Polydatin cataplasm and preparation method thereof

By adjusting the raw material ratio and preparation steps of Babu patch, a stable molding and strong adhesion force of Kabukiri was prepared, which solved the problem of inconvenience in carrying traditional external preparations of Kabukiri, and achieved effective transdermal administration of Kabukiri, and was equipped with Good efficacy and safety.

CN118986937APending Publication Date: 2024-11-22HUBEI UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410974082.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The traditional topical preparation of karuta is inconvenient to carry and has little application research, making it difficult to meet the needs of modern drug transdermal administration.

Method used

By adjusting the proportion and addition of raw materials in the babu patch, the main medicine is distributed evenly in the matrix in advance, a stool-spoken stool-spoken patch with stable molding, strong adhesion and uniform appearance and color are prepared. Carbomer , glycerol, polyethylene glycol 400, glycerol, azone and sodium polyacrylate and other raw materials, combined with specific preparation steps and stirring sequence, ensure the uniformity and moldability of the matrix.

Benefits of technology

The prepared syringae babu patch has stable molding, strong adhesion, uniform appearance and color, can be repeatedly uncovered, has good compatibility with the skin, and has a large amount of medicine. It can effectively exert the blood circulation and unblock the meridians, clear and relieve dampness and heat. , the effect of dispersing blood stasis and relieving pain, reducing toxic and side effects, and the dose is accurate, and the blood drug concentration is balanced without peaks and valleys.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118986937A_ABST
    Figure CN118986937A_ABST
Patent Text Reader

Abstract

The invention discloses a polydatin cataplasm and a preparation method thereof, and belongs to the technical field of pharmaceutical preparations. The cataplasm patch is prepared from the following raw materials: 0.1 to 0.2 g of polydatin, 0.10 to 0.12 g of carbomer, 0.06 to 0.08 g of dihydroxyaluminium aminoacetate, 0.01 to 0.015 g of tartaric acid, 1.016 to 1.397 g of polyethylene glycol 400, 2.7 to 3.3 g of glycerol, 0.225 to 0.27 g of azone and 0.83 to 1.02 g of sodium polyacrylate. The polydatin cataplasm prepared by optimizing the raw materials in the polydatin cataplasm and the addition amount of the raw materials and adopting a mode of uniformly distributing the main medicines in the matrix in advance has the advantages of being stable in forming, strong in adhesion force, uniform in appearance color, smooth in paste surface, capable of being repeatedly uncovered and pasted, good in compatibility with skin and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of pharmaceutical preparations, and in particular to a polydatin cataplasm patch and a preparation method thereof. Background Art

[0002] Babu is a new type of transdermal drug delivery preparation, mainly composed of water-soluble polymer skeleton materials, cross-linking agents, moisturizers, fillers, extracts, etc. Compared with traditional Chinese medicine external plasters, it has obvious advantages, such as large drug loading, strong moisturizing properties, good compatibility with the skin, and anti-aging; it can be repeatedly peeled and pasted, and the drug delivery can be terminated at any time; the dosage is accurate, the blood drug concentration is balanced without peaks and valleys, and the toxic side effects can be reduced. In recent years, it has attracted the attention of a large number of scientific researchers and has become a hot spot for development in the domestic and foreign pharmaceutical industries.

[0003] The Chinese medicine Polygonum cuspidatum is the dried stem and root of Polygonum cuspidatum, a plant of the Polygonaceae family. It has the effects of clearing away heat and detoxifying, dispersing blood stasis and relieving pain, relieving cough and reducing phlegm, and promoting dampness and jaundice. It is mostly used to treat blood diseases, joint pain, traumatic injuries, amenorrhea, lung heat cough, snake bites and traumatic bleeding, etc. Its main chemical components include quinones represented by rhamnolide, diphenylethylenes represented by resveratrol and rhamnolide, flavonoids represented by quercetin and other compounds, a total of four categories. Among them, rhamnolide and rhamnolide are used as content determination indicators for quality evaluation and control in the 2020 edition of the Chinese Pharmacopoeia.

[0004] Modern pharmacological studies have found that Polygonum cuspidatum has multiple pharmacological activities such as anti-AIDS, anti-cancer, antibacterial, antiviral, anti-inflammatory, antioxidant, hypoglycemic, anti-tissue (heart, brain, lung, kidney) damage, anti-lipid peroxidation, anti-osteoporosis, neuroprotection, hypolipidemic, and liver protection. Among them, Polygonum cuspidatum glycosides can not only relieve the pain caused by chronic pelvic endometriosis, but also have a skin care effect. In clinical practice, Polygonum cuspidatum can not only be taken orally, but also made into decoction or ointment for external application. At this stage, the research on Polygonum cuspidatum is mostly focused on analyzing its chemical composition, pharmacological effects, etc., and its application research is relatively small.

[0005] Therefore, the present invention aims at the disadvantages of traditional external preparations of Polygonum cuspidatum such as inconvenience in use and carrying, and provides a Babu patch containing active ingredients of Polygonum cuspidatum. Summary of the invention

[0006] In view of the above deficiencies in the prior art, the purpose of the present invention is to provide a polydatin cataplasm patch and a preparation method thereof. The present invention adjusts the raw materials and the amount of raw materials added in the cataplasm patch, and adopts a method of evenly distributing the main drug in the matrix in advance, so that the prepared polydatin cataplasm patch has the advantages of stable molding, strong adhesion, uniform appearance and color, smooth paste surface, repeated peeling, and good compatibility with the skin.

[0007] To achieve the above purpose, the specific technical solutions of the present invention are as follows:

[0008] A polydatin papu patch, the raw materials of which include: polydatin: 0.1-0.2g, carbomer: 0.10-0.12g, aluminum glycolate: 0.06-0.08g, tartaric acid: 0.01-0.015g, polyethylene glycol 400: 1.016-1.397g, glycerol: 2.7-3.3g, azone: 0.225-0.27g, sodium polyacrylate: 0.83-1.02g.

[0009] Preferably, the carbomer: 0.11 g, polyethylene glycol 400: 1.256 g, sodium polyacrylate: 0.899 g.

[0010] The present invention also provides a method for preparing a polydatin cataplasm patch, comprising the following steps:

[0011] (1) preparing an aqueous phase: weighing carbomer, preparing a carbomer matrix with deionized water, sealing and storing in a cool place for more than 12 hours; adding tartaric acid to the carbomer matrix to adjust the pH, stirring thoroughly, and then adding polyethylene glycol 400 to mix evenly to obtain an aqueous phase; preparing an oil phase: weighing glycerol, adding sodium polyacrylate to mix evenly, then adding aluminum glycolate to mix evenly, and then adding polydatin to mix evenly to obtain an oil phase;

[0012] (2) Preparing the matrix: firstly, the aqueous phase and the oil phase are mixed evenly, and then azone is added and mixed evenly to obtain the matrix;

[0013] (3) The matrix is ​​coated on a non-woven fabric, pressed into shape, and allowed to stand to obtain a polydatin patch.

[0014] Preferably, in step (1), the mass ratio of deionized water to carbomer is 10:(0.10-0.12).

[0015] Preferably, in step (1), the carbomer matrix needs to be sealed and stored in a cool place for 24 hours.

[0016] Preferably, steps (1) to (3) are all carried out at room temperature.

[0017] The use of the above-mentioned polydatin cataplasm patch in external patches.

[0018] The matrix in the Polydatin Babu patch provided by the present invention is a drug carrier of the main drug Polydatin, which ensures the release of the drug without affecting the stability of the drug. The inventors found in the process of establishing the present invention that in the preparation of the matrix, the proportion of each component, the order of addition, the stirring time, and whether the stirring is sufficient will affect the molding result of the matrix; in the preparation of the matrix, the mass of carbomer and sodium polyacrylate accounts for 3%-10% of the mass of the matrix. Carbomer and sodium polyacrylate are used as viscosity agents. Adding too much will cause the matrix to be more viscous, forming prematurely or not easy to be pressed by a mold; adding too little will cause the matrix to be difficult to form and present a mucus state; in the preparation of the oil phase, when aluminum glycolate and sodium polyacrylate are added at the same time, It will form a powdery mass that is difficult to dissolve, which not only affects the stickiness after the matrix is ​​formed, but also affects the dissolution of Polydatin in the matrix, so the present invention first adds a relatively large sodium polyacrylate and fully mixes it, and then adds aluminum glycolate; in the preparation process of the aqueous phase, after the carbomer is sealed and stored for 24 hours, it is necessary to first add tartaric acid, so that the jelly-like carbomer becomes liquid, and then mix it with the oil phase matrix; in the process of adding the component, if the added component fails to be mixed in time or fails to be fully mixed, it is easy to form a solid mass that is difficult to dissolve or a prematurely formed shaped block. The Polydatin Babu patch provided by the present invention can better play the effect of Polydatin in promoting blood circulation and unblocking collaterals, clearing dampness and heat, and dispersing blood stasis and relieving pain, and its drug loading is large, and it has strong moisture retention, good compatibility with the skin, and is resistant to aging. It can be repeatedly uncovered and pasted, and administration can be terminated at any time; the dosage is accurate, and the blood drug concentration is balanced without peak and valley phenomenon, which can reduce toxic and side effects.

[0019] Compared with the prior art, the present invention is beneficial in that:

[0020] (1) The present invention optimizes the raw materials of the matrix in the polydatin patch, the amount of raw materials added and the preparation method, and adopts a method of evenly distributing the main drug in the matrix in advance. The prepared polydatin patch has the advantages of stable molding, strong adhesion, uniform appearance and color, smooth paste surface, repeated peeling, and good compatibility with the skin.

[0021] (2) The Babu patch provided by the present invention has a large drug loading capacity and can better exert the effects of Polygonum cuspidatum on promoting blood circulation, unblocking meridians, clearing away dampness and heat, and dispersing blood stasis and relieving pain.

[0022] (3) The preparation method of the Babu patch provided by the present invention is simple and has a wide range of applications. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 is the response surface result of the interaction between factors A and B;

[0024] Figure 2 is the response surface result of the interaction between factors A and C;

[0025] Figure 3This is the response surface result of the interaction between factors C and B. DETAILED DESCRIPTION

[0026] The technical solution of the present invention will be described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0027] The invention provides a polydatin bap patch, the raw materials of which include: polydatin: 0.1-0.2g, carbomer: 0.10-0.12g, aluminum glyoxylate: 0.06-0.08g, tartaric acid: 0.01-0.015g, polyethylene glycol 400: 1.016-1.397g, glycerol: 2.7-3.3g, azone: 0.225-0.27g, and sodium polyacrylate: 0.83-1.02g.

[0028] The present invention also provides a method for preparing a polydatin cataplasm patch, comprising the following steps:

[0029] (1) preparing an aqueous phase: weighing carbomer, preparing a carbomer matrix with deionized water, sealing and storing in a cool place for more than 12 hours; adding tartaric acid to the carbomer matrix to adjust the pH, stirring thoroughly, and then adding polyethylene glycol 400 to mix evenly to obtain an aqueous phase; preparing an oil phase: weighing glycerol, adding sodium polyacrylate to mix evenly, then adding aluminum glycolate to mix evenly, and then adding polydatin to mix evenly to obtain an oil phase;

[0030] (2) Preparing the matrix: firstly, the aqueous phase and the oil phase are mixed evenly, and then azone is added and mixed evenly to obtain the matrix;

[0031] (3) The matrix is ​​coated on a non-woven fabric, pressed into shape, and allowed to stand to obtain a polydatin patch.

[0032] In some examples, the mass ratio of the deionized water to carbomer is 10:(0.10-0.12).

[0033] In some examples, the carbomer base needs to be sealed and stored in a cool place for 24 hours.

[0034] In some examples, steps (1)-(3) are all performed at room temperature.

[0035] Example 1

[0036] The present embodiment provides a polydatin cataplasm patch, the raw materials of which are: polydatin: 0.1g, water: 10g, carbomer: 0.12g, aluminum glycolate: 0.08g, tartaric acid: 0.015g, polyethylene glycol 400: 1.016g, glycerol: 2.7g, azone: 0.27g, sodium polyacrylate: 0.83g, and the preparation method is as follows:

[0037] (1) preparing an aqueous phase: weighing 0.12 g of carbomer, preparing a carbomer matrix with 10 g of deionized water, sealing and storing in a cool place for 24 hours; adding 0.015 g of tartaric acid to the carbomer matrix to adjust the pH, stirring thoroughly, and then adding 1.016 g of polyethylene glycol 400 to mix evenly to obtain an aqueous phase; weighing 2.7 g of glycerol, adding 0.83 g of sodium polyacrylate to mix evenly, then adding 0.08 g of aluminum glycolate to mix evenly, and then adding 0.1 g of polydatin to mix evenly to obtain an oil phase;

[0038] (2) Preparation of matrix: firstly, the aqueous phase and the oil phase were mixed evenly, and then 0.27 g of azone was added and mixed evenly to obtain the matrix;

[0039] (3) The matrix is ​​coated on a non-woven fabric, pressed into shape by a molding machine, and allowed to stand to obtain a polydatin patch.

[0040] Example 2

[0041] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.12g, aluminum glycoside: 0.08g, tartaric acid: 0.01g, polyethylene glycol 400: 1.016g, glycerol: 3.3g, azone: 0.225g, sodium polyacrylate: 0.83g.

[0042] Example 3

[0043] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.10g, aluminum glycoside: 0.06g, tartaric acid: 0.01g, polyethylene glycol 400: 1.016g, glycerol: 2.7g, azone: 0.225g, sodium polyacrylate: 0.83g.

[0044] Example 4

[0045] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.12g, aluminum glycoside: 0.06g, tartaric acid: 0.015g, polyethylene glycol 400: 1.016g, glycerol: 3.3g, azone: 0.225g, sodium polyacrylate: 1.02g.

[0046] Example 5

[0047] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.10g, aluminum glycoside: 0.06g, tartaric acid: 0.015g, polyethylene glycol 400: 1.397g, glycerol: 3.3g, azone: 0.225g, sodium polyacrylate: 0.83g.

[0048] Example 6

[0049] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1 g, water: 10 g, carbomer: 0.10 g, aluminum glycoside: 0.08 g, tartaric acid: 0.01 g, polyethylene glycol 400: 1.397 g, glycerol: 2.7 g, azone: 0.225 g, sodium polyacrylate: 1.02 g.

[0050] Example 7

[0051] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.10g, aluminum glycoside: 0.08g, tartaric acid: 0.01g, polyethylene glycol 400: 1.016g, glycerol: 3.3g, azone: 0.27g, sodium polyacrylate: 1.02g.

[0052] Example 8

[0053] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.10g, aluminum glycoside: 0.06g, tartaric acid: 0.015g, polyethylene glycol 400: 1.016g, glycerol: 2.7g, azone: 0.27g, sodium polyacrylate: 1.02g.

[0054] Example 9

[0055] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.12g, aluminum glycoside: 0.08g, tartaric acid: 0.015g, polyethylene glycol 400: 1.24g, glycerol: 2.7g, azone: 0.225g, sodium polyacrylate: 1.02g.

[0056] Example 10

[0057] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.10g, aluminum glycoside: 0.08g, tartaric acid: 0.015g, polyethylene glycol 400: 1.24g, glycerol: 3.3g, azone: 0.27g, sodium polyacrylate: 0.83g.

[0058] Embodiment 11

[0059] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.12g, aluminum glycoside: 0.06g, tartaric acid: 0.01g, polyethylene glycol 400: 1.24g, glycerol: 3.3g, azone: 0.27g, sodium polyacrylate: 0.83g.

[0060] Example 12

[0061] The preparation method of the polydatin patch provided in this embodiment is basically the same as that in Example 1, except that the raw materials of the polydatin patch are: polydatin: 0.1g, water: 10g, carbomer: 0.12g, aluminum glycoside: 0.06g, tartaric acid: 0.01g, polyethylene glycol 400: 1.24g, glycerol: 3.3g, azone: 0.27g, sodium polyacrylate: 1.02g.

[0062] Comparative Example 1

[0063] The preparation method of the polydatin patch of this comparative example is basically the same as that of Example 1, except that the carbomer in the preparation of the aqueous phase is replaced by an equal mass of sodium polyacrylate, that is, the raw materials of the polydatin patch of this comparative example are: polydatin: 0.1 g, water: 10 g, aluminum glycoside: 0.08 g, tartaric acid: 0.015 g, polyethylene glycol 400: 1.016 g, glycerol: 2.7 g, azone: 0.27 g, sodium polyacrylate: 0.95 g.

[0064] Comparative Example 2

[0065] The preparation method of the polydatin patch of this comparative example is basically the same as that of Example 1, except that the sodium polyacrylate in the oil phase preparation is replaced by carbomer of equal mass, that is, the raw materials of the polydatin patch of this comparative example are: polydatin: 0.1g, water: 10g, carbomer: 0.95g, aluminum glycoside: 0.08g, tartaric acid: 0.015g, polyethylene glycol 400: 1.016g, glycerol: 2.7g, azone: 0.27g.

[0066] Comparative Example 3

[0067] The preparation method of the polydatin patch of this comparative example is basically the same as that of Example 1, except that the raw materials of the polydatin patch of this comparative example are: polydatin: 0.1g, water: 10g, carbomer: 0.15g, aluminum glycoside: 0.08g, tartaric acid: 0.015g, polyethylene glycol 400: 1.016g, glycerol: 2.7g, azone: 0.27g, sodium polyacrylate: 1.1g.

[0068] Comparative Example 4

[0069] The preparation method of the polydatin patch of this comparative example is basically the same as that of Example 1, except that the raw materials of the polydatin patch of this comparative example are: polydatin: 0.1g, water: 10g, carbomer: 0.07g, aluminum glycoside: 0.08g, tartaric acid: 0.015g, polyethylene glycol 400: 1.016g, glycerol: 2.7g, azone: 0.27g, sodium polyacrylate: 0.7g.

[0070] Comparative Example 5

[0071] The raw material dosage of the polydatin cataplasm patch in this comparative example is the same as that in Example 1, and the preparation method is as follows:

[0072] (1) Preparing an aqueous phase: weighing 0.12 g of carbomer, preparing a carbomer matrix with 10 g of deionized water, sealing and storing in a cool place for 24 hours; adding 0.015 g of tartaric acid to the carbomer matrix to adjust the pH, stirring thoroughly, and then adding 1.016 g of polyethylene glycol 400 to mix evenly to obtain an aqueous phase; preparing an oil phase: weighing 2.7 g of glycerol, adding 0.83 g of sodium polyacrylate and 0.08 g of aluminum glycolate to mix evenly, and then adding 0.1 g of polydatin to mix evenly to obtain an oil phase;

[0073] (2) Preparation of matrix: firstly, the aqueous phase and the oil phase were mixed evenly, and then 0.27 g of azone was added and mixed evenly to obtain the matrix;

[0074] (3) The matrix is ​​coated on a non-woven fabric, pressed into shape by a molding machine, and allowed to stand to obtain a polydatin patch.

[0075] Comparative Example 6

[0076] The raw material dosage of the polydatin cataplasm patch in this comparative example is the same as that in Example 1, and the preparation method is as follows:

[0077] (1) preparing an aqueous phase: weighing 0.12 g of carbomer, preparing a carbomer matrix with 10 g of deionized water, sealing and storing in a cool place for 24 hours; adding 0.015 g of tartaric acid to the carbomer matrix to adjust the pH, stirring thoroughly, and then adding 1.016 g of polyethylene glycol 400 to mix evenly to obtain an aqueous phase; preparing an oil phase: weighing 2.7 g of glycerol, adding 0.27 g of azone, mixing evenly, then adding 0.83 g of sodium polyacrylate, mixing evenly, then adding 0.08 g of aluminum glycolate, mixing evenly, and then adding 0.1 g of polydatin to mix evenly to obtain an oil phase;

[0078] (2) Preparing the matrix: mixing the aqueous phase and the oil phase evenly to obtain the matrix;

[0079] (3) The matrix is ​​coated on a non-woven fabric, pressed into shape by a molding machine, and allowed to stand to obtain a polydatin patch.

[0080] Comparative Example 7

[0081] The raw material dosage of the polydatin cataplasm patch in this comparative example is the same as that in Example 1, and the preparation method is as follows:

[0082] (1) preparing an aqueous phase: weighing 0.12 g of carbomer, mixing it with 10 g of deionized water, then adding 0.015 g of tartaric acid to adjust the pH, stirring thoroughly, and then adding 1.016 g of polyethylene glycol 400 to mix evenly to obtain an aqueous phase; preparing an oil phase: weighing 2.7 g of glycerol, adding 0.83 g of sodium polyacrylate to mix evenly, then adding 0.08 g of aluminum glycolate to mix evenly, and then adding 0.1 g of polydatin to mix evenly to obtain an oil phase;

[0083] (2) Preparation of matrix: firstly, the aqueous phase and the oil phase were mixed evenly, and then 0.27 g of azone was added and mixed evenly to obtain the matrix;

[0084] (3) The matrix is ​​coated on a non-woven fabric, pressed into shape by a molding machine, and allowed to stand to obtain a polydatin patch.

[0085] Comparative Example 8

[0086] The raw material dosage of the polydatin cataplasm patch in this comparative example is the same as that in Example 1, and the preparation method is as follows:

[0087] (1) Preparing an aqueous phase: weighing 0.12 g of carbomer, preparing a carbomer matrix with 10 g of deionized water, sealing and storing in a cool place for 24 hours; adding 1.016 g of polyethylene glycol 400 to the carbomer matrix, mixing evenly, and then adding 0.015 g of tartaric acid to adjust the pH to obtain an aqueous phase; preparing an oil phase: weighing 2.7 g of glycerol, adding 0.83 g of sodium polyacrylate, mixing evenly, then adding 0.08 g of aluminum glycolate, mixing evenly, and then adding 0.1 g of polydatin, mixing evenly to obtain an oil phase;

[0088] (2) Preparation of matrix: firstly, the aqueous phase and the oil phase were mixed evenly, and then 0.27 g of azone was added and mixed evenly to obtain the matrix;

[0089] (3) The matrix is ​​coated on a non-woven fabric, pressed into shape by a molding machine, and allowed to stand to obtain a polydatin patch.

[0090] According to the scoring items and standards in Table 1, the polydatin cataplasm patches prepared in Examples 1-12 and Comparative Examples 1-8 were scored, and the initial adhesion, appearance, selective permeability, repeated peeling and pasting, skin followability, skin residue and other factors were used as indicators for evaluation. The higher the score, the better the comprehensive index. The scoring results are shown in Table 2.

[0091] Table 1: Scoring criteria for Polydatin Babu Patch

[0092]

[0093] Table 2: Scoring results of Polydatin Babu Patch

[0094]

[0095] Based on the role and influence of each raw material component of the polydatin plaque patch matrix in the preparation, the Plackett-Burman test was used to determine the influencing factors and their levels, among which the influencing factors were sodium polyacrylate (A), polyethylene glycol 400 (B) and carbomer (C). The specific steps are as follows:

[0096] (1) Using the Box-Behnken model experimental design, factors A, B and C are used as response variables, and the response value is a comprehensive score. Response surface analysis is performed. The response surface reflects the response values ​​under different parameters, and the interaction between the parameters and the relationship with the response value can be intuitively seen. The response surface results are shown in Figure 1-3 shown.

[0097] Among them, factor A takes values ​​of 0.80g, 0.90g, and 1.00g, corresponding to levels -1, 0, and 1 respectively; factor B takes values ​​of 0.80ml, 0.95ml, and 1.10ml, corresponding to levels -1, 0, and 1 respectively; factor C takes values ​​of 0.10g, 0.11g, and 0.12g, corresponding to levels -1, 0, and 1 respectively; the factor level table is shown in Table 3.

[0098] (2) The Box-Behnken model test in Design-Expert.11.1.0.1 obtained the quadratic polynomial equation for the comprehensive score of polydatin patch with three factors: sodium polyacrylate (A), polyethylene glycol 400 (B) and carbomer (C) as follows:

[0099] Y(OD)=78.53+0.04A+0.24B+0.06C-0.08AB+0.85AC-0.36BC-0.47A 2 -0.40B 2 -1.16C 2

[0100] The Box-Behnken test design and results are shown in Table 4; the response surface regression analysis model variance analysis is shown in Table 5.

[0101] Table 3: Box-Behnken test factor level table

[0102]

[0103] Table 4: Box-Behnken test design and results

[0104]

[0105] Table 5: Analysis of variance of response surface regression model

[0106]

[0107] As shown in Table 5, the regression model P < 0.05 has statistical significance, indicating that the model has a good fit and can reflect the impact of the three factors on the comprehensive score. 2 It has a significant effect on the comprehensive score of Polydatin Babu Patch (P<0.05), which shows that there is no simple linear relationship between the factors and the response values, and it has a certain statistical significance.

[0108] The maximum estimated value of the response value is 78.57, at which the amounts of carbomer, polyethylene glycol 400, and sodium polyacrylate used are 0.110 g, 0.997 ml, and 0.899 g, respectively.

[0109] The above specific embodiments describe the implementation of the present invention in detail, but the present invention is not limited to the specific details in the above embodiments. Within the scope of the claims and technical concept of the present invention, the technical solution of the present invention can be modified and changed in many simple ways, and these simple modifications all belong to the protection scope of the present invention.

Claims

1. A polydatin basilixin patch, It is characterized in that The raw materials include: polydatin: 0.1-0.2g, carbomer: 0.10-0.12g, aluminum glycolate: 0.06-0.08g, tartaric acid: 0.01-0.015g, polyethylene glycol 400: 1.016-1.397g, glycerol: 2.7-3.3g, azone: 0.225-0.27g, sodium polyacrylate: 0.83-1.02g.

2. A polydatin cataplasm patch according to claim 1, It is characterized in that The carbomer: 0.11 g, polyethylene glycol 400: 1.256 g, sodium polyacrylate: 0.899 g.

3. A method for preparing a polydatin cataplasm patch according to claim 1, It is characterized in that The following steps are involved: (1) preparing an aqueous phase: weighing carbomer, preparing a carbomer matrix with deionized water, sealing and storing in a cool place for more than 12 hours; adding tartaric acid to the carbomer matrix to adjust the pH, stirring thoroughly, and then adding polyethylene glycol 400 to mix evenly to obtain an aqueous phase; preparing an oil phase: weighing glycerol, adding sodium polyacrylate to mix evenly, then adding aluminum glycolate to mix evenly, and then adding polydatin to mix evenly to obtain an oil phase; (2) Preparing the matrix: firstly, the aqueous phase and the oil phase are mixed evenly, and then azone is added and mixed evenly to obtain the matrix; (3) The matrix is ​​coated on a non-woven fabric, pressed into shape, and allowed to stand to obtain a polydatin patch.

4. A method for preparing a polydatin cataplasm patch according to claim 3, It is characterized in that In step (1), the mass ratio of deionized water to carbomer is 10:(0.10-0.12).

5. A method for preparing a polydatin cataplasm patch according to claim 3, It is characterized in that In step (1), the carbomer matrix needs to be sealed and stored in a cool place for 24 hours.

6. A method for preparing a polydatin cataplasm patch according to claim 3, It is characterized in that The steps (1) to (3) are all carried out at room temperature.

7. Use of the polydatin cataplasm patch according to any one of claims 1 to 2 or the polydatin cataplasm patch prepared by the method according to any one of claims 3 to 6 in external patches.