Copper antioxidant and preparation method thereof

By using agitated preparation method of components such as methylbenzotriazole on the copper metal, a copper antioxidant is formed, which solves the problem of copper metal oxidation and maintains the excellent conductivity and decorative properties.

CN118957591APending Publication Date: 2024-11-15TIANJIN INST OF SYNTHETIC MATERIALS IND
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411031257.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Copper metal is prone to oxidation in the air, causing the material to darken its color and deteriorate its decorative properties. The oxide is an insulator, making it difficult to maintain good conductivity.

Method used

The copper antioxidant is prepared by stirring to form a stable emulsion by using methylbenzotriazole, ethanol, emulsifier combination, phosphonocarboxylic acid copolymer, aminotrimethylphosphonic acid, triethanolamine and lithium silicate. , prevent copper metal oxidation.

Benefits of technology

Effectively prevent copper metal oxidation, maintain good conductivity, and extend service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118957591A_ABST
    Figure CN118957591A_ABST
Patent Text Reader

Abstract

The invention discloses a copper antioxidant and a preparation method thereof, and the preparation method comprises the following steps: S1, determining a system boundary: determining which parts belong to a system range and which parts do not belong to the system range, thereby facilitating the subsequent formulation of a corresponding strategy in the system range; s2, determining the role of an attacker: according to the attack mode, means and angle of the attacker, preliminarily determining the type of the attacker, such as hackers, internal employees and the like; s3, constructing an attack tree: generally, determining a final target of an attacker, dividing the final target into sub-targets and constructing a tree diagram of the attack tree; wherein the final target is a tree root, the sub-target is a branch, and the means for completing the sub-target is a leaf; s4, analyzing an attack tree: identifying heavy vulnerabilities and weaknesses of the system, and formulating a corresponding defense strategy; and S5, actively setting the trapping vulnerabilities: actively setting the trapping vulnerabilities on the final target and the sub-target so as to obtain the information of an attacker or capture the attacker when the attacker attacks the trapping vulnerabilities.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of copper antioxidants, in particular to a copper antioxidant and a preparation method thereof. Background Art

[0002] Copper metal has good luster and its conductivity is almost the same as silver, while its price is only one twentieth of silver. Therefore, in terms of cost performance, copper metal is a relatively ideal conductive material and is widely used in conductive adhesives, conductive plastics, conductive coatings and other fields. However, copper metal has active chemical properties and is easily oxidized in the air, causing the material color to darken and the decorative effect to deteriorate. In addition, oxides are insulators, which makes it difficult for copper metal to maintain good conductivity during long-term use. Therefore, how to prevent copper metal from being oxidized during the preparation stage and during use is a key issue in the application research of copper-based materials. Summary of the invention

[0003] The purpose of this section is to summarize some aspects of the embodiments of the present invention and briefly introduce some preferred embodiments. Some simplifications or omissions may be made in this section and the specification abstract and the invention title of this application to avoid blurring the purpose of this section, the specification abstract and the invention title, and such simplifications or omissions cannot be used to limit the scope of the present invention.

[0004] In view of the above and / or existing problems in a copper antioxidant and a preparation method thereof, the present invention is proposed.

[0005] Therefore, the object of the present invention is to provide a copper antioxidant and a preparation method thereof. When preparing the copper antioxidant, 10-15 parts of methylbenzotriazole and 30-45 parts of ethanol are first mixed, and stirred at 300-500 rpm for 5-15 minutes at 15-30°C to obtain a primary corrosion inhibitor; then 5-10 parts of an emulsifier combination are added to the primary corrosion inhibitor, and stirred at 300-500 rpm for 1-5 minutes, and then 10-20 parts of a phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and 20-35 parts of water are added, and stirred at 300-500 rpm for 2-5 hours at 60-80°C to obtain the copper antioxidant.

[0006] To solve the above technical problems, according to one aspect of the present invention, the present invention provides the following technical solutions:

[0007] A copper antioxidant and a preparation method thereof, comprising the following components in parts by weight:

[0008] 10-15 parts of methyl benzotriazole, 30-45 parts of ethanol, 5-10 parts of emulsifier combination, 10-20 parts of phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate, and the balance is water; wherein the preparation method is: firstly mix 10-15 parts of methyl benzotriazole and 30-45 parts of ethanol, stir at 15-30°C and 300-500 rpm for 5-15 minutes , to obtain a primary corrosion inhibitor; then add 5-10 parts of the emulsifier combination to the primary corrosion inhibitor, stir at 300-500 rpm for 1-5 minutes, then add 10-20 parts of phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and 20-35 parts of water, stir at 60-80°C at 300-500 rpm for 2-5 hours to obtain a copper antioxidant.

[0009] As a preferred embodiment of the copper antioxidant and the preparation method thereof described in the present invention, the emulsifier combination is a non-ionic surfactant polysorbate 80.

[0010] As a preferred embodiment of the copper antioxidant and preparation method thereof described in the present invention, potassium hydroxide can be dissolved in water to obtain a potassium hydroxide aqueous solution to replace the emulsifier combination. The method of use is to add the potassium hydroxide solution to the primary corrosion inhibitor to make the solution a dilute alkaline solution, that is: 7<primary corrosion inhibitor pH<8.

[0011] As a preferred embodiment of the copper antioxidant and the preparation method thereof described in the present invention, the concentration of the potassium hydroxide aqueous solution is 2-3 mol / L.

[0012] As a preferred embodiment of the copper antioxidant and preparation method thereof described in the present invention, the volume ratio of water, potassium hydroxide aqueous solution and ethanol is 1-8:1-3:10-50.

[0013] Compared with the prior art, the invention has the beneficial effects that: when preparing the copper antioxidant, 10-15 parts of methylbenzotriazole and 30-45 parts of ethanol are first mixed, and stirred at 300-500 rpm for 5-15 minutes at 15-30°C to obtain a primary corrosion inhibitor; then 5-10 parts of an emulsifier combination are added to the primary corrosion inhibitor, and stirred at 300-500 rpm for 1-5 minutes; then 10-20 parts of a phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and 20-35 parts of water are added, and stirred at 300-500 rpm for 2-5 hours at 60-80°C to obtain the copper antioxidant. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the present invention will be described in detail below in combination with the accompanying drawings and detailed embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative labor. Among them:

[0015] Figure 1 The invention discloses a copper antioxidant and a preparation method thereof. DETAILED DESCRIPTION

[0016] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0017] Secondly, the present invention is described in detail with reference to schematic diagrams. When describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.

[0018] In order to make the objectives, technical solutions and advantages of the present invention more clear, the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings.

[0019] The invention provides a copper antioxidant and a preparation method thereof. When preparing the copper antioxidant, 10-15 parts of methylbenzotriazole and 30-45 parts of ethanol are firstly mixed, and stirred at 300-500 rpm for 5-15 minutes at 15-30 DEG C to obtain a primary corrosion inhibitor; then 5-10 parts of an emulsifier combination are added to the primary corrosion inhibitor, and stirred at 300-500 rpm for 1-5 minutes; then 10-20 parts of a phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and 20-35 parts of water are added, and stirred at 60-80 DEG C at 300-500 rpm for 2-5 hours to obtain the copper antioxidant.

[0020] Figure 1 The overall structure diagram of a copper antioxidant and a preparation method thereof according to the present invention is shown. Figure 1 , a copper antioxidant and a preparation method thereof according to the present embodiment:

[0021] The invention comprises the following components in parts by weight: 10-15 parts of methyl benzotriazole, 30-45 parts of ethanol, 5-10 parts of emulsifier combination, 10-20 parts of phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate, and the balance is water; wherein the preparation method comprises: firstly mixing 10-15 parts of methyl benzotriazole and 30-45 parts of ethanol, stirring at 15-30°C and 300-500 rpm for 5-15 minutes, and obtaining primary corrosion inhibition. agent; then adding 5-10 parts of the emulsifier combination to the primary corrosion inhibitor, stirring at 300-500 rpm for 1-5 minutes, then adding 10-20 parts of phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and 20-35 parts of water, stirring at 60-80°C at 300-500 rpm for 2-5 hours to obtain a copper antioxidant, wherein the emulsifier combination includes an emulsifier and a nonionic surfactant polysorbate 80;

[0022] Among them, because methylbenzotriazole is insoluble in water, an emulsifier combination can be added to form a stable emulsion. By forming an emulsion, methylbenzotriazole is dispersed in water in the form of tiny droplets, and then the surfactant polysorbate 80 can allow the emulsion to form a stable methylbenzotriazole water emulsion, thereby dissolving in water; in addition, methylbenzotriazole is soluble in dilute alkali solution, and potassium hydroxide is dissolved in water to obtain a potassium hydroxide aqueous solution to replace the emulsifier combination. The method of use is to add potassium hydroxide solution to the primary corrosion inhibitor to make the solution a dilute alkali solution, that is: 7 < primary corrosion inhibitor pH < 8, the concentration of potassium hydroxide aqueous solution is 2-3 mol / L, and the volume ratio of water, potassium hydroxide aqueous solution, and ethanol is 1-8:1-3:10-50.

[0023] Combination Figure 1 , a copper antioxidant and a preparation method thereof according to the present embodiment, the specific use process is as follows: when preparing the copper antioxidant, first mix 10-15 parts of methylbenzotriazole and 30-45 parts of ethanol, and stir at 15-30°C at 300-500 rpm for 5-15 minutes to obtain a primary corrosion inhibitor; then add 5-10 parts of the emulsifier combination to the primary corrosion inhibitor, stir at 300-500 rpm for 1-5 minutes, and then add 10-20 parts of a phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and 20-35 parts of water, and stir at 60-80°C at 300-500 rpm for 2-5 hours to obtain a copper antioxidant.

[0024] Although the present invention has been described above with reference to the embodiments, various modifications may be made thereto and parts thereof may be replaced by equivalents without departing from the scope of the present invention. In particular, as long as there is no structural conflict, the various features in the embodiments disclosed in the present invention may be used in combination with each other in any manner, and the fact that these combinations are not exhaustively described in this specification is only for the sake of omitting space and saving resources. Therefore, the present invention is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.

Claims

1. A copper antioxidant, characterized in that The invention is composed of the following components in parts by weight: 10-15 parts of methylbenzotriazole, 30-45 parts of ethanol, 5-10 parts of emulsifier combination, 10-20 parts of phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and the balance is water.

2. A copper antioxidant according to claim 1, characterized in that: The emulsifier combination includes an emulsifier and a non-ionic surfactant, polysorbate 80.

3. The method for preparing the copper antioxidant according to claim 1, characterized in that: The steps include: S1. First, 10-15 parts of methylbenzotriazole and 30-45 parts of ethanol are mixed, and stirred at 15-30° C. and 300-500 rpm for 5-15 minutes to obtain a primary corrosion inhibitor; S2, then add 5-10 parts of the emulsifier combination to the primary corrosion inhibitor, and stir at 300-500 rpm for 1-5 minutes; S3, add 10-20 parts of phosphonocarboxylic acid copolymer, 10-20 parts of aminotri(methylenephosphonic acid), 5-10 parts of triethanolamine, 3-5 parts of lithium silicate and 20-35 parts of water, stir at 60-80°C and 300-500 rpm for 2-5 hours to obtain a copper antioxidant.

4. The method for preparing the copper antioxidant according to claim 3, characterized in that: In S2, potassium hydroxide can also be dissolved in water to obtain a potassium hydroxide aqueous solution to replace the emulsifier combination. The method of use is to add the potassium hydroxide solution to the primary corrosion inhibitor to make the solution a dilute alkaline solution, that is: 7<primary corrosion inhibitor pH<8.

5. A copper antioxidant and a preparation method thereof according to claim 4, characterized in that: The concentration of the potassium hydroxide aqueous solution is 2-3 mol / L.