductor layer 320 of the light emitting element 300, respectively. The first contact electrode 230 and the second contact electrode 240 may transmit the electrical signal applied to the reflective partition wall electrode layer 210_2 and 220_2 through the first electrode line 250 and the second electrode line (not shown) to the light emitting element 300 to emit light.

[0059] The first contact electrode 230 and the second contact electrode 240 may include a conductive material, for example, ITO, IZO, IGO, or aluminum (Al). However, the present invention is not limited thereto.

[0060] In order to protect and electrically insulate the first contact electrode 230 and the second contact electrode 240, the first contact electrode 230 and the second contact electrode 240 are disposed on the light emitting element 300 to be spaced apart from each other, and the second insulating material layer 420 may be disposed in the spaced region. In an embodiment, the second insulating material layer 420 is the same as the first insulating material layer 410 except that the second insulating material layer 420 is formed on the light emitting element 300. Further details thereof will not be described.

[0061] The third insulating material layer 430 may be formed on the first contact electrode 230, the second contact electrode 240, and the second insulating material layer 420 to serve as a protective layer against the external environment. When the contact electrodes 230 and 240 are exposed, since the problem of disconnection of the contact electrode material due to electrode damage may occur, the contact electrodes 230 and 240 may be covered with the third insulating material layer 430. The third insulating material layer 430 may be provided to cover the first electrode 210, the second electrode 220, and the light emitting element 300. In an embodiment, the third insulating material layer 430 is the same as the first insulating material layer 410 except for the position where it is provided.

[0062] In an implementation, at least one outer partition wall 500 is disposed on the base substrate 100 to separate the plurality of pixels PX. Figure 1 As shown in FIG. 1 , a plurality of outer partition walls 500 are spaced apart from each other, and the first electrode 210, the second electrode 220, and the light emitting element 300 are formed between the spaced apart outer partition walls 500. The outer partition walls 500 may be formed to cover the first electrode lines 250 and the second electrode lines (not shown).

[0063] Based on the light emitting element 300 emitting light of a specific wavelength band, the pixel PX is separated by the outer partition wall 500. When the light emitting element 300 is aligned, the outer partition wall 500 can prevent or substantially prevent the light emitting element 300 from moving to another adjacent pixel PX. For example, the outer partition wall 500 can be made of polyimide (PI). However, the present invention is not limited thereto, and the material of the outer partition wall 500 is not particularly limited as long as its surface is made of a hydrophobic material.

[0064] The outer partition wall 500 can prevent or substantially prevent color mixing of light emitted from the light emitting element 300. When adjacent pixels PX include light emitting elements 300 that emit light of different wavelength bands from each other, the colors of light emitted from the respective pixels PX may be mixed. In order to prevent or substantially prevent such color mixing, the outer partition wall 500 is provided between the pixels PX so that light emitted from one pixel PX cannot be incident on another pixel PX to prevent or substantially prevent color mixing, thereby improving the color purity of the display device.

[0065] The plurality of light emitting elements 300 disposed between the first electrode 210 and the second electrode 220 may each include an active layer 350 to emit light of the above-mentioned specific wavelength band. The light emitting elements 300 may emit light of different wavelength bands, or may emit light of the same wavelength band.

[0066] The light emitting element 300 according to the embodiment may be manufactured on a substrate by an epitaxial growth method. A seed layer for forming a semiconductor layer may be formed on the substrate, and a desired semiconductor material may be deposited and grown. Crystals grow on the seed layer to form a plurality of semiconductor layers 310 and 320, thereby manufacturing the light emitting element 300. The manufactured light emitting element 300 may be separated from the substrate and aligned between the first electrode 210 and the second electrode 220. Herein, reference will be made to Figures 2 to 6 The structure of the light emitting element 300 will be described.

[0067] Figure 2 is a schematic diagram of a light emitting element 300 according to an embodiment; and Figure 3 It is along Figure 2 A cross-sectional view taken along line I-I'.

[0068] Reference Figure 2 and Figure 3 , the light emitting element 300 may include a plurality of semiconductor layers 310 and 320 and an active layer 350 disposed between the plurality of semiconductor layers 310 and 320. An electrical signal applied from the first electrode 210 and the second electrode 220 is transmitted to the active layer 350 via the plurality of semiconductor layers 310 and 320 to emit light.

[0069] In an embodiment, the light emitting element 300 includes a first semiconductor layer 310 , a second semiconductor layer 320 , an active layer 350 between the first semiconductor layer 310 and the second semiconductor layer 320 , and an insulating layer 380 . Figure 2 The light emitting element 300 shows a structure in which a first semiconductor layer 310, an active layer 350 and a second semiconductor layer 320 are sequentially stacked in a length direction.

[0070] In an embodiment, the first semiconductor layer 310 may be an n-type semiconductor layer. For example, when the light emitting element 300 emits light in the blue wavelength band, the first semiconductor layer 310 may be composed of a semiconductor layer having a chemical formula of In x Al y Ga 1-x-yThe first semiconductor layer 310 may be formed of a semiconductor material having a thickness of N (0≤x≤1, 0≤y≤1, 0≤x+y≤1). For example, the semiconductor material may be at least one of InAlGaN, GaN, AlGaN, InGaN, AlN, and InN doped with n-type impurities. The first semiconductor layer 310 may be doped with a first conductive dopant. For example, the first conductive dopant may be Si, Ge, or Sn. The length of the first semiconductor layer 310 may be in the range of 1.5 μm to 5 μm, but is not limited thereto.

[0071] In an embodiment, the second semiconductor layer 320 may be a p-type semiconductor layer. For example, when the light emitting element 300 emits light in the blue wavelength band, the second semiconductor layer 320 may be composed of a semiconductor layer having a chemical formula of In x Al y Ga 1-x-y The second semiconductor layer 320 may be formed of a semiconductor material having a thickness of N (0≤x≤1, 0≤y≤1, 0≤x+y≤1). For example, the semiconductor material may be at least one of InAlGaN, GaN, AlGaN, InGaN, AlN, and InN doped with p-type impurities. The second semiconductor layer 320 may be doped with a second conductive dopant. For example, the second conductive dopant may be Mg, Zn, Ca, Se, or Ba. The length of the second semiconductor layer 320 may be in the range of 0.08 μm to 0.25 μm, but is not limited thereto.

[0072] In this specification, the case where the first semiconductor layer 310 and the second semiconductor layer 320 are respectively an n-type semiconductor layer and a p-type semiconductor layer will be described as an example. However, the present invention is not limited thereto, and may also include a case where the first semiconductor layer 310 is a p-type semiconductor layer and the second semiconductor layer 320 is an n-type semiconductor layer.

[0073] The active layer 350 is disposed between the first semiconductor layer 310 and the second semiconductor layer 320, and may include a material having a single quantum well structure or a multi-quantum well structure. When the active layer 350 includes a material having a multi-quantum well structure, the active layer 350 may have a structure in which a plurality of quantum layers and a plurality of well layers are alternately stacked. The active layer 350 may emit light by combining electron-hole pairs according to an electrical signal applied via the first semiconductor layer 310 and the second semiconductor layer 320. For example, when the active layer 350 emits light in a blue band, the active layer 350 may include a material such as AlGaN or AlInGaN. In an embodiment, when the active layer 350 has a multi-quantum well structure in which quantum layers and well layers are alternately stacked, the quantum layers may include AlGaN or AlInGaN, and the well layers may include a material such as GaN or AlGaN. However, the present invention is not limited thereto, and depending on the wavelength band of light to be emitted, the active layer 350 may include other Group 3 to Group 5 semiconductor materials. Therefore, light emitted by the active layer 350 is not limited to light of a blue band, and in some cases, the active layer 350 may emit light of red and green wavelengths. The length of the active layer 350 may be in the range of 0.05 μm to 0.25 μm, but is not limited thereto.

[0074] Light emitted from the active layer 350 may be emitted not only to the longitudinal outer surface of the light emitting element 300 but also to both side surfaces of the light emitting element 300. That is, the directivity of light emitted from the active layer 350 is not limited to one direction.

[0075] The insulating layer 380 may be formed outside the light emitting element 300 to protect the light emitting element 300. For example, the insulating layer 380 may be formed to surround the side surface of the light emitting element 300, and therefore, the insulating layer 380 may not be formed at both ends of the light emitting element 300 in the length direction, for example, may not be formed at both ends of the light emitting element 300 where the first semiconductor layer 310 and the second semiconductor layer 320 are provided. However, the present invention is not limited thereto. The insulating layer 380 may include any material having an insulating property, such as silicon oxide (SiO x ), silicon nitride (SiN x ), silicon oxynitride (SiO x N y ), aluminum nitride (AlN) and aluminum oxide (Al 2 O 3 ). Therefore, it is possible to prevent an electrical short circuit that may occur when the active layer 350 is in direct contact with the first electrode 210 or the second electrode 220. In addition, since the light emitting element 300 includes the insulating layer 380 to protect the outer surface of the light emitting element 300, a decrease in light emitting efficiency can be prevented or substantially prevented.

[0076] The thickness of the insulating layer 380 may be in the range of 0.5 μm to 1.5 μm, but is not limited thereto. In addition, at least one passivation layer may be formed on the outer surface of the insulating layer 380 of the light emitting element 300 .

[0077] Refer again Figure 2 , the light emitting element 300 may have a cylindrical shape. However, the shape of the light emitting element 300 is not limited thereto, and the light emitting element 300 may have, but is not limited to, any of various shapes such as a cube, a cuboid, and a hexagonal column. In an embodiment, the light emitting element 300 may have a length l in a range of 1 μm to 10 μm or 2 μm to 5 μm, and in an embodiment, the light emitting element 300 may have a length of about 4 μm. In an embodiment, the light emitting element 300 may have a diameter in a range of 400 nm to 700 nm, and in an embodiment, the light emitting element 300 may have a diameter of about 500 nm. Herein, the case where the light emitting element 300 is cylindrical will be described as an example.

[0078] Figure 4 and Figure 5 are schematic diagrams of a light emitting element 300' according to another embodiment and Figure 4 A cross-sectional view taken along line II-II'; and Figure 6 is a schematic diagram of a light emitting element 300" according to another embodiment.

[0079] The light emitting element 300 ′ and the light emitting element 300 ″ may further include an electrode layer 360 or 370 on at least one of both side surfaces of the first semiconductor layer 310 and the second semiconductor layer 320 .

[0080] Figure 4 and Figure 5 The light emitting element 300 ′ shows a case where the second semiconductor layer 320 further includes an electrode layer 370, and Figure 6 The light emitting element 300” shows a case where the first semiconductor layer 310 and the second semiconductor layer 320 further include electrode layers 360 and 370, respectively. For convenience of description, the electrode layer formed on one side surface of the first semiconductor layer 310 is referred to as the first electrode layer 360, and the electrode layer formed on the other side surface of the second semiconductor layer 320 is referred to as the second electrode layer 370. However, the present invention is not limited thereto, and either electrode layer may be referred to as the first electrode layer.

[0081] Reference Figures 4 to 6, each of the light emitting elements 300' and 300" may include at least one of the first electrode layer 360 and the second electrode layer 370, and in this case, the insulating layer 380 may extend in the length direction to cover the outer surfaces of the first electrode layer 360 and the second electrode layer 370. However, the present invention is not limited thereto, and the insulating layer 380 may cover only the first semiconductor layer 310, the active layer 350, and the second semiconductor layer 320, or may cover only a portion of the outer surface of the electrode layer 360 or 370 to expose another portion of the outer surface of the electrode layer 360 or 370.

[0082] The first electrode layer 360 and the second electrode layer 370 may be ohmic contact electrodes. However, the present invention is not limited thereto, and the first electrode layer 360 and the second electrode layer 370 may be Schottky contact electrodes. The first electrode layer 360 and the second electrode layer 370 may include a conductive metal. For example, the first electrode layer 360 and the second electrode layer 370 may include at least one of aluminum (Al), titanium (Ti), indium (In), gold (Au), and silver (Ag). The first electrode layer 360 and the second electrode layer 370 may include the same material or may include different materials. However, the present invention is not limited thereto.

[0083] In this article, for the sake of convenience, Figure 4 The light emitting element 300' shown in FIG. 1 is described as an example, but similar to the light emitting elements shown in other drawings, the first electrode layer 360 and the second electrode layer 370 may be formed, or both the first electrode layer 360 and the second electrode layer 370 may be omitted.

[0084] Figure 7 yes Figure 1 Magnified view of area "A" in FIG.

[0085] Reference Figure 1 and Figure 7 , the light emitting element 300 may be connected to the first contact electrode 230 and the second contact electrode 240 to receive an electrical signal.

[0086] In an embodiment, the light emitting element 300 may be connected to the first electrode 210 and the second electrode 220 via the contact electrodes 230 and 240 without directly contacting the first electrode 210 and the second electrode 220. Therefore, when the light emitting element 300 is aligned between the first electrode 210 and the second electrode 220, even if a high voltage is applied to the first electrode 210 and the second electrode 220, the high voltage is not applied to the light emitting element 300, and thus damage can be prevented.

[0087] However, the light emitting element 300 is in contact with the first contact electrode 230 and the second contact electrode 240. As described above, the light emitting element 300 manufactured by the epitaxial method may have a surface separated from the substrate, and the separation surface has an uneven structure or a non-flat inclined shape. Since the light emitting element 300 grown on the substrate is separated from the substrate by a physical method, the separation surface of the manufactured light emitting element 300 may be uneven and may have roughness.

[0088] Specifically, in the case where a partially inclined region is formed on the separation surface of the light emitting element 300, when the light emitting element 300 aligned on the first insulating material layer 410 is connected to the contact electrodes 230 and 240, the materials of the contact electrodes 230 and 240 may be disconnected. Therefore, the contact electrodes 230 and 240 may be disconnected to cause an open circuit failure, and an electrical signal may not be applied to the light emitting element 300.

[0089] In order to prevent or substantially prevent this situation, the light emitting element 300 needs to have a smooth surface separated from the substrate. The method of manufacturing the light emitting element 300 according to the embodiment of the present invention may include the following method: chemically separating the light emitting element 300 by forming a sacrificial layer on at least a portion of the region in the element stack grown by the epitaxial method and etching the sacrificial layer. Therefore, in the light emitting element 300 according to the embodiment, the two side surfaces contacting the first contact electrode 230 and the second contact electrode 240 may have a flat shape to be parallel to a plane perpendicular to the substrate, and the problem of disconnection of the materials of the contact electrodes 230 and 240 may be prevented or substantially prevented. Herein, reference will be made to Figures 8 to 20 A method of manufacturing the light emitting element 300 according to the embodiment is described in more detail.

[0090] Figures 8 to 20 A method of manufacturing the light emitting element 300 according to the embodiment is sequentially illustrated.

[0091] According to an embodiment, a method for manufacturing a light emitting element 300 may include the following steps: preparing a lower plate 11 including a substrate 10 and a first sub-conductive semiconductor layer 31' formed on the substrate 10; forming a first mask layer 20 including at least one mask pattern 21 and an opening 22, wherein at least one mask pattern 21 is arranged to be spaced apart from each other on at least a portion of the lower plate 11, and the opening 22 is a region in which the mask patterns 21 are spaced apart from each other; stacking a first conductive semiconductor layer 31, an active material layer 35 and a second conductive semiconductor layer 32 on the first mask layer 20 to form an element stack 30'; etching the element stack 30' in a vertical direction to form an element rod 30; and removing the mask pattern 21 to separate the element rod 30 from the lower plate 11.

[0092] First, a lower plate 11 in which a first sub-conductive semiconductor layer 31' is stacked on a substrate 10 is prepared. Figure 8 As shown in , the lower plate 11 has a structure in which the substrate 10 and the first sub-conductive semiconductor layer 31' are sequentially stacked. In an embodiment, the first sub-conductive semiconductor layer 31' may include the same material as the first semiconductor layer 310 of the light emitting element 300. For example, the first sub-conductive semiconductor layer 31' may be an n-type semiconductor layer, and may include the same material as the first semiconductor layer 310 doped with n-type impurities. However, the present invention is not limited thereto.

[0093] The substrate 10 may include a sapphire substrate (Al 2 O 3 ) and any one of a transparent substrate such as a glass substrate. However, the present invention is not limited thereto, and the substrate 10 may be a conductive substrate including GaN, SiC, ZnO, Si, GaP, or GaAs. Herein, the lower plate 11 includes a sapphire substrate (Al 2 O 3 ) is described as an example.

[0094] The thickness of the substrate 10 is not particularly limited, but may be, for example, in the range of 400 μm to 1500 μm.

[0095] A plurality of conductive semiconductor layers are formed on the substrate 10. The plurality of conductive semiconductor layers grown by the epitaxial method may be grown by forming a seed crystal and depositing a material. In an embodiment, the plurality of conductive semiconductor layers may be formed by physical vapor deposition (PVD), chemical vapor deposition (CVD), plasma laser deposition (PLD), dual-type thermal evaporation, sputtering, or metal organic chemical vapor deposition (MOCVD). In an exemplary embodiment, the plurality of conductive semiconductor layers may be formed by metal organic chemical vapor deposition (MOCVD). However, the present invention is not limited thereto.

[0096] The precursor material for forming the plurality of conductive semiconductor layers is not particularly limited to the range that can be generally selected to form the target material. In an example, the precursor material may be a metal precursor including an alkyl group such as a methyl group or an ethyl group. For example, the metal precursor may be a metal precursor such as trimethylgallium (Ga(CH 3 ) 3 ), trimethylaluminum (Al(CH 3 ) 3 ), triethyl phosphate ((C 2 H 5 ) 3 PO 4 ) compounds, but not limited thereto.

[0097] The first sub-conductive semiconductor layer 31' is formed on the substrate 10. As will be described later, in the method of manufacturing the light emitting element 300 according to the embodiment, the first mask layer 20 is formed before forming the first semiconductor layer 310 of the light emitting element 300. Therefore, the first sub-conductive semiconductor layer 31' may provide a seed crystal of the first semiconductor layer 310 grown on the first mask layer 20.

[0098] In an implementation, at least one buffer layer 15 may be disposed between the substrate 10 and the first sub-conductive semiconductor layer 31'. Figure 8 As shown in , the buffer layer 15 may be formed on the substrate 10 , and the first sub-conductive semiconductor layer 31 ′ may be formed on the buffer layer 15 .

[0099] The buffer layer 15 may be provided to reduce the difference in lattice constant between the substrate 10 and the first sub-conductive semiconductor layer 31'. Although the first sub-conductive semiconductor layer 31' may be formed directly on the substrate 10, the buffer layer 15 may be formed to allow crystals of the first sub-conductive semiconductor layer 31' to grow easily, thereby providing a seed crystal. In an embodiment, the buffer layer 15 may be an undoped semiconductor layer, and the undoped semiconductor layer may include the same material as the first sub-conductive semiconductor layer 31', but may be an undoped material. For example, the undoped semiconductor layer may include at least one of InAlGaN, GaN, AlGaN, InGaN, AlN, and InN, but is not limited thereto. Herein, a case where an undoped semiconductor layer is formed on the substrate 10 as the buffer layer 15 is described.

[0100] Next, if Fig. 9 As shown in FIG. 1 , a first mask layer 20 including a plurality of mask patterns 21 is formed on at least a portion of the prepared lower plate 11. The first mask layer 20 may be configured such that the plurality of mask patterns 21 are spaced apart from each other. The first mask layer 20 may include openings 22 between the mask patterns 21 spaced apart from each other. Crystals of the first sub-conductive semiconductor layer 31 'may grow through the openings 22 of the first mask layer 20.

[0101] The mask pattern 21 of the first mask layer 20 may include at least one of an insulating material and a conductive material. For example, the insulating material may be silicon oxide (SiO x ), silicon nitride (SiN x ) or silicon oxynitride (SiO x N y ), and the conductive material may be ITO, IZO, GO, ZnO, graphene, or graphene oxide. However, the present invention is not limited thereto.

[0102] When the crystal of the first sub-conductive semiconductor layer 31' grows, the crystal is not uniform at the grain boundary, and thus, defects may be formed in the grown semiconductor layer. The defects may be a factor that hinders electron mobility in the semiconductor layers 310 and 320 of the light emitting element 300 or the light emitting efficiency of the light emitting element 300.

[0103] In contrast, when the first mask layer 20 is formed to grow crystals of the first sub-conductive semiconductor layer 31', defects at grain boundaries are blocked by the mask pattern 21, and only defects formed in the openings 22 remain. Therefore, the amount of defects formed in the finally formed first semiconductor layer 310 can be reduced.

[0104] In addition, as will be described later, when the light emitting element 300 is separated from the substrate 10 or the lower plate 11, the first mask layer 20 may be etched and removed. Therefore, the separation surface of the light emitting element 300 formed on the mask pattern 21 of the first mask layer 20 may have the same shape as the surface of the mask pattern 21. That is, the separation surface of the light emitting element 300 may have any one of a variety of shapes depending on the pattern of the first mask layer 20, the shape or structure of the mask pattern 21, etc. As shown in FIG. Figure 8 As described, this may be associated with a problem of disconnection associated with the contact electrodes 230 and 240 according to the shape of one side surface (or separation surface) of the light emitting element 300. More details thereof will be described later.

[0105] Next, the first conductive semiconductor layer 31, the active material layer 35, and the second conductive semiconductor layer 32 are stacked on the first mask layer 20 to form an element stack 30'. The first conductive semiconductor layer 31, the active material layer 35, and the second conductive semiconductor layer 32 stacked on the first mask layer 20 are separated from the substrate 10 or the lower plate 11, thereby forming a light emitting element 300. Therefore, the first conductive semiconductor layer 31, the active material layer 35, and the second conductive semiconductor layer 32 may include the same Figures 2 to 6 The material of the light emitting element 300 is the same as that described herein. Herein, a method of forming the first conductive semiconductor layer 31, the active material layer 35, and the second conductive semiconductor layer 32 will be described in more detail.

[0106] First, the first conductive semiconductor layer 31 includes the same material as the first sub-conductive semiconductor layer 31' and may be formed by metal organic chemical vapor deposition (MOCVD) (as an example of the above method). Crystals of the first sub-conductive semiconductor layer 31' may provide seed crystals of the first conductive semiconductor layer 31 and may grow through the opening 22 of the first mask layer 20.

[0107] Figures 10 to 12 is a schematic diagram illustrating a process of growing crystals of the first sub-conductive semiconductor layer 31 ′ according to an embodiment.

[0108] In an embodiment, the crystals of the first sub-conductive semiconductor layer 31' grow in a vertical direction in a region overlapping with the opening 22, and grow to a height the same as the thickness of the mask pattern 21. In an embodiment, the crystals grown in the opening 22 grow upward in a horizontal direction relative to the mask pattern 21 so that the crystals of the first sub-conductive semiconductor layer 31' spread. Finally, the crystals of the first sub-conductive semiconductor layer 31' fuse in a portion of the mask pattern 21 to form a portion of the first conductive semiconductor layer 31. The crystals of the first sub-conductive semiconductor layer 31' become grain boundaries on the mask pattern 21, and thus may form defects. However, the defects formed in the region overlapping with the mask pattern 21 may not grow, and the amount of defects in the finally formed first semiconductor layer 310 may be reduced.

[0109] like Fig.13 As shown in , when the crystal of the first sub-conductive semiconductor layer 31' grows to form the first conductive semiconductor layer 31, the active material layer 35 and the second conductive semiconductor layer 32 are stacked on the first conductive semiconductor layer 31 to form the element stack 30'. In an embodiment, the active material layer 35 and the second conductive semiconductor layer 32 are formed in the same manner as the first conductive semiconductor layer 31, except that the crystal of the first sub-conductive semiconductor layer 31' is formed and grown through the opening 22. Further details thereof will not be described.

[0110] In an embodiment, the light emitting element 300 may further include an electrode layer 360 or 370 located on at least one of the first semiconductor layer 310 and the second semiconductor layer 320. Therefore, the method may further include the step of forming a conductive electrode layer 37 on the formed element stack 30'. Fig.14 , it can be seen that the conductive electrode layer 37 is formed on the second conductive semiconductor layer 32. The conductive electrode layer 37 may include a conductive material as described above, and may be formed in the same manner as the second conductive semiconductor layer 32. The formed conductive electrode layer 37 may form an ohmic contact or a Schottky contact with the second conductive semiconductor layer 32. Herein, the element stack 30' provided with only the conductive electrode layer 37 will be described as an example.

[0111] Next, the element stack 30' is etched in the vertical direction to prepare the element rod 30. The step of vertically etching the element stack 30' can be performed by a common method. For example, the element rod 30 can be prepared by forming a second mask layer 40 including a hard mask layer and a nano pattern layer 42 on the element stack 30' and then etching the second mask layer 40. Fig.15 and Fig.16 Describe its description.

[0112] Reference Fig.15 , in the component stack 30' (reference Fig.14 ) is formed on the second conductive semiconductor layer 32 including a second mask layer 40 including a hard mask layer and a nano pattern layer 42.

[0113] The hard mask layer may be used as a mask for sequentially etching the first conductive semiconductor layer 31, the active material layer 35, and the second conductive semiconductor layer 32 included in the element stack 30'. In an embodiment, the hard mask layer may include a first layer 41_1 including an insulating material and a second layer 41_2 including a metal.

[0114] As the insulating material included in the first layer 41_1 of the hard mask layer, oxide or nitride may be used. Examples of the insulating material may include silicon oxide (SiO x ), silicon nitride (SiN x ) or silicon oxynitride (SiO x N y The thickness of the first layer 41_1 may be in the range of 0.5 μm to 1.5 μm, but is not limited thereto.

[0115] The material of the second layer 41_2 is not particularly limited, and may be a known material that can be used as a mask for continuously etching the element stack 30'. For example, the second layer 41_2 may include chromium (Cr), etc. The thickness of the second layer 41_2 may be in the range of 30nm to 150nm, but is not limited thereto.

[0116] Next, a nano-pattern layer 42 in which nano-patterns are arranged to be spaced apart from each other may be formed on the hard mask layer. In the nano-pattern layer 42, the nano-patterns spaced apart from each other may be used as a mask for continuously etching the element stack 30'. The method of forming the nano-pattern layer 42 is not particularly limited as long as a nano-pattern including a polymer, a polystyrene sphere, and a silica sphere can be formed.

[0117] As an example, when the nano-pattern layer 42 includes a polymer, a known method of forming a pattern using a polymer may be used. For example, the nano-pattern layer 42 including a polymer may be formed by a method such as photolithography, electron beam lithography, or nanoimprint lithography.

[0118] The structure and shape of the nano-pattern layer 42 and the spacing between the nano-patterns may be related to the form of the light-emitting element 300 finally manufactured. However, as described above, since the light-emitting element 300 may have any one of a variety of shapes, the structure of the nano-pattern layer 42 is not particularly limited. For example, when the nano-pattern layer 42 has circular patterns spaced apart from each other, the element rod 30 prepared by vertically etching the element stack 30' may have a cylindrical shape. Therefore, the light-emitting element 300 separated from the substrate 10 or the lower plate 11 may have a cylindrical shape. However, the present invention is not limited thereto.

[0119] Next, refer to Fig.16 When the second mask layer 40 is formed on the element stack 30', the region where the nano-pattern layer 42 is formed is not etched, and the region where the nano-patterns of the nano-pattern layer 42 are spaced apart from each other is vertically etched to form a hole. The hole can be selectively formed from the hard mask layer to the region where the first mask layer 20 is formed.

[0120] The method of forming a hole by etching the element stack 30' may be performed in a conventional manner. Examples of etching may include dry etching, wet etching, reactive ion etching (RIE), and inductively coupled plasma reactive ion etching (ICP-RIE). Dry etching is suitable for forming a hole by vertical etching because it can perform anisotropic etching. In an embodiment, when the above etching method is used, the etchant may be Cl 2 or 2 However, the present invention is not limited thereto.

[0121] In some embodiments, the etching of the element stack 30' may be performed by using a combination of dry etching or wet etching. For example, first, the element stack 30' may be etched in the depth direction by dry etching, and then the etched sidewalls of the element stack 30' may be placed in a plane perpendicular to its surface by wet etching which is isotropic etching.

[0122] The second mask layer 40 remaining on the vertically etched element stack 30 ′ is removed by a known method (eg, dry etching or wet etching) to form the element rods 30 .

[0123] Finally, the light emitting element 300 is formed by forming an insulating film 38 on the element rod 30 and removing the mask pattern 21 to separate at least a portion of the element rod 30 from the substrate 10 or the lower board 11 .

[0124] The insulating film 38 (the insulating film 38 is a film formed on the outer surface of the element rod 30) can be formed by applying an insulating material to the outer surface of the vertically etched element rod 30 or immersing its outer surface in an insulating material, but the present invention is not limited thereto. For example, the insulating film 38 can be formed by atomic layer deposition (ALD). The insulating film 38 can form an insulating layer 380 of the light emitting element 300. As described above, in an embodiment, the insulating film 38 may include silicon oxide (SiO x ), silicon nitride (SiN x ), silicon oxynitride (SiO x N y ), aluminum oxide (Al 2 O 3 ) or aluminum nitride (AlN).

[0125] Reference Fig.17 In addition to the outer surface of the element rod 30, the insulating film 38 may also be formed on a portion of the surface of the mask pattern 21 that is exposed to the outside by etching the element rod 30 to be spaced apart from each other. When the insulating film 38 is formed even on the conductive electrode layer 37 that is the upper surface of the element rod 30, the light emitting element 300 can be insulated from the connection with the contact electrodes 230 and 240. Therefore, it is necessary to partially remove the insulating film 38 formed in a direction perpendicular to the length direction of the element rod 30, that is, the insulating film 38 formed in a direction parallel to the substrate 10 or the lower plate 11. That is, as Fig.18 As shown in FIG. 1 , at least the insulating film 38 disposed on the upper surface of the element rod 30 is removed to expose the upper surface of the element rod 30. To this end, a process such as dry etching or etching-back, which is anisotropic etching, may be performed.

[0126] At least a portion of the element rod 30 is separated from the substrate 10 or the lower plate 11 by removing the mask pattern 21 to manufacture the light emitting element 300. The mask pattern 21 can be dissolved by an etchant such as hydrofluoric acid (HF). Fig.19 As shown in , the mask pattern 21 is dissolved and the element rod 30 formed on the mask pattern 21 of the first mask layer 20 is chemically separated (chemically stripped) from the lower plate 11 to manufacture the light emitting element 300_1. Since the light emitting element 300_1 is separated by dissolving and removing the mask pattern 21, its separation surface 390_1 may be relatively flat. In some embodiments, the surface roughness of the separation surface 390_1 may be different from the surface roughness of the upper surface of the second conductive semiconductor layer 32. However, the present invention is not limited thereto, and in some cases, the separation surface 390_1 may be substantially flat and may be parallel to the upper surface of the second conductive semiconductor layer 32.

[0127] On the other hand, the element rods 30 formed on the openings 22 of the first mask layer 20 remain without being removed. Fig. 20 , the element rod 30 formed on the opening 22 of the first mask layer 20 can be physically separated from the substrate 10 or the lower plate 11. In the light emitting element 300_2 manufactured by the above method, the separation surface 390_2 as the surface separated from the substrate 10 can have a concavo-convex structure, or a partially inclined area can be formed.

[0128] As described above, when the light emitting element 300_2 is connected to the contact electrodes 230 and 240, this may cause a problem of disconnection of the contact electrode material. To solve this problem, it may be necessary to make the separation surface 390_2 of the light emitting element 300_2 flat by additional etching.

[0129] On the other hand, the light emitting element 300_1 manufactured according to the embodiment is formed on the mask pattern 21 provided in a portion of the element stack 30' of the first mask layer 20, and is separated by a chemical method to flatten the separation surface 390_1. That is, the element rod 30 formed by crystal growth can be separated from the substrate 10, and the flattening of the separation surface 390_1 can be performed.

[0130] That is, refer to Fig.19 and Fig. 20 , the first mask layer 20 formed on the lower board 11 may be removed by etching, and the element rods 30 may be separated. The element rods 30 formed on the mask pattern 21 of the first mask layer 20 may be separated by etching, and the element rods 30 formed on the openings 22 may be separated by a physical method. Here, the light emitting element 300_1 and the light emitting element 300_2, which are separated from the mask pattern 21 and the opening 22, respectively, may include separation surfaces having shapes different from each other.

[0131] In this article, we will refer to Fig.21 and Fig. 22 For convenience of explanation, the light emitting element 300_1 formed on and separated from the mask pattern 21 is referred to as the first light emitting element 300_1, and the light emitting element 300_2 formed on and separated from the opening 22 is referred to as the second light emitting element 300_2.

[0132] Fig.21 and Fig. 22 1 is an enlarged view showing a separation surface 390_1 of a first light emitting element 300_1 and a separation surface 390_2 of a second light emitting element 300_2 according to an embodiment.

[0133] Reference Fig.21 and Fig. 22, the first light emitting element 300_1 and the second light emitting element 300_2 have a separation surface 390_1 and a separation surface 390_2 on which the first semiconductor layer 310 is disposed. The separation surface 390_1 of the first light emitting element 300_1 is a surface in contact with the mask pattern 21 of the first mask layer 20. When the first light emitting element 300_1 is separated, the separation surface 390_1 has a relatively flat shape. On the other hand, the separation surface 390_2 of the second light emitting element 300_2 can be separated from the area of ​​the opening 22 contacting the first mask layer 20. When the first mask layer 20 is removed, the element rod 30 formed on the opening 22 is not separated together, but remains engaged with the first sub-conductive semiconductor layer 31 '. When the element rod 30 is separated by a physical method, the separation surface 390_2 of the second light emitting element 300_2 has a rough surface.

[0134] Since the second light emitting element 300_2 is separated from the lower board 11 by a physical method, the second light emitting element 300_2 cannot be smoothly separated from the grain boundary between the first sub-conductive semiconductor layer 31' and the first semiconductor layer 310. Since a portion of the second light emitting element 300_2 having relatively weak lattice attraction is decomposed at each grain boundary, a separation surface 390_2 of the second light emitting element 300_2 has various shapes without uniformity.

[0135] Specifically, when a portion of the separation surface 390_2 of the second light emitting element 300_2 protrudes or is recessed to be inclined or has a rough surface, an empty space may be formed in the region connected to the contact electrodes 230 and 240. Figure 7 Disconnection of the contact electrode material occurs in region III-III' where the light emitting element 300 is connected to the contact electrodes 230 and 240. As described above, disconnection of the contact electrode material may cause problems of open circuit failure and light emission failure of the light emitting element 300.

[0136] On the other hand, when the separation surface 390_1 of the first light emitting element 300_1 is relatively flat, Figure 7 The disconnection of the contact electrode material may not occur in the region III-III', and the open circuit failure and the light emitting failure of the light emitting element 300_1 having the semiconductor layers 310 and 320 or the electrode layer 360 or 370 may be prevented or substantially prevented. Thus, the reliability of the light emitting element 300 in the display device may be improved.

[0137] According to an embodiment, the roughness of the separation surface 390_1 of the first light emitting element 300_1 may have a value of about 10% of the roughness of the separation surface 390_2 of the second light emitting element 300_2. For example, the roughness of the separation surface 390_1 of the first light emitting element 300_1 may have a value of 8nm Ra to 12nm Ra, and the roughness of the separation surface 390_2 of the second light emitting element 300_2 may have a value of 90nm Ra to 110nm Ra. However, the present invention is not limited thereto.

[0138] As described above, the first mask layer 20 may have any of a variety of structures. Since the light emitting element 300 according to the embodiment has a relatively flat separation surface, the structure of the first mask layer 20 is not particularly limited to a range in which a disconnection failure associated with the first contact electrode 230 or the second contact electrode 240 does not occur. Herein, various structures of the first mask layer 20 formed on the substrate 10 or the lower board 11 will be described.

[0139] Figure 23 to Figure 26 is a plan view of the lower plate 11 on which the first mask layer 20 is formed according to an embodiment.

[0140] The first mask layer 20 formed on the lower board 11 may include a mask pattern 21 and an opening 22, and may form a pattern on at least a portion of the lower board 11. The mask patterns 21 may be disposed to be spaced apart from each other, and the opening 22 may be formed in a region where the mask patterns 21 are spaced apart from each other.

[0141] In an embodiment, if Fig.23 As shown in , the first mask layer 20_1 may include a plurality of flat circular mask patterns 21_1, and the plurality of flat circular mask patterns 21_1 may be disposed to be spaced apart from each other. The opening 22_1 may be formed in a region where the plurality of mask patterns 21_1 are spaced apart from each other.

[0142] Fig.23 The configuration in which the circular mask pattern 21_1 is formed to protrude from the lower plate 11 and the opening 22_1 is formed to be recessed is shown. However, the present invention is not limited thereto. Fig.24 As shown in , the circular opening 22_2 may be formed to be recessed, and the mask pattern 21_2 may be formed to protrude from the lower board 11 in other regions. When the material of the mask pattern 21_1 is deposited in the step of forming the first mask layer 20_1, the mask pattern 21_1 may protrude according to the pattern of the first mask layer 20_1. Conversely, when the opening 22_2 is formed by forming a layer including the mask pattern 21_2 on the lower board 11 and then etching the layer according to the pattern of the first mask layer 20_2, the opening 22_2 may be formed to be recessed according to the shape of the pattern.

[0143] In addition, if Fig.25 As shown in , each of the mask patterns 21_3 may have a rectangular shape. However, the present invention is not limited thereto, and the mask pattern 21_3 formed on the lower plate 11 may have any one of a variety of shapes. In addition to the mask pattern 21_3 being formed to have a rectangular shape, Fig.25 The first mask layer 20_3 may be Fig.23 The first mask layer 20_1 is the same as that of the first mask layer 20_1. Fig.23 As shown in Fig.25 The first mask layer 20_3 may have a configuration in which the mask pattern 21_3 is formed to protrude from the lower board 11 and the opening 22_3 is formed to be recessed.

[0144] like Fig.26 As shown in , the first mask layer 20_4 may include a plurality of linear mask patterns 21_4 located on the lower plate 11, and the plurality of linear mask patterns 21_4 may be arranged to be spaced apart from each other. The opening 22_4 may be formed in a region where the plurality of linear mask patterns 21_4 are spaced apart from each other. According to an embodiment, the first mask layer 20_4 may be configured such that at least one mask pattern 21_4 is disposed between one side of the lower plate 11 and the other side of the lower plate 11 facing the side thereof. The mask patterns 21_4 may be arranged to be spaced apart from each other in a second direction perpendicular to the first direction, wherein the first direction is a direction in which the mask patterns 21_4 are connected to each other, and the opening 22_4 may be formed between the mask patterns 21_4. In addition to the mask patterns 21_4 being formed in a linear shape, Fig.26 The first mask layer 20_4 and Fig.25 The first mask layer 20_3 is the same.

[0145] Refer again Figures 10 to 12 as well as Fig.26 , the crystals of the first sub-conductive semiconductor layer 31' may grow through the opening 22 in the vertical direction, and may grow on the mask pattern 21 in the horizontal direction. Here, the ratio of the diameter (or width) d1 of the mask pattern 21 to the diameter (or width) d2 of the opening 22 may be changed, wherein the diameter (or width) d2 of the opening 22 corresponds to the distance between the mask patterns 21. However, when the diameter d2 of the opening 22 is too small, the crystal growth rate of the first sub-conductive semiconductor layer 31' may be slow. Conversely, when the diameter d2 of the opening 22 is too large, the growth of the crystals on the first mask layer 20 in the horizontal direction may be slower than the growth of the crystals on the first mask layer 20 in the vertical direction. Therefore, the crystals of the first sub-conductive semiconductor layer 31' may not be fused on the mask pattern 21. Therefore, in an embodiment, the diameter ratio of the mask pattern 21 to the opening 22 in the first mask layer 20 is adjusted within a specific range.

[0146] In an embodiment, the diameter d1 of the mask pattern 21 measured in one axis direction may be 3 to 5 times the diameter d2 of the opening 22 measured in the same direction as the one axis direction. In other words, the diameter d1 between any first opening 22 and a second opening 22 formed at an opposite side of the mask pattern 21 adjacent to the first opening 22 may be 3 to 5 times the diameter d2 of the opening 22. Fig.26 As shown in , the diameter d1 of the mask pattern 21_4 may be larger than the diameter d2 of the opening 22_4. For example, when the diameter d1 of the mask pattern 21_4 has a range of 3.5 μm to 4.5 μm, the diameter d2 of the opening 22 may have a range of 1 μm to 1.8 μm.

[0147] When the diameters of the mask pattern 21 and the opening 22 of the first mask layer 20 have values ​​within the above range, growth of crystals of the first sub-conductive semiconductor layer 31' in the vertical direction and fusion of the crystals on the mask pattern 21 may be appropriately performed. Specifically, in order to fuse the crystals of the first sub-conductive semiconductor layer 31' on the mask pattern 21, the diameter d1 of the mask pattern 21 may be adjusted not to be too large compared to the diameter d2 of the opening 22. Therefore, a portion of the first conductive semiconductor layer 31 is formed on the first mask layer 20, and the first conductive semiconductor layer 31 may be completely formed by continuous crystal growth.

[0148] In addition, as described above, the mask pattern 21 of the first mask layer 20 may include at least one of an insulating material and a conductive material. Fig. 27 ) may be formed of a single layer or a multilayer of two or more layers including the above materials. According to an embodiment, the mask pattern 21_5 may have a structure in which one or more layers are stacked, an insulating material layer 21_5' including an insulating material may be provided on its surface in contact with the lower plate 11, and a conductive material layer 21_5" including a conductive material may be provided on the insulating material layer 21_5'.

[0149] Fig. 27 is a cross-sectional view of a lower board 11 on which a first mask layer 20_5 is formed according to another embodiment.

[0150] In an embodiment, the mask pattern 21_5 may include an insulating material layer 21_5' disposed on a surface contacting the lower board 11 and a conductive material layer 21_5' disposed on the insulating material layer 21_5'. However, the present invention is not limited thereto, and the mask pattern 21_5 may include three or more different material layers, and the stacking order thereof may be reversed. Fig. 27 A double-layer mask pattern 21_5 in which an insulating material layer 21_5 ′ and a conductive material layer 21_5 ″ are sequentially stacked is shown.

[0151] The mask pattern 21_5 may be formed in multiple layers including a combination of the above materials. For example, when the mask pattern 21_5 has a double-layer structure, it has a structure of an insulating material layer 21_5' / a conductive material layer 21_5", and may include ITO / SiO x 、ZnO / SiO x , ITO / ZnO, ZnO / ITO, graphene / SiO x Or graphene / graphene oxide. In an embodiment, when the mask pattern 21_5 has a structure in which an insulating material layer 21_5' and a conductive material layer 21_5" are sequentially stacked upward, in the step of removing the mask pattern 21_5 (i.e., when separating the element rod 30 from the substrate 10 or the lower plate 11), only the insulating material layer 21_5' may be etched, and the conductive material layer 21_5" may be attached to the light emitting element 300 to form an electrode layer 360. However, this is merely an embodiment of the present invention, and the present invention is not limited thereto and may have various types of structures.

[0152] As described above, according to the method for manufacturing a light-emitting element according to an embodiment, the element rod grown on the substrate is separated from the substrate by a chemical separation method, so that the separation surface of the manufactured light-emitting element can be flat. In addition, the light-emitting element can be manufactured by forming an insulating layer on the outer surface of the element rod and then separating the element rod from the substrate. Therefore, a light-emitting element with two flat side surfaces can be manufactured without an additional etching process.

[0153] In addition, since the light emitting element disposed between the electrodes of the display device has two substantially flat surfaces substantially parallel to each other, disconnection or open circuit failure of the contact electrode material can be prevented or substantially prevented when connected to the contact electrode.

[0154] However, the effects of the present invention are not limited to the foregoing, and other various effects are expected herein.

[0155] Although some exemplary embodiments of the present invention have been disclosed for illustrative purposes, those skilled in the art will appreciate that various modifications, additions and substitutions are possible, without departing from the scope and spirit of the invention as disclosed in the accompanying claims.

Claims

1. Display device, include: base substrate; a first electrode and a second electrode, the first electrode and the second electrode being spaced apart from each other; a first contact electrode, the first contact electrode being located on an upper surface of the first electrode; a second contact electrode, the second contact electrode being located on an upper surface of the second electrode; as well as at least one light emitting element, the at least one light emitting element being located in a region where the first electrode and the second electrode are spaced apart from each other, Wherein, the two side surfaces of the light-emitting element in contact with the first contact electrode and the second contact electrode have a flat shape so as to be parallel to a surface perpendicular to the base substrate, wherein the side surface of the two side surfaces of the light-emitting element separated from the substrate on which the light-emitting element is pre-formed has a surface roughness of 8nm Ra to 12nm Ra.

2. The display device according to claim 1, in, The light emitting element comprises: n-type semiconductor layer; an active layer, the active layer being located on the n-type semiconductor layer to emit light in a specific wavelength band; a p-type semiconductor layer, the p-type semiconductor layer being located on the active layer; and an insulating film surrounding side surfaces of the n-type semiconductor layer, the p-type semiconductor layer, and the active layer, The length measured in the direction in which the n-type semiconductor layer and the p-type semiconductor layer are stacked is longer than the spacing length between the first electrode and the second electrode.

3. The display device according to claim 2, in, A contact surface between the light emitting element and the first contact electrode or the second contact electrode includes at least one surface perpendicular to the base substrate. 4 . The display device according to claim 2 , further comprising at least one passivation layer located on an outer surface of the insulating film of the light emitting element.