All-trace section roughness characterization method and system

Through the full trace section roughness characterization method, the surface point cloud data of the material is obtained by using three-dimensional laser scanning technology, and the two-dimensional and three-dimensional roughness are extracted and calculated, which solves the problems of uneven defects inside the material and the differences in different profiles, and realizes the Accurate roughness characterization of various materials and quantification of crack development paths have improved the basis for crack repair in engineering.

CN118960627AInactive Publication Date: 2024-11-15TIANJIN UNIV

Patent Information

Application Number
CN202411060591.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing two-dimensional joint contour roughness characterization method cannot effectively solve the problem of uneven distribution defects inside the material and the large differences in the contour traces of different sections of the same section. The three-dimensional structural surface roughness characterization method is only suitable for materials with fractal characteristics. , cannot be applied to all materials.

Method used

The full-trace cross-roughness characterization method is used to obtain surface point cloud data by scanning the fracture surface of the sample material, extract two-dimensional traces of the cross-section, and calculate the two-dimensional and three-dimensional roughness. The elevation information is obtained by using a three-dimensional laser scanner to develop along the cracks. Scan the direction to achieve a leap from two-dimensional to three-dimensional, and eliminate the major problem of contour discreteness.

Benefits of technology

It improves the accuracy of cross-section trace roughness characterization, can effectively understand the development path of cracks, and is suitable for various materials, especially materials with uneven distribution of defects, providing a reliable basis for crack repair.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118960627A_ABST
    Figure CN118960627A_ABST
Patent Text Reader

Abstract

The invention discloses a full-trace section roughness characterization method and system, and relates to the field of rock mass structural planes, and the method comprises the steps: scanning a fracture surface of a sample material, and obtaining the surface point cloud data of a section; according to the surface point cloud data, extracting a section two-dimensional trace; and respectively calculating the two-dimensional roughness of each two-dimensional trace, and calculating the three-dimensional roughness of the section by using each two-dimensional roughness. According to the method, the problem that the discreteness of each contour line is too large due to defects can be eliminated, the crack development path of the whole section can be extracted and quantified, transition from a traditional two-dimensional trace roughness characterization method to three dimensions is achieved, the development path of the crack can be well known, and the method is suitable for popularization and application. And an implementation basis is conveniently provided for crack repair and other work in engineering.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of rock mass structural surfaces, and more particularly to a full-trace cross-section roughness characterization method and system. Background Art

[0002] At present, the methods for characterizing the cross-section roughness of rock materials and rock-like materials mainly include two-dimensional joint contour roughness characterization methods and three-dimensional structural surface roughness characterization methods.

[0003] In the quantitative characterization of the roughness of two-dimensional joint contour lines, there are mainly description methods such as statistical parameters, comprehensive parameters and straight edge diagrams. The profile trace of the structural surface can reflect the development path of cracks to a certain extent, which is of great significance for correcting fracture energy and guiding the grouting repair of cracks in actual engineering. Therefore, the profile of the cross-section is used as the main roughness analysis parameter. However, the two-dimensional joint contour roughness characterization method cannot solve the situation where there are unevenly distributed defects inside the material and the profile traces of different sections of the same section are very different. For example, taking the jute fiber reinforced concrete sample as an example, there are unevenly distributed defects inside it, and the profile traces of different sections of the same section are very different. Obviously, it cannot be quantified by partial random section profile traces. At present, the most commonly used method for characterizing the roughness of three-dimensional structural surfaces is the fractal dimension method. Although this method can reflect the roughness characteristics of the structural surface, it requires the structural surface to have fractal characteristics and is only applicable to certain specific materials.

[0004] Therefore, how to provide a method for characterizing the roughness of a three-dimensional structural surface and improve the accuracy of characterizing the roughness of a cross-sectional trace is an urgent problem that needs to be solved by those skilled in the art. Summary of the invention

[0005] In view of this, the present invention provides a method and system for characterizing the roughness of a full-trace section, which extracts and integrates all two-dimensional contour lines in a certain order, thereby achieving a transition from two-dimensional to three-dimensional, eliminating the problem of excessive discreteness of contour lines, and accurately characterizing the roughness of the section trace.

[0006] In order to achieve the above object, the present invention provides the following technical solutions:

[0007] The present invention discloses a method for characterizing the roughness of a full-trace cross-section, and the specific steps are as follows:

[0008] Scan the fracture surface of the sample material to obtain surface point cloud data of the fracture surface;

[0009] Extracting a two-dimensional cross-section trace according to the surface point cloud data;

[0010] The two-dimensional roughness of each two-dimensional trace is calculated respectively, and the three-dimensional roughness of the cross section is calculated using each of the two-dimensional roughnesses.

[0011] Furthermore, the surface point cloud data is obtained by:

[0012] Propagating the crack along the crack development direction of the sample material until the sample material splits;

[0013] placing the split portion of the sample material on a three-dimensional laser scanner so that the cross section is in a horizontal direction;

[0014] The scanning start and end positions are set, and the section is subjected to three-dimensional laser scanning in the vertical direction to obtain the elevation information of each point on the scanning surface, thereby obtaining the three-dimensional coordinate information of each acquisition point as the surface point cloud data of the section.

[0015] Furthermore, the three-dimensional coordinate information is exported in a txt format.

[0016] Furthermore, the extracting of the two-dimensional trace of the cross section includes:

[0017] The horizontal plane where the surface point cloud data is located is determined, and the normal plane of the horizontal plane is scanned from the length direction and the width direction of the horizontal plane at a fixed scanning interval to extract the two-dimensional traces in the length direction and the two-dimensional traces in the width direction.

[0018] Furthermore, the calculation formula of the two-dimensional roughness is:

[0019]

[0020] In the formula, R p is the two-dimensional roughness, L′ is the two-dimensional trace projection length, n′ is the total number of two-dimensional trace point clouds, (x i ′,y i ′)、(x i ' +1 ,y i ' +1 ) are the two-dimensional coordinates of the i-th point and the i+1-th point on the two-dimensional trace.

[0021] Furthermore, the calculation formula of the three-dimensional roughness is:

[0022]

[0023]

[0024]

[0025] in, are the sum of the roughness of the two-dimensional traces in the length direction of the section, the sum of the roughness of the two-dimensional traces in the width direction, and the three-dimensional roughness of the section, respectively. m and n are the total number of single two-dimensional trace point clouds in the length and width directions of the section, respectively. α and β are the effective scanning lines in the length and width directions, respectively. L and D are the length and width of the material section, respectively. (x j ,y j ,z j )、(x j+1 ,y j+1 ,z j+1 ) represents the three-dimensional coordinates of the j-th point and the j+1-th point on the two-dimensional trajectory.

[0026] The present invention also discloses a full-trace cross-section roughness characterization system, which is characterized by comprising:

[0027] Data acquisition module: scan the material section and obtain the surface point cloud data of the section;

[0028] Trace extraction module: extracting cross-section two-dimensional traces according to the surface point cloud data;

[0029] Roughness calculation module: calculates the two-dimensional roughness of each two-dimensional trace respectively, and calculates the three-dimensional roughness of the cross section using each of the two-dimensional roughnesses.

[0030] It can be seen from the above technical solutions that, compared with the prior art, the present invention discloses a method and system for characterizing the roughness of a full-trace section. The elevation information of the scanned section can be obtained by using a three-dimensional laser scanner, and then all traces of the material section are extracted with the crack development direction as the section direction, so as to obtain the roughness of the test material according to the roughness calculation formula. The present invention can not only eliminate the problem of too large discreteness of each contour line caused by defects, but also extract and quantify the crack development path of the full section, realizing the transition from the traditional two-dimensional trace roughness characterization method to three-dimensional, and can better understand the crack development path, which is convenient for providing an implementation basis for crack repair and other work in engineering. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.

[0032] Figure 1 It is a schematic diagram of the overall process of an embodiment of the present invention.

[0033] Figure 2 Schematic diagram of a two-dimensional trace of a cross section of an embodiment of the present invention. DETAILED DESCRIPTION

[0034] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0035] The embodiment of the present invention discloses a method for characterizing the roughness of a full trace section, such as Figure 1 As shown, the specific steps are as follows:

[0036] Scan the fracture surface of the sample material to obtain surface point cloud data of the fracture surface;

[0037] Extract the two-dimensional trace of the cross section based on the surface point cloud data;

[0038] The two-dimensional roughness of each two-dimensional trace is calculated respectively, and the three-dimensional roughness of the cross section is calculated using each two-dimensional roughness.

[0039] In a specific embodiment, the surface point cloud data is obtained by:

[0040] Crack propagation is performed along the crack development direction of the sample material until the sample material splits;

[0041] The split part of the sample material is placed on a three-dimensional laser scanner so that the cross section is in the horizontal direction;

[0042] Set the scanning start and end positions, and perform three-dimensional laser scanning on the section from the vertical direction. During scanning, a high-frequency laser is emitted by the laser source. The laser is reflected by the scanning section to obtain the elevation information of each point on the scanning surface, thereby obtaining the three-dimensional coordinate information of each acquisition point as the surface point cloud data of the section.

[0043] In a specific embodiment, the three-dimensional coordinate information is exported in a txt format to facilitate subsequent related quantitative calculation work.

[0044] In a specific embodiment, extracting a two-dimensional cross-section trace includes:

[0045] Determine the horizontal plane where the surface point cloud data is located, for example, use the least squares method to fit the plane equation, and use the normal plane of the horizontal plane to scan the length direction and width direction of the horizontal plane at a fixed scanning interval to extract the two-dimensional traces in the length direction and the two-dimensional traces in the width direction. Figure 2As shown in the figure, three different two-dimensional traces are shown. Based on the non-contact three-dimensional laser scanning technology, the full range of traces are extracted, thereby optimizing the two-dimensional trace length characterization method and compensating for the drawback of too large discreteness of the contour trace roughness.

[0046] In a specific embodiment, the calculation formula of the two-dimensional roughness is:

[0047]

[0048] In the formula, R p is the two-dimensional roughness, L′ is the two-dimensional trace projection length, n′ is the total number of two-dimensional trace point clouds, (x i ′,y i ′)、(x i ' +1 ,y i ' +1 ) are the two-dimensional coordinates of the i-th point and the i+1-th point on the two-dimensional trace.

[0049] In a specific embodiment, the calculation formula of the three-dimensional roughness is:

[0050]

[0051]

[0052]

[0053] in, are the sum of the roughness of the two-dimensional traces in the length direction of the section, the sum of the roughness of the two-dimensional traces in the width direction, and the three-dimensional roughness of the section, respectively. m and n are the total number of single two-dimensional trace point clouds in the length and width directions of the section, respectively. α and β are the effective scanning lines in the length and width directions, respectively. L and D are the length and width of the material section, respectively. (x j ,y j ,z j )、(x j+1 ,y j+1 ,z j+1 ) represents the three-dimensional coordinates of the j-th point and the j+1-th point on the two-dimensional trajectory.

[0054] The embodiment of the present invention also discloses a full-trace cross-section roughness characterization system, including:

[0055] Data acquisition module: scan the material section and obtain the surface point cloud data of the section;

[0056] Trace extraction module: extracts the cross-section two-dimensional trace according to the surface point cloud data;

[0057] Roughness calculation module: calculate the two-dimensional roughness of each two-dimensional trace respectively, and use each two-dimensional roughness to calculate the three-dimensional roughness of the cross section.

[0058] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.

[0059] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A method for characterizing the roughness of a full-trace section, characterized in that: The specific steps are as follows: Scan the fracture surface of the sample material to obtain surface point cloud data of the fracture surface; Extracting a two-dimensional cross-section trace according to the surface point cloud data; The two-dimensional roughness of each two-dimensional trace is calculated respectively, and the three-dimensional roughness of the cross section is calculated using each of the two-dimensional roughnesses.

2. A method for characterizing the roughness of a full-trace section according to claim 1, characterized in that: The surface point cloud data is obtained by: Propagating the crack along the crack development direction of the sample material until the sample material splits; placing the split portion of the sample material on a three-dimensional laser scanner so that the cross section is in a horizontal direction; The scanning start and end positions are set, and the section is subjected to three-dimensional laser scanning in the vertical direction to obtain the elevation information of each point on the scanning surface, thereby obtaining the three-dimensional coordinate information of each acquisition point as the surface point cloud data of the section.

3. A method for characterizing the roughness of a full-trace section according to claim 2, characterized in that: The three-dimensional coordinate information is exported in txt format.

4. A method for characterizing the roughness of a full-trace section according to claim 1, characterized in that: The step of extracting the two-dimensional trace of the cross section comprises: The horizontal plane where the surface point cloud data is located is determined, and the normal plane of the horizontal plane is scanned from the length direction and the width direction of the horizontal plane at a fixed scanning interval to extract the two-dimensional traces in the length direction and the two-dimensional traces in the width direction.

5. A method for characterizing the roughness of a full-trace section according to claim 1, characterized in that: The calculation formula of the two-dimensional roughness is: In the formula, R p is the two-dimensional roughness, L′ is the two-dimensional trace projection length, n′ is the total number of two-dimensional trace point clouds, (x i ′,y i ′)、(x i ' +1 ,y i ' +1 ) are the two-dimensional coordinates of the i-th point and the i+1-th point on the two-dimensional trace.

6. A method for characterizing the roughness of a full-trace section according to claim 1, characterized in that: The calculation formula of the three-dimensional roughness is: in, are the sum of the roughness of the two-dimensional traces in the length direction of the section, the sum of the roughness of the two-dimensional traces in the width direction, and the three-dimensional roughness of the section, respectively. m and n are the total number of single two-dimensional trace point clouds in the length and width directions of the section, respectively. α and β are the effective scanning lines in the length and width directions, respectively. L and D are the length and width of the material section, respectively. (x j ,y j ,z j )、(x j+1 ,y j+1 ,z j+1 ) represents the three-dimensional coordinates of the j-th point and the j+1-th point on the two-dimensional trajectory.

7. A full trace cross-section roughness characterization system, characterized in that: include: Data acquisition module: scan the material section and obtain the surface point cloud data of the section; Trace extraction module: extracting cross-section two-dimensional traces according to the surface point cloud data; Roughness calculation module: calculates the two-dimensional roughness of each two-dimensional trace respectively, and uses each of the two-dimensional roughness to calculate the three-dimensional roughness of the cross section.

Citation Information

Patent Citations

  • Structural surface three-dimensional roughness coefficient determining method based on progressive sampling

    CN109443256A

  • Full-coverage sampling method for three-dimensional surface topography of a structural surface

    CN109493424A

  • Determination of 3D roughness coefficients of structural planes based on full coverage sampling

    CN109509184A

  • Slope excavation digital construction and quality control method

    CN110409369A

  • Automatic earth surface roughness measuring device and method

    CN114777690A

Cited By

  • Fracture surface fractal dimension calculation method of brittle material, storage medium and electronic equipment

    CN122471878A