Early warning method, device and equipment for lithium precipitation of lithium battery and storage medium

By obtaining the battery information and cell thickness of the lithium battery, drawing the expansion curve and comparing it with the lithium-ion standard line, the problem that the existing technology cannot detect lithium-ion in real time is solved, and the safety and cycle life of the lithium battery are improved.

CN118983553APending Publication Date: 2024-11-19DONGFENG MOTOR GRP

Patent Information

Application Number
CN202410991627.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The prior art cannot accurately detect lithium extraction during use in real time and online, resulting in safety and cycle life problems that are difficult to meet the needs of modern battery management systems.

Method used

By obtaining the battery information, charging ratio and cell thickness of the lithium battery, drawing the cell thickness expansion curve, comparing it with the lithium-ion standard line, monitoring it in real time and issuing a lithium-ion warning signal, and remedial measures are taken.

Benefits of technology

Early warning and effective response to lithium-ion evolution phenomenon of lithium batteries has been achieved, and the safety and cycle life of lithium batteries have been improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983553A_ABST
    Figure CN118983553A_ABST
Patent Text Reader

Abstract

The invention discloses a lithium battery lithium precipitation early warning method, device and equipment and a storage medium, and relates to the technical field of lithium batteries, and the method comprises the steps: obtaining the battery information, the charging rate, the cell thickness and the lithium precipitation standard line in the current lithium battery charging and discharging process; obtaining a battery cell thickness expansion curve based on the battery information, the charging rate and the battery cell thickness; and according to the cell thickness expansion curve and the lithium precipitation standard line, carrying out lithium battery lithium precipitation early warning. The problem of how to accurately detect lithium precipitation of the lithium battery in the battery using process is solved, and the safety and the cycle life of the lithium battery are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of lithium batteries, and in particular to a lithium battery lithium plating early warning method, device, equipment and storage medium. Background Art

[0002] With the vigorous development of the new energy industry, the performance and safety of lithium iron phosphate batteries, as important energy storage components, have received widespread attention. During the charging and discharging process of lithium iron phosphate batteries, lithium plating is one of the key factors affecting the safety performance and cycle life of batteries. Lithium plating, that is, the deposition of lithium ions on the surface of the negative electrode of the battery to form lithium dendrites, will not only reduce the energy efficiency of the battery, but may also cause serious safety problems such as short circuit and thermal runaway. At present, the industry's detection of lithium plating in lithium batteries mainly uses the method of cell disassembly, which is limited to conventional cell disassembly. However, this method is destructive, not only complicated to operate and costly, but also unable to monitor the lithium plating of the battery in real time and online, and it is difficult to meet the needs of modern battery management systems for efficient, accurate and non-destructive monitoring.

[0003] Therefore, how to accurately detect lithium plating in lithium batteries during battery use is a problem that urgently needs to be solved. Summary of the invention

[0004] The main purpose of this application is to provide a lithium battery lithium plating early warning method, device, equipment and storage medium, aiming to solve the technical problem of how to accurately detect lithium plating in lithium batteries during battery use.

[0005] To achieve the above objectives, the present application proposes a lithium battery lithium plating early warning method, the method comprising:

[0006] Obtain the battery information, charging rate, cell thickness and lithium plating standard line during the current lithium battery charging and discharging process;

[0007] Obtaining a cell thickness expansion curve based on the battery information, the charging rate and the cell thickness;

[0008] A lithium battery lithium deposition warning is performed according to the battery cell thickness expansion curve and the lithium deposition standard line.

[0009] In one embodiment, the step of obtaining a cell thickness expansion curve based on the battery information, the charging rate and the cell thickness comprises:

[0010] Obtaining a state of charge and a temperature of the battery according to the battery information;

[0011] A cell thickness expansion curve is obtained according to the state of charge, the temperature, the cell thickness and the charging rate.

[0012] In one embodiment, before obtaining the battery information, charging rate, cell thickness, and lithium plating standard line during the current lithium battery charging and discharging process, the method further includes:

[0013] Obtain the battery's historical state of charge, historical temperature, historical voltage, historical charging rate, and historical cell thickness during the battery's cyclic charge and discharge process;

[0014] Obtaining a voltage differential curve and a historical battery cell thickness expansion curve according to the historical state of charge, the historical temperature, the historical voltage, the historical charging rate, and the historical battery cell thickness;

[0015] The lithium plating standard line is determined according to the voltage differential curve and the historical battery cell thickness expansion curve.

[0016] In one embodiment, the step of determining the lithium deposition standard line according to the voltage differential curve and the historical battery cell thickness expansion curve comprises:

[0017] Obtaining a voltage change rate according to the voltage differential curve;

[0018] Obtaining a cell thickness expansion rate according to the historical cell thickness expansion curve;

[0019] Obtaining a lithium deposition inflection point according to the voltage change rate and the battery core thickness expansion rate;

[0020] The lithium precipitation standard line is determined according to the lithium precipitation inflection point.

[0021] In one embodiment, the step of obtaining a voltage differential curve and a historical battery cell thickness expansion curve according to the historical state of charge, the historical temperature, the historical voltage, the historical charging rate and the historical battery cell thickness comprises:

[0022] Obtaining a voltage differential curve according to the historical state of charge, the historical temperature, the historical voltage, and the historical charging rate;

[0023] A historical battery cell thickness expansion curve is obtained according to the historical state of charge, the historical temperature, the historical battery cell thickness and the historical charging rate.

[0024] In one embodiment, the step of providing a lithium battery lithium deposition warning according to the battery cell thickness expansion curve and the lithium deposition standard line comprises:

[0025] Fitting the battery core thickness expansion curve with the lithium precipitation standard line to obtain a fitting deviation value;

[0026] When the fitting deviation value is within a preset fitting deviation range, a lithium plating warning signal is issued.

[0027] In one embodiment, after the lithium battery lithium deposition warning is performed according to the battery cell thickness expansion curve and the lithium deposition standard line, the method further includes:

[0028] A preset current is obtained, and the lithium battery is controlled to discharge according to the preset current.

[0029] In addition, to achieve the above-mentioned purpose, the present application also proposes a lithium battery lithium deposition early warning device, the device comprising:

[0030] The data acquisition module is used to obtain the battery information, charging rate, cell thickness and lithium plating standard line during the current lithium battery charging and discharging process;

[0031] A lithium analysis calibration module, used for obtaining a cell thickness expansion curve based on the battery information, the charging rate and the cell thickness;

[0032] The lithium deposition early warning module is used to provide early warning of lithium deposition of the lithium battery according to the battery cell thickness expansion curve and the lithium deposition standard line.

[0033] In addition, to achieve the above-mentioned purpose, the present application also proposes a lithium battery lithium plating warning device, which includes: a memory, a processor, and a computer program stored in the memory and executable on the processor, and the computer program is configured to implement the steps of the lithium battery lithium plating warning method as described above.

[0034] In addition, to achieve the above-mentioned purpose, the present application also proposes a storage medium, which is a computer-readable storage medium, and a computer program is stored on the storage medium. When the computer program is executed by a processor, the steps of the lithium battery lithium plating warning method as described above are implemented.

[0035] In addition, to achieve the above-mentioned purpose, the present application also provides a computer program product, which includes a computer program, and when the computer program is executed by a processor, the steps of the lithium battery lithium plating early warning method as described above are implemented.

[0036] The present application provides a lithium battery lithium plating early warning method, which obtains the battery information, charging rate, cell thickness and lithium plating standard line during the current lithium battery charging and discharging process; obtains the cell thickness expansion curve based on the battery information, the charging rate and the cell thickness; and performs lithium battery lithium plating early warning according to the cell thickness expansion curve and the lithium plating standard line. In summary, the present application realizes early warning and effective response to lithium plating phenomenon by real-time monitoring of the changes in physical parameters during battery charging and discharging, combined with data analysis technology, solves the problem of how to accurately detect lithium plating in lithium batteries during battery use, and improves the safety and cycle life of lithium batteries. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present application and, together with the description, serve to explain the principles of the present application.

[0038] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0039] Figure 1 A schematic diagram of a process flow provided for the first embodiment of the lithium battery lithium deposition early warning method of the present application;

[0040] Figure 2 This is a schematic diagram of a voltage differential curve and a cell thickness expansion curve in an embodiment of a lithium battery lithium plating early warning method of the present application;

[0041] Figure 3 A schematic diagram of a second embodiment of the lithium battery lithium deposition early warning method provided in this application;

[0042] Figure 4 A schematic diagram of a process flow provided for the third embodiment of the lithium battery lithium deposition early warning method of the present application;

[0043] Figure 5 This is a schematic diagram of the module structure of the lithium battery lithium deposition warning device according to an embodiment of the present application;

[0044] Figure 6 Schematic diagram of the equipment structure of the hardware operating environment involved in the lithium battery lithium plating early warning method in the embodiment of the present application.

[0045] The purpose, features and advantages of this application will be further described in conjunction with the embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0046] It should be understood that the specific embodiments described herein are only used to explain the technical solutions of the present application and are not used to limit the present application.

[0047] In order to better understand the technical solution of the present application, a detailed description will be given below in conjunction with the accompanying drawings and specific implementation methods.

[0048] The main solution of the embodiment of the present application is: by obtaining the battery information, charging rate, cell thickness and lithium plating standard line during the current lithium battery charging and discharging process; obtaining the cell thickness expansion curve based on the battery information, the charging rate and the cell thickness; and providing lithium plating warning for lithium batteries according to the cell thickness expansion curve and the lithium plating standard line.

[0049] With the vigorous development of the new energy industry, the performance and safety of lithium iron phosphate batteries, as important energy storage components, have received widespread attention. During the charging and discharging process of lithium iron phosphate batteries, lithium plating is one of the key factors affecting the safety performance and cycle life of batteries. Lithium plating, that is, the deposition of lithium ions on the surface of the negative electrode of the battery to form lithium dendrites, will not only reduce the energy efficiency of the battery, but may also cause serious safety problems such as short circuit and thermal runaway. At present, the industry's detection of lithium plating in lithium batteries mainly uses the method of cell disassembly, which is limited to conventional cell disassembly. However, this method is destructive, not only complicated to operate and costly, but also unable to monitor the lithium plating of the battery in real time and online, and it is difficult to meet the needs of modern battery management systems for efficient, accurate and non-destructive monitoring. Therefore, how to accurately detect lithium plating in lithium batteries during battery use is a problem that needs to be solved urgently.

[0050] This application achieves early warning and effective response to lithium plating by real-time monitoring of changes in physical parameters during battery charging and discharging, combined with data analysis technology, solves the problem of how to accurately detect lithium plating in lithium batteries during battery use, and improves the safety and cycle life of lithium batteries.

[0051] It should be noted that the execution subject of this embodiment can be a lithium battery lithium deposition early warning system, or a computing service device with data processing, network communication and program running functions, such as a tablet computer, a personal computer, a mobile phone, etc., or an electronic device capable of realizing the above-mentioned lithium battery lithium deposition early warning function, etc., and this embodiment does not specifically limit this. The following takes the lithium battery lithium deposition early warning system as an example to illustrate this embodiment and the following embodiments.

[0052] Based on this, the present application embodiment provides a lithium battery lithium deposition early warning method, referring to Figure 1 , Figure 1 This is a flow chart of the first embodiment of the lithium battery lithium plating early warning method of the present application.

[0053] In this embodiment, the lithium battery lithium deposition early warning method includes steps S10 to S30:

[0054] Step S10: Obtaining battery information, charging rate, cell thickness, and lithium plating standard line during the current lithium battery charging and discharging process.

[0055] It should be noted that in this step, the system will first obtain the current basic information of the lithium battery such as voltage, power, temperature, etc. in real time through the BMS (Battery Management System). Then determine the current charging rate based on the current charging strategy of the lithium battery. The system will also use high-precision sensors to obtain the thickness of the battery cell in real time. It is understandable that the change in the thickness of the battery cell can indirectly reflect the lithium deintercalation and deintercalation of the internal material of the battery cell, which is one of the important factors in judging the lithium precipitation phenomenon. In addition, the system will also load the lithium precipitation standard line under the corresponding conditions from the preset database for comparison.

[0056] In addition, it should be noted that the lithium plating standard line is formulated based on the changing characteristics of battery cell thickness under different SOC (State of Charge), different temperatures, and different charging rates.

[0057] Step S20: obtaining a cell thickness expansion curve based on the battery information, the charging rate and the cell thickness.

[0058] It should be noted that in this step, the system will first pre-process the collected battery information, charging rate and cell thickness to remove noise and outliers. Then, based on the processed data, the cell thickness expansion curve is drawn. The expansion curve reflects the change of the cell thickness during the charging process. Specifically, by extracting key features in the cell thickness expansion curve, such as slope change, peak position, etc. For example, during the battery charging process, the cell thickness will gradually increase as the charging proceeds. By drawing the cell thickness expansion curve in real time and observing the slope change and peak position of the curve, it is possible to preliminarily determine whether lithium plating has occurred inside the cell.

[0059] It is understandable that the slope change and peak position of the cell thickness expansion curve are important indicators for judging lithium deposition. A sudden increase in the slope or an abnormal shift in the peak position indicates that lithium deposition has occurred inside the cell.

[0060] In a feasible implementation manner, the step S20 specifically includes:

[0061] Step S201: Obtaining the state of charge and temperature of the battery according to the battery information.

[0062] It should be noted that in this step, the system will use the BMS or a separate sensor to collect key data such as the battery voltage, current and temperature in real time, and calculate the current state of charge (SOC) of the battery based on the collected voltage and current data using the ampere-hour integration method, open circuit voltage method or a combination of these algorithms.

[0063] It is understandable that SOC reflects the percentage of the remaining available capacity of the battery, while temperature is an important factor affecting battery performance and has a direct impact on the lithium deposition process of the battery cell. These data are important indicators for evaluating the charging and discharging status of the battery.

[0064] Step S202: obtaining a cell thickness expansion curve according to the state of charge, the temperature, the cell thickness and the charging rate.

[0065] It should be noted that if Figure 2 As shown, in this step, the system will synchronize the SOC and temperature data obtained in step S201 with the cell thickness data collected at the same time to ensure that the timestamps of the three are consistent. Based on the synchronized data, the cell thickness expansion curve at the current temperature is drawn with SOC as the horizontal axis and the cell thickness change as the vertical axis.

[0066] In this embodiment, by drawing the thickness expansion curve of the battery cell, the thickness change law of the battery cell during the charging and discharging process is intuitively displayed. Combined with the analysis of the charging rate, the time and degree of lithium deposition in the battery cell under different charging conditions can be further revealed, providing a basis for determining the specific time when lithium deposition occurs.

[0067] Step S30: providing a lithium battery lithium deposition warning according to the battery cell thickness expansion curve and the lithium deposition standard line.

[0068] It should be noted that in this step, the system will compare and analyze the cell thickness expansion curve with the lithium precipitation standard line to determine whether lithium precipitation occurs in the cell. If the characteristics of the cell thickness expansion curve meet the warning conditions for lithium precipitation, it will be judged that lithium precipitation occurs in the cell and the warning mechanism will be triggered. Specifically, once the warning mechanism is triggered, the system will take remedial measures. For example, reducing the charging rate to the pre-set safety rate in the system, performing small current discharge, etc., to mitigate the impact of lithium precipitation on battery performance. For example, during the battery charging process, if the slope of the cell thickness expansion curve suddenly increases and the peak position is abnormally offset, and after comparison with the lithium precipitation standard line, it is confirmed that lithium precipitation occurs, the system will immediately trigger the warning mechanism and send a warning message to the driver through the on-board display. At the same time, the system will automatically adjust the charging strategy, reduce the charging rate or perform small current discharge operations to mitigate the impact of lithium precipitation on battery performance.

[0069] In a feasible implementation manner, the step S30 specifically includes:

[0070] Step S301: fitting the battery cell thickness expansion curve with a lithium plating standard line to obtain a fitting deviation value.

[0071] It should be noted that in this step, the system will compare the thickness expansion curve of the battery cell under different working conditions (such as different SOC, different temperature, and different charging rate) with the lithium precipitation standard line obtained by fitting a large amount of experimental data in advance. The lithium precipitation standard line is based on the thickness expansion data obtained by testing multiple battery cell samples under various working conditions. It is determined through statistical analysis and curve fitting technology. It represents the abnormal thickness expansion trend that should not occur in the normal charging and discharging process of the battery cell. It is understandable that by fitting the real-time curve with the standard line, the system can calculate the deviation between the two. This deviation value reflects the degree of deviation between the current state of the battery cell and the normal state, and is an important basis for judging whether lithium precipitation occurs in the battery cell.

[0072] In addition, it should be noted that the fitting deviation value refers to the difference between the real-time thickness expansion curve and the lithium deposition standard line, usually expressed in numerical form. The size of the deviation value directly reflects the degree of deviation between the battery cell state and the standard lithium deposition state, and is a key indicator for determining whether the battery cell is lithium deposited.

[0073] Specifically, assuming that a battery cell is charged to 50% SOC at 0.8C rate and 25°C temperature, the real-time thickness expansion curve shows an abnormal growth trend. At this time, the system fits this curve with the lithium precipitation standard line at 0.8C rate and 25°C temperature, and finds that there is a slight deviation between the two. This deviation value is within the system's preset threshold, indicating that the current situation is within the range where lithium precipitation may occur. Therefore, the system determines that the battery cell may have lithium precipitation and triggers the early warning mechanism.

[0074] Step S302: When the fitting deviation value is within a preset fitting deviation range, a lithium plating warning signal is issued.

[0075] It should be noted that in this step, specifically, when the system detects that the fitting deviation value is within the preset fitting deviation range (the range is set in advance according to the specific type and performance requirements of the battery cell), the system will immediately trigger the lithium plating warning mechanism. At this time, the system will prompt the user that the battery has a risk of lithium plating through sound and light prompts and take corresponding measures. For example, assuming that the preset fitting deviation range is ±0.5%, when the fitting deviation value calculated in step S301 is within this range, the system immediately activates the warning mechanism, displays the words "Battery Cell Lithium Plating Warning" on the display screen of the control center, and issues a prompt sound to ensure that the user can receive the warning information in time.

[0076] In addition, it should be noted that the preset fitting deviation range is a reasonable range obtained through a large number of experiments and data analysis based on factors such as the specific type of battery cell, manufacturing process and performance requirements. The setting of this range should take into account the safety of the battery cell and the sensitivity of the early warning system, and should be able to accurately identify the lithium plating risk of the battery cell while avoiding the occurrence of false alarms and missed alarms.

[0077] The present embodiment provides a lithium battery lithium plating warning method, the method of the present embodiment includes: obtaining the battery information, charging rate and cell thickness and the lithium plating standard line during the current lithium battery charging and discharging process; obtaining the cell thickness expansion curve based on the battery information, the charging rate and the cell thickness; and performing lithium battery lithium plating warning according to the cell thickness expansion curve and the lithium plating standard line. In summary, the present embodiment realizes early warning and effective response to the lithium plating phenomenon by real-time monitoring of the changes in physical parameters during the battery charging and discharging process, combined with data analysis technology, solves the problem of how to accurately detect lithium plating in lithium batteries during battery use, and improves the safety and cycle life of lithium batteries.

[0078] Based on the first embodiment of the present application, in the second embodiment of the present application, the same or similar contents as those in the above-mentioned embodiment 1 can refer to the above introduction, and will not be repeated later. Figure 3 , Figure 3 This is a flow chart of the second embodiment of the lithium battery lithium deposition early warning method of the present application. Before step S10, it also includes:

[0079] Step S01: Obtain the historical state of charge, historical temperature, historical voltage, historical charging rate and historical cell thickness of the battery during the battery cyclic charge and discharge process.

[0080] It should be noted that in this step, the system will monitor and record the battery's state of charge (SOC), temperature, voltage, charge rate, and cell thickness changes under different conditions in real time. During multiple cycles of charging and discharging of the battery, the system automatically collects these data and stores them in a preset database. For example, the system selected 10 identical lithium batteries and performed 50 consecutive charge and discharge cycles in a laboratory environment. In each cycle, the changes in its SOC from 0% to 100% at different temperatures were recorded, while monitoring and recording real-time data on voltage, charge rate, and cell thickness.

[0081] In addition, it should be noted that these historical data refer to the changes in parameters such as voltage and thickness collected when the battery is charged and discharged under different conditions (such as different charging rates, different battery states SOC, different temperatures, etc.).

[0082] Step S02: obtaining a voltage differential curve and a historical battery cell thickness expansion curve according to the historical state of charge, the historical temperature, the historical voltage, the historical charging rate and the historical battery cell thickness.

[0083] It should be noted that in this step, specifically, the system uses SOC as the horizontal coordinate and the change in cell thickness as the vertical coordinate. At the same time, according to different charging rates, the thickness expansion curves at different rates and the voltage differential curves at different rates are plotted respectively.

[0084] In addition, it should be noted that the voltage differential curve is obtained by calculating the first-order inverse of the voltage data, which can reflect the rate of change of the voltage. It can be understood that this data is convenient for identifying the occurrence of lithium deposition inside the battery.

[0085] In a feasible implementation manner, the step S02 specifically includes:

[0086] Step A10: obtaining a voltage differential curve according to the historical state of charge, the historical temperature, the historical voltage and the historical charging rate.

[0087] It should be noted that, specifically, in this step, the system will perform differential processing based on the collected voltage data under different SOCs, temperatures, and charging rates, that is, calculate the rate of change of voltage over time to obtain a voltage differential curve. For example, the SOC is set to 20%, 40%, 60%, 80%, and 100%, the temperature is -7°C, 0°C, 10°C, 25°C, and 45°C, and the charging rate is selected to be 0.2C, 0.5C, 0.8C, 1.0C, and 1.5C. Perform charge and discharge cycles under each condition, and record the voltage data as historical data. Subsequently, the historical voltage data under different historical states are differentiated to obtain voltage differential curves under different conditions.

[0088] Step A20: obtaining a historical battery cell thickness expansion curve according to the historical state of charge, the historical temperature, the historical battery cell thickness and the historical charging rate.

[0089] It should be noted that, similar to step A10, the system also needs to collect the thickness data of the battery cell under different conditions and use these data as historical data. During the charge and discharge cycle, the thickness changes of the historical battery cell under different historical conditions are recorded in real time and plotted into a thickness expansion curve.

[0090] Step S03: determining a lithium deposition standard line according to the voltage differential curve and the historical battery cell thickness expansion curve.

[0091] It should be noted that in this step, the system determines the lithium precipitation standard line through data analysis and fitting algorithm based on the voltage differential curve and the historical battery cell thickness expansion curve obtained in step S02. Specifically, the system will identify abnormal points or turning points in the voltage differential curve and the historical battery cell thickness expansion curve, perform statistics and analysis on the abnormal points or turning points, and use mathematical fitting methods (such as linear regression, polynomial fitting, etc., which are not limited in this embodiment) to draw a lithium precipitation standard line based on the data of the turning point. This standard line will serve as a benchmark for subsequent judgment of whether lithium precipitation occurs in the battery.

[0092] In this embodiment, by obtaining the voltage data and the data on the change in battery cell thickness under different states during the battery cycle charging process and analyzing them as historical data, a standard line is obtained that can accurately reflect whether lithium deposition occurs in the battery cell, thereby improving the accuracy of lithium deposition detection in lithium batteries.

[0093] Based on the first and second embodiments of the present application, in the third embodiment of the present application, the same or similar contents as those in the first and second embodiments can be referred to the above description, and will not be described in detail later. Figure 4 , Figure 4 This is a flow chart of the third embodiment of the lithium battery lithium deposition early warning method of the present application, wherein step S03 specifically includes:

[0094] Step B10: Obtaining the voltage change rate according to the voltage differential curve.

[0095] It should be noted that if Figure 2 As shown in the figure, the voltage differential curve is obtained by real-time monitoring of the charging process of the battery cell at different charging rates (such as 0.2C, 0.5C, 0.8C, 1.0C, 1.5C), recording the voltage change data over time, and performing differential processing on it. Differential processing can highlight the inflection points of voltage change, which are closely related to the rate change of electrochemical reactions inside the battery cell. Specifically, in a preset test environment, such as a specific temperature (such as 25°C) and an initial SOC value (such as SOC=0%). Then, the system will charge at the set charging rate while collecting voltage data. The voltage data is processed using a numerical differential method (such as the difference method) to obtain a voltage differential curve. The voltage change rate is the slope of each point on the curve, which reflects the speed of the instantaneous change of voltage over time.

[0096] In addition, it should be noted that the "differential" in the voltage differential curve refers to the concept of derivative in mathematics, which is used to describe the instantaneous rate of change of a function at a certain point. In this embodiment, it is only used to describe the characteristics of the voltage change speed.

[0097] Step B20: obtaining the cell thickness expansion rate according to the historical cell thickness expansion curve.

[0098] It should be noted that the cell thickness expansion rate is an important indicator for measuring the volume change of the cell during the charge and discharge process. In this embodiment, by recording the thickness data of the cell at different charge rates, different SOCs and different temperatures, a historical cell thickness expansion curve is drawn. The cell thickness expansion rate is the rate of change of each point on the curve relative to the initial thickness.

[0099] It is understandable that the role of the cell thickness expansion rate is to directly reflect the changes in the internal structure of the cell, especially when lithium deposition occurs, lithium metal will be deposited on the negative electrode surface, causing the cell thickness to increase rapidly. Therefore, the abnormal cell thickness expansion rate can be used as an important criterion for the occurrence of lithium deposition.

[0100] Step B30: obtaining a lithium deposition inflection point according to the voltage change rate and the battery cell thickness expansion rate.

[0101] It should be noted that the lithium deposition inflection point refers to the point where the voltage change rate and the thickness expansion rate of the battery cell fluctuate abnormally during the charging process, which marks the beginning of the lithium deposition phenomenon. In this embodiment, by comprehensively analyzing the voltage differential curve and the battery cell thickness expansion curve, the point where the change trends of the two are inconsistent or significantly change at the same time is found, which is the lithium deposition inflection point.

[0102] Step B40: determining the lithium deposition standard line according to the lithium deposition inflection point.

[0103] It should be noted that in this step, the system will collect lithium deposition inflection point data of multiple cells at different charging rates, different SOCs and different temperatures. Then, statistical analysis is performed on these data to find statistical parameters such as the mean value and standard deviation of the lithium deposition inflection point. Finally, a lithium deposition standard line is drawn based on the statistical parameters. The line is usually a straight line or a curve used to distinguish between the normal charging state and the lithium deposition state.

[0104] In addition, it should be noted that the lithium precipitation standard line is a dynamic concept, which changes with the changes in battery performance, test conditions and other factors. Therefore, in practical applications, the lithium precipitation standard line needs to be regularly updated and maintained to ensure its accuracy and effectiveness.

[0105] It is understandable that the role of the lithium deposition standard line is to provide a unified judgment standard for battery cell lithium deposition detection and improve the accuracy and reliability of detection. In practical applications, the lithium deposition standard line can be adjusted and optimized according to different application scenarios and requirements.

[0106] In this embodiment, by comparing and analyzing the voltage differential curve and the historical cell thickness expansion curve, the lithium deposition inflection point where the lithium deposition phenomenon occurs is determined and the lithium deposition standard line is divided accordingly, providing a unified judgment standard for cell lithium deposition detection and improving the accuracy and reliability of detection.

[0107] This application also provides a lithium battery lithium deposition warning device, please refer to Figure 5 , the lithium battery lithium deposition early warning device comprises:

[0108] The data acquisition module 10 is used to obtain the battery information, charging rate, cell thickness and lithium precipitation standard line during the current lithium battery charging and discharging process;

[0109] A lithium analysis calibration module 20, configured to obtain a cell thickness expansion curve based on the battery information, the charge rate and the cell thickness;

[0110] The lithium deposition early warning module 30 is used to provide early warning of lithium deposition of the lithium battery according to the battery cell thickness expansion curve and the lithium deposition standard line.

[0111] The lithium battery lithium deposition early warning device provided by the present application adopts the lithium battery lithium deposition early warning method in the above embodiment, which can solve the technical problem of how to accurately detect lithium deposition in the lithium battery during the use of the battery. Compared with the prior art, the beneficial effects of the lithium battery lithium deposition early warning device provided by the present application are the same as the beneficial effects of the lithium battery lithium deposition early warning method provided by the above embodiment, and the other technical features of the lithium battery lithium deposition early warning device are the same as the features disclosed in the above embodiment method, which will not be repeated here.

[0112] The present application provides a lithium battery lithium deposition early warning device, the lithium battery lithium deposition early warning device comprising: at least one processor; and a memory communicatively connected to the at least one processor; wherein the memory stores instructions executable by the at least one processor, and the instructions are executed by the at least one processor so that the at least one processor can execute the lithium battery lithium deposition early warning method in the above-mentioned embodiment one.

[0113] Reference below Figure 6 , which shows a schematic diagram of the structure of a lithium battery lithium deposition early warning device suitable for implementing the embodiment of the present application. The lithium battery lithium deposition early warning device in the embodiment of the present application may include but is not limited to mobile terminals such as mobile phones, laptop computers, digital broadcast receivers, PDAs (Personal Digital Assistants), PADs (Portable Application Descriptions), PMPs (Portable Media Players), vehicle-mounted terminals (such as vehicle-mounted navigation terminals), etc., and fixed terminals such as digital TVs, desktop computers, etc. Figure 6 The lithium battery lithium plating warning device shown is merely an example and should not bring any limitation to the functions and scope of use of the embodiments of the present application.

[0114] like Figure 6As shown, the lithium battery lithium deposition early warning device may include a processing device 1001 (such as a central processing unit, a graphics processing unit, etc.), which can perform various appropriate actions and processes according to a program stored in a read-only memory (ROM: Read Only Memory) 1002 or a program loaded from a storage device 1003 to a random access memory (RAM: Random Access Memory) 1004. In RAM1004, various programs and data required for the operation of the lithium battery lithium deposition early warning device are also stored. The processing device 1001, ROM1002 and RAM1004 are connected to each other via a bus 1005. An input / output (I / O) interface 1006 is also connected to the bus. Typically, the following systems can be connected to the I / O interface 1006: input devices 1007 including, for example, a touch screen, a touchpad, a keyboard, a mouse, an image sensor, a microphone, an accelerometer, a gyroscope, etc.; output devices 1008 including, for example, a liquid crystal display (LCD), a speaker, a vibrator, etc.; storage devices 1003 including, for example, a magnetic tape, a hard disk, etc.; and communication devices 1009. The communication device 1009 can allow the lithium battery lithium deposition early warning device to communicate wirelessly or wired with other devices to exchange data. Although the figure shows a lithium battery lithium deposition early warning device with various systems, it should be understood that it is not required to implement or have all the systems shown. More or fewer systems may be implemented or provided alternatively.

[0115] In particular, according to the embodiments disclosed in the present application, the process described above with reference to the flowchart can be implemented as a computer software program. For example, the embodiments disclosed in the present application include a computer program product, which includes a computer program carried on a computer-readable medium, and the computer program includes a program code for executing the method shown in the flowchart. In such an embodiment, the computer program can be downloaded and installed from a network through a communication device, or installed from a storage device 1003, or installed from a ROM 1002. When the computer program is executed by the processing device 1001, the above-mentioned functions defined in the method of the embodiment disclosed in the present application are executed.

[0116] The lithium battery lithium deposition early warning device provided by the present application adopts the lithium battery lithium deposition early warning method in the above embodiment, which can solve the technical problem of how to accurately detect lithium deposition in the lithium battery during the use of the battery. Compared with the prior art, the beneficial effects of the lithium battery lithium deposition early warning device provided by the present application are the same as the beneficial effects of the lithium battery lithium deposition early warning method provided by the above embodiment, and the other technical features of the lithium battery lithium deposition early warning device are the same as the features disclosed in the method of the previous embodiment, which will not be repeated here.

[0117] It should be understood that the various parts disclosed in this application can be implemented by hardware, software, firmware or a combination thereof. In the description of the above embodiments, specific features, structures, materials or characteristics can be combined in any one or more embodiments or examples in a suitable manner.

[0118] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any person skilled in the art who is familiar with the present technical field can easily think of changes or substitutions within the technical scope disclosed in the present application, which should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.

[0119] The present application provides a computer-readable storage medium having computer-readable program instructions (ie, computer programs) stored thereon, and the computer-readable program instructions are used to execute the lithium battery lithium plating early warning method in the above-mentioned embodiment.

[0120] The computer-readable storage medium provided in the present application may be, for example, a USB flash drive, but is not limited to electrical, magnetic, optical, electromagnetic, infrared, or semiconductor systems, systems or devices, or any combination of the above. More specific examples of computer-readable storage media may include, but are not limited to: an electrical connection with one or more wires, a portable computer disk, a hard disk, a random access memory (RAM), a read-only memory (ROM), an erasable programmable read-only memory (EPROM or flash memory), an optical fiber, a portable compact disk read-only memory (CD-ROM), an optical storage device, a magnetic storage device, or any suitable combination of the above. In this embodiment, the computer-readable storage medium may be any tangible medium containing or storing a program that can be used by or in combination with an instruction execution system, system or device. The program code contained on the computer-readable storage medium may be transmitted using any appropriate medium, including but not limited to: wires, optical cables, RF (Radio Frequency), etc., or any suitable combination of the above.

[0121] The above-mentioned computer-readable storage medium may be included in the lithium battery lithium deposition early warning device; or it may exist independently without being assembled into the lithium battery lithium deposition early warning device.

[0122] The above-mentioned computer-readable storage medium carries one or more programs. When the above-mentioned one or more programs are executed by the lithium battery lithium deposition early warning device, the lithium battery lithium deposition early warning device: obtains the battery information, charging rate, battery cell thickness and lithium deposition standard line during the current lithium battery charging and discharging process; obtains the battery cell thickness expansion curve based on the battery information, the charging rate and the battery cell thickness; and performs lithium battery lithium deposition early warning according to the battery cell thickness expansion curve and the lithium deposition standard line.

[0123] Computer program code for performing the operations of the present application may be written in one or more programming languages ​​or a combination thereof, including object-oriented programming languages ​​such as Java, Smalltalk, C++, and conventional procedural programming languages ​​such as "C" or similar programming languages. The program code may be executed entirely on the user's computer, partially on the user's computer, as a separate software package, partially on the user's computer and partially on a remote computer, or entirely on a remote computer or server. In the case of a remote computer, the remote computer may be connected to the user's computer through any type of network, including a local area network (LAN) or a wide area network (WAN), or may be connected to an external computer (e.g., via the Internet using an Internet service provider).

[0124] The flow chart and block diagram in the accompanying drawings illustrate the possible architecture, function and operation of the system, method and computer program product according to various embodiments of the present application. In this regard, each square box in the flow chart or block diagram can represent a module, a program segment or a part of a code, and the module, the program segment or a part of the code contains one or more executable instructions for realizing the specified logical function. It should also be noted that in some alternative implementations, the functions marked in the square box can also occur in a sequence different from that marked in the accompanying drawings. For example, two square boxes represented in succession can actually be executed substantially in parallel, and they can sometimes be executed in the opposite order, depending on the functions involved. It should also be noted that each square box in the block diagram and / or flow chart, and the combination of the square boxes in the block diagram and / or flow chart can be implemented with a dedicated hardware-based system that performs a specified function or operation, or can be implemented with a combination of dedicated hardware and computer instructions.

[0125] The modules involved in the embodiments described in this application may be implemented by software or hardware, wherein the name of the module does not constitute a limitation on the unit itself in some cases.

[0126] The readable storage medium provided in this application is a computer-readable storage medium, which stores computer-readable program instructions (i.e., computer programs) for executing the above-mentioned lithium battery lithium deposition early warning method, and can solve the technical problem of how to accurately detect lithium deposition in lithium batteries during battery use. Compared with the prior art, the beneficial effects of the computer-readable storage medium provided in this application are the same as the beneficial effects of the lithium battery lithium deposition early warning method provided in the above-mentioned embodiment, and will not be repeated here.

[0127] The present application also provides a computer program product, including a computer program, which implements the steps of the lithium battery lithium plating early warning method as described above when executed by a processor.

[0128] The computer program product provided in this application can solve the technical problem of how to accurately detect lithium deposition in lithium batteries during battery use. Compared with the prior art, the beneficial effects of the computer program product provided in this application are the same as those of the lithium deposition early warning method provided in the above embodiment, and will not be elaborated here.

[0129] The above descriptions are only some embodiments of the present application, and are not intended to limit the patent scope of the present application. All equivalent structural changes made using the contents of the present application specification and drawings under the technical concept of the present application, or direct / indirect applications in other related technical fields are included in the patent protection scope of the present application.

Claims

1. A lithium battery lithium deposition early warning method, characterized in that: The method comprises: Obtain the battery information, charging rate, cell thickness and lithium plating standard line during the current lithium battery charging and discharging process; Obtaining a cell thickness expansion curve based on the battery information, the charging rate and the cell thickness; A lithium battery lithium deposition warning is performed according to the battery cell thickness expansion curve and the lithium deposition standard line.

2. The method according to claim 1, characterized in that The step of obtaining a cell thickness expansion curve based on the battery information, the charging rate and the cell thickness comprises: Obtaining a state of charge and a temperature of the battery according to the battery information; A cell thickness expansion curve is obtained according to the state of charge, the temperature, the cell thickness and the charging rate.

3. The method according to claim 1, characterized in that Before obtaining the battery information, charging rate, cell thickness and lithium plating standard line during the current lithium battery charging and discharging process, the method further includes: Obtain the battery's historical state of charge, historical temperature, historical voltage, historical charging rate, and historical cell thickness during the battery's cyclic charge and discharge process; Obtaining a voltage differential curve and a historical battery cell thickness expansion curve according to the historical state of charge, the historical temperature, the historical voltage, the historical charging rate, and the historical battery cell thickness; The lithium plating standard line is determined according to the voltage differential curve and the historical battery cell thickness expansion curve.

4. The method according to claim 3, characterized in that The step of determining the lithium precipitation standard line according to the voltage differential curve and the historical battery cell thickness expansion curve comprises: Obtaining a voltage change rate according to the voltage differential curve; Obtaining a cell thickness expansion rate according to the historical cell thickness expansion curve; Obtaining a lithium deposition inflection point according to the voltage change rate and the battery core thickness expansion rate; The lithium precipitation standard line is determined according to the lithium precipitation inflection point.

5. The method according to claim 3, characterized in that The step of obtaining a voltage differential curve and a historical battery cell thickness expansion curve according to the historical state of charge, the historical temperature, the historical voltage, the historical charging rate and the historical battery cell thickness comprises: Obtaining a voltage differential curve according to the historical state of charge, the historical temperature, the historical voltage, and the historical charging rate; A historical battery cell thickness expansion curve is obtained according to the historical state of charge, the historical temperature, the historical battery cell thickness and the historical charging rate.

6. The method according to claim 1, characterized in that The step of performing lithium battery lithium deposition early warning according to the battery cell thickness expansion curve and the lithium deposition standard line comprises: Fitting the battery core thickness expansion curve with the lithium precipitation standard line to obtain a fitting deviation value; When the fitting deviation value is within a preset fitting deviation range, a lithium plating warning signal is issued.

7. The method according to claim 1, characterized in that After the lithium battery lithium deposition warning is performed according to the battery cell thickness expansion curve and the lithium deposition standard line, the method further includes: A preset current is obtained, and the lithium battery is controlled to discharge according to the preset current.

8. A lithium battery lithium deposition early warning device, characterized in that: The device comprises: The data acquisition module is used to obtain the battery information, charging rate, cell thickness and lithium plating standard line during the current lithium battery charging and discharging process; A lithium analysis calibration module, used for obtaining a cell thickness expansion curve based on the battery information, the charging rate and the cell thickness; The lithium deposition early warning module is used to provide early warning of lithium deposition of the lithium battery according to the battery cell thickness expansion curve and the lithium deposition standard line.

9. A lithium battery lithium deposition early warning device, characterized in that: The device comprises: a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the computer program is configured to implement the steps of the lithium battery lithium plating early warning method as described in any one of claims 1 to 7.

10. A storage medium, characterized in that: The storage medium is a computer-readable storage medium, and a computer program is stored on the storage medium. When the computer program is executed by a processor, the steps of the lithium battery lithium deposition early warning method as described in any one of claims 1 to 7 are implemented.

Citation Information

Patent Citations

  • Cathode mix lithium precipitation parameter detection method, device, cathode mix detection system and computer readable storage medium

    CN110109029A

  • Method and system for judging lithium precipitation of battery cell

    CN110456275A

  • Nondestructive testing method for lithium precipitation of lithium ion battery

    CN111077456A

  • Battery charging lithium precipitation detection method and device and computer equipment

    CN112710957A

  • Battery lithium precipitation processing method and device and battery charging and discharging control device

    CN115765108A

Cited By

  • Lithium precipitation prediction method and device

    CN120870869A

  • A lithium precipitation prediction method and device

    CN120870869B

  • Battery performance evaluation method

    CN121208649A