Method for rapidly judging hydrophilicity and hydrophobicity of wafer surface

By forming a photoresist layer on the wafer surface and judging the hydrophilicity of the wafer surface using the mask development pattern, the complex measurement problem in the prior art is solved, and a fast and accurate hydrophilicity judgment is achieved.

CN118961512APending Publication Date: 2024-11-15SHANGHAI HUAHONG GRACE SEMICON MFG CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410907039.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

In the prior art, measuring the hydrophilicity of wafer surfaces is complex and requires a quick judgment method.

Method used

By forming a photoresist layer on the wafer surface and developing a specific pattern on the mask plate with a light transmittance higher than the preset value, the hydrophilicity of the wafer surface is judged based on the development morphology. If the pattern development is not missing, it will be biased. Hydrophobicity, if there is a lack, it is hydrophilic.

Benefits of technology

The rapid and accurate judgment of the hydrophilicity of the wafer surface is achieved, the measurement process is simplified, and complex operations in the prior art are avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118961512A_ABST
    Figure CN118961512A_ABST
Patent Text Reader

Abstract

The invention provides a method for quickly judging the hydrophilicity and hydrophobicity of a wafer surface, which comprises the following steps: providing a front-layer structure of which the hydrophilicity and hydrophobicity are to be detected, and removing a tackifier or not forming the tackifier before spin coating of photoresist on the front-layer structure; forming a photoresist layer on the front layer structure; a mask with the light transmittance higher than a preset value is selected, the mask comprises a specific pattern, the specific pattern can present different developing morphologies according to the hydrophilic-hydrophobic property, and then the mask is used for patterning the photoresist layer; judging the hydrophilicity and hydrophobicity of the front-layer structure according to the morphology of the specific pattern after development on the photoresist layer; if the specific pattern is not lost after development on the photoresist layer, judging that the front-layer structure is slightly hydrophobic; and if the specific pattern is missed in development on the photoresist layer, judging that the front-layer structure is partially hydrophilic. According to the invention, the hydrophilicity and hydrophobicity of the wafer surface can be rapidly determined.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for rapidly judging the hydrophilicity and hydrophobicity of a wafer surface. Background Art

[0002] The main component of the wafers currently used in semiconductors is silicon dioxide, which does not contain hydrophilic groups such as hydroxyl or carboxyl groups in its chemical structure. These groups usually make the surface of a material hydrophilic, so the wafer surface is highly hydrophobic.

[0003] The hydrophilicity and hydrophobicity of the wafer surface is a point that is easily overlooked and may affect the performance of the entire chip. From photoresist coating to cleaning and wetting, or the preparation of certain thin films, appropriate surface hydrophilicity and hydrophobicity need to be adapted.

[0004] See also Figure 1 At present, the commonly used method for determining hydrophilicity and hydrophobicity is the contact angle measurement method. The contact angle refers to the angle formed by the contact between the liquid and the solid surface. The contact angle of the hydrophilic surface is less than 90 degrees, and the contact angle of the hydrophobic surface is greater than 90 degrees. By measuring the contact angle, the hydrophilicity and hydrophobicity of the solid surface can be known. This method requires professional tools and methods and is relatively complicated.

[0005] ,To solve the above problems, it is necessary to propose a new ,method to quickly judge the hydrophilicity and hydrophobicity of the wafer surface. Summary of the invention

[0006] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a method for quickly judging the hydrophilicity and hydrophobicity of a wafer surface, so as to solve the problem that measuring the contact angle to obtain the hydrophilicity and hydrophobicity of a solid surface in the prior art is relatively complicated.

[0007] To achieve the above-mentioned object and other related objects, the present invention provides a method for quickly judging the hydrophilicity and hydrophobicity of a wafer surface, comprising:

[0008] Step 1, providing a front layer structure whose hydrophilicity and hydrophobicity are to be tested, wherein a tackifier needs to be removed or not formed before spin coating the photoresist on the front layer structure;

[0009] Step 2, forming a photoresist layer on the front layer structure;

[0010] Step 3, selecting a mask with a transmittance higher than a preset value, wherein the mask includes a specific pattern, and the specific pattern can present different development morphologies according to hydrophilicity and hydrophobicity, and then using the mask to pattern the photoresist layer;

[0011] Step 4: judging the hydrophilicity and hydrophobicity of the front layer structure according to the morphology of the specific pattern after the development of the photoresist layer:

[0012] If the specific pattern is developed on the photoresist layer without any defect, it is judged that the front layer structure is partially hydrophobic;

[0013] If the specific pattern is missing when developed on the photoresist layer, it is determined that the front layer structure is partially hydrophilic.

[0014] Preferably, the front layer structure in step one is a wafer or a thin film formed on the wafer.

[0015] Preferably, the material of the thin film in step 1 is an oxide layer or a nitride layer.

[0016] Preferably, the material of the adhesion promoter in step one includes hexamethyldisilazane, which reacts with hydroxyl groups on the surface of the wafer to change the surface of the wafer from hydrophilic to hydrophobic, so as to improve the adhesion between the photoresist layer and the wafer.

[0017] Preferably, the light transmittance of the mask in step three is greater than 80%.

[0018] Preferably, the specific graphics in step three are multiple broken line graphics.

[0019] Preferably, in step 4, a post-development measurement method is used to obtain the post-development morphology of the photoresist layer.

[0020] As described above, the method for quickly determining the hydrophilicity and hydrophobicity of a wafer surface of the present invention has the following beneficial effects:

[0021] The present invention can quickly determine the hydrophilicity and hydrophobicity of the wafer surface. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 Shown is a schematic diagram of determining the hydrophilicity and hydrophobicity of a wafer surface in the prior art;

[0023] Figure 2 Shown is a schematic diagram of a method for rapidly determining the hydrophilicity and hydrophobicity of a wafer surface according to the present invention;

[0024] Figure 3 Shown is a development schematic diagram of the present invention;

[0025] Figure 4 Shown is a schematic diagram of the morphology of the hydrophobic surface after development of the present invention;

[0026] Figure 5 Shown is a schematic diagram of the morphology of the hydrophilic surface after development of the present invention. DETAILED DESCRIPTION

[0027] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0028] See also Figure 2 The present invention provides a method for quickly judging the hydrophilicity and hydrophobicity of a wafer surface, comprising:

[0029] Step 1, providing a front layer structure to be tested for hydrophilicity and hydrophobicity, and removing a tackifier or not forming a tackifier before spin coating photoresist on the front layer structure;

[0030] In some embodiments, the front layer structure in step 1 is a wafer 1 or a thin film 2 formed on the wafer 1 .

[0031] In some embodiments, the material of the thin film 2 in step 1 is an oxide layer or a nitride layer or other known materials.

[0032] In some embodiments, the material of the adhesion promoter in step 1 includes hexamethyldisilazane, which reacts with hydroxyl groups on the surface of wafer 1 to change the surface of wafer 1 from hydrophilic to hydrophobic, thereby improving the adhesion between photoresist layer 3 and wafer 1 .

[0033] Step 2: forming a photoresist layer 3 on the front layer structure;

[0034] Step 3, selecting a mask with a transmittance higher than a preset value, the mask including a specific pattern, the specific pattern can present different development morphologies according to hydrophilicity and hydrophobicity, and then using the mask to pattern the photoresist layer 3;

[0035] In some embodiments, the transmittance of the mask in step three is greater than 80%.

[0036] In some embodiments, the specific graphics in step 3 are multiple broken line graphics. It should be noted that the specific graphics here can present different development morphologies according to hydrophilicity and hydrophobicity, and can also adopt other shapes, which are not specifically limited here.

[0037] Step 4: judging the hydrophilicity and hydrophobicity of the front layer structure according to the morphology of the specific pattern after the development of the photoresist layer 3:

[0038] If the specific pattern is developed on the photoresist layer 3 without any defect, it is judged that the front layer structure is partially hydrophobic;

[0039] If there is a defect in the development of a specific pattern on the photoresist layer 3, it is determined that the previous layer structure is hydrophilic.

[0040] In some embodiments, in step 4, a post-development measurement method is used to obtain the post-development morphology of the photoresist layer 3 .

[0041] For example, a thin film 2 is formed on a wafer 1, a photoresist layer 3 is formed on the thin film 2, the material of the thin film 2 is an oxide layer or a nitride layer, and the specific pattern is a plurality of broken line patterns;

[0042] See also Figure 4 , the specific pattern is developed on the photoresist layer 3 without loss, and the front layer structure is partially hydrophobic;

[0043] See also Figure 5 , there is a lack of specific graphics developed on the photoresist layer 3, and the front layer structure is hydrophilic.

[0044] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner. Therefore, the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0045] In summary, the present invention can quickly determine the hydrophilicity and hydrophobicity of the wafer surface. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has high industrial utilization value.

[0046] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for quickly judging the hydrophilicity and hydrophobicity of a wafer surface, characterized in that: At least: Step 1, providing a front layer structure whose hydrophilicity and hydrophobicity are to be tested, wherein a tackifier needs to be removed or not formed before spin coating the photoresist on the front layer structure; Step 2, forming a photoresist layer on the front layer structure; Step 3, selecting a mask with a transmittance higher than a preset value, wherein the mask includes a specific pattern, and the specific pattern can present different development morphologies according to hydrophilicity and hydrophobicity, and then using the mask to pattern the photoresist layer; Step 4: judging the hydrophilicity and hydrophobicity of the front layer structure according to the morphology of the specific pattern after the development of the photoresist layer: if the specific pattern is developed on the photoresist layer without defect, the front layer structure is judged to be partially hydrophobic; If the specific pattern is missing when developed on the photoresist layer, it is determined that the front layer structure is partially hydrophilic.

2. The method for rapidly determining the hydrophilicity and hydrophobicity of a wafer surface according to claim 1, characterized in that: The front layer structure in step 1 is a wafer or a thin film formed on the wafer.

3. The method for rapidly determining the hydrophilicity and hydrophobicity of a wafer surface according to claim 3, characterized in that: The material of the thin film in step 1 is an oxide layer or a nitride layer.

4. The method for rapidly determining the hydrophilicity and hydrophobicity of a wafer surface according to claim 1, characterized in that: The material of the adhesion promoter in step 1 includes hexamethyldisilazane, which reacts with hydroxyl groups on the surface of the wafer to change the surface of the wafer from hydrophilic to hydrophobic, so as to improve the adhesion between the photoresist layer and the wafer.

5. The method for rapidly determining the hydrophilicity and hydrophobicity of a wafer surface according to claim 1, characterized in that: The light transmittance of the mask in step three is greater than 80%.

6. The method for rapidly determining the hydrophilicity and hydrophobicity of a wafer surface according to claim 1, characterized in that: The specific graphics in step three are multiple broken line graphics.

7. The method for rapidly determining the hydrophilicity and hydrophobicity of a wafer surface according to claim 1, characterized in that: In step 4, the post-development morphology of the photoresist layer is obtained by using a post-development measurement method.