Plating current and deplating current for material coplanary in semiconductor plating process
By alternately applying forward plating current and reverse deplating current in the plating chamber, combined with substrate pattern characteristics and physical parameters, the problems of material coplanarity and uniformity in the semiconductor plating process are solved, achieving more efficient Plating process.
Patent Information
- Application Number
- CN202380032473.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-03
- Filing Date
- 2023-01-13
- Publication Date
- 2024-11-15
AI Technical Summary
In semiconductor plating processes, pattern density changes lead to differences in local current density and ion concentration, affecting the uniformity of deposition thickness. It is difficult for the prior art to effectively improve the material coplanarity in the plating chamber and the uniformity in the substrate.
By alternately applying the forward plating current and reverse deplating current in the plating chamber, combined with the pattern characteristics and physical parameters of the substrate, the plating process is optimized by calculating the working cycle and current value to ensure uniformity of the material. Deposition and removal.
The material uniformity and coplanarity within the die are significantly improved, the dependence on individual deplating chambers and liquid chemicals is reduced, and the substrate batch processing speed and material height uniformity is improved.
Smart Images

Figure CN118974910A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the benefit of and priority to U.S. Non-Provisional Application No. 17 / 686,129, filed on March 3, 2022, and entitled “PLATING AND DEPLATING CURRENTS FOR MATERIAL CO-PLANARITY IN SEMICONDUCTOR PLATING PROCESSES,” the contents of which are incorporated herein by reference in their entirety for all purposes. Technical Field
[0003] The field of the invention is the electroplating of semiconductor material substrates or wafers, and other similar types of substrates. Background Art
[0004] Metallization of electrical connections has been widely used in many semiconductor applications, ranging from dual damascene to various packaging structures, including C4 bumping, pillars, micro-bumps, redistribution layers (RDL), through-silicon vias (TSV), etc. Such metallization is usually performed using techniques such as electrodeposition of different metals, such as copper, gold, nickel, solder and others. As technology advances, chip layouts increasingly have features and pattern densities that are difficult to plate or metallize uniformly.
[0005] Electrodeposition of advanced microelectronic device packaging typically uses a mask or photoresist layer to define the pattern of metal lines or contacts. The pattern can also be defined by a non-reactive or non-conductive surface. As used herein, the term patterned substrate refers to a substrate having a mask or photoresist layer or non-reactive or non-conductive areas. The pattern density can vary between sparsely patterned areas and densely patterned areas. This causes corresponding changes in local current density and differences in ion concentration, which affects the uniformity of deposition thickness within the die (so-called within die non-uniformity or WID non-uniformity).
[0006] A technique for improving thickness uniformity or thickness flatness (levelling) is to reduce the overall applied current density. Alternatively, a plating bath with high throwing power (throwing power) can be used. Throwing power can be defined as the ability of a plating bath to produce a deposit of more or less uniform thickness on a cathode with macroscopic irregularities. The higher the throwing power, the more uniform the resulting deposit. For example, in the case of a copper acid bath, a common bath formula with high throwing power is a formula with low copper concentration and high acid concentration. However, improved plating technology is needed. Summary of the invention
[0007] In some embodiments, a method of plating a substrate may include placing the substrate in a plating chamber containing a liquid and applying an electric current to the liquid in the plating chamber to deposit metal on exposed portions of the substrate, wherein the electric current may include alternating cycles of a forward plating current and a reverse deplating current.
[0008] In some embodiments, a system may include a plating chamber including a liquid and a controller configured to receive a substrate, wherein the controller may be configured to cause an electric current to be applied to the liquid in the plating chamber to deposit metal on exposed portions of the substrate, wherein the electric current may include alternating cycles of a forward plating current and a reverse deplating current.
[0009] In some embodiments, a non-transitory computer-readable medium may include instructions that, when executed by one or more processors, cause the one or more processors to perform operations, the operations comprising simulating a model of a substrate in a plating process to generate data points that relate characteristics of the plating process and a pattern on the substrate to a range of non-uniformities of material formed on the substrate during the plating process; using information from these data points, determining values for a forward plating current and a reverse deplating current to be applied in a plating chamber; and providing values for the forward plating current and the reverse deplating current to the plating chamber to perform the plating process.
[0010] In any embodiment, any and all of the following features may be implemented in any combination and without limitation. The substrate may include a photoresist or mask layer that defines a pattern on the substrate, and the pattern may include an exposed portion of the substrate adjacent to an open area, wherein the current density during the plating process may be more concentrated on the exposed portion of the substrate adjacent to the open area than the exposed portion of the substrate that is not adjacent to the open area. During the forward plating current, the metal may be unevenly deposited on the exposed portion of the substrate. During the reverse deplating current, the metal may be removed so that the metal becomes evenly distributed on the exposed portion of the substrate. When the substrate is in a liquid, both the forward plating current and the reverse deplating current may be applied in an alternating cycle in the plating chamber without using a separate chamber or liquid to apply the forward plating current and the reverse deplating current. The exposed portion of the substrate may include a plurality of silicon vias (TSVs), wherein the difference between the maximum height of the TSV and the minimum height of the TSV may be greater than the threshold distance. Before applying current to the liquid in the plating chamber, the method / operation may also include a model of the substrate simulated during the plating process to generate data points, which relate the characteristics of the plating process and the pattern on the substrate to the predicted range non-uniformity of the metal on the substrate for the forward plating current and the reverse deplating current. Before applying current to the liquid in the plating chamber, the method / operation may also include using the data points that relate the characteristics of the plating process and the pattern on the substrate to the predicted range non-uniformity of the metal on the substrate to determine the value for the reverse deplating current. Before applying current to the liquid in the plating chamber, the method / operation may also include using the data points that relate the characteristics of the plating process and the pattern on the substrate to the predicted range non-uniformity of the metal on the substrate to determine the duty cycle for the alternating cycle of the forward plating current and the reverse deplating current. The controller may be further configured to apply the alternating cycle of the forward plating current and the reverse deplating current based at least in part on the rotation speed of the substrate in the plating chamber. The controller may be further configured to apply alternating cycles of forward plating current and reverse deplating current based at least in part on the movement of the paddle in the plating chamber. The plating chamber may include an electrochemical deposition chamber, and the liquid may include an electrolyte. The time for applying the forward plating current may be at least 10 times longer than the deplating current. Determining the values for the forward plating current and the reverse deplating current may include receiving a target deposition rate for the plating process; receiving a forward plating rate for the plating process; determining a reverse deplating rate for the plating process; and / or determining a duty cycle for the forward plating current and the reverse deplating current based on the target deposition rate, the forward plating rate, and the reverse deplating rate. The reverse deplating rate may minimize the range non-uniformity of the material formed on the substrate during the plating process. The data points associating the characteristics of the plating process and the pattern on the substrate with the range non-uniformity of the material formed on the substrate during the plating process may include a linear or non-linear relationship. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] A further understanding of the nature and advantages of the various embodiments may be achieved by reference to the remainder of the specification and the drawings, wherein like reference numerals are used throughout the several drawings to designate like parts. In some cases, a sub-label is associated with a reference numeral to indicate one of a plurality of similar parts. When a reference numeral is cited without specifying the presence of a sub-label, it is intended to refer to all such plurality of similar parts.
[0012] Figure 1 and Figure 2 An electrochemical processor according to some embodiments is illustrated.
[0013] Figure 3 A substrate that may be subjected to non-uniform plating is illustrated according to some embodiments.
[0014] Figure 4 A conventional method for plating and deplating material from a feature to achieve a non-uniform coplanar design is illustrated in accordance with some embodiments.
[0015] Figure 5 A single chamber configuration for plating and deplating materials for coplanarity is shown in accordance with some embodiments.
[0016] Figure 6 Illustrated is a graph and relationship that may be used to determine forward current characteristics and reverse current characteristics for combined plating and deplating processes in a single chamber according to some embodiments.
[0017] Figure 7 Graph illustrating paddle motion and substrate rotation according to some embodiments.
[0018] Figure 8 The graph shows a characterizing curve that can be generated for a target deposition rate for a given process.
[0019] Fig. 9 A flow chart illustrating a method for plating a substrate according to some embodiments.
[0020] Fig.10 A flow chart illustrating a method for determining forward and reverse current values for a plating process, according to some embodiments.
[0021] Fig.11 An example computer system is shown in which various embodiments may be implemented. DETAILED DESCRIPTION
[0022] Embodiments described herein provide for the improved method of plating substrate with material while maximizing uniformity and coplanarity in bare chip. In the case of the number / position of open areas with unique pattern, mask and bare chip, each patterned substrate will react differently in the plating chamber. The open area covered by mask or photoresist layer can cause electric current to converge on adjacent exposed areas during plating process, causing more material to be deposited on these adjacent exposed areas. Traditionally, substrate is then transferred from plating chamber to separate plating chamber and enters electrochemical bath with low conductivity. Reverse current is then applied to remove the redundant material on substrate, so that via (via) and trace (trace) finally reach consistent height. However, when processing substrate batches with the same pattern, transferring substrate to separate chamber, using different chemicals in liquid and changing the used all-plating capacity during plating process cause bottleneck.
[0023] These embodiments improve batch processing patterned substrates and improve the uniformity of plating process by maintaining substrate in the same processing chamber and in the same liquid bath to apply the alternating current circulation of forward plating current and reverse deplating current.Technology can first produce the relationship of graph or data, and the relationship of described graph or data relates range non-uniformity to the physical parameter of technology.This data set can then be used to calculate the part of duty cycle, and during the described part of process cycle, the forward plating current in reverse deplating current can be applied.This curve can also be used to determine the forward and reverse current that should be applied in order to reach the target plating rate.The frequency of forward / reverse current circulation can be made consistent with the substrate rotation and paddle movement in the chamber, to ensure that technology is uniformly applied.This increment is applied and in the same chamber, the removal of the material using forward and reverse current improves the overall uniformity of material height across bare chip, bare chip coupon (coupon) and substrate as a whole, and greatly improves the speed that each substrate can be processed.
[0024] By way of example, a plating chamber using an electrochemical deposition (ECD) process is described below. However, other plating processes besides ECD can be used with the forward / reverse current technique described herein. Therefore, this specific ECD chamber and ECD process are generally not meant to be limiting.
[0025] Figure 1 and Figure 2An electrochemical processor 20 according to some embodiments is shown. The electrochemical processor 20 may include a head positioned above a container assembly 50. The container assembly 50 may be supported on a deck plate 24 or a relief plate 26, which is attached to a bracket 38 or other structure. A single processor 20 may be used as a stand-alone unit. Alternatively, multiple processors 20 may be provided in an array, with workpieces loaded into and unloaded from the processor by one or more robots. The head 30 may be supported on a lift / rotation unit 34 for lifting and inverting the head 30 to load and unload workpieces into the head, and for lowering the head 30 to engage with the container assembly 50 for processing.
[0026] Electrical control and power cables 40 may be connected to the lift / rotate unit 34 and to the internal head assembly and may lead from the processor 20 to a facility connection, or to a connection within a multi-processor automation system. A purge assembly 28 having a tiered drain ring may be provided above the container assembly 50. A drain pipe 42 may connect the purge assembly 28 (if used) to a facility drain. An optional lift 36 may be provided below the container assembly 50 to support the anode cup when the anode is replaced. Alternatively, the lift 36 may be used to hold the anode cup upward against other portions of the container assembly 50.
[0027] The container assembly 50 may include an anode housing 52, a lower diaphragm support 54, and an upper diaphragm support 56 held together by fasteners 60. Within the anode housing 52, a first or inner anode 70 may be positioned near the bottom of an inner anolyte chamber 110. A second or outer anode 72 may be positioned near the bottom of an outer anolyte chamber 112 surrounding the inner anolyte chamber 110. The inner anode 70 may be a flat circular metal plate, and the outer anode 72 may be a flat annular metal plate, such as a platinum-plated titanium plate. The inner anolyte chamber and the outer anolyte chamber may be filled with copper particles. The inner anode 70 may be electrically connected to a first electrical lead or connector 130, and the outer anode 72 may be electrically connected to a separate second electrical lead or connector 132. In some embodiments, for example, to process 300 mm diameter wafers, the processor may have a central anode and a single outer anode. Designs with three or more anodes may also be optionally used, especially for even larger wafers.
[0028] The upper cover 76 may be housed within or surrounded by the upper cover housing 58. The upper cover housing 58 may be attached to and sealed against the upper cover 76. The upper cover housing 76 may have a curved upper surface 124 and a central through opening that forms a central or inner catholyte chamber 120. This chamber 120 is defined by a generally cylindrical space within the diffuser 74 leading to a bell-shaped or angular space defined by the curved upper surface 124 of the upper cover 76. A series of concentric annular grooves extend downwardly from the curved upper surface 124 of the upper cover 76. The outer catholyte chamber 78 formed by the bottom of the upper cover 76 is connected to the ring via an array of tubing or other passages.
[0029] Similarly, a second or outer diaphragm 86 may be secured between upper and lower diaphragm supports and may separate outer anolyte chamber 112 from outer catholyte chamber 78. Outer diaphragm supports 89, which may be provided in the form of radial legs 116 on upper diaphragm support 56, support the outer diaphragm from above.
[0030] A diffuser peripheral horizontal supply conduit 84 may be formed in the outer cylindrical wall of the upper shroud 76, with the conduit 84 sealed between the outer wall of the upper shroud 76 and the inner cylindrical wall of the upper shroud housing 58 by an O-ring or similar element. A radial supply conduit 80 may extend radially inward from the peripheral conduit 84 to an annular shroud plenum 87 surrounding the upper end of the diffuser shroud 82. The radial conduit 80 passes through the upper shroud 76 between vertical tubulars that connect annular grooves in the curved upper surface 124 of the upper shroud 76 to the outer catholyte chamber 78. The peripheral conduit 84 and the radial conduit 80 lead to the shroud plenum 87, while an outer catholyte path may be formed between the diffuser shroud 82 and the diffuser 74. During operation of the processor 20, these outer catholyte paths may normally be filled with liquid catholyte.
[0031] In use, a workpiece, typically with a conductive seed layer, is loaded into the head. In some embodiments, the workpiece is first loaded into a wafer carrier or wafer holder, and then the wafer carrier / folder can be transferred into the chamber. The seed layer on the workpiece is connected to an electrical supply, typically to a cathode. If the head is loaded in a face-up position, the head is flipped so that the rotor and the workpiece held in the rotor face downward. The head is then lowered onto the container until the workpiece contacts the cathode liquid in the container. The spacing between the workpiece and the curved upper surface of the upper cover affects the uniformity of the current density at the surface of the workpiece. This gap can change during processing. The workpiece can be moved upward and gradually away from the surface, or the workpiece can be quickly moved from the starting gap to the ending gap. A lifting / rotating mechanism can be used to lift the head.
[0032] Anolyte is provided into the inner anolyte chamber and separately into the outer anolyte chamber. Catholyte is provided into the surrounding supply conduit. Catholyte is supplied to the inlet fitting. The workpiece is moved into contact with the catholyte, typically by lowering the head. Current is opened to the anodes 70 and 72 by current from the anode through the anolyte in the inner and outer anolyte chambers. Current from the inner and outer anodes passes through the anolyte and through the inner and outer diaphragms and into the catholyte contained in the open space in the upper cover 76.
[0033] Within the upper shroud 76, the catholyte flows radially inward from the supply conduit 84 to the diffuser cover plenum 87 and then into the diffuser 74. The catholyte flows upward from the diffuser 74 and moves radially outward in all directions through the curved upper surface 124 of the upper shroud 76. The metal ions in the catholyte are deposited onto the workpiece, establishing a metal layer on the workpiece. The motor can be turned on to rotate the rotor and workpiece to provide a more uniform deposition on the workpiece. Most of the catholyte then flows into the collection ring 122. A small portion of the catholyte flows downward through the grooves and tubing into the outer catholyte chamber 78. The catholyte then flows out of the processor 20.
[0034] Figure 3 A substrate 302 that may be subjected to non-uniform plating according to some embodiments is illustrated. The substrate 302 may include any type of material, such as a silicon semiconductor substrate on which integrated circuits or other electrical components may be fabricated. The substrate 302 may include a plurality of individual dies 304. When processing is complete, the substrate 302 may be separated into individual dies 304 and packaged individually. When considering the uniformity of a material layer formed on the substrate 302, some processes may focus on uniformity within a single die 304. Other processes may focus more on uniformity within a sample, or within a subset of dies on the substrate 302. Other processes may additionally or alternatively focus on uniformity across the substrate 302 as a whole.
[0035] The terms "wafer," "workpiece," and "substrate" may be used interchangeably herein. The substrate may have a variety of shapes, sizes, and materials. The present method may be used in plating copper as well as other materials, such as silver, gold, nickel, cobalt, palladium, tin, and the like. A patterned substrate may refer to a substrate having a photoresist or mask layer that defines a pattern. Alternatively, a patterned substrate may refer to a substrate containing patterned structures, such as a redistribution layer (RDL) after photoresist removal, or a through silicon via (TSV) layer after plating. Although patterning on a substrate is typically a source of non-uniformity in the plated film, the present method may be used to provide a more uniform plated film regardless of the source of the non-uniformity in the initial plated film.
[0036] During the plating process, the substrate 320 may be immersed in a liquid electrolyte, and a forward current may be applied to the anode in the chamber to deposit a metal layer on the substrate 302. For example, each die 304 may include a mask or photoresist layer that covers the die 304. The area on the mask may leave a portion of the substrate exposed to the plating process. In this example, the mask on the die 304 may leave a series of circular openings on the surface of the die 304, and metal vias may be deposited on this surface. Any gaps in the mask that leave the substrate exposed to the plating process may be referred to as "exposed" areas of the substrate.
[0037] The purpose of most plating processes is to deposit material uniformly on the exposed areas of substrate 302. However, each new design for substrate pattern may have a unique layout, feature density and circuit pattern of the open areas of the design itself, as defined by the mask during the plating process. Because these patterns will be different for each design, the current can be collected differently during the plating process. For example, the die 304 includes a large open area in the center of the die 304. The term "open" area as used herein may refer to an area or gap that does not include features in the mask that retains the substrate exposure. For example, the large open area on the die 304 may include a central section of the die 304, where the density of the exposed area is significantly less than the area with vias around the open area. The chemical bath liquid can evenly cover the die, and the current can flow through the chemical in a relatively uniform manner. However, during plating, the open area can cause the current flux to gather (funnel) from these open areas to the adjacent vias. It is also more difficult to evenly deliver the current to the relatively dense via area. For example, current may tend to collect or concentrate in an open area at the center of the die 304, and thus concentrate more heavily into features defined by exposed portions of the substrate 302 adjacent to the open area. This may include vias 306 adjacent to the open area. When more current concentrates into these vias adjacent to the open area, more material will be deposited into these vias during the plating process.
[0038] The cross-sectional view 300 of the die 304 illustrates how an exposed area 310 of the die 304 adjacent to an open area in the center of the die 304 can cause more material to be plated in the exposed area 310. The photoresist mask 308 can leave the via open (e.g., 200 microns deep), and then fill the via with metal during the plating process. This causes the via to have a higher height than other exposed areas 312 that are not adjacent to the open area, even though the mask 308 may have the same uniform height. Coplanarity can be defined as the difference between the maximum height of the via (or other feature) and the minimum height of the via (or other feature). Coplanarity is usually measured as maximum-minimum on the same die 304, but can also be measured on a sample of the die and or the substrate 302 as a whole.
[0039] Figure 4 The conventional method for plating and removing materials from features to achieve uniform coplanar design according to some embodiments is illustrated. First, substrate 406 may be placed in plating chamber 402. Plating chamber 402 may include liquid chemicals having relatively high conductivity. A forward current may then be applied through the liquid to perform the plating process. A forward current may be defined as a current configured to cause material to form on the substrate. As described above, this forward current process in plating chamber 402 may cause non-coplanar features across the die or the substrate as a whole. Although other types of substrates or metals may be used, the substrate may include a silicon wafer plated with an initial pattern copper film. This patterning may affect current density during plating, making the initial plated film somewhat non-uniform. For example, the initial film may be at least 3, 5, 8, or 10% non-uniform (per three sigma / mean). The initial metal film may be formed in various ways, such as electrochemical deposition (plating).
[0040] To remove excess material, substrate 406 is then moved from plating chamber 402 to deplating chamber 404. For example, deplating chamber 404 typically contains a low conductivity liquid solution, compared to the high conductivity liquid of plating chamber 402. Deplating chamber 404 then applies a reverse current through the liquid to perform the deplating process. Reverse current can be defined as a current configured to cause material to be removed from the substrate. Using a low conductivity electrolyte bath causes the reverse process to be amplified and remove material faster from vias adjacent to open areas, ultimately balancing feature heights across the die. This allows the process to preferentially remove material from taller vias and achieve coplanarity.
[0041] For example, substrate 406 can be moved into deplating chamber 404, which is adapted for non-uniform deplating. Deplating chamber 404 can have a low throwing power, such as a lower throwing power than plating chamber 402. The deplating bath can have a low conductivity, such as 1mS / cm to 250mS / cm or from 10mS / cm to 100mS / cm. When in the deplating bath, the plated substrate can be partially electroetched or deplated in the deplating bath by conducting a reverse current through the substrate and the bath. Like the plating step, the deplating step can be non-uniform. For example, the deplating step can remove metal from the protrusion faster than from the surrounding area. The remaining metal film can therefore become more uniform. Deplating substrate 406 can be cleaned and dried, and / or then moved for additional chemical or electrochemical treatment.
[0042] Figure 5A single chamber configuration for plating and deplating materials for coplanarity is illustrated in accordance with some embodiments. To improve the plating process, the embodiments described herein may use the same chamber 502 to perform the plating and deplating processes described above. This greatly improves the uniformity of the height of the material within the die or substrate, eliminates the need for a separate chamber for performing the deplating process, and greatly improves the speed at which batches of substrates can be processed. This also eliminates the need to use two separate chemistries in different liquid baths in separate chambers.
[0043] The substrate 506 can be placed in the plating chamber 502. The plating and deplating currents can then be applied to the substrate 506 in the same liquid or chemical bath used for both the plating and deplating processes. For example, the liquid may contain a single electrolyte, such as an anolyte or a catholyte from the same solution or like the same tank. Instead of relying on a change in the chemical chemistry of the liquid to produce the increased effect required for the deplating process, these embodiments use a duty cycle forward current 512 and a reverse current 510. The current levels for the forward current 512 and the reverse current 510 can also be adjusted to produce an increased removal effect. Recall that during the electroplating process, an increased reverse current effect is required to preferentially remove material from the areas of the substrate that are exposed through the mask and are subject to current collection. This duty cycle and the use of the same chamber allow the process to incrementally correct differences in the planarity of the die because this process occurs instead of producing very large errors and attempting to correct errors in a separate deplating process. This brings more accurate and more uniform material heights.
[0044] At Figure 5The diagram 500 illustrated in the figure illustrates an example of how a forward current 512 can be cycled using a square wave with a reverse current 510. Typically, the forward current 512 can occupy a large portion of the duty cycle compared to the reverse current 510. For example, the application time of the forward current 512 can be at least 10 times longer than the application time of the reverse current 510. Note that the square wave in the diagram 500 is provided only by way of example and is not meant to be limiting. Numerous other square waves can be used in addition to a regular square wave to apply a forward current 512 and a reverse current 510. At different stages of recipe execution, some recipes can also be used with the amount and length of the intervals for the forward current 512 and / or the reverse current 510 being changed. Some embodiments can also apply alternating forward currents 512 and reverse currents 510 during a portion of the recipe, while applying other waveforms or DC currents during the remainder of the recipe. For example, a recipe for a plating chamber can include alternating reverse current and forward current waveforms for a portion of the recipe, and a DC waveform for the remainder of the recipe. The recipe can include pulsed forward current, pulsed reverse current and DC waveform in any combination and without limitation. Multiple sequences of these waveforms can be performed individually or in loops. Therefore, alternating forward current 512 and reverse current 510 can be applied to all or any sub-parts of the plating process.
[0045] Figure 6 A graph 600 and a relationship are shown that can be used to determine forward current characteristics and reverse current characteristics for a combined plating and deplating process in a single chamber according to some embodiments. Because each substrate design can include different mask patterns, and because each process can use different target deposition rates, different liquid chemistries, and other unique physical properties, each design can be characterized to determine the appropriate duty cycle and current values for the forward and reverse currents during the process. This characterization can occur through a model that simulates the physical process, or by performing the plating / deplating process on a test substrate using experimental data. The experimental or simulated data can be gathered before performing the plating process on the current substrate (e.g., before applying the forward and reverse currents).
[0046] The graph 600 includes an x-axis representing a dimensionless parameter 612 that characterizes the substrate pattern and the plating chamber conditions. This parameter 612 may be referred to as λ and is defined as follows:
[0047]
[0048] The variables K, Wa, and D used in defining the lambda parameter 612 may be defined as follows:
[0049]
[0050] In these equations (2) to (4), K is a dimensionless number representing the product of the bath conductivity κ, the die width w, and the film resistance Rs, which represents the film resistivity divided by the film thickness. Wa stands for the Waggoner number, which is a dimensionless number that characterizes the solution and reflects the ratio of the interface resistance to the bath resistance and is a property well known in the electrochemical art. In this particular characterization, different values of α can be used for plating and deplating (e.g., αc for plating and αa for deplating), resulting in different values of Wa for plating and deplating in the same conditions as shown in graph 600. L pattern It can represent the characteristic length of the pattern on the die, and j ave It can represent the average current density of the via. D can represent the length L of the pattern. pattern The ratio of the distance, D, to the width w of the pattern can be approximated as a measure of the distance between sparse and dense areas on the die.
[0051] For a particular die pattern, various variables in the lambda parameter 612 can be adjusted and simulated to produce the resulting range non-uniformity 610 for the conditions represented on the y-axis of the graph 600. Each simulated data point can be plotted on the graph 600 for both the plating process and the deplating process. Note that these data points can also be aggregated with experimental data, using different bath conductivities and plating rates to characterize the range non-uniformity 610. Note that the graph 600 divides the range non-uniformity 610 by the average range non-uniformity to normalize the data so that different bath conductivities and film sheet resistances can be represented on the same graph 600.
[0052] An important observation from the ideal data plotted on the chart 600 is that when the range non-uniformity 610 is plotted relative to the λ parameter 612, the result is linear. This linear relationship is maintained in both the plating direction and the deplating direction. Therefore, the range non-uniformity 610 can be associated with a set of operating conditions, which are represented by the λ parameter 612 through the slope of the interpolated line 602 of the data points. The slope of this line 602 can be different for each substrate pattern. For example, in this example, using a set of experimental data, the slope of line 610 can be approximately 29.101. Note that this relationship may not be completely linear in the case of additive and other non-ideal factors. For non-linear data, a non-linear relationship can be similarly used to predict the range non-uniformity 610 from a given λ parameter 612.
[0053] For a linear relationship, the information from the data set of graph 600 can be simplified using a linear approximation. This yields a simple relationship between range non-uniformity 610 and lambda parameter 612 as follows:
[0054]
[0055] Equation (5) assumes a linear relationship between range non-uniformity 610 and lambda parameter 612, so that function G (λ) can be replaced by the numerical slope of linear relationship. For the data set that does not produce linear relationship, function G (λ) can be replaced by corresponding non-linear function, such as exponential or polynomial function. Use ideal linear data to simplify the quadratic solution process described below. However, for non-linear relationship, numerical solution method can be used to solve the following equation for duty cycle and deplating current. Therefore this relationship can be used to the characteristic of the pattern on the plating process and substrate is associated to the prediction range non-uniformity of metal on the substrate. As described below, this relationship can be used to determine the reverse deplating current and the value of duty cycle of the alternating cycle for forward plating current and reverse deplating current under given process and pattern.
[0056] The data in the relationship found experimentally or by simulation in graph 600 can be used to determine the duty cycle and deplating current that will result in a minimized range non-uniformity 610 that is ideally close to 0. An equation can be derived to determine the range non-uniformity based on corresponding plating and deplating conditions as follows:
[0057]
[0058] The left side of equation (6) represents the above average range non-uniformity. The right side of equation (6) represents this average range non-uniformity with respect to the physical properties of the pattern, electrochemical bath, etc. and the current density used for the plating step and the deplating step, where f represents the part of the working cycle for the plating process and 1-f represents the part of the working cycle for the deplating process.
[0059] To minimize the overall range non-uniformity for the combined process, the right hand side of the combined plating and deplating cycles of equation (6) can be set to 0. The only unknown in equation (6) is then the deplating current density (j deplate ). Plating current density (j plate ) and the overall current density (j target ) can be selected for the process. The dimensionless parameters can be determined as described above. Therefore, after setting equation (1) to 0, the deplating current density (j) required to minimize the range non-uniformity can be deplate ) to obtain the representation obtained by solving .
[0060] To solve equation (6), G(λ) = A(λ), where A is a dimensionless constant representing the slope of the linear relationship from graph 600 (e.g., 29.101 for a particular design), and λ is a dimensionless representation of the operating parameters for a particular process and substrate pattern. By setting the right hand side of equation (6) to 0, this solution leads to the deplating current density (j deplate) is a quadratic equation.
[0061]
[0062] Equation (2) can be solved using the quadratic equation formula.
[0063]
[0064] a=4KA-CD (9)
[0065] b=-C(2B+Dj target ) (10)
[0066] c=-2BCj target (11)
[0067] A=29.101 (12)
[0068]
[0069] Calculate the plating current density (j deplate ) This value can then be used to determine the f-value, which represents the portion of the duty cycle used in the plating process.
[0070]
[0071] Note that the value for f indicates only the portion of the duty cycle for each plating / deplating current cycle that will be used for the plating current. The total cycle time (eg, the frequency of alternating application of plating and deplating currents) may be selected based on other process considerations.
[0072] Additionally, the phase and frequency of the deplating current may be timed so that the deplating current is evenly distributed during other cycles in the plating process. Figure 7 Graph illustrating paddle motion and substrate rotation according to some embodiments. Line 704 indicates the angle of rotation used for the substrate during the plating / deplating process. Curve 702 represents the position of the paddle, which stirs the liquid chemistry in the plating chamber during the plating process. In some embodiments, the position of the paddle can use a staggered periodic motion.
[0073] The phase and / or cycle time of the duty cycle for the forward and reverse currents can be selected so that the reverse current can be evenly distributed relative to the rotation of the substrate and the movement of the paddle. In chart 700, segment 706 of curve 702 represents the portion of the duty cycle during which the reverse current is applied. Note that this captures an approximately complete cycle of paddle motion while also being distributed to different locations in the wafer cycle over time. Using paddle motion and a wafer as shown in chart 700, the alternating cycle of the forward plating current and the reverse deplating current can be based at least in part on the rotation speed of the substrate and / or the movement of the paddle in the plating chamber to ensure that the two current waveforms are applied as evenly as possible in the chamber.
[0074] Figure 8 The diagram shows a characterization curve that can be generated for a target deposition rate for a particular process. Using the above equations and algorithms, the deplating rate can be selected to minimize the range of non-uniformity of the material formed on the substrate during the plating process, as represented on the y-axis. For example, a set of characterization curves illustrated in chart 800 can be generated for a target deposition rate of 1 μm / m. Characterization curves can be generated for different forward plating rates, such as 4 μm / m (curve 802), allowed 2.5 μm (curve 804), 2 μm / m (curve 806), 1.5 μm / m (curve 808), etc. The corresponding deplating rate can be selected based on the minimum value of these characterization curves.
[0075] Fig. 9 A flow chart 900 of a method for plating a substrate according to some embodiments is illustrated. The method may include placing a substrate in a plating chamber containing a liquid (902). The plating chamber may include an electrochemical deposition chamber, and the liquid may include an electrolyte bath in which the substrate is immersed. The substrate may include a photoresist or mask layer that defines a pattern on the substrate, and the pattern may include exposed portions of the substrate adjacent to an open area on a die. The current density during the plating process may be more concentrated at the exposed portions of the substrate adjacent to the open area when compared to the exposed portions of the substrate not adjacent to the open area, as described above. Figure 3 As shown in . The exposed portion of the substrate may include through silicon vias (TSVs), and the difference between the maximum height of the TSV and the minimum height of the TSV may represent a measure of coplanarity or uniformity of the TSV height. For example, a maximum-minimum value below a threshold may represent coplanarity, while a maximum-minimum value above a threshold may represent an uneven distribution of material at different locations on the substrate.
[0076] The method may also include applying an electric current to the liquid in the plating chamber to deposit metal on the exposed portion of the substrate (904). The electric current may include an alternating cycle of a forward plating current and a reverse deplating current. During the forward plating current, due to current convergence or other effects, the metal may be unevenly deposited on the exposed portion of the substrate. During the reverse deplating current, the metal may be removed so that the metal becomes evenly distributed on the exposed portion of the substrate. The alternating cycle of this forward plating current and the reverse deplating current may be a duty cycle in the entire plating process to remove the coplanarity error introduced. For example, when the substrate is in the liquid, both the forward plating current and the reverse deplating current may be applied in the alternating cycle in the plating chamber, without using a separate chamber or liquid to apply the forward plating current and the reverse deplating current.
[0077] It should be understood that the diagram shown in Fig. 9 The specific steps in the present invention provide specific methods for coating substrates according to different embodiments. Other sequences of steps may also be performed according to alternative embodiments. For example, alternative embodiments may perform the above steps in a different order. Furthermore, in Fig. 9 The individual steps illustrated in the figure may include multiple sub-steps, which may be implemented in various orders suitable for the individual steps. Further, additional steps may be added or removed according to specific applications. Numerous variations, modifications and substitutions also fall within the scope of the present invention. These method steps may be implemented on a controller of a plating chamber or on a separate computer system.
[0078] Fig.10 Flowchart 1000 of a method for determining forward and reverse current values for a plating process according to some embodiments is illustrated. This method includes simulating a model of a substrate during a plating process to generate data points, which relate the characteristics of the plating process and the pattern on the substrate to the range of non-uniformity of the metal formed on the substrate during the plating process (1002). This simulation can be performed by any computer system, including a controller of a computer system and / or plating chamber described below. For example, a computer system and / or controller can access or receive information that describes the pattern on the substrate, and / or the configuration of the plating chamber and liquid bath, automatically retrieve or generate the results of the simulation, and implement the other steps shown in flowchart 1000 without human intervention. These steps can be performed as part of a recipe for a plating process. The data points can be as described above with respect to Figure 6 Described is produced.
[0079] The method may also include determining values for a forward plating current and a reverse deplating current to be applied to the plating chamber (1004). The values of the currents may be generated as described above with respect to Figure 6For example, a process may receive a target deposition rate and a forward plating rate for a deposition process, and then determine a reverse deplating rate and / or duty cycle for a forward / reverse current, as described above. Current values may also be determined to minimize the range non-uniformity of the material formed in the substrate during the plating process.
[0080] The method may further include providing values for a forward plating current and a reverse deplating current to a plating chamber to perform a plating process (1006). For example, the current values may be determined in a simulation, which may be executed on a separate computer system, and may be provided to a controller of the plating chamber. In some embodiments, the current values may be provided to a plurality of plating chambers that sequentially perform a plating process on batches of semiconductor substrates having the same pattern.
[0081] It should be understood that Fig.10 The specific steps illustrated in the figure provide a particular method for determining the forward and reverse currents for the plating process according to various embodiments. Other sequences of steps may also be implemented according to alternative embodiments. For example, alternative embodiments may perform the above steps in a different order. Furthermore, Fig.10 The individual steps in the method may include multiple sub-steps, which may be performed in various orders suitable for the individual steps. In addition, additional steps may be added or removed according to specific applications. Numerous changes, modifications and substitutions also fall within the scope of the present invention.
[0082] Each method described herein can be implemented by a computer system. Each step of these methods can be automatically executed by a computer system, and / or can be provided with input / output involving a user. For example, a user can provide input for each step in the method, and each of these inputs can respond to a specific output requesting such input, wherein the output is generated by a computer system. Each input can respond to a corresponding request output. In addition, the input can be received by a user, received as a data stream from other computer systems, retrieved from a memory location, retrieved through a network, requested from a network service, and / or the like. Similarly, the output can be provided to a user, provided to other computer systems as a data stream, stored in a memory location, sent through a network, provided to a network service, and / or the like. Simply put, each step described herein can be implemented by a computer system, and can involve any number of inputs, outputs, and / or requests of a computer system or from a computer system, which may or may not involve a user. These steps that do not involve a user can be referred to as being automatically implemented by a computer system without human intervention. Therefore, it will be understood that in light of the present disclosure, each step of each method described herein can be modified to include input and output to or from a user, or can be completed automatically by a computer without human intervention, in which case any determination is made by the processor. Further, some embodiments of each of the methods described herein can be implemented as a set of instructions stored on a tangible, non-transitory storage medium to form a tangible software product.
[0083] Fig.11 An example computer system 1100 is shown in which various embodiments may be implemented. System 1100 may be used to implement any of the above-described computer systems. As shown, computer system 1100 includes a processing unit 1104, which communicates with several peripheral subsystems via a bus subsystem 1102. These peripheral subsystems may include a processing acceleration unit 1106, an I / O subsystem 1108, a storage subsystem 1118, and a communication subsystem 1124. Storage subsystem 1118 includes a non-transitory tangible computer-readable medium and a system memory 1110. The non-transitory tangible computer-readable medium may store instructions that cause one or more processors to perform operations as described throughout this disclosure.
[0084] The bus subsystem 1102 provides a mechanism for allowing the various components and subsystems of the computer system 1100 to communicate with each other as intended. Although the bus subsystem 1102 is shown as a single bus, alternative embodiments of the bus subsystem may apply multiple buses. The bus subsystem 1102 may be any of several types of bus structures, including a memory bus or memory controller, a peripheral bus, and a local bus using any of a variety of bus architectures. For example, such an architecture may include an Industry Standard Architecture (ISA) bus, a Micro Channel Architecture (MCA) bus, an Enhanced ISA (EISA) bus, a Video Electronics Standards Association (VESA) local bus, and a Peripheral Component Interconnect (PCI) bus, which may be implemented as a Mezzanine bus manufactured to the IEEE P1386.1 standard.
[0085] Processing unit 1104 may be implemented as one or more integrated circuits (e.g., conventional microprocessors or microcontrollers) to control the operation of computer system 1100. One or more processors may be included in processing unit 1104. These processors may include single-core or multi-core processors. In some embodiments, processing unit 1104 may be implemented as one or more independent processing units 1132 and / or 1134, with a single-core or multi-core processor included in each processing unit. In other embodiments, processing unit 1104 may also be implemented as a quad-core processing unit by integrating two dual-core processors into a single chip.
[0086] In various embodiments, the processing unit 1104 can execute a variety of programs in response to program code, and can maintain multiple programs or processes that are executed in parallel. At any given time, some or all of the program code to be executed may reside in the processor 1104 and / or in the storage subsystem 1118. Through appropriate programming, the processor 1104 can provide the various functions described above. The computer system 1100 can additionally include a processing acceleration unit 1106, which can include a digital signal processor (DSP), a special processor, and / or the like.
[0087] I / O subsystem 1108 may include user interface input devices and user interface output devices. User interface input devices may include a keyboard, a pointing device (such as a mouse or trackball), a touch pad or a touch screen incorporated into a display, a scroll wheel, a click wheel, a dial, buttons, switches, a keypad, an audio input device with a voice command recognition system, a microphone, and other types of input devices. User interface input devices may include, for example, a Microsoft Motion sensing and / or gesture recognition devices such as motion sensors that enable a user to control and interact with an input device, such as a Microsoft
[0088] 360 game controller. User interface input devices may also include Eye gesture recognition devices such as blink detectors that detect eye movement from the user (e.g., "blinking" when taking a picture and / or making a menu selection) and translate the eye movement to an input device (e.g., Google ). In addition, the user interface input device may include a voice recognition sensing device that enables the user to communicate with the voice recognition system (e.g. Navigator) interaction.
[0089] User interface input devices may also include, but are not limited to, three-dimensional (3D) mice, joysticks or pointing sticks, game controllers and graphic tablets, and auditory / visual devices such as speakers, digital cameras, digital camcorders, portable media players, webcams, image scanners, fingerprint scanners, barcode readers 3D scanners, 3D printers, laser rangefinders, and eye tracking devices. In addition, user interface input devices may include, for example, medical imaging input devices such as computed tomography, magnetic resonance imaging, positional radiation tomography, medical ultrasonography devices. User interface input devices may also include, for example, audio input devices such as MIDI keyboards, digital musical instruments, and the like.
[0090] The user interface output device may include a display subsystem, indicator lights, or non-visual displays such as audio output devices. The display subsystem may be a cathode ray tube (CRT), a flat panel device (such as a flat panel device using a liquid crystal display (LCD) or plasma display), a projection device, a touch screen, and the like. In general, the use of the term "output device" is intended to include all possible types of devices and mechanisms for outputting information from the computer system 1100 to a user or other computer. For example, the user interface output device may include, but is not limited to, various display devices that visually convey text, graphics, and audio / video information, such as monitors, printers, speakers, headphones, car navigation systems, plotters, voice output devices, and modems.
[0091] Computer system 1100 may include storage subsystem 1118 including software elements presently shown as being located within system memory 1110. System memory 1110 may store program instructions that are loadable and executable on processing unit 1104, as well as data generated during the execution of these programs.
[0092] Depending on the configuration and type of computer system 1100, system memory 1110 may be volatile (such as random access memory (RAM)) and / or non-volatile (such as read-only memory (ROM), flash memory, etc.). RAM typically contains data and / or program modules that are immediately accessible to and / or currently being operated and executed by processing unit 1104. In some embodiments, system memory 1110 may include a variety of different types of memory, such as static random access memory (SRAM) or dynamic random access memory (DRAM). In some embodiments, a basic input / output system (BIOS) containing basic routines such as those that help transfer information between elements within computer system 1110 during startup may typically be stored in ROM. By way of example and not limitation, system memory 1110 may also illustrate application programs 1112, which may include client applications, web browsers, mid-tier applications, relational database management systems (RDBMS), etc., program data 1114, and operating system 1116. Application programs 1112 may include client applications, web browsers, mid-tier applications, relational database management systems (RDBMS), etc. By way of example, operating system 1116 may include various versions of Microsoft Apple and / or Linux operating system, various commercially available or UNIX-like operating systems (including, without limitation, various GNU / Linux operating systems, Google OS and the like) and / or mobile operating systems such as iOS, Phone, OS, 10OS, and OS operating system.
[0093] The storage subsystem 1118 may also provide a tangible computer-readable storage medium to store basic programming and data structures that provide the functionality of some embodiments. Software (programs, code modules, instructions) that provide the above-described functionality when executed by a processor may be stored in the storage subsystem 1118. These software modules or instructions may be executed by the processing unit 1104. The storage subsystem 1118 may also provide a repository for storing data used in accordance with some embodiments.
[0094] Storage subsystem 1118 may also include a computer-readable storage media reader 1120, which may further be connected to computer-readable storage media 1122. Together with and optionally in conjunction with system memory 1110, computer-readable storage media 1122 may collectively represent remote, local, fixed, and / or removable storage devices plus storage media for temporarily and / or more permanently containing, storing, transferring, and retrieving computer-readable information.
[0095] The computer-readable storage medium 1122 containing the code or portions of the code may also include any suitable media, including storage media and communication media, such as, but not limited to, volatile and non-volatile, removable and non-removable media implemented in any method or technology for storing and / or transmitting information. This may include tangible computer-readable storage media such as RAM, ROM, electronically erasable programmable ROM (EEPROM), flash memory or other memory technology, CD-ROM, digital versatile disk (DVD) or other optical storage, magnetic cassettes, magnetic tape, magnetic disk storage or other magnetic storage devices, or other tangible computer-readable media. This may also include intangible computer-readable media, such as data signals, data transmissions, or any other medium that can be used to transmit the desired information and can be accessed by the computer system 1100.
[0096] By way of example, the computer readable storage media 1122 may include a hard disk drive that reads from or writes to a non-removable non-volatile magnetic media, a magnetic disk drive that reads from or writes to a removable non-volatile magnetic disk, and a removable non-volatile optical disk such as a CD ROM, a DVD, and a hard disk drive that reads from or writes to a removable non-volatile optical disk. The computer readable storage medium 1122 may include, but is not limited to, The computer-readable storage medium 1122 may include: a solid-state drive (SSD) based on nonvolatile memory, such as a flash memory-based SSD, an enterprise flash drive, a solid-state ROM, and the like; a volatile memory-based SSD, such as a solid-state RAM, a dynamic RAM, a static RAM, a DRAM-based SSD, a magnetoresistive RAM (MRAM) SSD; and a hybrid SSD using a combination of DRAM and a flash memory-based SSD. The disk drive and the computer-readable media associated with the disk drive may provide nonvolatile storage of computer-readable instructions, data structures, program modules, and other data for the computer system 1100.
[0097] The communication subsystem 1124 provides an interface to other computer systems and networks. The communication subsystem 1124 serves as an interface for receiving data from other systems from the computer system 1100 and sending data to the other systems. For example, the communication subsystem 1124 may enable the computer system 1100 to be connected to one or more devices via the Internet. In some embodiments, the communication subsystem 1124 may include a radio frequency (RF) transceiver component for accessing a wireless voice and / or data network (e.g., using cellular phone technology, advanced data network technology (such as 3G, 4G or EDGE (Enhanced Data Rates for Global Evolution)), WiFi (IEEE 802.11 series standards or other mobile communication technologies, or any combination of the above items to access a wireless voice and / or data network), a global positioning system (GPS) receiver component, and / or other components. In some embodiments, in addition to or in place of a wireless interface, the communication subsystem 1124 may provide a wired network connection (e.g., Ethernet).
[0098] In some implementations, the communication subsystem 1124 may also represent one or more users who may use the computer system 1100 to receive incoming communications in the form of structured and / or unstructured data feeds 1126, event streams 1128, event updates 1130, and the like.
[0099] By way of example, the communication subsystem 1124 may be configured to receive data feeds 1126 in real time from users of a social network and / or other communication service, such as feed, Updates, web page feeds (such as Rich Site Summary (RSS) feeds), and / or real-time updates from one or more third-party information sources.
[0100] Additionally, the communication subsystem 1124 may also be configured to receive data in the form of a continuous data stream, which may include an event stream 1128 of real-time events and / or event updates 1130, which may be continuous or unbounded in nature and have no clear endpoints. Examples of applications that generate continuous data may include, for example, sensor data applications, financial tickers, network performance measurement tools (e.g., network monitoring and traffic management applications), click stream analysis tools, automobile traffic monitoring, and the like.
[0101] The communication subsystem 1124 may also be configured to output structured and / or unstructured data feeds 1126 , event streams 1128 , event updates 1130 , and the like to one or more databases that may be in computer communication with one or more streaming data sources coupled to the computer system 1100 .
[0102] Computer system 1100 may be one of various types, including a handheld portable device (e.g., Cellular phone, computing tablets and PDAs), wearable devices (such as Google head mounted display), PC, workstation, mainframe, kiosk and server rack, or any other data processing system.
[0103] Due to the ever-changing nature of computers and networks, the description of the computer system 1100 depicted in the figure is intended only as a specific example. Many other configurations with more or fewer components than the system depicted in the figure are possible. For example, customized hardware may also be used and / or specific elements may be implemented in hardware, firmware, software (including applets), or a combination. Further, connections to other computing devices (such as network input / output devices) may be employed. Based on the disclosure and teachings provided herein, other ways and / or methods of implementing various embodiments should be apparent.
[0104] In the foregoing description, for the purpose of explanation, many specific details are set forth to provide a thorough understanding of various embodiments. However, it will be apparent that some embodiments may be implemented without some of these specific details. In other examples, well-known structures and devices are shown in the form of block diagrams.
[0105] The foregoing description only provides exemplary embodiments and is not intended to limit the scope, applicability, or configuration of the present disclosure. Rather, the foregoing description of each embodiment will provide a disclosure that can be implemented for implementing at least one embodiment. It should be understood that various changes may be made to the function and configuration of the elements without departing from the spirit and scope of some embodiments set forth in the appended claims.
[0106] Specific details are given in the foregoing description to provide a thorough understanding of the embodiments. However, it will be understood that the embodiments may be implemented without these specific details. For example, circuits, systems, networks, programs, and other components may be shown as components in block diagram form to avoid obscuring the embodiments in unnecessary detail. In other cases, well-known circuits, programs, algorithms, structures, and techniques may be shown without unnecessary detail to avoid obscuring the embodiments.
[0107] In addition, it is noted that individual embodiments may be described as processes, which are depicted as flow charts, flow charts, data flow diagrams, structure diagrams, or block diagrams. Although a flow chart may illustrate operations as a sequential process, many operations may be performed in parallel or simultaneously. In addition, the order of operations may be rearranged. When the operations of the process are completed, the process terminates, but may have additional steps not included in the figure. A process may correspond to a method, function, program, subroutine, subprogram, etc. When a process corresponds to a function, the termination of the process may correspond to the function returning to the calling function or main function.
[0108] The term "computer-readable medium" includes, but is not limited to, portable or fixed storage devices, optical storage devices, wireless channels, and various other media that can store, hold, or carry (multiple) instructions and / or data. Code segments or machine executable instructions can represent any combination of processes, functions, subroutines, programs, routines, subroutines, modules, software encapsulation, classes, or instructions, data structures, or program statements. Code segments can be coupled to another code segment or hardware circuit by transmitting and / or receiving information, data, independent variables, parameters, or memory contents. Information, independent variables, parameters, data, etc. can be transmitted, forwarded, or transmitted in any suitable manner. Any suitable manner includes memory sharing, information transmission, token transmission, network transmission, etc.
[0109] Furthermore, the embodiments may be implemented by hardware, software, firmware, middleware, microcode, hardware description language, or any combination thereof. When implemented by software, firmware, middleware, or microcode, the program code or code segments that perform the necessary tasks may be stored in a machine-readable medium. The processor may perform the necessary tasks.
[0110] In the foregoing description, features are described with reference to specific embodiments of the features, but it should be recognized that not all embodiments are limited thereto. Various features and aspects of some embodiments may be used individually or in combination. Furthermore, the embodiments may be used in any number of environments and applications beyond those described herein without departing from the broader spirit and scope of the specification. Accordingly, the description and drawings are to be regarded as illustrative rather than restrictive.
[0111] In addition, for the purpose of illustration, the method is described in a specific order. It should be understood that in an alternative embodiment, the method can be performed in a different order than described. It should also be understood that the above method can be performed by hardware components or can be implemented by a sequence of machine executable instructions, which can be used to cause the machine to perform the method. This machine is, for example, a general or special processor, or a logic circuit programmed with instructions. These machine executable instructions can be stored on one or more machine readable media, such as CD-ROM or other types of optical disks, floppy disks, ROM, RAM, EPROM, EEPROM, magnetic cards or optical cards, flash memory or other types of machine readable media suitable for storing electronic instructions. Alternatively, the method can be performed by a combination of hardware and software.
Claims
1. A method for plating a substrate, the method comprising: placing a substrate in a plating chamber containing a liquid; and Applying an electric current to the liquid in the plating chamber to deposit metal on the exposed portion of the substrate, wherein the electric current comprises alternating cycles of: forward plating current; and Reverse deplating current.
2. A method as claimed in claim 1, wherein the substrate includes a photoresist or mask layer, the photoresist or mask layer defines a pattern on the substrate, and the pattern includes an exposed portion of the substrate adjacent to the open area, wherein the current density during the plating process is more concentrated at the exposed portion of the substrate adjacent to the open area compared to the exposed portion of the substrate not adjacent to the open area.
3. The method of claim 1, wherein during the forward plating current, the metal is deposited non-uniformly on the exposed portion of the substrate.
4. The method of claim 3, wherein during the reverse deplating current, the metal is removed such that the metal becomes evenly distributed on the exposed portion of the substrate.
5. The method of claim 1 , wherein both the forward plating current and the reverse deplating current are applied in the plating chamber in the alternating cycle while the substrate is in the liquid, without using separate chambers or liquids to apply the forward plating current and the reverse deplating current. 6 . The method of claim 1 , wherein the exposed portion of the substrate comprises a plurality of through silicon vias (TSVs), wherein a difference between a maximum height of the TSVs and a minimum height of the TSVs is greater than a threshold distance.
7. The method of claim 1, before applying the current to the liquid in the plating chamber, further comprising: During a plating process, a model of the substrate is simulated to generate data points relating characteristics of the plating process and a pattern on the substrate to a predicted range of non-uniformity of the metal on the substrate for the forward plating current and the reverse deplating current.
8. The method of claim 7, before applying the current to the liquid in the plating chamber, further comprising: Using the data points relating the characteristics of the plating process and the pattern on the substrate to the predicted range of non-uniformity of the metal on the substrate, a value for the reverse deplating current is determined.
9. The method of claim 7, before applying the current to the liquid in the plating chamber, further comprising: A duty cycle for the alternating cycles of the forward plating current and the reverse deplating current is determined using the data points relating the characteristics of the plating process and the pattern on the substrate to the predicted range of non-uniformity of the metal on the substrate.
10. A system comprising: a plating chamber containing a liquid configured to receive a substrate; and A controller configured to cause application of an electric current to the liquid in the plating chamber to deposit metal on the exposed portion of the substrate, wherein the electric current comprises alternating cycles of: forward plating current; and Reverse deplating current.
11. The system of claim 10, wherein the controller is further configured to apply the alternating cycles of the forward plating current and the reverse deplating current based at least in part on a rotational speed of the substrate in the plating chamber.
12. The system of claim 10, wherein the controller is further configured to apply the alternating cycles of the forward plating current and the reverse deplating current based at least in part on movement of a paddle in the plating chamber.
13. The system of claim 10, wherein the plating chamber comprises an electrochemical deposition chamber and the liquid comprises an electrolyte.
14. The system of claim 10, wherein the forward plating current is applied for a time at least 10 times longer than the deplating current.
15. A non-transitory computer-readable medium comprising instructions that, when executed by one or more processors, cause the one or more processors to perform operations comprising: a model of a substrate simulated in a plating process to generate data points relating characteristics of the plating process and a pattern on the substrate to a range of non-uniformities of material formed on the substrate during the plating process; Using information from the data points, determining values for a forward plating current and a reverse deplating current to be applied in the plating chamber; and The values for the forward plating current and the reverse deplating current are provided to the plating chamber to perform a plating process.
16. The non-transitory computer readable medium of claim 15, wherein determining the values for the forward plating current and the reverse deplating current comprises: receiving a target deposition rate for the plating process; receiving a forward plating rate for the plating process; and A reverse deplating rate is determined for the plating process.
17. The non-transitory computer readable medium of claim 16, wherein determining the values for the forward plating current and the reverse deplating current comprises: Based on the target deposition rate, the forward plating rate, and the reverse deplating rate, duty cycles for the forward plating current and the reverse deplating current are determined.
18. The non-transitory computer readable medium of claim 16, wherein the reverse deplating rate minimizes non-uniformity in the range of the material formed on the substrate during the plating process.
19. The non-transitory computer readable medium of claim 15, wherein the data points relating characteristics of a plating process and a pattern on the substrate to a range of non-uniformities of a material formed on the substrate during the plating process comprise a linear relationship.