Low-viscosity ultrahigh-strength concrete member
By setting splicing grooves and plug-ins in concrete components, combining foamed concrete and polyurethane paint hardened layers, the splicing strength and wear resistance are solved, and high-strength, durability and low-cost concrete components are achieved, suitable for complex building shapes and high intensity demand.
Patent Information
- Application Number
- CN202411001322.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The splicing strength of existing concrete components is low, prone to cracks or looseness, poor wear resistance, easy to wear, and lack effective waterproofing measures, which affects structural stability and aesthetics and increases construction difficulty and cost.
Low viscosity ultra-high strength concrete components are used, and splicing grooves and ear lifting grooves are provided on the surface of the main building block, and plugs are provided on the surface of the splicing block, combining the inner core, outer cover and hardened layer structure to increase splicing strength and wear resistance. And improve strength and durability by slag grinding and adding fiber reinforced materials.
It improves the splicing strength and stability of components, extends service life, reduces construction costs, and enhances crack resistance and wear resistance, suitable for complex building shapes and high-strength needs.
Smart Images

Figure CN118933257A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of concrete components, in particular to a low-viscosity ultra-high-strength concrete component. Background Art
[0002] In the field of construction engineering, concrete components, as an important part of building structures, have a long history of technological development and are constantly innovating. Existing concrete component technologies widely use cement, water, aggregates (including fine aggregates and coarse aggregates) and appropriate amounts of additives as the main raw materials, and are made through processes such as mixing, molding, and curing. With the advancement of science and technology, the performance of concrete components has been continuously improved, including significant improvements in strength, durability, and crack resistance. For example, by adding mineral admixtures (such as fly ash, slag, etc.) and superplasticizers, the fluidity and strength of concrete can be effectively improved, while reducing water consumption and improving the working performance and mechanical properties of concrete. In addition, the research and development and application of new concrete technologies such as high-strength concrete and self-compacting concrete have further broadened the application scope of concrete components and met the higher requirements of modern buildings for structural safety, durability, construction efficiency, etc.
[0003] Existing concrete components are still simple block structures or hollow brick structures, and the inherent block structure and its splicing combination methods still have many shortcomings. Traditional concrete components are mostly regular block shapes. Although this design is easy to make and transport, in the actual splicing process, a simple splicing method is often used, such as direct stacking or fixing with a small number of connectors. This splicing method has the problem of low splicing strength, which is easy to cause cracks or looseness between components, affecting the stability and safety of the overall structure. At the same time, due to the relatively low surface hardness of concrete and poor wear resistance, it is susceptible to wear during long-term use, affecting the appearance and service life. In addition, the concrete material itself has a certain water absorption, and traditional concrete components often lack effective waterproof measures at the splicing point, which is easy to cause water seepage problems, further aggravating the aging and damage of the structure. More importantly, due to the large structural mass of traditional concrete components, not only the difficulty of transportation and installation is increased, but also the use cost of the overall project is increased. Therefore, improving and innovating these defects of traditional concrete components is of great significance for improving the performance of building structures and reducing the use cost.
[0004] In view of this, research and improvement are carried out on the existing problems, and a low-viscosity ultra-high-strength concrete component is provided to solve the current problems. The purpose is to solve the problems and improve the practical value through this technology. Summary of the invention
[0005] The present invention aims to solve one of the technical problems existing in the prior art or related technology.
[0006] To this end, the technical solution adopted by the present invention is: a low-viscosity ultra-high-strength concrete component, comprising: a main block and a splicing block, the surface of the main block is provided with a splicing groove and a lug groove, the surface of the splicing block is provided with an insert, the splicing groove comprises a first slot and a second slot, the length of the first slot is twice the length of the second slot, the length of the splicing block is less than or equal to the length of the second slot, both ends of the first slot and both ends of the second slot are provided with entry slots for inserting the splicing block, and the cross-sectional shapes of the first slot and the second slot are adapted to the cross-sectional shapes of the splicing block and the insert;
[0007] The main structural block comprises an inner core, an outer covering layer and a hardened layer. The inner core is formed by pouring foamed concrete, the outer covering layer is formed by pouring non-foamed concrete, and the hardened layer is a polyurethane paint coating.
[0008] In a preferred example, the present invention can be further configured as follows: the outer coating layer includes the following raw materials in weight percentage:
[0009] Cement: 30%-50%, fine aggregate: 20%-40%, coarse aggregate: 10%-30%, water: 5%-15%, superplasticizer: 0.5%-5%, mineral admixture: 5%-20%, fiber reinforcement material: 0.1%-2%; wherein the inner core body is further added with a foaming agent: 1%-5% in the raw materials with this weight percentage.
[0010] In a preferred example, the present invention can be further configured as follows: the cement is high-performance silicate cement, the fine aggregate is sand with a particle size of less than 5 mm, the coarse aggregate is crushed stone or mineral particles with a particle size between 5 mm and 20 mm, the superplasticizer is a polycarboxylic acid-based high-efficiency water reducer, the mineral admixture includes one or more of fly ash, silica fume and slag powder, and the fiber reinforcement material is polypropylene fiber or steel fiber. By adding mineral admixtures and fiber reinforcement materials, low-viscosity ultra-high-strength concrete has high durability. It can resist erosion from various external environments, including chloride ions, sulfates, alkali-aggregate reactions, etc., thereby extending the service life of components.
[0011] In a preferred example, the present invention can be further configured as follows: the fine aggregate is processed by grinding the slag to destroy the glassy crystal structure of the slag and fully stimulate the activity of the slag, thereby improving the strength of the slag cement; potassium sulfate, slaked lime and grinding aids are added during the slag grinding process to increase the reaction activity and strength, fully stimulate the activity of the slag powder, and improve the hardness of the cement after hardening. By grinding the slag, the glassy crystal structure of the slag is destroyed, and the activity of the slag can be fully stimulated, thereby improving the strength of the slag cement. The high activity of the slag enables the cement to form more hydration products during the hardening process, thereby enhancing the strength of the cement.
[0012] In a preferred example, the present invention can be further configured as follows: the relationship between the length, width and height of the main building blocks is: the width and height are equal, and the length is equal to twice the width and height. The appropriate length, width and height ratio facilitates the regular splicing and combination of the main building blocks.
[0013] In a preferred example, the present invention can be further configured as follows: the first slots are located on the upper and lower surfaces of the main block, the number of the second slots is twelve, four of which are combined in pairs to form a cross arrangement at both ends of the main block and are interconnected with the ends of the first slots, and the other eight second slots are respectively combined to form two rings arranged parallel to each other on the surface of the main block and staggered with the first slots, and the spacing between the two ring-arranged second slots is equal to the length of the splicing block.
[0014] In a preferred example, the present invention can be further configured as follows: the number of the plug-ins is four and they are arranged in groups of two on both sides of the splicing block and parallel to each other, gaps are provided between the plug-ins in the same group, and the spacing between the plug-ins on both sides is equal to twice the height of the plug-ins, and the surface of the splicing block is provided with anchor bolt holes that penetrate the splicing block, and the plug-ins on the surface of the splicing block are inserted into the first slot and the inner side of the second slot to realize the splicing connection between the two adjacent main blocks, and the locking positioning of the splicing state of the entire main block can be realized by inserting structures such as steel bars through the anchor bolt holes.
[0015] In a preferred example, the present invention can be further configured as follows: the outer covering layer is located at the periphery of the inner core and has a thickness of 1-2 cm, the hardened layer is located at the periphery of the outer covering layer and has a thickness of 0.3-0.5 cm, and a layer of polyurethane paint is coated on the surface of the outer covering layer, which is cured to form a polyurethane coating as a hardened layer structure to improve the surface hardness and wear resistance of the main structural block.
[0016] The beneficial effects achieved by the present invention are:
[0017] 1. In the present invention, a novel split splicing structure is provided, wherein the first slot and the second slot on the surface of the main block are adapted to and plugged into the splicing block, and adjacent main blocks are combined and spliced through the splicing block. The appropriate proportion design makes the components more regular during splicing, reduces the splicing gap, and improves the stability and aesthetics of the overall structure. The splicing structure of the main block and the splicing block not only enhances the splicing strength, but also makes the splicing process more flexible and diverse, and adapts to the needs of different building shapes.
[0018] 2. In the present invention, a multi-layer main structural block structure is adopted, which is composed of an inner core, an outer covering layer and a hardened layer. The foamed concrete structure is used internally to reduce the overall main structural block mass to reduce construction costs, and the outer covering layer and the hardened layer improve the surface hardness and wear resistance of the main structural block.
[0019] 3. In the present invention, the glass crystal structure of slag is destroyed by grinding it. The high activity of slag enables cement to form more hydration products during the hardening process, thereby enhancing the strength of cement. Potassium sulfate, slaked lime and grinding aids are added during the slag grinding process. Due to the high activity of slag, it can partially replace the traditional cement dosage, thereby optimizing the cement mix ratio, significantly reducing the cement dosage and reducing production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the overall structure of the present invention;
[0021] Figure 2 It is a schematic diagram of the main building block and the splicing block structure of the present invention;
[0022] Figure 3 It is a schematic diagram of the main building block structure of the present invention;
[0023] Figure 4 It is a schematic diagram of a partial cross-sectional structure of a main building block of the present invention;
[0024] Figure 5 It is a schematic diagram of the structure of the splicing block of the present invention.
[0025] Reference numerals:
[0026] 100, main block; 110, splicing groove; 120, ear groove; 111, first slot; 112, second slot; 113, entrance slot; 101, inner core; 102, outer covering layer; 103, hardening layer;
[0027] 200, splicing block; 210, plug-in unit; 220, rebar hole. DETAILED DESCRIPTION
[0028] To make the purpose, technical solution and advantages of the present invention more clear, the present invention is further described in detail below in combination with specific implementations and with reference to the accompanying drawings. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.
[0029] A low-viscosity ultra-high-strength concrete component provided by some embodiments of the present invention will be described below in conjunction with the accompanying drawings.
[0030] Combination Figure 1-Figure 5As shown, a low-viscosity ultra-high-strength concrete component provided by the present invention comprises: a main block 100 and a splicing block 200, wherein a splicing groove 110 and a lifting ear groove 120 are provided on the surface of the main block 100, and an insert 210 is provided on the surface of the splicing block 200, wherein the splicing groove 110 comprises a first slot 111 and a second slot 112, wherein the length of the first slot 111 is twice the length of the second slot 112, and the length of the splicing block 200 is less than or equal to the length of the second slot 112, and both ends of the first slot 111 and the second slot 112 are provided with an entrance groove 113 for inserting the splicing block 200, and the cross-sectional shapes of the first slot 111 and the second slot 112 are adapted to the cross-sectional shapes of the splicing block 200 and the insert 210;
[0031] The main structural block 100 includes an inner core 101 , an outer covering layer 102 and a hardening layer 103 . The inner core 101 is formed by pouring foamed concrete, the outer covering layer 102 is formed by pouring non-foamed concrete, and the hardening layer 103 is a polyurethane paint coating.
[0032] In this embodiment, the outer cover 102 includes the following raw materials in weight percentage:
[0033] Cement: 30%-50%, fine aggregate: 20%-40%, coarse aggregate: 10%-30%, water: 5%-15%, superplasticizer: 0.5%-5%, mineral admixture: 5%-20%, fiber reinforcement material: 0.1%-2%; wherein the inner core 101 further adds a foaming agent: 1%-5% to the raw materials in this weight percentage.
[0034] Specifically, low-viscosity ultra-high-strength concrete has very high compressive strength and flexural strength, which can meet the extremely high requirements of material strength for some special projects. The strength of this concrete is usually several times that of ordinary concrete, and is suitable for structures that require high-strength materials, such as high-rise buildings and large-span bridges.
[0035] Furthermore, the cement is high-performance silicate cement, the fine aggregate is sand with a particle size of less than 5 mm, the coarse aggregate is crushed stone or mineral particles with a particle size between 5 mm and 20 mm, the superplasticizer is a polycarboxylic acid-based high-efficiency water reducer, the mineral admixture includes one or more of fly ash, silica fume and slag powder, and the fiber reinforcement material is polypropylene fiber or steel fiber.
[0036] Furthermore, by adding mineral admixtures and fiber reinforcement materials, low-viscosity ultra-high-strength concrete has high durability. It can resist erosion from various external environments, including chloride ions, sulfates, alkali-aggregate reactions, etc., thereby extending the service life of the component; low viscosity allows the concrete to have good fluidity during the pouring process, making it easier to fill complex molds and small gaps. This not only improves construction efficiency, but also reduces the generation of bubbles and honeycomb defects on the surface of the outer covering layer 102, ensuring the density and uniformity of the concrete component.
[0037] In this embodiment, the fine aggregate is processed by grinding slag to destroy the glassy crystal structure of the slag and fully stimulate the activity of the slag, thereby improving the strength of the slag cement. Potassium sulfate, slaked lime and grinding aids are added during the slag grinding process to increase the reaction activity and strength, fully stimulate the activity of the slag powder, and improve the hardness of the cement after hardening.
[0038] Specifically, by grinding slag, its glassy crystal structure is destroyed, which can fully stimulate the activity of slag, thereby improving the strength of slag cement. The high activity of slag enables cement to form more hydration products during the hardening process, thereby enhancing the strength of cement. Adding potassium sulfate, slaked lime and grinding aids during the slag grinding process can further stimulate the activity of slag. These additives can promote chemical reactions between slag and other components in cement, accelerate the hydration process, and improve the early strength and long-term strength of cement; through this grinding and additive treatment, the activity of slag powder can be fully stimulated, so that concrete has a higher hardness after hardening. Due to the high activity of slag, it can partially replace the traditional amount of cement, thereby optimizing the mix ratio of cement. This can not only reduce the amount of cement used and reduce production costs, but also reduce carbon dioxide emissions generated during cement production, which is of environmental significance.
[0039] In this embodiment, the relationship between the length, width and height of the main building block 100 is: the length of the width is equal to the length of the height, and the length is equal to twice the width and the height.
[0040] Specifically, a suitable length, width and height ratio is adopted to facilitate the regular splicing and combination of the main building blocks 100 .
[0041] In this embodiment, the first slots 111 are located on the upper and lower surfaces of the main block 100, and the number of second slots 112 is twelve, of which four are combined in pairs to form a cross arrangement at both ends of the main block 100 and are interconnected with the ends of the first slots 111, and the other eight second slots 112 are respectively combined to form two rings arranged parallel to each other on the surface of the main block 100 and staggered with the first slots 111, and the spacing between the two ring-arranged second slots 112 is equal to the length of the splicing block 200.
[0042] Specifically, the splicing blocks 200 are inserted into the first slots 111 and the second slots 112 on the surface of the main building blocks 100 to realize the mutual splicing between adjacent main building blocks 100, and the construction speed of the building is improved by the split splicing method.
[0043] In this embodiment, the number of plug-ins 210 is four and they are arranged in groups of two on both sides of the splicing block 200 and parallel to each other. Gaps are provided between the plug-ins 210 in the same group, and the spacing between the plug-ins 210 on both sides is equal to twice the height of the plug-ins 210. The surface of the splicing block 200 is provided with a rebar hole 220 that penetrates the splicing block 200.
[0044] Specifically, the surface plug-in 210 of the splicing block 200 is inserted into the first slot 111 and the inner side of the second slot 112 to realize the splicing connection between two adjacent main blocks 100, and the locking and positioning of the splicing state of the entire main block 100 can be realized by inserting steel bars and other structures through the anchor hole 220.
[0045] In this embodiment, the outer covering layer 102 is located on the outer periphery of the inner core 101 and has a thickness of 1-2 cm, and the hardening layer 103 is located on the outer periphery of the outer covering layer 102 and has a thickness of 0.3-0.5 cm.
[0046] Specifically, a layer of polyurethane paint is coated on the surface of the outer coating 102 after the dust removal operation, and the polyurethane coating is cured to form a hardened layer 103 structure to improve the surface hardness and wear resistance of the main block 100. The working principle and use process of the present invention are as follows:
[0047] During the construction of the concrete component, the main blocks 100 are mutually constructed according to the design of the building shape, and the adjacent main blocks 100 are spliced and joined by inserting the splicing blocks 200 through the first slots 111 and the second slots 112 on the surface of the main blocks 100. Reinforcing bars can be inserted into the rebar holes 220 on the surface of the splicing blocks 200 to connect the main blocks 100 to an integrated structure and lock them. After the construction is completed, concrete is poured into the rebar holes 220 to connect the inserted rebars to the splicing blocks 200 to form an integrated structure. After curing, the connection strength of the two is increased to completely fix the splicing structure of the main blocks 100.
[0048] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A low-viscosity ultra-high-strength concrete component, It is characterized in that include: A main structure block (100) and a splicing block (200), wherein a splicing groove (110) and a lug groove (120) are provided on the surface of the main structure block (100), and an insert (210) is provided on the surface of the splicing block (200), wherein the splicing groove (110) comprises a first slot (111) and a second slot (112), wherein the length of the first slot (111) is twice the length of the second slot (112), and the length of the splicing block (200) is less than or equal to the length of the second slot (112), and both ends of the first slot (111) and the second slot (112) are provided with entrance grooves (113) for inserting the splicing block (200), and the cross-sectional shapes of the first slot (111) and the second slot (112) are adapted to the cross-sectional shapes of the splicing block (200) and the insert (210); The main structural block (100) comprises an inner core (101), an outer covering layer (102) and a hardened layer (103); the inner core (101) is formed by pouring foamed concrete, the outer covering layer (102) is formed by pouring non-foamed concrete, and the hardened layer (103) is a polyurethane paint coating.
2. A low-viscosity ultra-high-strength concrete component according to claim 1, It is characterized in that The outer coating (102) comprises the following raw materials in weight percentage: Cement: 30%-50%, fine aggregate: 20%-40%, coarse aggregate: 10%-30%, water: 5%-15%, superplasticizer: 0.5%-5%, mineral admixture: 5%-20%, fiber reinforcement material: 0.1%-2%; wherein the inner core (101) is further added with a foaming agent: 1%-5% in the raw materials of the weight percentage.
3. A low-viscosity ultra-high-strength concrete component according to claim 2, It is characterized in that The cement is high-performance silicate cement, the fine aggregate is sand with a particle size of less than 5 mm, the coarse aggregate is crushed stone or mineral particles with a particle size between 5 mm and 20 mm, the superplasticizer is a polycarboxylic acid-based high-efficiency water reducer, the mineral admixture includes one or more of fly ash, silica fume and slag powder, and the fiber reinforcement material is polypropylene fiber or steel fiber.
4. A low-viscosity ultra-high-strength concrete component according to claim 3, It is characterized in that The fine aggregate is processed by grinding slag to destroy the glassy crystal structure of the slag and fully stimulate the activity of the slag, thereby improving the strength of slag cement. Potassium sulfate, slaked lime and grinding aids are added during the slag grinding process to increase the reaction activity and strength, fully stimulate the activity of slag powder, and improve the hardness of cement after hardening.
5. A low-viscosity ultra-high-strength concrete component according to claim 1, It is characterized in that The relationship between the length, width and height of the main building block (100) is: the length of the width is equal to the length of the height, and the length is equal to twice the width and the height.
6. A low-viscosity ultra-high-strength concrete component according to claim 1, It is characterized in that The first slots (111) are located on the upper and lower surfaces of the main block (100); the number of the second slots (112) is twelve, four of which are combined in pairs to form a cross and arranged at both ends of the main block (100) and are interconnected with the ends of the first slots (111); the other eight second slots (112) are respectively combined to form two rings and arranged parallel to each other on the surface of the main block (100) and staggered with the first slots (111); the spacing between the two ring-arranged second slots (112) is equal to the length of the splicing block (200).
7. The low-viscosity ultra-high-strength concrete component according to claim 1, It is characterized in that The number of the plug-ins (210) is four and they are arranged in groups of two on both sides of the splicing block (200) and are arranged parallel to each other. Gaps are provided between the plug-ins (210) in the same group, and the spacing between the plug-ins (210) on both sides is equal to twice the height of the plug-ins (210). The surface of the splicing block (200) is provided with a rebar hole (220) that penetrates the splicing block (200).
8. The low-viscosity ultra-high-strength concrete component according to claim 1, It is characterized in that The outer coating layer (102) is located on the outer periphery of the inner core (101) and has a thickness of 1-2 cm. The hardening layer (103) is located on the outer periphery of the outer coating layer (102) and has a thickness of 0.3-0.5 cm.
Citation Information
Patent Citations
Explosion-proof heat-preservation multifunctional sheet material of foaming concrete sandwich and preparation method of material
CN102747789A
Self-compacting ultrahigh-strength concrete material and preparation method thereof
CN117534391A
Autoclaved aerated concrete plate
CN221143259U
Spliced concrete block
CN221321454U