Magnetic tunnel junction and magnetic memory cell

By stacking the composite layer structure of the oxide conduction layer and the interface energy enhancement layer in the magnetic tunnel junction, the problem of reducing the storage time of small-size MTJ data is solved, and a longer data holding time is achieved.

CN119012896APending Publication Date: 2024-11-22ZHEJIANG HIKSTOR TECHOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310582712.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

With the miniaturization of the size of the magnetic tunnel junction (MTJ) device, the data storage time is reduced sharply, and data storage time needs to be improved by optimizing the MTJ structure.

Method used

By stacking the composite layer structure of the oxide conducting layer and the interface energy enhancement layer on the magnetic recording layer, the interface perpendicular magnetic anisotropy density of the MTJ is improved, and the stacked structure of the free layer is optimized.

Benefits of technology

The data retention time of small-size MTJ is significantly improved, and the data retention time is extended by enhancing the perpendicular magnetic anisotropy performance density of the interface.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119012896A_ABST
    Figure CN119012896A_ABST
Patent Text Reader

Abstract

The invention provides a magnetic tunnel junction and a magnetic storage unit, the magnetic tunnel junction comprises a reference layer, a barrier layer, a free layer and an oxide covering layer, the free layer comprises a magnetic recording layer and one or more composite layer structures which are sequentially stacked along the direction of the magnetic recording layer away from the barrier layer, and each composite layer structure comprises an oxide conducting layer and an interface energy enhancing layer, wherein the oxide conducting layer closest to the magnetic recording layer is adjacent to the magnetic recording layer, and the interface between the oxide conducting layer and the interface energy enhancement layer is used for improving the interface perpendicular magnetic anisotropy energy density of the whole free layer. According to the invention, the data retention time of the small-size magnetic tunnel junction can be prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of magnetic memory, and in particular to a magnetic tunnel junction and a magnetic memory unit. Background Art

[0002] Spin-transfer torque magnetic random access memory (STT-MRAM) is a highly promising non-volatile memory, whose core structure is a magnetic tunnel junction (MTJ), including a free layer (FL), a barrier layer (TB), a reference layer (RL) and a pinned layer (PL). Compared with traditional memory, STT-MRAM has better scalability and can further improve storage density.

[0003] As the device size shrinks, the data retention time of the MTJ (which can be represented by the thermal stability factor Δ) will decrease sharply, so it is necessary to improve the data retention time by optimizing the structure of the MTJ. Summary of the invention

[0004] In order to solve the above problems, the present invention provides a magnetic tunnel junction and a magnetic storage unit, which improve the data retention time of a small-size MTJ.

[0005] In a first aspect, the present invention provides a magnetic tunnel junction, comprising:

[0006] Reference layer;

[0007] Barrier layer;

[0008] A free layer, wherein the free layer comprises a magnetic recording layer, the magnetic recording layer is located on a surface of the barrier layer away from the reference layer, the magnetization direction of the magnetic recording layer is the same as or opposite to the magnetization direction of the reference layer, and is used to realize data storage;

[0009] The free layer further comprises one or more composite layer structures stacked in sequence along the direction in which the magnetic recording layer is away from the barrier layer, the composite layer structure comprising an oxide conductive layer and an interface energy enhancement layer, wherein the oxide conductive layer closest to the magnetic recording layer is adjacent to the magnetic recording layer, and the interface between the oxide conductive layer and the interface energy enhancement layer is used to improve the interface perpendicular magnetic anisotropy energy density of the entire free layer;

[0010] and an oxide capping layer adjacent to an interface energy enhancing layer farthest from the magnetic recording layer.

[0011] Optionally, the interface energy enhancement layer is a single-layer structure, and is made of a ferromagnetic material in which boron (B) atoms account for between 25% and 40%.

[0012] Optionally, the thickness of the interface energy enhancement layer is between 0.2 nm and 0.6 nm, and the saturation magnetization intensity of the interface energy enhancement layer is lower than 100 emu / cc.

[0013] Optionally, the magnetic recording layer is a single-layer structure, and is made of a ferromagnetic material in which boron (B) atoms account for less than 25%.

[0014] Optionally, the thickness of the magnetic recording layer is between 0.9 and 2.2 nm, and the saturation magnetization intensity of the magnetic recording layer is higher than 1000emu / cc.

[0015] Optionally, the material of the oxide conductive layer is MgO, AlO x One of MgAlO and HfO2.

[0016] Optionally, the RA of the oxide conductive layer is less than 1Ωμm 2 .

[0017] Optionally, the magnetic recording layer is a composite magnetic layer including two sub-magnetic layers and a non-magnetic metal spacer layer sandwiched between the two sub-magnetic layers, and the two sub-magnetic layers are made of ferromagnetic material in which boron (B) atoms account for less than 25%.

[0018] Optionally, the interface energy enhancement layer is a composite magnetic layer, including two sub-magnetic layers and a non-magnetic metal spacer layer sandwiched between the two sub-magnetic layers, and the two sub-magnetic layers are made of ferromagnetic materials with boron (B) atoms accounting for between 25% and 40%.

[0019] In a second aspect, the present invention provides a magnetic storage unit, comprising the magnetic tunnel junction provided in the first aspect.

[0020] The magnetic tunnel junction and magnetic storage unit provided by the present invention optimize the stacked structure of the free layer, and stack a composite layer structure including an oxide conductive layer / interface energy enhancement layer on the magnetic recording layer. The composite layer structure can improve the perpendicular magnetic anisotropy energy density of the MTJ interface, thereby improving the data retention time of a small-sized MTJ. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a schematic diagram of the structure of a magnetic tunnel junction according to an embodiment of the present invention;

[0022] Figure 2 This is a schematic diagram of the structure of a magnetic tunnel junction according to an embodiment of the present invention;

[0023] Figure 3 FIG. 4 is a schematic diagram of the structure of a magnetic tunnel junction according to an embodiment of the present invention. DETAILED DESCRIPTION

[0024] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0025] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0026] Some embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.

[0027] An embodiment of the present invention provides a magnetic tunnel junction, such as Figure 1 As shown, the magnetic tunnel junction includes: a reference layer 10, a barrier layer 11, a free layer 12, and an oxide capping layer 13, wherein:

[0028] The free layer 12 is located on a surface of the barrier layer 11 away from the reference layer 10. The free layer 12 includes a magnetic recording layer 121 and one or more composite layer structures stacked in sequence along the direction of the magnetic recording layer 121 away from the barrier layer 11. The magnetic recording layer 121 is located on a surface of the barrier layer 11 away from the reference layer 10. The magnetization direction of the magnetic recording layer 121 is the same as or opposite to the magnetization direction of the reference layer 10, and is used to realize data storage. Figure 1 Two composite layer structures are shown as exemplary illustrations, which are, from bottom to top, the first oxide conductive layer 122, the first interface energy enhancing layer 123, the second oxide conductive layer 124, and the second interface energy enhancing layer 125. The first oxide conductive layer 122 closest to the magnetic recording layer 121 is adjacent to the magnetic recording layer 121, and the interface energy enhancing layer 125 farthest from the magnetic recording layer 121 is adjacent to the oxide capping layer 13. The interfaces between the oxide conductive layers 122, 124 and the interface energy enhancing layers 123, 125 are used to improve the interface perpendicular magnetic anisotropy energy density of the entire free layer.

[0029] like Figure 2 As shown, Figure 2 In the structure of the magnetic tunnel junction shown, the free layer structure is a structure in which n (n is an integer greater than or equal to 2) oxide conductive layer / interface energy enhancement layer composite layers are stacked on the magnetic recording layer 121 .

[0030] Furthermore, in one embodiment, the interface energy enhancement layer (e.g., the first interface energy enhancement layer 123, the second interface energy enhancement layer 125) is a single-layer structure, and a ferromagnetic material with a boron (B) atomic ratio between 25% and 40% is used, such as CoFeB and FeB alloy. When the B atom ratio is high, the interface oxidation caused by the oxide conductive layer can be effectively alleviated, which is beneficial to control the thickness of the interface energy enhancement layer. The thickness of the interface energy enhancement layer needs to be as thin as possible, which can be between 0.2 and 0.6 nm, and the saturation magnetization of the interface energy enhancement layer is less than 100emu / cc. Emu represents magnetization, and cc represents cubic centimeters. It should be noted that in addition to the thickness of the interface energy enhancement layer itself, the saturation magnetization of the interface energy enhancement layer can also be controlled by the oxide conductive layer.

[0031] Further, in one embodiment, the magnetic recording layer 121 is a single-layer structure, and is made of a ferromagnetic material in which the boron (B) atoms account for less than 25%, for example, one or any combination of the following materials: CoFeB, FeB, CoFe, CoFeAl. The function of the magnetic recording layer is to store data, and its thickness needs to be greater than the interface energy enhancement layer, and can be between 0.9 and 2.2 nm. The saturation magnetization of the magnetic recording layer is higher than 1000emu / cc.

[0032] It should be emphasized here that in the present application, although the magnetic recording layer and the interface energy enhancement layer are both ferromagnetic materials, the thickness of the magnetic recording layer is higher than that of the single interface energy enhancement layer, and the boron atom content is different, and the saturation magnetization is different. Therefore, the function of the interface energy enhancement layer in the present application is not equivalent to the magnetic recording layer. In the present application, due to the thin thickness of the interface energy enhancement layer itself and the effect of the interface dead layer (dead layer, the saturation magnetization of the interface energy enhancement layer will be reduced due to the fact that some atomic layers at the magnetic interface do not show magnetism, so it is expressed as a dead layer, and the corresponding saturation magnetization will be reduced), the saturation magnetization Ms of the interface energy enhancement layer is lower than 100emu / cc. Therefore, when the magnetization is reversed, the interface energy enhancement layer hardly contributes to the magnetic moment, and its role is to provide a strong interface perpendicular magnetic anisotropy through the interface of the multi-stacked interface energy enhancement layer / oxide conduction layer composite layer structure, and to assist in improving the perpendicular magnetic anisotropy (high Hk) of the free layer through strong interlayer coupling.

[0033] In addition, in this application, the combination of low Ms ultra-thin interface energy enhancement layer / oxide conduction layer can be infinitely stacked under the premise of consistent flipping, greatly improving the perpendicular magnetic anisotropy. Empirically, the coupling strength increases as the thickness of the coupling layer decreases. Since the thickness of the interface energy enhancement layer and the oxide conduction layer is thin, the interlayer coupling strength is strong. After measurement, the interlayer coupling energy density Jex*t of the interface energy enhancement layer / oxide conduction layer is higher than 0.4mJ / m 2 Therefore, for a small-sized MTJ, high-speed switching of the free layer can be achieved without relying on the magnetostatic coupling provided at an extremely small size.

[0034] Furthermore, in one embodiment, the material of the oxide conductive layer (eg, the first oxide conductive layer 122, the second oxide conductive layer 124) is MgO, AlO x , MgAlO, HfO2. The oxide conduction layer provides interface magnetic anisotropy for the interface energy enhancement layer on the one hand, and enhances the magnetic coupling between neighboring interface energy enhancement layers on the other hand, ultimately achieving an improvement in the interface perpendicular magnetic anisotropy of the free layer. In order to ensure strong interlayer coupling, the oxide conduction layer also needs to be made as thin as possible. The thickness of a single oxide conduction layer is much smaller than that of the barrier layer, so the RA contributed by the oxide conduction layer is very small, and has little effect on the resistance of the MTJ, RA < 1Ωμm 2 RA is the product of resistance and junction area.

[0035] Further, in one embodiment, if Figure 3 As shown, the magnetic recording layer 121 is a composite magnetic layer, including two sub-magnetic layers and a non-magnetic metal spacer layer sandwiched between the two sub-magnetic layers. The two sub-magnetic layers are made of ferromagnetic materials with a boron (B) atomic ratio of less than 25%. The non-magnetic metal spacer layer can be one or any combination of W, Mo, Ta, and Hf. The thickness of the magnetic recording layer 121 of the composite magnetic layer structure needs to be between 0.9 and 2.2 nm.

[0036] A single interface energy enhancement layer can also sample the structure of a composite magnetic layer, including two sub-magnetic layers and a non-magnetic metal spacer layer sandwiched between the two sub-magnetic layers. The two sub-magnetic layers use ferromagnetic materials with boron (B) atoms accounting for between 25% and 40%. The non-magnetic metal spacer layer can be one or any combination of W, Mo, Ta, and Hf. The thickness of the interface energy enhancement layer of the composite magnetic layer structure needs to be between 0.2 and 0.6 nm.

[0037] Of course, it should be noted that in a specific embodiment, the magnetic recording layer is a single magnetic layer or a composite magnetic layer, and the interface energy enhancement layer is a single magnetic layer or a composite magnetic layer, without specific limitation, and can be a combination of various methods.

[0038] The barrier layer 11 and the oxide capping layer 13 in the present application are usually made of MgO, which is beneficial to improving the perpendicular magnetic anisotropy of the device.

[0039] A magnetic tunnel junction of an embodiment of the present invention proposes a new free layer structure, in which a composite layer structure including an oxide conductive layer / interface energy enhancement layer is stacked on a magnetic recording layer. The composite layer structure can improve the perpendicular magnetic anisotropy energy density of the MTJ interface, thereby improving the data retention time of a small-size MTJ.

[0040] The following is an analysis of the technical effect produced by the magnetic tunnel junction of the embodiment of the present invention from the principle.

[0041] According to the formula,

[0042]

[0043] Among them, K u *t is the interface perpendicular magnetic anisotropy energy density, which is mainly contributed by the interface between the free layer and the barrier layer. Δ is the thermal stability factor, which is used to characterize the data retention time of the MTJ. s (T) is the saturation magnetization, V is the free layer volume, k B is the Boltzmann constant and T is the temperature.

[0044] From formulas (1) and (2), we can see that by increasing K u *t to increase Δ. The magnetic tunnel junction of the embodiment of the present invention is realized based on this principle.

[0045] On the other hand, an embodiment of the present invention further provides a magnetic storage unit, comprising the magnetic tunnel junction provided by the above embodiment.

[0046] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A magnetic tunnel junction, characterized in that: include: Reference layer; Barrier layer; A free layer, wherein the free layer comprises a magnetic recording layer, the magnetic recording layer is located on a surface of the barrier layer away from the reference layer, the magnetization direction of the magnetic recording layer is the same as or opposite to the magnetization direction of the reference layer, and is used to realize data storage; The free layer further comprises one or more composite layer structures stacked in sequence along the direction in which the magnetic recording layer is away from the barrier layer, the composite layer structure comprising an oxide conductive layer and an interface energy enhancement layer, wherein the oxide conductive layer closest to the magnetic recording layer is adjacent to the magnetic recording layer, and the interface between the oxide conductive layer and the interface energy enhancement layer is used to improve the interface perpendicular magnetic anisotropy energy density of the entire free layer; and an oxide capping layer adjacent to an interface energy enhancing layer farthest from the magnetic recording layer.

2. The magnetic tunnel junction according to claim 1, characterized in that: The interface energy enhancement layer is a single-layer structure, and is made of a ferromagnetic material in which the proportion of boron (B) atoms is between 25% and 40%.

3. The magnetic tunnel junction according to claim 1, characterized in that: The thickness of the interface energy enhancement layer is between 0.2 nm and 0.6 nm, and the saturation magnetization intensity of the interface energy enhancement layer is lower than 100 emu / cc.

4. The magnetic tunnel junction according to claim 1, characterized in that: The magnetic recording layer is a single-layer structure, and is made of a ferromagnetic material in which the boron (B) atoms account for less than 25%.

5. The magnetic tunnel junction according to claim 1, characterized in that: The thickness of the magnetic recording layer is between 0.9 nm and 2.2 nm, and the saturation magnetization intensity of the magnetic recording layer is higher than 1000 emu / cc.

6. The magnetic tunnel junction according to claim 1, characterized in that: The material of the oxide conductive layer is MgO, AlO x One of MgAlO and HfO2.

7. The magnetic tunnel junction according to claim 1, characterized in that: The RA of the oxide conductive layer is less than 1Ωμm 2 .

8. The magnetic tunnel junction according to claim 1, characterized in that: The magnetic recording layer is a composite magnetic layer, including two sub-magnetic layers and a non-magnetic metal spacer layer sandwiched between the two sub-magnetic layers. The two sub-magnetic layers are made of ferromagnetic materials with boron (B) atoms accounting for less than 25%.

9. The magnetic tunnel junction according to claim 1, characterized in that: The interface energy enhancement layer is a composite magnetic layer, including two sub-magnetic layers and a non-magnetic metal spacer layer sandwiched between the two sub-magnetic layers. The two sub-magnetic layers are made of ferromagnetic materials with boron (B) atoms accounting for between 25% and 40%.

10. A magnetic storage unit, characterized in that: The magnetic memory cell comprises a magnetic tunnel junction as claimed in any one of claims 1 to 9.