Tungsten diselenide two-dimensional radio frequency switch and preparation method thereof
By adopting high electron mobility tungsten diselenide two-dimensional material and advanced preparation technology in RF switches, the performance limitations of RF switches in high-frequency applications are solved, and the high-frequency performance and ultra-high-speed switching capabilities are improved. The material and structure of the RF switch.
Patent Information
- Application Number
- CN202411117613.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-12
AI Technical Summary
Existing RF switches have high insertion losses, lower switching speeds and poor linearity in high-frequency applications, limiting their application in high-frequency bands, and the application of two-dimensional materials in RF switches has not yet reached commercial level. Chemical demand is mainly due to the technical bottlenecks and immature preparation technology of materials under high-frequency operation.
The two-dimensional tungsten diselenide material with high electron mobility is used as the radio frequency signal switching functional layer, combined with the electron beam exposure system and thermal evaporation process, the patterned bottom electrode and top electrode are accurately prepared, and nano-layered diselenide is prepared by mechanical peeling method. Tungsten chemical significantly improves the operating frequency and performance stability of RF switches.
It significantly improves the high-frequency performance and ultra-high-speed switching capabilities of RF switches, achieves good RF transmission characteristics and performance stability, and optimizes the materials and structure of traditional RF switches.
Smart Images

Figure CN118943700A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field related to the preparation of radio frequency switches. Specifically, it is the first time that a two-dimensional layered tungsten diselenide film is used as a radio frequency signal switching functional layer. By adopting a thinner and higher mobility tungsten diselenide two-dimensional material, the switching speed and transmission quality of the radio frequency switch are improved, thereby improving the electrical performance of the radio frequency switch. Background Art
[0002] In the field of radio frequency (RF) switch technology, traditional solutions mainly include micro-electro-mechanical systems (MEMS) switches, PIN diode switches, and field effect transistors (FET) switches. Although PIN and FET switches can provide faster switching speeds, their cutoff frequencies usually do not exceed 10 terahertz (THz), which limits their effectiveness in high-frequency applications. On the other hand, although MEMS switches can achieve cutoff frequencies of up to hundreds of THz, they require a high control voltage, which not only increases the complexity of the system, but also limits their application potential in low-power devices. With the gradual increase in wireless communication frequencies, especially in 5G and future 6G communications, the performance limitations of traditional semiconductor materials at high frequencies have become increasingly apparent. These limitations are mainly manifested in higher insertion loss, lower switching speed, and poor linearity, which limits the application of RF switches in high frequency bands.
[0003] In recent years, as a new type of nanomaterial, two-dimensional materials have great application potential in high-frequency electronic devices that require miniaturization and lightweight due to their unique physical and chemical properties, such as ultra-thin thickness, high electron mobility and good thermal stability. However, these excellent properties of two-dimensional materials are far from being fully utilized in RF switches. Most of the existing RF switches based on molybdenum disulfide remain in the laboratory research stage and have not yet met the needs of large-scale commercial applications. This is mainly due to several technical bottlenecks under high-frequency operation, including transmission loss of high-frequency signals, unsatisfactory switching speed, complexity of integrated processes and material stability. In addition, the relevant preparation and processing technologies are not yet mature, which further limits the feasibility of these materials in practical applications. Summary of the invention
[0004] The present invention aims to provide a tungsten diselenide two-dimensional material radio frequency switch and a preparation method thereof. For the first time, the radio frequency switch uses a tungsten diselenide two-dimensional material with high electron mobility as the radio frequency signal switching functional layer, and uses gold and silver as the transmission electrodes of the radio frequency signal. In the device structure design, the physical advantages of tungsten diselenide are fully utilized. The present invention combines a high-precision electron beam exposure system with a thermal evaporation process to accurately prepare a patterned bottom electrode at the nanoscale. Subsequently, a mechanical stripping method is used to prepare nano-layered tungsten diselenide, and it is non-destructively transferred to a precisely configured bottom electrode. Finally, the electron beam exposure system and thermal evaporation technology are used again to accurately prepare a top electrode above the tungsten diselenide two-dimensional material, thereby completing the construction of the radio frequency switch. The high-precision preparation process adopted by the present invention significantly improves the operating frequency and performance stability of the radio frequency switch.
[0005] The specific technical solution for achieving the purpose of the present invention is: A method for preparing a tungsten diselenide two-dimensional radio frequency switch comprises the following specific steps: Step 1: Prepare the bottom electrode layer A1: Cleaning the substrate Select a high-resistance Si / SiO2 substrate, place the substrate in acetone, isopropanol and deionized water in turn, ultrasonically clean it for 30 minutes, and blow dry the substrate surface with a nitrogen gun for later use; A2: Patterned bottom electrode Fix the substrate cleaned in step A1 on a spin coater, spin-coat polymethyl methacrylate photoresist, then heat at 120-150° C. for 3-5 minutes using a temperature-controlled heating table to cure the photoresist, then perform patterned exposure using an electron beam exposure system, and then develop and fix to obtain a patterned bottom electrode; A3: Evaporation of bottom electrode layer Fix the bottom electrode substrate patterned in step A2 on the substrate plate of the thermal evaporation coating apparatus, put gold particles in the tungsten boat in the chamber of the thermal evaporation coating apparatus, turn on the mechanical pump and molecular pump in turn to evacuate the chamber to 3´10 -4 Pa, and after adding current to raise the temperature to the melting point of gold (about 120 A), a 100-150 nm thick gold film is evaporated, and then the substrate is heated with acetone to remove the glue and blow dry, thus completing the preparation of the bottom electrode layer; Step 2: Preparation of tungsten diselenide two-dimensional material functional layer B1: Mechanical exfoliation of 2D tungsten diselenide layers First, the nano-layered tungsten diselenide was peeled off from the tungsten diselenide bulk crystal using a special blue tape for mechanical peeling, and the nano-layered tungsten diselenide was thinned multiple times by stacking and unfolding the blue tape multiple times; secondly, the nano-layered tungsten diselenide was removed from the blue tape using a polydimethylsiloxane film and thinned again, and then pasted on a corner of a clean glass slide; then, it was placed under an optical microscope for observation, and the nano-layered tungsten diselenide with a thickness of 10-15 nm, translucent and uniform texture was selected as the target material; finally, the excess polydimethylsiloxane film on the glass slide was cut off with a blade and used as a backup; B2: Transfer of 2D tungsten diselenide material layer First, the bottom electrode substrate patterned in step A3 is placed on the stage of the two-dimensional material transfer system, and fixed by vacuum adsorption through a mechanical pump; secondly, the glass slide prepared in step B1 is fixed on the stage, and then the Z-axis knob of the two-dimensional material transfer system is adjusted to completely overlap the polydimethylsiloxane film on the glass slide and the substrate, and then the Z-axis knob is adjusted to slowly move it upward until the two are completely separated and the transfer is successful, thus completing the transfer of the two-dimensional material layer and obtaining a tungsten diselenide two-dimensional material functional layer; Step 3: Prepare the top electrode layer C1: Patterned top electrode The substrate with the tungsten diselenide two-dimensional material layer transferred in step B2 is fixed on a spin coater, polymethyl methacrylate photoresist is spin-coated, and then the photoresist is cured by heating at 150° C. for 3 minutes using a temperature-controlled heating table, and then patterned exposure is performed using an electron beam exposure system, and then development and fixing are performed to obtain a patterned top electrode; C2: Evaporated top electrode layer Fix the top electrode substrate patterned in step C1 on the substrate plate of the thermal evaporation coating apparatus, put silver particles in the tungsten boat in the chamber of the thermal evaporation coating apparatus, turn on the mechanical pump and molecular pump in turn to evacuate the chamber to 3´10 -4 Pa, and after adding current to raise the temperature to the melting point of silver (about 80 A), a 100-200 nm thick silver film is evaporated, and then the substrate is heated with acetone to remove the glue and blow dry to obtain the tungsten diselenide two-dimensional radio frequency switch.
[0006] A tungsten diselenide two-dimensional radio frequency switch prepared by the above method.
[0007] Compared with the existing technology, the biggest advantage of this invention is that it innovatively uses tungsten diselenide two-dimensional materials with high electron mobility to significantly improve the high-frequency performance and ultra-high-speed switching capability of the RF switch. By combining advanced electron beam exposure and thermal evaporation processes, nanometer-level precision electrode construction is achieved, improving the performance stability and reliability of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 This is a schematic diagram of the cross-sectional structure of a two-dimensional tungsten diselenide radio frequency switch prepared by the method of the present invention; Figure 2 This is a DC IV curve of a tungsten diselenide two-dimensional radio frequency switch prepared in an embodiment of the present invention; Figure 3 The IV curve of the tungsten diselenide two-dimensional radio frequency switch prepared in an embodiment of the present invention before and after a 20 ns pulse; Figure 4 RF performance of the tungsten diselenide two-dimensional RF switch prepared in an embodiment of the present invention within DC-67 GHz: (a) insertion loss and (b) isolation curves. DETAILED DESCRIPTION
[0009] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0010] See also Figure 1 The tungsten diselenide two-dimensional radio frequency switch described in the present invention includes a high-resistance Si / SiO2 substrate 1, a gold bottom electrode layer 2, a two-dimensional material functional layer 3, and a silver top electrode layer 4; wherein the gold bottom electrode layer 2 and the silver top electrode layer 4 are both prepared by a resistance thermal evaporation coating apparatus, and the tungsten diselenide two-dimensional material functional layer 3 is prepared by mechanical stripping. Example
[0011] (1) Select a high-resistance Si / SiO2 substrate, place the substrate in acetone, isopropanol and deionized water in turn, ultrasonically clean it for 30 minutes, and blow dry the substrate surface with a nitrogen gun for later use; (2) Fix the substrate cleaned in step (1) on a spin coater, spin coat polymethyl methacrylate photoresist, then heat at 150 °C for 3 minutes using a temperature-controlled heating table to cure the photoresist, then use an electron beam exposure system to perform patterned exposure, and then develop and fix to obtain a patterned bottom electrode; fix the bottom electrode substrate patterned in the above step on a substrate plate of a thermal evaporation coating instrument, put gold particles in a tungsten boat in the chamber of the thermal evaporation coating instrument, and turn on the mechanical pump and the molecular pump in turn to evacuate the chamber to 3´10 -4 Pa, and after adding current to raise the temperature to the melting point of gold (about 120 A), a 150 nm thick gold film is evaporated, and then the substrate is heated with acetone to remove the glue and blow dry, thus completing the preparation of the bottom electrode layer.
[0012] (3) Using a special blue tape for mechanical stripping, nano-layered tungsten diselenide was stripped from the two-dimensional bulk tungsten diselenide crystal, and the nano-layered tungsten diselenide was thinned multiple times by repeatedly stacking and unfolding the blue tape. Secondly, the nano-layered tungsten diselenide was removed from the blue tape using a polydimethylsiloxane film and thinned again, and then pasted on a corner of a clean glass slide. Then, it was placed under an optical microscope for observation, and the nano-layered tungsten diselenide with a thickness of 12 nm, translucent and uniform texture was selected as the target material. Finally, the excess polydimethylsiloxane film on the glass slide was cut off with a blade and kept as a backup. (4) Place the bottom electrode substrate patterned in step (2) on the stage of the two-dimensional material transfer system and fix it by vacuum adsorption using a mechanical pump; secondly, fix the glass slide prepared in step (3) on the stage, and then adjust the Z-axis knob of the two-dimensional material transfer system to completely overlap the polydimethylsiloxane film on the glass slide and the substrate, and then adjust the Z-axis knob to slowly move it upward until the two are completely separated and successfully transferred, thereby completing the preparation of the tungsten diselenide two-dimensional material functional layer.
[0013] (5) Fix the substrate to which the two-dimensional material layer has been transferred in step (4) on a spin coater, prepare polymethyl methacrylate photoresist by spin coating, then heat at 150°C for 3 minutes using a temperature-controlled heating table to cure the photoresist, then perform patterned exposure using an electron beam exposure system, and then develop and fix the patterned top electrode; fix the patterned top electrode substrate in step C1 on the substrate plate of a thermal evaporation coating apparatus, place silver particles in a tungsten boat in the chamber of the thermal evaporation coating apparatus, and turn on the mechanical pump and the molecular pump in turn to evacuate the chamber to 3´10 -4 Pa, and after adding current to raise the temperature to the melting point of silver (about 80 A), a 150 nm thick silver film is evaporated, and then the substrate is heated with acetone to remove the glue and blow dry. At this point, the preparation of the tungsten diselenide two-dimensional radio frequency switch is completed. Its structure is as follows Figure 1 shown.
[0014] Figure 2 The DC IV curve of the tungsten diselenide two-dimensional radio frequency switch prepared in an embodiment of the present invention; Figure 3 The IV curve of the tungsten diselenide two-dimensional material radio frequency switch prepared in an embodiment of the present invention before and after a 20 ns pulse; Figure 4 (a) insertion loss and (b) isolation of the tungsten diselenide two-dimensional radio frequency switch prepared in an embodiment of the present invention within the range of DC-67 GHz.
[0015] from Figure 2 It can be seen that the tungsten diselenide two-dimensional RF switch can be turned on and off at 2.3 V and -1.5 V respectively, showing obvious switching characteristics.
[0016] from Figure 3It can be seen that the tungsten diselenide two-dimensional RF switch can achieve state switching from the off state to the on state under a 20 ns pulse, demonstrating ultra-high-speed switching characteristics.
[0017] Depend on Figure 4 It can be seen that the RF performance of the tungsten diselenide two-dimensional RF switch in the DC-67 GHz range is: (a) insertion loss <1.5 dB and (b) isolation >11 dB, which has good RF transmission characteristics. Therefore, the tungsten diselenide two-dimensional RF switch prepared by the present invention optimizes the materials and structure of the traditional RF switch, and the switching speed and RF transmission performance are significantly improved, which is of great significance to the future development of RF switches.
Claims
1. A method for preparing a tungsten diselenide two-dimensional radio frequency switch, It is characterized in that The method comprises the following specific steps: Step 1: Prepare the bottom electrode layer A1: Cleaning the substrate Choose high resistance Si / SiO 2 Substrate: Place the substrate in acetone, isopropanol and deionized water in turn, ultrasonically clean for 30 minutes, and blow dry the substrate surface with a nitrogen gun for later use; A2: Patterned bottom electrode Fix the substrate cleaned in step A1 on a spin coater, spin-coat polymethyl methacrylate photoresist, then heat at 120-150° C. for 3-5 minutes using a temperature-controlled heating table to cure the photoresist, then perform patterned exposure using an electron beam exposure system, and then develop and fix to obtain a patterned bottom electrode; A3: Evaporation of bottom electrode layer Fix the bottom electrode substrate patterned in step A2 on the substrate plate of the thermal evaporation coating apparatus, put gold particles in the tungsten boat in the chamber of the thermal evaporation coating apparatus, turn on the mechanical pump and molecular pump in turn to evacuate the chamber to 3´10 -4 Pa, and after adding current to raise the temperature to the melting point of gold, a 100-150 nm thick gold film is evaporated, and then the substrate is heated with acetone to remove the glue and blow dry, thus completing the preparation of the bottom electrode layer; Step 2: Preparation of tungsten diselenide two-dimensional material functional layer B1: Mechanical exfoliation of 2D tungsten diselenide layers First, the nano-layered tungsten diselenide was peeled off from the tungsten diselenide bulk crystal using a special blue tape for mechanical peeling, and the nano-layered tungsten diselenide was thinned multiple times by stacking and unfolding the blue tape multiple times; secondly, the nano-layered tungsten diselenide was removed from the blue tape using a polydimethylsiloxane film and thinned again, and then pasted on a corner of a clean glass slide; then, it was placed under an optical microscope for observation, and the nano-layered tungsten diselenide with a thickness of 10-15 nm, translucent and uniform texture was selected as the target material; finally, the excess polydimethylsiloxane film on the glass slide was cut off with a blade and used as a backup; B2: Transfer of 2D tungsten diselenide material layer First, the bottom electrode substrate patterned in step A3 is placed on a stage on a two-dimensional material transfer system, and fixed by vacuum adsorption using a mechanical pump; Secondly, fix the glass slide prepared in step B1 on the stage, and then adjust the Z-axis knob of the two-dimensional material transfer system to completely overlap the polydimethylsiloxane film on the glass slide and the substrate, and then adjust the Z-axis knob to slowly move it upward until the two are completely separated and the transfer is successful, thus completing the transfer of the two-dimensional material layer and obtaining a tungsten diselenide two-dimensional material functional layer; Step 3: Prepare the top electrode layer C1: Patterned top electrode The substrate with the tungsten diselenide two-dimensional material layer transferred in step B2 is fixed on a spin coater, polymethyl methacrylate photoresist is spin-coated, and then the photoresist is cured by heating at 120-150 °C for 3-5 minutes using a temperature-controlled heating table, and then patterned exposure is performed using an electron beam exposure system, and then developed and fixed to obtain a patterned top electrode; C2: Evaporated top electrode layer Fix the top electrode substrate patterned in step C1 on the substrate plate of the thermal evaporation coating apparatus, put silver particles in the tungsten boat in the chamber of the thermal evaporation coating apparatus, turn on the mechanical pump and molecular pump in turn to evacuate the chamber to 3´10 -4 Pa, and after adding current to raise the temperature to the melting point of silver, a 100-200 nm thick silver film is evaporated, and then the acetone is heated to remove the glue and blow dry the substrate to obtain the tungsten diselenide two-dimensional radio frequency switch.
2. A tungsten diselenide two-dimensional radio frequency switch prepared by the method of claim 1.