Semiconductor device and method for manufacturing the same

By forming spacer structures of different thicknesses in the core and peripheral areas of the semiconductor device, and using interlayer dielectric layer and high-k layer deposition technology, the spacer thickness is optimized, and the problem of reducing the thickness of the conductive pattern spacer is solved. Improves the reliability and performance of the equipment.

CN119012688APending Publication Date: 2024-11-22SK HYNIX INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311726128.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-17
Filing Date
2023-12-15
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In semiconductor devices, as the high integration of the core region decreases, the thickness of the spacer between the conductive patterns decreases, and the optimization of the spacer thickness of the peripheral region is difficult to improve, affecting the equipment performance and short channel effect.

Method used

By forming spacer structures with different total thicknesses in the core area and the peripheral area, the gap is filled with interlayer dielectric layers, and concaves are formed by removing dummy patterns to deposit high k layers and conductive materials, an RMG structure is formed to optimize the spacing to optimize the spacing Thickness of the object.

Benefits of technology

Spacer thickness optimization for different regions is achieved, sense amplifier transistor mismatch based on ion implantation changes is reduced, and reliability and performance of semiconductor devices are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119012688A_ABST
    Figure CN119012688A_ABST
Patent Text Reader

Abstract

The invention relates to a semiconductor device and a method for manufacturing the same. A semiconductor device includes: a substrate including a peripheral region and a core region; a first conductive pattern disposed over the substrate in the peripheral region; a second conductive pattern disposed over the substrate in the core region; first spacer structures formed on both sidewalls of the first conductive pattern; and second spacer structures formed on both sidewalls of the second conductive pattern, the second spacer structures having a thickness less than a total thickness of the first spacer structures.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to Korean Patent Application No. 10-2023-0063654, filed on May 17, 2023, which is hereby incorporated by reference in its entirety. Technical Field

[0003] Various embodiments of the present invention relate to a method for manufacturing a semiconductor device, and more particularly, to a spacer formed on both sidewalls of a conductive pattern in a core region and a peripheral region, and a method for forming the spacer. Background Art

[0004] As the core region is reduced due to high integration of semiconductor devices, the interval between conductive patterns formed in the core region is also reduced, and this requires that the spacers formed on both sidewalls of the conductive patterns have a minimized thickness.

[0005] Meanwhile, in the peripheral region, it is necessary to optimize the thickness of the spacers formed on both sidewalls of the conductive pattern in order to improve the performance gain and the short channel effect of the device. Summary of the invention

[0006] An embodiment of the present invention is directed to dualizing the thickness of spacers formed in a core region and a peripheral region to optimize the thickness of the spacers according to their needs.

[0007] According to one embodiment of the present invention, a semiconductor device includes: a substrate, which includes a peripheral region and a core region; a first conductive pattern, which is arranged above the substrate in the peripheral region; a second conductive pattern, which is arranged above the substrate in the core region; a first spacer structure, which is formed on two side walls of the first conductive pattern; and a second spacer structure, which is formed on two side walls of the second conductive pattern, the second spacer structure having a thickness less than the total thickness of the first spacer structure.

[0008] According to another embodiment of the present invention, a method for manufacturing a semiconductor device includes: providing a substrate including a core region and a peripheral region; forming a first conductive pattern and a second conductive pattern over the substrate in the peripheral region and the core region, respectively; and forming a first spacer structure and a second spacer structure with different total thicknesses on two side walls of the first conductive pattern and two side walls of the second conductive pattern.

[0009] According to another embodiment of the present invention, a method for manufacturing a semiconductor device includes: providing a substrate including a core region and a peripheral region; forming a first dummy pattern over the substrate in the peripheral region; forming a second dummy pattern over the substrate in the core region; forming a spacer structure with different total thicknesses on two side walls of the first conductive pattern and two side walls of the second conductive pattern; forming an interlayer dielectric layer, the interlayer dielectric layer filling the gap between the first dummy pattern and the second dummy pattern; forming recesses in the core region and the peripheral region by removing the first dummy pattern and the second dummy pattern; forming an RMG (replacement metal gate) structure by depositing a high-k layer and a conductive material layer in the recesses in the core region and the peripheral region. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figures 1 to 4 is a cross-sectional view of a semiconductor device including a buffer spacer according to an embodiment of the present invention.

[0011] Figures 5 to 8 is a cross-sectional view of a semiconductor device including offset spacers according to an embodiment of the present invention.

[0012] Figures 9 to 12 is a cross-sectional view of a semiconductor device including a buffer spacer and a replacement metal gate (RMG) structure according to an embodiment of the present invention.

[0013] Figures 13 to 16 is a cross-sectional view of a semiconductor device including an offset spacer and an RMG structure according to an embodiment of the present invention.

[0014] FIG. 17A to FIG. 17E is a cross-sectional view illustrating one example of a method for manufacturing a semiconductor device including a buffer spacer according to one embodiment of the present invention.

[0015] 18A to 18F is a cross-sectional view illustrating one example of a method for manufacturing a semiconductor device including an offset spacer according to one embodiment of the present invention.

[0016] FIG. 19A to FIG. 19H is a cross-sectional view illustrating one example of a method for manufacturing a semiconductor device including an RMG structure according to one embodiment of the present invention. DETAILED DESCRIPTION

[0017] Various embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. However, the present invention can be embodied in different forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, these embodiments are provided so that the present disclosure will be thorough and complete, and the scope of the present invention will be fully conveyed to those skilled in the art. Throughout the present disclosure, throughout the various figures and embodiments of the present invention, similar reference numerals refer to similar parts.

[0018] The drawings are not necessarily to scale, and in some instances, the proportions may have been exaggerated in order to clearly illustrate features of the embodiments. When a first layer is referred to as being "on" a second layer or "on" a substrate, this refers not only to the case where the first layer is directly formed on the second layer or substrate, but also to the case where a third layer exists between the first layer and the second layer or substrate. In the present disclosure, the singular form is intended to include the plural form as well, unless the context clearly indicates otherwise.

[0019] Semiconductor memory devices, particularly dynamic random access memory (DRAM) devices, typically may include three regions. The first region may be a cell array in which memory cells are arranged in a matrix form, and the second region may be a peripheral circuit region, which is a non-repetitive circuit that stores and transmits data and drives the cell array. Hereinafter, the peripheral circuit region will be referred to as the peripheral region. The third region may be a core region, which is a repetitive circuit including a sense amplifier, a decoder, etc.

[0020] Each of the peripheral region and the core region may include an NMOS region or a PMOS region. A high voltage NMOS transistor and a low voltage NMOS transistor may be formed in the NMOS region of the peripheral region, and a high voltage PMOS transistor and a low voltage PMOS transistor may be formed in the PMOS region of the peripheral region. A high voltage NMOS transistor and a low voltage NMOS transistor may be formed in the NMOS region of the core region, and a high voltage PMOS transistor and a low voltage PMOS transistor may be formed in the PMOS region of the core region.

[0021] In the embodiment of the present invention, for the convenience of description, only the peripheral region and the core region are illustrated and described, and the cell region is omitted. Moreover, according to the embodiment of the present invention, the NMOS region and the PMOS region in the peripheral region and the core region, the NMOS transistor and the PMOS transistor, and the high voltage transistor and the low voltage transistor are not described separately, but the embodiment of the present invention can be applied according to the type and transistor in each region.

[0022] Figures 1 to 4 1 is a cross-sectional view of a semiconductor device including a buffer spacer according to an embodiment of the present invention. In addition to the stacking structure and materials of the buffer spacer, Figures 1 to 4 The components of can be the same. Figures 2 to 4 In the Figure 1 Description of the same constituent elements also appearing in .

[0023] refer to Figure 1 , the substrate 101 may include a peripheral region PERI and a core region CORE.

[0024] The substrate 101 may be a material suitable for semiconductor processing. The substrate 101 may include a semiconductor substrate. The substrate 101 may be formed of a silicon-containing material. The substrate 101 may include silicon, single crystal silicon, polycrystalline silicon, amorphous silicon, silicon germanium, single crystal silicon germanium, polycrystalline silicon germanium, carbon-doped silicon, a combination thereof, or a multilayer thereof. The substrate 101 may also include other semiconductor materials, such as germanium. The substrate 101 may include a III / V semiconductor substrate, such as a compound semiconductor substrate, such as GaAs. The substrate 101 may include a silicon-on-insulator (SOI) substrate.

[0025] In the substrate 101 , the isolation layer 102 may divide the substrate 101 into a peripheral region PERI and a core region CORE, and define an active region.

[0026] The peripheral conductive pattern PG may be formed over the substrate 101 of the peripheral region PERI. The core conductive pattern CG may be formed over the substrate 101 of the core region CORE. A bit line structure or a gate structure disposed at the same level as the peripheral conductive pattern PG of the peripheral region PERI and the core conductive pattern CG of the core region CORE may be formed in the cell region.

[0027] The line width of the peripheral conductive pattern PG and the line width of the core conductive pattern CG may be the same. According to another embodiment of the present invention, the line width of the peripheral conductive pattern PG and the line width of the core conductive pattern CG may be different. As the core region adjacent to the cell region becomes smaller due to the miniaturization of the semiconductor device, the distance Dp between the peripheral conductive patterns PG may be longer than the distance Dc between the core conductive patterns CG (Dp>Dc).

[0028] The peripheral conductive pattern PG and the core conductive pattern CG may include a planar gate pattern. The peripheral conductive pattern PG and the core conductive pattern CG may include a stacked structure of the same material. In other words, the peripheral conductive pattern PG and the core conductive pattern CG may be formed simultaneously by sequentially stacking layers of the same material and patterning them once. Each of the peripheral conductive pattern PG and the core conductive pattern CG may be formed as a stacked structure of a gate dielectric layer 103, a first gate electrode 104, a second gate electrode 105, and a gate hard mask 106, and the gate dielectric layer 103, the first gate electrode 104, the second gate electrode 105, and the gate hard mask 106 are stacked above the substrate 101 in the peripheral region PERI and the core region CORE, respectively, in the order described.

[0029] The peripheral spacer structure PSP may be formed on both side walls of the peripheral conductive pattern PG, and the core spacer structure CSP may be formed on both side walls of the core conductive pattern CG. A portion of the peripheral spacer structure PSP may also be formed above the top surface of the peripheral conductive pattern PG. A portion of the core spacer structure CSP may also be formed above the top surface of the core conductive pattern CG. The total thickness Wp of the peripheral spacer structure PSP may be greater than the total thickness Wc of the core spacer structure CSP (Wp>Wc).

[0030] The gate dielectric layer 103 may include a dielectric material. For example, the gate dielectric layer 103 may include silicon oxide. According to another embodiment of the present invention, the gate dielectric layer 103 may include a high-k material.

[0031] The first gate electrode 104 and the second gate electrode 105 may include a conductive material. The first gate electrode 104 may include a semiconductor material. For example, the first gate electrode 104 may include polysilicon, but the concept and scope of the present invention are not limited thereto. The second gate electrode 105 may include a metal material. For example, the gate electrode 105 may include tungsten or a tungsten-containing material, but the concept and scope of the present invention are not limited thereto.

[0032] The gate hard mask 106 may include a dielectric material. The gate hard mask 106 may be provided to protect the upper surface of the second gate electrode 105 and pattern the gate dielectric layer 103, the first gate electrode 104, and the second gate electrode 105, and the gate hard mask 106 may be formed of a material having an etching selectivity with respect to the gate dielectric layer 103, the first gate electrode 104, and the second gate electrode 105. For example, the gate hard mask 106 may include silicon nitride.

[0033] The peripheral spacer structure PSP and the core spacer structure CSP may include different stack structures. The peripheral spacer structure PSP may include at least one more layer of spacer material than the core spacer structure CSP.

[0034] The peripheral spacer structure PSP may include a stack structure of a nitride spacer 107, a first oxide spacer 108, and a second oxide spacer 109. The nitride spacer 107 may also be formed over the top surface of the peripheral conductive pattern PG.

[0035] The core spacer structure CSP may include a stack structure of a nitride spacer 107 and a second oxide spacer 109. The nitride spacer 107 may also be formed over a top surface of the core conductive pattern CG.

[0036] refer to Figure 2 , the peripheral spacer structure PSP may include a stacked structure of a nitride spacer 107, a low-k spacer 201, and a second oxide spacer 109. For example, the low-k spacer 201 may include one selected from the group consisting of SiBN (silicon boron nitride), SiBCN (silicon boron carbon nitride), SiCO (silicon carbon oxide), and SiCON (silicon carbon oxide nitride).

[0037] The core spacer structure CSP may include a stack structure of a nitride spacer 107 and an oxide spacer 109 .

[0038] refer to Figure 3 , the peripheral spacer structure PSP may include a stack structure of a first nitride spacer 107 , an oxide spacer 108 , and a second nitride spacer 301 .

[0039] The core spacer structure CSP may include a stack structure of a first nitride spacer 107 and a second nitride spacer 301 .

[0040] refer to Figure 4 , the peripheral spacer structure PSP may include a stack structure of nitride spacers 107 , oxide spacers 108 , and low-k spacers 401 .

[0041] The core spacer structure CSP may include a stack structure of the nitride spacer 107 and the low-k spacer 401. For example, the low-k spacer 401 may include one selected from the group consisting of SiBN, SiBCN, SiCO, and SiCON.

[0042] Refer to the above Figures 1 to 4 According to an embodiment of the present invention, the first nitride spacers 107 in the peripheral spacer structure PSP and the core spacer structure CSP may be continuous buffer spacers covering an upper portion of the substrate 101 between the conductive patterns and a sidewall of each conductive pattern.

[0043] Moreover, by binarizing the spacer thickness of the peripheral spacer structure PSP and the spacer thickness of the core spacer structure CSP and applying the spacer thickness optimized for each region, the reliability of the semiconductor device can be ensured. In particular, by forming the total thickness of the core spacer structure CSP smaller than the total thickness Wp of the peripheral spacer structure PSP, the mismatch of the sense amplifier transistor based on the change of ion implantation can be reduced.

[0044] Figures 5 to 8 1 is a cross-sectional view of a semiconductor device including an offset spacer according to an embodiment of the present invention. In addition to the stacking structure and materials of the offset spacer, Figures 5 to 8 All components of can be the same. Figures 6 to 8 In the Figure 5 Description of the same constituent elements also appearing in .

[0045] refer to Figure 5 , the substrate 101 may include a peripheral region PERI and a core region CORE.

[0046] The substrate 101 may be a material suitable for semiconductor processing. The substrate 101 may include a semiconductor substrate. The substrate 101 may be formed of a silicon-containing material. The substrate 101 may include silicon, single crystal silicon, polycrystalline silicon, amorphous silicon, silicon germanium, single crystal silicon germanium, polycrystalline silicon germanium, carbon-doped silicon, a combination thereof, or a multilayer thereof. The substrate 101 may also include other semiconductor materials, such as germanium. The substrate 101 may include a III / V semiconductor substrate, such as a compound semiconductor substrate, such as GaAs. The substrate 101 may include a silicon-on-insulator (SOI) substrate.

[0047] In the substrate 101 , the isolation layer 102 may divide the substrate 101 into a peripheral region PERI and a core region CORE, and define an active region.

[0048] The peripheral conductive pattern PG may be formed over the substrate 101 of the peripheral region PERI. The core conductive pattern CG may be formed over the substrate 101 of the core region CORE. A bit line structure or a gate structure disposed at the same level as the peripheral conductive pattern PG of the peripheral region PERI and the core conductive pattern CG of the core region CORE may be formed in the cell region.

[0049] The line width of the peripheral conductive pattern PG and the line width of the core conductive pattern CG may be the same. As the core region adjacent to the cell region becomes smaller due to miniaturization of semiconductor devices, the distance Dp between the peripheral conductive patterns PG may be longer than the distance Dc between the core conductive patterns CG (Dp>Dc).

[0050] The peripheral conductive pattern PG and the core conductive pattern CG may include a stacked structure of the same material. In other words, the peripheral conductive pattern PG and the core conductive pattern CG may be formed simultaneously by sequentially stacking layers of the same material and patterning them once. The peripheral conductive pattern PG and the core conductive pattern CG may be formed as a stacked structure of a gate dielectric layer 103, a first gate electrode 104, a second gate electrode 105, and a gate hard mask 106, and the gate dielectric layer 103, the first gate electrode 104, the second gate electrode 105, and the gate hard mask 106 are stacked above the substrate 101 in the peripheral region PERI and the core region CORE, respectively, in the order described.

[0051] The peripheral spacer structure PSP may be formed on both sidewalls of the peripheral conductive pattern PG, and the core spacer structure CSP may be formed on both sidewalls of the core conductive pattern CG. The total thickness Wp of the peripheral spacer structure PSP may be greater than the total thickness Wc of the core spacer structure CSP (Wp>Wc).

[0052] The gate dielectric layer 103 may include a dielectric material. For example, the gate dielectric layer 103 may include silicon oxide. According to another embodiment of the present invention, the gate dielectric layer 103 may include a high-k material.

[0053] The first gate electrode 104 and the second gate electrode 105 may include a conductive material. The first gate electrode 104 may include a semiconductor material. For example, the first gate electrode 104 may include polysilicon, but the concept and scope of the present invention are not limited thereto. The second gate electrode 105 may include a metal material. For example, the gate electrode 105 may include tungsten or a tungsten-containing material, but the concept and scope of the present invention are not limited thereto.

[0054] The gate hard mask 106 may include a dielectric material. The gate hard mask 106 may be provided to protect the upper surface of the second gate electrode 105 and pattern the gate dielectric layer 103, the first gate electrode 104, and the second gate electrode 105, and the gate hard mask 106 may be formed of a material having an etching selectivity with respect to the gate dielectric layer 103, the first gate electrode 104, and the second gate electrode 105. For example, the gate hard mask 106 may include silicon nitride.

[0055] The peripheral spacer structure PSP and the core spacer structure CSP may include different stack structures. The peripheral spacer structure PSP may include at least one more layer of spacer material than the core spacer structure CSP.

[0056] The peripheral spacer structure PSP may include a stack structure of a nitride spacer 501 , a first oxide spacer 108 , and a second oxide spacer 109 .

[0057] The core spacer structure CSP may include a stack structure of a nitride spacer 501 ′ and a second oxide spacer 109 .

[0058] refer to Figure 6 , the peripheral spacer structure PSP may include a stack structure of a nitride spacer 501, a low-k spacer 201, and an oxide spacer 109. For example, the low-k spacer 201 may include one selected from the group consisting of SiBN, SiBCN, SiCO, and SiCON.

[0059] The core spacer structure CSP may include a stack structure of a nitride spacer 501 ′ and an oxide spacer 109 .

[0060] refer to Figure 7 , the peripheral spacer structure PSP may include a stack structure of a first nitride spacer 501 , an oxide spacer 108 , and a second nitride spacer 301 .

[0061] The core spacer structure CSP may include a stack structure of a first nitride spacer 501 ′ and a second nitride spacer 301 .

[0062] refer to Figure 8 , the peripheral spacer structure PSP may include a stack structure of nitride spacers 501 , oxide spacers 108 , and low-k spacers 401 .

[0063] The core spacer structure CSP may include a stack structure of a nitride spacer 501' and a low-k spacer 401. For example, the low-k spacer 401 may include one selected from the group consisting of SiBN, SiBCN, SiCO, and SiCON.

[0064] refer to Figures 5 to 8 According to an embodiment of the present invention, the nitride spacer 501 of the peripheral spacer structure PSP may be an offset spacer disposed only on both sidewalls of the peripheral conductive pattern PG. Therefore, since dopants may be directly implanted into the substrate 101 during ion implantation for the junction, it may be advantageous for junction engineering. In the core spacer structure CSP, the nitride spacer 501' may be a buffer spacer covering portions of the substrate 101 between the conductive patterns and both sidewalls of each conductive pattern.

[0065] Moreover, by binarizing the spacer thickness of the peripheral spacer structure PSP and the spacer thickness of the core spacer structure CSP and applying the spacer thickness optimized for each region, the reliability of the semiconductor device can be ensured. In particular, by forming the total thickness of the core spacer structure CSP smaller than the total thickness Wp of the peripheral spacer structure PSP, the mismatch of the sense amplifier transistor based on the change of ion implantation can be improved.

[0066] According to another embodiment of the present invention, like the peripheral spacer structure PSP, the core spacer structure CSP may also use the nitride spacers 501 ′ as offset spacers disposed only on both sidewalls of the core conductive pattern CG.

[0067] Figures 9 to 12 is a cross-sectional view of a semiconductor device including a buffer spacer and a replacement metal gate (RMG) structure according to one embodiment of the present invention. In addition to the stacked structure of the conductive pattern, Figures 9 to 12 All components can be Figures 1 to 4 The components of Figures 9 to 12 In the Figures 1 to 4 Description of the same constituent elements also appearing in .

[0068] refer to Fig. 9 , the substrate 101 may include a peripheral region and a core region.

[0069] The substrate 101 may be a material suitable for semiconductor processing. The substrate 101 may include a semiconductor substrate. The substrate 101 may be formed of a silicon-containing material. The substrate 101 may include silicon, single crystal silicon, polycrystalline silicon, amorphous silicon, silicon germanium, single crystal silicon germanium, polycrystalline silicon germanium, carbon-doped silicon, a combination thereof, or a multilayer thereof. The substrate 101 may also include other semiconductor materials, such as germanium. The substrate 101 may include a III / V semiconductor substrate, such as a compound semiconductor substrate, such as GaAs. The substrate 101 may include a silicon-on-insulator (SOI) substrate.

[0070] In the substrate 101 , the isolation layer 102 may divide the substrate 101 into a peripheral region PERI and a core region CORE, and define an active region.

[0071] The peripheral conductive pattern PG may be formed over the substrate 101 in the peripheral region PERI. The core conductive pattern CG may be formed over the substrate 101 in the core region CORE. The peripheral conductive pattern PG and the core conductive pattern CG may include a replacement metal gate (RMG) structure. The interlayer dielectric layer 605 may gap-fill the space between the peripheral conductive pattern PG and the core conductive pattern CG. A bit line structure or a gate structure may be formed in the cell region, and the bit line structure or the gate structure is arranged at the same level as the peripheral conductive pattern and the core conductive pattern of the peripheral region PERI and the core region CORE.

[0072] The line width of the peripheral conductive pattern PG and the line width of the core conductive pattern CG may be different or the same. For example, in one embodiment, as the core region adjacent to the cell region may be smaller for improving the miniaturization of the semiconductor device, the distance Dp between the peripheral conductive patterns PG may be longer than the distance Dc between the core conductive patterns CG (Dp>Dc).

[0073] The peripheral conductive pattern PG and the core conductive pattern CG may include a replacement metal gate (RMG) structure. The RMG structure in the peripheral conductive pattern PG and the core conductive pattern CG may include a stacked structure of the same material. The peripheral conductive pattern PG and the core conductive pattern CG may be formed as a stacked structure of a gate dielectric layer 601, a high-k layer 602, and a gate electrode 603, which are stacked above the substrate 101 in the peripheral region PERI and the core region CORE in the order described. The dielectric layer 601 may have a linear shape, the high-k layer 602 may have a U-shape, and the gate electrode 603 may have a columnar shape filling the space within the U-shaped high-k layer 602. The high-k layer 602 may have a flat bottom and vertical sidewalls formed on the dielectric layer 601.

[0074] The peripheral spacer structure PSP may be formed on both sidewalls of the peripheral conductive pattern PG, and the core spacer structure CSP may be formed on both sidewalls of the core conductive pattern CG. The total thickness Wp of the peripheral spacer structure PSP may be greater than the total thickness Wc of the core spacer structure CSP (Wp>Wc).

[0075] The gate dielectric layer 601 may include a dielectric material. For example, the gate dielectric layer 601 may include silicon oxide.

[0076] The high-k layer 602 may include a high-k material having a higher dielectric constant than silicon oxide. For example, the high-k layer 602 may include at least one of boron nitride, hafnium oxide, hafnium silicon oxide, hafnium aluminum oxide, lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, yttrium oxide, aluminum oxide, lead scandium tantalum oxide, or lead zinc niobate.

[0077] The gate electrode 603 may include at least one of the following: a metal, a metal alloy, a conductive metal nitride, a metal silicide, a doped semiconductor material, a conductive metal oxide, and a conductive metal oxynitride. The gate electrode 603 may include at least one of the following: for example, titanium nitride (TiN), tantalum carbide (TaC), tantalum nitride (TaN), titanium silicon nitride (TiSiN), tantalum silicon nitride (TaSiN), tantalum titanium nitride (TaTiN), titanium aluminum nitride (TiAlN), tantalum aluminum nitride (TaAlN), tungsten nitride (WN), ruthenium (Ru), titanium aluminum (TiAl), titanium aluminum carbonitride (TiAlC-N), titanium aluminum carbide (TiAlC), titanium carbide (TiC), tantalum carbonitride (TaCN) , tungsten (W), aluminum (Al), copper (Cu), cobalt (Co), titanium (Ti), tantalum (Ta), nickel (Ni), platinum (Pt), nickel platinum (Ni-Pt), niobium (Nb), niobium nitride (NbN), niobium carbide (NbC), molybdenum (Mo), molybdenum nitride (MoN), molybdenum carbide (MoC), tungsten carbide (WC), rhodium (Rh), palladium (Pd), iridium (Ir), osmium (Os), silver (Ag), gold (Au), zinc (Zn), vanadium (V) and combinations thereof, but the concept and scope of the present invention are not limited thereto. The conductive metal oxides and conductive metal oxynitrides may include oxidized forms of the above materials, but the concept and scope of the present invention are not limited thereto.

[0078] The interlayer dielectric layer 605 may include a dielectric material. The interlayer dielectric layer 605 may include, for example, one selected from among silicon oxide, silicon nitride, and silicon oxynitride.

[0079] The peripheral spacer structure PSP may include a stack structure of a nitride spacer 107 , a first oxide spacer 108 , and a second oxide spacer 109 .

[0080] The core spacer structure CSP may include a stack structure of a nitride spacer 107 and a second oxide spacer 109 .

[0081] refer to Fig.10 , the peripheral spacer structure PSP may include a stack structure of a nitride spacer 107, a low-k spacer 201, and a second oxide spacer 109. For example, the low-k spacer 201 may include one selected from the group consisting of SiBN, SiBCN, SiCO, and SiCON.

[0082] The core spacer structure CSP may include a stack structure of a nitride spacer 107 and an oxide spacer 109 .

[0083] refer to Fig.11 , the peripheral spacer structure PSP may include a stack structure of a first nitride spacer 107 , an oxide spacer 108 , and a second nitride spacer 301 .

[0084] The core spacer structure CSP may include a stack structure of a first nitride spacer 107 and a second nitride spacer 301 .

[0085] refer to Fig.12 , the peripheral spacer structure PSP may include a stack structure of nitride spacers 107 , oxide spacers 108 , and low-k spacers 401 .

[0086] The core spacer structure CSP may include a stack structure of the nitride spacer 107 and the low-k spacer 401. For example, the low-k spacer 401 may include one selected from the group consisting of SiBN, SiBCN, SiCO, and SiCON.

[0087] Figures 13 to 16 is a cross-sectional view of a semiconductor device including an offset spacer and an RMG structure according to an embodiment of the present invention. In addition to the stacked structure of the conductive pattern, Figures 13 to 16 All components can be Figures 5 to 8 Therefore, the components of Figures 13 to 16 Description of the same constituent elements also appearing in .

[0088] refer to Fig.13 , the peripheral conductive pattern PG and the core conductive pattern CG may include a replacement metal gate (RMG) structure. The RMG structure in the peripheral conductive pattern PG and the core conductive pattern CG may include a stacked structure of the same material. The peripheral conductive pattern PG and the core conductive pattern CG may be formed as a stacked structure of a gate dielectric layer 601, a high-k layer 602, and a gate electrode 603, and the gate dielectric layer 601, the high-k layer 602, and the gate electrode 603 are stacked above the substrate 101 in the peripheral region PERI and the core region CORE in the order described.

[0089] The peripheral spacer structure PSP may be formed on both sidewalls of the peripheral conductive pattern PG, and the core spacer structure CSP may be formed on both sidewalls of the core conductive pattern CG. The total thickness Wp of the peripheral spacer structure PSP may be greater than the total thickness Wc of the core spacer structure CSP (Wp>Wc).

[0090] The gate dielectric layer 601 may include a dielectric material. For example, the gate dielectric layer 601 may include silicon oxide.

[0091] The high-k layer 602 may include a high-k material having a higher dielectric constant than silicon oxide. For example, the high-k layer 602 may include at least one of boron nitride, hafnium oxide, hafnium silicon oxide, hafnium aluminum oxide, lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, yttrium oxide, aluminum oxide, lead scandium tantalum oxide, and lead zinc niobate.

[0092] The gate electrode 603 may include at least one of the following: a metal, a metal alloy, a conductive metal nitride, a metal silicide, a doped semiconductor material, a conductive metal oxide, and a conductive metal oxynitride. The gate electrode 603 may include at least one of the following: for example, titanium nitride (TiN), tantalum carbide (TaC), tantalum nitride (TaN), titanium silicon nitride (TiSiN), tantalum silicon nitride (TaSiN), tantalum titanium nitride (TaTiN), titanium aluminum nitride (TiAlN), tantalum aluminum nitride (TaAlN), tungsten nitride (WN), ruthenium (Ru), titanium aluminum (TiAl), titanium aluminum carbonitride (TiAlC-N), titanium aluminum carbide (TiAlC), titanium carbide (TiC), tantalum carbonitride (TaCN) , tungsten (W), aluminum (Al), copper (Cu), cobalt (Co), titanium (Ti), tantalum (Ta), nickel (Ni), platinum (Pt), nickel platinum (Ni-Pt), niobium (Nb), niobium nitride (NbN), niobium carbide (NbC), molybdenum (Mo), molybdenum nitride (MoN), molybdenum carbide (MoC), tungsten carbide (WC), rhodium (Rh), palladium (Pd), iridium (Ir), osmium (Os), silver (Ag), gold (Au), zinc (Zn), vanadium (V) and combinations thereof, but the concept and scope of the present invention are not limited thereto. The conductive metal oxides and conductive metal oxynitrides may include oxidized forms of the above materials, but the concept and scope of the present invention are not limited thereto.

[0093] The peripheral spacer structure PSP may include a stack structure of a nitride spacer 501 , a first oxide spacer 108 , and a second oxide spacer 109 .

[0094] The core spacer structure CSP may include a stack structure of a nitride spacer 501 ′ and a second oxide spacer 109 .

[0095] refer to Fig.14 , the peripheral spacer structure PSP may include a stack structure of a nitride spacer 501, a low-k spacer 201, and an oxide spacer 109. For example, the low-k spacer 201 may include one selected from the group consisting of SiBN, SiBCN, SiCO, and SiCON.

[0096] The core spacer structure CSP may include a stack structure of a nitride spacer 501 ′ and an oxide spacer 109 .

[0097] refer to Fig.15 , the peripheral spacer structure PSP may include a stack structure of a first nitride spacer 501 , an oxide spacer 108 , and a second nitride spacer 301 .

[0098] The core spacer structure CSP may include a stack structure of a first nitride spacer 501 ′ and a second nitride spacer 301 .

[0099] In particular, according to an embodiment of the present invention, the nitride spacer 501 of the peripheral spacer structure PSP may be an offset spacer disposed only on both sidewalls of the peripheral conductive pattern PG. Moreover, in the core spacer structure CSP, the nitride spacer 501' may be a buffer spacer that covers not only both sidewalls of each conductive pattern but also portions of the substrate 101 between the conductive patterns.

[0100] refer to Fig.16 , the peripheral spacer structure PSP may include a stack structure of nitride spacers 501 , oxide spacers 108 , and low-k spacers 401 .

[0101] The core spacer structure CSP may include a stack structure of a nitride spacer 501' and a low-k spacer 401. For example, the low-k spacer 401 may include one selected from the group consisting of SiBN, SiBCN, SiCO, and SiCON.

[0102] FIG. 17A to FIG. 17E is a cross-sectional view illustrating one example of a method for manufacturing a semiconductor device including a buffer spacer according to one embodiment of the present invention. FIG. 17A to FIG. 17E Description for manufacturing Figure 1 The method of the semiconductor device shown in FIG. 1 and except for the type of spacer material, the process can be used to manufacture Figures 2 to 4 The method is the same as the semiconductor device shown in FIG.

[0103] refer to Fig.17A In the substrate 11 , the isolation layer 12 may divide the substrate 11 into a peripheral region PERI and a core region CORE, and define an active region.

[0104] The substrate 11 may be a material suitable for semiconductor processing. The substrate 11 may include a semiconductor substrate. The substrate 11 may be formed of a silicon-containing material. The substrate 11 may include silicon, single crystal silicon, polycrystalline silicon, amorphous silicon, silicon germanium, single crystal silicon germanium, polycrystalline silicon germanium, carbon-doped silicon, a combination thereof, or a multilayer thereof. The substrate 11 may also include other semiconductor materials, such as germanium. The substrate 11 may include a III / V semiconductor substrate, such as a compound semiconductor substrate, such as GaAs. The substrate 11 may include a silicon-on-insulator (SOI) substrate.

[0105] Subsequently, a peripheral conductive pattern PG and a core conductive pattern CG may be formed over the substrate in the peripheral region PERI and the core region CORE, respectively. The peripheral conductive pattern PG and the core conductive pattern CG may have the same stack structure.

[0106] The line width of the peripheral conductive pattern PG and the line width of the core conductive pattern CG may be different or the same. For example, in one embodiment, as the core region adjacent to the cell region becomes smaller due to the miniaturization of the semiconductor device, the distance Dp between the peripheral conductive patterns PG may be longer than the distance Dc between the core conductive patterns CG (Dp>Dc).

[0107] The peripheral conductive pattern PG and the core conductive pattern CG may include a stacked structure of the same material. In other words, the peripheral conductive pattern PG and the core conductive pattern CG may be formed simultaneously by sequentially stacking layers of the same material and patterning them once. The peripheral conductive pattern PG and the core conductive pattern CG may be formed as a stacked structure of a gate dielectric layer 13, a first gate electrode 14, a second gate electrode 15, and a gate hard mask 16, and the gate dielectric layer 13, the first gate electrode 14, the second gate electrode 15, and the gate hard mask 16 are stacked above the substrate 11 in the peripheral region PERI and the core region CORE, respectively, in the order described.

[0108] The gate dielectric layer 13 may include a dielectric material. For example, the gate dielectric layer 13 may include silicon oxide. According to another embodiment of the present invention, the gate dielectric layer 13 may include a high-k material.

[0109] The first gate electrode 14 and the second gate electrode 15 may include a conductive material. The first gate electrode 14 may include a semiconductor material. For example, the first gate electrode 14 may include polysilicon, but the concept and scope of the present invention are not limited thereto. The second gate electrode 15 may include a metal material. For example, the gate electrode 15 may include tungsten or a tungsten-containing material, but the concept and scope of the present invention are not limited thereto.

[0110] The gate hard mask 16 may include a dielectric material. The gate hard mask 16 may be provided to protect the upper surface of the second gate electrode 15 and pattern the gate dielectric layer 13, the first gate electrode 14, and the second gate electrode 15. The gate hard mask 16 may be formed of a material having an etching selectivity with respect to the gate dielectric layer 13, the first gate electrode 14, and the second gate electrode 15. For example, the gate hard mask 16 may include silicon nitride.

[0111] Subsequently, a nitride layer 17 may be formed along the outline of the entire structure including the peripheral conductive pattern PG and the core conductive pattern CG.

[0112] refer to Fig. 17B , a first oxide layer 18A may be formed over the nitride layer 17 .

[0113] refer to Fig. 17C , the first oxide layer 18A in the peripheral region PERI (reference Fig. 17B ) is formed over the core opening mask 19. The core opening mask 19 may be formed of, for example, a photoresist.

[0114] Subsequently, the first oxide layer 18A of the core region CORE may be removed (see Fig. 17B ). Therefore, the first oxide layer 18B may remain only in the peripheral region PERI.

[0115] refer to Fig.17D A second oxide layer 20A may be formed over the nitride layer 17 of the core region CORE and the first oxide layer 18B of the peripheral region PERI.

[0116] refer to Fig.17E , spacer etching may be performed. As a result of the spacer etching, a peripheral spacer structure PSP may be formed on both sidewalls of the peripheral conductive pattern PG, in which the buffer nitride spacer 17, the first oxide spacer 18, and the second oxide spacer 20 are stacked. Also, a core spacer structure CSP may be formed on both sidewalls of the core conductive pattern CG, in which the buffer nitride spacer 17 and the second oxide spacer 20 are stacked.

[0117] As described above, according to an embodiment of the present invention, a spacer material having an etching selectivity can be applied to form a spacer structure that is independently optimized for the requirements of the peripheral region PERI and the core region CORE. In particular, by forming the total thickness of the core spacer structure CSP to be less than the total thickness Wp of the peripheral spacer structure PSP, the mismatch of the sense amplifier transistor based on the change of ion implantation can be reduced.

[0118] 18A to 18F is a cross-sectional view illustrating one example of a method for manufacturing a semiconductor device including an offset spacer according to one embodiment of the present invention. 18A to 18F Description for manufacturing Figure 5 The method of the semiconductor device shown in FIG. 1 and except for the type of spacer material, the process can be used to manufacture Figures 6 to 8 The method is the same as the semiconductor device shown in FIG.

[0119] refer to Fig.18A In the substrate 11 , the isolation layer 12 may divide the substrate 11 into a peripheral region PERI and a core region CORE, and define an active region.

[0120] The substrate 11 may be a material suitable for semiconductor processing. The substrate 11 may include a semiconductor substrate. The substrate 11 may be formed of a silicon-containing material. The substrate 11 may include silicon, single crystal silicon, polycrystalline silicon, amorphous silicon, silicon germanium, single crystal silicon germanium, polycrystalline silicon germanium, carbon-doped silicon, a combination thereof, or a multilayer thereof. The substrate 11 may also include other semiconductor materials, such as germanium. The substrate 11 may include a III / V semiconductor substrate, such as a compound semiconductor substrate, such as GaAs. The substrate 11 may include a silicon-on-insulator (SOI) substrate.

[0121] Subsequently, a peripheral conductive pattern PG and a core conductive pattern CG may be formed over the substrate in the peripheral region PERI and the core region CORE, respectively. The peripheral conductive pattern PG and the core conductive pattern CG may have the same stack structure.

[0122] The line width of the peripheral conductive pattern PG and the line width of the core conductive pattern CG may be different or the same. For example, in one embodiment, as the core region adjacent to the cell region becomes smaller due to the miniaturization of the semiconductor device, the distance Dp between the peripheral conductive patterns PG may be longer than the distance Dc between the core conductive patterns CG (Dp>Dc).

[0123] The peripheral conductive pattern PG and the core conductive pattern CG may include a stacked structure of the same material. In other words, the peripheral conductive pattern PG and the core conductive pattern CG may be formed simultaneously by sequentially stacking layers of the same material and patterning them once. The peripheral conductive pattern PG and the core conductive pattern CG may be formed as a stacked structure of a gate dielectric layer 13, a first gate electrode 14, a second gate electrode 15, and a gate hard mask 16, and the gate dielectric layer 13, the first gate electrode 14, the second gate electrode 15, and the gate hard mask 16 are stacked above the substrate 11 in the peripheral region PERI and the core region CORE, respectively, in the order described.

[0124] The gate dielectric layer 13 may include a dielectric material. For example, the gate dielectric layer 13 may include silicon oxide. According to another embodiment of the present invention, the gate dielectric layer 13 may include a high-k material.

[0125] The first gate electrode 14 and the second gate electrode 15 may include a conductive material. For example, the first gate electrode 14 may include a semiconductor material such as polysilicon. For example, the second gate electrode 15 may include a metal material such as tungsten or a tungsten-containing material. However, the present invention is not limited thereto. The second gate electrode 15 may include other conductive materials such as cobalt or ruthenium.

[0126] The gate hard mask 16 may include a dielectric material. The gate hard mask 16 may be provided to protect the upper surface of the second gate electrode 15 and pattern the gate dielectric layer 13, the first gate electrode 14, and the second gate electrode 15, and the gate hard mask 16 may be formed of a material having an etching selectivity with respect to the gate dielectric layer 13, the first gate electrode 14, and the second gate electrode 15. For example, the gate hard mask 16 may include silicon nitride.

[0127] Subsequently, a nitride layer 31A may be formed along the outline of the entire structure including the peripheral conductive pattern PG and the core conductive pattern CG.

[0128] refer to Fig.18B , the nitride layer 31A in the core region CORE (see Fig.18A ) is formed on the outer surface of the substrate 10, and the outer surface of the substrate 10 opens the outer surface of the outer surface PERI. The outer surface of the substrate 10 can be formed of, for example, a photoresist.

[0129] Subsequently, spacer etching may be performed to form offset nitride spacers 31 on both sidewalls of the peripheral conductive pattern PG. The substrate 11 between the peripheral conductive patterns PG may be exposed by the spacer etching. At the same time, the nitride layer 31A above the peripheral conductive pattern PG may be etched (see Fig.18A ), but the concept and scope of the present invention are not limited thereto. In one embodiment, the nitride layer 31A over the top surface of the peripheral conductive pattern PG may not be etched.

[0130] Therefore, the continuous nitride layer 31B covering the substrate 11 between the core conductive patterns CG may remain in the core region CORE, and the offset nitride spacers 31 disposed only on both sidewalls of the peripheral conductive patterns PG may be formed in the peripheral region PERI.

[0131] Next, the peripheral opening mask 32 may be removed.

[0132] refer to Fig.18C , the first oxide layer 18A may be formed over the nitride layer 31B of the core region CORE and the peripheral conductive pattern PG of the peripheral region PERI.

[0133] refer to Fig.18D , the first oxide layer 18A in the peripheral region PERI (reference Fig.18C ) is formed above a core opening mask 33.

[0134] Subsequently, the first oxide layer 18A of the core region CORE may be removed (see Fig.18C ). The first oxide layer 18B may remain only in the peripheral region PERI.

[0135] Next, the core opening mask 33 may be removed.

[0136] refer to Fig.18E A second oxide layer 20A may be formed over the nitride layer 31B of the core region CORE and the first oxide layer 18B of the peripheral region PERI.

[0137] refer to Fig.18F , spacer etching may be performed. As a result of the spacer etching, a peripheral spacer structure PSP may be formed on both sidewalls of the peripheral conductive pattern PG, in which the offset nitride spacer 31, the first oxide spacer 18, and the second oxide spacer 20 are stacked. Also, a core spacer structure CSP may be formed on both sidewalls of the core conductive pattern CG, in which the buffer nitride spacer 31' and the second oxide spacer 20 are stacked.

[0138] As described above, according to an embodiment of the present invention, a spacer material having an etching selectivity can be applied to form a spacer structure that is independently optimized for the requirements of the peripheral region PERI and the core region CORE. In particular, by forming the total thickness of the core spacer structure CSP to be less than the total thickness Wp of the peripheral spacer structure PSP, the mismatch of the sense amplifier transistor based on the change of ion implantation can be reduced.

[0139] Moreover, since dopants can be directly injected into the substrate 11 by applying the offset nitride spacers 31 remaining only on both sidewalls of the peripheral conductive pattern PG to the peripheral region PERI, it can be advantageous for junction engineering. By applying the first oxide layer as a buffer layer before forming the second oxide spacer, the loss of the substrate 11 during the spacer etching can also be minimized. Therefore, the characteristics of the ring oscillator delay (ROD), which is a main indicator of the operating speed characteristics of the device, can be improved.

[0140] FIG. 19A to FIG. 19H is a cross-sectional view illustrating one example of a method for manufacturing a semiconductor device including an RMG structure according to one embodiment of the present invention. FIG. 19A to FIG. 19H Description for manufacturing Fig. 9 The method of the semiconductor device shown in FIG. 1 and except for the type of spacer material, the process can be used to manufacture Figures 10 to 12 The method of the semiconductor device shown in FIG. is the same. Moreover, in addition to the stacked structure of the conductive pattern, Figures 13 to 16 The semiconductor device shown in the figure may undergo 18A to 18F The same process as shown in FIG. 1 is used to form a spacer structure, and in addition to the spacer structure, Figures 13 to 16 The semiconductor device shown in the figure may undergo FIG. 19F to FIG. 19HThe same process illustrated in FIG. 2 is applied to the RMG structure.

[0141] refer to Fig.19A In the substrate 11 , the isolation layer 12 may divide the substrate 11 into a peripheral region PERI and a core region CORE, and define an active region.

[0142] The substrate 11 may be a material suitable for semiconductor processing. The substrate 11 may include a semiconductor substrate. The substrate 11 may be formed of a silicon-containing material. The substrate 11 may include silicon, single crystal silicon, polycrystalline silicon, amorphous silicon, silicon germanium, single crystal silicon germanium, polycrystalline silicon germanium, carbon-doped silicon, a combination thereof, or a multilayer thereof. The substrate 11 may also include other semiconductor materials, such as germanium. The substrate 11 may include a III / V semiconductor substrate, such as a compound semiconductor substrate, such as GaAs. The substrate 11 may include a silicon-on-insulator (SOI) substrate.

[0143] Subsequently, a peripheral dummy pattern DPG and a core dummy pattern DCG may be formed over the substrate 11 in the peripheral region PERI and the core region CORE, respectively. The peripheral dummy pattern DPG and the core dummy pattern DCG may include the same stack structure.

[0144] The line width of the peripheral dummy pattern DPG and the line width of the core dummy pattern DCG may be different or the same. For example, in one embodiment, as the core region adjacent to the cell region becomes smaller due to the miniaturization of the semiconductor device, the distance Dp between the peripheral dummy patterns DPG may be longer than the distance Dc between the core dummy patterns DCG (Dp>Dc).

[0145] The peripheral dummy pattern DPG and the core dummy pattern DCG may include a stacked structure of the same material. In other words, the peripheral dummy pattern DPG and the core dummy pattern DCG may be simultaneously formed by sequentially stacking the same material layers and patterning them once. The peripheral dummy pattern DPG and the core dummy pattern DCG may be independently formed as a stacked structure of a gate dielectric layer 41 and a dummy gate electrode 42.

[0146] Subsequently, a nitride layer 17 may be formed along the outline of the entire structure including the peripheral dummy pattern DPG and the core dummy pattern DCG.

[0147] refer to Fig.19B , a first oxide layer 18A may be formed over the nitride layer 17 .

[0148] refer to Fig.19C , the first oxide layer 18A in the peripheral region PERI (reference Fig.19B ) is formed over the core opening mask 19. The core opening mask 19 may be formed of, for example, a photoresist.

[0149] Subsequently, the first oxide layer 18A of the core region CORE may be removed (see Fig.19B ). The first oxide layer 18B may remain only in the peripheral region PERI.

[0150] refer to Fig.19D , the core opening mask 19 may be removed. Subsequently, a second oxide layer 20A may be formed over the nitride layer 17 of the core region CORE and the first oxide layer 18B of the peripheral region PERI.

[0151] refer to Fig.19E , spacer etching may be performed. As a result of the spacer etching, a peripheral spacer structure PSP may be formed on both sidewalls of the peripheral dummy pattern DPG, in which the buffer nitride spacer 17, the first oxide spacer 18, and the second oxide spacer 20 are stacked. Also, a core spacer structure CSP may be formed on both sidewalls of the core dummy pattern DCG, in which the buffer nitride spacer 17 and the second oxide spacer 20 are stacked.

[0152] refer to Fig.19F , an interlayer dielectric layer 61 may be formed to gap-fill the space between the core dummy pattern DCG and the peripheral dummy pattern DPG. The interlayer dielectric layer 61 may be formed by a series of processes as follows: a dielectric material is formed to fill the space between the core dummy pattern DCG and the peripheral dummy pattern DPG, and the dielectric material is etched, with the goal of exposing the upper surface of the core dummy pattern DCG and the upper surface of the peripheral dummy pattern DPG. The interlayer dielectric layer 61 may include a material having an etching selectivity relative to the dummy gate electrode 42. The interlayer dielectric layer 61 may include, for example, one selected from silicon oxide, silicon nitride, and silicon oxynitride.

[0153] refer to Figure 19G , the core dummy pattern DCG and the peripheral dummy pattern DPG can be removed (see Fig.19F ) of the dummy gate electrode 42. Therefore, the recess 62 may be formed in the core dummy pattern DCG (see Figure 19G ) and the peripheral dummy pattern DPG (see Figure 19G Herein, the gate dielectric layer 41 may remain on the bottom surface of the recess 62.

[0154] refer to Fig.19H, a core RMG structure CG and a peripheral RMG structure PG may be formed by gap-filling the recesses 62 of the core region CORE and the peripheral region PERI with the high-k layer 52 and the gate electrode 53, respectively. The upper surface of the core RMG structure CG and the upper surface of the peripheral RMG structure PG may be set at the same level as the upper surface of the interlayer dielectric layer 61. To this end, the following series of processes may be performed: a high-k material is deposited along the contour of the entire structure including the recesses of the core region CORE and the peripheral region PERI, a conductive material filling the recess is formed above the high-k material, and then the high-k material and the conductive material are etched with the upper surface of the interlayer dielectric layer 61 as a target.

[0155] The high-k layer 52 may be formed to cover the recess 62 (see Figure 19G ) bottom surface and inner side surface. High-k layer 52 may include a high-k material having a higher dielectric constant than silicon oxide. For example, high-k layer 52 may include at least one of the following: boron nitride, hafnium oxide, hafnium silicon oxide, hafnium aluminum oxide, lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, yttrium oxide, aluminum oxide, lead scandium tantalum oxide, and lead zinc niobate.

[0156] The gate electrode 53 may include at least one of the following: a metal, a metal alloy, a conductive metal nitride, a metal silicide, a doped semiconductor material, a conductive metal oxide, and a conductive metal oxynitride. The gate electrode 53 may be, for example, titanium nitride (TiN), tantalum carbide (TaC), tantalum nitride (TaN), titanium silicon nitride (TiSiN), tantalum silicon nitride (TaSiN), tantalum titanium nitride (TaTiN), titanium aluminum nitride (TiAlN), tantalum aluminum nitride (TaAlN), tungsten nitride (WN), ruthenium (Ru), titanium aluminum (TiAl), titanium aluminum carbonitride (TiAlC-N), titanium aluminum carbide (TiAlC), titanium carbide (TiC), tantalum carbonitride (TaCN), tungsten (W), aluminum (Al), copper (Cu), cobalt (Co), titanium (Ti), tantalum (Ta), nickel (Ni), platinum (Pt), nickel-platinum (Ni-Pt), niobium (Nb), niobium nitride (NbN), niobium carbide (NbC), molybdenum (Mo), molybdenum nitride (MoN), molybdenum carbide (MoC), tungsten carbide (WC), rhodium (Rh), palladium (Pd), iridium (Ir), osmium (Os), silver (Ag), gold (Au), zinc (Zn), vanadium (V) and combinations thereof, but the concept and scope of the present invention are not limited thereto. The conductive metal oxides and conductive metal oxynitrides may include oxidized forms of the above materials, but the concept and scope of the present invention are not limited thereto.

[0157] As described above, according to an embodiment of the present invention, a spacer material having an etching selectivity can be applied to form a spacer structure that is independently optimized for the requirements of the peripheral region PERI and the core region CORE. In particular, by forming the total thickness of the core spacer structure CSP to be less than the total thickness Wp of the peripheral spacer structure PSP, the mismatch of the sense amplifier transistor based on the change of ion implantation can be reduced.

[0158] According to an embodiment of the present invention, the thickness of the spacer formed in the core region and the peripheral region may be binary, so that the spacer may have an optimal thickness adjusted for each region.

[0159] According to an embodiment of the present invention, the reliability of a semiconductor device can be ensured by forming a spacer to have an optimized thickness in a core region and a peripheral region.

[0160] While the present invention has been described with respect to the specific embodiments, it will be apparent to those skilled in the art that various changes and modifications may be made without departing from the spirit and scope of the invention as defined in the following claims.

Claims

1. A semiconductor device comprising: a substrate comprising a peripheral region and a core region; a first conductive pattern disposed over the substrate in the peripheral region; a second conductive pattern disposed over the substrate in the core region; a first spacer structure formed on both sidewalls of the first conductive pattern; as well as A second spacer structure is formed on both sidewalls of the second conductive pattern, the second spacer structure having a thickness smaller than a total thickness of the first spacer structure. 2 . The semiconductor device of claim 1 , wherein the first spacer structure and the second spacer structure comprise buffer spacers. 3 . The semiconductor device according to claim 1 , wherein the first spacer structure and the second spacer structure have different stack structures.

4. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stack structure of a buffer nitride spacer, a first oxide spacer, and a second oxide spacer, and The second spacer structure includes a stack structure of the buffer nitride spacer and the second oxide spacer.

5. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stacked structure of a buffer nitride spacer, a low-k spacer, and an oxide spacer, and The second spacer structure includes a stack structure of the buffer nitride spacer and the oxide spacer.

6. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stack structure of a buffer first nitride spacer, an oxide spacer, and a second nitride spacer, and The second spacer structure includes a stack structure of the buffer first nitride spacer and the second nitride spacer.

7. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stacked structure of a buffer nitride spacer, an oxide spacer, and a low-k spacer, and The second spacer structure includes a stack structure of the buffer nitride spacer and the low-k spacer. 8 . The semiconductor device of claim 1 , wherein the first spacer structure comprises an offset spacer.

9. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stacked structure of an offset nitride spacer, a first oxide spacer, and a second oxide spacer, and The second spacer structure includes a stack structure of a buffer nitride spacer and the second oxide spacer.

10. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stacked structure of an offset nitride spacer, a low-k spacer, and an oxide spacer, and The second spacer structure includes a stack structure of a buffer nitride spacer and the oxide spacer.

11. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stacked structure of an offset first nitride spacer, an oxide spacer, and a second nitride spacer, and The second spacer structure includes a stack structure of a buffer first nitride spacer and a second nitride spacer.

12. The semiconductor device according to claim 1, wherein the first spacer structure comprises a stacked structure of offset nitride spacers, oxide spacers, and low-k spacers, and The second spacer structure includes a stack structure of a buffer nitride spacer and the low-k spacer. 13 . The semiconductor device of claim 1 , wherein the first conductive pattern and the second conductive pattern comprise planar gate patterns. 14 . The semiconductor device according to claim 1 , wherein the first conductive pattern and the second conductive pattern include a replacement metal gate (RMG) structure.

15. A method for manufacturing a semiconductor device, comprising: providing a substrate including a core region and a peripheral region; forming a first conductive pattern over the peripheral region and a second conductive pattern over the core region; as well as A first spacer structure is formed on both sidewalls of the first conductive pattern and a second spacer structure is formed on both sidewalls of the second conductive pattern, the first spacer structure and the second spacer structure having different total thicknesses.

16. The method according to claim 15, wherein the forming of the first conductive pattern and the second conductive pattern comprises: forming a dielectric material layer over the substrate in the peripheral region and the core region; forming a semiconductor material layer over the dielectric material layer; forming a conductive material layer above the semiconductor material layer; forming a hard mask layer over the conductive material layer; forming a mask pattern over the hard mask layer in the peripheral region and the core region; The hard mask layer, the conductive material layer, the semiconductor material layer, and the dielectric material layer of the peripheral region and the core region are sequentially etched using the mask pattern.

17. The method of claim 15, wherein the first spacer structure and the second spacer structure comprise buffer spacers.

18. The method of claim 15, wherein the forming of the first spacer structure and the second spacer structure comprises: forming a first spacer layer along an outline of the entire surface of the semiconductor device including the first conductive pattern and the second conductive pattern; forming a second spacer layer over the first spacer layer; forming a core opening mask over the second spacer layer in the peripheral region to open the core region; removing the second spacer layer from the core region; forming a third spacer layer over the second spacer layer in the peripheral region and the first spacer layer in the core region; as well as Spacer etching is performed on the third spacer layer and the second spacer layer of the peripheral region and on the third spacer layer of the core region.

19. The method of claim 18, wherein the first spacer layer comprises a nitride layer, and The second spacer layer and the third spacer layer include oxide layers.

20. The method of claim 18, wherein the first spacer layer comprises a nitride layer, and The second spacer layer includes a low-k layer, and The third spacer layer includes an oxide layer.

21. The method of claim 18, wherein the first spacer layer comprises a nitride layer, and The second spacer layer includes an oxide layer, and The third spacer layer includes a nitride layer.

22. The method of claim 18, wherein the first spacer layer comprises a nitride layer, and The second spacer layer includes an oxide layer, and The third spacer layer includes a low-k layer.

23. The method of claim 15, wherein the first spacer structure and the second spacer structure comprise offset spacers.

24. The method of claim 15, wherein the forming of the first spacer structure and the second spacer structure comprises: forming a first spacer layer along an outline of the entire surface of the semiconductor device including the first conductive pattern and the second conductive pattern formed over the substrate in the peripheral region and the core region; forming a peripheral opening mask over the substrate in the core region to open the peripheral region; forming an offset first spacer by etching the first spacer layer of the peripheral region, the offset first spacer remaining only on the sidewall of the first conductive pattern; forming a second spacer layer over the first spacer layer in the core region and the first conductive pattern in the peripheral region; forming a core opening mask over the second spacer layer in the peripheral region to open the core region; removing the second spacer layer from the core region; forming a third spacer layer over the first spacer layer in the core region and the second spacer layer in the peripheral region; as well as Spacer etching is performed on the third spacer layer and the second spacer layer of the peripheral region and on the third spacer layer and the first spacer layer of the core region.

25. The method of claim 24, wherein the first spacer layer comprises a nitride layer, and The second spacer layer and the third spacer layer include oxide layers.

26. The method of claim 24, wherein the first spacer layer comprises a nitride layer, and The second spacer layer includes a low-k layer, and The third spacer layer includes an oxide layer.

27. The method of claim 24, wherein the first spacer layer comprises a nitride layer, and The second spacer layer includes an oxide layer, and The third spacer layer includes a nitride layer.

28. The method of claim 24, wherein the first spacer layer comprises a nitride layer, and The second spacer layer includes an oxide layer, and The third spacer layer includes a low-k layer.

29. A method for manufacturing a semiconductor device, comprising: providing a substrate including a core region and a peripheral region; forming a first dummy pattern over the substrate in the peripheral region; forming a second dummy pattern over the substrate in the core region; forming a first spacer structure on both sidewalls of the first dummy pattern and a second spacer structure on both sidewalls of the second dummy pattern, the second spacer structure having a different total thickness from the first spacer structure; forming an interlayer dielectric layer, wherein the interlayer dielectric layer fills a gap between the first dummy pattern and the second dummy pattern; forming recesses in the core region and the peripheral region by removing the first dummy pattern and the second dummy pattern; The RMG structure is formed by depositing a high-k layer and a conductive material layer in the recesses of the core region and the peripheral region, The first spacer structure and the second spacer structure have different total thicknesses.

30. The method of claim 29, wherein a total thickness of the first spacer structure is greater than a total thickness of the second spacer structure.

31. The method according to claim 29, wherein the first spacer structure comprises a stacked structure of a buffer nitride spacer, a first oxide spacer, and a second oxide spacer, and The second spacer structure includes a stack structure of the buffer nitride spacer and the second oxide spacer.

32. The method according to claim 29, wherein the first spacer structure comprises a stacked structure of a buffer nitride spacer, a low-k spacer, and an oxide spacer, and The second spacer structure includes a stack structure of the buffer nitride spacer and the oxide spacer.

33. The method according to claim 29, wherein the first spacer structure comprises a stack structure of a buffer first nitride spacer, an oxide spacer, and a second nitride spacer, and The second spacer structure includes a stack structure of the buffer first nitride spacer and a second nitride spacer.

34. The method according to claim 29, wherein the first spacer structure comprises a stack structure of a buffer nitride spacer, an oxide spacer, and a low-k spacer, and The second spacer structure includes a stack structure of the buffer nitride spacer and the low-k spacer.

35. The method according to claim 29, wherein the first spacer structure comprises a stacked structure of an offset nitride spacer, a first oxide spacer, and a second oxide spacer, and The second spacer structure includes a stack structure of a buffer nitride spacer and the second oxide spacer.

36. The method of claim 29, wherein the first spacer structure comprises a stacked structure of offset nitride spacers, low-k spacers, and oxide spacers, and The second spacer structure includes a stack structure of a buffer nitride spacer and the oxide spacer.

37. The method according to claim 29, wherein the first spacer structure comprises a stacked structure of an offset first nitride spacer, an oxide spacer, and a second nitride spacer, and The second spacer structure includes a stack structure of a buffer first nitride spacer and the second nitride spacer.