Deep rare metal supercritical CO2 fracturing rock mass integrated mining method
Through intelligent sorting of rock mass and crushed substances caused by supercritical CO2 jets, combined with CO2 mineralization treatment, an integrated deep rare metal mining method is formed, which solves the problems of low mining efficiency and environmental pollution in deep rare metals, and achieves high efficiency Resource utilization and environmental protection.
Patent Information
- Application Number
- CN202411209644.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-12
AI Technical Summary
The mining efficiency of deep rare metals is low, has serious environmental damage and large CO2 emissions. The separate implementation of traditional mining methods leads to prolonging production cycles, waste of resources and environmental pollution problems.
Using supercritical CO2 jet cracking rock mass, intelligent sorting of crushed objects and CO2 mineralization treatment, an integrated green mining system is formed, and the CO2 recovery and mineral waste are converted into gelled materials for backfill, achieving efficient resource utilization and environmental protection. .
It improves the efficiency of deep rare metal mining, reduces CO2 emissions, realizes the dual protection of sustainable resources and environment, and forms a complete, closed-loop environmental protection system.
Smart Images

Figure CN118933775A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of deep rare metal mining, and in particular to a deep rare metal supercritical CO2 fractured rock mass integrated mining method. Background Art
[0002] In the field of deep rare metal mining, traditional mining technology usually faces many challenges, including low mining efficiency, serious environmental damage and large CO2 emissions. Specifically, the mining of deep ore bodies is difficult, and conventional mechanical crushing technology is difficult to implement effectively, resulting in a low extraction rate of rare metal resources. At the same time, traditional mining methods are often accompanied by a large amount of CO2 emissions, and how to recycle and treat it has become a major problem for environmental protection. In addition, mine waste treatment and backfilling of goafs are also issues that need to be urgently addressed in current mining.
[0003] In traditional mining, mining, mineral processing and backfilling are usually carried out separately. The connection between each stage takes a lot of time, which prolongs the production cycle and reduces the overall efficiency. Traditional mineral processing methods such as crushing, screening, grinding and mineral processing are inefficient in the process of deep ore mining. The application of intelligent sorting technology is not yet mature. The separation efficiency of rare metal ores and impurity rocks in the crushed rock fragments is low, resulting in serious waste of resources. At the same time, if the large amount of waste rock and tailings generated during the mining process are not handled in time, they will accumulate on the surface to form tailings piles, causing environmental pollution and safety hazards.
[0004] Therefore, there is an urgent need for an emerging technology that can improve the efficiency of deep rare metal mining, achieve effective CO2 recovery and treatment, and combine mining, selection, and filling to solve the above-mentioned problems. Summary of the invention
[0005] In view of the technical problems that the existing deep rare metal mining has low efficiency, serious environmental damage and large CO2 emissions, mining, ore dressing and backfilling are usually carried out separately in mining, and the connection between each stage takes a lot of time, which prolongs the production cycle and reduces the overall efficiency, the present invention provides a deep rare metal supercritical CO2 fractured rock integrated mining method.
[0006] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0007] A method for integrated mining of deep rare metal supercritical CO2 fractured rock mass, comprising the following steps:
[0008] S1. Supercritical CO2 jet fracturing rock mass: CO2 is introduced from a CO2 tanker into a pressurizing and heating unit to reach a supercritical state, then introduced into a drilling rig through a CO2 input pipeline, and then a supercritical CO2 jet is ejected through a Laval nozzle to the mining area to fracture the rock mass. To prevent CO2 from escaping, a surrounding barrier is pre-laid on the working face, and a CO2 recovery device is started while breaking the rock, and the CO2 is recovered to a CO2 mineralization reactor through a CO2 recovery pipeline;
[0009] S2. Intelligent sorting of broken materials: In the sorting area, machine learning image recognition technology is used to scan and identify the rock fragments after fracture in real time, and rare metal ores and impurity ores are quickly distinguished. The sorted rare metal ores are transported to the metal ore purification workshop through the metal ore conveying tunnel for further refining and processing, while the impurity ores are collected as mining waste through the mining waste conveying tunnel to the CO2 mineralization reactor and used as mineralization backfill raw materials;
[0010] S3, CO2 mineralization treatment: In the CO2 mineralization reactor, the waste is ground and evenly mixed with ammonium nitrate for molten salt activation, the waste raw materials are converted into corresponding metal nitrates and the ammonia generated during the activation process is collected, the metal nitrate activated mixture is treated by water leaching, and the water leaching slag with SiO2 as the main component and Ca-rich slag is obtained by filtration. 2+ Mg 2+ 、Al 3+ The water extract is obtained; the collected ammonia gas, the obtained water extract and the CO2 recovered in the CO2 mineralization reactor in step S1 are introduced into a reaction vessel to undergo a carbonation reaction, and filtered to obtain a filtrate containing ammonium nitrate and mineralized slag whose main phases are CaCO3, MgCO3 and Al2(CO3)3; the mineralized slag, cement, gypsum and calcium oxide are mixed to form a cementitious material, and the cementitious material is mixed with water and whole tailings and stirred, and mineral powder is added to form a cementitious filling material;
[0011] S4. Backfill the goaf: The mineralized cemented filling material is transported through the filling material tunnel fluid into the backfill area to backfill the goaf, which plays a role in supporting and stabilizing the underground structure.
[0012] Furthermore, in step S3, the particle size of the ground mineral waste is 50 to 150 μm, the ground mineral waste is evenly mixed with ammonium nitrate in a mass ratio of 1:4 to 1:6, the temperature of molten salt activation is 250 to 450° C., the time of molten salt activation is 40 to 90 min, and during the molten salt activation process, the ambient humidity is maintained at 10 to 20% to promote the formation of nitrate.
[0013] Furthermore, in step S3, the solid-liquid ratio of the water immersion treatment is 1:4 to 1:7, and the unit of the solid-liquid ratio is g / ml; the temperature of the water immersion treatment is 30 to 90° C., and the time of the water immersion treatment is 10 to 90 min.
[0014] Furthermore, in step S3, the CO2 flow rate into the reaction container is 0.2-0.8 L / min, the ammonia concentration is 0.1-0.3 mol / L, the mineralization temperature of the carbonation reaction is 20-90°C, the mineralization time is 90-120 min, and the CO2 partial pressure is 0.5-1.5 MPa.
[0015] Furthermore, in step S3, the mass proportions of mineralized slag, cement, gypsum and calcium oxide are 74%, 10%, 13% and 3% respectively.
[0016] Furthermore, in step S3, the mass ratio of the cementitious material, water, whole tailings and mineral powder is 1:0.55:6:3, and the concentration of the prepared cementitious filling material is 68-72%.
[0017] Compared with the prior art, the integrated mining method of deep rare metal supercritical CO2 fracturing rock mass provided by the present invention proposes a comprehensive solution. Through integrated technologies such as supercritical CO2 jet fracturing rock mass, intelligent sorting of broken materials, CO2 mineralization of solid ore waste and backfilling of goaf areas, a complete, closed-loop green mining and environmental protection system is formed, achieving the dual goals of environmental protection and efficient utilization of resources, and providing innovative solutions for the sustainable development of deep rare metal resources, with high mining efficiency, less damage to the environment and low CO2 emissions. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a schematic diagram of the process of the deep rare metal supercritical CO2 fractured rock mass integrated mining method provided by the present invention.
[0019] Figure 2 It is a schematic diagram of the working section of the deep rare metal supercritical CO2 rock fracturing integrated treatment provided by the present invention.
[0020] In the figure, 1. Mining area; 2. CO2 tanker; 3. Pressurization and heating unit; 4. CO2 input pipeline; 5. Drilling rig; 6. CO2 recovery device; 7. CO2 recovery pipeline; 8. CO2 mineralization reactor; 9. Sorting area; 10. Metal ore transportation tunnel; 11. Metal ore purification workshop; 12. Mine waste transportation tunnel; 13. Filling material transportation tunnel; 14. Backfill area. DETAILED DESCRIPTION
[0021] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further described below with reference to specific diagrams.
[0022] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0023] Please refer to Figure 1 and Figure 2 As shown, the present invention provides a deep rare metal supercritical CO2 fractured rock mass integrated mining method, comprising the following steps:
[0024] S1. Supercritical CO2 jet fracturing of rock mass: CO2 is introduced from the CO2 tanker 2 into the existing pressurization and heating unit 3 to reach the supercritical state, and then introduced into the drilling rig 5 through the CO2 input pipeline 4, and then the supercritical CO2 jet is ejected through the Laval nozzle to the mining area 1 to fracture the rock mass. In order to prevent CO2 from escaping, a surrounding barrier is pre-laid on the working face, and the existing CO2 recovery device 6 is started while breaking the rock, and it is recovered to the CO2 mineralization reactor 8 through the CO2 recovery pipeline 7 to reduce CO2 emissions to the atmosphere; wherein, the jet velocity ejected from the Laval nozzle can reach supersonic speed, and the jet fracturing range of the rock mass can reach 8 times the nozzle diameter.
[0025] S2. Intelligent sorting of broken materials: The rock fragments after fracture contain rare metal ores and impurity ores. In the sorting area 9, the existing machine learning image recognition technology is used to scan and identify the rock fragments after fracture in real time, and the rare metal ores and impurity ores are quickly distinguished. The sorted rare metal ores are transported to the metal ore purification workshop 11 through the metal ore conveying tunnel 10 for further refining and processing, while the impurity ores are collected as mining waste through the mining waste conveying tunnel 12 to the CO2 mineralization reactor 8 and used as mineralization backfill raw materials;
[0026] S3, CO2 mineralization treatment: In the CO2 mineralization reactor 8, the waste is ground and evenly mixed with ammonium nitrate for molten salt activation, the waste raw materials are converted into corresponding metal nitrates and the ammonia generated during the activation process is collected, the metal nitrate activated mixture is subjected to water leaching treatment, and the water leaching slag with SiO2 as the main component and Ca-rich slag is obtained by filtration. 2+ Mg 2+ 、Al 3+water extract; the collected ammonia, the obtained water extract and the CO2 (pre-prepared CO2) recovered in the CO2 mineralization reactor in step S1 are introduced into the reaction vessel for carbonation reaction, and filtered to obtain a filtrate containing ammonium nitrate and mineralized slag whose main phases are CaCO3, MgCO3 and Al2(CO3)3; the mineralized slag, cement, gypsum and a trace amount of calcium oxide are mixed to form a cementitious material, the cementitious material is mixed with water and whole tailings, and a small amount of mineral powder is added to form a cementitious filling material;
[0027] S4. Backfilling the goaf: The mineralized cementing filling material is transported through the filling material conveying tunnel 13 into the backfilling area 14 to backfill the goaf, thereby supporting and stabilizing the underground structure. The cementing filling material has a certain pore structure, which can further absorb the CO2 escaped in the goaf, thereby achieving more thorough CO2 storage. In addition, this filling material can enhance the stability of the goaf and prevent surface subsidence and collapse.
[0028] As a specific embodiment, in step S3, the particle size of the ground mineral waste is 50-150 μm, the ground mineral waste is uniformly mixed with ammonium nitrate at a mass ratio of 1:4-1:6, the temperature of molten salt activation is 250-450°C, the time of molten salt activation is 40-90 min, and during the molten salt activation process, the ambient humidity is maintained at 10-20% to promote the generation of nitrate. By adopting the technical solution in this embodiment, the generation and reaction uniformity of metal nitrate can be optimized during the molten salt activation process, the collection efficiency of ammonia can be increased, and the side reactions in the reaction can be effectively controlled, thereby improving the conversion rate of mineral waste and the stability of subsequent treatment.
[0029] As a specific embodiment, the solid-liquid ratio of the water immersion treatment in step S3 is 1:4 to 1:7, and the unit of the solid-liquid ratio is g / ml; the temperature of the water immersion treatment is 30 to 90°C, and the time of the water immersion treatment is 10 to 90 minutes. This can improve the solubility and separation effect of metal ions during the water immersion process, ensure the stability of the components in the water immersion residue and the water immersion liquid, optimize the initial raw materials required for the mineralization reaction, and promote the efficient generation of mineralized products.
[0030] As a specific embodiment, in step S3, the CO2 flow rate introduced into the reaction container is 0.2-0.8 L / min, the ammonia concentration is 0.1-0.3 mol / L, the mineralization temperature of the carbonation reaction is 20-90°C, the mineralization time is 90-120 min, and the CO2 partial pressure is 0.5-1.5 MPa. This can effectively control the rate and conversion efficiency of the carbonation reaction, optimize the utilization of CO2, enhance the effect of the mineralization reaction, generate high-purity mineralized products and improve the overall mineralization efficiency.
[0031] As a specific embodiment, in step S3, the mass proportions of mineralized slag, cement, gypsum and calcium oxide are 74%, 10%, 13% and 3% respectively. The cementitious material obtained thereby can better meet engineering requirements while improving crack resistance and stability.
[0032] As a specific embodiment, the mass ratio of cementitious material, water, whole tailings and mineral powder in step S3 is 1:0.55:6:3, and the concentration of the prepared cementitious filling material is 68-72%. The obtained cementitious filling material has higher strength, more advantageous performance, and can absorb more CO2.
[0033] Compared with the prior art, the integrated mining method of deep rare metal supercritical CO2 fracturing rock mass provided by the present invention proposes a comprehensive solution. Through integrated technologies such as supercritical CO2 jet fracturing rock mass, intelligent sorting of broken materials, CO2 mineralization of solid ore waste and backfilling of goaf areas, a complete, closed-loop green mining and environmental protection system is formed, achieving the dual goals of environmental protection and efficient utilization of resources, and providing innovative solutions for the sustainable development of deep rare metal resources, with high mining efficiency, less damage to the environment and low CO2 emissions.
[0034] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.
Claims
1. A deep rare metal supercritical CO2 fractured rock mass integrated mining method, characterized in that: The following steps are involved: S1. Supercritical CO2 jet fracturing rock mass: CO2 is introduced from a CO2 tanker into a pressurizing and heating unit to reach a supercritical state, then introduced into a drilling rig through a CO2 input pipeline, and then a supercritical CO2 jet is ejected through a Laval nozzle to the mining area to fracture the rock mass. To prevent CO2 from escaping, a surrounding barrier is pre-laid on the working face, and a CO2 recovery device is started while breaking the rock, and the CO2 is recovered to a CO2 mineralization reactor through a CO2 recovery pipeline; S2. Intelligent sorting of broken materials: In the sorting area, machine learning image recognition technology is used to scan and identify the rock fragments after fracture in real time, and rare metal ores and impurity ores are quickly distinguished. The sorted rare metal ores are transported to the metal ore purification workshop through the metal ore conveying tunnel for further refining and processing, while the impurity ores are collected as mining waste through the mining waste conveying tunnel to the CO2 mineralization reactor and used as mineralization backfill raw materials; S3, CO2 mineralization treatment: In the CO2 mineralization reactor, the waste is ground and evenly mixed with ammonium nitrate for molten salt activation, the waste raw materials are converted into corresponding metal nitrates and the ammonia generated during the activation process is collected, the metal nitrate activated mixture is treated by water leaching, and the water leaching slag with SiO2 as the main component and Ca-rich slag is obtained by filtration. 2+ Mg 2+ 、Al 3+ The water extract is obtained; the collected ammonia gas, the obtained water extract and the CO2 recovered in the CO2 mineralization reactor in step S1 are introduced into a reaction vessel to undergo a carbonation reaction, and filtered to obtain a filtrate containing ammonium nitrate and mineralized slag whose main phases are CaCO3, MgCO3 and Al2(CO3)3; the mineralized slag, cement, gypsum and calcium oxide are mixed to form a cementitious material, and the cementitious material is mixed with water and whole tailings and stirred, and mineral powder is added to form a cementitious filling material; S4. Backfill the goaf: The mineralized cemented filling material is transported through the filling material tunnel fluid into the backfill area to backfill the goaf, which plays a role in supporting and stabilizing the underground structure.
2. The deep rare metal supercritical CO2 fractured rock mass integrated mining method according to claim 1 is characterized in that: In step S3, the particle size of the ground mineral waste is 50-150 μm, the ground mineral waste is evenly mixed with ammonium nitrate in a mass ratio of 1:4-1:6, the temperature of molten salt activation is 250-450° C., the time of molten salt activation is 40-90 min, and during the molten salt activation process, the ambient humidity is maintained at 10-20% to promote the generation of nitrate.
3. The deep rare metal supercritical CO2 fractured rock mass integrated mining method according to claim 1 is characterized in that: The solid-liquid ratio of the water immersion treatment in step S3 is 1:4 to 1:7, and the unit of the solid-liquid ratio is g / ml; the temperature of the water immersion treatment is 30 to 90° C., and the time of the water immersion treatment is 10 to 90 minutes.
4. The deep rare metal supercritical CO2 fractured rock mass integrated mining method according to claim 1 is characterized in that: In step S3, the flow rate of CO2 introduced into the reaction container is 0.2-0.8 L / min, the ammonia concentration is 0.1-0.3 mol / L, the mineralization temperature of the carbonation reaction is 20-90°C, the mineralization time is 90-120 min, and the CO2 partial pressure is 0.5-1.5 MPa.
5. The deep rare metal supercritical CO2 fractured rock mass integrated mining method according to claim 1 is characterized in that: In step S3, the mass proportions of mineralized slag, cement, gypsum and calcium oxide are 74%, 10%, 13% and 3% respectively.
6. The deep rare metal supercritical CO2 fractured rock mass integrated mining method according to claim 1 is characterized in that: In step S3, the mass ratio of the cementitious material, water, whole tailings and mineral powder is 1:0.55:6:3, and the concentration of the prepared cementitious filling material is 68-72%.