Flexible clamping structure and manufacturing method thereof
By using a combination of an electric heating layer, an active layer and a flexible adsorption layer in the clamp, flexible clamping of electronic components is achieved, solving the problems of cumbersome and large loading force of the pneumatic clamp, providing a simple and applicable clamping solution.
Patent Information
- Application Number
- CN202411111009.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-13
- Publication Date
- 2024-11-12
AI Technical Summary
The existing pneumatic clamps have cumbersome processes and are pre-loaded with large pre-loading forces, making them difficult to adapt to their transfer and transportation.
Using a flexible clamping structure including an electric heating layer, an active layer and a flexible adsorption layer, the electric heating layer is energized to generate heat to cause reversible shape changes in the active layer and a flexible adsorption layer, realizing state switching of picking and loosening objects, and realizing loading force through controlling voltage. Small and flexible.
It simplifies the clamping process and reduces the risk of damage to electronic components. It is suitable for the transfer and transportation of precision, fragile and deformable objects.
Smart Images

Figure CN118927281A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of clamps, and in particular to a flexible clamping structure and a manufacturing method thereof. Background Art
[0002] With the rapid development of industrial robots, the requirements for their end grippers are increasing day by day. Especially when it is necessary to clamp delicate, fragile and deformable electronic components, the end grippers are required to be highly flexible to reduce damage to the electronic components.
[0003] Pneumatic grippers are usually used to clamp electronic components. Pneumatic grippers require a pneumatic control module and an external air pump to control the pneumatic grippers, as well as a van der Waals suction cup that is preloaded in order to adsorb the object. The clamping process is very cumbersome, and the preload force is large, making it difficult to apply to the transfer and transportation of electronic components.
[0004] It should be noted that the information disclosed in the above background technology section is only used to enhance the understanding of the background of the present invention, and therefore may include information that does not constitute prior art known to ordinary technicians in the field. Summary of the invention
[0005] The purpose of the present invention is to overcome the problem that the clamping process of a pneumatic clamper is complicated and the pre-load force is large, which makes it difficult to apply it to the transfer and transportation of electronic components, and to provide a flexible clamping structure and a manufacturing method thereof.
[0006] According to one aspect of the present invention, a flexible clamping structure is provided, which includes an electric heating layer, an active layer and a flexible adsorption layer. The electric heating layer can generate heat when energized; the active layer is arranged on one side of the electric heating layer, the active layer includes a liquid crystal elastomer film, and the active layer will undergo a reversible shape change under the thermal action of the electric heating layer; the flexible adsorption layer is arranged on the side of the active layer away from the electric heating layer.
[0007] In one embodiment of the present invention, the electric heating layer includes an electric heating flexible film and a conductive layer, and the conductive layer is arranged on a side of the flexible film close to the active layer.
[0008] In one embodiment of the present invention, the flexible adsorption layer comprises an adsorption flexible film, and a surface of the adsorption flexible film away from the active layer has a plurality of adsorption protrusions.
[0009] In one embodiment of the present invention, the adsorption protrusion is a columnar structure, and the adsorption protrusion includes a first columnar segment and a second columnar segment. The first columnar segment is connected to the adsorption flexible film, and the second columnar segment is connected to one end of the first columnar segment away from the adsorption flexible film. The maximum width of the cross section of the second columnar segment is greater than the maximum width of the cross section of the first columnar segment.
[0010] In one embodiment of the present invention, a plurality of nano-micro-pillars are disposed at one end of the second columnar segment away from the first columnar segment.
[0011] In one embodiment of the present invention, a plurality of rigid particles are disposed in the first columnar segment, and the number of the rigid particles gradually increases in a direction away from the adsorption flexible film.
[0012] In one embodiment of the present invention, at least some of the adsorption protrusions have different heights.
[0013] According to another aspect of the present invention, a method for manufacturing a flexible clamping structure is provided, the method comprising: forming an electric heating layer, which can generate heat when energized; forming an active layer on one side of the electric heating layer, the active layer being a liquid crystal elastomer film, the active layer undergoing a reversible shape change under the heat of the electric heating layer; forming a flexible adsorption layer on a side of the active layer away from the electric heating layer; and bonding the electric heating layer, the active layer and the flexible adsorption layer together by an adhesive.
[0014] In one embodiment of the present invention, forming a flexible adsorption layer includes: forming a first template, the first template having a plurality of first grooves matching the shape of the adsorption protrusions; pouring a precursor solution of the flexible adsorption layer into the first template; after the precursor solution of the flexible adsorption layer is solidified, removing the first template to form an adsorption flexible film and a plurality of adsorption protrusions on a side of the adsorption flexible film away from the active layer.
[0015] In one embodiment of the present invention, forming a flexible adsorption layer includes: forming a second template, the second template having a plurality of second grooves matching the shape of the first columnar segment; pouring a precursor solution of the flexible adsorption layer into the second template, removing the second template after the precursor solution of the flexible adsorption layer is solidified, forming an adsorbed flexible film and a plurality of first columnar segments on a side of the adsorbed flexible film away from the active layer; immersing the plurality of first columnar segments in a partially cross-linked precursor solution of the flexible adsorption layer; contacting the end of the first columnar segment with the partially cross-linked precursor solution of the flexible adsorption layer and a support sheet, removing the support sheet after the precursor solution of the partially cross-linked flexible adsorption layer is solidified, and forming a second columnar segment at the end of the first columnar segment away from the first columnar segment.
[0016] The flexible clamping structure of the present invention includes an electric heating layer, an active layer and a flexible adsorption layer. The active layer undergoes a reversible shape change under the thermal effect of the electric heating layer, and the flexible adsorption layer undergoes synchronous deformation driven by the active layer. When voltage is applied, the electric heating layer generates heat, and the temperature around it rises, triggering the liquid crystal elastomer film to undergo a phase transition, causing the active layer to produce a macroscopic contraction, driving the flexible adsorption layer to undergo bending deformation, and thus contacting the object to be picked up. When the voltage is removed, the electric heating layer begins to cool, and the temperature around it decreases, triggering the liquid crystal molecules in the liquid crystal elastomer film to restore their orientation, causing the active layer to produce a macroscopic expansion, driving the flexible adsorption layer to return to its original state, and thus releasing the picked up object. By controlling the power on or off of the electric heating layer, the state switching of the flexible clamping structure to pick up and release can be achieved, which is relatively simple, and the loading force generated by the electric drive is small, which can be well applied to the transfer and transportation of electronic components.
[0017] It is to be understood that both the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The accompanying drawings herein are incorporated into and constitute a part of the specification, illustrate embodiments consistent with the present invention, and together with the specification are used to explain the principles of the present invention. Obviously, the accompanying drawings described below are only some embodiments of the present invention, and for those of ordinary skill in the art, other accompanying drawings can be obtained based on these accompanying drawings without creative work.
[0019] Figure 1 It is a cross-sectional schematic diagram of a flexible clamping structure involved in an embodiment of the present invention.
[0020] Figure 2 It is a schematic plan view of the liquid crystal molecules in the liquid crystal elastomer film according to an embodiment of the present invention arranged along one direction.
[0021] Figure 3 It is a plan view schematically showing the random arrangement of liquid crystal molecules according to an embodiment of the present invention.
[0022] Figure 4 It is a schematic diagram of the three-dimensional structure of the flexible adsorption layer involved in an embodiment of the present invention.
[0023] Figure 5 It is a front view of the flexible adsorption layer involved in an embodiment of the present invention.
[0024] Figure 6 It is a side view of the flexible adsorption layer involved in an embodiment of the present invention.
[0025] Figure 7 It is a top view of the flexible adsorption layer involved in an embodiment of the present invention.
[0026] Figure 8 It is a cross-sectional schematic diagram of the flexible adsorption layer involved in an embodiment of the present invention when a plurality of nano-micro-pillars are arranged at one end of the second columnar segment away from the first columnar segment.
[0027] Fig. 9 It is a cross-sectional schematic diagram of the flexible adsorption layer involved in an embodiment of the present invention when a plurality of nano-micro-pillars are arranged at one end of the second columnar segment away from the first columnar segment, and a plurality of rigid particles are arranged in the first columnar segment.
[0028] Fig.10 It is a schematic diagram of the three-dimensional structure of the flexible clamping structure involved in the embodiment of the present invention when picking up an object.
[0029] Fig.11 It is a schematic diagram of the three-dimensional structure of the flexible clamping structure involved in the embodiment of the present invention when releasing an object.
[0030] Fig.12 It is a schematic diagram of the structure after spin coating a photoresist coating on a glass substrate according to an embodiment of the present invention.
[0031] Fig.13 It is a structural schematic diagram of an embodiment of the present invention when a mask plate with a circular hole pattern is used to expose a side of a photoresist coating away from a glass substrate.
[0032] Fig.14 It is a structural schematic diagram of an embodiment of the present invention when performing maskless exposure on a side of a photoresist coating layer close to a glass substrate.
[0033] Fig.15 It is a schematic structural diagram of developing an exposure pattern according to an embodiment of the present invention.
[0034] Fig.16 It is a schematic structural diagram of pouring the precursor solution of the flexible adsorption layer into the first template according to an embodiment of the present invention.
[0035] Fig.17 It is a schematic structural diagram of an embodiment of the present invention when the first template is removed to form an adsorption flexible film and a plurality of adsorption protrusions on a side of the adsorption flexible film away from the active layer.
[0036] Fig.18 It is a schematic structural diagram of an embodiment of the present invention when a flexible material for forming a first template is cast on a male mold.
[0037] Fig.19 A schematic structural diagram of an embodiment of the present invention in which the convex mold is removed to form a first template having a plurality of first grooves matching the shape of the adsorption protrusions.
[0038] Fig. 20This is a structural schematic diagram of pouring a precursor solution of a flexible adsorption layer into a first template according to an embodiment of the present invention, and the precursor solution of the flexible adsorption layer fills the first grooves and covers the portion between two adjacent first grooves.
[0039] Fig.21 It is a schematic structural diagram of separating the flexible adsorption layer from the first template according to an embodiment of the present invention.
[0040] Fig. 22 A schematic structural diagram of an embodiment of the present invention when forming a second template having a plurality of second grooves matching the shape of the first columnar segment.
[0041] Fig.23 It is a schematic structural diagram of pouring a precursor solution of a flexible adsorption layer containing rigid particles into a second template according to an embodiment of the present invention.
[0042] Fig.24 This is a schematic diagram of the structure when obtaining a rigid particle distribution gradient according to an embodiment of the present invention.
[0043] Fig.25 This is a schematic diagram of the structure of the precursor solution of the flexible adsorption layer containing rigid particles after solidification according to an embodiment of the present invention.
[0044] Fig.26 This is a schematic structural diagram of an embodiment of the present invention when the precursor solution of the partially cross-linked flexible adsorption layer applied to the end of the first columnar segment is in contact with the support sheet.
[0045] Fig. 27 This is a schematic structural diagram of the embodiment of the present invention in which the precursor solution of the partially cross-linked flexible adsorption layer is cured and the support sheet is removed to form a second columnar segment at the end of the first columnar segment away from the adsorption flexible film.
[0046] In the figure: 1-electric heating layer, 2-active layer, 21-liquid crystal molecules, 3-flexible adsorption layer, 31-adsorbed flexible film, 32-adsorbed protrusions, 321-first columnar segment, 322-second columnar segment, 323-nano-micro-columns, 324-rigid particles, 4-first template, 41-first groove, 411-first groove segment, 412-second groove segment, 42-glass substrate, 43-photoresist coating, 431-exposure pattern, 4311-first exposure part, 4312-second exposure part, 5-second template, 51-second groove, 6-support sheet, 7-partially cross-linked precursor solution, 8-mask plate, 9-convex mold, 100-object to be picked up. DETAILED DESCRIPTION
[0047] Example embodiments will now be described more fully with reference to the accompanying drawings. However, the example embodiments can be implemented in a variety of forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided so that the present invention will be comprehensive and complete and fully convey the concepts of the example embodiments to those skilled in the art. The same reference numerals in the figures represent the same or similar structures, and thus their detailed description will be omitted. In addition, the drawings are only schematic illustrations of the present invention and are not necessarily drawn to scale.
[0048] Although relative terms such as "upper" and "lower" are used in this specification to describe the relative relationship of one component of the diagram to another component, these terms are used in this specification only for convenience, such as according to the direction of the examples in the drawings. It is understood that if the device of the diagram is turned upside down, the component described as "upper" will become the component "lower". When a structure is "on" other structures, it may mean that the structure is formed integrally on the other structure, or that the structure is "directly" disposed on the other structure, or that the structure is "indirectly" disposed on the other structure through another structure.
[0049] The terms "a", "an", "the", "said" and "at least one" are used to indicate the presence of one or more elements / components / etc.; the terms "including" and "having" are used to express an open-ended inclusive meaning and mean that additional elements / components / etc. may exist in addition to the listed elements / components / etc.; the terms "first", "second" and "third" etc. are used merely as labels and are not intended to limit the quantity of their objects.
[0050] With the rapid development of industrial robots, the requirements for their end grippers are increasing. In particular, when it is necessary to clamp delicate, fragile and deformable objects, such as electronic components, the end grippers are required to be highly flexible to reduce damage to the electronic components during movement. At present, soft robots used to pick objects usually use pneumatic grippers and van der Waals suction cups to pick up and adsorb objects. Pneumatic grippers usually require pneumatic control modules and external air pumps to control the pneumatic grippers, which is very cumbersome and greatly reduces portability. The van der Waals suction cup uses the polymer surface microstructure design to enable the suction cup to generate a strong intermolecular force with the surface of the object, but it needs to be pre-loaded to allow the van der Waals suction cup to adsorb the object. The load loaded on the van der Waals suction cup is usually 2-20N, which makes it difficult to apply to the transfer and transportation of electronic components.
[0051] Based on this, an embodiment of the present invention provides a flexible clamping structure. Figures 3 to 6As shown, the flexible clamping structure includes an electric heating layer 1, an active layer 2 and a flexible adsorption layer 3, the electric heating layer 1 is a flexible electric heating film; the active layer 2 is arranged on one side of the electric heating layer 1, the active layer 2 is a liquid crystal elastomer film, and the active layer 2 will undergo a reversible shape change under the heat of the electric heating layer 1; the flexible adsorption layer 3 is arranged on the side of the active layer 2 away from the electric heating layer 1, the flexible adsorption layer 3 includes an adsorption flexible film 31, and the side of the adsorption flexible film 31 away from the active layer 2 has a plurality of adsorption protrusions 32.
[0052] The flexible clamping structure includes an electric heating layer 1, an active layer 2 and a flexible adsorption layer 3. The active layer 2 undergoes a reversible shape change under the thermal effect of the electric heating layer 1, and the flexible adsorption layer 3 undergoes synchronous deformation driven by the active layer 2. When voltage is applied, the electric heating layer 1 generates heat, and the temperature around it rises, triggering the liquid crystal elastomer film to undergo a phase transition, causing the active layer 2 to produce a macroscopic contraction, driving the flexible adsorption layer 3 to bend and deform, thereby contacting the object to be picked up. When the voltage is removed, the electric heating layer 1 begins to cool, and the temperature around it decreases, triggering the liquid crystal molecules 21 in the liquid crystal elastomer film to restore their orientation, causing the active layer 2 to produce a macroscopic expansion, driving the flexible adsorption layer 3 to return to its original state, thereby releasing the picked up object. By controlling the power on or off of the electric heating layer 1, the state switching of the flexible clamping structure to pick up and release can be achieved, which is relatively simple, and the loading force generated by the electric drive is small, which can be well applied to the transfer and transportation of electronic components.
[0053] The flexible clamping structure involved in the implementation mode of the present invention is described in detail below with reference to specific embodiments.
[0054] like Figure 1 As shown, the flexible clamping structure includes an electric heating layer 1, an active layer 2 and a flexible adsorption layer 3. The active layer 2 is arranged on one side of the electric heating layer 1, and the flexible adsorption layer 3 is arranged on the side of the active layer 2 away from the electric heating layer 1.
[0055] The electric heating layer 1 includes an electric heating flexible film and a conductive layer, the conductive layer is arranged on the side of the flexible film close to the active layer 2, the material of the electric heating flexible film can be at least one of polydimethylsiloxane (PDMS), polyurethane (PU), butadiene-styrene block copolymer (SEBS), platinum cured silicone (Ecoflex), and the material of the conductive layer can be at least one of graphene, carbon nanotubes, silver nanoparticles, silver nanowires, two-dimensional transition metal carbon (nitride) (MXene), poly (3,4-ethylenedioxythiophene): polystyrene sulfonate (PEDOT:PSS). The electric heating layer 1 can also only include a conductive layer, and the conductive layer is directly arranged on the side of the active layer 2 away from the flexible adsorption layer 3.
[0056] The active layer 2 includes a liquid crystal elastomer film, which undergoes a reversible shape change under the action of heat. The deformation principle of the liquid crystal elastomer film is as follows: Figure 2 As shown, at room temperature, the liquid crystal molecules 21 inside the liquid crystal elastomer film are arranged in one direction; Figure 3 As shown, when the temperature exceeds the liquid crystal phase transition temperature, the oriented liquid crystal molecules 21 begin to arrange randomly, causing the liquid crystal elastomer film to shrink along the arrangement direction of the liquid crystal molecules 21; when the temperature drops, the randomly oriented liquid crystal molecules 21 return to the initial orientation state, causing the liquid crystal elastomer film to stretch along the arrangement direction of the liquid crystal molecules 21.
[0057] like Figures 4 to 7 As shown, the flexible adsorption layer 3 includes an adsorption flexible film 31, and a side of the adsorption flexible film 31 away from the active layer 2 has a plurality of adsorption protrusions 32. The material of the flexible adsorption layer 3 can be at least one of polydimethylsiloxane (PDMS), polyurethane (PU), butadiene-styrene block copolymer (SEBS), and platinum cured silicone (Ecoflex).
[0058] The adsorption protrusion 32 is a step columnar structure, and the adsorption protrusion 32 includes a first columnar section 321 and a second columnar section 322. The first columnar section 321 is connected to the adsorption flexible film 31, and the second columnar section 322 is connected to the end of the first columnar section 321 away from the adsorption flexible film 31. The maximum width of the cross section of the second columnar section 322 is greater than the maximum width of the cross section of the first columnar section 321. Compared with hemispherical structures, straight columns and other structures, the step columnar structure has a larger contact area and can generate greater adhesion. It is also possible to set the width of the second columnar section 322 close to the end of the first columnar section 321 to be equal to the width of the first columnar section 321, and the width of the second columnar section 322 gradually increases in the direction away from the first columnar section 321.
[0059] The shape of the first columnar segment 321 and the second columnar segment 322 can be a cylinder or a prism, which is not specifically limited here. When the shape of the first columnar segment 321 and the second columnar segment 322 is a cylinder, the diameter of the cross section of the second columnar segment 322 is greater than the diameter of the cross section of the first columnar segment 321. In addition, the shape of the first columnar segment 321 and the shape of the second columnar segment 322 can be the same or different. For example, when the shape of the first columnar segment is a cylinder, the shape of the second columnar segment can be set to a prism.
[0060] In order to ensure the adsorption effect of the flexible adsorption layer 3, at least some of the adsorption protrusions 32 may be set to have different heights according to the shapes of the object 100 to be picked up. For example, when the edge of the object 100 to be picked up is protruding relative to other parts, the height of the adsorption protrusions 32 at the edge of the flexible adsorption layer 3 may be set lower than the height of the adsorption protrusions 32 at other parts. When the object 100 to be picked up is spherical, the height of the adsorption protrusions 32 may be set to gradually decrease from the edge to the center of the flexible adsorption layer 3.
[0061] The height of the adsorption protrusion 32 is 10-100 microns, the diameter of the adsorption protrusion 32 is 5-50 microns, and the spacing between the centers of two adjacent adsorption protrusions 32 is 20-70 microns. In this embodiment, the height of the adsorption protrusion 32 can be 10 microns, 30 microns, 50 microns, 80 microns or 100 microns, the diameter of the adsorption protrusion 32 can be 5 microns, 15 microns, 25 microns, 35 microns or 50 microns, and the spacing between the centers of two adjacent adsorption protrusions 32 is 20 microns, 30 microns, 40 microns, 60 microns or 70 microns.
[0062] like Figure 8 As shown, in order to further enhance the adhesion effect of the adsorption protrusion 32, a plurality of nano-micro-pillars 323 can be arranged at one end of the second columnar segment 322 away from the first columnar segment 321, and two adjacent nano-micro-pillars 323 are arranged at intervals. The height of the nano-micro-pillars 323 can be 0.5-1 microns, and the diameter of the nano-micro-pillars 323 can be 1-2 microns. The height of the nano-micro-pillars 323 can be 0.5 microns, 0.6 microns, 0.8 microns, 0.9 microns or 1 micron, and the diameter of the nano-micro-pillars 323 can be 1-2 microns, and the diameter of the nano-micro-pillars 323 can be 1 micron, 1.2 microns, 1.4 microns, 1.6 microns or 2 microns.
[0063] like Fig. 9 As shown, the adsorption protrusion 32 generally deforms the second columnar segment 322 to adsorb the object 100 to be picked up, and the first columnar segment 321 maintains a certain strength to avoid mutual interference between the adsorption protrusions 32. In order to prevent the first columnar segment 321 from deforming, a plurality of rigid particles 324 can be arranged in the first columnar segment 321, and the rigid particles 324 can enhance the strength of the first columnar segment 321. In this embodiment, the rigid particles 324 can be nanoparticles, and the material of the rigid particles 324 can be calcium carbonate, silicon dioxide, iron or ferroferric oxide.
[0064] The number of rigid particles 324 can be set to gradually increase in the direction away from the adsorption flexible film 31, forming a modulus gradient along the length direction of the first columnar segment 321. Compared with the adsorption protrusion 32 with uniform modulus, the adsorption protrusion 32 with a modulus gradient can reduce the stress around the side of the second columnar segment 322 away from the adsorption flexible film 31 when it contacts the object 100 to be picked up, and increase the stress in the center when the side of the second columnar segment 322 away from the adsorption flexible film 31 contacts the object 100 to be picked up, which is conducive to forming a stable contact between the adsorption protrusion 32 and the object 100 to be picked up.
[0065] The flexible clamping structure is usually used on a clamp. After the flexible clamping structure is powered on, the electric heating layer 1 can provide heat to the liquid crystal elastomer active layer 2 through the Joule heat generated by the low voltage, thereby driving the liquid crystal elastomer film of the active layer 2 to shrink along the arrangement direction of the liquid crystal molecules 21. The flexible adsorption layer 3 can spontaneously adhere to the surface of the object 100 to be picked up according to the state on the active layer 2, thereby picking up the object. The feature of the flexible clamping structure is that it is electrically driven and does not require additional external force for loading. In this embodiment, the voltage of the electrical drive can be less than or equal to 10V.
[0066] like Fig.10 and Fig.11 As shown, the working process of the flexible clamping structure is as follows: Fig.10 As shown, when voltage is applied, the temperature around the electric heating layer 1 rises, triggering the phase transition of the liquid crystal elastomer film, causing the active layer 2 to shrink macroscopically, driving the flexible adsorption layer 3 to bend and deform, thereby contacting the object to be picked up. Fig.11 As shown, when the voltage is removed, the temperature around the electric heating layer 1 decreases, triggering the liquid crystal molecules 21 in the liquid crystal elastomer film to restore their orientation, causing the active layer 2 to expand macroscopically, driving the flexible adsorption layer 3 to return to its original state, thereby releasing the picked-up object. By controlling the power on or off of the electric heating layer 1, the state switching of the flexible clamping structure to pick up and release can be achieved.
[0067] The embodiment of the present invention provides a method for manufacturing a flexible clamping structure. Figures 12 to 27 As shown, the method may include:
[0068] Step S10, forming an electric heating layer 1, which can generate heat when powered on.
[0069] Step S20 , forming an active layer 2 on one side of the electric heating layer 1 , wherein the active layer 2 is a liquid crystal elastomer film, and the active layer 2 undergoes a reversible shape change under the heat of the electric heating layer 1 .
[0070] Step S30 , forming a flexible adsorption layer 3 on a side of the active layer 2 away from the electric heating layer 1 .
[0071] Step S40, bonding the electric heating layer 1, the active layer 2 and the flexible adsorption layer 3 together by an adhesive.
[0072] The method for manufacturing the flexible clamping structure according to the embodiment of the present invention will be described in detail below with reference to specific examples.
[0073] The step S10 of forming the electric heating layer 1 may include:
[0074] The electrothermal flexible film is prepared by spin coating one of the precursor solutions of polydimethylsiloxane, polyurethane, butadiene-styrene block copolymer, and platinum-cured silicone. Subsequently, a conductive material selected from graphene, carbon nanotubes, silver nanoparticles, silver nanowires, two-dimensional transition metal carbon (nitride), and poly (3,4-ethylenedioxythiophene): polystyrene sulfonate is loaded on the surface of the electrothermal flexible film through film-forming processes such as scraping, spraying, spin coating, screen printing, and 3D printing, thereby forming a conductive layer on the surface of the electrothermal flexible film.
[0075] In step S20, forming the active layer 2 on one side of the electric heating layer 1 may include: using a liquid crystal cell to prepare a liquid crystal elastomer film having liquid crystal molecules 21 arranged in one direction. The direction may be any direction as long as the arrangement direction of all liquid crystal molecules 21 is the same. In this embodiment, the arrangement direction of the liquid crystal molecules 21 may be a horizontal direction.
[0076] like Figures 12 to 17 As shown, forming the flexible adsorption layer 3 in step S30 may include:
[0077] Step S301, forming a first template 4, wherein the first template 4 has a plurality of first grooves 41 matching the shape of the adsorption protrusions 32. Step S301 may specifically include:
[0078] like Fig.12 As shown, a photoresist coating 43 is spin-coated on a glass substrate 42, and the rotation speed during the spin coating can be 1000-2000 rpm. The thickness of the photoresist coating 43 can be controlled by multiple spin coatings. The photoresist coating 43 can be a positive photoresist.
[0079] like Fig.13 As shown, a mask plate 8 with a circular hole pattern is used to perform a first exposure on a side of the photoresist coating 43 away from the glass substrate 42 to form a first exposure portion 4311. The diameter of each circular hole in the first exposure portion 4311 can be 5-50 microns, and the distance between the centers of two adjacent circular holes can be 20-70 microns. The exposure time is controlled according to the thickness of the photoresist coating 43. For example, when the thickness of the photoresist coating 43 is 30 microns, the exposure time can be 70-100s, and when the thickness of the photoresist coating 43 is 15 microns, the exposure time can be 30-50s.
[0080] like Fig.14 As shown, the side of the photoresist coating 43 close to the glass substrate 42 is exposed without a mask plate 8 for 2-5 seconds, and the side of the photoresist coating 43 close to the glass substrate 42 is exposed to form a second exposure part 4312. The second exposure part 4312 is connected to the first exposure part 4311 to form an exposure pattern 431.
[0081] like Fig.15 As shown, the exposure pattern 431 is developed, and the development time is controlled under the influence of the diffusion speed of the developer to etch away the first exposure portion 4311 and part of the second exposure portion 4312. A plurality of first grooves 41 matching the shape of the adsorption protrusions 32 can be formed on the photoresist coating 43, and the remaining portion of the photoresist coating 43 and the glass substrate 42 constitute a first template 4.
[0082] The first groove 41 includes a first groove section 411 and a second groove section 412 which are connected to each other. The first groove section 411 matches the shape and size of the first columnar section 321. The first groove section 411 is far away from the glass substrate 42. The second groove section 412 matches the shape and size of the second columnar section 322. The second groove section 412 is close to the glass substrate 42. The width of the second groove section 412 at one end close to the first groove section 411 is equal to the width of the first groove section 411. The width of the second groove section 412 gradually increases in a direction away from the first groove section 411.
[0083] Step S302, pouring the precursor solution of the flexible adsorption layer 3 into the first template 4, step S302 may specifically include: pouring one of the precursor solutions of polydimethylsiloxane, polyurethane, butadiene-styrene block copolymer, and platinum-cured silicone into the first template 4, and vacuuming to ensure that the precursor solution of the flexible adsorption layer 3 completely fills the first template 4, such as Fig.16 shown.
[0084] Step S303, as Fig.17 As shown, after the precursor solution of the flexible adsorption layer 3 is solidified, the first template 4 is removed to form an adsorption flexible film 31 and a plurality of adsorption protrusions 32 on a side of the adsorption flexible film 31 away from the active layer 2. Because the first template 4 is mainly the remaining part of the photoresist coating 43, the first template 4 can be ultrasonically removed using a solvent such as ethanol or acetone. The width of the second columnar segment 322 formed by this method at one end close to the first columnar segment 321 is equal to the width of the first columnar segment 321, and the width of the second columnar segment 322 gradually increases in a direction away from the first columnar segment 321.
[0085] like Figures 18 to 21 As shown, forming the flexible adsorption layer 3 in step S30 may include:
[0086] The convex mold 9 with the same shape and size as the adsorption protrusion 32 is prepared by 3D printing technology. In order to facilitate subsequent demoulding, a demoulding agent is sprayed on the coated surface, and a flexible material such as polyvinyl chloride gel and silicone rubber is poured on the convex mold 9. After curing, the convex mold 9 is removed to form a first template 4 with multiple first grooves 41 matching the shape of the adsorption protrusion 32, such as Fig.18 and Fig.19 As shown. A precursor solution of polydimethylsiloxane, polyurethane, butadiene-styrene block copolymer, or platinum-cured silica gel is poured into the first template 4, and the precursor solution of the flexible adsorption layer 3 fills the first groove 41 and covers the portion between two adjacent first grooves 41. After the precursor solution of the flexible adsorption layer 3 is cured, the first template 4 is removed, and the flexible adsorption layer 3 is separated from the first template 4, as shown. Fig. 20 and Fig.21 shown.
[0087] like Figure 22 to Figure 27 As shown, forming the flexible adsorption layer 3 in step S30 may include:
[0088] Step S3001, forming a second template 5, wherein the second template 5 has a plurality of second grooves 51 matching the shape of the first columnar segment 321. Step S3001 may specifically include:
[0089] like Fig. 22 As shown, a convex mold 9 having the same shape and size as the first columnar segment 321 is prepared, and epoxy resin, paraffin wax, polyurethane or silicone rubber is poured into it to form a second template 5 having a plurality of second grooves 51 matching the shape of the first columnar segment 321. It should be noted that the convex mold 9 can be made of negative photoresist.
[0090] Step S3002, pouring the precursor solution of the flexible adsorption layer 3 into the second template 5, removing the second template 5 after the precursor solution of the flexible adsorption layer 3 is solidified, and forming the adsorption flexible film 31 and a plurality of first columnar segments 321 on the side of the adsorption flexible film 31 away from the active layer 2. Step S3002 may specifically include:
[0091] like Figure 23 to Figure 25 As shown, the rigid particles 324 are mixed into the precursor solution of the flexible adsorption layer 3, and the precursor solution of the flexible adsorption layer 3 containing the rigid particles 324 is poured into the second template 5, and the distribution gradient of the rigid particles 324 is obtained by centrifugation, natural sedimentation or magnetic attraction. The precursor solution of the flexible adsorption layer 3 is one of the precursor solutions of polydimethylsiloxane, polyurethane, butadiene-styrene block copolymer, and platinum-cured silicone.
[0092] After the precursor solution of the flexible adsorption layer 3 containing the rigid particles 324 is solidified, the second template 5 is removed to form an adsorption flexible film 31 and a plurality of first columnar segments 321 on a side of the adsorption flexible film 31 away from the active layer 2 , wherein the first columnar segments 321 contain rigid particles 324 .
[0093] Step S3003, immersing the plurality of first columnar segments 321 into a precursor solution of the partially cross-linked flexible adsorption layer 3. Step S3003 may specifically include:
[0094] like Fig.26 As shown, one of the precursor solutions of partially cross-linked polydimethylsiloxane, polyurethane, butadiene-styrene block copolymer, and platinum-cured silica gel is prepared, and the end of the first columnar segment 321 having rigid particles 324 away from the adsorption flexible film 31 is immersed in the precursor solution of the partially cross-linked flexible adsorption layer 3, and the first columnar segment 321 is taken out after the end portion is covered with the partially cross-linked precursor solution 7 of the flexible adsorption layer 3.
[0095] Step S3004, as Fig. 27 As shown, the precursor solution of the partially cross-linked flexible adsorption layer 3 stained at the end of the first columnar segment 321 is brought into contact with the support sheet 6, and the support sheet 6 is removed after the precursor solution of the partially cross-linked flexible adsorption layer 3 is solidified, and the second columnar segment 322 is formed at the end of the first columnar segment 321 away from the adsorption flexible film 31. The width of the second columnar segment 322 formed by this method at the end close to the first columnar segment 321 is equal to the width of the first columnar segment 321, and the width of the second columnar segment 322 gradually increases in the direction away from the first columnar segment 321. It should be noted that the support sheet 6 can be a fluorinated silicon sheet.
[0096] Nano grooves can also be set on the surface of the support sheet 6. When the precursor solution of the partially cross-linked flexible adsorption layer 3 applied to the end of the first columnar segment 321 is brought into contact with the nano grooves on the surface of the support sheet 6 in step S3004, after the precursor solution of the partially cross-linked flexible adsorption layer 3 is cured, a nano groove can be formed at the end of the second columnar segment 322 away from the first columnar segment 321. Figure 8 A plurality of nano-pillars 323 are shown.
[0097] Those skilled in the art will readily appreciate other embodiments of the present invention after considering the specification and practicing the disclosure of the invention herein. This application is intended to cover any variations, uses or adaptations of the present invention, which follow the general principles of the present invention and include common knowledge or customary techniques in the art that are not disclosed by the present invention. The specification and examples are intended to be exemplary only, and the true scope and spirit of the present invention are indicated by the appended claims.
Claims
1. A flexible clamping structure, characterized in that: include: The electric heating layer can generate heat when electricity is applied; An active layer, disposed on one side of the electric heating layer, the active layer comprising a liquid crystal elastomer film, and the active layer undergoes a reversible shape change under the heat of the electric heating layer; The flexible adsorption layer is arranged on a side of the active layer away from the electric heating layer.
2. The flexible clamping structure according to claim 1, characterized in that: The electric heating layer includes an electric heating flexible film and a conductive layer, and the conductive layer is arranged on a side of the flexible film close to the active layer.
3. The flexible clamping structure according to claim 1, characterized in that: The flexible adsorption layer comprises an adsorption flexible film, and a side of the adsorption flexible film away from the active layer has a plurality of adsorption protrusions.
4. The flexible clamping structure according to claim 3, characterized in that: The adsorption protrusion is a columnar structure, and the adsorption protrusion includes a first columnar segment and a second columnar segment, the first columnar segment is connected to the adsorption flexible film, the second columnar segment is connected to an end of the first columnar segment away from the adsorption flexible film, and the maximum width of the cross section of the second columnar segment is greater than the maximum width of the cross section of the first columnar segment.
5. The flexible clamping structure according to claim 4, characterized in that: A plurality of nano-micro-pillars are disposed at one end of the second columnar segment away from the first columnar segment.
6. The flexible clamping structure according to claim 4, characterized in that: A plurality of rigid particles are arranged in the first columnar segment, and the number of the rigid particles gradually increases in a direction away from the adsorption flexible film.
7. The flexible clamping structure according to claim 3, characterized in that: At least some of the adsorption protrusions have different heights.
8. A method for manufacturing a flexible clamping structure, characterized in that: The method comprises: forming an electric heating layer capable of generating heat when electricity is supplied to the electric heating layer; An active layer is formed on one side of the electric heating layer, wherein the active layer is a liquid crystal elastomer film, and the active layer undergoes a reversible shape change under the heat of the electric heating layer; forming a flexible adsorption layer on a side of the active layer away from the electric heating layer; The electric heating layer, the active layer and the flexible adsorption layer are bonded together by an adhesive.
9. The method for manufacturing a flexible clamping structure according to claim 8, characterized in that: The flexible clamping structure is the flexible clamping structure according to claim 3, and forming the flexible adsorption layer comprises: forming a first template, wherein the first template has a plurality of first grooves matching the shape of the adsorption protrusions; pouring the precursor solution of the flexible adsorption layer into the first template; After the precursor solution of the flexible adsorption layer is solidified, the first template is removed to form the adsorption flexible film and a plurality of adsorption protrusions on a side of the adsorption flexible film away from the active layer.
10. The method for manufacturing a flexible clamping structure according to claim 8, characterized in that: The flexible clamping structure is the flexible clamping structure according to claim 4, and forming the flexible adsorption layer comprises: forming a second template having a plurality of second grooves matching the shape of the first columnar segment; Pour the precursor solution of the flexible adsorption layer into the second template, and remove the second template after the precursor solution of the flexible adsorption layer is solidified, so as to form the adsorption flexible film and a plurality of the first columnar segments on a side of the adsorption flexible film away from the active layer; immersing the plurality of the first columnar segments into a partially cross-linked precursor solution of the flexible adsorbent layer; The precursor solution of the partially cross-linked flexible adsorption layer applied to the end of the first columnar segment is brought into contact with a support sheet, and the support sheet is removed after the partially cross-linked precursor solution of the flexible adsorption layer is solidified, so as to form a second columnar segment at the end of the first columnar segment away from the first columnar segment.
Citation Information
Patent Citations
Flexible adsorption device and making method thereof
CN108784670A
Multilayer microstructure bionic dry adhesion structure, mold and preparation method of multilayer microstructure bionic dry adhesion structure
CN116750712A
Folding electronic device
CN117041396A
Flexible device based on porous structure and capable of being attached to complex surface and manufacturing method of flexible device
CN118368818A
Claw manipulator based on shape memory alloy
CN220972410U
Cited By
Electric heating type liquid crystal elastomer artificial muscle and preparation method thereof
CN119610824A