Denitration catalyst coating method
By separately coating the catalyst support and active ingredients and controlling the load ratio, the problem of insufficient uniformity and loading rate in the catalyst coating process is solved, and efficient nitrogen oxide removal is achieved, meeting ultra-low emission standards.
Patent Information
- Application Number
- CN202411033631.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-12
AI Technical Summary
In the existing catalyst coating process, due to the large amount of slurry components, it is difficult to ensure the uniformity of the coating. When the coating is too thick or too thin, the loading rate of the active component is insufficient, which affects the performance of the catalyst.
The catalyst support component TiO2 and active ingredient V2O5 are separately coated, and the load ratio between V2O5 and TiO2 is controlled by repeated impregnation and drying steps to form a solid coating to ensure stable catalyst performance.
The catalyst performance is improved, the stability and service life of the catalyst during the heating and cooling process is ensured, and the nitrogen oxide removal rate that meets the ultra-low emission standards is met.
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of flue gas treatment, in particular to the field of flue gas denitration, and specifically to a denitration catalyst coating method. Background Art
[0002] The main components of atmospheric pollutants are nitrogen oxides (NO). X , sulfur dioxide SO2 and particulate matter PM. Among them, NO X It can lead to acid rain, photochemical smog and ozone layer depletion. X As emission standards become increasingly stringent, selective catalytic reduction denitrification technology (SCR) is currently the most widely used and most efficient flue gas denitrification technology, and denitrification catalyst is the core of SCR denitrification technology.
[0003] At present, the most commonly used catalyst coating process is slurry coating (direct coating). In this process, the carrier component TiO2 and the active component V2O5 are first prepared into catalyst particles in a certain ratio, and then the prepared catalyst particles are ball-milled to the required particle size, and a surfactant is added to improve the dispersibility of the catalyst particles. Inorganic binders and organic binders are added to make the catalyst particles in the slurry adhere to the cordierite carrier. Finally, the cordierite with the catalyst coated on the surface is calcined at a high temperature to obtain an integral catalyst. Because the direct coating method has more slurry components, it is difficult to ensure the uniformity of the coating during the impregnation process. If the coating is thick, the surface part of the coating may not be firmly bonded to the cordierite carrier and is easy to fall off; if the coating is too thin, the active component loading rate is insufficient, resulting in unsatisfactory catalyst performance. Summary of the invention
[0004] The present invention provides a denitration catalyst coating method in order to solve the problems that when direct coating is currently used in the catalyst coating process, it is difficult to ensure the uniformity of the coating during the impregnation process due to the large number of slurry components; when the coating is too thick, the surface layer of the coating is not firmly bonded to the carrier; when the coating is too thin, the active component loading rate is insufficient and affects the catalyst performance.
[0005] The present invention is implemented by the following technologies: The present invention provides a denitration catalyst coating method, comprising the following steps: a. Preparation of cordierite standard blocks A honeycomb catalyst with cordierite as the basic carrier is used. The honeycomb catalyst is generally a homogeneous catalyst. A honeycomb cordierite with a mesh size of 200 is cut into cordierite standard blocks as catalyst elements. The cross section of the cordierite standard block is 150mm×150mm and the length is 300mm. b. Preprocessing The cordierite standard block was soaked in a pretreatment agent at room temperature for 10 hours. The pretreatment agent was a citric acid aqueous solution with a mass fraction of 5%. The acid solution would make the surface of the cordierite rough, increase the porosity, and reduce its thermal expansion coefficient. After being taken out, it was rinsed with distilled water for 0.5 hours, and then stood at room temperature for 10 hours to dry, thereby preparing a pretreated honeycomb cordierite as a coating substrate. c. TiO2 coating The catalyst carrier component TiO2 and the active component V2O5 are coated separately, the TiO2 organic precursor solution tetrabutyl titanate and the organic chelating agent sodium dithioformate are dissolved in an alcohol solvent such as ethanol or ethylene glycol, the dispersant sodium pyrophosphate is added and stirred evenly, and the mixture is allowed to stand for aging in a water bath at 60°C for 2 hours to prepare a TiO2 sol, an equal volume of pretreated cordierite is immersed in the TiO2 sol, and after being immersed at room temperature for 10 hours, the mixture is taken out, allowed to stand for 2 hours to drain the residual glue in the pores, and dried at 450-600°C for 6 hours to obtain a cordierite coated with a TiO2 coating; d, V2O5 coating V2O5 was ground into powder and then added to distilled water to prepare an impregnation solution, the ratio of V2O5 to distilled water was 1:10 by mass, and the cordierite coated with TiO2 was placed in the impregnation solution, immersed in equal volume for 5 hours, taken out, left to stand until the residual liquid in the pores was drained, and dried at 450-600°C for 6 hours to obtain a cordierite with a complete coating; e. Repeated V2O5 coating To control the coating ratio of V2O5 and TiO2, repeat step d 4 to 6 times and repeatedly apply the V2O5 coating.
[0006] Compared with the prior art, the present invention has the following beneficial effects: The present invention provides a denitration catalyst coating method, which controls the loading amount of the active ingredient V2O5 during impregnation through repeated impregnation, avoids changes in the relative content of the active ingredient V2O5 and the carrier ingredient TiO2 causing unstable catalyst performance, and ultimately produces a catalyst with ideal performance.
[0007] The present invention adopts a method of separately coating the catalyst carrier component TiO2 and the active component V2O5, first coating the carrier component TiO2 on cordierite, and then coating the active component V2O5 on the carrier component TiO2; the loading ratio of the active component V2O5 to the carrier component TiO2 can be effectively controlled at the highest point of the performance curve, and the catalyst efficiency is high.
[0008] The present invention has high thermal stability. When the coating is prepared by the coating method, the carrier component TiO2 can be bonded with the cordierite carrier by selecting the loading method to form a relatively firm coating, and then the active component V2O5 is loaded. It is ensured that during the heating and cooling process, the catalyst coating is closely attached to the cordierite carrier and is not easy to fall off, thereby extending the service life of the catalyst. DETAILED DESCRIPTION
[0009] The specific embodiments of the present invention are described in detail below.
[0010] A denitration catalyst coating method, the specific steps are as follows: The following steps are involved: a. Preparation of cordierite standard blocks A honeycomb catalyst with cordierite as the basic carrier is used. The honeycomb catalyst is generally a homogeneous catalyst. A honeycomb cordierite with a mesh size of 200 is cut into cordierite standard blocks as catalyst elements. The cross section of the cordierite standard block is 150mm×150mm and the length is 300mm. b. Preprocessing The cordierite standard block was soaked in a pretreatment agent at room temperature for 10 hours. The pretreatment agent was a 5% by mass citric acid aqueous solution. The acid solution would make the cordierite surface rough, increase the porosity, and reduce its thermal expansion coefficient. After being taken out, it was rinsed with distilled water for 0.5 hours, and then allowed to stand at room temperature for 10 hours to dry, thereby preparing a pretreated honeycomb cordierite as a coating substrate. c. TiO2 coating The catalyst carrier component TiO2 and the active component V2O5 are coated separately, the TiO2 organic precursor solution tetrabutyl titanate and the organic chelating agent sodium dithioformate are dissolved in an alcohol solvent such as ethanol or ethylene glycol, the dispersant sodium pyrophosphate is added and stirred evenly, and the mixture is allowed to stand for aging in a water bath at 60°C for 2 hours to prepare a TiO2 sol, an equal volume of pretreated cordierite is immersed in the TiO2 sol, and after being immersed at room temperature for 10 hours, the cordierite is taken out, allowed to stand for 2 hours to drain the residual glue in the pores, and dried at 550°C for 6 hours to obtain a cordierite coated with a TiO2 coating; d, V2O5 coating V2O5 was ground into powder and then added to distilled water to prepare an impregnation solution, the ratio of V2O5 to distilled water was 1:10 by mass, and the cordierite coated with TiO2 was placed in the impregnation solution, immersed in equal volume for 5 hours, taken out, left to stand until the residual liquid in the pores was drained, and dried at 550°C for 6 hours to obtain a cordierite with a complete coating; e. Repeated V2O5 coating In order to control the coating ratio of V2O5 and TiO2, the coating amount was detected by weighing after coating, and step d was repeated 5 times to repeat the V2O5 coating.
[0011] The coated denitration catalyst prepared by the above method was tested. In a small flue gas denitration device, exhaust gas was introduced, the exhaust gas treatment capacity was 200m³ / h, the initial NOx concentration was 300mg / m³, the exhaust gas temperature was heated to 350°C and then passed through the denitration device. The denitration device was mainly composed of a denitration reactor, and the catalyst prepared in this embodiment was built in the denitration reactor to convert NO X The concentration is qualified when it drops below 50mg / m³.
[0012] According to test results, the denitration catalyst prepared by this embodiment can achieve a nitrogen oxide removal rate of more than 85%, meeting the national ultra-low emission standards for nitrogen oxides.
[0013] The scope of protection claimed by the present invention is not limited to the above specific embodiments. For those skilled in the art, the present invention may have various deformations and changes. Any modifications, improvements and equivalent substitutions made within the concept and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A denitration catalyst coating method, characterized in that: The following steps are involved: a. Preparation of cordierite standard blocks Take honeycomb cordierite with a mesh size of 200 and cut it into cordierite standard blocks; b. Preprocessing The cordierite standard block was immersed in the pretreatment agent at room temperature for 10 hours, and then washed with distilled water for 0.5 hours, and then allowed to stand at room temperature for 10 hours to dry, thereby preparing the pretreated honeycomb cordierite; c. TiO2 coating Dissolve a TiO2 organic precursor solution and an organic chelating agent in alcohol, add a dispersant and stir evenly, let stand for 2 hours to prepare a TiO2 sol, immerse an equal volume of pretreated cordierite in the TiO2 sol, take it out after immersion at room temperature for 10 hours, let stand for 2 hours to drain the residual glue in the pores, dry it at 450-600°C for 6 hours, and obtain a cordierite coated with a TiO2 coating; d, V2O5 coating Grind V2O5 into powder and add distilled water to make an impregnation solution, place the cordierite coated with TiO2 in the impregnation solution, immerse in equal volume for 5 hours, take out, let stand until the residual liquid in the pores is drained, and dry at 450-600℃ for 6 hours to obtain a cordierite with a complete coating; e. Repeated V2O5 coating Repeat step d 4 to 6 times to repeat the V2O5 coating.
2. A denitration catalyst coating method according to claim 1, characterized in that: In step b, the pretreatment agent is a citric acid aqueous solution with a mass fraction of 5%.
3. A denitration catalyst coating method according to claim 1, characterized in that: In step d, the ratio of V2O5 to distilled water is 1:10 by mass.
4. A denitration catalyst coating method according to claim 1, characterized in that: In step a, the cordierite standard block has a cross-section of 150 mm×150 mm and a length of 300 mm.
5. A denitration catalyst coating method according to claim 1, characterized in that: In step c, the static aging is carried out in a 60° C. water bath.
6. A denitration catalyst coating method according to claim 1, characterized in that: In step c, the TiO2 organic precursor solution is tetrabutyl titanate, the organic chelating agent is sodium dithioformate, the alcohol is ethanol or ethylene glycol solvent, and the dispersant is sodium pyrophosphate.