Crystallizer and method for uniformly cooling crystallizer

By dividing copper pipes in the crystallizer and setting cooling water sleeves to adjust the width of the water joints, the cracks and steel leakage problems caused by uneven cooling of the corners of the casting machine in the continuous casting machine are solved, and the uniformity of the corners of the casting billet is achieved. and improve heat transfer efficiency.

CN118989259APending Publication Date: 2024-11-22SHANDONG IRON & STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411207220.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In continuous casting machines, uneven cooling of the corners of the crystallizer casting billet leads to cracks and steel leakage, which is difficult to effectively solve in the prior art.

Method used

Design a crystallizer, by dividing the copper tube into upper and lower copper tubes and setting a cooling water jacket on its outer wall, adjusting the width of the water joint to reduce two-dimensional heat transfer at the corners, increasing the heat transfer on the face, and ensuring the corners of the casting blank Thickness uniformity.

Benefits of technology

It effectively reduces the solidification and shrinkage of the primary blank shell at the corner of the crystallizer meniscus, reduces the formation of air gaps, improves the thickness and uniformity of the corner shell of the casting billet, and controls cracks and steel leakage accidents.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118989259A_ABST
    Figure CN118989259A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of continuous casting, and particularly discloses a crystallizer which comprises a crystallizer copper pipe and a cooling water jacket. And a water seam is formed between the outer wall surface of the crystallizer copper pipe and the inner wall surface of the cooling water jacket. The crystallizer copper pipe is divided into an upper copper pipe body and a lower copper pipe body, the upper copper pipe body is located above the lower copper pipe body, and the thickness of the face of the upper copper pipe body is smaller than that of the corner so that the width of a water seam, corresponding to the corner, of the upper copper pipe body can be smaller than that of a water seam, corresponding to the face, of the upper copper pipe body. The thickness of the surface part of the lower copper pipe is equal to that of the corner part, and the thicknesses of the surface parts of the upper copper pipe and the lower copper pipe are the same; wherein the corner part is in the range of 30-50mm from the outer wall of the crystallizer copper pipe to the vertex angle. According to the crystallizer provided by the invention, the two-dimensional heat transfer of the meniscus corner of the crystallizer is reduced, the uniformity of a casting blank shell discharged from the crystallizer is improved, and the accidents of casting blank corner cracks and corner crack bleed-out are effectively controlled. The invention further discloses a method for uniformly cooling the crystallizer, and the method also has the technical effects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of continuous casting, and more particularly to a crystallizer and a method for uniformly cooling the crystallizer. Background Art

[0002] During the production of the continuous casting machine, after the molten steel in the tundish is injected into the crystallizer, the molten steel on the curved surface of the crystallizer directly contacts the copper tube wall to form the primary billet shell. Under the static pressure of the molten steel, the billet shell is in close contact with the copper tube wall. Since the corners of the crystallizer are two-dimensional heat transfer with a fast heat transfer rate, air gaps first appear at the corners of the billet when the primary billet shell solidifies; the face of the crystallizer is one-dimensional heat transfer with a slow heat transfer rate, and air gaps are formed later, resulting in the thickness of the billet shell on the face of the crystallizer being greater than the thickness of the billet shell at the corners. Therefore, when there are abnormal conditions such as fast pulling speed, high tundish temperature, and large fluctuations in the crystallizer liquid level, cracks are formed at the corners of the billet under the static pressure and thermal stress of the molten steel at the bottom of the crystallizer or after exiting the crystallizer. When the crack depth exceeds the critical point, steel leakage occurs.

[0003] In summary, how to effectively solve the problems of uneven crystallizer shell, corner cracks and even steel leakage is a problem that technical personnel in this field need to solve. Summary of the invention

[0004] In view of this, an object of the present invention is to provide a crystallizer and a method for uniformly cooling the crystallizer, the structural design of which can effectively solve the problem of corner cracks or even steel leakage in the crystallizer casting.

[0005] In order to achieve the above object, the present invention provides the following technical solutions:

[0006] A crystallizer comprises a crystallizer copper tube and a cooling water jacket sleeved outside the crystallizer copper tube, a water gap is formed between the outer wall surface of the crystallizer copper tube and the inner wall surface of the cooling water jacket, the crystallizer copper tube is divided into an upper copper tube and a lower copper tube, the upper copper tube is located above the lower copper tube, the thickness of the face of the upper copper tube is smaller than the thickness of the corner, so that the width of the water gap corresponding to the corner of the upper copper tube is smaller than the width of the water gap corresponding to the face; the thickness of the face of the lower copper tube is equal to the thickness of the corner, and the thicknesses of the faces of the upper copper tube and the lower copper tube are the same; wherein the corner is a range of 30-50 mm from the outer wall of the crystallizer copper tube to the top angle.

[0007] Optionally, in the above-mentioned crystallizer, the thickness of the face of the crystallizer copper tube is in the range of 12-16 mm, and the width of the water seam corresponding to the face of the crystallizer copper tube is in the range of 3.0-4.5 mm;

[0008] The thickness of the corner of the lower copper tube ranges from 12 to 16 mm, and the corresponding width of the water gap ranges from 3.0 to 4.5 mm.

[0009] Optionally, in the above-mentioned crystallizer, the corner thickness of the upper copper tube ranges from 13 to 17 mm, and the corresponding width of the water seam ranges from 2.0 to 3.5 mm.

[0010] Optionally, in the above-mentioned crystallizer, the width of the water gap corresponding to the surface of the upper copper tube is 1.0-1.5 mm larger than the width of the water gap corresponding to the corner.

[0011] Optionally, in the above crystallizer, the length of the crystallizer copper tube ranges from 800 to 1100 mm;

[0012] The upper copper tube is a portion corresponding to a length range of 400-500 mm downward from the top of the crystallizer copper tube;

[0013] The lower copper tube is a portion corresponding to a length range of 400-600 mm upward from the bottom end of the crystallizer copper tube.

[0014] Optionally, in the above-mentioned crystallizer, the crystallizer copper tube includes four sides of equal length, and two adjacent sides are respectively perpendicular, the outer wall of each side corresponding to the corner protrudes from the outer wall of the face, and the outer wall corresponding to the corner and the outer wall corresponding to the face are transitioned through an inclined surface.

[0015] Optionally, in the above-mentioned crystallizer, the thickness of the corners of the upper copper tube gradually decreases from top to bottom.

[0016] Optionally, in the above-mentioned crystallizer, the crystallizer copper tube is formed by integral stamping.

[0017] The crystallizer provided by the present invention includes a crystallizer copper tube and a cooling water jacket. The cooling water jacket is arranged outside the crystallizer copper tube, and a water gap is formed between the outer wall surface of the crystallizer copper tube and the inner wall surface of the cooling water jacket. The crystallizer copper tube is divided into an upper copper tube and a lower copper tube, the upper copper tube is located above the lower copper tube, and the thickness of the face of the upper copper tube is less than the thickness of the corner, so that the width of the water gap corresponding to the corner of the upper copper tube is less than the width of the water gap corresponding to the face; the thickness of the face of the lower copper tube is equal to the thickness of the corner, and the thickness of the face of the upper copper tube and the lower copper tube are the same; wherein the corner is the outer wall of the crystallizer copper tube and is within the range of 30-50mm from the top angle.

[0018] By using the crystallizer provided by the present invention, the copper tube of the crystallizer is divided into an upper copper tube and a lower copper tube, and the corner thickness of the upper copper tube is set to be greater than the face thickness, so that the width of the water gap corresponding to the corner of the upper copper tube is smaller than the width of the water gap corresponding to the face, thereby reducing the two-dimensional heat transfer at the corner of the curved liquid surface of the crystallizer, slowing down the solidification shrinkage of the raw billet shell at the corner of the curved liquid surface of the crystallizer copper tube, and reducing the air gap between the raw billet shell and the crystallizer copper tube, thereby increasing the heat transfer efficiency at the corner below the curved liquid surface of the crystallizer, improving the billet shell thickness at the corner of the cast billet leaving the crystallizer, increasing the uniformity of the billet shell of the cast billet leaving the crystallizer, and effectively controlling the cracks at the corner of the cast billet and the corner crack steel leakage accidents.

[0019] In order to achieve the above object, the present invention provides the following technical solutions:

[0020] A method for uniformly cooling a crystallizer, used for any of the above-mentioned crystallizers, comprising:

[0021] Check the shell formed by the crystallizer;

[0022] Take the billet shell with corner cracks and steel leakage as the test billet shell, and measure the corner thickness and face thickness of the test billet shell;

[0023] Calculating the difference between the face thickness and the corner thickness of the test blank shell, and calculating the proportional relationship between the difference and the corner thickness;

[0024] According to the proportional relationship, the face thickness and corner thickness of the upper copper tube of the crystallizer are set so that the ratio of the difference between the width of the water gap corresponding to the face of the upper copper tube and the width of the water gap corresponding to the corner to the width of the water gap corresponding to the face satisfies the proportional relationship.

[0025] The method for uniform cooling of the crystallizer provided by the present invention is applied to actually measure the billet shell that produces corner cracks or steel leakage in the crystallizer, obtain the proportional relationship between the difference between the face thickness and the corner thickness of the billet shell and the corner thickness, and set the size of the crystallizer steel tube accordingly, so that the ratio of the difference between the width of the water gap corresponding to the face of the upper copper tube and the width of the water gap corresponding to the corner and the width of the water gap corresponding to the face satisfies the above proportional relationship, thereby reducing the heat transfer at the upper corner of the crystallizer, reducing the cold water flow at the upper corner of the crystallizer, and then slowing down the solidification shrinkage of the raw billet shell at the corner of the curved liquid surface of the crystallizer copper tube, reducing the air gap between the raw billet shell and the crystallizer copper tube, thereby increasing the heat transfer efficiency of the corner below the curved liquid surface of the crystallizer, improving the billet shell thickness at the corner of the cast billet out of the crystallizer, increasing the uniformity of the billet shell of the cast billet out of the crystallizer, and effectively controlling the cracks at the corner of the cast billet and the corner crack steel leakage accidents. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0027] Figure 1 It is a schematic diagram of the upper cross section of a crystallizer according to a specific embodiment of the present invention;

[0028] Figure 2 It is a schematic cross-sectional view of the lower part of a crystallizer according to a specific embodiment of the present invention;

[0029] Figure 3 The present invention is a schematic flow chart of a method for uniformly cooling a crystallizer according to a specific embodiment of the present invention.

[0030] Reference numerals:

[0031] 110-upper copper tube; 120-lower copper tube; 101-face; 102-corner; 200-cooling water jacket; 300-water seam. DETAILED DESCRIPTION

[0032] The embodiment of the present invention discloses a crystallizer and a method for uniformly cooling the crystallizer, so as to avoid uneven shell of the continuous casting machine crystallizer and cracks and steel leakage at the corners of the casting, promote the improvement of product quality, and ensure stable and smooth production.

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] In the process of realizing the present invention, the inventors found that in order to make the shell of the continuous casting machine crystallizer blank uniform and avoid cracks and steel leakage at the corners of the casting blank, the corners of the cooling water jacket can be arranged close to the corners of the crystallizer copper tube, so that the width of the corner water gap of the crystallizer copper tube is smaller than the width of the side water gap. When water flows through the corner water gap and the face water gap, the water flow in the face water gap is larger, which can better cool the face of the crystallizer copper tube. The water flow in the corner water gap is smaller, which weakens the cooling of the corner of the crystallizer copper tube, but the corner cooling improvement effect is not obvious. Small water gap control is only achieved in a very small range of the copper tube corner, that is, the water gap width is within 10 mm, and the thickness of the crystallizer copper tube is generally above 12 mm. Therefore, the actual two-dimensional heat transfer situation at the corner is not effectively improved.

[0035] In the present application, the crystallizer copper tube is divided into an upper copper tube and a lower copper tube, and unlike the position adjustment, the thickness of the copper tube is set accordingly in the present application to change the width of the water gap, thereby substantially improving the cooling uniformity of the crystallizer shell.

[0036] See also Figure 1 -Figure, in some embodiments, the crystallizer provided by the present invention includes a crystallizer copper tube and a cooling water jacket 200. Among them, the cooling water jacket 200 is sleeved outside the crystallizer copper tube, and a water gap 300 is formed between the outer wall surface of the crystallizer copper tube and the inner wall surface of the cooling water jacket 200. The crystallizer copper tube is divided into an upper copper tube 110 and a lower copper tube 120, and the upper copper tube 110 is located above the lower copper tube 120, that is, the crystallizer copper tube is divided into an upper copper tube 110 and a lower copper tube 120 along the up and down direction. It can be understood that the upper copper tube 110 and the lower copper tube 120 are only used to distinguish different parts of the crystallizer copper tube, and the two can be specifically an integrated structure. In the use state, the upper copper tube 110 is located above the lower copper tube 120. The shape of the cavity surrounded by the crystallizer copper tube is set accordingly according to the structure of the required forming blank shell. The present application can be applied to square billets (especially small square billets) to solve the problem of uneven cooling of the corners 102 and the face 101 when the crystallizer is cooled. The crystallizer copper tube includes a face portion 101 and a corner portion 102. The corner portion 102 is a portion connected between two adjacent face portions 101. The number of face portions 101 can be set accordingly according to the structure of the required blank shell. For example, when a square billet is formed, the number of face portions 101 is four, and the number of corresponding corner portions 102 is also four.

[0037] The thickness of the face 101 of the upper copper tube 110 is smaller than the thickness of the corner 102, so that the width of the water gap 300 corresponding to the corner 102 of the upper copper tube 110 is smaller than the width of the water gap 300 corresponding to the face 101, the thickness of the face 101 of the lower copper tube 120 is equal to the thickness of the corner 102, and the thickness of the face 101 of the upper copper tube 110 and the lower copper tube 120 are the same. The inventor of the present application found in the process of realizing the present application that the solidification heat transfer in the crystallizer is mainly concentrated in the upper part of the crystallizer, so by reducing the cooling intensity of the corner of the primary blank shell of the upper part of the crystallizer, the solidification shrinkage of the primary blank shell at the corner is delayed, the thickness of the primary blank shell at the corner is increased, and the solidification uniformity of the cast blank at the upper part of the crystallizer is improved. Corresponding to the lower part of the crystallizer, the primary blank shell has reached a certain thickness and strength at this time, and it is not easy to crack at the corner, so the cooling intensity of the corner 102 and the face 101 corresponding to the lower part of the crystallizer can be equal. Based on this, in the present application, different structural designs are adopted for the upper and lower parts of the crystallizer copper tube. The thickness of the face 101 of the upper copper tube 110 is less than the thickness of the corner 102, that is, the copper tube at the corner 102 is thickened. On the one hand, the width of the water gap 300 corresponding to the corner 102 of the upper copper tube 110 is smaller than the width of the water gap 300 corresponding to the face 101, so that the water flow rate of the water gap 300 at the corner 102 is smaller than the water flow rate of the water gap 300 at the face 101, thereby weakening the cooling of the corner of the crystallizer copper tube; on the other hand, since the thickness of the crystallizer copper tube at the corner 102 is thicker, the heat transfer effect can also be reduced to a certain extent. Therefore, the above arrangement of the upper copper tube 110 reduces the two-dimensional heat transfer at the corner of the curved liquid surface of the crystallizer, slows down the solidification shrinkage of the primary billet shell at the corner of the curved liquid surface of the crystallizer copper tube, reduces the air gap between the primary billet shell and the crystallizer copper tube, thereby increasing the heat transfer efficiency at the corner below the curved liquid surface of the crystallizer, improving the billet shell thickness at the corner of the billet leaving the crystallizer, and increasing the uniformity of the billet shell of the billet leaving the crystallizer.

[0038] The corner 102 is the range of 30-50 mm from the outer wall of the crystallizer copper tube to the top corner. That is, the portion of the outer wall of the crystallizer copper tube within the range of 30-50 mm from the top corner of the crystallizer copper tube is taken as the corner 102, and the portion between two adjacent corners 102 is the face 101. The corner 102 is limited to the above range, and the thickness of the upper copper tube 110 is specially designed accordingly to make the shell uniform.

[0039] By using the crystallizer provided by the present invention, the crystallizer copper tube is divided into an upper copper tube 110 and a lower copper tube 120, and the thickness of the corner 102 of the upper copper tube 110 is set to be greater than the thickness of the face 101, so that the width of the water gap 300 corresponding to the corner 102 of the upper copper tube 110 is smaller than the width of the water gap 300 corresponding to the face 101, thereby reducing the two-dimensional heat transfer at the corner 102 of the curved liquid surface of the crystallizer, slowing down the solidification shrinkage of the raw billet shell at the corner 102 of the curved liquid surface of the crystallizer copper tube, and reducing the air gap between the primary billet shell and the crystallizer copper tube, thereby increasing the heat transfer efficiency of the corner 102 below the curved liquid surface of the crystallizer, improving the billet shell thickness at the corner 102 of the crystallizer billet, increasing the uniformity of the billet shell of the crystallizer billet, and effectively controlling the cracks at the corner 102 of the billet and the corner crack steel leakage accidents.

[0040] Specifically, the portion of the outer wall of the upper copper tube 110 corresponding to the corner 102 protrudes from the portion corresponding to the face 101, that is, the outer wall of the corner 102 protrudes, so that the thickness of the corner 102 is greater than the thickness of the face 101, and thus the width of the water gap 300 of the corner 102 is smaller than the width of the water gap 300 of the face 101. With such a configuration, the cooling water jacket 200 can adopt a conventional structure, especially when modifying the existing crystallizer structure, only the crystallizer copper tube needs to be modified, and the cooling water jacket 200 does not need to be replaced, thereby reducing the cost.

[0041] In some embodiments, the thickness of the face 101 of the crystallizer copper tube ranges from 12 to 16 mm, and the width of the water gap 300 corresponding to the face 101 of the crystallizer copper tube ranges from 3.0 to 4.5 mm. The thickness of the face 101 of the crystallizer copper tube is consistent between the upper copper tube 110 and the lower copper tube 120, so the thickness of the face 101 is set within the range of 12 to 16 mm, and a good heat transfer effect can be obtained. Correspondingly, the width of the water gap 300 corresponding to the face 101 of the crystallizer copper tube is also consistent between the upper copper tube 110 and the lower copper tube 120, so the width of the water gap 300 is set within the range of 3.0 to 4.5 mm, and a good heat transfer effect can be obtained. For the lower copper tube 120, the thickness of its corner 102 is equal to the thickness of the face 101, and the width of the water gap 300 of the corner 102 corresponding to the corresponding lower copper tube 120 is also equal to the width of the water gap 300 of the face 101. Therefore, the thickness of the corner portion 102 of the lower copper tube 120 is in the range of 12-16 mm, and the corresponding width of the water gap 300 is in the range of 3.0-4.5 mm.

[0042] In some embodiments, the thickness of the corner 102 of the upper copper tube 110 is in the range of 13-17 mm, and the corresponding width of the water gap 300 is in the range of 2.0-3.5 mm. It is understandable that the thickness of the corner 102 of the upper copper tube 110 is in the range of 13-17 mm, and the thickness of the face 101 is in the range of 12-16 mm. For any crystallizer, the thickness of the corner of the upper copper tube 110 is greater than the thickness of the face, and the thickness of the corner and the thickness of the face are respectively within the above numerical range. Since when the thickness of the corner of the upper copper tube 110 is lower than this range, the smaller the angle thickness, the greater the cooling intensity of the upper corner 102 of the crystallizer, and the uniform cooling effect is not achieved. The primary shell of the corner 102 is still thin, and it is easy to have cracks in the corner of the casting and steel leakage from the corner cracks. When the corner thickness of the upper copper tube 110 is greater than this range, the greater the corner thickness, the lower the cooling strength of the upper corner 102 of the crystallizer. Too low cooling strength and insufficient cooling strength also lead to a thin primary shell at the corner. Therefore, the corner thickness of the upper copper tube 110 is set within the range of 13-17 mm, and the width of the corresponding water gap 300 is within the range of 2.0-3.5 mm, which can provide a cooling strength similar to that of the surface 101, thereby improving the uniformity of the shell.

[0043] In some embodiments, the width of the water gap 300 corresponding to the upper copper tube 110 at the face 101 is 1.0-1.5 mm greater than the width of the water gap 300 corresponding to the corner 102. The width of the water gap 300 corresponding to the lower copper tube 120 at the face 101 is equal to the width of the water gap 300 corresponding to the corner 102. By setting the face thickness and angle thickness of the upper copper tube 110, the width of the water gap 300 corresponding to the upper copper tube 110 at the face 101 is 1.0-1.5 mm greater than the width of the water gap 300 corresponding to the corner 102. The difference in the width of the water gap 300 is controlled within the above range, which can make the two-dimensional heat transfer at the corner of the curved liquid surface of the crystallizer similar to the heat transfer effect at the face, thereby achieving uniform cooling of the face and corner.

[0044] In some embodiments, the length of the copper tube of the crystallizer ranges from 800 to 1100 mm; the upper copper tube 110 is a portion corresponding to a length range of 400 to 500 mm from the top of the copper tube of the crystallizer downward; and the lower copper tube 120 is a portion corresponding to a length range of 400 to 600 mm from the bottom of the copper tube of the crystallizer upward. According to the growth of the blank shell during the operation of the crystallizer and the position where the blank shell is uneven, the division position of the upper copper tube 110 and the lower copper tube 120 is set accordingly to make the crystallizer cool evenly.

[0045] In some embodiments, the crystallizer copper tube includes four sides of equal length, and two adjacent sides are respectively perpendicular, the outer wall of each side corresponding to the corner 102 protrudes from the outer wall of the face 101, and the outer wall of the corresponding corner 102 and the outer wall of the corresponding face 101 are transitioned through an inclined surface. That is, the crystallizer copper tube is suitable for square billets, and its four sides are surrounded by a square, which can be a square. The outer wall of each side corresponding to the corner 102 protrudes from the outer wall of the face 101 to form a structure where the thickness of the corner 102 is greater than the thickness of the face 101. It can be understood that the corner 102 refers to the range of 30-50mm from the outer wall of the above-mentioned crystallizer copper tube to the top angle, and the top angle can be specifically the angle formed by two adjacent sides. Through the inclined transition, the water gap width is evenly transitioned, so that the cold distribution is more uniform, and the uniformity of the formed billet shell is better.

[0046] In some embodiments, the thickness of the corner 102 of the upper copper tube 110 gradually decreases from top to bottom. Corresponding to the upper copper tube 110, the thickness and strength of the primary blank shell gradually increase from top to bottom, and the probability of cracking at the corner gradually decreases. Therefore, the thickness of the corner 102 of the upper copper tube 110 is set to gradually decrease from top to bottom, and the cooling capacity provided is more uniform, which can not only improve the uniformity of the blank shell, but also save the material of the crystallizer copper tube and reduce the cost. In other embodiments, the thickness of the corner 102 of the upper copper tube 110 can also be equal from top to bottom, and the structure is relatively simple, which is convenient for the processing and forming of the crystallizer copper tube.

[0047] In some embodiments, the crystallizer copper tube is integrally stamped. The integral stamping is convenient to prepare, and the integral structure is high in strength. Specifically, after stamping, fine processing can be performed as needed, such as using a CNC machine tool for fine processing. In other embodiments, the corner 102 and the face 101 of the upper copper tube 110 can also be made of different materials, such as the thermal conductivity of the material of the face 101 is greater than the thermal conductivity of the material of the corner 102.

[0048] In order to achieve the above object, the present invention provides the following technical solutions:

[0049] A method for uniformly cooling a crystallizer, used for any of the above-mentioned crystallizers, comprises the following steps:

[0050] S1: Check the shell formed by the crystallizer;

[0051] S2: Take the billet shell with corner cracks or steel leakage as the test billet shell, and measure the corner thickness and face thickness of the test billet shell;

[0052] S3: Calculate the difference between the face thickness and the corner thickness of the tested blank shell, and calculate the proportional relationship between the difference and the corner thickness;

[0053] S4: According to the proportional relationship, the face thickness and corner thickness of the upper copper tube of the crystallizer are set so that the ratio of the difference between the width of the water gap corresponding to the face of the upper copper tube and the width of the water gap corresponding to the corner and the width of the water gap corresponding to the face satisfies the proportional relationship.

[0054] The blank shell formed by the existing crystallizer is inspected, and the blank shell with corner cracks or steel leakage is used as the detection blank shell, and the corner thickness and face thickness of the detection blank shell are measured, and the difference between the face thickness and the corner thickness is calculated, and the proportional relationship between the difference and the corner thickness, that is, the ratio of the two is calculated; then the face thickness and corner thickness of the upper copper tube are set according to the proportional relationship, so that the ratio of the difference between the width of the water gap corresponding to the corner of the upper copper tube and the width of the water gap corresponding to the face and the width of the water gap corresponding to the face satisfies the proportional relationship, that is, the ratio of the difference between the width of the water gap corresponding to the corner of the upper copper tube and the width of the water gap corresponding to the face and the width of the water gap corresponding to the face is equal to the ratio of the difference between the face thickness and the corner thickness of the detection blank shell and the corner thickness. Specifically, the face thickness of the blank shell is 20-30% thicker than the corner thickness of the blank shell. In order to reduce the heat transfer at the upper corner of the crystallizer, the corner water gap width of the upper crystallizer is reduced by 20-30% compared with the face water gap width, thereby reducing the cold water flow at the upper corner of the crystallizer.

[0055] The method for uniform cooling of the crystallizer provided by the present invention is applied to actually measure the billet shell that produces corner cracks or steel leakage in the crystallizer, obtain the proportional relationship between the difference between the face thickness and the corner thickness of the billet shell and the corner thickness, and set the size of the crystallizer steel tube accordingly, so that the ratio of the difference between the width of the water gap corresponding to the face of the upper copper tube and the width of the water gap corresponding to the corner and the width of the water gap corresponding to the face satisfies the above proportional relationship, thereby reducing the heat transfer at the upper corner of the crystallizer, reducing the cold water flow at the upper corner of the crystallizer, and then slowing down the solidification shrinkage of the raw billet shell at the corner of the curved liquid surface of the crystallizer copper tube, reducing the air gap between the raw billet shell and the crystallizer copper tube, thereby increasing the heat transfer efficiency of the corner below the curved liquid surface of the crystallizer, improving the billet shell thickness at the corner of the cast billet out of the crystallizer, increasing the uniformity of the billet shell of the cast billet out of the crystallizer, and effectively controlling the cracks at the corner of the cast billet and the corner crack steel leakage accidents.

[0056] In some embodiments, a blank shell with corner cracks or steel leakage is taken as a detection blank shell, and the corner thickness and face thickness of the detection blank shell are measured, specifically including: taking multiple blank shells with corner cracks or steel leakage as detection blank shells, measuring the corner thickness of each detection blank shell and taking the average value as the average corner thickness, measuring the face thickness of each detection blank shell and taking the average value as the face average thickness; calculating the difference between the face thickness and the corner thickness of the detection blank shell, and calculating the proportional relationship between the difference and the corner thickness, specifically including: calculating the difference between the face average thickness and the corner average thickness of the detection blank shell, and calculating the proportional relationship between the difference and the corner average thickness. By taking multiple blank shells with corner cracks or steel leakage as detection blank shells, measuring the corner thickness and face thickness of each detection blank shell, and then taking the average of the two and calculating the proportional relationship of the averages. Taking multiple blank shells as detection blank shells can better reflect the uneven cooling of the corners and faces, so that the corner water seam width and the face water seam width can be controlled more accurately.

[0057] In order to better illustrate the crystallizer and the method for uniform cooling thereof provided in the present application, an embodiment and a comparative example are used for comparison and explanation below.

[0058] Example 1

[0059] For the crystallizer of 160mm*160mm small square billet continuous casting machine, the water pressure of the crystallizer water is P≥0.8MPa, and the water volume of the crystallizer water ranges from 120-160m 3 / h, the pulling speed is 3.5m / min. The length of the crystallizer copper tube is 1000mm, the length of the upper copper tube is 450mm, and the length of the lower copper tube is 550mm. The face thickness of the crystallizer copper tube is 13-15mm, and the width of the face water seam that matches the cooling water jacket is 3.5±0.2mm. The corner thickness of the upper copper tube is 14-16mm, and the width of the corner water seam that matches the cooling water jacket is 2.3±0.2mm. The corner thickness of the lower copper tube is 13-15mm, and the width of the corner water seam that matches the cooling water jacket is 3.5±0.2mm. The face water seam width of the upper copper tube is 1.2mm larger than the corner water seam width, and the face water seam width of the lower copper tube is the same as the corner water seam width. The corner is the range of 40mm from the outer wall of the crystallizer copper tube to the top angle.

[0060] The face thickness of the shell formed by the above-mentioned crystallizer is 13-14 mm, the corner thickness is 13-14 mm, and the shell is uniform.

[0061] Comparative Example

[0062] For the crystallizer of the 160mm*160mm small square billet continuous casting machine, the pulling speed is 3.5m / min, and the other parameters of the crystallizer are the same as those in the above-mentioned Example 1, except that the copper tube of the crystallizer adopts a conventional design, the width of the corner water seam and the face water seam are the same, the face thickness of the crystallizer billet shell is 13-14mm, and the thickness of the corner billet shell is about 10-11mm. The corner thickness is relatively thin, and corner cracks and steel leakage are prone to occur.

[0063] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0064] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A crystallizer, characterized in that: The invention comprises a crystallizer copper tube and a cooling water jacket (200) sleeved outside the crystallizer copper tube, a water gap (300) is formed between the outer wall surface of the crystallizer copper tube and the inner wall surface of the cooling water jacket (200), the crystallizer copper tube is divided into an upper copper tube (110) and a lower copper tube (120), the upper copper tube (110) is located above the lower copper tube (120), the thickness of the face portion (101) of the upper copper tube (110) is smaller than the thickness of the corner portion (102), so that the upper copper tube (110) The width of the water gap (300) corresponding to the corner (102) of the copper tube (110) is smaller than the width of the water gap (300) corresponding to the face (101); the thickness of the face (101) of the lower copper tube (120) is equal to the thickness of the corner (102), and the thicknesses of the face (101) of the upper copper tube (110) and the lower copper tube (120) are the same; wherein the corner (102) is the range of 30-50 mm from the outer wall of the crystallizer copper tube to the top corner.

2. The crystallizer according to claim 1, characterized in that The thickness of the surface (101) of the crystallizer copper tube is in the range of 12-16 mm, and the width of the water gap (300) corresponding to the surface (101) of the crystallizer copper tube is in the range of 3.0-4.5 mm; The thickness of the corner portion (102) of the lower copper tube (120) ranges from 12 to 16 mm, and the corresponding width of the water gap (300) ranges from 3.0 to 4.5 mm.

3. The crystallizer according to claim 1, characterized in that The thickness of the corner portion (102) of the upper copper tube (110) ranges from 13 to 17 mm, and the corresponding width of the water gap (300) ranges from 2.0 to 3.5 mm.

4. The crystallizer according to claim 1, characterized in that The width of the water gap (300) corresponding to the surface (101) of the upper copper tube (110) is 1.0-1.5 mm greater than the width of the water gap (300) corresponding to the corner (102).

5. The crystallizer according to any one of claims 1 to 4, characterized in that: The length of the crystallizer copper tube ranges from 800 to 1100 mm; The upper copper tube (110) is a portion corresponding to a length range of 400-500 mm downward from the top of the crystallizer copper tube; The lower copper tube (120) is a portion corresponding to a length range of 400-600 mm upward from the bottom end of the crystallizer copper tube.

6. The crystallizer according to any one of claims 1 to 4, characterized in that: The crystallizer copper tube comprises four sides of equal length, and two adjacent sides are respectively perpendicular, the outer wall of each side corresponding to the corner (102) protrudes from the outer wall of the face (101), and the outer wall corresponding to the corner (102) and the outer wall corresponding to the face (101) are transitioned through an inclined surface.

7. The crystallizer according to claim 1, characterized in that The thickness of the corner portion (102) of the upper copper tube (110) gradually decreases from top to bottom.

8. The crystallizer according to claim 1, characterized in that The crystallizer copper tube is integrally formed by stamping.

9. A method for uniformly cooling a crystallizer, characterized in that: A crystallizer for use in any one of claims 1 to 8, comprising: Check the shell formed by the crystallizer; Taking a billet shell with corner cracks or steel leakage as a test billet shell, and measuring the corner thickness and face thickness of the test billet shell; Calculating the difference between the face thickness and the corner thickness of the test blank shell, and calculating the proportional relationship between the difference and the corner thickness; According to the proportional relationship, the face thickness and corner thickness of the upper copper tube of the crystallizer are set so that the ratio of the difference between the width of the water gap corresponding to the face of the upper copper tube and the width of the water gap corresponding to the corner to the width of the water gap corresponding to the face satisfies the proportional relationship.

10. The method for uniformly cooling a crystallizer according to claim 9, characterized in that: Take the billet shell with corner cracks or steel leakage as the test billet shell, and measure the corner thickness and face thickness of the test billet shell, including: Taking multiple blank shells with corner cracks or steel leakage as test blank shells, measuring the corner thickness of each test blank shell and taking the average value as the average corner thickness, measuring the face thickness of each test blank shell and taking the average value as the average face thickness; Calculating the difference between the face thickness and the corner thickness of the blank shell, and calculating the proportional relationship between the difference and the corner thickness, specifically includes: The difference between the average thickness of the face portion and the average thickness of the corner portion of the test blank shell is calculated, and the proportional relationship between the difference and the average thickness of the corner portion is obtained by calculation.