Optimization design method and device for pressure-bearing plugging effect of well wall reinforcing material
By establishing a prediction model of the formation leakage state before the well wall strengthening construction and analyzing model of the pressure-bearing and sealing effect, combining the dynamic deformation of the cracks and dynamic material filling, the particle size and injection concentration of the well wall strengthening material are optimized, and the well wall in the existing technology is solved. The problems of low success rate of reinforced materials and unreal simulation effects have achieved a more efficient well wall reinforcement and sealing effect.
Patent Information
- Application Number
- CN202310531416.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-11
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-05-11
AI Technical Summary
The existing evaluation methods and optimization design criteria for well wall reinforcement materials cannot meet the on-site demand, resulting in a low success rate of well wall reinforcement materials and the inability to truly simulate the impact of formation high temperature, high pressure and dynamic crack opening on the pressure-bearing and sealing effect. .
Establish a prediction model of the formation leakage state before the well wall reinforcement construction and an analysis model of the pressure-bearing and blocking effect, combining the dynamic deformation of the cracks and dynamic material filling, analyze the pressure-bearing and blocking effect of the well wall reinforcement material before and after the cracks, and optimize the particle size and particle size Inject concentration formula.
It simulates the pressure-bearing sealing situation in the actual state of the formation more realistically, improves the sealing effect and success rate of well wall reinforcement materials, and makes up for the defect that traditional methods cannot consider the impact of material filling characteristics on crack morphology.
Smart Images

Figure CN118940349A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of drilling engineering, and in particular to a method and a device for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material. Background Art
[0002] Wellbore strengthening technology is the main means to prevent well leakage. Since the existing evaluation methods and optimization design criteria for wellbore strengthening materials cannot meet the needs of on-site use, the success rate of the implementation of this technology is relatively low. Therefore, it is urgent to carry out research on the evaluation of the pressure-bearing plugging effect and optimization design methods of wellbore strengthening materials.
[0003] The existing evaluation methods of wellbore reinforcement materials are mainly based on experimental research, using plugging simulation experimental devices to evaluate the plugging and pressure bearing capacity of wellbore reinforcement materials under different fracture characteristics and simulated formation temperature conditions. However, since the simulation experimental devices are all made of steel plates, they cannot simulate the actual conditions of high temperature and high pressure in the actual formation, resulting in limited experimental conditions and unable to simulate the impact of the dynamic opening change of the fracture on the pressure-bearing and plugging effect of the wellbore reinforcement material; in addition, during the filling process of the wellbore reinforcement material, the filtration effect of the fracture wall can improve the squeezing effect of the fracture on the plugging layer. Limited by the experimental conditions, the indoor experimental process is difficult to simulate.
[0004] The existing numerical simulation methods for the plugging effect of wellbore reinforcement materials are mainly based on the particle flow model established by the discrete element method or the fracture propagation model established by the finite element method. The particle flow simulation research conducted by the discrete element method cannot consider the fracture propagation morphology under the influence of rock mechanics, while the fracture propagation simulation research conducted by the finite element method cannot combine the influence of the plugging characteristics of the wellbore reinforcement materials. Therefore, the crack propagation and the plugging process of the wellbore reinforcement materials cannot be combined, and the pressure plugging under the actual formation conditions cannot be truly simulated. Summary of the invention
[0005] In order to solve the above problems, the present invention provides a method and device for optimizing the design of the pressure-bearing plugging effect of well wall reinforcement materials, and provides a computer device and a computer-readable storage medium. The optimization design method and device provided by the present invention fully consider the dynamic characteristics and leakage state of the cracks before the well wall reinforcement construction, establish a prediction model for the leakage state of the formation before the well wall reinforcement construction, and based on the calculation results of the model, establish an analysis model for the pressure-bearing plugging effect after the well wall reinforcement material is filled, and analyze the pressure-bearing plugging effect of the well wall reinforcement material under the action of two processes (front end and back end of the crack plugging); make up for the defect that the traditional well wall reinforcement plugging effect prediction model method cannot consider the influence of the material filling characteristics on the crack morphology, and combine the dynamic deformation of the cracks with the dynamic filling of the materials, so as to more realistically simulate the pressure-bearing plugging situation under the actual state of the formation.
[0006] The first object of the present invention is to provide a method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material, comprising:
[0007] S1: Establish a prediction model for formation leakage status before wellbore strengthening construction;
[0008] According to the formation leakage state prediction model before wellbore strengthening construction, the fracture characteristics and fluid leakage characteristics at different times before construction are calculated;
[0009] S2: Establish a model for analyzing the pressure-bearing and plugging effect of wellbore strengthening materials;
[0010] S3: According to the pressure-bearing plugging effect analysis model of the wellbore strengthening material, and using the leakage characteristics and crack characteristics before construction obtained in S1 as calculation initial values, calculate the changes of the crack characteristics and leakage characteristics after wellbore strengthening at different plugging positions over time;
[0011] S4: According to the changes described in S3, relevant parameters are adjusted, and the amount of wellbore strengthening material and the optimized value of particle size distribution are calculated by reverse calculation in combination with the fluid loss required for plugging;
[0012] The fracture characteristics include the pressure, length and opening in the fracture, and the fluid loss characteristics include the loss amount at any position in the fracture and the total loss amount.
[0013] In an optional embodiment, the method for establishing the formation leakage state prediction model before the wellbore strengthening construction is:
[0014] S101: Obtaining basic parameters including fractures and wellbore reinforcement materials;
[0015] S102: establishing a formation leakage state prediction model before wellbore strengthening construction according to basic parameters and based on the fluid leakage state prediction model of wellbore strengthening materials under different rheological modes;
[0016] The method for establishing the pressure-bearing and plugging effect analysis model of the wellbore strengthening material is as follows:
[0017] S201: Considering the fracture characteristics and fluid loss characteristics obtained in S102, as well as the fluid flow characteristics and filling and plugging factors of the wellbore strengthening material, a calculation model for the pressure inside the fracture after the wellbore strengthening material is filled is established to obtain the change of the pressure inside the fracture over time after filling;
[0018] S202: Based on the relationship between the pressure in the fracture and the fracture aperture obtained in S201 and the continuity equation of the radial flow of the fluid in the fracture, a calculation model for the fracture morphology change after the wellbore strengthening material is established to obtain the change of the fracture length and aperture over time after filling;
[0019] S203: Based on the changing relationship between the wellbore strengthening material concentration and the fracture aperture obtained in S202 and the fact that the injected wellbore strengthening material complies with the mass conservation equation, a calculation model for the particle distribution in the fracture after the wellbore strengthening material is filled is established to obtain the concentration distribution of the wellbore strengthening material in the fracture after filling, the plugging position, the leakage at any position, and the total leakage.
[0020] In an optional embodiment, the basic parameters include the length and aperture of natural fractures in the formation, the plastic viscosity, dynamic shear force and rheological characteristic parameters of the well repair fluid, the wellbore pressure and rock fracture strength parameters, the initial concentration, maximum accumulation concentration, material particle size, permeability and filtration loss of the wellbore strengthening material.
[0021] In an optional embodiment, the rheological mode of the wellbore strengthening material includes a Bingham mode and an HB mode, which respectively form a Bingham mode fluid loss state prediction model and an HB mode fluid loss state prediction model.
[0022] In an optional embodiment, based on the Bingham mode fluid loss state prediction model or the HB mode fluid loss state prediction model, the influence of workover fluid loss and fracture dynamic expansion is coupled to establish a formation loss state prediction model before wellbore strengthening construction.
[0023] In an optional embodiment, the filling and packaging factors of the well wall strengthening material include the concentration distribution and the plugging position of the well wall strengthening material;
[0024] For the flow of lost fluid before the wellbore enhanced plugging position, the rheological mode of the lost fluid is set to a power law flow type with a yield value, and the flow mode conforms to the Poiseuille flow model, and the pressure drop in the fracture from the fracture entrance to the plugging layer position is calculated;
[0025] For the fracture plugging area, the flow pattern of the lost fluid is assumed to conform to Darcy's law, and the pressure drop from the fracture plugging position to the fracture tip is calculated.
[0026] In an optional embodiment, the process of calculating using the formation leakage state prediction model before wellbore strengthening construction in step S1 is:
[0027] Step 1: Set the time step and total duration of the calculation;
[0028] Step 2: Set the pressure distribution in the fracture at the current moment, and calculate the fracture opening and fracture length at the current moment according to the formation leakage state prediction model before well wall strengthening construction;
[0029] Step 3: Recalculate the pressure distribution in the crack according to the functional relationship between the crack length and time, compare it with the set value in step 2, and calculate the pressure distribution error;
[0030] If the error meets the requirement, the next time step is calculated until the crack characteristic parameters and fluid loss characteristic parameters at the last moment of the last time step before construction are calculated;
[0031] If the error does not meet the requirement, the pressure distribution is corrected until the calculation results of two adjacent iterative calculations meet the error requirement.
[0032] In an optional embodiment, in step S3, the method for calculating using the pressure-bearing plugging effect analysis model of the wellbore strengthening material is:
[0033] Step 1: Set the time step and total duration of the calculation;
[0034] Step 2: The crack and leakage characteristic parameters obtained at the last moment before construction are used as the initial values of the calculation of the pressure-bearing plugging effect analysis model of the wellbore strengthening material, and the plugging position is set to calculate the crack characteristic parameters and leakage characteristic parameters after filling;
[0035] Step 3: Calculate the concentration distribution and plugging position of the wellbore strengthening material after filling according to the characteristic parameters of the filled fractures and leakage, compare with the plugging position set in step 2, and calculate the position error;
[0036] If the error is within the range, calculate the fluid loss after enhancement, and calculate the situation of the next time step until the loss at any position of the fracture at the last moment of the last time step after filling, the total loss and fracture characteristics are obtained;
[0037] If the error is not within the range, the blocking position is corrected until the calculation results of two adjacent iterations meet the error requirements.
[0038] In an optional embodiment, in step S4, based on the required leakage amount, the particle size, injection concentration and plugging layer loss coefficient are back-calculated to obtain the amount of wellbore strengthening material added and the optimized value of particle size gradation.
[0039] In an optional embodiment, the particle size of the well wall strengthening material adopts any one of the normal distribution criterion, the log-normal distribution criterion, the Alfred criterion, the RR criterion, the GS criterion, and the Weibull distribution.
[0040] The second object of the present invention is to provide a device for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material, comprising:
[0041] The first model establishment and pre-construction characteristic parameter calculation module is used to establish a formation leakage state prediction model before wellbore reinforcement construction, and calculate the fracture characteristics and fluid leakage characteristics at different times before construction based on the formation leakage state prediction model before wellbore reinforcement construction;
[0042] The second model building module is used to establish a pressure-bearing and plugging effect analysis model of the wellbore strengthening material;
[0043] The module for calculating characteristic parameters after strengthening is used to calculate the change of crack characteristics and leakage characteristics of wellbore strengthening at different plugging positions over time according to the analysis model of the pressure-bearing plugging effect of wellbore strengthening materials, and to use the leakage characteristics and crack characteristics obtained before construction as the initial values for calculation. The third object of the present invention is to provide a computer device, including a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein when the processor executes the computer program, it realizes the optimization design method for the pressure-bearing plugging effect of wellbore strengthening materials as described in any one of the above items.
[0044] The fourth object of the present invention is to provide a computer-readable storage medium having a computer program stored thereon, which, when executed by a processor, implements a method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material as described in any one of the above items.
[0045] Compared with the prior art, the present invention has the following advantages and beneficial effects:
[0046] The optimization design method and device provided by the present invention fully consider the dynamic characteristics and leakage status of cracks before wellbore reinforcement construction, establish a prediction model for the leakage status of formations before wellbore reinforcement construction, and based on the calculation results of the model, establish a pressure-bearing plugging effect analysis model after wellbore reinforcement material filling, and analyze the pressure-bearing plugging effect of wellbore reinforcement materials under the action of the two processes; it makes up for the defect that the traditional wellbore reinforcement plugging effect prediction model method cannot consider the influence of material filling characteristics on crack morphology, combines the dynamic deformation of cracks with the dynamic filling of materials, and thus more realistically simulates the pressure-bearing plugging situation under the actual state of the formation. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] In order to more clearly illustrate the technical solutions of the exemplary embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments. It should be understood that the following drawings only illustrate certain embodiments of the present invention and should not be regarded as limiting the scope. For those of ordinary skill in the art, other relevant drawings can be obtained based on these drawings without creative work. In the drawings:
[0048] Figure 1 A flow chart of a method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material provided by an embodiment of the present invention;
[0049] Figure 2 This is the calculation flow chart of the leakage state prediction model before wellbore strengthening construction;
[0050] Figure 3 A crack propagation model for the wellbore reinforcement construction process;
[0051] Figure 4 Fill the model with wellbore reinforcement material.
[0052] Figure 5 This is the calculation flow chart of the pressure-bearing and plugging effect analysis model of the wellbore strengthening material;
[0053] Figure 6 It is a curve diagram showing the changes of fracture characteristics and leakage characteristics over time before wellbore strengthening;
[0054] Figure 7 It is the curve diagram of total leakage change on the fracture surface after plugging by wellbore strengthening materials;
[0055] Figure 8 This is a curve diagram of crack length changes after wellbore strengthening materials are used for plugging;
[0056] Fig. 9 This is a curve diagram of the change of leakage on the fracture surface after the wellbore strengthening material is plugged;
[0057] Fig.10 This is a curve diagram of pressure distribution changes in the cracks after the wellbore strengthening material is used for plugging;
[0058] Fig.11 It is the curve diagram of the concentration distribution of the well wall strengthening material;
[0059] Fig.12 A diagram of a device for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material provided by an embodiment of the present invention.
[0060] Marks and corresponding parts names in the attached drawings:
[0061] 101 - first model establishment and characteristic parameter calculation module before construction, 102 - second model establishment module, 103 - characteristic parameter calculation module after strengthening. DETAILED DESCRIPTION
[0062] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with embodiments and drawings. The exemplary embodiments of the present invention and their description are only used to explain the present invention and are not intended to limit the present invention.
[0063] In order to solve the problem that it is currently impossible to truly evaluate and optimize the pressure-bearing plugging effect of wellbore strengthening materials in the real environment of the formation, the present invention provides a method for optimizing the design of the pressure-bearing plugging effect of wellbore strengthening materials, comprehensively considering the influence of factors such as fluid loss in the fracture, fracture expansion, fluid flow and solid-phase particle filling, and establishing a wellbore strengthening material pressure-bearing plugging effect analysis model; based on the optimization method theory, an optimization model for parameters such as particle size, injection concentration and filtration coefficient is established. The above model is also used to evaluate the changes in the cumulative leakage, fracture opening and fracture concentration at different plugging positions during the filling process of the wellbore strengthening material; based on the leakage demand, the optimization design of the wellbore strengthening formula is guided.
[0064] Specific optimization design methods, such as Figure 1 The following process is used as shown in:
[0065] S1: Establish a prediction model for formation leakage status before wellbore strengthening construction
[0066] Created using the following method:
[0067] S101: Obtain basic parameters including fractures and wellbore reinforcement materials
[0068] Specifically, the basic parameters of fractures and wellbore reinforcement materials are obtained through field data or indoor experiments to provide initial values for the simulation evaluation method. For example, the length and opening of natural fractures in the formation are obtained through logging data; the plastic viscosity, dynamic shear force and rheological characteristic parameters of the wellbore repair fluid are obtained through rheological test of the wellbore repair fluid; the wellbore pressure and rock fracture strength parameters are obtained based on the well history data and rock mechanics parameter test of the reservoir core; and the initial construction parameters such as the initial concentration of materials, the maximum accumulation concentration, the material particle size, the permeability of the accumulation plugging layer and the filtration loss of the accumulation plugging layer are set through wellbore reinforcement construction.
[0069] S102: According to the basic parameters obtained in S101 and based on the fluid loss state prediction model of the wellbore strengthening material under different rheological modes, a formation loss state prediction model before wellbore strengthening construction is established;
[0070] The rheological modes of wellbore strengthening materials include Bingham mode and HB mode, which respectively form a Bingham mode fluid loss state prediction model and an HB mode fluid loss state prediction model.
[0071] When the rheological mode is the Bingham mode, based on the Bingham mode fluid loss state prediction model, the influence of workover fluid loss and dynamic fracture expansion is coupled to establish a formation loss state prediction model before wellbore strengthening construction. The current fracture characteristics and fluid loss characteristics of the fracture before construction are calculated, including the expansion morphology (crack length, fracture aperture), the pressure in the fracture and the loss situation (the loss situation refers to the loss amount at any position in the fracture and the total loss amount).
[0072] The calculation formula of the crack internal pressure is:
[0073]
[0074] In the formula, p(r) is the pressure inside the fracture, △p is the formation pressure difference, r is the radial distance from a certain position in the fracture to the center of the wellbore, and r w is the wellbore radius, r f is the radial distance from the fracture tip to the wellbore center, n q The calculation formula of the characteristic index fracture aperture for calculating the pressure inside the fracture is:
[0075]
[0076] Where w0 is the initial crack opening, w0=0 for induced cracks and w0>0 for natural cracks. f is the crack fracture strength factor.
[0077] The calculation formula for the leakage at any position in the crack is:
[0078]
[0079] In the formula, q is the leakage at any point, Q is the total leakage, t is the leakage time, is the inverse function of crack length and loss time, C L is the workover fluid loss coefficient, r * is the integral value.
[0080] The calculation formula of total leakage is:
[0081]
[0082] Where w0 is the initial crack opening, r f is the radial distance from the fracture tip to the wellbore center (i.e., fracture length), K f is the crack fracture strength factor, n q Characteristic index for calculating the pressure inside the fracture.
[0083] The formula for calculating the crack length is:
[0084]
[0085]
[0086]
[0087]
[0088] In the formula, τ y is the dynamic shear force of the workover fluid, μp is the plastic viscosity of the workover fluid, C L is the workover fluid loss coefficient, F1, F2 and F3 are the integral parameters of the fracture dynamic length calculation formula, t a (r*) is the inverse function of the leakage time t and the integral value r*.
[0089] When the rheological mode is the HB mode, based on the HB mode fluid loss state prediction model, the influence of workover fluid loss and fracture dynamic expansion is coupled to establish a formation loss state prediction model before wellbore strengthening construction. The current fracture characteristics and fluid loss characteristics of the fracture before construction are calculated, including the expansion morphology (crack length, fracture aperture), the pressure in the fracture and the loss situation (loss amount at any position in the fracture, the total loss amount).
[0090] The calculation formula of the fracture pressure in this model is:
[0091]
[0092] Where △p is the formation pressure difference, m and k are the characteristic coefficients of the rheological parameters of the workover fluid, Q is the total leakage, r f is the crack length, w is the crack opening, τ y is the shear force of the workover fluid, u is the leakage rate at a certain position in the fracture at a certain moment, and r* is the integral value.
[0093] The calculation formula of crack opening is:
[0094]
[0095] Where w0 is the initial crack opening, p(r) is the expression of the pressure distribution in the crack, and K f is the crack fracture strength factor.
[0096] The formula for calculating the crack length is:
[0097]
[0098] The leakage volume can be calculated based on the fracture length, aperture and pressure inside the fracture and substituted into formulas (3) and (4) to obtain the total leakage volume and transient leakage volume.
[0099] Then, according to the formation leakage state prediction model before wellbore strengthening construction established in S1, the fracture characteristics (including fracture length, fracture aperture, and pressure inside the fracture) and fluid leakage characteristics (transient leakage at any position in the fracture and total leakage) at different times before construction are calculated.
[0100] Specifically, the numerical solution method is used to determine the flow of the leakage model before the wellbore strengthening construction. The calculation flow of the leakage state prediction model before the wellbore strengthening construction is as follows: Figure 2shown.
[0101] Depend on Figure 2 It can be seen that before the calculation, the time step and total time of the calculation are set. According to the basic data collected in step S101 and the model established in step S102, the pressure distribution in the crack at the current moment is first assumed, the crack opening at the current moment is calculated, and then the crack length at the current moment is calculated. According to the functional relationship between the crack length and time, the pressure distribution in the crack is recalculated, and the new pressure distribution is compared with the assumed value to obtain the pressure distribution error. If the error meets the requirements, the next time step is calculated until the leakage characteristics and crack characteristics at the last moment of the last time step before construction are calculated, including the crack opening, crack length and total leakage; if the error does not meet the requirements, the pressure distribution is corrected, and the latest calculated pressure distribution in the crack is re-iterated to calculate the crack characteristic parameters until the calculation results of two adjacent iterative calculations meet the error requirements. After the pressure calculation in the crack meets the error, the crack opening, length and total leakage at that moment can be calculated.
[0102] S2: Establish a model for analyzing the pressure-bearing and plugging effect of wellbore reinforcement materials
[0103] The specific methods are as follows:
[0104] S201: Considering the fracture characteristics and fluid loss characteristics obtained in S102, as well as the fluid flow characteristics and filling and plugging factors of the wellbore strengthening material, a calculation model for the pressure inside the fracture after the wellbore strengthening material is established to obtain the change of the pressure inside the fracture over time after filling.
[0105] Specifically, the influence of factors such as fluid loss in the fracture, fracture expansion, fluid flow and wellbore strengthening material filling and plugging is comprehensively considered, and a calculation model for the pressure in the fracture after the wellbore strengthening material is filled is established. Among them, the filling and packaging factors of the wellbore strengthening material include the concentration distribution and plugging position of the wellbore strengthening material.
[0106] Assuming that during the wellbore strengthening process, the cracks expand outward in a circular ring shape, the expansion model is as follows: Figure 3 shown.
[0107] Depend on Figure 3 It can be seen that the fracture has an initial opening w0, and the established model is a transient model. With the increase of injection time, the fracture opening and length continue to expand. The schematic diagram of the fracture after the wellbore strengthening material is filled is as follows: Figure 4 shown.
[0108] For the flow before the wellbore enhanced plugging position, assuming that the rheological mode of the lost fluid is a power law flow type with a yield value, and the flow mode conforms to the Poiseuille flow model, the calculation formula for the pressure drop in the fracture from the fracture entrance to the plugging layer position is:
[0109]
[0110] Where k and m are the characteristic coefficients of rheological parameters of workover fluid under the power law mode with yield value, τ y is the dynamic shear force of the workover fluid under the power law mode with yield value, w is the fracture opening, r is the radial distance from a certain position in the fracture to the center of the wellbore, q is the leakage, r p It is the radial distance from the plugging position to the center of the wellbore.
[0111] For the front end of the fracture plugging area, assuming that the flow pattern conforms to Darcy's law, the pressure drop from the fracture plugging position to the fracture tip is calculated as:
[0112]
[0113]
[0114] In the formula, μ f is the viscosity of the workover fluid filtrate in the fracture plugging layer, k p is the permeability of the fracture sealing layer, q f is the flow rate of the fluid in the plugging layer, w is the fracture opening, r is the radial distance from a certain position in the fracture to the center of the wellbore, c max It is the maximum accumulation concentration of plugging material.
[0115] S202: Based on the relationship between the pressure in the fracture and the fracture aperture obtained in S201 (such as formulas 12, 13, and 14) and the continuity equation of the radial flow of the fluid in the fracture, a calculation model for the fracture morphology change after the wellbore strengthening material is established to obtain the change of the fracture length and aperture over time after filling;
[0116] The calculation equation for crack morphology change is:
[0117]
[0118] Where w0 is the initial crack opening, p is the pressure inside the crack, and K f is the crack fracture strength factor.
[0119] The continuity equation for radial flow is:
[0120]
[0121] In the formula, C L is the filtration coefficient, It is the inverse function of crack length and time.
[0122] S203: Based on the change of the wellbore strengthening material concentration and the fracture aperture obtained in S202 (such as c in formula 14 maxThe relationship between w and the injected wellbore strengthening material conforms to the mass conservation equation, and a particle distribution calculation model in the fracture after the wellbore strengthening material is filled (that is, a plugging agent concentration calculation model) is established. According to the particle distribution in the fracture, the concentration distribution of the wellbore strengthening material in the fracture after filling, the plugging position, the leakage at any position, and the total leakage are obtained.
[0123] At the rear end of the fracture plugging layer, the distribution equation of the wellbore strengthening material concentration along the radial distance within the fracture is as follows:
[0124]
[0125] c(r)=c max ,r p ≤r<r f (18);
[0126] The mass conservation equation of the wellbore reinforcement material is:
[0127]
[0128] Where c0 is the designed wellbore strengthening material injection concentration, c max It is the maximum concentration of the plugging layer formed after the wellbore strengthening material is filled, and q is the leakage at a certain time and position.
[0129] At the same time, based on the model assumptions, calculation boundary conditions such as plugging agent concentration, fracture aperture and pressure distribution within the fracture also need to be determined.
[0130] The concentration boundary condition of the model is: the initial concentration is at the fracture entrance; the fracture aperture boundary condition is: the fracture entrance and the fracture tip are the initial fracture aperture; the fracture entrance pressure is the wellbore pressure, and the fracture tip pressure is the formation pore pressure. The specific boundary conditions are expressed as:
[0131] r p (t) = r w
[0132] r f (t) = r w
[0133] p(r w )=p w
[0134] p(r f )=p p
[0135] c(r w ) = c0 (20);
[0136] Where P p is the formation pore pressure, P wis the wellbore pressure, r w is the wellbore radius, c0 is the initial concentration.
[0137] S3: Based on the pressure-bearing plugging effect analysis model of the wellbore strengthening material established in S2, and using the leakage characteristics and crack characteristics before construction obtained in S1 as the calculation initial values of the pressure-bearing plugging effect analysis model, the changes of the crack characteristics and leakage characteristics after wellbore strengthening at different plugging positions over time are calculated;
[0138] Specifically: adopt numerical solution method to determine the calculation process of the analysis model of the pressure-bearing and plugging effect of wellbore strengthening materials.
[0139] Depend on Figure 5 From the calculation process, we can see that before the calculation, we first set the time step and total duration. The leakage characteristic parameters and fracture characteristic parameters calculated in S1 are used as the initial values (i.e., as initial parameters) of the pressure-bearing plugging effect analysis model. The filling position of the wellbore strengthening material (i.e., the plugging position) is assumed. Based on the fracture pressure calculation model (such as formulas 12, 13, and 14) and the fracture morphology change model (such as formulas 15 and 16) in the effect analysis model, the fracture pressure, leakage and total leakage (such as formulas 3 and 4), fracture opening and fracture length are calculated. Then, according to the fracture characteristics and leakage parameters, the wellbore strengthening material concentration distribution (i.e., the plugging concentration) and the plugging position are calculated based on the particle distribution calculation model in the fracture after filling (such as formulas 17 and 18). The calculated plugging position is compared with the assumed value. If it is within the error range, the leakage is calculated, and all values are used as initial values to calculate the situation in the next time step until the leakage at any position of the crack at the last moment of the last time step after filling, the total leakage, and the crack characteristics are obtained; if the error does not meet the requirements, the calculated crack plugging position is used as the initial value, the plugging position is corrected, and the parameters at that moment are re-iteratively calculated until the error meets the requirements.
[0140] S4: According to the changes of the fracture characteristics and leakage characteristics of the wellbore reinforcement at different plugging positions described in S3 over time, the relevant parameters are adjusted, and the amount of wellbore reinforcement material and the optimized value of particle size distribution are calculated by reverse calculation in combination with the fluid leakage required for plugging;
[0141] Specifically: according to the required loss volume, the particle size, injection concentration and filtration coefficient are calculated inversely to obtain the amount of wellbore strengthening material and the particle size gradation.
[0142] First, the leakage and fracture aperture characteristics before wellbore strengthening are calculated. Then, the influence of the amount of existing wellbore strengthening material, particle size and the filtration coefficient of different particle size gradations on the leakage after wellbore strengthening is calculated. According to the actual leakage reduction demand, the optimal solution that satisfies the following equation is obtained:
[0143] ① After the well wall strengthening construction, the leakage is minimal;
[0144] ② The concentration of the well wall strengthening material used is minimal;
[0145] ③Indoor experimental test shows that the filtration coefficient of the plugging layer of the well wall strengthening material is the smallest;
[0146] ④ The particle size of the wellbore strengthening material adopts the normal distribution criterion, lognormal distribution criterion, Alfred criterion, RR criterion, GS criterion or Weibull distribution;
[0147] The calculation formulas for various particle size distribution models are as follows:
[0148] The calculation formula of Weibull distribution model is as follows:
[0149]
[0150] Where d is the particle size, k is w is the shape factor, λ is the scaling factor, and e is a natural constant.
[0151] The calculation formula of the Gaudin-Schuhmann (GS) model is as follows:
[0152]
[0153] Where y is the cumulative mass fraction of particles smaller than particle size d, d L is the maximum particle size value.
[0154] The Alfred model is improved on the basis of the Gaudin-Schuhmann model. The calculation formula is as follows:
[0155]
[0156] Where, d S is the minimum particle size of the particle system, and n is a model parameter, dimensionless.
[0157] The Rosin-Rammler (RR) model calculation formula is as follows:
[0158]
[0159] Where d is the particle size of any particle, R is the cumulative mass fraction of particles larger than particle size d, and d e is the characteristic particle size, the particle size corresponding to R=0.368, and n is the model parameter, dimensionless.
[0160] The cumulative normal distribution model calculation formula is as follows:
[0161]
[0162] Where F is the cumulative mass fraction of particles not larger than the particle size x, μ is the mean particle size, σ is the standard deviation of the particle size, and x is the particle size of any particle to be solved.
[0163] The log-cumulative normal distribution model calculation formula is as follows:
[0164]
[0165] According to the particle size range of the plugging materials available on site, different particle size characteristic parameters, different addition amounts, and indoor experimental tests are performed on the plugging layer loss coefficient under various conditions to obtain the initial value of the pressure-bearing plugging effect analysis model of the wellbore strengthening material in step S2, and analyze whether the loss amount in each case meets the requirements. Based on the optimal solution that satisfies the above equation, the addition amount and particle size gradation of the wellbore strengthening material are obtained.
[0166] The following are specific embodiments.
[0167] It is assumed that the basic parameters of fractures and wellbore strengthening materials are obtained through field data or indoor experiments to provide initial values for the simulation evaluation method. The rheological mode of the workover fluid is the HB mode, as shown in Table 1.
[0168] Table 1 Simulation parameters before shaft wall strengthening construction
[0169]
[0170]
[0171] According to the parameters in Table 1, the crack characteristics and leakage characteristics before wellbore strengthening construction can be calculated, such as Figure 6 The figure shows the changes of fracture characteristics and leakage characteristics over time before wellbore strengthening.
[0172] according to Figure 6 The calculated fracture characteristics and leakage characteristics are used as initial values to calculate the pressure-bearing and plugging effect of the wellbore strengthening material. The basic parameters of the simulation are shown in Table 2.
[0173] Table 2 Simulation parameters of wellbore strengthening materials
[0174] parameter Numeric Crack length 0.1m Fracture strength factor <![CDATA[2MPa·m 0.5 ]]> Initial crack opening 500μm Pressure difference 5MPa Dynamic shear force 5Pa Rheological characteristic coefficient m 0.5 Rheological characteristic coefficient k 0.6Pa·s Plugging layer filtration coefficient <![CDATA[1.5×10 -6 m·s -0.5 ]]> Initial wellbore strengthening material concentration 0.1 Maximum filling concentration of wellbore strengthening material 0.7 Permeability of sealing layer 10D
[0175] According to the data in Table 2, the fracture characteristics and leakage after wellbore strengthening can be calculated, such as Figure 7 , 8 , 9, 10, and 11 respectively show the changes in the total leakage of the fracture surface after plugging with the wellbore strengthening material, the changes in the fracture length, the changes in the leakage of the fracture surface, the changes in the pressure distribution in the fracture, and the changes in the concentration distribution of the wellbore strengthening material.
[0176] according to Figure 7 , 8 Based on the results of , 9, 10, and 11, the relevant parameters can be adjusted to calculate the influence of different wellbore strengthening material characteristics on the leakage characteristics as shown in Table 3.
[0177] Table 3 Effect of wellbore strengthening material properties on leakage characteristics
[0178]
[0179] According to the optimization design method, the leakage is required to be reduced to 0.2m after the wellbore strengthening. 3 ,Therefore, the optimal design method for wellbore strengthening materials is the normal distribution criterion, the addition amount is 15%, the mean of the matching criterion is 400μm, and the variance is 200μm.
[0180] The embodiment of the present invention fully considers the dynamic characteristics and leakage status of cracks before wellbore reinforcement construction, and based on the calculation results of the model, establishes a calculation model for the leakage characteristics after wellbore reinforcement material filling, and analyzes the pressure-bearing and plugging effect of wellbore reinforcement materials under the action of the two processes; it makes up for the defect that the traditional wellbore reinforcement and plugging effect prediction model method cannot consider the influence of material filling characteristics on crack morphology, and combines the dynamic deformation of cracks with the dynamic filling of materials.
[0181] Embodiment 2:
[0182] The present invention provides a device, and the device described below and the method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material described above can correspond to each other.
[0183] A device for optimizing the design of pressure-bearing and plugging effects of well wall strengthening materials, such as Fig.12 As shown, including:
[0184] The first model establishment and pre-construction characteristic parameter calculation module 101 is used to establish a formation leakage state prediction model before wellbore reinforcement construction, and calculate the fracture characteristics and fluid leakage characteristics at different times before construction based on the formation leakage state prediction model before wellbore reinforcement construction;
[0185] The second model building module 102 is used to build a pressure-bearing plugging effect analysis model of the wellbore strengthening material;
[0186] The post-enhancement characteristic parameter calculation module 103 is used to calculate the changes of the fracture characteristics and leakage characteristics of the wellbore after strengthening at different plugging positions over time based on the pressure-bearing plugging effect analysis model of the wellbore strengthening material, and use the leakage characteristics and crack characteristics obtained before construction as the calculation initial values.
[0187] Embodiment 3:
[0188] The present invention provides a computer device. The computer device described below and the method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material described above can be referred to each other.
[0189] A computer device comprises a memory, a processor and a computer program stored in the memory and executable on the processor, wherein when the processor executes the computer program, a method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material as described in Example 1 is implemented.
[0190] Embodiment 4:
[0191] The present invention provides a computer-readable storage medium. The computer-readable storage medium described below and the method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material described above can be referred to each other.
[0192] A computer-readable storage medium having a computer program stored thereon, wherein when the computer program is executed by a processor, a method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material as described in Example 1 is implemented.
[0193] The processes and methods not mentioned in the present invention are all known technologies or obtained through known technologies and will not be described in detail here.
[0194] It will be appreciated by those skilled in the art that embodiments of the present invention may be provided as methods, devices, or computer program products. Therefore, the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD / ROM, optical storage, etc.) containing computer-usable program codes.
[0195] The present invention is described with reference to flowcharts and / or block diagrams of methods, devices (apparatus), and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0196] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0197] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 A step that specifies a function in one or more boxes.
[0198] The above is only a specific embodiment of the present invention, and cannot be used to limit the scope of the invention. Therefore, the replacement of equivalent components, or equivalent changes and modifications made according to the protection scope of the patent of the present invention, should still fall within the scope of this patent. In addition, the technical features of the present invention can be freely combined with each other, with each other and with each other, and with each other.
Claims
1. A method for optimizing the design of pressure-bearing and plugging effects of wellbore reinforcement materials, characterized in that: include S1: Establish a prediction model for formation leakage status before wellbore strengthening construction; According to the formation leakage state prediction model before wellbore strengthening construction, the fracture characteristics and fluid leakage characteristics at different times before construction are calculated; S2: Establish a model for analyzing the pressure-bearing and plugging effect of wellbore strengthening materials; S3: According to the pressure-bearing plugging effect analysis model of the wellbore strengthening material, and using the leakage characteristics and crack characteristics before construction obtained in S1 as calculation initial values, calculate the changes of the crack characteristics and leakage characteristics after wellbore strengthening at different plugging positions over time; S4: According to the changes described in S3, relevant parameters are adjusted, and the amount of wellbore strengthening material and the optimized value of particle size distribution are calculated by reverse calculation in combination with the fluid loss required for plugging; The fracture characteristics include the pressure, length and opening in the fracture, and the fluid loss characteristics include the loss amount at any position in the fracture and the total loss amount.
2. The method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material according to claim 1, characterized in that: The method for establishing the formation leakage state prediction model before the wellbore strengthening construction is as follows: S101: Obtaining basic parameters including fractures and wellbore reinforcement materials; S102: establishing a formation leakage state prediction model before wellbore strengthening construction according to basic parameters and based on the fluid leakage state prediction model of wellbore strengthening materials under different rheological modes; The method for establishing the pressure-bearing and plugging effect analysis model of the wellbore strengthening material is as follows: S201: Considering the fracture characteristics and fluid loss characteristics obtained in S102, as well as the fluid flow characteristics and filling and plugging factors of the wellbore strengthening material, a calculation model for the pressure inside the fracture after the wellbore strengthening material is filled is established to obtain the change of the pressure inside the fracture over time after filling; S202: Based on the relationship between the pressure in the fracture and the fracture aperture obtained in S201 and the continuity equation of the radial flow of the fluid in the fracture, a calculation model for the fracture morphology change after the wellbore strengthening material is established to obtain the change of the fracture length and aperture over time after filling; S203: Based on the changing relationship between the wellbore strengthening material concentration and the fracture aperture obtained in S202 and the fact that the injected wellbore strengthening material complies with the mass conservation equation, a calculation model for the particle distribution in the fracture after the wellbore strengthening material is filled is established to obtain the concentration distribution of the wellbore strengthening material in the fracture after filling, the plugging position, the leakage at any position, and the total leakage.
3. The method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material according to claim 2, characterized in that: The basic parameters include the length and opening of natural fractures in the formation, the plastic viscosity, dynamic shear force and rheological characteristic parameters of the workover fluid, the wellbore pressure and rock fracture strength parameters, the initial concentration, maximum accumulation concentration, material particle size, permeability and filtration loss of the wellbore strengthening material.
4. The method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material according to claim 2, characterized in that: The rheological modes of wellbore strengthening materials include Bingham mode and HB mode, which respectively form a Bingham mode fluid loss state prediction model and an HB mode fluid loss state prediction model.
5. The method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material according to claim 4, characterized in that: Based on the Bingham mode fluid loss state prediction model or the HB mode fluid loss state prediction model, the influence of workover fluid loss and fracture dynamic expansion is coupled to establish a formation loss state prediction model before wellbore strengthening construction.
6. The method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material according to claim 2, characterized in that: The filling and packaging factors of the well wall strengthening material include the concentration distribution and the plugging position of the well wall strengthening material; For the flow of lost fluid before the wellbore enhanced plugging position, the rheological mode of the lost fluid is set to a power law flow type with a yield value, and the flow mode conforms to the Poiseuille flow model, and the pressure drop in the fracture from the fracture entrance to the plugging layer position is calculated; For the fracture plugging area, the flow pattern of the lost fluid is assumed to conform to Darcy's law, and the pressure drop from the fracture plugging position to the fracture tip is calculated.
7. The method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material according to claim 1, characterized in that: The process of calculating using the formation leakage state prediction model before wellbore strengthening construction in step S1 is as follows: Step 1: Set the time step and total duration of the calculation; Step 2: Set the pressure distribution in the fracture at the current moment, and calculate the fracture opening and fracture length at the current moment according to the formation leakage state prediction model before well wall strengthening construction; Step 3: Recalculate the pressure distribution in the crack according to the functional relationship between the crack length and time, compare it with the set value in step 2, and calculate the pressure distribution error; If the error meets the requirement, the next time step is calculated until the crack characteristic parameters and fluid loss characteristic parameters at the last moment of the last time step before construction are calculated; If the error does not meet the requirement, the pressure distribution is corrected until the calculation results of two adjacent iterative calculations meet the error requirement.
8. The method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material according to claim 7, characterized in that: In step S3, the method for calculating using the pressure-bearing plugging effect analysis model of the wellbore strengthening material is: Step 1: Set the time step and total duration of the calculation; Step 2: The crack and leakage characteristic parameters obtained at the last moment before construction are used as the initial values of the calculation of the pressure-bearing plugging effect analysis model of the wellbore strengthening material, and the plugging position is set to calculate the crack characteristic parameters and leakage characteristic parameters after filling; Step 3: Calculate the concentration distribution and plugging position of the wellbore strengthening material after filling according to the characteristic parameters of the filled fractures and leakage, compare with the plugging position set in step 2, and calculate the position error; If the error is within the range, calculate the fluid loss after enhancement, and calculate the situation of the next time step until the loss at any position of the fracture at the last moment of the last time step after filling, the total loss and fracture characteristics are obtained; If the error is not within the range, the blocking position is corrected until the calculation results of two adjacent iterations meet the error requirements.
9. The method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material according to claim 1, characterized in that: In step S4, according to the required leakage amount, the particle size, injection concentration and plugging layer loss coefficient are back-calculated to obtain the amount of wellbore strengthening material added and the optimized value of particle size gradation.
10. The method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material according to claim 9, characterized in that: The particle size of the wellbore strengthening material adopts any one of the normal distribution criterion, the log-normal distribution criterion, the Alfred criterion, the RR criterion, the GS criterion and the Weibull distribution.
11. A device for optimizing the design of pressure-bearing and plugging effects of well wall strengthening materials, characterized in that: include: The first model establishment and pre-construction characteristic parameter calculation module is used to establish a formation leakage state prediction model before wellbore reinforcement construction, and calculate the fracture characteristics and fluid leakage characteristics at different times before construction based on the formation leakage state prediction model before wellbore reinforcement construction; The second model building module is used to establish a pressure-bearing and plugging effect analysis model of the wellbore strengthening material; The module for calculating characteristic parameters after strengthening is used to analyze the pressure-bearing plugging effect of the wellbore strengthening material according to the model, and uses the leakage characteristics and crack characteristics obtained before construction as the initial calculation values to calculate the changes of the crack characteristics and leakage characteristics after strengthening the wellbore at different plugging positions over time.
12. A computer device comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein when the processor executes the computer program, the method for optimizing the design of the pressure-bearing and plugging effect of a well wall strengthening material as claimed in any one of claims 1 to 10 is implemented.
13. A computer-readable storage medium having a computer program stored thereon, wherein when the computer program is executed by a processor, the method for optimizing the design of the pressure-bearing and plugging effect of a wellbore strengthening material according to any one of claims 1 to 10 is implemented.
Citation Information
Patent Citations
Method for predicting high steep structure stratum leakage velocity before drilling
CN103015996A
Prediction method for fractured formation plugging pressure-bearing capacity
CN110826142A
Indoor simulation evaluation method for well leakage and leaking stoppage
CN110826245A
Drilling fluid leakage prediction method for fissured formation
CN111236925A
Fluid-solid coupling numerical simulation method for evaluating fractured formation well wall strengthening effect
CN112036096A