Method for integrating copper-graphene stack (CGL) in multi-layer PCB manufacturing process
By applying a protective layer on the laminated stack of the printed circuit board and removing it at appropriate temperature, the problem of graphene damage during drilling and plating is solved, improving the conductivity of copper and the high-frequency performance of the PCB.
Patent Information
- Application Number
- CN202410632035.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-22
- Filing Date
- 2024-05-21
- Publication Date
- 2024-11-22
AI Technical Summary
When graphene is integrated into printed circuit boards (PCBs), graphene is prone to damage, resulting in inappropriate passivation of copper and low conductivity, and it is difficult to maintain graphene integrity during drilling and plating.
The protective layer is applied on the surface of the laminated stacked material, and the protective layer is heat-applied and removed to prevent the metal plating from contacting the graphene layer directly, ensuring that the graphene is not damaged during drilling and electroplating, and the protective layer is removed at a predetermined temperature. To remove the metal coating.
Effectively protect the graphene layer from damage, maintain its integrity, ensure the conductivity of copper and the performance of PCB, and achieve the improvement of high-frequency conductivity and thermal management capabilities.
Smart Images

Figure CN119012567A_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention generally relate to printed circuit board (PCB) structures and methods for integrating copper-graphene in PCB structures. Background Art
[0002] A PCB is a laminated structure of conductive and insulating layers that are used to support electronic components and to provide electrical connections and open circuits between electrical terminals. Typically, each of the conductive layers includes a pattern of electrical paths or traces that provide electrical connections on the conductive layers. In addition, vias or plated-through holes may be provided to allow electrical interconnection between different conductive layers.
[0003] Graphene is known to have several beneficial properties that, when incorporated into a PCB, can, among other things, passivate copper metal lines and improve high frequency conductivity. Incorporating graphene into a PCB can be difficult because graphene is easily damaged or destroyed, for example, during a lamination process, photolithography, drilling process, and / or plating process. Such damage or destruction can, in turn, result in improper passivation of copper and / or lower conductivity. Thus, there are problems in incorporating graphene into a PCB and maintaining the integrity of the graphene. Summary of the invention
[0004] Embodiments of the present invention provide improved methods of creating PCBs that integrate graphene as a passivation layer on copper and allow drilling and plating without damaging or inadvertently removing portions of the graphene, which could render the PCB useless (e.g., could remove the copper cover and render the PCB susceptible to oxidation and rapid degradation), and related methods for forming a lamination stack including the graphene.
[0005] In some embodiments, a method of forming a laminate stack includes: providing a core; applying a first graphene layer to a surface portion of the core; applying a metal layer to the first graphene layer; applying a second graphene layer to the metal layer; applying a photoresist layer to the second graphene layer; applying a protective layer to the photoresist layer; drilling through the protective layer and at least one of the photoresist layer, the second graphene layer, the metal layer, the first graphene layer or the core; applying a metal coating to the laminate stack, wherein the metal coating is applied to the laminate stack so that the metal coating covers an inner surface of the laminate stack formed by the drilling; and removing the protective layer from the photoresist layer, wherein the removal of the protective layer results in the removal of the metal coating in contact with the protective layer.
[0006] In some embodiments, the metal plating is a material including at least one of palladium, tin, or copper.
[0007] In some embodiments, removing the protective layer comprises applying heat to the laminate stack at a predetermined temperature, wherein the temperature is based on the protective layer. In some embodiments, the temperature is in a range of about 90 degrees Celsius to about 180 degrees Celsius.
[0008] In some embodiments, the protective layer is a material that includes resilience to at least one, two, three, four, eleven, twelve, thirteen, or fourteen hydrogen scores.
[0009] In some embodiments, the protective layer is a material comprising at least one of polymethyl methacrylate (PMMA), polydimethyloxyaniline (PDMA), polyethylene vinyl acetate, a water-insoluble film polymer, polyetherimide, a thermoplastic polymer, or an elastomeric polymer.
[0010] In some embodiments, the protective layer includes at least one of an adhesive tape, a thermal release tape, a dry film photoresist, an atomic deposition layer, or a photoresist.
[0011] In some embodiments, the protective layer is applied in a room temperature environment.
[0012] In some embodiments, a laminate stack of an integrated copper-graphene lamination includes: a core; a first graphene layer, the first graphene layer disposed on a surface portion of the core; a metal layer, the metal layer disposed on the first graphene layer; a second graphene layer, the second graphene layer disposed on the metal layer; a photoresist layer, the photoresist layer disposed on the second graphene layer; and a protective layer disposed on the photoresist layer, wherein the laminate stack defines an opening through the protective layer and at least one of the photoresist layer, the second graphene layer, the metal layer, the first graphene layer, or the core.
[0013] In some embodiments, the metal coating is disposed on the surface of the laminate stack such that the metal coating covers an inner surface of the laminate stack defined by the opening. In some embodiments, the metal coating is a material comprising at least one of palladium or copper. In some embodiments, the protective layer and the metal coating in contact with the protective layer are removed.
[0014] In some embodiments, the metal layer defines a gap. In some embodiments, the first graphene layer and the second graphene layer are cut to correspond to the gap.
[0015] In some embodiments, the protective layer is a material comprising a hydrogen ion concentration index score of one, two, three, four, eleven, twelve, thirteen, or fourteen.
[0016] In some embodiments, the protective layer is a material comprising at least one of polymethyl methacrylate (PMMA), polydimethyloxyaniline (PDMA), polyethylene vinyl acetate, polyetherimide, a water-insoluble film polymer, a thermoplastic polymer, or an elastomeric polymer.
[0017] In some embodiments, the protective layer includes at least one of an adhesive tape, a dry film photoresist, an atomic deposition layer, or a photoresist.
[0018] In some embodiments, the protective layer is applied in a room temperature environment.
[0019] In some embodiments, the opening is a via.
[0020] The above overview is provided only for the purpose of summarizing some exemplary embodiments, so as to provide a basic understanding of certain aspects of the present disclosure. Therefore, it should be understood that the above embodiments are only examples and should not be interpreted as narrowing the scope or spirit of the present disclosure in any way. It should be understood that in addition to the embodiments summarized herein, the scope of the present disclosure also includes many possible embodiments, some of which will be further described below. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Having thus generally described the present disclosure, reference will now be made to the accompanying drawings, which are not necessarily drawn to scale. The components shown in the drawings may or may not be present in certain embodiments described herein. Some embodiments may include fewer (or more) components than those shown in the drawings.
[0022] Figure 1A shows an exemplary diagram of a laminate stack according to one or more embodiments of the present invention;
[0023] Figure 1B According to one or more embodiments of the present invention, Figure 1A A top plan view of a laminate stack provided in;
[0024] Figure 2A shows an exemplary cross-sectional view of a laminate stack including at least vias drilled through layers of the laminate stack according to one or more embodiments of the present invention;
[0025] Figure 2B According to one or more embodiments of the present invention, Figure 2A A top plan view of a laminate stack provided in;
[0026] Figure 3A shows an exemplary cross-sectional view of a laminate stack including a metal plating layer according to one or more embodiments of the present invention;
[0027] Figure 3B According to one or more embodiments of the present invention, Figure 3A A top plan view of a laminate stack provided in;
[0028] Figure 4A shows an exemplary cross-sectional view of a laminate stack after removal of at least a metal plating layer and / or a protective layer according to one or more embodiments of the present invention;
[0029] Figure 4B According to one or more embodiments of the present invention, Figure 4A A top plan view of a laminate stack provided in;
[0030] Figure 5 An exemplary flow chart illustrating a process for creating a laminate stack according to one or more embodiments of the present invention; and
[0031] Figure 6 An exemplary flow chart of a process for removing a protective layer from a photoresist layer in a laminate stack in accordance with one or more embodiments of the present invention is shown. DETAILED DESCRIPTION
[0032] Exemplary embodiments will now be described more fully below with reference to the accompanying drawings, in which some but not all embodiments are shown. In fact, these embodiments can take many different forms and should not be construed as being limited to the embodiments set forth herein; on the contrary, these embodiments are provided so that the present disclosure will satisfy applicable legal requirements. The same reference numerals always represent the same elements. The terms "exemplary" and "examples" that may be used herein are not set to convey any qualitative assessment, but merely to convey the description of the examples. As used herein, terms such as "front", "rear", "top", "bottom", "interior", "exterior", "interior", "exterior", etc. are used for illustrative purposes in the examples provided below to describe the relative positions of certain components or parts of components. In addition, as will be apparent to those of ordinary skill in the art in view of the present disclosure, the terms "substantially" and "approximately" indicate that the elements or associated descriptions mentioned are accurate to within applicable engineering tolerances. Therefore, the use of any such terms should not be considered to limit the spirit and scope of the embodiments of the present invention.
[0033] A laminate stack is typically a structure formed by layers of materials (e.g., conductive and non-conductive) that are heated, pressed, and / or further processed to form a PCB. For example, such materials may include a non-conductive material (e.g., a core) having dielectric properties, an adhesive layer, and a conductive material, such as a commonly used metal, copper (e.g., copper foil). The laminate stack may then be laminated (i.e., heated and / or pressurized under a vacuum and / or controlled gas atmosphere) to cure the bonding between the material layers to create the structure of the PCB. In some aspects of the invention, heat may be applied to the bottom of the laminate stack (e.g., from below the laminate stack), to the top of the laminate stack (e.g., from above the laminate stack), and / or from different directions around the laminate stack (e.g., using an oven chamber to heat the laminate stack from multiple sides). Then, the conductive and thermally conductive material (e.g., copper) may be etched to create the conductive traces of the PCB. In some aspects, a process of adding a metal plating layer after drilling and plating the laminate stack may be used to create the PCB. For example, metal plating (such as copper, palladium, tin, etc.) is often used in vias drilled through a laminate stack to promote conductivity between the top and bottom surfaces of the laminate stack. However, when applying the metal plating on the inner surface of the via, a problem arises when the metal plating is applied over the entire surface of the laminate stack (e.g., including the top and bottom of the laminate stack). Therefore, the metal plating must be removed from certain locations (e.g., the top and bottom of the laminate stack) without damaging materials adjacent to the metal plating (e.g., a protective layer, any photolithographic patterning materials such as a photoresist layer, a graphene layer, and / or the like).
[0034] Graphene (carbon allotrope) is composed of a single layer of atoms (one graphite atomic layer) arranged in a two-dimensional honeycomb lattice nanostructure. It is considered to be a semi-metal with unusual electronic properties, which can be described by the theory of massless relativistic particles. One feature of graphene is that it conducts heat and electricity very efficiently along its plane. In addition, it has particularly high tensile strength, conductivity, and transparency. In addition, graphene can passivate the surface of copper and prevent oxidation of copper wires exposed to air. In high-frequency copper transmission lines, electrical signals are concentrated at positions close to the outer skin of copper, where the conductivity of the covering layer accounts for a significant part of the total conductivity. In the case where graphene is grown on copper by CVD, thermal annealing causes copper grain growth and causes the thermal conductivity of copper to increase by about 20%. The surface roughness of copper is significantly improved after graphene growth, and a smoother surface has a lower impedance at high frequencies.
[0035] Due to such properties of graphene, using graphene as a cover layer for copper within a lamination stack can have a beneficial effect on the properties of the resulting PCB, including higher bandwidth, greater conductivity, and better thermal management than conventional PCBs. However, when integrating graphene in the lamination process of the PCB (pre-lamination of PCB layers within the lamination stack), there are problems in creating the PCB structure. Therefore, it is important to protect the graphene from damage caused during the lamination process, brown copper oxidation, drilling process, and removal of the protective layer, as well as metal plating.
[0036] According to embodiments of the present invention, a protective layer may be placed on the outer surface of the material of the laminate stack (e.g., a core, a graphene layer, an adhesive layer, a photolithographic patterned layer (e.g., a photoresist layer), a conductive metal layer (such as copper), and / or the like) prior to applying the metal plating. By adding the protective layer to the outer surface of the material of the laminate stack, the metal plating may be removed in certain locations without damaging the underlying material. In contrast, if the metal plating is applied directly to the graphene layer or other layers (e.g., a photolithographic patterned layer), attempting to remove the metal plating to complete the PCB structure may damage the underlying layers. Thus, according to embodiments of the present invention, the use of a protective layer between the metal plating and the bottom layer of the laminate stack allows portions of the metal plating to be removed from the laminate stack without causing damage to the underlying material, and may allow only portions of the metal plating to be removed (e.g., the metal plating on the top and bottom surfaces of the laminate stack that are in contact with the protective layer) without removing the metal plating on other surfaces of the laminate stack (e.g., the metal plating inside the via).
[0037] refer to Figure 1A , Figure 1B , Figure 2A , Figure 2B , Figure 3A , Figure 3B , Figure 4A and Figure 4B , shows a laminate stack and a method of forming a laminate stack including a protective layer according to an embodiment of the present invention. Figure 1A , a side view of a laminate stack 100 (which forms a PCB) is shown, which includes a core material 116, a first graphene layer 118, a metal layer 110 (such as copper), a second graphene layer 108, a photoresist (or any graphene protective film) layer 106, and at least one protective layer (e.g., 104 and / or 114) (such as a photoresist dry film). In some embodiments, a connecting layer (e.g., a dielectric glue) is disposed between adjacent layers of the laminate stack 100. Although the metal layer 110 is described herein as a metal layer, the metal layer 110 may also be any conductive material. Reference Figure 1B , showing Figure 1A 100. Similarly, Figure 2A and Figure 2BA side view of a laminate stack 200 (which includes the material of the laminate stack 100 ) and a top view of the laminate stack 200 are shown, respectively.
[0038] Figure 2A and Figure 2B Also included are vias 151 drilled through the laminate stack 200. Likewise, Figure 3A and Figure 3B A side view of a laminate stack 300 (which includes the materials of laminate stacks 100 and 200) and a top view of the laminate stack 300 are shown, respectively. Figure 3A and Figure 3B Also included is a metal plating 102 that has been applied to the surface of the laminate stack 300 (including the inner surface of the via 151). Finally, Figure 4A and Figure 4B A side view of a laminate stack 400 (which includes materials of laminate stacks 100 , 200 , and 300 ) and a top view of the laminate stack 400 are shown, respectively. Figure 4A and Figure 4B Additionally depicted is the laminate stack after removal of the protective layer and overlying portions of the metallization, such that strategic remaining portions of the metallization 102 exist (e.g., inside the vias and on the outer portions of the laminate stack 400). Figure 4A and Figure 4B Removal of the bottom and top portions of the metal plating adjacent to the top surface of the photoresist layer (or other such lithographically patterned layer) 106 and the metal plating adjacent to the bottom surface of the core 116 is depicted.
[0039] Turn again Figure 1A and Figure 1B , the laminate stack 100 includes a core material 116, a first graphene layer 118 applied to the surface of the core material, a metal layer 110 (such as copper), a second graphene layer 108, a photoresist layer 106, and at least one protective layer (e.g., 104 and / or 114) (such as a photoresist dry film). In some embodiments, a connecting layer (e.g., a dielectric glue) is disposed between adjacent layers of the laminate stack 100. In some embodiments, a first protective layer 104 can be applied to the top surface of the core 116, and a second protective layer 114 can be applied to the bottom surface of the core 116. The first and / or second protective layers 104, 114 can be used to protect the surface of the core from any damage that may occur during the process of adding metal coatings to the stack and / or removing metal coatings. The following is about Figure 2A and Figure 2B , Figure 3A and Figure 3B , Figure 4A and Figure 4B Such embodiments are further described.
[0040] In some embodiments, and as described above, prior to photolithography and / or photoetching of the photoresist layer 106, the protective layer 104 (and / or 114) may be added to an outer surface(s) of the laminate stack, such as a top portion of the laminate stack (e.g., protective layer 104), a bottom portion of the laminate stack (e.g., protective layer 114), a side portion of the laminate stack (not shown), etc. This addition of a protective layer may be strategically added to specific surfaces or locations on the laminate stack, such as locations where metal plating will need to be removed during the process of creating the PCB.
[0041] In some embodiments, and as Figure 1A As shown in , a portion of the laminate stack 100 may include internal holes or micro vias, such as those shown as gaps 150, where gaps 150 are formed in only a portion of some layers within the laminate stack (e.g., a portion of the first graphene layer 118, a portion of the metal layer 110, a portion of the second graphene layer 108, and a portion of the photoresist layer 106, as depicted in the figure). In some embodiments, these portions of the laminate stack missing from the material that creates the gaps 150 may be pre-drilled and / or etched before the protective layer 104 is applied to the top surface of the photoresist layer 106. Reference Figure 1B , showing an embodiment of the present invention Figure 1A A top-level view of a laminate stack 100. For example, in Figure 1B , the protective layer 104 is shown from a top view.
[0042] In some embodiments, a patterned mask (not shown) can be applied adjacent to the photoresist layer (or any photolithographic patterned material or layer) 106 so that when light is applied, the mask disposed between the light source and the photoresist layer will change its solubility, and then the photoresist layer not protected by the mask will change its solubility. In other areas, the patterned mask will block light so that no change in the photoresist material occurs in the area below the mask. The mask can then be removed and a solvent or developer can be applied to the surface of the photoresist. Because the solubility of portions of the photoresist has changed, those portions will be dissolved by the solvent or developer, forming a gap (150) in the photoresist layer 106 and exposing the second graphene layer 108 below (e.g., the graphene layer directly below the photoresist layer 106). In some cases (e.g., when a negative photoresist is used), the application of light will be used to enhance the unshielded areas of the photoresist material. Therefore, in these cases, the application of a solvent will only degrade or wear away the portions of the photoresist layer 106 that are not exposed to light.
[0043] In the case where the gap is formed in the photoresist layer 106, the first and second graphene layers 118 and the metal layer 110 may be etched (e.g., via wet etching) to the same pattern of the gap in the photoresist layer 106. In some embodiments, the gap 150 in the photoresist layer 106 may have a different size (e.g., width and / or length) than the gap 150 formed in the graphene layers (118 and 108) and the metal layer 110. Subsequently, and in some embodiments, as Figure 2A and Figure 3A As shown, protective layer 104 and / or 114 can be applied to the top and bottom of laminated stack 100 in preparation for drilling process. In some embodiments, protective layer 104 is a material comprising at least one layer of polymethyl methacrylate (PMMA), polydimethyloxyaniline (PDMA), polyethylene vinyl acetate, polyetherimide, water-insoluble film polymer, thermoplastic polymer or elastomeric polymer. In some embodiments, protective layer 104 includes adhesive tape, thermoplastic release tape, dry film photoresist, atomic deposition layer, photoresist and / or the like. In some embodiments, and based on the material of the protective layer, protective layer 104 and / or 114 can be applied to laminated stack 100 by applying protective layer 104 and / or 114 at room temperature, such as when protective layer 104 is a photoresist material. In some embodiments, photoresist material can be baked and / or heated at a temperature range of 90 degrees Celsius to 180 degrees Celsius. In some embodiments, photoresist material can be applied by spraying and / or ultrasonic spraying.
[0044] In some embodiments, and where the protective layer 104 is a thermal release tape, the protective layer 104 can be applied to the photoresist layer 106 by laying down the sticky (or adhesive) surface of the thermal release tape on the top surface of the photoresist layer 106 and / or laying down the sticky surface of the thermal release tape on the bottom surface of the core 116. As will be appreciated by one of ordinary skill in the art, the sticky surface of the thermal release tape can be applied to any outer surface of the laminate stack (e.g., the bottom surface of the core, the top surface of the core, the bottom surface of the photolithographic patterned material, the top surface of the photolithographic patterned material, the top surface or bottom surface of the metal layer, etc.). In some embodiments, when the protective layer 104 is a dry film photoresist, heat and pressure can be applied to the protective layer 104 simultaneously.
[0045] The protective layers 104 and 114 can thus be used to shield and protect one or more intermediate layers (e.g., the core material 116, the first graphene layer 118, the metal layer 110, the second graphene layer 108, the photoresist layer 106 in the depicted embodiment) when applying and / or removing the metal plating. Figure 2A , Figure 2B , Figure 3A , Figure 3B , Figure 4A , Figure 4B , Figure 5 and Figure 6 Such embodiments are described more fully.
[0046] refer to Figure 2A and Figure 2B , vias 151 can be drilled through the layers of the laminate stack 100 to form the laminate stack 200. As such, once electroplating and / or application of a metal coating has occurred, the vias 151 can be used, for example, to create a conductive path between layers of a PCB. In some embodiments, and after the vias 151 have been drilled, a metal coating can be applied to the outer surface of the laminate stack (100, 200, 300), for example, by an electroplating process. Such (one or more) vias 151 can be used as conductive paths between layers of a PCB (e.g., different laminate stacks can be adjacent to each other to form a PCB) and / or as threaded holes to hold different layers of a PCB in a particular position.
[0047] As a non-limiting example, electroplating of the laminate stack may include applying a metal plating to the inner surface of the via, wherein the metal plating may include copper and / or other such conductive materials (tin, palladium, copper, etc.). The metal plating applied to the inner surface of the via may provide a conductive path from the top surface of the laminate stack to the bottom surface of the laminate stack, and such a conductive path may include material layers within the laminate stack. For example, the conductive path may pass through at least the core layer 116, the first graphene layer 118, the metal layer 110, the second graphene layer 108, and / or the photoresist layer 106 from the top surface to the bottom surface.
[0048] See also Figure 3A and Figure 3B , a depiction of a laminate stack including a metal plating layer 102 is shown. As a non-limiting example, the metal plating layer 102 of a metal plating process (e.g., an electroplating process for applying the metal plating layer) can be disposed on the top, bottom, and sides of the laminate stack, as well as inside any vias (e.g., via 151) drilled through the laminate stack 100, such as Figure 3A and Figure 3B The inner surface of the drilled via 151 is shown. In some embodiments, the metal plating layer 102 may include at least one of palladium and / or copper materials. Figure 3B , showing an embodiment of the present invention Figure 3A A top-level view of a laminate stack 300 is shown. For example, in Figure 3B , a top view of the laminate stack 300 is shown, and the metal plating 102 and the via 151 are shown from the top view.
[0049] refer to Figure 4A and Figure 4B, showing the laminate stack 400 from a side view and a top view, respectively. In some embodiments, the protective layer 104 adjacent to the top surface of the photoresist layer 106 can be removed without damaging the underlying photoresist layer 106. In some embodiments, the photoresist layer 106 adjacent to the graphene surface below the protective layer 104 can be removed along with the layer 104 without damaging the underlying graphene surface. For example, where the protective layer 104 includes a thermal release tape, the protective layer 104 and the photoresist layer can be removed by applying heat to the surface of the protective layer 104. In some embodiments, the removal of the protective layer can further include a metal coating 102 (such as Figure 3A 1 and 10. Additional removal of the top surface of the metallization layer 102 and the bottom surface of the metallization layer 102 as shown in FIG.
[0050] In some embodiments, the protective layer ( Figure 3A 104) and metal plating ( Figure 3A The top layer 102) shown in FIG. 1 can be removed by applying heat to the laminate stack at a predetermined temperature based on the protective layer 104 and its characteristics. Figure 5 and Figure 6 Such a process is described more fully.
[0051] See also Figure 5 , describes a method 500 for creating a lamination stack according to one or more embodiments of the present invention. In some embodiments, lamination stacks 100, 200, 300, and 400 may be used as a depiction of the processes described herein.
[0052] As shown in block 502, the method 500 may include the step of providing a core. In some embodiments, the laminate stack (100, 200, 300, 400) may include a core 116 as a dielectric. In some embodiments, the core 116 may include at least one of polyimide, polyester, polyurethane, bismaleimide triazine (BT), cyanate ester, fused silica, woven glass, fiberglass, microfiber glass, epoxy resin, phenolic compound, polytetrafluoroethylene (PTFE), low density polyethylene (LDPE), high density polyethylene (HDPE), polyethylene terephthalate (PET), thermoplastic polyurethane (TPU), or ceramic material.
[0053] As shown in block 504, method 500 may include the step of applying a first graphene layer to a surface portion of the core. In some embodiments and by way of non-limiting example, the laminate stack (100, 200, 300, 400) may include a plurality of graphene layers, including a first graphene layer 118, which may be disposed and / or grown on 110. For example, the graphene layers (at least the first graphene layer 118 and the second graphene layer 108) may be simultaneously grown on a surface of the core 110. In some embodiments, and when growing at least one graphene layer on the metal layer 110, the metal layer including at least one graphene layer (e.g., the first graphene layer 118 and / or the second graphene layer 108) may be placed on a surface portion of the core 116.
[0054] As shown in block 506, method 500 may include the step of applying a conductive layer to the first graphene layer. In some embodiments, the laminate stack (100, 200, 300, 400) may include a conductive layer that is a metal layer 110, such as a copper layer and / or the like, which may be used to grow the first graphene layer 118 on a surface (e.g., a top surface) of the conductive layer. In some embodiments, the metal layer 110 may include copper.
[0055] As shown in block 508, method 500 may include the step of applying a second graphene layer to metal layer (e.g., copper layer) 110. In some embodiments, the laminate stack (100, 200, 300, 400) may include a second graphene layer, such as in Figure 1A , Figure 2A , Figure 3A and Figure 4A 10 is a graphene layer 108. In some embodiments, the second graphene layer 108 may be grown on the metal layer 110 and / or the graphene layer 108 may be placed on the metal layer 110 to create a laminated stack. In some embodiments, each graphene layer adjacent to the metal layer (e.g., graphene layer 108 and graphene layer 118) may be simultaneously grown on the metal layer 110. In some embodiments, each graphene layer (108 and / or 118) may include multiple graphene layers.
[0056] As shown in block 510, the method 500 may include the step of applying a photoresist layer (106) onto the second graphene layer. In some embodiments, the laminate stack (100, 200, 300, 400) may include a photoresist layer 106 attached to and / or placed on the second graphene layer 108. In some embodiments, the photoresist layer 106 may be patterned such that the photosensitive material of the photoresist layer may be exposed to light or another focused energy source (such as a laser beam) that will change the solubility or sensitivity of the layer relative to the developer, thereby allowing the layer to be patterned.
[0057] As shown in block 512, method 500 may include the step of applying a protective layer to the photoresist layer. In some embodiments, protective layer 104 may be a material that is elastic to acidic and alkaline materials, such as elastic to materials containing hydrogen scores of 1, 2, 3, 4, 11, 12, 13, or 14. Such elasticity may be necessary for the protection of metal layer 110 during the metal deposition process when forming vias (e.g., via 151). In some embodiments, protective layer 104 is a material comprising at least one of polymethyl methacrylate (PMMA), polydimethyloxyaniline (PDMA), polyethylene vinyl acetate, polyetherimide, or a thermoplastic polymer or an elastomeric polymer. In some embodiments, protective layer 104 comprises an adhesive tape, a thermoplastic release tape, a dry film photoresist, an atomic deposition layer, or a photoresist. In some embodiments, when protective layer 104 is a dry film photoresist, protective layer 104 may be placed on top of photoresist layer 106. In some embodiments, the properties of the dry film photoresist may be such that the protective layer 104 may be stripped from the underlying photoresist layer 106 .
[0058] As shown in block 514, method 500 may include the step of drilling through the protective layer and at least one of the photoresist layer, the second graphene layer, the metal layer, the first graphene layer, and / or the core. In some embodiments, the laminate stack may thus include vias (such as vias) drilled through a portion of each layer. Figure 3A and Figure 4A The via 151 shown in FIG. 1 is shown in FIG. 1 . Figure 6 Describe this method more fully.
[0059] refer to Figure 6 , describes a method 600 for removing a protective layer from a photoresist layer in a laminate stack according to one or more embodiments of the present invention. In some embodiments, laminate stacks 100, 200, 300, and 400 may be used as depictions of the processes described herein.
[0060] In some embodiments, and as indicated by block 602, method 600 may include the step of applying a metal plating to the laminate stack, wherein the metal plating is applied to an outer surface of the laminate stack such that the metal plating covers an inner surface of the laminate stack formed by drilling (e.g., an inner surface of via 151). In some embodiments, block 602 and its associated processes may be performed at Figure 5151 and its associated processes. In some embodiments, and before drilling has occurred, the laminate stack may include strategic application of the protective layer 104 to the laminate stack such that where the protective layer 104 is placed, the protective layer 104 and any material overlying the protective layer may be removed from the laminate stack. For example, once drilling has occurred, the metal plating 102 may be applied to the protective layer 104 and the remaining portion of the surface of the laminate stack (e.g., the entire surface of the laminate stack and within the via 151).
[0061] In some embodiments, as shown in block 604, method 600 may include the step of removing the protective layer from the photoresist layer, wherein removing the protective layer results in removing the metal plating in contact with the protective layer. In some embodiments, and once heat at a predetermined temperature has been applied to the laminate stack, the protective layer 104 and / or 114 (and the adjacent metal plating 102) may be removed by simply pulling the protective layer 104 and / or 114 (and therewith, the adjacent metal plating 102) away from the photoresist layer 106. In some embodiments, the protective layer 104 (and / or 114) and the metal plating 102 may be removed by etching the protective layer 104 (and / or 114) and the metal plating 102.
[0062] As a non-limiting example, the metal plating layer 102 in contact with (eg, covering) the protective layers 104, 114 may include a metal plating layer in contact with and / or directly adjacent to the protective layers 104, 114 (eg, Figure 3A Thus, after removing the metal plating from areas where plating is not desired (such as the top and bottom), the metal plating will remain present in other areas of the PCB (e.g., within via 151) to create a conductive path between the layers of the PCB.
[0063] In some embodiments, removing the protective layer from the photoresist layer may include applying heat to the laminate stack at a predetermined temperature, where the temperature is based on the material properties of the selected protective layer. For example, and by way of non-limiting example, the protective layer 104 may be removed from another material layer (such as the photoresist layer 106) by applying heat to the laminate stack (including the core 116, the first graphene layer 118, the metal layer 110, the second graphene layer 108, the photoresist layer 106, the protective layer 104, and the metal plating layer 102) at a predetermined temperature. In some embodiments, the predetermined heat may include a temperature ranging from about 90 degrees Celsius to about 180 degrees Celsius. In some embodiments, and based on the properties (e.g., material) used in the protective layer 104, the protective layer 104 may be removed by applying a predetermined heat to the laminate stack. In some embodiments, the protective layer may be a thermal release tape that can be removed from the photoresist layer by applying heat and / or a specific solvent. For example, and in some embodiments, heat at a temperature between 180 degrees Celsius and 220 degrees Celsius may be applied to a protective layer comprising a prepreg having adhesive properties, such as a thermal release tape.
[0064] In some embodiments, the protective layer may include a dry film. Such a dry film may be removed as a protective layer by spraying and / or applying a dry film solvent to the surface of the protective layer. In some embodiments, and when the dry film solvent is applied, the protective layer may be stripped or removed from the photoresist layer 106.
[0065] In some embodiments, the photoresist layer 106 may be additionally removed from the laminate stack during and / or after removing the protective layer 106 and the metal plating 102 on the top and bottom surfaces of the laminate stack. For example, and in some embodiments, a secondary laminate stack may be applied to a (first) laminate stack to generate a multilayer PCB so that the multilayer PCB includes a plurality of different photolithographic patterned circuits. In some embodiments, one or more vias (e.g., via 151) may be in the same position for each layer of the laminate stack within the multilayer PCB, so that each via in the vias (e.g., via 151) is aligned to electrically connect the layers of the laminate stack. As will be appreciated by those skilled in the art, similar processes described herein may be used for each laminate stack within a multilayer PCB.
[0066] Those skilled in the art to which the present invention belongs will think of many modifications and other embodiments of the present invention as set forth herein, which have the benefit of the teachings presented in the above description and the related drawings. Therefore, it should be understood that the present invention is not limited to the specific embodiments disclosed, and modifications and other embodiments are intended to be included within the scope of the appended claims. In addition, although the above description and the related drawings describe exemplary embodiments in the context of certain exemplary combinations of elements and / or functions, it should be understood that different combinations of elements and / or functions may be provided by alternative embodiments without departing from the scope of the appended claims. In this regard, for example, as may be set forth in some of the appended claims, it is also envisioned that the combination of elements and / or functions that are different from those explicitly described above. Although specific terms are employed herein, they are used only in a general and descriptive sense, and not for the purpose of limitation.
Claims
1. A method of forming a laminate stack, include: Providing a core; applying a first graphene layer to a surface portion of the core; applying a metal layer to the first graphene layer; applying a second graphene layer to the metal layer; applying a photoresist layer to the second graphene layer; applying a protective layer to the photoresist layer; drilling through the protective layer and at least one of the photoresist layer, the second graphene layer, the metal layer, the first graphene layer, or the core; applying a metal coating to the laminate stack, wherein the metal coating is applied to the laminate stack such that the metal coating covers an inner surface of the laminate stack formed by the drilling; as well as The protective layer is removed from the photoresist layer, wherein the removal of the protective layer results in the removal of the metal plating layer in contact with the protective layer.
2. The method of claim 1, wherein the metal plating layer is a material including at least one of palladium, tin or copper.
3. The method of claim 1, wherein removing the protective layer include: Heat is applied to the laminate stack at a predetermined temperature, wherein the temperature is based on the protective layer.
4. The method of claim 3, wherein the temperature is in the range of about 90 degrees Celsius to about 180 degrees Celsius.
5. The method of claim 1, wherein the protective layer is a material comprising resilience to at least one, two, three, four, eleven, twelve, thirteen, or fourteen hydrogen scores.
6. The method of claim 1, wherein the protective layer is a material comprising at least one of polymethyl methacrylate (PMMA), polydimethyloxyaniline (PDMA), polyethylene vinyl acetate, a water-insoluble film polymer, polyetherimide, a thermoplastic polymer, or an elastomeric polymer.
7. The method of claim 1, wherein the protective layer comprises at least one of an adhesive tape, a thermal release tape, a dry film photoresist, an atomic deposition layer, or a photoresist.
8. The method of claim 1, wherein the protective layer is applied in a room temperature environment.
9. A laminate stack of integrated copper-graphene laminates, include: core; a first graphene layer disposed on a surface portion of the core; a metal layer, wherein the metal layer is disposed on the first graphene layer; a second graphene layer, wherein the second graphene layer is disposed on the metal layer; a photoresist layer, wherein the photoresist layer is disposed on the second graphene layer; as well as a protective layer, the protective layer being disposed on the photoresist layer, Wherein the laminate stack defines an opening through the protective layer and at least one of the photoresist layer, the second graphene layer, the metal layer, the first graphene layer, or the core.
10. The laminate stack of claim 9, further comprising a metal coating disposed on a surface of the laminate stack such that the metal coating covers an inner surface of the laminate stack defined by the opening.
11. The laminate stack of claim 10, wherein the metal coating is a material comprising at least one of palladium or copper.
12. The laminate stack of claim 10, wherein the protective layer and the metal plating layer in contact with the protective layer are removed.
13. The laminate stack of claim 9, wherein the metal layers define a gap. 14 . The laminate stack of claim 13 , wherein the first graphene layer and the second graphene layer are cut to correspond to the gap.
15. The laminate stack of claim 9, wherein the protective layer is a material comprising a hydrogen ion concentration index score of one, two, three, four, eleven, twelve, thirteen, or fourteen.
16. The laminate stack of claim 9, wherein the protective layer is a material comprising at least one of polymethyl methacrylate (PMMA), polydimethyloxyaniline (PDMA), polyethylene vinyl acetate, polyetherimide, a water-insoluble film polymer, a thermoplastic polymer, or an elastomeric polymer.
17. The laminate stack of claim 9, wherein the protective layer comprises at least one of an adhesive tape, a dry film photoresist, an atomic deposition layer, or a photoresist.
18. The laminate stack of claim 9, wherein the protective layer is applied in a room temperature environment.
19. The laminate stack of claim 9, wherein the opening is a via.