Low-frequency self-biased magnetoelectric transmitting antenna and receiving antenna based on sound wave excitation
By introducing a magnetization gradient structure of a high magnetic permeability layer and a magnetostrictive layer into the magnetoelectric antenna, combined with acoustic excitation technology, the problem of insufficient stability and anti-interference ability of magnetoelectric antennas in good conductor media is solved, and the problem of insufficient stability and anti-interference ability of magnetoelectric antennas in good conductor media is realized. Longer communication distance and higher sensitivity.
Patent Information
- Application Number
- CN202411228584.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-11-12
AI Technical Summary
The existing magnetoelectric antennas have problems such as poor stability, weak anti-interference ability and limited transmission distance in good conductor media, resulting in reduced stability and reliability of communication systems, and the problems of frequency mismatch and narrow bandwidth limit their application. .
Using low-frequency self-biased magnetoelectric transmitting antennas and receiving antennas based on sound wave excitation, the magnetization gradient structure is formed by introducing high magnetic permeability layers and magnetostrictive layers into the transmitting and receiving antennas, and the self-biased coupling effect is achieved, avoiding permanent The additional electromagnetic field and noise disturbances generated by the magnets and improve the sensitivity of the receiving antenna through the cantilever structure.
It effectively improves the stability and anti-interference ability of magnetoelectric antennas, expands communication distance, and enhances communication performance in underwater and underground good conductor media.
Smart Images

Figure CN118943734A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of wireless communication and relates to a low-frequency self-biased magnetoelectric antenna which can be used for low-frequency signal transmission in good conductor media such as underwater and underground. Background Art
[0002] The acoustic wave excited low-frequency magnetoelectric antenna has the advantages of small size and strong anti-interference ability, and can realize communication applications in good conductor media such as underwater and underground. The communication system composed of magnetoelectric antenna has great application potential in underwater Internet of Things and underground Internet of Things, and can realize marine resource exploration, underground pipeline monitoring, environmental monitoring, etc., and provide data support for the development of marine and underground resources.
[0003] Patent document with application number CN116031639 A discloses a "miniaturized low-frequency bidirectional communication magnetoelectric antenna based on acoustic wave excitation and preparation method thereof", such as Figure 1 As shown, it includes a surface magnetostrictive layer 1, an upper electrode layer 2, a piezoelectric layer 3, a lower electrode layer 4, a bottom magnetostrictive layer 5, a permanent magnet 6 and an SMA interface 7. The antenna structure is a laminated structure with one side aligned by bonding and stacking two magnetostrictive layers and a piezoelectric layer 3. The permanent magnet 6 is adsorbed on the side of the laminated structure by magnetic force to provide a bias magnetic field. It is based on the magnetoelectric coupling effect and uses a permanent magnet and a laminated magnetoelectric composite structure to form a magnetoelectric antenna with an integrated bias magnetic field to achieve low-frequency signal transmission and reception in a good conductor medium. However, since the antenna needs to adsorb the permanent magnet on one end of the magnetoelectric composite structure to provide a bias magnetic field, there is a problem that the permanent magnet will generate additional electromagnetic fields and noise interference, which will reduce the stability and reliability of the communication system.
[0004] Dong et al. proposed a magnetoelectric antenna-to-antenna system, in which the magnetoelectric transmitting antenna and the magnetoelectric receiving antenna have the same structure. However, the working conditions of the magnetoelectric transmitting antenna and the magnetoelectric receiving antenna are different. The magnetoelectric transmitting antenna works under high-voltage driving conditions, and the magnetoelectric receiving antenna works under weak magnetic fields. Since the effective elastic modulus of the magnetostrictive material of the magnetoelectric antenna depends on the change of the external stress, that is, the ΔE effect, the magnetoelectric transmitting antenna under high-voltage driving can show strong nonlinear characteristics, resulting in changes in the resonant frequency of the transmitting antenna. The problem of mismatch between the transmitting antenna and the receiving antenna of the communication system will further amplify the limitation of the narrow bandwidth of the magnetoelectric antenna, resulting in limited communication distance.
[0005] In summary, existing magnetoelectric antennas have problems of poor stability and weak anti-interference ability, and magnetoelectric antenna systems have the problem of limited transmission distance, which restricts the communication application of magnetoelectric antennas in good conductor media environments. Summary of the invention
[0006] The purpose of the present invention is to address the deficiencies of the above-mentioned prior art and to propose a low-frequency self-biased magnetoelectric transmitting antenna and receiving antenna based on acoustic wave excitation, so as to improve the stability and anti-interference capability of the magnetoelectric antenna, enhance the sensitivity of the magnetoelectric receiving antenna, and extend the transmission distance of the antenna system.
[0007] To achieve the above object, the technical solution of the present invention includes the following:
[0008] 1. A low-frequency self-biased magnetoelectric transmitting antenna based on acoustic wave excitation, comprising a transmitting magnetoelectric composite unit (1) and a transmitting bias magnetic field unit (2), characterized in that:
[0009] The transmitting magnetoelectric composite unit 1 includes, from top to bottom, an transmitting surface magnetostrictive layer 11, an transmitting upper electrode layer 12, an transmitting piezoelectric layer 13, an transmitting lower electrode layer 14 and an transmitting bottom magnetostrictive layer 15, forming a stacked structure aligned on one side;
[0010] The emission bias magnetic field unit 2 comprises an emission surface high magnetic permeability layer 21 and an emission bottom high magnetic permeability layer 22, which respectively form a magnetization gradient structure with the emission surface magnetostrictive layer 11 and the emission bottom magnetostrictive layer 15.
[0011] Furthermore, the emission surface magnetostrictive layer 11 and the emission bottom magnetostrictive layer 15 are both rectangular sheets with a length of 6-20 mm, a width of 3-8 mm, and a thickness of 0.1-0.8 mm, and the materials thereof are Terfenol-D or GaFe alloy with the easy magnetization axis along the length direction;
[0012] The emission upper electrode layer 12 and the emission lower electrode layer 14 have a thickness of 30-100 nm and are made of one of Ag, Au or Pt;
[0013] The emitting piezoelectric layer 13 is a rectangular sheet with a length of 8-22 mm, a width of 3-8 mm, and a thickness of 0.1-0.8 mm. Its material is one of piezoelectric ceramics, piezoelectric single crystals, aluminum nitride, lithium niobate, zinc oxide, or polymer piezoelectric materials with polarization direction along the thickness direction.
[0014] Furthermore, the emitting surface high magnetic permeability layer 21 and the emitting bottom layer high magnetic permeability layer 22 are both obtained by bonding 1-10 layers of high magnetic permeability materials, and each layer of high magnetic permeability material has a length of 6-20 mm, a width of 3-8 mm, and a thickness of 20-30 μm, and the material is one of Ni, FeCuNbSiB nano alloy or CoFe soft magnetic alloy.
[0015] 2. A low-frequency self-biased magnetoelectric receiving antenna based on acoustic wave excitation, comprising a receiving magnetoelectric composite unit 3, a receiving bias magnetic field unit 4 and a fixture 5, characterized in that:
[0016] The receiving magnetoelectric composite unit 3 includes, from top to bottom, a receiving surface magnetostrictive layer 31, a receiving upper electrode layer 32, a receiving piezoelectric layer 33, a receiving lower electrode layer 34 and a receiving bottom magnetostrictive layer 35, forming a cantilever magnetoelectric composite structure with the receiving upper electrode layer 32, the receiving piezoelectric layer 33 and the receiving lower electrode layer 34 as cantilever beams;
[0017] The receiving bias magnetic field unit 4 comprises a receiving surface high magnetic permeability layer 41 and a receiving bottom high magnetic permeability layer 42, which respectively form a magnetization gradient structure with the receiving surface magnetostrictive layer 31 and the receiving bottom magnetostrictive layer 35;
[0018] The fixture 5 is fixed on one side of the cantilever beam formed by the receiving upper electrode layer 32 , the receiving piezoelectric layer 33 and the receiving lower electrode layer 34 .
[0019] Furthermore, the receiving upper electrode layer 32, the receiving piezoelectric layer 33 and the receiving lower electrode layer 34 constitute a cantilever beam with a length of 6-14 mm.
[0020] Compared with the prior art, the present invention has the following advantages:
[0021] The present invention uses a bias magnetic field unit with a high magnetic permeability layer and a magnetostrictive layer to form a magnetization gradient structure, thereby realizing a self-bias coupling effect, thereby effectively avoiding the additional electromagnetic field and noise interference generated by the existing magnetoelectric antenna using a permanent magnet to provide a bias magnetic field, and improving the stability and reliability of the transmitting antenna and the receiving antenna. At the same time, since the present invention uses a cantilever magnetoelectric composite unit, the sensitivity of the receiving antenna is further improved, thereby effectively extending the communication distance of the magnetoelectric antenna, and it is expected to be applied to underwater and underground good conductor media communications. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0023] Figure 1 A schematic diagram of the structure of an existing magnetoelectric antenna that uses a permanent magnet to provide a bias magnetic field.
[0024] Figure 2 It is a schematic structural diagram of the self-biased magnetoelectric transmitting antenna of the present invention.
[0025] Figure 3 It is a schematic structural diagram of the self-biased magnetoelectric receiving antenna of the present invention.
[0026] Figure 4 The graph is a frequency response graph of the self-biased magnetoelectric transmitting antenna of the present invention and the existing magnetoelectric antenna under a zero bias magnetic field.
[0027] Figure 5 The figure is a relationship diagram between the output magnetoelectric induction voltage of the self-biased magnetoelectric receiving antenna of the present invention and the existing magnetoelectric antenna when used as receiving ends and the radiation distance of the self-biased magnetoelectric transmitting antenna of the present invention.
[0028] Figure 6 This is a diagram of ASK communication test results of an antenna system composed of the self-biased magnetoelectric transmitting antenna of the present invention and the self-biased magnetoelectric receiving antenna of the present invention. DETAILED DESCRIPTION
[0029] The low-frequency self-biased magnetoelectric antenna of this example includes a low-frequency self-biased magnetoelectric transmitting antenna and a low-frequency self-biased magnetoelectric receiving antenna. The structures and effects of these two antennas will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them.
[0030] 1. Low frequency self-biased magneto-electro-optical transmitting antenna.
[0031] Embodiment 1:
[0032] Reference Figure 2 The low-frequency self-biased magnetoelectric transmitting antenna of this embodiment includes a transmitting magnetoelectric composite unit 1 and a transmitting bias magnetic field unit 2. The transmitting magnetoelectric composite unit 1 includes a transmitting surface magnetostrictive layer 11, a transmitting upper electrode layer 12, a transmitting piezoelectric layer 13, a transmitting lower electrode layer 14, and a transmitting bottom magnetostrictive layer 15; the transmitting bias magnetic field unit 2 includes a transmitting surface high magnetic permeability layer 21 and a transmitting bottom high magnetic permeability layer 22.
[0033] The five layers of the emitting surface magnetostrictive layer 11, the emitting upper electrode layer 12, the emitting piezoelectric layer 13, the emitting lower electrode layer 14 and the emitting bottom magnetostrictive layer 15 form a right-aligned laminated magnetoelectric composite structure from top to bottom.
[0034] The emission surface high magnetic permeability layer 21 is bonded to the upper surface of the emission surface magnetostrictive layer 11 by epoxy resin glue to form a magnetization gradient structure.
[0035] The transmitting bottom surface high magnetic permeability layer 22 is bonded to the lower surface of the transmitting bottom magnetostrictive layer 15 by epoxy resin glue to form a magnetization gradient structure.
[0036] In this example, the emitting surface magnetostrictive layer 11 and the emitting bottom magnetostrictive layer 15 are both rectangular sheets with a length of 12 mm, a width of 6 mm, and a thickness of 0.5 mm. The materials used are Terfenol-D with the easy magnetization axis along the length direction to ensure that the resonant mode of the magnetoelectric antenna is longitudinal resonance, and have a larger magnetostriction coefficient and magnetomechanical coupling coefficient, thereby improving the magnetoelectric coupling coefficient and radiation performance of the magnetoelectric antenna.
[0037] In this example, the emission upper electrode layer 12 and the emission lower electrode layer 14 are both prepared by evaporation method, and the thickness thereof is 50 nm. The material thereof is Ag to ensure good conductivity.
[0038] In this example, the emitting piezoelectric layer 13 uses a rectangular thin sheet with a length of 14 mm, a width of 6 mm, and a thickness of 0.5 mm. The material is lead zirconate titanate piezoelectric ceramic with a polarization direction along the thickness direction and a high piezoelectric coefficient, dielectric properties, and electromechanical coupling coefficient, so as to reduce costs and improve the magnetoelectric coupling coefficient and radiation performance of the magnetoelectric antenna.
[0039] In this example, the transmitting surface high magnetic permeability layer 21 and the transmitting bottom layer high magnetic permeability layer 22 are both composed of three layers of high magnetic permeability materials bonded together by epoxy resin glue, and each layer of high magnetic permeability material has a length of 12 mm, a width of 6 mm, and a thickness of 25 μm. The material is a FeCuNbSiB nano-alloy with a large relative magnetic permeability, which forms a magnetization gradient structure with Terfenol-D to achieve a self-bias effect, thereby improving the stability and reliability of the magnetoelectric antenna.
[0040] In this example, the transmitting upper electrode layer 13 and the transmitting lower electrode layer 15 are respectively connected to two ports of the radio frequency line for inputting driving signals to excite the magnetoelectric antenna to transmit electromagnetic waves.
[0041] Embodiment 2:
[0042] The structure of this example is the same as that of Example 1, and its parameters and materials are changed as follows:
[0043] The emission surface magnetostrictive layer 11 and the emission bottom magnetostrictive layer 15 are both rectangular sheets with a length of 16 mm, a width of 8 mm and a thickness of 0.8 mm, and are made of GaFe alloy with the easy magnetization axis along the length direction.
[0044] The emission upper electrode layer 12 and the emission lower electrode layer 14 are both prepared by evaporation method, and both have a thickness of 80 nm and are made of Ag.
[0045] The emitting piezoelectric layer 13 is a rectangular sheet with a length of 18 mm, a width of 8 mm, and a thickness of 0.8 mm, and its material is a lead magnesium niobate piezoelectric single crystal with a polarization direction along the thickness direction.
[0046] The transmitting surface high magnetic permeability layer 21 and the transmitting bottom high magnetic permeability layer 22 are both composed of 5 layers of high magnetic permeability materials bonded by epoxy resin glue, and each layer of high magnetic permeability material has a length of 16 mm, a width of 8 mm, and a thickness of 25 μm, and the material is CoFe soft magnetic alloy.
[0047] Embodiment 3:
[0048] The structure of this example is the same as that of Example 1, and its parameters and materials are changed as follows:
[0049] The emitting surface magnetostrictive layer 11 and the emitting bottom magnetostrictive layer 15 are both rectangular sheets with a length of 10 mm, a width of 5 mm and a thickness of 0.3 mm, and the material thereof is Terfenol-D with the easy magnetization axis along the length direction.
[0050] The emission upper electrode layer 12 and the emission lower electrode layer 14 are both prepared by magnetron sputtering, and both have a thickness of 30 nm and are made of Pt.
[0051] The emission piezoelectric layer 13 is a rectangular sheet with a length of 12 mm, a width of 5 mm, and a thickness of 0.3 mm, and is made of a PVDF piezoelectric polymer with a polarization direction along the thickness direction.
[0052] The transmitting surface high magnetic permeability layer 21 and the transmitting bottom high magnetic permeability layer 22 are both composed of two layers of high magnetic permeability materials bonded by epoxy resin glue, and each layer of high magnetic permeability material has a length of 10 mm, a width of 5 mm, and a thickness of 20 μm, and the material is Ni.
[0053] 2. Low frequency self-biased magnetoelectric receiving antenna
[0054] Embodiment 4:
[0055] Reference Figure 3 The low-frequency self-biased magnetoelectric receiving antenna of this embodiment includes a receiving magnetoelectric composite unit 3, a receiving bias magnetic field unit 4 and a fixture 5. The receiving magnetoelectric composite unit 3 includes a receiving surface magnetostrictive layer 31, a receiving upper electrode layer 32, a receiving piezoelectric layer 33, a receiving lower electrode layer 34 and a receiving bottom magnetostrictive layer 35; the receiving bias magnetic field unit 4 includes a receiving surface high magnetic permeability layer 41 and a receiving bottom high magnetic permeability layer 42.
[0056] The five layers of the receiving surface magnetostrictive layer 31, the receiving upper electrode layer 32, the receiving piezoelectric layer 33, the receiving lower electrode layer 34 and the receiving bottom magnetostrictive layer 35 form a cantilever magnetoelectric composite structure with the receiving upper electrode layer 32, the receiving piezoelectric layer 33 and the receiving lower electrode layer 34 as cantilever beams from top to bottom, so as to improve the sensitivity of the magnetoelectric receiving antenna and extend the communication distance of the magnetoelectric antenna.
[0057] The receiving surface high magnetic permeability layer 41 is bonded to the upper surface of the receiving surface magnetostrictive layer 31 by epoxy resin glue to form a magnetization gradient structure.
[0058] The receiving bottom surface high magnetic permeability layer 42 is bonded to the lower surface of the transmitting bottom magnetostrictive layer 35 by epoxy resin glue to form a magnetization gradient structure.
[0059] The fixture 5 is fixed on one side of the cantilever beam composed of the receiving upper electrode layer 32, the receiving piezoelectric layer 33 and the receiving lower electrode layer 34. The distance between the fixture and the edge of the cantilever beam is 3 mm. The material is plastic insulating material, which is non-magnetic and non-conductive, thus avoiding interference with the normal operation of the magnetoelectric antenna.
[0060] The receiving surface magnetostrictive layer 31 and the receiving bottom magnetostrictive layer 35 are both rectangular sheets with a length of 12 mm, a width of 6 mm, and a thickness of 0.5 mm, and the material thereof is Terfenol-D with the easy magnetization axis along the length direction.
[0061] The receiving upper electrode layer 32 and the receiving lower electrode layer 34 are both prepared by evaporation, and both have a thickness of 50 nm and are made of Ag.
[0062] The receiving piezoelectric layer 33 is a rectangular sheet with a length of 14 mm, a width of 6 mm, and a thickness of 0.5 mm. The material of the receiving piezoelectric layer 33 is lead zirconate titanate piezoelectric ceramic with the polarization direction along the thickness direction.
[0063] In this example, the length of the cantilever beam formed by the receiving upper electrode layer 32, the receiving piezoelectric layer 33 and the receiving lower electrode layer 34 is 9 mm.
[0064] In this example, the receiving surface high magnetic permeability layer 41 and the receiving bottom high magnetic permeability layer 42 are both composed of three layers of high magnetic permeability materials bonded by epoxy resin glue, and each layer of high magnetic permeability material has a length of 12 mm, a width of 6 mm, and a thickness of 25 μm, and the material is FeCuNbSiB nano alloy.
[0065] In this example, the upper receiving electrode layer 32 and the lower receiving electrode layer 34 are respectively connected to two ports of the radio frequency line for outputting the magnetoelectric induction voltage signal of the magnetoelectric receiving antenna.
[0066] Embodiment 5:
[0067] The structure of this example is the same as that of Example 4, and its parameters and materials are changed as follows:
[0068] The receiving surface magnetostrictive layer 31 and the receiving bottom magnetostrictive layer 35 are both rectangular sheets with a length of 16 mm, a width of 8 mm, and a thickness of 0.8 mm, and are made of GaFe alloy with the easy magnetization axis along the length direction.
[0069] The receiving upper electrode layer 32 and the receiving lower electrode layer 34 are both prepared by evaporation method, and both have a thickness of 80 nm and are made of Ag.
[0070] The receiving piezoelectric layer 33 is a rectangular sheet with a length of 18 mm, a width of 8 mm, and a thickness of 0.8 mm, and its material is a lead magnesium niobate piezoelectric single crystal with a polarization direction along the thickness direction.
[0071] The length of the cantilever beam formed by the receiving upper electrode layer 32 , the receiving piezoelectric layer 33 and the receiving lower electrode layer 34 is 13 mm.
[0072] The receiving surface high magnetic permeability layer 41 and the receiving bottom high magnetic permeability layer 42 are both composed of 5 layers of high magnetic permeability materials bonded by epoxy resin glue, and each layer of high magnetic permeability material has a length of 16 mm, a width of 8 mm, and a thickness of 25 μm, and the material is CoFe soft magnetic alloy.
[0073] The clamp 5 is fixed at 6 mm from the edge of the cantilever beam and is made of plastic insulating material.
[0074] Embodiment 6:
[0075] The structure of this example is the same as that of Example 4, and its parameters and materials are changed as follows:
[0076] The receiving surface magnetostrictive layer 31 and the receiving bottom magnetostrictive layer 35 are both rectangular sheets with a length of 10 mm, a width of 5 mm and a thickness of 0.3 mm, and the material thereof is Terfenol-D with the easy magnetization axis along the length direction.
[0077] The receiving upper electrode layer 32 and the receiving lower electrode layer 34 are both prepared by magnetron sputtering, and both have a thickness of 30 nm and are made of Pt.
[0078] The receiving piezoelectric layer 33 is a rectangular sheet with a length of 12 mm, a width of 5 mm, and a thickness of 0.3 mm, and is made of a PVDF piezoelectric polymer with a polarization direction along the thickness direction.
[0079] The receiving upper electrode layer 32, the receiving piezoelectric layer 33 and the receiving lower electrode layer 34 form a cantilever beam with a length of 5 mm.
[0080] The receiving surface high magnetic permeability layer 41 and the receiving bottom high magnetic permeability layer 42 are both composed of two layers of high magnetic permeability materials bonded by epoxy resin glue, and each layer of high magnetic permeability material has a length of 10 mm, a width of 5 mm, and a thickness of 20 μm, and the material is Ni.
[0081] The clamp 5 is fixed at 2 mm from the edge of the cantilever beam and is made of plastic insulating material.
[0082] The effect of the present invention can be further illustrated by the following test results.
[0083] 1. Test conditions
[0084] The sinusoidal signal generated by the signal generator is used to excite the transmitting antenna to transmit an electromagnetic wave signal, and the phase-locked amplifier is used to test and record the magnetoelectric induction voltage signal generated after the receiving antenna senses the electromagnetic wave signal.
[0085] 2. Test content
[0086] Test 1: Under the test conditions of zero DC bias magnetic field and 13.5 A / m AC magnetic field amplitude, the frequency response test of the self-biased magnetoelectric transmitting antenna of Example 1 was performed, and the performance was compared with that of the existing magnetoelectric antenna under zero bias magnetic field. The results are as follows: Figure 4 shown.
[0087] from Figure 4 It can be seen that the output magnetic induction voltage of the self-biased magnetoelectric transmitting antenna of the present invention at the resonant frequency is significantly higher than that of the existing magnetoelectric antenna, indicating that the self-biased magnetoelectric transmitting antenna of the present invention has a strong magnetoelectric coupling effect under a zero bias magnetic field and realizes the self-bias function.
[0088] Test 2: Using the transmitting antenna of Example 1 of the present invention and the receiving antenna of Example 4 to form an antenna system, using the transmitting antenna of Example 1 of the present invention and the existing magnetoelectric antenna to form an antenna system, under zero bias magnetic field, with 40V pp The sine AC signal excites the transmitting antenna of Example 1 of the present invention to transmit electromagnetic wave signals. The radiation intensity of the transmitting antenna of Example 1 at different positions is tested using the receiving antenna of Example 4 and the existing magnetoelectric antenna. The results are as follows: Figure 5 shown.
[0089] from Figure 5 It can be seen that the radiation intensity of the self-biased magnetoelectric transmitting antenna of the present invention gradually decays with increasing distance. Compared with the existing magnetoelectric antenna, the self-biased magnetoelectric receiving antenna of the present invention can detect weaker magnetic fields and show higher sensitivity. Under the influence of test equipment and environmental noise, the test distance limits of the self-biased magnetoelectric receiving antenna of the present invention and the existing magnetoelectric antenna are 1.7m and 0.4m respectively. The transmission distance of the antenna system composed of the self-biased magnetoelectric antenna of the present invention is significantly improved.
[0090] Test 3: An antenna system with a communication distance of 1 m is formed by using the transmitting antenna of Example 1 of the present invention and the receiving antenna of Example 4. A 10 Hz ASK baseband signal with "0" and "1" logic information is loaded into the carrier signal to test the communication performance of the antenna system. The results are as follows: Figure 6 shown.
[0091] from Figure 6 It can be seen that the antenna system composed of the self-biased magnetoelectric antenna of the present invention can effectively demodulate the logical information of "0" and "1", and realize effective communication within a distance of 1m at a 10Hz ASK modulation frequency.
[0092] The above descriptions are only a few specific examples of the present invention and do not constitute any limitation to the present invention. Obviously, for professionals in this field, after understanding the content and principles of the present invention, it is possible to make various modifications and changes in form and details without departing from the principles and structures of the present invention. For example, in addition to Ag and Pt, the material of the electrode layer can also be Au, and in addition to lead zirconate titanate piezoelectric ceramics, lead magnesium niobate piezoelectric single crystals and PVDF piezoelectric polymers, the material of the piezoelectric layer can also be other types of piezoelectric ceramics, piezoelectric single crystals, polymers, aluminum nitride, lithium niobate, zinc oxide and other piezoelectric materials. However, these modifications and changes based on the ideas of the present invention are still within the scope of protection of the claims of the present invention.
Claims
1. A low-frequency self-biased magnetoelectric transmitting antenna based on acoustic wave excitation, comprising a transmitting magnetoelectric composite unit (1) and a transmitting bias magnetic field unit (2), characterized in that: The emission magnetoelectric composite unit (1) comprises, from top to bottom, an emission surface magnetostrictive layer (11), an emission upper electrode layer (12), an emission piezoelectric layer (13), an emission lower electrode layer (14) and an emission bottom magnetostrictive layer (15), forming a stacked structure aligned on one side; The emission bias magnetic field unit (2) comprises an emission surface high magnetic permeability layer (21) and an emission bottom high magnetic permeability layer (22), which respectively form a magnetization gradient structure with the emission surface magnetostrictive layer (11) and the emission bottom magnetostrictive layer (15).
2. The transmitting antenna according to claim 1, characterized in that: The emission surface magnetostrictive layer (11) is a rectangular sheet with a length of 6-20 mm, a width of 3-8 mm, and a thickness of 0.1-0.8 mm, and its material is Terfenol-D or GaFe alloy with its easy magnetization axis along the length direction; The emission upper electrode layer (12) has a thickness of 30-100 nm and is made of one of Ag, Au or Pt; The emitting piezoelectric layer (13) is a rectangular sheet with a length of 8-22 mm, a width of 3-8 mm and a thickness of 0.1-0.8 mm, and its material is one of piezoelectric ceramics, piezoelectric single crystals, aluminum nitride, lithium niobate, zinc oxide or polymer piezoelectric materials with a polarization direction along the thickness direction.
3. The transmitting antenna according to claim 1, characterized in that: The material and size parameters of the emission lower electrode layer (14) are the same as those of the emission upper electrode layer (12); The material and size parameters of the emitting bottom magnetostrictive layer (15) are the same as those of the emitting surface magnetostrictive layer (11).
4. The transmitting antenna according to claim 1, characterized in that: The emitting surface high magnetic permeability layer (21) and the emitting bottom high magnetic permeability layer (22) are both obtained by bonding 1-10 layers of high magnetic permeability materials, and each layer of high magnetic permeability material has a length of 6-20 mm, a width of 3-8 mm, and a thickness of 20-30 μm, and the material is one of Ni, FeCuNbSiB nano alloy or CoFe soft magnetic alloy.
5. A low-frequency self-biased magnetoelectric receiving antenna based on acoustic wave excitation, comprising a receiving magnetoelectric composite unit (3), a receiving bias magnetic field unit (4) and a fixture (5), characterized in that: The receiving magnetoelectric composite unit (3) comprises, from top to bottom, a receiving surface magnetostrictive layer (31), a receiving upper electrode layer (32), a receiving piezoelectric layer (33), a receiving lower electrode layer (34) and a receiving bottom magnetostrictive layer (35), forming a cantilever magnetoelectric composite structure with the receiving upper electrode layer (32), the receiving piezoelectric layer (33) and the receiving lower electrode layer (34) as cantilever beams; The receiving bias magnetic field unit (4) comprises a receiving surface high magnetic permeability layer (41) and a receiving bottom high magnetic permeability layer (42), which respectively form a magnetization gradient structure with the receiving surface magnetostrictive layer (31) and the receiving bottom magnetostrictive layer (35); The fixture (5) is fixed on one side of a cantilever beam formed by the receiving upper electrode layer (32), the receiving piezoelectric layer (33) and the receiving lower electrode layer (34).
6. The receiving antenna according to claim 4, characterized in that: The receiving surface magnetostrictive layer (31), the receiving upper electrode layer (32), the receiving piezoelectric layer (33), the receiving lower electrode layer (34), and the receiving bottom magnetostrictive layer (35) are respectively the same in material and size parameters as the corresponding layers of the transmitting antenna; The receiving upper electrode layer (32), the receiving piezoelectric layer (33) and the receiving lower electrode layer (34) together form a cantilever beam with a length of 6-14 mm.
7. The receiving antenna according to claim 4, characterized in that: The material and size parameters of the receiving surface high magnetic permeability layer (41) and the receiving bottom high magnetic permeability layer (42) are respectively the same as those of the corresponding layers of the transmitting antenna.
8. The receiving antenna according to claim 4, characterized in that: The fixture (5) is fixed at 1-10 mm from the edge of the cantilever beam formed by the receiving upper electrode layer (32), the receiving piezoelectric layer (33) and the receiving lower electrode layer (34), and is made of plastic insulating material.
Citation Information
Patent Citations
Zero-bias magnetic sensor probe
CN103105591A
Magnetoelectric antenna based on magnetoelectric composite material
CN117410695A