Method and system for monitoring life cycle of concrete bridge
By constructing an environmentally specific fatigue model and calculating the full life cycle parameters of concrete bridges, the problems of on-time and accuracy of life cycle monitoring of concrete bridges in the existing technology are solved, and scientific monitoring and performance evaluation of bridge structures are achieved.
Patent Information
- Application Number
- CN202410940697.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-11-12
AI Technical Summary
The prior art cannot reflect the life cycle of concrete bridges on time and accurately, especially in the case of high stress cyclic loads and steel bar corrosion, which makes it difficult to effectively monitor fatigue problems.
Using a monitoring method and system, by clarifying the environmental type of concrete bridges (atmospheric environment and coastal environment), obtaining relevant influencing factors (carbonization efficiency and chloride ion content), constructing fatigue models, and calculating the parameters of the whole life cycle, including reinforcement corrosion The situation can achieve scientific and accurate monitoring of the bridge life cycle.
Real and accurate monitoring of the life cycle of concrete bridges is achieved. By scientifically calculating parameters such as reinforcement corrosion, it reflects the service performance of the bridge structure, and provides an effective assessment of the bridge health status.
Smart Images

Figure CN118940358A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of concrete bridge evaluation, and more specifically, relates to a monitoring method and system for the life cycle of a concrete bridge. Background Art
[0002] Concrete bridges are one of the main transportation infrastructures in highway transportation. In recent years, due to the substantial increase in vehicle load levels, the application of high-strength concrete and high-strength steel bars has led to the development of lightweight concrete bridges, which has frequently put in-service concrete bridges in a high-stress state, leading to increasingly prominent fatigue problems for such components during service.
[0003] Nowadays, the limit state design theory with "full utilization of material strength" as the core is increasingly applied in concrete structures. Coupled with the development trend of lightweight and high-strength structures, the working stress of concrete bridges is getting closer and closer to the fatigue stress amplitude in the laboratory. In addition, as the proportion of heavy-load traffic on bridge decks gradually increases, the cyclic load level of concrete bridges continues to increase, and the number of high-stress cycles is also increasing. Therefore, fatigue of concrete bridges has become an important issue that cannot be ignored in engineering design.
[0004] Therefore, there is an urgent need for a monitoring method and system for the life cycle of concrete bridges to truly and accurately reflect the life cycle of bridges. Summary of the invention
[0005] The purpose of the present invention is to provide a monitoring method and system for the life cycle of a concrete bridge, aiming to solve the technical problem in the prior art that the life cycle of the beam of the bridge structure cannot be reflected timely and accurately.
[0006] To achieve the above object, the technical solution adopted by the present invention is: to provide a monitoring method for the life cycle of a concrete bridge, comprising the following steps:
[0007] Clarify the environment in which the concrete bridge is located; the environment includes: atmospheric environment and coastal environment;
[0008] Obtaining influencing factors related to the corrosion of steel bars in a concrete bridge under the environment; the influencing factors include: concrete carbonization efficiency and / or chloride ion content;
[0009] A concrete bridge fatigue model is constructed, and the concrete bridge fatigue model is used to calculate the size of parameters related to the entire life cycle of the concrete bridge.
[0010] Preferably, the concrete bridge fatigue model includes an atmospheric environment sub-model and a coastal environment sub-model; the atmospheric environment sub-model is used to complete the calculation of the steel corrosion condition of the concrete bridge fatigue during the entire life cycle in the atmospheric environment; the coastal environment sub-model is used to complete the calculation of the steel corrosion condition of the concrete bridge fatigue during the entire life cycle in the coastal environment.
[0011] Preferably, the atmospheric environment sub-model includes:
[0012] Calculate the carbonization depth and the time t when carbonization causes the initial rusting of the steel bar;
[0013] Among them, the time t for the initial embroidery of the steel bar is:
[0014]
[0015] Among them, d c represents the thickness of the concrete protective layer, in mm; x0 represents the carbonation residue, in mm; m represents the local environmental coefficient, which is 3.5 for dry environment and 4.0 for wet environment; D c represents the parameters related to the thickness of the protective layer and the carbonization coefficient k. Specifically, when d c ≤28, k≥0.8, D c The value of d c Same. When d c ≤28, k<0.8, D c The value of is d c -0.16 / k; when d c >28, k≥1.0 (k>3.3, k=3.3), D c The value of is d c +0.066(d c -28) 0.47k When d c >28, k<1.0, D c The value of is d c -0.389(d c -28)(0.16 / k) 1.5 .
[0016] Preferably, the atmospheric environment sub-model includes:
[0017] Calculate the rate of steel bar corrosion using the following formula:
[0018]
[0019] Where r1(t) and r2(t) represent the annual average corrosion rate of steel bars before and after the concrete cover cracks (mm / year); K clIt represents the influence coefficient of the steel bar position. The steel bar in the corner area is taken as 1.6, and the steel bar in the non-corner area is taken as 1.0. T and RH represent the annual average temperature (℃) and annual average humidity of the bridge site respectively. When RH>0.8, it is taken as 0.8.
[0020] Preferably, the atmospheric environment sub-model includes:
[0021] Calculate the time for the steel bar protection layer to rust and crack according to the steel bar corrosion depth:
[0022]
[0023] δ cr =0.012(d c / D0)+0.00084f cuk +0.018
[0024] In the formula, δ cr is the critical depth of steel bar corrosion (mm); D0 is the initial steel bar diameter (mm); f cuk It is the standard value of concrete compressive strength (MPa).
[0025] Preferably, the large coastal environment sub-model includes:
[0026] Calculate the relationship between chloride ion concentration, concrete cover thickness and environmental factors, and calculate the critical chloride ion concentration C crit Calculate the steel bar rusting time t init ;
[0027] Obtain the steel bar corrosion rate and steel bar corrosion depth, and calculate the time for the concrete cover to rust and crack;
[0028] According to the crack width of concrete cover and the parameters of steel bar corrosion area loss, a crack width prediction model based on steel bar area loss was constructed.
[0029] Obtain the remaining area and corrosion depth of the steel bars when the concrete component reaches severe cracking.
[0030] Preferably, obtaining the steel bar corrosion rate and steel bar corrosion depth, and calculating the time of rust expansion and cracking of the concrete protective layer comprises:
[0031] The calculation formula for the steel bar corrosion depth is:
[0032]
[0033] Where p(t) is the steel bar corrosion depth (mm); δ ave is the uniform corrosion depth; R is the pitting coefficient, i.e. the maximum pit depth (p max ) and the average pit depth (p mean), R follows an extreme value distribution with location and scale parameters of 6.07 and 1.12 respectively;
[0034] The calculation formula for the critical value of uniform corrosion depth is:
[0035]
[0036] The calculation formula for the time of rust expansion and cracking of concrete cover is:
[0037]
[0038] A monitoring system for the life cycle of a concrete bridge, characterized by comprising:
[0039] An environment acquisition module is used to clarify the environment in which the concrete bridge is located; the environment includes: atmospheric environment and coastal environment;
[0040] An influencing factor module is used to obtain influencing factors related to the corrosion of steel bars in concrete bridges in the environment; the influencing factors include: concrete carbonization efficiency and / or chloride ion content;
[0041] The parameter calculation module is used to construct a concrete bridge fatigue model and use the concrete bridge fatigue model to calculate the parameter sizes related to the entire life cycle of the concrete bridge.
[0042] An electronic device, comprising a bus, a transceiver, a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the transceiver, the memory, and the processor are connected via the bus, wherein the computer program, when executed by the processor, implements the steps in the method for monitoring the life cycle of a concrete bridge as described in any one of the above
[0043] A computer-readable storage medium having a computer program stored thereon, characterized in that when the computer program is executed by a processor, a monitoring method for the life cycle of a concrete bridge as described in any one of the above items is implemented.
[0044] The beneficial effect of the monitoring method and system for the life cycle of a concrete bridge provided by the present invention is that compared with the prior art, the monitoring method and system for the life cycle of a concrete bridge provided by the present invention, from the perspective of the entire life cycle, according to the different external environments in which the concrete bridge is located, by scientifically and accurately calculating parameters such as steel corrosion of the concrete bridge throughout the life cycle, truly and accurately reflects the service performance of the bridge structure, thereby realizing the monitoring of the life cycle of the concrete bridge. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0046] Figure 1 A flow chart of a steel bar corrosion model in the full life cycle of a concrete bridge fatigue provided by an embodiment of the present invention;
[0047] Figure 2 A flowchart of a method for monitoring the life cycle of a concrete bridge provided by an embodiment of the present invention;
[0048] Figure 3 A structural diagram of a monitoring system for the life cycle of a concrete bridge provided in an embodiment of the present invention.
[0049] In the figure: 1. Environment acquisition module; 2. Influencing factor module; 3. Parameter calculation module. DETAILED DESCRIPTION
[0050] In the description of the present invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0051] The "multiple" mentioned in this embodiment refers to two or more. "And / or" describes the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. The words "exemplary" or "for example" are used to indicate examples, illustrations or explanations, and are intended to present related concepts in a specific way, and should not be interpreted as being more preferred or more advantageous than other embodiments or design solutions.
[0052] Please also read Figures 1 to 3 Now, a monitoring method for the life cycle of a concrete bridge provided by the present invention is described. The monitoring method for the life cycle of a concrete bridge comprises the following steps:
[0053] Step S1, clarifying the environment in which the concrete bridge is located; the environment includes: atmospheric environment and coastal environment.
[0054] Step S2, obtaining influencing factors related to the corrosion of steel bars in concrete bridges in the current environment; the influencing factors include: concrete carbonization efficiency and / or chloride ion content.
[0055] In this step, the influencing factors related to the atmospheric environment and the corrosion of steel bars in concrete bridges are obtained, including: the carbonization efficiency of concrete.
[0056] Specifically, in the atmospheric environment, concrete is less likely to be corroded by the outside world, but carbonization of concrete will still cause steel corrosion. The corrosion rate of steel bars in bridges in dry and rainy areas is slower, while the corrosion rate of steel bars in bridges in humid and rainy areas will increase significantly.
[0057] In this step, the influencing factors related to the coastal environment and the corrosion of concrete bridge reinforcement are obtained, including: chloride ion content.
[0058] Specifically, in coastal environments, the carbonation rate of concrete will cause steel corrosion. Another cause of steel corrosion is chloride ion corrosion. And the steel corrosion caused by chloride ion corrosion is much faster than the carbonation rate of concrete. The steel corrosion caused by chloride ion corrosion in concrete bridges in coastal environments is the main disease.
[0059] Step S3: construct a concrete bridge fatigue model, and use the concrete bridge fatigue model to calculate the size of parameters related to the entire life cycle of the concrete bridge.
[0060] In this step, the concrete bridge fatigue model includes an atmospheric environment sub-model and a coastal environment sub-model. The atmospheric environment sub-model is used to complete the calculation of the steel corrosion of the concrete bridge fatigue in the atmospheric environment during the full life cycle. The coastal environment sub-model is used to complete the calculation of the steel corrosion of the concrete bridge fatigue in the coastal environment during the full life cycle.
[0061] In step S3, the construction process of the atmospheric environment sub-model includes the following steps:
[0062] S3.1. Calculate the carbonization depth and the time t when the steel bar is first rusted due to carbonization; where the time t when the steel bar is first rusted is:
[0063]
[0064] Among them, d c represents the thickness of the concrete protective layer, in mm; x0 represents the carbonation residue, in mm; m represents the local environmental coefficient, which is 3.5 for dry environment and 4.0 for wet environment; D c represents the parameters related to the thickness of the protective layer and the carbonization coefficient k. Specifically, when d c ≤28, k≥0.8, D c The value of dc Same. When d c ≤28, k<0.8, D c The value of is d c -0.16 / k; when d c >28, k≥1.0 (k>3.3, k=3.3), D c The value of is d c +0.066(d c -28) 0.47k When d c >28, k<1.0, D c The value of is d c -0.389(d c -28)(0.16 / k) 1.5 .
[0065] The calculation formula for carbonization depth is:
[0066]
[0067] Among them, x c (t) is the carbonation depth of the concrete structure at time t; k is the coefficient affecting the carbonation rate; K represents the CO2 concentration influence coefficient, with a range of values: urban bridges: 1.2 to 1.4; non-urban bridges: 1.1 to 1.2; kl Indicates the position influence coefficient; the value range is: corner area components: 1.4; non-corner area components: 1.0; K kt Indicates the curing and pouring influence coefficient, and its value is 1.2; K ks Indicates the working stress influence coefficient, the value range is: compression zone components: 1.0; tension zone components: 1.1; K F represents the fly ash replacement coefficient, specifically, K F =1.0+13.34F 3.3 , F is the fly ash replacement amount (weight ratio), and the F of high-density concrete mixed with Class I fly ash and low water-binder ratio is 1.0; T represents the ambient temperature; RH represents the relative ambient humidity.
[0068] S3.2. Calculate the rate of steel bar corrosion using the following formula:
[0069]
[0070] Where r1(t) and r2(t) represent the annual average corrosion rate of steel bars before and after the concrete cover cracks (mm / year); K clIt represents the influence coefficient of the steel bar position. The steel bar in the corner area is taken as 1.6, and the steel bar in the non-corner area is taken as 1.0. T and RH represent the annual average temperature (℃) and annual average humidity of the bridge site respectively. When RH>0.8, it is taken as 0.8.
[0071] S3.3. Calculate the time for the steel bar protection layer to rust and crack according to the steel bar corrosion depth:
[0072]
[0073] δ cr =0.012(d c / D0)+0.00084f cuk +0.018
[0074] In the formula, δ cr is the critical depth of steel bar corrosion (mm); D0 is the initial steel bar diameter (mm); f cuk It is the standard value of concrete compressive strength (MPa).
[0075] In step S3, specifically, the construction process of the coastal environment sub-model includes the following steps:
[0076] Initial stage of rust
[0077] SS3.1. Calculate the relationship between chloride ion concentration, concrete cover thickness and environmental factors, and calculate the critical chloride ion concentration C crit Calculate the steel bar rusting time t init ;
[0078] in,
[0079] Where X1 represents the model uncertainty coefficient, which is log-normally distributed with distribution parameters μ = 1.00, σ = 0.05; D cl (mm 2 / year) represents the chloride ion diffusion coefficient, which is normally distributed with distribution parameters μ=220.9, σ=25.4; k e represents the temperature load factor, which is Gamma distributed, with distribution parameters α=0.676, λ=0.114; k c represents the curing time factor, which is normally distributed with distribution parameters μ=0.80, σ=0.10; k t It represents the test correction factor, which is normally distributed, with distribution parameters μ=0.832; σ=0.024; n cl represents the time factor, which is Beta distributed, with distribution parameters α=4.075, β=9.508;
[0080]
[0081] Critical chloride ion concentration C for steel bar corrosion crit Value
[0082]
[0083] Chloride ion concentration C on the surface of concrete components so Value
[0084] The calculation formula for chloride ion concentration is:
[0085]
[0086] Where x is the penetration depth of chloride ions; t is the time when the bridge is completed and opened to traffic (year); C so is the chloride ion concentration on the component surface; d c is the thickness of the concrete cover; k e is the temperature load factor; k c is the curing time factor; k t is the test correction factor; D app is the apparent diffusion coefficient of chloride ions; D cl is the chloride ion diffusion coefficient; t0 is the reference time, which is generally taken as 28 days (0.0767 years); n cl is the time factor; erf(·) is the Gaussian error function.
[0087] Corrosion development stage. The type of chloride ion corrosion of steel bars belongs to pitting corrosion. Because the environment of reinforced concrete structure bridges in coastal environments is relatively complex, in the early stage of corrosion, as the corrosion process deepens, corrosion products begin to be produced, blocking the input of O2, H2O and Cl-, and the corrosion rate gradually decreases; when the concrete protective layer cracks, air, moisture and chlorides are more likely to enter, and the corrosion rate of the steel bars will be greatly increased; when the concrete reaches a critical cracking state (severe cracking), more corrosion products accumulate, and air and moisture will find it difficult to reach the surface of the steel bars. At this time, the corrosion rate of the steel bars will gradually decrease slowly. Therefore, the steel bar corrosion rate in the corrosion development stage is divided into three stages.
[0088] SS3.2, obtain the steel corrosion rate and steel corrosion depth, and calculate the time of rust expansion and cracking of the concrete cover;
[0089] In this step, the steel bar corrosion rate is divided into three stages: the initial corrosion stage, the concrete cover rust expansion cracking stage, and the concrete severe cracking stage. The calculation formulas for the three stages are:
[0090]
[0091] w / c=27 / (f cuk +13.5)
[0092] In the formula, i corr,0 is the corrosion current density at the beginning of the corrosion stage (μA / cm2); w / c is the water-cement ratio.
[0093] The calculation formula for the steel bar corrosion depth is:
[0094]
[0095] Where p(t) is the steel bar corrosion depth (mm); δ ave is the uniform corrosion depth; R is the pitting coefficient, i.e. the maximum pit depth (p max ) and the average pit depth (p mean ), R follows an extreme value distribution with location and scale parameters of 6.07 and 1.12 respectively.
[0096] The calculation formula for the critical value of uniform corrosion depth is:
[0097]
[0098] The calculation formula for the time of rust expansion and cracking of concrete cover is:
[0099]
[0100] SS3.3. According to the crack width of the concrete cover and the steel bar corrosion area loss parameters, a crack width prediction model based on steel bar area loss is constructed:
[0101] W(t)=K(ΔA(t)-ΔA(t cr ))
[0102] Where W(t) is the crack width of the concrete cover at time t (mm); K is the regression coefficient, which is taken as 0.0575; ΔA(t) is the area reduced by steel corrosion at time t (mm 2 ); ΔA(t cr ) is the area of steel bar corrosion reduction when the concrete cover expands and cracks (mm 2 ).
[0103] SS3.4. Obtain the remaining area and corrosion depth of the steel bars when the concrete component reaches severe cracking, and obtain the following formula:
[0104] A(t det )=A0-ΔA(t cr )-3.478
[0105]
[0106] In the formula, A(t det )、P(t det) are the remaining area of steel bars and the corrosion depth when the concrete is severely cracked, where ΔA(t det )=3.478. The maximum permissible crack width of reinforced concrete components and prestressed concrete type B components is 0.2mm.
[0107] Compared with the prior art, the present invention provides a monitoring method and system for the life cycle of a concrete bridge. From the perspective of the entire life cycle, based on the different external environments in which the concrete bridge is located, the present invention scientifically and accurately calculates parameters such as steel corrosion throughout the life cycle of the concrete bridge, truly and accurately reflects the service performance of the bridge structure, and thus realizes the monitoring of the life cycle of the concrete bridge.
[0108] The present invention also provides a monitoring system for the life cycle of concrete bridges. Figures 1 to 3 The monitoring system for the life cycle of a concrete bridge comprises: an environment acquisition module 1, an influencing factor module 2, and a parameter calculation module 3. The environment acquisition module 1 is used to clarify the environment in which the concrete bridge is located; the environment includes: atmospheric environment and coastal environment; the influencing factor module 2 is used to obtain influencing factors related to the corrosion of steel bars of the concrete bridge in the environment; the influencing factors include: the carbonization efficiency of concrete and / or the chloride ion content; the parameter calculation module 3 is used to construct a fatigue model of the concrete bridge, and use the fatigue model of the concrete bridge to calculate the parameter size related to the entire life cycle of the concrete bridge.
[0109] In addition, an embodiment of the present invention also provides an electronic device, including a bus, a transceiver, a memory, a processor, and a computer program stored in the memory and executable on the processor. The transceiver, the memory, and the processor are respectively connected via a bus. When the computer program is executed by the processor, each process of the above-mentioned embodiment of a monitoring method for the life cycle of a concrete bridge is implemented, and the same technical effect can be achieved. To avoid repetition, it will not be described here.
[0110] In addition, an embodiment of the present invention also provides a computer-readable storage medium on which a computer program is stored. When the computer program is executed by a processor, the various processes of the above-mentioned embodiment of a monitoring method for the life cycle of a concrete bridge are implemented, and the same technical effect can be achieved. To avoid repetition, it will not be repeated here.
[0111] Computer readable storage media include: permanent and non-permanent, removable and non-removable media, which are tangible devices that can retain and store instructions for use by instruction execution devices. Computer readable storage media include: electronic storage devices, magnetic storage devices, optical storage devices, electromagnetic storage devices, semiconductor storage devices, and any suitable combination of the above. Computer readable storage media include: phase change memory (PRAM), static random access memory (SRAM), dynamic random access memory (DRAM), other types of random access memory (RAM), read-only memory (ROM), non-volatile random access memory (NVRAM), electrically erasable programmable read-only memory (EEPROM), flash memory or other memory technology, compact disk read-only memory (CD-ROM), digital versatile disk (DVD) or other optical storage, magnetic cassette storage, magnetic tape disk storage or other magnetic storage devices, memory sticks, mechanical encoding devices (such as punched cards or raised structures in grooves with instructions recorded thereon) or any other non-transmission medium that can be used to store information that can be accessed by a computing device. As defined in the embodiments of the present invention, computer-readable storage media do not include temporary signals themselves, such as radio waves or other freely propagating electromagnetic waves, electromagnetic waves propagating through waveguides or other transmission media (such as light pulses passing through fiber optic cables), or electrical signals transmitted through wires.
[0112] In the several embodiments provided in the present application, it should be understood that the disclosed devices, electronic devices and methods can be implemented in other ways. For example, the device embodiments described above are only schematic. For example, the division of the modules or units is only a logical function division. There may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. In addition, the mutual coupling or direct coupling or communication connection shown or discussed can be an indirect coupling or communication connection through some interfaces, devices or units, or it can be an electrical, mechanical or other form of connection.
[0113] The units described as separate components may or may not be physically separated, and the components shown as units may or may not be physical units, and may be located in one location or distributed over multiple network units. Some or all of the units may be selected according to actual needs to solve the problem to be solved by the embodiments of the present invention.
[0114] In addition, each functional unit in each embodiment of the present invention may be integrated into one processing unit, or each unit may exist physically separately, or two or more units may be integrated into one unit. The above integrated unit may be implemented in the form of hardware or in the form of software functional units.
[0115] If the integrated unit is implemented in the form of a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. Based on this understanding, the technical solution of the embodiment of the present invention is essentially or part of the contribution to the prior art, or all or part of the technical solution can be embodied in the form of a software product, which is stored in a storage medium and includes several instructions for a computer device (including: a personal computer, a server, a data center or other network device) to perform all or part of the steps of the method described in each embodiment of the present invention. The above-mentioned storage medium includes various media that can store program codes as listed above.
[0116] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any technical solution that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be based on the protection scope of the claims.
[0117] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for monitoring the life cycle of a concrete bridge, characterized in that: The following steps are involved: Identify the environment in which the concrete bridge is located; The environment includes: atmospheric environment and coastal environment; Obtaining influencing factors related to the corrosion of steel bars in a concrete bridge under the environment; the influencing factors include: concrete carbonization efficiency and / or chloride ion content; A concrete bridge fatigue model is constructed, and the concrete bridge fatigue model is used to calculate the size of parameters related to the entire life cycle of the concrete bridge.
2. A method for monitoring the life cycle of a concrete bridge as claimed in claim 1, characterized in that: The concrete bridge fatigue model includes an atmospheric environment sub-model and a coastal environment sub-model; the atmospheric environment sub-model is used to complete the calculation of the steel corrosion situation of the concrete bridge fatigue in the atmospheric environment during the entire life cycle; the coastal environment sub-model is used to complete the calculation of the steel corrosion situation of the concrete bridge fatigue in the coastal environment during the entire life cycle.
3. A method for monitoring the life cycle of a concrete bridge as claimed in claim 2, characterized in that: The atmospheric environment sub-model includes: Calculate the carbonization depth and the time t when carbonization causes the initial rusting of the steel bar; Among them, the time t for the initial embroidery of the steel bar is: Among them, d c represents the thickness of the concrete protective layer, in mm; x0 represents the carbonation residue, in mm; m represents the local environmental coefficient, which is 3.5 for dry environment and 4.0 for wet environment; D c represents the parameters related to the thickness of the protective layer and the carbonization coefficient k. Specifically, when d c ≤28, k≥0.8, D c The value of d c Same. When d c ≤28, k<0.8, D c The value of is d c -0.16 / k; when d c >28, k≥1.0 (k>3.3, k=3.3), D c The value of is d c +0.066(d c -28) 0.47k When d c >28, k<1.0, D c The value of is d c -0.389(d c -28)(0.16 / k) 1.5 .
4. A method for monitoring the life cycle of a concrete bridge as claimed in claim 3, characterized in that: The atmospheric environment sub-model includes: Calculate the rate of steel bar corrosion using the following formula: Where r1(t) and r2(t) represent the annual average corrosion rate of steel bars before and after the concrete cover cracks (mm / year); K cl It represents the influence coefficient of the steel bar position. The steel bar in the corner area is taken as 1.6, and the steel bar in the non-corner area is taken as 1.
0. T and RH represent the annual average temperature (℃) and annual average humidity of the bridge site respectively. When RH>0.8, it is taken as 0.
8.
5. A method for monitoring the life cycle of a concrete bridge as claimed in claim 4, characterized in that: The atmospheric environment sub-model includes: Calculate the time for the steel bar protection layer to rust and crack according to the steel bar corrosion depth: d cr =0.012(d c / D0)+0.00084f cuk +0.018 In the formula, δ cr is the critical depth of steel bar corrosion; D0 is the initial steel bar diameter; f cuk It is the standard value of concrete compressive strength.
6. A method for monitoring the life cycle of a concrete bridge as claimed in claim 5, characterized in that: The large coastal environment sub-model includes: Calculate the relationship between chloride ion concentration, concrete cover thickness and environmental factors, and calculate the critical chloride ion concentration C crit Calculate the steel bar rusting time t init ; Obtain the steel bar corrosion rate and steel bar corrosion depth, and calculate the time for the concrete cover to rust and crack; According to the crack width of concrete cover and the parameters of steel bar corrosion area loss, a crack width prediction model based on steel bar area loss was constructed. Obtain the remaining area and corrosion depth of the steel bars when the concrete component reaches severe cracking.
7. A method for monitoring the life cycle of a concrete bridge as claimed in claim 6, characterized in that: The method of obtaining the steel bar corrosion rate and steel bar corrosion depth, and calculating the time of rust expansion and cracking of the concrete protective layer comprises: The calculation formula for the steel bar corrosion depth is: Where p(t) is the steel bar corrosion depth (mm); δ ave is the uniform corrosion depth; R is the pitting coefficient, i.e. the maximum pit depth (p max ) and the average pit depth (p mean ), R follows an extreme value distribution with location and scale parameters of 6.07 and 1.12 respectively; The calculation formula for the critical value of uniform corrosion depth is: The calculation formula for the time of rust expansion and cracking of concrete cover is:
8. A monitoring system for the life cycle of a concrete bridge, characterized in that: include: An environment acquisition module (1) is used to identify the environment in which the concrete bridge is located; The environment includes: atmospheric environment and coastal environment; The influencing factor module (2) is used to obtain influencing factors related to the corrosion of steel bars in concrete bridges in the environment; the influencing factors include: concrete carbonization efficiency and / or chloride ion content; The parameter calculation module (3) is used to construct a concrete bridge fatigue model and use the concrete bridge fatigue model to calculate the size of parameters related to the entire life cycle of the concrete bridge.
9. An electronic device, comprising a bus, a transceiver, a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the transceiver, the memory, and the processor are connected via the bus, wherein: When the computer program is executed by the processor, the steps of the method for monitoring the life cycle of a concrete bridge as claimed in any one of claims 1 to 7 are implemented.
10. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the computer program is executed by a processor, a monitoring method for the life cycle of a concrete bridge as described in any one of claims 1 to 7 is implemented.
Citation Information
Cited By
Numerical simulation method considering influence of carbonization on reinforced concrete performance
CN119150637A
Method and system for calculating degradation process of welding stud connecting piece of composite beam bridge