Method for using household garbage incineration slag as cement stabilized macadam base
Through harmless treatment of high temperature and fine screening, impurities are removed, combined with particle size grouping and proportion adjustment, the differences and uncertainties of domestic waste incinerator slag in cement-stabilized gravel base are solved, and the construction control is unified and unified The dual goal of environmental protection.
Patent Information
- Application Number
- CN202411151052.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-12
AI Technical Summary
The lack of unified technical guidance and quality control standards in the existing technology, resulting in differences and uncertainties in the application of domestic waste incinerator slag in cement-stabilized gravel bases, affecting construction control.
Through high-temperature harmless treatment, screening, magnetic separation and air selection, harmful substances and impurities are removed, combined with particle size grouping and proportion adjustment, reasonable cement content and grading are designed to ensure the optimal moisture content and maximum dry density of the mixture. , and carry out strict construction and maintenance processes.
It has realized the effective application of domestic waste incinerator slag in cement-stabilized gravel base, reduced environmental pollution and construction difficulties, and improved the benefits of resource recycling and environmental protection.
Smart Images

Figure CN118930100A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of domestic waste treatment, in particular to a method of utilizing domestic waste incineration slag as a cement-stabilized gravel base. Background Art
[0002] Domestic waste incineration slag refers to the solid waste generated during the incineration of domestic waste, mainly composed of ash and waste residue. These slags are the residual materials after domestic waste is incinerated at high temperature, and their composition mainly includes glass, metal and various inorganic substances, such as manganese oxide, silicon dioxide, calcium oxide, aluminum oxide, iron oxide, etc., as well as a small amount of unburned organic matter and scrap metal.
[0003] In recent years, with the continuous improvement of environmental awareness and the increasing demand for sustainable development, the application of domestic waste incineration slag as cement stabilized crushed stone base has gradually emerged and received widespread attention. Studies have shown that cement stabilized crushed stone is a mixture formed by mixing cement with crushed stone aggregate by adding water and cement as a binder. It has the characteristics of strong integrity, large bearing capacity, moderate strength and stiffness. By using domestic waste incineration slag as aggregate to replace part of the natural crushed stone aggregate, through reasonable proportioning and process control, a base material that meets the engineering requirements can be obtained. This practice not only embodies the concept of resource recycling, but also reduces environmental pollution, has significant environmental and social benefits, and has been a research hotspot and practice direction in the field of road engineering in recent years.
[0004] However, the current technical standards and specifications for the application of slag in cement-stabilized gravel base are not perfect enough, and there is a lack of unified technical guidance and quality control standards, which leads to differences and uncertainties in the application of slag in different regions and projects. In addition, slag aggregates from different batches and different beneficiation processes differ in physical and mechanical properties, such as density, water absorption, crushing value, etc., which will affect the optimal moisture content, maximum dry density and other performance parameters of the mixture, bringing certain difficulties to construction control.
[0005] Therefore, it is urgent to improve this shortcoming. The present invention studies and improves the existing technology and its shortcomings, and provides a method for utilizing domestic waste incineration slag as a cement stabilized gravel base. Summary of the invention
[0006] The object of the present invention is to provide a method for utilizing domestic waste incineration slag as a cement stabilized gravel base layer to solve the problems raised in the above-mentioned background technology.
[0007] To achieve the above object, the present invention provides the following technical solution: a method for using domestic waste incineration slag as a cement stabilized gravel base, comprising the following steps: S1. Slag pretreatment: The slag from the incineration of domestic waste is subjected to high-temperature harmless treatment to remove harmful substances and residual organic matter, and then screened to classify the slag according to particle size, and then subjected to impurity removal treatment, using magnetic separation and air separation to remove metal impurities, unburned organic matter, etc. in the slag; S2. Mix design: According to the project requirements, slag properties and test data, determine the amount of slag in the cement-stabilized crushed stone base (the amount of slag aggregate affects the optimal moisture content, maximum dry density and other properties of the cement-stabilized crushed stone mixture), and adjust the cement content according to the slag content and the performance requirements of the mixture (the amount of cement added should be sufficient to effectively solidify the slag and ensure the strength and durability of the mixture), and then optimize the gradation of the mixture in combination with the characteristics of the slag particle size distribution; S3, Mixing and paving: Mix the pre-treated slag aggregate, cement and water in proportion at a mixing station to form a uniform cement-stabilized slag crushed stone mixture, and transport the mixed mixture to the construction site for paving; S4. Compaction and maintenance: Use a vibratory roller or a tire roller to compact the paved mixture to form an integral structure with certain strength and rigidity, and sprinkle water on the paved and compacted cement-stabilized slag gravel base to keep the surface of the base moist; S5. Quality inspection: During the construction process and after the maintenance, the cement-stabilized slag gravel base layer shall be subjected to quality inspection, and the inspection results must comply with the design requirements and relevant standards.
[0008] Furthermore, in step S1, the specific operation of the screening treatment is: use sieves with three specifications of apertures of 9.5 mm, 4.75 mm and 2.36 mm to screen the waste incineration slag; crush the part above 9.5 mm to ensure that the particle size meets the requirements of subsequent utilization, and further subdivide the part less than 9.5 mm, among which the 4.75-9.5 mm part is used as recycled coarse aggregate, the 2.36-4.75 mm part is used as recycled fine aggregate, and the part below 2.36 mm is used as mineral processing raw material or other purposes.
[0009] Furthermore, in step S1, magnetic separation utilizes the difference in magnetic properties of various components in the material to perform separation in an uneven magnetic field to remove metal impurities in the slag; the specific operation process of magnetic separation is as follows: the slag is sent into the separation space of the separator, and there is a strong magnetic field in the space. Magnetic materials (such as metal impurities such as iron and steel) are affected by the magnetic force in the magnetic field and are adsorbed on the magnetic poles of the magnetic separator, while non-magnetic materials are not affected by the magnetic force and continue to flow or fall. Subsequently, the magnetic materials adsorbed on the magnetic poles are removed by mechanical or electromagnetic devices to achieve separation of magnetic materials from non-magnetic materials.
[0010] Furthermore, in step S1, air separation (also known as airflow sorting) utilizes the difference in suspension speed between materials and impurities to perform sorting under the action of airflow; the specific operation process of air separation is: the slag is sent into the air separator and blown by the high-speed airflow. Due to differences in density, shape, particle size, etc. of the material particles, their suspension speeds in the airflow are different. Light impurities such as unburned organic matter and dust are suspended in the airflow at a faster speed and are carried away and collected by the airflow; while the heavy slag particles are suspended at a slower speed and eventually fall to the bottom of the air separator or a specific collection device.
[0011] Furthermore, in step S2, the optimization design includes the following process: Particle size grouping: group the slag according to particle size; Proportion adjustment: According to the design requirements of the mixture and the particle size distribution characteristics of the slag, the proportion of slag of each particle size group is adjusted. Among them, the large particle size slag should account for a larger proportion to form a skeleton structure, the medium particle size slag fills the gaps between the skeletons, and the small particle size slag plays the role of micro-aggregate; Mixing natural aggregates: If some particle size components of slag are insufficient or have poor performance, add appropriate amount of natural aggregates (such as crushed stone, sand, etc.) to improve the performance of the mixture; Test verification: After the gradation design is completed, indoor tests and field tests are carried out to verify its performance, evaluate the rationality of the gradation design and make necessary adjustments.
[0012] Furthermore, in step S3, the mixing time is controlled within 3 to 5 minutes, and during the mixing process, the moisture content of the material is controlled within 5% to 7% by adding water.
[0013] Furthermore, in step S3, a paver is used for paving operations, and the surface of the mixture after paving should be flat, without obvious bumps and waves, and the paving thickness and width are controlled according to design requirements to ensure that the bearing capacity and use requirements of the project are met.
[0014] Furthermore, in step S4, the compaction operation requires that the compaction degree reaches more than 90% of the design requirement, and the compaction strength should be gradually increased during the compaction process to avoid over-vibration and displacement.
[0015] Furthermore, in step S4, the curing time is not less than 7 days, and watering is carried out by using a spray or fine water mist nozzle to avoid using a high-pressure nozzle to directly impact the surface of the base layer to avoid damaging the base layer structure. The number of watering times is increased when the temperature is high and the wind is strong; the number of watering times is reduced on rainy days or when the surface of the base layer is already relatively moist.
[0016] Furthermore, in step S5, the quality inspection indexes of the cement-stabilized slag gravel base layer include compaction, strength, and flatness, and the inspection process of each index is as follows: Compactness: The test is carried out by using the sand filling method (the volume of the test pit is converted by the volume of standard sand to calculate the density and compactness of the material) or the nuclear density meter method (the density and water content of the material are measured by using radioactive elements to calculate the compactness), and the sampling positions are randomly distributed and cover the entire test area; Strength: The test is carried out through the unconfined compressive strength test. The specific operation is as follows: before the test, a standard specimen needs to be made and cured under the specified conditions. Then, a press is used to apply vertical pressure to the specimen until the specimen is destroyed. The maximum pressure value at the time of destruction is recorded, and the unconfined compressive strength is calculated based on it. Flatness: Use the 3m ruler method for testing. The specific operation is: place a 3m ruler at the test point, measure the maximum gap between the bottom of the ruler and the surface of the base layer, which is used as the flatness index of the point, and then measure at multiple test points. Calculate statistical indicators including the mean or standard deviation to evaluate the flatness of the entire base layer.
[0017] The present invention provides a method for using domestic waste incineration slag as a cement-stabilized gravel base, which has the following beneficial effects: The present invention has formulated a set of unified technical guidance and quality control standards so as to utilize domestic waste incineration slag as cement stabilized gravel base, and reduces the differences and uncertainties in its application in different regions and projects by strictly controlling the process links such as slag pretreatment, proportion design, mixing and paving; and realizes the effective application of domestic waste incineration slag in cement stabilized gravel base, thereby achieving the dual goals of resource recycling and environmental protection, reducing environmental pollution, and having significant environmental and social benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 A schematic flow chart of the steps of a method of using domestic waste incineration slag as a cement stabilized gravel base layer according to the present invention; Figure 2 It is a screening processing logic block diagram of a method of using domestic waste incineration slag as a cement stabilized gravel base layer according to the present invention; Figure 3 This is a schematic diagram of the classification of quality inspection methods for a method of using domestic waste incineration slag as a cement stabilized gravel base layer according to the present invention. DETAILED DESCRIPTION
[0019] The following embodiments of the present invention are described in further detail in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.
[0020] like Figure 1-Figure 3 As shown, a method for using domestic waste incineration slag as a cement stabilized gravel base comprises the following steps: S1. Slag pretreatment: The slag from the incineration of domestic waste is subjected to high-temperature harmless treatment to remove harmful substances and residual organic matter, and then screened to classify the slag according to the particle size. The specific operation of the screening treatment is as follows: use sieves with three specifications of apertures of 9.5 mm, 4.75 mm and 2.36 mm to screen the slag from the incineration of waste; crush the part above 9.5 mm to ensure that the particle size meets the requirements for subsequent utilization, and further subdivide the part less than 9.5 mm, of which the part between 4.75 and 9.5 mm is used as recycled coarse aggregate, the part between 2.36 and 4.75 mm is used as recycled fine aggregate, and the part below 2.36 mm is used as mineral processing raw material or other purposes, and then the impurity removal treatment is carried out to remove metal impurities, unburned organic matter, etc. in the slag by magnetic separation and air separation; Magnetic separation utilizes the difference in magnetic properties of various components in the material to separate them in an uneven magnetic field, and is used to remove metal impurities in slag. The specific operation process of magnetic separation is as follows: the slag is sent into the separation space of the separator, where there is a strong magnetic field. Magnetic materials (such as iron, steel and other metal impurities) are affected by the magnetic force in the magnetic field and are adsorbed on the magnetic poles of the magnetic separator, while non-magnetic materials are not affected by the magnetic force and continue to flow or fall. Subsequently, the magnetic materials adsorbed on the magnetic poles are removed by mechanical or electromagnetic devices to separate the magnetic materials from the non-magnetic materials. Air separation (also known as airflow separation) uses the difference in suspension speed between materials and impurities to separate them under the action of airflow. The specific operation process of air separation is as follows: the slag is sent into the air separator and blown by the high-speed airflow. Due to the differences in density, shape, particle size, etc. of the material particles, their suspension speeds in the airflow are different. Light impurities such as unburned organic matter and dust are suspended faster in the airflow and are carried away and collected by the airflow; while heavy slag particles are suspended slower and eventually fall to the bottom of the air separator or a specific collection device. S2. Mix design: According to the project requirements, slag properties and test data, determine the amount of slag in the cement-stabilized crushed stone base (the amount of slag aggregate affects the optimal moisture content, maximum dry density and other properties of the cement-stabilized crushed stone mixture), and adjust the cement content according to the slag content and the performance requirements of the mixture (the amount of cement added should be sufficient to effectively solidify the slag and ensure the strength and durability of the mixture). Combined with the characteristics of slag particle size distribution, optimize the gradation of the mixture. The optimization design includes the following processes: Particle size grouping: group the slag according to particle size; Proportion adjustment: According to the design requirements of the mixture and the particle size distribution characteristics of the slag, the proportion of slag of each particle size group is adjusted. Among them, the large particle size slag should account for a larger proportion to form a skeleton structure, the medium particle size slag fills the gaps between the skeletons, and the small particle size slag plays the role of micro-aggregate; Mixing natural aggregates: If some particle size components of slag are insufficient or have poor performance, add appropriate amount of natural aggregates (such as crushed stone, sand, etc.) to improve the performance of the mixture; Test verification: After the gradation design is completed, indoor tests and field tests are carried out to verify its performance, evaluate the rationality of the gradation design and make necessary adjustments; S3, Mixing and paving: The pre-treated slag aggregate, cement and water are mixed in proportion at a mixing station. The mixing time is controlled within 3 to 5 minutes. During the mixing process, the moisture content of the material is controlled within 5% to 7% by adding water until a uniform cement-stabilized slag crushed stone mixture is formed. The mixed mixture is then transported to the construction site for paving. A paver is used for paving. The surface of the paved mixture should be flat without obvious bumps and waves. The paving thickness and width are controlled according to the design requirements to ensure that the bearing capacity and use requirements of the project are met. S4. Compaction and maintenance: Use a vibrating roller or a tire roller to compact the paved mixture to form an integral structure with certain strength and rigidity. The compaction operation requires that the compaction degree reach more than 90% of the design requirements, and the compaction strength should be gradually increased during the compaction process to avoid over-vibration and displacement. The cement-stabilized slag gravel base after paving and compaction should be watered to maintain the surface of the base moist. The maintenance time should be no less than 7 days. Spraying or fine water mist nozzles should be used for watering. Avoid using high-pressure nozzles to directly impact the surface of the base to avoid damaging the base structure. In the case of high temperature and strong wind, increase the number of watering; in rainy days or when the surface of the base is already relatively moist, reduce the number of watering; S5. Quality inspection: During the construction process and after the maintenance, the cement stabilized slag crushed stone base shall be inspected for quality. The inspection results must meet the design requirements and relevant standards. The quality inspection indicators of the cement stabilized slag crushed stone base include compaction, strength, and flatness, and the inspection process of each indicator is as follows: Compactness: The test is carried out by using the sand filling method (the volume of the test pit is converted by the volume of standard sand to calculate the density and compactness of the material) or the nuclear density meter method (the density and water content of the material are measured by using radioactive elements to calculate the compactness), and the sampling positions are randomly distributed and cover the entire test area; Strength: The test is carried out through the unconfined compressive strength test. The specific operation is as follows: before the test, a standard specimen needs to be made and cured under the specified conditions. Then, a press is used to apply vertical pressure to the specimen until the specimen is destroyed. The maximum pressure value at the time of destruction is recorded, and the unconfined compressive strength is calculated based on it. Flatness: Use the 3m ruler method for testing. The specific operation is: place a 3m ruler at the test point, measure the maximum gap between the bottom of the ruler and the surface of the base layer, which is used as the flatness index of the point, and then measure at multiple test points. Calculate statistical indicators including the mean or standard deviation to evaluate the flatness of the entire base layer.
[0021] The embodiments of the present invention are given for the purpose of illustration and description, and are not intended to be exhaustive or to limit the invention to the disclosed forms. Many modifications and variations will be apparent to those of ordinary skill in the art. The embodiments are selected and described in order to better illustrate the principles and practical applications of the present invention and to enable those of ordinary skill in the art to understand the present invention and thereby design various embodiments with various modifications suitable for specific uses.
Claims
1. A method for using domestic waste incineration slag as cement stabilized gravel base, characterized in that: The following steps are involved: S1. Slag pretreatment: The slag from the incineration of domestic waste is subjected to high-temperature harmless treatment to remove harmful substances and residual organic matter, and then screened to classify the slag according to particle size, and then subjected to impurity removal treatment to remove metal impurities and unburned organic matter in the slag by magnetic separation and air separation; S2. Mix design: Determine the amount of slag added to the cement-stabilized crushed stone base according to the project requirements, slag properties and test data, adjust the cement content according to the slag content and the performance requirements of the mixture, and optimize the gradation of the mixture in combination with the slag particle size distribution characteristics; S3, Mixing and paving: Mix the pre-treated slag aggregate, cement and water in proportion at a mixing station to form a uniform cement-stabilized slag crushed stone mixture, and transport the mixed mixture to the construction site for paving; S4. Compaction and maintenance: Use a vibratory roller or a tire roller to compact the paved mixture to form an integral structure with certain strength and rigidity, and sprinkle water on the paved and compacted cement-stabilized slag gravel base to keep the surface of the base moist; S5. Quality inspection: During the construction process and after the maintenance, the cement-stabilized slag gravel base layer shall be subjected to quality inspection, and the inspection results must comply with the design requirements and relevant standards.
2. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In the step S1, the specific operation of the screening treatment is: using sieves with three specifications of apertures of 9.5 mm, 4.75 mm and 2.36 mm to screen the waste incineration slag; crushing the part above 9.5 mm, and further subdividing the part less than 9.5 mm, wherein the part of 4.75-9.5 mm is used as recycled coarse aggregate, the part of 2.36-4.75 mm is used as recycled fine aggregate, and the part below 2.36 mm is used as mineral processing raw material or other purposes.
3. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S1, magnetic separation utilizes the difference in magnetic properties of various components in the material to perform separation in an uneven magnetic field, so as to remove metal impurities in the slag. The specific operation process of magnetic separation is as follows: the slag is sent into the separation space of the separator, and there is a strong magnetic field in the space. The magnetic material is acted upon by the magnetic force in the magnetic field and is adsorbed on the magnetic pole of the magnetic separator, while the non-magnetic material is not affected by the magnetic force and continues to flow or fall. Subsequently, the magnetic material adsorbed on the magnetic pole is removed by mechanical or electromagnetic devices to achieve separation of the magnetic material from the non-magnetic material.
4. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S1, air separation utilizes the difference in suspension speed between materials and impurities to perform separation under the action of airflow; the specific operation process of air separation is as follows: the slag is sent into the air separator and blown by the high-speed airflow. Light impurities such as unburned organic matter and dust are suspended in the airflow at a faster speed and are carried away and collected by the airflow; while the heavy slag particles are suspended at a slower speed and eventually fall to the bottom of the air separator or a specific collection device.
5. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S2, the optimization design includes the following process: Particle size grouping: group the slag according to particle size; Proportion adjustment: According to the design requirements of the mixture and the particle size distribution characteristics of the slag, the proportion of slag of each particle size group is adjusted. Among them, the large particle size slag should account for a larger proportion to form a skeleton structure, the medium particle size slag fills the gaps between the skeletons, and the small particle size slag plays the role of micro-aggregate; Blending with natural aggregates: If certain particle size components of slag are insufficient or have poor performance, natural aggregates can be blended to improve the performance of the mixture; Test verification: After the gradation design is completed, indoor tests and field tests are carried out to verify its performance, evaluate the rationality of the gradation design and make necessary adjustments.
6. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S3, the mixing time is controlled within 3 to 5 minutes, and during the mixing process, the moisture content of the material is controlled within 5% to 7% by adding water.
7. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S3, a paver is used for paving operations, and the surface of the mixture after paving should be flat, without obvious bumps and waves. The paving thickness and width are controlled according to the design requirements to ensure that the bearing capacity and use requirements of the project are met.
8. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S4, the compaction operation requires that the compaction degree reaches more than 90% of the design requirement, and the compaction strength should be gradually increased during the compaction process.
9. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S4, the curing time is not less than 7 days, and watering is carried out by a spray or fine water mist nozzle. When the temperature is high and the wind is strong, the watering frequency is increased; when it is rainy or the surface of the base is already relatively moist, the watering frequency is reduced.
10. The method of using domestic waste incineration slag as cement stabilized gravel base according to claim 1, characterized in that: In step S5, the quality inspection indexes of the cement-stabilized slag gravel base layer include compaction, strength, and flatness, and the inspection process of each index is as follows: Compactness: The test is carried out by sand filling method or nuclear density meter method, and the sampling positions are randomly distributed and cover the entire test area; Strength: The test is carried out through the unconfined compressive strength test. The specific operation is as follows: before the test, a standard specimen needs to be made and cured under the specified conditions. Then, a press is used to apply vertical pressure to the specimen until the specimen is destroyed. The maximum pressure value at the time of destruction is recorded, and the unconfined compressive strength is calculated based on it. Flatness: Use the 3m ruler method for testing. The specific operation is: place a 3m ruler at the test point, measure the maximum gap between the bottom of the ruler and the surface of the base layer, which is used as the flatness index of the point, and then measure at several test points and calculate statistical indicators including the mean or standard deviation to evaluate the flatness of the entire base layer.