Diode cutting method for glass passivation
By selecting the cutting blade and speed for the product parameters of glass passivation diodes, and combining pure water and carbon dioxide technology for reference cross-approval cutting, the problems of fragility and electrostatic adsorption during the cutting process of glass passivation diodes are solved, achieving high Stability and low cost cutting effect.
Patent Information
- Application Number
- CN202410988941.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-12
AI Technical Summary
In the prior art, glass passivation diode chips are prone to fragility, electrostatic adsorption and cracks during the cutting process, resulting in product function failure, and the process is complicated and costly.
Use the selection of appropriate cutting blades and cutting speeds based on the product parameters of glass passivation diodes, combined with pure water cleaning and carbon dioxide foaming technology, and accurately cut through the reference cross approval method to ensure the matching of the remaining blade and the cutting speed. Use a microscope to test Cutting effect.
It improves the stability of diode chip scribe, reduces the risk of cracks and shedding, realizes a high-stability and low-cost cutting process, and meets the requirements of automotive-grade and above products.
Smart Images

Figure CN118927426A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of diode cutting, and in particular relates to a diode cutting method for glass passivation. Background Art
[0002] Electronic products may experience product anomalies and malfunctions during normal use for a period of time. By checking the production records and process records, it was found that all products were fully inspected and qualified before leaving the factory, and the products also met the specifications. By opening the products and analyzing them, it was found that the cause of many product failures was cracks in the chip dicing path or shedding on the surface.
[0003] The glass passivation GPP process of chips is widely used in the power device and microelectronics industries. The glass passivation GPP process uses glass powder to protect the PN junction of chip products. Glass has high hardness and high stability compared to traditional coating processes; however, glass also has its disadvantages, that is, it is easy to crack and break, which brings great challenges to chip cutting; the current traditional practice in the industry is to use a laser to open a U-shaped groove once, and then use a cutter to cut. This method of cutting twice with a laser and then a blade has a complicated process and high cutting cost, and also increases the equipment cost. Since chip production has a long production line and many processes, any process will cause the entire process to fail. Therefore, in response to the problems in the prior art, this technical solution provides a diode cutting method for glass passivation to improve the stability of glass-purified diode chip dicing and reduce the risk of cracks or surface detachment in the dicing path. Summary of the invention
[0004] The present invention provides a diode cutting method for glass passivation, which is used to solve the problems of glass purification used in diode chips being easy to break, electrostatic adsorption during the dicing process, and product leakage and functional failure caused by breakage.
[0005] In order to solve the above technical problems, the present invention is achieved through the following technical solutions:
[0006] A method for cutting a glass-passivated diode according to the present invention comprises the following steps:
[0007] S1. Product confirmation and blade selection: Select specific cutting blades according to the specific parameters of glass-purified diode products, and determine the parameters of the cleaning pure water, including water temperature, water pressure and pure water flow parameters;
[0008] The specific steps include the following:
[0009] S11. Check whether the product type, batch number, number of pieces, blue film thickness and wafer thickness are consistent with the engineering documents;
[0010] S12. Confirm the product category. For glass passivated diode products, the method for selecting cutting blades is as follows:
[0011] The remaining blade amount a ≥ wafer thickness b + film cutting amount c + blade remaining safety amount d;
[0012] Among them, the blade residual a is the residual height after the blade cuts into the blue film and the wafer; b is 0.02mm, c is 0.05mm;
[0013] S13, the cutting feed speed is selected according to the thickness of the glass, and the thickness of the anti-oxidation glass passivation layer of the diode power device determines the blade speed;
[0014] When the thickness of the anti-oxidation glass passivation layer is 10-50um, the blade cutting speed is 35-20mm / second, the chip junction depth is 30-55A / angstrom, and the spindle rotation number is 38000r.pm + 500r.pm;
[0015] When the thickness of the anti-oxidation glass passivation layer is 51um~55um, the blade cutting speed is 19~15mm / second, the chip junction depth is 50~55A / angstrom, and the spindle rotation number is 38000r.pm + 500r.pm;
[0016] When the thickness of the anti-oxidation glass passivation layer is > 56um, blade cutting speed is < 14mm / sec, chip junction depth is 50~55A / angstrom, spindle rotation speed is 45000r.pm + 500r.pm;
[0017] S14, confirm the blade and the cutting knife's speed, and then confirm the resistivity and temperature of the cutting cleaning water. The cleaning water is pure water. The pure water is used to generate static heat and clean the cutting residues during the cutting process. Carbon dioxide is added to the pure water for foaming. The purity of the carbon dioxide is 99.5%;
[0018] S15. Flow rate control of cleaning water: The flow rate of cleaning water is 0.8-1.2L / min. Considering the surface tension of water, the dyne value of 25℃ pure water is 72dyn / cm + 5% pure water;
[0019] S2. After confirming the process requirements according to step S1, the actual cutting operation is carried out, including the following steps:
[0020] S21. Place the product to be cut fixed with a frame and blue film on the workbench and check for film breakage, particles, debris and film scraps;
[0021] S22. When using Z-EM software for manual calibration, adjust the angle θ formed between the blade and the wafer so that the blade's reference line and the cutting path are on the same horizontal line; if the cutting equipment is automatically calibrated, the quality control personnel are required to confirm the first piece and reference data;
[0022] S23, using the reference cross verification method, find the crossroads on the chip graphics obtained by the Z-EM software through the industrial camera, and overlap the reference line with the cutting path;
[0023] After the calibration of the reference line and the cutting path is completed, the Z-EM software is used to measure whether the corresponding chip size meets the specification requirements; after entering the cutting state, the quality control personnel will check the position and state of the cutting marks on the first cut on the product to see if adjustments are needed. The cut marks must be ensured to be within the control line.
[0024] S3. Effectiveness control and inspection methods for chip cutting: Use a 100x microscope to inspect the chip. No water droplets, oil stains or photoresist residues are allowed on the crystal grains. Oxidation, corrosion or yellowing, coffee, dark brown or colorful changes of the diode PAD are considered control failures. Observe the diode PAD under a microscope to see if there is a lotus leaf or butterfly pattern. Observe whether its color is yellowish or grayish with obvious boundaries. Confirm the temperature and surface tension parameters of the pure water.
[0025] Furthermore, in the step S13, the thickness of the anti-oxidation glass passivation layer is set to x, in units of um; the blade cutting speed corresponding to x is set to y, in units of mm / second;
[0026] When x∈[10,50], (The value of y is rounded to the nearest integer)
[0027] When x∈[51,55],y=-X+70;
[0028] When x∈[56,+∞),y=<14;
[0029] In summary,
[0030] Furthermore, in the step S14, pure water belongs to the organic compound H 2 0, resistivity is 18MΩ·cm.
[0031] Furthermore, the cross verification method includes the judgment of the knife marks on the chip film, and the first chip inspection is required if abnormal situations such as starting up, changing the knife, first chip and waiting occur during the cutting process.
[0032] Compared with the prior art, the present invention has the following beneficial effects:
[0033] (1) The present invention uses pure water from reverse osmosis technology to dissipate heat from the cutting blade, and controls the water flow, resistivity and pressure; uses the reference cross verification method for cutting, and uses a microscope to confirm the effect after cutting, so that the stability of diode chip dicing after processing is significantly improved, and solves the problems of cutting deviation, edge collapse, cracks and scratches, which can meet the requirements of automotive-grade products and above; solves the problems of glass breakage caused by high-temperature sintering of existing glass passivated chips, electrostatic adsorption during the dicing process, and product reliability caused during the dicing process;
[0034] (2) Based on the method steps of the present invention, it is possible to automatically select a suitable cutting blade and configure a matching blade speed for accurate and stable cutting based on the type of the corresponding glass-passivated diode product, and to achieve automatic matching, automatically matching a specific blade cutting speed based on the thickness of the anti-oxidation glass passivation layer, thereby improving stability and reducing the risk of cracks in the chip dicing path or surface shedding;
[0035] (3) The blade of the present invention is selected based on the thickness of the wafer, and the blade edge residual amount is not less than the sum of the wafer thickness, the film cutting amount and the blade edge residual safety amount, thereby ensuring the stability of the blade during cutting.
[0036] Of course, any product implementing the present invention does not necessarily need to achieve all of the advantages described above at the same time. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0038] Figure 1 A step diagram of a method for cutting a glass-passivated diode according to the present invention;
[0039] Figure 2 A state diagram of the blade cutting the wafer surface;
[0040] Figure 3 A cross-sectional view of a blade cutting a wafer surface;
[0041] Figure 4 A pattern diagram for finding crossroads on chip graphics using the reference cross verification method based on Z-EM software;
[0042] Figure 5 This is a top view of the knife marks left after cutting using the crossroad method based on the Z-EM software. DETAILED DESCRIPTION
[0043] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0044] Working principle of wafer dicing knife: Wafer dicing knife is a high-precision cutting tool, mainly used to cut large-sized wafers into small-sized chips; its working principle mainly includes the following steps:
[0045] Positioning: First, the wafer is fixed on the workbench of the dicing machine and accurately positioned by the optical system. The accuracy of positioning directly affects the cutting precision and yield rate.
[0046] Slicing: Slicing blades are usually made of diamond or other high-hardness materials and cut the wafer by high-speed rotation. The feed speed and rotation speed of the tool need to be controlled during the cutting process to ensure the smoothness and accuracy of the cutting.
[0047] Cleaning: A large amount of debris and dust will be generated during the cutting process, which needs to be cleaned by the cleaning system to prevent contamination and damage to the chip;
[0048] At present, the traditional practice in the industry is to use a laser to open a U-shaped groove, and then use a cutter to cut it. This method of first using a laser and then cutting with a blade has a complicated process, high cutting cost, and also increases the equipment cost. The technical solution proposes to select a corresponding blade and configure a corresponding cutting speed according to the parameters of the corresponding glass-passivated diode, thereby eliminating the need for a laser cutter and having good stability, which can prevent the diode from being cut off-center, broken edges, cracked, and scratched during cutting.
[0049] See also Figure 1-5 As shown, a method for cutting a glass-passivated diode of the present invention comprises the following steps:
[0050] S1. Product confirmation and blade selection: Select specific cutting blades according to the specific parameters of glass-purified diode products, and determine the parameters of the cleaning pure water, including water temperature, water pressure and pure water flow parameters;
[0051] The specific steps include the following:
[0052] S11. Check whether the product type, batch number, number of pieces, blue film thickness and wafer thickness are consistent with the engineering documents;
[0053] S12. Confirm the product category. For glass passivated diode products, the method for selecting cutting blades is as follows:
[0054] The remaining blade amount a ≥ wafer thickness b + film cutting amount c + blade remaining safety amount d;
[0055] Among them, the blade residual a is the residual height after the blade cuts into the blue film and the wafer; b is 0.02mm, c is 0.05mm, and the corresponding b and c values are specific parameter values obtained after repeated numerous tests and inspections, which can ensure the stability of the blade after cutting;
[0056] S13, the cutting feed speed is selected according to the thickness of the glass, and the thickness of the anti-oxidation glass passivation layer of the diode power device determines the blade speed;
[0057] When the thickness of the anti-oxidation glass passivation layer is 10-50um, the blade cutting speed is 35-20mm / second, the chip junction depth is 30-55A / angstrom, and the spindle rotation number is 38000r.pm + 500r.pm;
[0058] When the thickness of the anti-oxidation glass passivation layer is 51um~55um, the blade cutting speed is 19~15mm / second, the chip junction depth is 50~55A / angstrom, and the spindle rotation number is 38000r.pm + 500r.pm;
[0059] When the thickness of the anti-oxidation glass passivation layer is > 56um, blade cutting speed is < 14mm / sec, chip junction depth is 50~55A / angstrom, spindle rotation speed is 45000r.pm + 500r.pm; see Table 1 for specific values:
[0060]
[0061]
[0062] Table 1: Thickness, blade speed and chip junction depth selection data table
[0063] S14. Confirm the blade and cutting knife speed, and then confirm the resistivity and temperature of the cutting cleaning water. The cleaning water is pure water. Pure water generates static heat and cleans the cutting residues during the cutting process. Pure water belongs to the organic compound H20. The diode process is generally 180nm (.18um) process and 350nm (.35um). The process below 180nm uses a resistivity of 18MΩ·cm, and the process between 180nm and 350nm uses a resistivity of 18MΩ·cm. When using pure water with a resistivity of 18MΩ·cm, it is necessary to add carbon dioxide to the water for foaming process, which helps to eliminate static electricity, silicon, and accumulation of surface layer materials. The purity of carbon dioxide is 99.5%, and the cleaning water can effectively dissipate heat for the cutting blade.
[0064] S15, flow rate control of cleaning water, glass passivated diode chips are usually bipolar, the front and back chips are metallized, mainly Ti / Ni / Ag and Ti / Ni / Au three-layer materials, thickness is less than 300nm, select 0.8-1.2L / min flow rate, and the surface tension of water needs to be considered at the same time, the dyne value of pure water at 25℃ is 72dyn / cm+5%;
[0065] S2. After confirming the process requirements according to step S1, the actual cutting operation is carried out, including the following steps:
[0066] S21. Place the product to be cut fixed with a frame and blue film on the workbench and check for film breakage, particles, debris and film scraps;
[0067] S22. Use the software corresponding to the disc brand dicing machine: Z-EM software. When calibrating manually, adjust the angle θ formed by the blade and the wafer so that the blade's reference line and the cutting path are on the same horizontal line; if the dicing equipment is calibrated automatically, the quality control personnel are required to confirm the first piece and the reference data;
[0068] S23, using the reference cross verification method, find the crossroads on the chip graphics obtained by the Z-EM software through the industrial camera, and overlap the reference line with the cutting path; Figure 4 As shown, a schematic diagram of a crossroad formed by four adjacent chip layouts found using Z-EM software is shown;
[0069] After the calibration of the reference line and the cutting path is completed, use the Z-EM software to measure whether the corresponding chip size meets the specification requirements; after entering the cutting state, if Figure 5 As shown, the first cut on the product is checked by the quality control personnel for the position and status of the cut marks, whether adjustments are needed, and the cut marks must be ensured to be within the control line;
[0070] S3. Effectiveness control and inspection methods for chip cutting: Use a 100x microscope to inspect the chip. No water droplets, oil stains or photoresist residues are allowed on the crystal grains. Oxidation, corrosion or yellowing, coffee, dark brown or colorful changes of the diode PAD are considered control failures. Observe the diode PAD under a microscope to see if there is a lotus leaf or butterfly pattern. Observe whether its color is yellowish or grayish with obvious boundaries. Confirm the temperature and surface tension parameters of the pure water.
[0071] As a specific preferred embodiment, in step S13, the thickness of the anti-oxidation glass passivation layer is set to x, in units of um; the blade cutting speed corresponding to x is set to y, in units of mm / second;
[0072] When x∈[10,50], (The value of y is rounded to the nearest integer)
[0073] When x∈[51,55],y=-X+70;
[0074] When x∈[56,+∞),y=<14;
[0075] In summary,
[0076] This formula is a more detailed selection formula for the corresponding specific glass passivation layer thickness and the blade cutting speed based on the aforementioned step S13. Through detection, this formula can make the corresponding glass passivation layer thickness cooperate with the corresponding blade speed to obtain maximum cutting stability.
[0077] For example, when the thickness of the corresponding anti-oxidation glass passivation layer is 10um, the corresponding optimal blade cutting speed is directly output as 35mm / second; when the thickness of the corresponding anti-oxidation glass passivation layer is 50um, the corresponding optimal blade cutting speed is directly output as 20mm / second; when the thickness of the corresponding anti-oxidation glass passivation layer is 56um, the corresponding optimal blade cutting speed is directly output as < 14mm / sec, convenient and fast, can quickly give the specific optimal cutting speed;
[0078] Among them, the cross verification method includes the judgment of the knife marks on the chip film. If there are abnormal situations such as starting up, changing the knife, first cutting and standing by during the cutting process, the first cutting inspection is required.
[0079] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A method for cutting glass-passivated diodes, characterized in that: The steps include: S1. Product confirmation and blade selection: Select specific cutting blades according to the specific parameters of glass-purified diode products, and determine the parameters of the cleaning pure water, including water temperature, water pressure and pure water flow parameters; The specific steps include the following: S11. Check whether the product type, batch number, number of pieces, blue film thickness and wafer thickness are consistent with the engineering documents; S12. Confirm the product category. For glass passivated diode products, the method for selecting cutting blades is as follows: The remaining blade amount a ≥ wafer thickness b + film cutting amount c + blade remaining safety amount d; Among them, the blade residual a is the residual height after the blade cuts into the blue film and the wafer; b is 0.02mm, c is 0.05mm; S13, the cutting feed speed is selected according to the thickness of the glass, and the thickness of the anti-oxidation glass passivation layer of the diode power device determines the blade speed; When the thickness of the anti-oxidation glass passivation layer is 10-50um, the blade cutting speed is 35-20mm / second, the chip junction depth is 50-55A / angstrom, and the spindle rotation number is 38000r.pm + 500r.pm; When the thickness of the anti-oxidation glass passivation layer is 51um~55um, the blade cutting speed is 19~15mm / second, the chip junction depth is 50~55A / angstrom, and the spindle rotation number is 38000r.pm + 500r.pm; When the thickness of the anti-oxidation glass passivation layer is > 56um, blade cutting speed is less than 14mm / sec, chip junction depth is 50-55A / angstrom, spindle rotation number is 45000r.pm + 500r.pm; S14, confirm the blade and the cutting knife's speed, and then confirm the resistivity and temperature of the cutting cleaning water. The cleaning water is pure water. The pure water is used to generate static heat and clean the cutting residues during the cutting process. Carbon dioxide is added to the pure water for foaming. The purity of the carbon dioxide is 99.5%; S15. Flow rate control of cleaning water: The flow rate of cleaning water is 0.8-1.2L / min. Considering the surface tension of water, the dyne value of 25℃ pure water is 72dyn / cm + 5% pure water; S2. After confirming the process requirements according to step S1, the actual cutting operation is carried out, including the following steps: S21. Place the product to be cut fixed with a frame and blue film on the workbench and check for film breakage, particles, debris and film scraps; S22. When using Z-EM software for manual calibration, adjust the angle θ formed between the blade and the wafer so that the blade's reference line and the cutting path are on the same horizontal line; if the cutting equipment is automatically calibrated, the quality control personnel are required to confirm the first piece and reference data; S23, using the reference cross verification method, find the crossroads on the chip graphics obtained by the Z-EM software through the industrial camera, and overlap the reference line with the cutting path; After the calibration of the reference line and the cutting path is completed, the Z-EM software is used to measure whether the corresponding chip size meets the specification requirements; after entering the cutting state, the quality control personnel will check the position and state of the cutting marks on the first cut on the product to see if adjustments are needed. The cut marks must be ensured to be within the control line. S3. Effectiveness control and inspection methods for chip cutting: Use a 100x microscope to inspect the chip. No water droplets, oil stains or photoresist residues are allowed on the crystal grains. Oxidation, corrosion or yellowing, coffee, dark brown or colorful changes of the diode PAD are considered control failures. Observe the diode PAD under a microscope to see if there is a lotus leaf or butterfly pattern. Observe whether its color is yellowish or grayish with obvious boundaries. Confirm the temperature and surface tension parameters of the pure water.
2. A method for cutting glass-passivated diodes according to claim 1, characterized in that: In the step S13, the thickness of the anti-oxidation glass passivation layer is set to x, in units of um; the blade cutting speed corresponding to x is set to y, in units of mm / second; When x∈[10,50], (The value of y is rounded to the nearest integer) When x∈[51,55],y=-X+70; When x∈[56,+∞),y=<14; In summary, 3. A method for cutting glass-passivated diodes according to claim 1, characterized in that: In the step S14, pure water is an organic compound H20, and its resistivity is 18 MΩ·cm.
4. A method for cutting glass-passivated diodes according to claim 1, characterized in that: The cross verification method includes the judgment of the knife marks on the chip film. If there are abnormal situations such as starting up, changing the knife, first cutting and waiting during the cutting process, the first cutting inspection is required.