Method and equipment for improving wafer surface reaction uniformity
By monitoring and adjusting the annular reaction rate abnormal belt driven by the rotation of the showerhead, the problem of uneven wafer surface reaction rate caused by the showerhead defect is solved, and the wafer surface reaction uniformity is achieved under the use of defective showerheads. Improved performance reduces costs and improves the performance of semiconductor devices.
Patent Information
- Application Number
- CN202411105834.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-13
- Publication Date
- 2024-11-22
AI Technical Summary
During semiconductor manufacturing, due to the quality defect of the showerhead, abnormal points appear on the surface of the wafer surface, which affects the reaction uniformity, and the cost of replacing the showerhead is high. How to lift the wafer while using a defective showerhead Surface reaction uniformity is an important issue.
By monitoring the reaction rate of the wafer surface, using the drive member to drive the spray head to rotate, the reaction rate abnormal points form an annular rate abnormal band, and generate a reaction rate distribution map, adjust the process to make the reaction rate distribution flat, forming a comprehensive reaction Rate distribution map, cycle adjustment until the reaction rate distribution further flattens.
When using defective spray heads, the reaction uniformity of the wafer surface is effectively improved, the impact of abnormal points is reduced, the performance and reliability of semiconductor devices are improved, and the frequency and cost of replacing the spray head is reduced.
Smart Images

Figure CN119008466A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the field of semiconductor processing technology, and in particular to a method and device for improving the uniformity of wafer surface reaction. Background Art
[0002] In the semiconductor manufacturing process, the shower head is a key process component in the reaction chamber, and its performance directly affects the processing effect of the wafer surface. In existing equipment, due to the inadequacy of the processing process, the limitation of processing accuracy, and the influence of thermal stress in the high-temperature reaction environment, the shower head is prone to various quality defects, such as dimensional deviation, insufficient surface roughness, and local deformation.
[0003] When there are these defects in the shower head, the spraying effect near the defective location will be affected, resulting in abnormalities in the reaction rate of the wafer surface in the corresponding area. These abnormalities will further destroy the reaction uniformity of the wafer surface, thereby affecting the performance of semiconductor devices. However, considering the high difficulty of processing a perfect shower head, the cost of frequently replacing the shower head is high. Therefore, how to improve the reaction uniformity of the wafer surface when using a defective shower head is still an important issue. Summary of the invention
[0004] The purpose of the embodiments of the present application is to provide a method and device for improving the reaction uniformity of a wafer surface, which can improve the reaction uniformity of a wafer surface when a defective shower head is used.
[0005] To solve the above technical problems, the embodiments of the present application provide a method and device for improving the uniformity of wafer surface reaction, the method comprising: continuously monitoring the reaction rate of the wafer surface through a measuring device; controlling a driving member to drive a shower head to rotate; monitoring the reaction rate abnormal points on the wafer surface after the shower head rotates to form an annular rate abnormality band symmetrically distributed along the axis of the wafer, and generating a first reaction rate distribution diagram; determining the position and characteristics of the annular rate abnormality band according to the first reaction rate distribution diagram; adjusting the process program to make the reaction rate distribution on the wafer surface tend to be flat; adjusting the process program to make the reaction rate distribution on the wafer surface tend to be flat, including: adjusting the process program according to the first reaction rate distribution diagram to form a second reaction rate distribution diagram with a trend opposite to that of the annular rate abnormality band in the first reaction rate distribution diagram; numerically adding and averaging the first reaction rate distribution diagram and the second reaction rate distribution diagram to form a comprehensive reaction rate distribution diagram, so that the reaction rate distribution on the wafer surface tends to be flat.
[0006] In some embodiments, after the comprehensive reaction rate distribution graph is formed, the method further includes: cyclically adjusting the process formula until the comprehensive reaction rate distribution graph shows that the reaction rate distribution on the wafer surface further tends to be flat.
[0007] In some embodiments, the process recipe includes the flow rate of the reaction gas, the ratio of the reaction gas, the pressure of the reaction gas, the rotation speed of the showerhead, and the temperature of the reaction chamber.
[0008] In some embodiments, after adjusting the process program to make the reaction rate distribution on the wafer surface tend to be flat, it also includes continuing to monitor the reaction rate of the annular abnormal band formed on the wafer surface after adjusting the process program. If the value of the reaction rate of the annular abnormal band formed on the wafer surface after adjusting the process program is within a preset range, entering the formal process stage; if the value is not within the preset range, repeatedly adjusting the process program according to the result.
[0009] An embodiment of the present application also provides a device for improving the uniformity of wafer surface reaction, the device comprising: a cavity body, having a reaction chamber, in which a shower head and a wafer carrier are arranged; a driving member, and a controller connected to the driving member, the driving member comprising a shell and an output shaft, the output shaft drives the shower head to rotate, the controller is used to adjust the rotation speed and rotation direction of the driving member, the output shaft is provided with a first gear, the shower head is provided with a second gear, and the driving member drives the shower head to rotate through the meshing of the first gear and the second gear.
[0010] In some embodiments, the showerhead includes a showerhead body and a showerhead extension, and the second gear is disposed on the showerhead extension.
[0011] In some embodiments, the housing is mounted on an outer wall of an upper top plate of the cavity, and the output shaft is connected to the shower head extension portion through the upper top plate.
[0012] In some embodiments, the device for improving the uniformity of wafer surface reaction is further provided with a support member, which is arranged around the shower head in the reaction chamber and connected to the upper top plate, the support member is provided with a first guide rail, the shower head extension portion is provided with a second guide rail, the first guide rail overlaps with the second guide rail, and a rolling member is provided between the first guide rail and the second guide rail.
[0013] The embodiment of the present application provides a method and device for improving the reaction uniformity of the wafer surface, which uses a driving gear to drive the shower head to rotate in the reaction chamber, so that the reaction rate abnormal points that may be generated on the wafer surface form an annular rate abnormal band, and then the annular rate abnormal band is eliminated by adjusting the process program multiple times. In this way, the reaction uniformity of the wafer surface can be improved when using a defective shower head. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] One or more embodiments are exemplarily described by the corresponding pictures in the accompanying drawings, which do not constitute limitations on the embodiments. Elements with the same reference numerals in the drawings represent similar elements, and unless otherwise stated, the figures in the drawings do not constitute proportional limitations.
[0015] Figure 1 is a flow chart of a method for automatically adjusting uniformity of a semiconductor processing process provided by some embodiments of the present application;
[0016] Figure 2 It is a schematic diagram of a method for improving wafer surface reaction uniformity provided by some embodiments of the present application, in which a reaction rate abnormal point is rotated by a shower head to form a ring-shaped rate abnormal zone;
[0017] Figure 3 It is a curve diagram of the reaction rate of the abnormal point of the reaction rate before the shower head rotates in the method for improving the uniformity of the reaction on the wafer surface provided by some embodiments of the present application;
[0018] Figure 4 is a first reaction rate distribution diagram provided by some embodiments of the present application;
[0019] Figure 5 is a second reaction rate distribution diagram provided by some embodiments of the present application;
[0020] Figure 6 is a comprehensive reaction rate distribution diagram provided by some embodiments of the present application;
[0021] Figure 7 It is a schematic diagram of the overall structure of an apparatus for improving wafer surface reaction uniformity provided in some embodiments of the present application;
[0022] Figure 8 is a partial structural schematic diagram of a first guide rail and a second guide rail provided in some embodiments of the present application;
[0023] Fig. 9 It is a curve diagram of the reaction rate at an abnormal point of the reaction rate before the shower head rotates in another method for improving the uniformity of the reaction on the wafer surface provided by some embodiments of the present application;
[0024] Fig.10 is another first reaction rate distribution diagram provided by some embodiments of the present application;
[0025] Fig.11 is another second reaction rate distribution diagram provided by some embodiments of the present application;
[0026] Fig.12 is another comprehensive reaction rate distribution diagram provided by some embodiments of the present application;
[0027] Fig.13 It is a curve diagram of the reaction rate at an abnormal point of the reaction rate before the shower head rotates in another method for improving the uniformity of the reaction on the wafer surface provided by some embodiments of the present application;
[0028] Fig.14is another first reaction rate distribution diagram provided by some embodiments of the present application;
[0029] Fig.15 is another second reaction rate distribution diagram provided by some embodiments of the present application;
[0030] Fig.16 This is another comprehensive reaction rate distribution diagram provided by some embodiments of the present application. DETAILED DESCRIPTION
[0031] To make the purpose, technical scheme and advantages of the embodiments of the present application clearer, each embodiment of the present application will be described in detail below in conjunction with the accompanying drawings. However, it will be appreciated by those skilled in the art that in each embodiment of the present application, many technical details are proposed in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can also be implemented. The division of the following embodiments is for the convenience of description, and the specific implementation of the present application should not constitute any limitation, and the various embodiments can be combined with each other and referenced to each other without contradiction.
[0032] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by technicians in the technical field to which this application belongs; the terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" in the specification and claims of this application and the above-mentioned figure descriptions and any variations thereof are intended to cover non-exclusive inclusions.
[0033] In the description of the embodiments of the present application, the technical terms "first", "second", etc. are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of the embodiments of the present application, the meaning of "multiple" is more than two, unless otherwise clearly and specifically defined.
[0034] In the description of the embodiments of the present application, the term "and / or" is only a description of the association relationship of the associated objects, indicating that there may be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0035] In the semiconductor equipment processing, wafer surface uniformity is critical and directly related to the quality, performance and reliability of the final product. The reaction rate in the semiconductor manufacturing process directly determines the rate of material conversion, deposition or etching in different areas on the wafer surface. Therefore, any abnormal reaction rate point may have a negative impact on the reaction uniformity of the wafer surface.
[0036] As a key component in semiconductor manufacturing, the performance of the showerhead directly affects the distribution of reactive gases and the reaction rate. However, due to inadequate processing, limited processing accuracy, and the influence of thermal stress during high-temperature reactions, the showerhead may have quality defects such as dimensional deviation, substandard surface roughness, or local deformation. These defects will cause the reactive gas to be unevenly distributed on the wafer surface, resulting in abnormal reaction rate points in specific areas. The reaction rate at these abnormal points may be too fast or too slow compared to other areas, resulting in inconsistent material conversion or etching levels in different areas of the wafer surface. This inconsistency will destroy the reaction uniformity of the wafer surface, which may manifest as changes in wafer surface thickness, distortion of patterns, or an increase in defects. These inhomogeneities will directly affect the performance and reliability of semiconductor devices.
[0037] To this end, some embodiments of the present application provide a method for automatically adjusting the uniformity of semiconductor processing technology, which uses a driving gear to drive the shower head to rotate in the reaction chamber, so that the abnormal reaction rate points that may be generated on the wafer surface form an annular rate abnormality band, and then the annular rate abnormality band is eliminated by adjusting the process program multiple times. In this way, the reaction uniformity of the wafer surface can be improved when using a defective shower head.
[0038] Combine the following Figure 1 , illustrating a method for improving wafer surface reaction uniformity provided by some embodiments of the present application.
[0039] like Figure 1 As shown, some embodiments of the present application provide a method for improving the uniformity of wafer surface reaction, the method comprising:
[0040] S1: Continuously monitor the reaction rate on the surface of the wafer 13 by using a measurement device.
[0041] A measuring device is prepared and connected to the device for improving the uniformity of the wafer surface reaction to continuously monitor the film thickness change on the surface of the wafer 13, thereby characterizing the reaction rate and the uniformity of the reaction. During the monitoring process, the measuring device transmits the measurement data to the data processing system in real time for processing and analysis.
[0042] The reaction rate refers to the speed of a physical or chemical reaction occurring on the surface of the wafer 13 within a certain period of time, and is usually expressed as a film deposition thickness or etching depth per unit time. During the monitoring process, the measurement equipment can identify abnormal points in the reaction rate on the surface of the wafer 13, that is, points where the reaction rate is significantly higher or lower than the normal value.
[0043] S2: Control the driving member 20 to drive the sprinkler head to rotate.
[0044] The controller is responsible for sending precise instructions to the driver 20 to control the rotation of the shower head so that the abnormal reaction rate point originally appearing at one point on the surface of the wafer 13 is evenly distributed, and the reaction uniformity is greatly improved. The controller can adjust the rotation speed of the shower head according to the process requirements.
[0045] S3: monitoring the reaction rate abnormal points on the surface of the wafer 13 after the shower head rotates to form an annular rate abnormal zone 31 symmetrically distributed along the axis of the wafer 13, and generating a first reaction rate distribution diagram.
[0046] The measuring equipment can detect that the reaction rate anomaly points on the surface of the wafer 13 form a ring structure symmetrically distributed along the axis of the wafer 13 after the rotation of the shower head, that is, the annular rate anomaly band 31. The position, shape, size and other characteristics of the annular rate anomaly band 31 are recorded, and a first reaction rate distribution map is generated. The first reaction rate distribution map is based on the surface of the wafer 13, and the reaction rates of various areas can be marked with different colors or values, so as to intuitively display the position and range of the annular rate anomaly band 31.
[0047] Figure 2 It shows that after the shower head rotates, the reaction rate anomaly point on the surface of the wafer 13 changes from the original island-shaped reaction rate anomaly point 30 to the annular rate anomaly band 31. A straight line X in any direction passing through the center point of the wafer 13 and the island-shaped reaction rate anomaly point 30 is selected, and the reaction rate distribution from the center to the edge of the wafer 13 can be observed through the straight line X. Corresponding to the first reaction rate distribution diagram, the straight line is represented as the X-axis, and the Y-axis represents the value of the reaction rate, which intuitively shows the strength of the reaction rate at different positions, thereby identifying the impact of the reaction rate anomaly point or the annular rate anomaly band 31 on the overall reaction rate.
[0048] Figure 3 It is a curve diagram of the reaction rate of the abnormal reaction rate point before the sprinkler head rotates, indicating the abnormal reaction rate deviation Δ1 of the abnormal reaction rate point. This curve can help quickly identify the positions where the reaction rate is significantly different from the normal rate.
[0049] S4: Determine the position and characteristics of the annular rate anomaly zone 31 according to the first reaction rate distribution diagram.
[0050] Figure 4 It is a first reaction rate distribution diagram, which is a curve schematic diagram showing the reaction rate deviation Δ2 of the annular rate abnormal band 31. Δ2 is less than Δ1, and the curve of Δ2 intuitively shows the difference between the reaction rate in the annular rate abnormal band 31 and the normal reaction rate. Through this curve, the influence of the annular rate abnormal band 31 on the overall reaction rate can be understood, and the process parameters can be adjusted accordingly to reduce or eliminate the influence of the abnormal band.
[0051] like Figure 4 As shown, the characteristic of the annular rate anomaly band 31 is two symmetrical rate peaks or valleys, which may not be completely symmetrical, but should have similar amplitudes and shapes. The position of the annular rate anomaly band 31 can be determined by the coordinates on the x-axis. The curve of Δ2 is relatively gentle relative to the curve of Δ1, indicating that when the annular rate anomaly band 31 exists on the surface of the wafer 13, the change in its reaction rate is more uniform than that on the surface of the wafer 13 where there is a reaction rate anomaly point.
[0052] S5: According to the first reaction rate distribution diagram, the process formula is adjusted to form a second reaction rate distribution diagram having a trend opposite to that of the annular rate anomaly band 31 in the first reaction rate distribution diagram.
[0053] After determining the position and characteristics of the annular rate anomaly band 31, the process formula can be adjusted based on the analysis of the first reaction rate distribution diagram to eliminate or balance the annular rate anomaly band 31 on the surface of the wafer 13. The adjustment may involve changing the ratio, flow rate, pressure, temperature and other parameters of the reaction gas. The goal of adjusting the process formula is to make the reaction rate X-direction distribution in the ideal case without reaction rate anomaly opposite to the annular rate anomaly band 31 in the first reaction rate distribution diagram, such as Figure 5 As shown, a second reaction rate distribution diagram is formed, which is opposite to the trend of the annular rate anomaly band 31 in the first reaction rate distribution diagram. For example, when preparing SiO2 thin film by pecvd, the ratio of SiH4 to N2O, flow rate, reaction pressure, and the gap between the wafer and the shower head can be adjusted to adjust the second rate distribution diagram.
[0054] By continuously adjusting and optimizing the process parameters, the influence of the abnormal band is gradually reduced until the reaction rate distribution on the surface of the wafer 13 tends to be flat. Such adjustment can not only improve product quality, but also help to improve production efficiency and reduce costs.
[0055] S6: performing numerical addition and averaging on the first reaction rate distribution map and the second reaction rate distribution map to form a comprehensive reaction rate distribution map, so that the reaction rate distribution on the wafer surface tends to be flat.
[0056] After obtaining the second reaction rate distribution graph, it is numerically averaged with the first reaction rate distribution graph. This process is achieved by adding the corresponding data points on the two distribution graphs. By adding and averaging, it is possible to observe the changes in the reaction rate distribution after adjusting the process formula and whether the expected effect has been achieved. Figure 6 is an example of a comprehensive reaction rate distribution graph, where the reaction rate distribution curve is roughly flat.
[0057] Some embodiments of the present application provide a method for automatically adjusting uniformity of semiconductor processing technology, which uses a driving gear to drive a shower head to rotate in a reaction chamber, so that the abnormal reaction rate points that may be generated on the surface of the wafer form an annular abnormal rate band 31, and then eliminate the annular abnormal rate band 31 by adjusting the process program multiple times. In this way, the reaction uniformity of the wafer surface can be improved when a defective shower head is used.
[0058] In some embodiments, after the comprehensive reaction rate distribution graph is formed, the process further includes: cyclically adjusting the process formula until the comprehensive reaction rate distribution graph shows that the reaction rate distribution on the wafer surface further tends to be flat.
[0059] According to the comprehensive reaction rate distribution diagram after addition and averaging, it can be judged whether the reaction rate distribution on the surface of the wafer 13 has reached a flat state. If there is still an obvious annular rate anomaly band 31 or the reaction rate distribution is uneven, then it is necessary to continue to adjust the process program. This process may require multiple iterations until the comprehensive reaction rate distribution diagram shows that the reaction rate distribution on the surface of the wafer 13 has reached the expected flatness. In actual situations, it can be judged whether the reaction rate distribution on the surface of the wafer 13 has reached the expected flatness based on the reaction uniformity of the wafer surface. In other words, it can be judged whether it is necessary to continue iterating by presetting a standard for a uniformity value. Reaction uniformity refers to the consistency of the reaction rate on the entire surface of the wafer 13. The numerical value of reaction uniformity is generally expressed as a uniformity percentage (U%), and the formula is:
[0060]
[0061] Where R max is the maximum reaction rate, R min is the minimum reaction rate, R mean is the average reaction rate.
[0062] In some embodiments, the process recipe includes the flow rate of the reaction gas, the ratio of the reaction gas, the pressure of the reaction gas, the rotation speed of the showerhead, and the temperature of the reaction chamber 10 .
[0063] By adjusting the process formula, the reaction rate distribution of different areas at the edge and center of the surface of the wafer 13 can be adjusted. For example, by adjusting the flow rate of a specific gas and the pressure of the reaction gas, the reaction rate of different areas on the surface of the wafer 13 can be changed. The rotation speed of the shower head determines the uniformity of the distribution of the reaction gas on the surface of the wafer 13. If the rotation speed of the shower head is too slow, uneven gas distribution may result. By adjusting the rotation speed of the shower head, the uniformity of the gas distribution can be improved, thereby reducing the impact of the abnormal band.
[0064] In some embodiments, after adjusting the process formula to make the reaction rates on the surface of the wafer 13 tend to be flat, it also includes monitoring the comprehensive reaction rate distribution diagram. If the value of the annular rate anomaly band 31 is within the preset range, the formal process stage is entered; if the value of the annular rate anomaly band 31 is not within the preset range, the process formula is repeatedly adjusted according to the result.
[0065] After the process program adjustment is completed, the measurement equipment can be used to monitor the comprehensive reaction rate distribution diagram on the surface of the wafer 13. If the value of the annular rate anomaly band 31 is within the preset range, it means that the reaction rate distribution on the surface of the wafer 13 has become flat and has reached the expected uniformity. At this time, the formal process stage can be entered to carry out the subsequent wafer 13 production process. If the value of the annular rate anomaly band 31 is not within the preset range, it means that the current process adjustment has not eliminated the influence of the annular rate anomaly band 31. It is necessary to readjust the process program according to the monitoring results, and then monitor again until the value of the annular rate anomaly band 31 reaches the preset range.
[0066] Some embodiments of the present application also provide a device for improving the uniformity of wafer surface reaction, which is used to implement the above-mentioned method for improving the surface uniformity of wafer 13.
[0067] The device for improving the uniformity of wafer surface reaction includes: a cavity 100, which has a reaction chamber 10, in which a shower head and a wafer carrier 12 are arranged; a driving member 20, and a controller connected to the driving member 20, wherein the driving member 20 includes a shell and an output shaft, and the output shaft drives the shower head to rotate, and the controller is used to adjust the rotation speed and rotation direction of the driving member 20, the output shaft is provided with a first gear, and the shower head is provided with a second gear, and the driving member 20 drives the shower head to rotate through the meshing of the first gear and the second gear.
[0068] The shower head is located in the reaction chamber 10, and is used to spray the reaction gas evenly onto the surface of the wafer 13. The wafer carrier 12 is also located in the reaction chamber 10, and is used to carry the wafer 13 to be processed. The driving member 20 includes a housing and an output shaft, and a first gear may be provided on the output shaft, and the shower head may be provided with a second gear that matches the first gear. When the driving member 20 is working, the driving member 20 can drive the shower head to rotate through the engagement of the first gear and the second gear. In addition, the controller connected to the driving member 20 can be responsible for adjusting the rotation speed and rotation direction of the driving member 20 to ensure that the shower head rotates according to a preset trajectory and speed.
[0069] During the operation of the device, the wafer 13 can be placed on the wafer carrier 12, and the reaction gas can be sprayed onto the surface of the wafer 13 through the shower head. At the same time, the driving member 20 can drive the shower head to rotate under the regulation of the controller. By accurately controlling the rotation speed of the shower head, the device can make the reaction rate abnormal point on the surface of the wafer 13 form a ring-shaped rate abnormal zone 31.
[0070] In some embodiments, a device for improving wafer surface reaction uniformity further includes: the shower head includes a shower head body 11 and a shower head extension portion 14 , and the second gear is disposed on the shower head extension portion 14 .
[0071] In addition, the housing may be mounted on the outer wall of the upper plate of the chamber 100 , and the output shaft is connected to the shower head extension portion 14 through the upper plate.
[0072] The shower head is located in the reaction chamber 10, and includes a shower head body 11 and a shower head extension 14. The shower head body 11 is used to spray the reaction gas evenly onto the surface of the wafer 13, and the shower head extension 14 is used to connect with the output shaft of the driving member 20 to realize the rotation of the shower head. The housing of the driving member 20 can be installed on the outer wall of the upper top plate of the chamber 100, and the output shaft can be connected to the shower head extension 14 through the upper top plate, and a first gear is provided at the end thereof, which is meshed with the second gear of the shower head extension 14, and the shower head is driven to rotate through gear transmission.
[0073] In some embodiments, the device for improving the uniformity of wafer surface reaction may also be provided with a support member 15. The support member 15 may be arranged around the shower head in the reaction chamber 10 and connected to the upper top plate. The support member 15 may be provided with a first guide rail, and the shower head extension portion 14 may be provided with a second guide rail. The first guide rail overlaps with the second guide rail, and a rolling member 16 is provided between the first guide rail and the second guide rail.
[0074] The support member 15 can be disposed around the shower head in the reaction chamber 10 and connected to the upper top plate to provide additional support for the shower head, making the shower head more stable during operation, reducing displacement or deflection caused by vibration or external force, and ensuring the precise position of the shower head.
[0075] The first guide rail provided on the support member 15 overlaps with the second guide rail of the shower head extension 14, providing precise guidance for the shower head so that the shower head can move along a preset track when rotating or moving.
[0076] like Figure 8 As shown, a rolling element 16 may be provided between the first guide rail and the second guide rail. The rolling element 16 includes but is not limited to a ball or a roller.
[0077] The rolling element 16 is arranged between the first guide rail and the second guide rail, which can improve the stability and accuracy of the rotation of the shower head. The rolling element 16 can also reduce the friction between the guide rails, ensuring that the shower head can rotate smoothly, thereby improving the reaction uniformity.
[0078] In actual situations, abnormal points on the wafer surface may be randomly distributed in different areas. The following experiment uses methods and equipment to improve the uniformity of wafer surface reactions, and selects eight-inch wafers as experimental objects. The qualified standard for wafer surface uniformity is preset to 2%.
[0079] Figure 3 The reaction rate distribution diagram is shown when the abnormal point is close to the central area, and the wafer surface uniformity is 11.6%. The control drive 20 drives the shower head to rotate to form Figure 4 The first reaction rate distribution diagram shown in FIG. 1 shows that the wafer surface uniformity is 2.4%. According to the first reaction rate distribution diagram, the process formula is adjusted, such as Figure 5 As shown in FIG. 1 , a second reaction rate distribution diagram is formed which has a trend opposite to that of the annular rate anomaly band 31 in the first reaction rate distribution diagram. Then, the first reaction rate distribution diagram and the second reaction rate distribution diagram are numerically averaged to form the following diagram: Figure 6 As shown in the comprehensive reaction rate distribution diagram, the wafer surface uniformity is further reduced to 1.5%, which meets the preset standard, and its reaction rate distribution curve is roughly flat.
[0080] Fig. 9 The reaction rate distribution diagram with the abnormal point between the center and the edge is shown, and the wafer surface uniformity is 11.5%. The control drive 20 drives the shower head to rotate to form Fig.10 The first reaction rate distribution diagram shown in FIG. 1 shows that the wafer surface uniformity is 2.1%. According to the first reaction rate distribution diagram, the process formula is adjusted, such as Fig.11 As shown in FIG. 1 , a second reaction rate distribution diagram is formed which has a trend opposite to that of the annular rate anomaly band 31 in the first reaction rate distribution diagram. Then, the first reaction rate distribution diagram and the second reaction rate distribution diagram are numerically averaged to form the following diagram: Fig.12As shown in the comprehensive reaction rate distribution diagram, the wafer surface uniformity is further reduced to 1.6%, which meets the preset standard, and its reaction rate distribution curve is roughly flat.
[0081] Fig.13 The reaction rate distribution diagram when the abnormal point is close to the edge area is shown, and the wafer surface uniformity is 11.7%. The control drive 20 drives the shower head to rotate to form Fig.14 The first reaction rate distribution diagram shown in FIG. 1 shows that the wafer surface uniformity is 2%. According to the first reaction rate distribution diagram, the process formula is adjusted, such as Fig.15 As shown in FIG. 1 , a second reaction rate distribution diagram is formed which has a trend opposite to that of the annular rate anomaly band 31 in the first reaction rate distribution diagram. Then, the first reaction rate distribution diagram and the second reaction rate distribution diagram are numerically averaged to form the following diagram: Fig.16 As shown in the comprehensive reaction rate distribution diagram, the wafer surface uniformity is further reduced to 1.4%, which meets the preset standard, and its reaction rate distribution curve is roughly flat.
[0082] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0083] Those skilled in the art will appreciate that the above-mentioned embodiments are specific examples for implementing the present application, and in actual applications, various changes may be made thereto in form and detail without departing from the spirit and scope of the present application.
Claims
1. A method for improving the uniformity of wafer surface reaction, characterized in that: include: Continuously monitoring the reaction rate on the surface of the wafer by a measurement device; The control driving member drives the sprinkler head to rotate; Monitoring the reaction rate abnormal points on the surface of the wafer, which are formed by the rotation of the shower head and are symmetrically distributed along the axis of the wafer, to generate a first reaction rate distribution diagram; Determining the position and characteristics of the annular rate anomaly zone according to the first reaction rate distribution map; According to the first reaction rate distribution diagram, adjusting the process formula to form a second reaction rate distribution diagram which has a trend opposite to that of the annular rate anomaly band in the first reaction rate distribution diagram; The first reaction rate distribution map and the second reaction rate distribution map are numerically added and averaged to form a comprehensive reaction rate distribution map, so that the reaction rate distribution on the surface of the wafer tends to be flat.
2. A method for improving wafer surface reaction uniformity according to claim 1, characterized in that: After the comprehensive reaction rate distribution graph is formed, the method further includes: cyclically adjusting the process formula until the comprehensive reaction rate distribution graph shows that the reaction rate distribution on the surface of the wafer is further flattened.
3. A method for improving wafer surface reaction uniformity according to claim 2, characterized in that: The process formula includes the flow rate of the reaction gas, the ratio of the reaction gas, the pressure of the reaction gas, the rotation speed of the shower head and the temperature of the reaction chamber.
4. A method for improving wafer surface reaction uniformity according to claim 3, characterized in that: After the reaction rate distribution on the wafer surface is made flat by adjusting the process program, the method further includes continuing to monitor the reaction rate of the annular abnormal band formed on the wafer surface after the process program is adjusted. If the reaction rate value of the annular abnormal band formed on the wafer surface after the process program is adjusted is within a preset range, the formal process stage is entered; If the value is not within the preset range, the process is repeatedly adjusted according to the result.
5. A device for improving wafer surface reaction uniformity, used to implement a method for improving wafer surface reaction uniformity as claimed in any one of claims 1 to 4, characterized in that: include: A cavity body, comprising the reaction chamber, wherein the shower head and the wafer carrier are arranged; A driving member, and a controller connected to the driving member, the driving member includes a shell and an output shaft, the output shaft drives the spray head to rotate, the controller is used to adjust the rotation speed and rotation direction of the driving member, the output shaft is provided with a first gear, the spray head is provided with a second gear, and the driving member drives the spray head to rotate through the engagement of the first gear and the second gear.
6. The device for improving wafer surface reaction uniformity according to claim 5, characterized in that: The shower head comprises a shower head body and a shower head extension portion, and the second gear is arranged on the shower head extension portion.
7. The device for improving wafer surface reaction uniformity according to claim 6, characterized in that: The shell is mounted on the outer wall of the upper top plate of the cavity, and the output shaft is connected to the shower head extension portion through the upper top plate.
8. The device for improving wafer surface reaction uniformity according to claim 7, characterized in that: A support member is also provided, which is arranged around the shower head in the reaction chamber and connected to the upper top plate. The support member is provided with a first guide rail, and the shower head extension portion is provided with a second guide rail. The first guide rail coincides with the second guide rail, and a rolling member is provided between the first guide rail and the second guide rail.
Citation Information
Patent Citations
Database for etching rate distribution curves of layer to be etched, and forming and using methods
CN102456078A
Wafer treatment device and method
CN113725061A
Thin film deposition method and equipment
CN114150287A