Rainwash-resistant mancozeb water dispersible granule and preparation method thereof
By using polyvinylpyrrolidone and/or maleamic acid as binder, combining the coordination effect of 1,3-propanedithiol to form a protective film, the poor adhesion of mancozeb water dispersed granules is solved and the adhesion of mancozeb water dispersed granules is solved. The problem of insufficient rainwater erosion performance has achieved better adhesion and environmentally friendly use.
Patent Information
- Application Number
- CN202411058204.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-11-12
AI Technical Summary
The existing mancozeb water dispersed granules are easily washed by rainwater during use, resulting in environmental pollution and reduced prevention and control effects, and have poor adhesion. It is necessary to develop products that are resistant to rainwater erosion.
Polyvinylpyrrolidone and/or maleamic acid are used as binders, combined with 1,3-propanedithiol, and a protective film is formed through coordination and complexation reaction, which improves the adhesion of the granules and rainwater erosion resistance. performance.
It significantly improves the adhesion and rainwater erosion resistance of mancozeb water dispersed granules, extends the residence time of the granules on the plant surface, and reduces resource waste and environmental pollution.
Smart Images

Figure SMS_1 
Figure SMS_2
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of pesticide preparations, and in particular to a rain-resistant mancozeb water-dispersible granule and a preparation method thereof. Background Art
[0002] Mancozeb is one of the main protective fungicide products in my country's fruit and vegetable production areas. It has a good control effect on a variety of fungal diseases. With the widespread use of mancozeb in my country's fruit and vegetable production areas, some problems have gradually emerged. During use, some pesticides are easily washed into the soil, rivers and groundwater by rainwater, causing environmental pollution, which has an adverse effect on the soil ecosystem and the water ecosystem, destroying biodiversity and ecological balance. At the same time, the scouring of rainwater also causes the fungicide to stay on the crop surface for a shorter time, reducing the control effect. Farmers need to increase the number of times or dosages of pesticides, which leads to a waste of resources. Therefore, the development of a mancozeb water-dispersible granule with good adhesion and resistance to rainwater scouring is a problem that needs to be solved urgently. Summary of the invention
[0003] The invention provides a rain-resistant mancozeb water-dispersible granule and a preparation method thereof, which solves the problems of poor adhesion and low resistance to rain in the related art.
[0004] The technical scheme of the present invention is as follows: The present invention provides a mancozeb water-dispersible granule resistant to rain erosion, comprising the following raw materials in parts by weight: 20-80 parts of mancozeb, 6-12 parts of dispersant, 3-6 parts of wetting agent, 3-9 parts of disintegrant, 5-7 parts of binder, 1-3 parts of stabilizer, 2-6 parts of 1,3-propanedithiol, 10-20 parts of filler and 150-200 parts of water.
[0005] As a further technical solution, the binder includes polyvinyl pyrrolidone and / or maleamic acid.
[0006] As a further technical solution, when the binder is polyvinyl pyrrolidone and maleamic acid, the mass ratio of polyvinyl pyrrolidone to maleamic acid is 2-4:1.
[0007] In the present invention, maleamic acid is used as a binder, and the carboxyl group and amide group in the maleamic acid can enhance the adhesion of the mancozeb water dispersible granules on the plant surface through coordination with the metal ions in mancozeb, which helps to improve the residence time and effect of the mancozeb water dispersible granules on the plant, and achieves good adhesion and rain erosion resistance of the mancozeb water dispersible granules.
[0008] As a further technical solution, the dispersant includes one or more of sodium lignin sulfonate, polyoxyethylene oxypropylene, and sodium tripolyphosphate.
[0009] As a further technical solution, the wetting agent includes one or more of saponins, sodium lauryl sulfate, and sodium laurate.
[0010] As a further technical solution, the disintegrant includes one or both of hydroxymethyl cellulose and calcium chloride.
[0011] As a further technical solution, the stabilizer includes one or both of tributyl phosphate and triphenyl phosphite.
[0012] As a further technical solution, the filler includes one or more of bentonite, attapulgite, and talc.
[0013] The present invention also proposes a method for preparing a rain-resistant mancozeb water-dispersible granule, comprising the following steps: S1, mixing and evenly grinding mancozeb, a dispersant, a disintegrant, a stabilizer and a filler to obtain a mixed powder; S2, dissolving the wetting agent and the binder in water, adding the mixed powder and 1,3-propanedithiol, stirring evenly to obtain a mixture; S3, extruding, granulating and drying the mixture to obtain water-dispersible granules of mancozeb.
[0014] As a further technical solution, the drying temperature is 50-80°C.
[0015] The working principle and beneficial effects of the present invention are: In the present invention, 1,3-propanedithiol is used as a film-forming agent, and the thiol group in the film-forming agent can form a coordination bond with the metal ions in the mancozeb, thereby generating a complex reaction, and the complex reaction causes a chemical bond between the 1,3-propanedithiol molecules and the surface of the mancozeb particles to form a protective film structure. The film can block the erosion of the granules by the external environment such as rainwater, improve the stability of the water-dispersible granules, and delay the release rate of the active ingredients, which helps to increase the residence time and adhesion performance of the granules on the plant surface, and effectively improve the rain erosion resistance of the mancozeb water-dispersible granules. DETAILED DESCRIPTION
[0016] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0017] In the following examples and comparative examples: Hydroxymethyl cellulose: content ≥95%, manufacturer is Guangdong Zhongke Hongtai New Materials Co., Ltd.; Bentonite: particle size is 320 mesh, the manufacturer is Shenzhen Haiyang Powder Technology Co., Ltd.; Polyvinyl pyrrolidone: model K30, manufacturer is Henan Yueze Chemical Co., Ltd.; Polyoxyethylene oxypropylene: Model DW3432, manufacturer: Wuhan Lanabai Pharmaceutical Chemical Co., Ltd.; Attapulgite: particle size is 325 mesh, the manufacturer is Lingshou County Marble Mineral Products Processing Plant; Talc: particle size is 325 mesh, the manufacturer is Hebei Bingta Mineral Products Co., Ltd.; Corn starch: industrial grade, density 1.232g / cm 3 , the manufacturer is Wujiang Hengda Fine Chemical Co., Ltd.
[0018] Example 1 S1, weigh 20 parts of mancozeb, 6 parts of sodium lignin sulfonate, 3 parts of hydroxymethyl cellulose, 1 part of tributyl phosphate, and 10 parts of bentonite, mix and grind them evenly to obtain a mixed powder; S2, weigh 3 parts of sapodilla and 5 parts of polyvinyl pyrrolidone, dissolve them in 150 parts of water, add 2 parts of 1,3-propanedithiol, and stir to obtain a mixture; S3, extruding and granulating the mixture and drying it at 50° C. to obtain water-dispersible granules of mancozeb.
[0019] Example 2 S1, weigh 50 parts of mancozeb, 9 parts of polyoxyethylene propylene, 6 parts of hydroxymethyl cellulose, 2 parts of tributyl phosphate, and 15 parts of attapulgite, mix and grind them evenly to obtain a mixed powder; S2, weigh 4.5 parts of sodium lauryl sulfate and 6 parts of polyvinyl pyrrolidone, dissolve them in 175 parts of water, add 4 parts of 1,3-propanediol, and stir to obtain a mixture; S3, extruding and granulating the mixture and drying it at 65°C to obtain water-dispersible granules of mancozeb.
[0020] Example 3 S1, weigh 80 parts of mancozeb, 12 parts of sodium tripolyphosphate, 9 parts of calcium chloride, 3 parts of triphenyl phosphite, and 20 parts of talc, mix and grind them evenly to obtain a mixed powder; S2, weigh 6 parts of sodium laurate and 7 parts of polyvinyl pyrrolidone, dissolve them in 200 parts of water, add 6 parts of 1,3-propanedithiol, and stir to obtain a mixture; S3, extruding and granulating the mixture and drying it at 80° C. to obtain water-dispersible granules of mancozeb.
[0021] Example 4 Compared with Example 2, Example 4 is different in that polyvinyl pyrrolidone is replaced by an equal amount of maleamic acid.
[0022] Example 5 Compared with Example 2, Example 5 is different in that 6 parts of polyvinyl pyrrolidone are replaced by 3 parts of polyvinyl pyrrolidone and 3 parts of maleamic acid.
[0023] Example 6 Compared with Example 2, Example 6 is different in that 6 parts of polyvinyl pyrrolidone are replaced by 4 parts of polyvinyl pyrrolidone and 2 parts of maleamic acid.
[0024] Example 7 Compared with Example 2, Example 7 is different in that 6 parts of polyvinyl pyrrolidone are replaced by 4.5 parts of polyvinyl pyrrolidone and 1.5 parts of maleamic acid.
[0025] Example 8 Compared with Example 2, Example 8 is different in that 6 parts of polyvinyl pyrrolidone is replaced by 4.8 parts of polyvinyl pyrrolidone and 1.2 parts of maleamic acid.
[0026] Example 9 Compared with Example 2, Example 9 is different in that 6 parts of polyvinyl pyrrolidone are replaced by 5 parts of polyvinyl pyrrolidone and 1 part of maleamic acid.
[0027] Comparative Example 1 Compared with Example 2, the difference in Comparative Example 1 is that polyvinyl pyrrolidone is replaced by an equal amount of corn starch.
[0028] The rain-resistant mancozeb water dispersible granules prepared in Examples 1 to 9 and Comparative Example 1 were tested according to the following method: 1. Loss of drug film layer: Select a film material with similar smoothness to the plant surface as the attachment (9cm×5cm), put the attachment in a drying oven, dry it at 35℃ for 2 hours, and weigh it one by one; spray the agent evenly on the attachment to form a drug film layer, dry it under natural conditions for 24 hours, transfer it to a drying oven and dry it at 35℃ for 2 hours, weigh it again, and calculate the dry weight of the coating agent on each attachment. Set up 3 replicates for each drug treatment; fix the weighed attachments on the tree trunk with thumbtacks; on the 5th, 10th, 20th and 30th days, take one attachment from the east, south, west and north of the tree respectively, dry it in an oven at 35℃ for 2 hours, and then weigh it to calculate the loss of the coating agent on each attachment.
[0029] Data processing: All samples and blank attachments of the same specifications are dried and weighed; the difference between the mass of the sample with drug film and the blank attachment is the mass of the drug film of the sample; the mass of the drug film of the sample sample taken for the first time is taken as the reference value, and the difference between the mass of the drug film of the sample sample taken each time and the reference value is taken as the loss of the drug film of the sampling; 2. Ratio of drug spots before and after flushing: Dilute the water-dispersible granules of mancozeb 500 times, use a pipette to draw 1 μm of each treatment solution and drop it on a clean glass slide, place three glass slides for each treatment solution, place them in a 30°C incubator to dry for 3 hours, tilt the glass slide at 60 degrees under a spray tower, spray 1L of water, and dry them in a 30°C incubator after spraying. Use software to calculate the area of drug spots on the glass slides before and after spray flushing, and calculate the ratio of the area of drug spots after flushing to that before flushing to obtain the rain resistance effect.
[0030] The test results are shown in the following table: Table 1 Adhesion performance test results of the rain-resistant mancozeb water-dispersible granules prepared in Examples 1 to 9 and Comparative Example 1
[0031] Table 2 Test results of rainwater erosion resistance of water-dispersible granules of mancozeb prepared in Examples 1 to 9 and Comparative Example 1
[0032] Compared with Comparative Example 1, Examples 1 to 3 added polyvinyl pyrrolidone, and Example 4 added maleamic acid. As a result, the drug film loss rate of Examples 1 to 4 was less than that of Comparative Example 1, and the drug spot ratio before and after flushing of Examples 1 to 4 was greater than that of Comparative Example 1, indicating that the binder polyvinyl pyrrolidone or maleamic acid can improve the adhesion and rainwater scouring resistance of the water-dispersible granules.
[0033] Compared with Example 2 and Example 4, Examples 5 to 9 simultaneously added polyvinyl pyrrolidone and maleamic acid. As a result, the drug film loss rate of Examples 5 to 9 was less than that of Examples 2 and Example 4, and the drug spot ratio before and after flushing was greater than that of Examples 2 and Example 4, indicating that polyvinyl pyrrolidone and maleamic acid play a synergistic role, which can further improve the adhesion and rainwater resistance of the water dispersible granules.
[0034] Compared with Example 5, Examples 6 to 9 added polyvinyl pyrrolidone and maleamic acid in different proportions. As a result, the drug film loss rate of Examples 6 to 8 was less than that of Examples 5 and 9, and the drug spot ratio before and after flushing was greater than that of Examples 5 and 9, indicating that when the mass ratio of polyvinyl pyrrolidone and maleamic acid was 2 to 4:1, and the preferred mass ratio was 3:1, the adhesion and rainwater scouring resistance of the water dispersible granules were optimal.
[0035] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A water-dispersible granule of mancozeb that is resistant to rain erosion. It is characterized in that It includes the following raw materials in parts by weight: 20-80 parts of mancozeb, 6-12 parts of dispersant, 3-6 parts of wetting agent, 3-9 parts of disintegrant, 5-7 parts of binder, 1-3 parts of stabilizer, 2-6 parts of 1,3-propanedithiol, 10-20 parts of filler and 150-200 parts of water.
2. The rain-resistant mancozeb water dispersible granules according to claim 1, It is characterized in that The binder includes polyvinyl pyrrolidone and / or maleamic acid.
3. A rain-resistant mancozeb water dispersible granules according to claim 2, It is characterized in that When the binder is polyvinyl pyrrolidone and maleamic acid, the mass ratio of polyvinyl pyrrolidone to maleamic acid is 2-4:
1.
4. The rain-resistant mancozeb water dispersible granules according to claim 1, It is characterized in that The dispersant includes one or more of sodium lignin sulfonate, polyoxyethylene oxypropylene, and sodium tripolyphosphate.
5. The rain-resistant mancozeb water dispersible granules according to claim 1, It is characterized in that The wetting agent includes one or more of saponins, sodium lauryl sulfate, and sodium laurate.
6. The rain-resistant mancozeb water dispersible granules according to claim 1, It is characterized in that The disintegrant comprises one or both of hydroxymethyl cellulose and calcium chloride.
7. The rain-resistant mancozeb water dispersible granules according to claim 1, It is characterized in that The stabilizer includes one or both of tributyl phosphate and triphenyl phosphite.
8. The rain-resistant mancozeb water dispersible granules according to claim 1, It is characterized in that The filler includes one or more of bentonite, attapulgite and talc.
9. A method for preparing a rain-resistant mancozeb water dispersible granule according to any one of claims 1 to 8, It is characterized in that The following steps are involved: S1, mixing and evenly grinding mancozeb, a dispersant, a disintegrant, a stabilizer and a filler to obtain a mixed powder; S2, dissolving the wetting agent and the binder in water, adding the mixed powder and 1,3-propanedithiol, stirring evenly to obtain a mixture; S3, extruding, granulating and drying the mixture to obtain water-dispersible granules of mancozeb.
10. The method for preparing the rain-resistant mancozeb water dispersible granules according to claim 9, It is characterized in that The drying temperature is 50-80°C.