Treatment method of anti-static deodorant down feather
By pretreatment, grafting, and nano-carbon sol treatment, antistatic and deodorizing down fibers are formed, solving the problems of static electricity and odor in down products, improving comfort and service life, and reducing environmental impact.
Patent Information
- Application Number
- CN202411160481.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-22
AI Technical Summary
Down products are prone to static electricity and odors during use, affecting comfort and lifespan, and existing treatment methods have not been able to effectively solve these problems.
The process involves pretreatment, grafting, and nano-carbon sol treatment, including washing, glutaraldehyde grafting, and nano-carbon sol coating, to create down fibers with antistatic and deodorizing effects.
It effectively suppresses static electricity, removes odors, improves comfort and safety, extends service life, and reduces environmental impact.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of down fiber processing, and in particular relates to a processing method for antistatic and deodorizing down. Background Art
[0002] Down fiber is a natural animal protein fiber. It is light and fluffy, breathable and breathable, and has excellent warmth retention effect. It is often used in down clothing and products. During the production process, the down raw materials need to go through a series of treatments before they can be used as filling materials. The down wool materials must go through the procedures of cleaning, degreasing, deodorizing, disinfecting, and drying. If the pre-treatment process is not handled properly, it will directly affect the use effect of the down.
[0003] Since down is an animal product, it has the disadvantages of being flammable, easy to be eaten by insects, easy to breed microorganisms, low product added value, and high maintenance and washing requirements. If some processing methods can be applied to the down to maximize its strengths and avoid its weaknesses, the scope of use of down products will be greatly broadened. Existing down products have the problem that when the weather is dry, down jackets and other clothes are prone to static electricity, giving people an uncomfortable feeling, and the down itself has a certain odor. Therefore, it is necessary to find a method that can solve the above problems. Summary of the invention
[0004] The object of the present invention is to provide a method for treating antistatic and deodorizing down, which comprises the following steps: Pretreatment: First, wash the down, remove fat and impurities, then boil it in boiling water for 15 to 30 minutes, then take it out and wash it with pure water for 3 to 5 times before use; Pretreatment: The pretreated down is pretreated with a pretreatment liquid to improve the surface properties of the fiber and increase the reaction activity; Grafting treatment: In the subsequent cross-linking modification process, glutaraldehyde is first used for grafting treatment, which helps to activate the down fiber so that it can better combine with the subsequent treatment liquid; Nanocarbon sol treatment: Next, nanocarbon sol is used for treatment. The grafted activated down fibers can be firmly attached to the nanocarbon sol, introducing the advantages of nanocarbon materials to achieve a lasting modification effect; Post-treatment: The modified down fiber is further treated with post-treatment liquid, and finally has the effect of deodorization and antistatic. Final treatment: After cooling the post-treated down, wash it with pure water for 3 to 5 times, and then dry it in a dryer to obtain the finished down product.
[0005] Preferably, the pretreatment liquid comprises one or more of a surfactant, a solvent, a modifier and an activator.
[0006] Preferably, the post-treatment liquid includes one or more of an antistatic agent, a deodorant, and a softener.
[0007] Preferably, the pre-treatment comprises soaking the down fibers in a stirring tank and stirring the stirring tank at a speed of 100 to 300 r / min for 30 to 60 min, and then heating the down fibers to 70 to 80°C.
[0008] Preferably, the post-treatment is to place the down fibers in a stirring tank for soaking for 2 to 4 hours at a temperature of 50 to 70° C., during which the rotation speed of the stirring tank is 100-200 r / min.
[0009] Preferably, the drying temperature in the final treatment is 60-90° C. and the drying time is 5-10 min.
[0010] Beneficial effects: The beneficial effects of the present invention are: (1) Using deodorants in the pre-treatment and post-treatment liquids can effectively remove odors and dirt from down, keeping down products fresh; (2) Through grafting and nanocarbon sol treatment, a uniform nanocarbon sol coating is formed on the surface of the down fiber, which has good conductivity, can effectively inhibit the generation and accumulation of static electricity, and improve comfort and safety; (3) The nanocarbon sol is firmly bonded to the grafted activated down fiber and is not easily damaged by washing or wear during use, thereby extending the service life of down products; (4) The softener in the post-treatment liquid can make the down fiber soft and comfortable, improving the wearing experience; (5) Using improved processing methods, such as using environmentally friendly chemicals in pre-treatment and post-treatment, can reduce the impact on the environment and ensure the safety of down products for users’ skin; (6) By optimizing the processing steps and conditions, such as the control of stirring, heating and drying processes, production efficiency can be improved and the stability of product quality can be ensured. DETAILED DESCRIPTION
[0011] The technical solution of this patent is further described in detail below in conjunction with specific implementation methods.
[0012] Embodiment 1 The present embodiment provides a method for treating antistatic and deodorizing down, which includes the following steps: Pretreatment: First, wash the down, remove fat and impurities, and then boil it in boiling water for 15 to 30 minutes, then take it out and wash it with pure water for 3 to 5 times before use; put the down into an appropriate amount of clean water and wash it thoroughly. The purpose of washing is to remove dust and dirt on the surface of the down. After washing, use an appropriate degreasing agent solution to treat the down, mix the down and the degreasing agent solution thoroughly, and stir them at an appropriate temperature. Rinse the treated down with cold water for multiple times to thoroughly remove the residual degreasing agent and grease, and dry the down appropriately, either by air drying or low-temperature drying; Pretreatment: The pretreated down is pretreated with a pretreatment liquid to improve the surface properties of the fiber and increase the reaction activity; Grafting treatment: In the subsequent cross-linking modification process, glutaraldehyde is first used for grafting treatment, which helps to activate the down fiber and enable it to better combine with the subsequent treatment solution. Glutaraldehyde can be used as a cross-linking agent to form a cross-linking bridge on the surface of the down fiber, thereby enhancing the stability and durability of the fiber. This cross-linking effect can make the down fiber stronger and more wear-resistant, extending its service life. Glutaraldehyde grafting treatment can introduce more active functional groups to the surface of the down fiber, such as hydroxyl and formaldehyde groups. These functional groups can increase the ability of the fiber to bind to the functional substances in the subsequent treatment solution, thereby improving the effect and stability of the subsequent treatment. The surface of the down fiber after glutaraldehyde grafting treatment becomes more stable and uniform, which not only improves the tensile strength and durability of the fiber, but also increases its hygroscopicity and softness, and improves the overall quality and comfort of down products. Glutaraldehyde grafting can effectively improve the durability of down fibers and prevent them from being damaged by friction or cleaning in daily use. At the same time, it helps to keep the color and appearance of down products as new for a long time; Nanocarbon sol treatment: Next, nanocarbon sol is used for treatment. The grafted and activated down fibers can be firmly attached to the nanocarbon sol, and the advantages of nanocarbon materials are introduced to achieve a lasting modification effect. Nanocarbon sol has extremely high mechanical strength and hardness, and can enhance the strength and wear resistance of down fibers at a microscopic scale. By firmly combining with the grafted and activated fibers, nanocarbon sol can effectively improve the durability and tensile strength of down products. Nanocarbon sol can effectively inhibit the generation and accumulation of static electricity, making it less likely for down products to generate static electricity during use, thereby improving their comfort and safety of use; the surface of nanocarbon sol has a unique nanostructure that can inhibit the growth of bacteria and prevent the attachment of pollutants, thereby extending the cleaning cycle and service life of down products. As an excellent base material, nanocarbon sol can provide uniform and efficient functional coating adhesion for down fibers, ensuring the stability and durability of functional substances; Post-treatment: The modified down fiber is further treated with post-treatment liquid, and finally has the effect of deodorization and antistatic. Final treatment: After cooling the post-treated down, wash it with pure water for 3 to 5 times, and then dry it in a dryer to obtain the finished down product.
[0013] Furthermore, the pretreatment solution includes one or more of a surfactant, a solvent, a modifier and an activator.
[0014] Furthermore, the post-treatment liquid includes one or more of an antistatic agent, a deodorant, and a softener.
[0015] Furthermore, the pre-treatment is to soak the down fibers in a stirring tank and stir them at a speed of 100-300 r / min for 30-60 min, and then heat them to 70-80°C.
[0016] Furthermore, the post-treatment is to place the down fibers in a stirring tank for soaking for 2 to 4 hours at a temperature of 50 to 70° C., during which the speed of the stirring tank is 100-200 r / min.
[0017] Furthermore, the drying temperature in the final treatment is 60-90° C. and the drying time is 5-10 minutes.
[0018] In summary, the use of deodorants in the pretreatment and post-treatment liquids can effectively remove odors and dirt from down, keeping down products fresh; through grafting and nano-carbon sol treatment, a uniform nano-carbon sol coating is formed on the surface of the down fiber, which has good conductivity, can effectively inhibit the generation and accumulation of static electricity, and improve comfort and safety; the nano-carbon sol is firmly combined with the grafted and activated down fiber, and is not easily damaged by wear and tear during washing or use, thereby extending the service life of down products; the softener in the post-treatment liquid can make the down fiber soft and comfortable, improving the wearing experience; the use of improved treatment methods, such as the use of environmentally friendly chemicals in pre-treatment and post-treatment, can reduce the impact on the environment and ensure the safety of down products to the user's skin; by optimizing the treatment steps and conditions, such as the control of stirring, heating and drying processes, the production efficiency can be improved and the stability of product quality can be ensured.
[0019] The embodiments described above are preferred embodiments of the present invention, rather than all embodiments. The detailed description of the embodiments of the present invention is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
Claims
1. A method for treating antistatic and deodorizing down, characterized in that: The following steps are involved: Pretreatment: First, wash the down, remove fat and impurities, then boil it in boiling water for 15 to 30 minutes, then take it out and wash it with pure water for 3 to 5 times before use; Pretreatment: pretreating the down with a pretreatment liquid to improve the surface properties of the fiber and increase the reaction activity; Grafting treatment: In the subsequent cross-linking modification process, glutaraldehyde is first used for grafting treatment, which helps to activate the down fiber so that it can better combine with the subsequent treatment liquid; Nano-carbon sol treatment: Then, nano-carbon sol is used for treatment. The grafted activated down fibers can be firmly attached to the nano-carbon sol, introducing the advantages of nano-carbon materials to achieve a lasting modification effect; Post-treatment: The modified down fiber is further treated with post-treatment liquid, and finally obtains the deodorizing and antistatic effects; Final treatment: After cooling the post-treated down, wash it with pure water for 3 to 5 times, and then dry it in a dryer to obtain the finished down product.
2. The method for treating antistatic and deodorizing down according to claim 1, characterized in that: The pretreatment liquid includes one or more of a surfactant, a solvent, a modifier and an activator.
3. The method for treating antistatic and deodorizing down according to claim 1, characterized in that: The post-treatment liquid includes one or more of an electrostatic agent, a deodorant, and a softener.
4. The method for treating antistatic and deodorizing down according to claim 1, characterized in that: The pre-treatment comprises soaking the down fibers in a stirring tank and stirring the stirring tank at a speed of 100 to 300 r / min for 30 to 60 minutes, and then heating the mixture to 70 to 80°C.
5. The method for treating antistatic and deodorizing down according to claim 1, characterized in that: The post-treatment is to put the down fibers into a stirring tank for soaking for 2 to 4 hours at a temperature of 50 to 70° C., during which the rotating speed of the stirring tank is 100 to 200 r / min.
6. The method for treating antistatic and deodorizing down according to claim 1, characterized in that: The drying temperature in the final treatment is 60-90° C. and the drying time is 5-10 minutes.