Preparation method of refrigeration infrared detector

By removing the transition layer in the infrared detector, the photocurrent shunt and carrier recombination problems caused by the epitaxial layer component gradient are solved, and a narrower breakdown curve widening is achieved, which improves the performance of the infrared detection chip.

CN118983327APending Publication Date: 2024-11-19ZHEJIANG JUEXIN MICROELECTRONICS CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411471166.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-22
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The existing mercury cadmium tellurium infrared devices have a gradient of the epitaxial layer due to the high epitaxial temperature, which leads to the splitting of photocurrent between the cells, and thus widening the phenomenon on the test breaking diagram. At the same time, the transition layer defects lead to photogenerated carrier recombination or scattering. , causing a difference in the output level of the cell.

Method used

Provide a method for preparing a refrigeration infrared detector, including forming a metal electrode and an indium column on the device chip, filling the curing glue after resoldering, and removing the substrate and transition layer, using dry, wet or chemical polishing, etc. Methods remove the transition layer and reduce the epitaxial layer component gradient.

Benefits of technology

By removing the transition layer, the migration length of photogenerated carriers is reduced, the photocurrent shunt is reduced, the cell output level difference is avoided, the breakdown curve is significantly narrowed, and the performance of infrared detection chips is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983327A_ABST
    Figure CN118983327A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a refrigeration infrared detector, which comprises the following steps of: providing a device chip which comprises a laminated structure of a substrate, a transition layer and an epitaxial layer; forming a first metal electrode on the epitaxial layer of the device chip; forming a first indium column on the first metal electrode; providing a readout circuit chip, and forming a second metal electrode on the readout circuit chip; forming a second indium column on the second metal electrode; the first indium column and the second indium column are connected in a face-down bonding mode; the area around the interconnection indium column between the device chip and the readout circuit chip is filled with curing glue; removing the substrate of the device chip; and removing the transition layer of the device chip. According to the preparation method of the refrigeration infrared detector provided by the invention, the transition layer is removed, the component gradient is reduced, and then the problem of broadening on a breaking curve is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of infrared detectors, and in particular to a method for preparing a refrigerated infrared detector. Background Art

[0002] With the continuous promotion and development of infrared applications, advanced infrared detection technology requires detectors to have higher spatial resolution and better target recognition capabilities. Infrared detectors are photoelectric devices that convert infrared radiation into electronic signals. The photoelectric reaction only occurs on the photosensitive element, and the subsequent signal processing process only involves electronic technology. Therefore, infrared detection chips are the core components of infrared detectors.

[0003] The existing HgCdTe infrared device is an infrared focal plane detector formed by coupling the HgCdTe infrared chip and the silicon circuit through reverse solder interconnection. The chip is the core of the detector, and the epitaxial material is the basis of the chip. The mainstream growth process of the epitaxial material of the HgCdTe infrared chip is still liquid phase epitaxy (Liquid Phase Epitaxy, referred to as LPE). The substrate is CdZnTe, and liquid phase epitaxy is performed on CdZnTe through epitaxial technology. Due to the high epitaxial temperature of the existing technology, the grown epitaxial layer has a component gradient. The component gradient increases the migration length of the photogenerated carriers, making it easier for the photocurrent to be shunted between pixels, and then the phenomenon of excessive broadening appears on the test breakdown diagram. At the same time, the transition layer of the HgCdTe infrared device formed by the existing technology has many defects, which causes the photogenerated carriers to be recombinated or scattered, and the output level of the pixel is different, which is reflected in the broadening of the breakdown curve. Summary of the invention

[0004] In order to solve the problems existing in the prior art, the present invention provides a method for preparing a refrigerated infrared detector.

[0005] The present invention provides a method for preparing a refrigerated infrared detector, comprising the following steps: providing a device chip, wherein the device chip comprises a laminated structure of a substrate, a transition layer, and an epitaxial layer; forming a first metal electrode on the epitaxial layer of the device chip; forming a first indium column on the first metal electrode; providing a readout circuit chip, wherein a second metal electrode is formed on the readout circuit chip; forming a second indium column on the second metal electrode; interconnecting the first indium column and the second indium column by reverse soldering; filling a curing glue in an area around the interconnected indium columns between the device chip and the readout circuit chip; removing the substrate of the device chip; and removing the transition layer of the device chip.

[0006] Optionally, forming a metal electrode on the epitaxial layer of the device chip includes the steps of: depositing a first dielectric layer on the epitaxial layer; etching the first dielectric layer to form a first through hole; forming a first metal electrode, wherein the first metal electrode covers the first through hole and the first dielectric layer around the first through hole.

[0007] Optionally, the first metal electrode includes a first metal layer and a second metal layer, the first metal layer is located between the device chip and the second metal layer, the first metal layer and the second metal layer are formed by magnetron sputtering, electron beam evaporation, and thermal evaporation, respectively, the material of the first metal layer is at least one of chromium, tin, titanium and nickel, and the material of the second metal layer is at least one of platinum, palladium, gold and aluminum.

[0008] Optionally, forming the metal electrode on the readout circuit chip includes the steps of: depositing a second dielectric layer on the readout circuit chip; etching the second dielectric layer to form a second through hole; and forming a second metal electrode, wherein the second metal electrode covers the second through hole and the second dielectric layer around the second through hole.

[0009] Optionally, the second metal electrode includes a third metal layer and a fourth metal layer, the third metal layer is located between the readout circuit chip and the fourth metal layer, the third metal layer and the fourth metal layer are formed by magnetron sputtering, electron beam evaporation, and thermal evaporation, respectively, the material of the third metal layer is at least one of titanium and nickel, and the material of the fourth metal layer is at least one of platinum, palladium, gold, copper and aluminum.

[0010] Optionally, the removing of the transition layer of the device chip comprises: removing the transition layer by dry etching, the dry etching comprises: ICP etching, the power range of the ICP etching is 200-600w, and the radio frequency range of the dry etching is 10-100w.

[0011] Optionally, the gas used for the dry etching includes: CH4, Ar, H2, N2, wherein the pressure range of CH4 is 1-10mtorr, the pressure range of Ar is 5-20mtorr, the pressure range of H2 is 1-3mtorr, and the pressure range of N2 is 1-10mtorr.

[0012] Optionally, removing the transition layer of the device chip includes: removing the transition layer by a wet etching method, wherein a solution used in the wet etching includes at least one of bromomethanol, bromoethanol, and hydrobromic acid.

[0013] Optionally, the removing the transition layer of the device chip includes: removing the transition layer by chemical polishing, wherein the chemical polishing uses a bromine methanol solution with a concentration ranging from 0.1% to 5%.

[0014] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0015] The present invention provides a method for preparing a refrigerated infrared detector, which reduces the migration length of photogenerated carriers and the shunting of photocurrent between pixels by removing the transition layer and reducing the component gradient of the epitaxial layer, thereby widening and narrowing the test breakdown curve. At the same time, it alleviates the phenomenon of photogenerated carriers being recombined or scattered, and avoids differences in the output levels of the pixels. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.

[0017] Figure 1 A schematic diagram of a process for preparing a refrigerated infrared detector according to an embodiment of the present disclosure;

[0018] Figure 2a-2h It is a schematic diagram of an intermediate structure of a cooling infrared detector forming process according to an embodiment of the present disclosure;

[0019] Figure 3a-3c A schematic diagram of a test breakdown curve of a cooled infrared detector according to an embodiment of the present disclosure. DETAILED DESCRIPTION

[0020] The preferred embodiments of the present invention will be described in more detail below. Although the preferred embodiments of the present invention are described below, it should be understood that the present invention can be implemented in various forms and should not be limited to the embodiments set forth herein.

[0021] In the present invention, unless otherwise specified, the directional words used, such as "upper and lower", generally refer to the upper and lower parts of the device in normal use, and "inside and outside" refer to the outline of the device. In addition, the terms "first, second, third" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first, second, third" may explicitly or implicitly include one or more of the features. In the description of the present invention, "multiple" means two or more, unless otherwise clearly and specifically defined. In the present invention, it is an electrical device, so connection and interconnection both refer to conductive interconnection. Since the accompanying drawings are descriptions of the same device, the same numbers in the drawings represent the same components.

[0022] At present, in the process of preparing mercury cadmium telluride infrared devices, due to the high epitaxial temperature, the epitaxial layer grown on the mercury cadmium telluride infrared chip has a composition gradient. The composition gradient increases the migration length of the photogenerated carriers, causing the photocurrent to be more easily shunted between pixels, and then the test breakdown diagram shows an over-broadening phenomenon; at the same time, due to the large number of defects in the transition layer, the photogenerated carriers are easily recombined or scattered, and the output levels of the pixels are different, which is reflected in the broadening of the breakdown curve.

[0023] Therefore, the embodiments of the present disclosure provide a method for preparing a cooled infrared detector, which can effectively solve the above problems and greatly improve the performance of the infrared detection chip.

[0024] The embodiment of the present disclosure provides a method for preparing a cooled infrared detector, comprising the following steps: providing a device chip, wherein the device chip comprises a stacked structure of a substrate, a transition layer, and an epitaxial layer; forming a first metal electrode on the epitaxial layer of the device chip; forming a first indium column on the first metal electrode; providing a readout circuit chip, forming a second metal electrode on the readout circuit chip; forming a second indium column on the second metal electrode; interconnecting the first indium column and the second indium column by reverse soldering; filling a curing glue in an area around the interconnected indium columns between the device chip and the readout circuit chip; removing the substrate of the device chip; and removing the transition layer of the device chip.

[0025] The specific examples of the present invention are further described in detail below in conjunction with the accompanying drawings. Wherein, the substances not listed in detail in the embodiments can be selected from any substances on the market that can achieve corresponding functions.

[0026] The present disclosure provides a method for preparing a refrigerated infrared detector, the specific steps are as follows: Figure 1 As shown, Figure 2a-2h The figure shows an intermediate structure diagram of a cooling infrared detector forming process according to an embodiment of the present disclosure. Figure 1 and Figure 2a-2h The preparation method of the refrigerated infrared detector comprises the following steps:

[0027] S1: Provide a device chip, wherein the device chip includes a stacked structure of a substrate, a transition layer, and an epitaxial layer.

[0028] Specifically, a device chip 10 is provided. Figure 2a The device chip 10 is a stacked structure consisting of a substrate 100, a transition layer 110, and an epitaxial layer 120. The transition layer 110 is located between the substrate 100 and the epitaxial layer 120. An n region 121 is provided on the side of the epitaxial layer 120 away from the transition layer 110.

[0029] In the embodiment of the present disclosure, the substrate 100 is a cadmium zinc telluride substrate, and the epitaxial layer 120 is a mercury cadmium telluride epitaxial chip.

[0030] S2: forming a first metal electrode on the epitaxial layer of the device chip.

[0031] The n region 121 of the epitaxial layer 120 is led out through metal, and a first metal electrode 140 is formed on the n region 121 of the epitaxial layer 120. Specifically, the method includes the following steps: depositing a first dielectric layer 130 on the epitaxial layer 120; etching the first dielectric layer 130, forming a first through hole at a position of the first dielectric layer 130 corresponding to the n region 121 in the epitaxial layer 120, and then forming the first metal electrode 140 in the first through hole by electron beam evaporation, and the first metal electrode 140 covers the first through hole and the first dielectric layer 130 around the first through hole.

[0032] In some embodiments, the first metal electrode includes a first metal layer and a second metal layer, the first metal layer and the second metal layer are a stacked structure, and the first metal layer is located between the n-region in the epitaxial layer 120 and the second metal layer.

[0033] In some embodiments, the first metal layer and the second metal layer are formed by magnetron sputtering, electron beam evaporation, and thermal evaporation, respectively. In the disclosed embodiment, electron beam evaporation is preferred.

[0034] In some embodiments, the first metal layer is composed of at least one material including but not limited to chromium, tin, titanium and nickel, preferably chromium in the embodiment of the present disclosure; the second metal layer is composed of at least one material including but not limited to platinum, palladium, gold and aluminum, preferably gold in the embodiment of the present disclosure.

[0035] S3: forming a first indium column on the first metal electrode.

[0036] like Figure 2b As shown, a first indium column 150 is formed on the first metal electrode 140 by thermal evaporation. The first indium column 150 is used to connect the device chip and the readout circuit together through a bonding process in the subsequent process. Because the hardness of indium material is relatively low, indium material is preferably used for the bonding process, and thermal evaporation is preferably used for the formation method.

[0037] S4: providing a readout circuit chip, and forming a second metal electrode on the readout circuit chip.

[0038] A readout circuit chip 20 is provided, and an n region 221 is provided on one side of the readout circuit chip 20. Figure 2c, forming a second metal electrode 240 on the readout circuit chip 20, specifically, comprising the steps of: depositing a second dielectric layer 230 on the readout circuit chip 20; etching the second dielectric layer 230, forming a second through hole at a position of the second dielectric layer 230 corresponding to the n region 221 in the readout circuit chip 20, and then forming the second metal electrode 240 in the second through hole by electron beam evaporation, and the second metal electrode 240 covers the second through hole and the second dielectric layer 230 around the second through hole.

[0039] In some embodiments, the second metal electrode includes a third metal layer and a fourth metal layer, the third metal layer and the fourth metal layer are a stacked structure, and the third metal layer is located between the readout circuit chip and the fourth metal layer.

[0040] In some embodiments, the third metal layer and the fourth metal layer are formed by magnetron sputtering, electron beam evaporation, and thermal evaporation, respectively. In the embodiment of the present disclosure, electron beam evaporation is preferred.

[0041] In some embodiments, the third metal layer is composed of at least one material including but not limited to titanium and nickel, preferably titanium in the embodiment of the present disclosure. The fourth metal layer is composed of at least one material including but not limited to platinum, palladium, gold, copper and aluminum, preferably gold in the embodiment of the present disclosure.

[0042] S5: forming a second indium column on the second metal electrode.

[0043] like Figure 2d As shown, a second indium column 250 is formed on the second metal electrode 240 by thermal evaporation. The second indium column 250 is used to connect the readout circuit and the device chip together through a bonding process in the subsequent process. Because the hardness of indium material is relatively low, indium is preferably used for the bonding process, and thermal evaporation is preferably used for the formation method.

[0044] S6: interconnecting the first indium column and the second indium column by reverse soldering.

[0045] Specifically, refer to Figure 2e The first indium column 150 on the device chip 10 and the second indium column 250 on the readout circuit chip 20 are reversely soldered and interconnected through a bonding interconnection process.

[0046] S7: Filling the area around the interconnected indium pillars between the device chip and the readout circuit chip with cured glue.

[0047] like Figure 2fAs shown, after the device chip 10 and the readout circuit chip 20 are interconnected by reverse soldering, it is necessary to fill the area around the indium column between the device chip 10 and the readout circuit chip 20 with curing glue 300. After curing, the curing glue 300 can improve the mechanical strength of the semiconductor device, improve its ability to resist various mechanical loads, improve its corrosion resistance and high temperature resistance, and prevent mutual interference between electronic components inside the device, thereby improving the reliability and life of the device.

[0048] In some embodiments, the curing adhesive may be any curing adhesive available on the market that can achieve corresponding functions, and the embodiments of the present disclosure are not limited to this.

[0049] S8: removing the substrate of the device chip.

[0050] like Figure 2g As shown, after the device chip 10 and the readout circuit chip 20 are interconnected by flip-flop soldering, the substrate 100 of the device chip is removed from one side of the substrate of the device chip by an etching process.

[0051] In some embodiments, the substrate of the device chip may be removed by different process methods such as dry etching, wet etching, and chemical polishing, which is not limited in the present disclosure.

[0052] S9: Remove the transition layer of the device chip.

[0053] Reference Figure 2h In different embodiments, the transition layer 110 of the device chip can be removed by different process methods such as dry etching, wet etching and chemical polishing.

[0054] In a specific embodiment, the transition layer can be removed by dry etching, wherein the power range of ICP etching is 200-600W, preferably 400W; the radio frequency range used in the dry etching is 10-100W, preferably 50W.

[0055] In some embodiments, the gas used for dry etching to remove the transition layer includes but is not limited to at least one or a combination of CH4, Ar, H2, and N2, wherein the pressure range of CH4 is 1-10mtorr, and preferably 5mtorr in the embodiment of the present disclosure; the pressure range of Ar is 5-20mtorr, and preferably 11mtorr in the embodiment of the present disclosure; the pressure range of H2 is 1-3mtorr, and preferably 2mtorr in the embodiment of the present disclosure; the pressure range of N2 is 1-10mtorr, and preferably 5mtorr in the embodiment of the present disclosure.

[0056] In some embodiments, the transition layer may be removed by wet etching. The solutions that may be used for wet etching include but are not limited to bromomethanol, bromoethanol, hydrobromic acid and the like. In the disclosed embodiment, Br2 / HBr solution is preferred, with a ratio of 0.2%.

[0057] In some embodiments, the transition layer can also be removed by chemical polishing, and the chemical polishing can be performed using a bromine methanol solution, and the concentration range of the bromine methanol solution is 0.1%-5%. In the embodiment of the present disclosure, when chemical polishing is used to remove the transition layer, the preferred solution is a bromine methanol solution with a concentration of 0.3%.

[0058] The present invention provides a method for preparing a refrigerated infrared detector. Figure 3a-3c The test results of the cooled infrared detector prepared by removing the transition layer on the device chip by dry etching, wet etching and chemical polishing processes are shown respectively. Compared with the cooled infrared detector in the prior art in which the transition layer is not removed, the test results show that in the preparation process of the cooled infrared detector, the different methods of removing the transition layer can reduce the component gradient of the epitaxial layer, thereby reducing the migration length of the photogenerated carriers and reducing the shunting of the photocurrent between pixels, which is reflected in the widening and narrowing of the breakdown curve.

[0059] The above descriptions are merely embodiments of the present application and are not intended to limit the patent scope of the present application. Any equivalent structural or equivalent process transformations made using the contents of the specification and drawings of the present application, such as the mutual combination of technical features between the embodiments, or direct or indirect application in other related technical fields, are also included in the patent protection scope of the present application.

Claims

1. A method for preparing a refrigerated infrared detector, characterized in that: Includes steps: Providing a device chip, the device chip comprising a stacked structure of a substrate, a transition layer, and an epitaxial layer; forming a first metal electrode on the epitaxial layer of the device chip; forming a first indium column on the first metal electrode; providing a readout circuit chip, and forming a second metal electrode on the readout circuit chip; forming a second indium column on the second metal electrode; interconnecting the first indium column and the second indium column by reverse soldering; Filling a curing glue in an area around the interconnected indium pillars between the device chip and the readout circuit chip; removing the substrate of the device chip; Remove the transition layer of the device chip.

2. The method for preparing a refrigerated infrared detector according to claim 1, characterized in that: The step of forming a metal electrode on the epitaxial layer of the device chip comprises the following steps: depositing a first dielectric layer on the epitaxial layer; Etching the first dielectric layer to form a first through hole; A first metal electrode is formed, wherein the first metal electrode covers the first through hole and the first dielectric layer around the first through hole.

3. The method for preparing a refrigerated infrared detector according to claim 2, characterized in that: The first metal electrode includes a first metal layer and a second metal layer, the first metal layer is located between the device chip and the second metal layer, the first metal layer and the second metal layer are formed by magnetron sputtering, electron beam evaporation, and thermal evaporation, respectively, the first metal layer is made of at least one of chromium, tin, titanium and nickel, and the second metal layer is made of at least one of platinum, palladium, gold and aluminum.

4. The method for preparing a refrigerated infrared detector according to claim 1, characterized in that: The forming of the metal electrode on the readout circuit chip comprises the steps of: depositing a second dielectric layer on the readout circuit chip; Etching the second dielectric layer to form a second through hole; A second metal electrode is formed, wherein the second metal electrode covers the second through hole and the second dielectric layer around the second through hole.

5. The method for preparing a refrigerated infrared detector according to claim 4, characterized in that: The second metal electrode includes a third metal layer and a fourth metal layer, the third metal layer is located between the readout circuit chip and the fourth metal layer, the third metal layer and the fourth metal layer are formed by magnetron sputtering, electron beam evaporation, and thermal evaporation, respectively, the third metal layer is made of at least one of titanium and nickel, and the fourth metal layer is made of at least one of platinum, palladium, gold, copper and aluminum.

6. The method for preparing a refrigerated infrared detector according to claim 1, characterized in that: The method of removing the transition layer of the device chip includes: removing the transition layer by dry etching, wherein the dry etching includes: ICP etching, the power range of the ICP etching is 200-600w, and the radio frequency range used by the dry etching is 10-100w.

7. The method for preparing a refrigerated infrared detector according to claim 6, characterized in that: The gases used for the dry etching include: CH4, Ar, H2, and N2, wherein the pressure range of CH4 is 1-10 mtorr, the pressure range of Ar is 5-20 mtorr, the pressure range of H2 is 1-3 mtorr, and the pressure range of N2 is 1-10 mtorr.

8. The method for preparing a refrigerated infrared detector according to claim 1, characterized in that: The method of removing the transition layer of the device chip comprises: removing the transition layer by a wet etching method, wherein the solution used in the wet etching method comprises at least one of bromomethanol, bromoethanol and hydrobromic acid.

9. The method for preparing a refrigerated infrared detector according to claim 1, characterized in that: The method of removing the transition layer of the device chip comprises: removing the transition layer by chemical polishing, wherein the chemical polishing adopts a bromine methanol solution, and the concentration of the solution ranges from 0.1% to 5%.

Citation Information

Patent Citations

  • InGaAs infrared detector and preparing method thereof

    CN104362196A

  • Light reception element, production method for light reception element, and imaging device

    CN113366656A

  • Refrigeration infrared detector and preparation method of indium column thereof

    CN115763617A

  • Refrigeration infrared detector and indium column preparation method thereof

    CN116913936A