Method and device for evaluating welding quality of weld seam between end sections of two conductor elements

Through image processing technology, the pixel intensity levels of the welds are divided and compared, which solves the complex and expensive problems of existing welding quality control methods, and achieves a fast, accurate and cost-effective welding quality evaluation, which improves the reliability of the welding process. .

CN119013694AActive Publication Date: 2024-11-22GEHRING TECHNOLOGIES GMBH CO KG
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202380029376.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-01
Filing Date
2023-03-29
Publication Date
2024-11-22
Estimated Expiration
2043-03-29

AI Technical Summary

Technical Problem

Existing welding quality control methods are complex, expensive and error-prone, making it difficult to achieve rapid and accurate evaluation of multiple welds.

Method used

By capturing the image of the weld, using the intensity levels of the pixels to divide into different subsets, and comparing them with the target value or range, weld quality is evaluated, using a non-destructive, simple, and cost-effective approach.

Benefits of technology

It realizes fast, accurate and cost-effective quality control of multiple welds, reduces error rates, and improves the reliability of the welding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119013694A_ABST
    Figure CN119013694A_ABST
Patent Text Reader

Abstract

The invention relates to a method (40) and a device (200) for evaluating the welding quality of a weld seam (14) between end sections of at least two elongate conductor elements (12) welded to one another by irradiating end faces (13) of the end sections.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a method and a device for evaluating the welding quality of a weld seam, in which end sections of at least two elongated conductor elements are welded to one another by irradiating the end faces of the end sections through the weld seam.

[0002] Methods and devices for producing stators are known in the prior art.Stators are used in electrical machines or electromechanical converters, for example in electric motors.

[0003] When producing electromechanical transducers, in particular electric motors, in particular for traction drives, individual winding elements (insertion coils, so-called “hairpins”) are produced which are processed further during further processes to form stator windings.

[0004] In order to achieve a higher efficiency of the electric machine by a higher filling degree, a change was made in hairpin technology from a round conductor cross section to a rectangular conductor cross section. Within the scope of the invention, any conductor cross section can be used, ie for example a round cross section or a rectangular cross section.

[0005] In the context of producing a winding element, the corresponding conductor segment is separated from the continuous material, for example by cutting. The conductor segment is then stripped of insulation at the portion to be welded in a later step. The conductor segment can then be formed into a suitable winding element, for example by bending the conductor segment into a corresponding hairpin. A hairpin usually has two legs connected to each other by a connecting portion (similar to the closed end of a U-shaped hairpin). On the side facing away from the connecting portion, the legs each have a free end. The legs are usually parallel to each other and each have a stripping portion in the region of their ends, in which region the hairpin is later welded.

[0006] A plurality of hairpins can be joined together to form a basket (stator basket), and optionally a paper insulation can be inserted into the stator. The hairpins or the basket are then inserted into the stator and, if necessary, their ends are twisted against each other ("twisted"), which allows the hairpins to be held in the stator core in a positive fit in a certain way. The winding elements or the hairpins can be welded to one another at their ends after positioning on the stator. In order for this welding to be safe and reproducible, the hairpins to be welded together should be positioned in precisely defined positions relative to each other to ensure their desired mutual contact.

[0007] The welding itself is usually done using laser radiation. For this purpose, a corresponding laser beam source and a so-called scanner optics with a camera are usually used. The scanner optics enable the camera to detect the position of the ends of the conductor elements before welding, and the scanner optics also use two movable mirrors to enable a highly dynamic movement of the laser beam on the end faces of the two conductor elements to be welded. The number of conductor elements to be welded per stator is usually in the three-digit range. Defective welding can lead to failure of the stator. Since the quality of the weld depends on many factors, quality control is necessary. The quality standards for the welds can be determined individually, but they usually have in common a certain connection cross-section necessary to ensure the desired current flow.

[0008] Different methods for quality control of welded hairpins are known. This includes, for example, a cross section through the weld. The disadvantage is that this type of quality control is a destructive test and is expensive and time-consuming. For example, it is also known to use optical coherence tomography or a laser sensor for profile measurement to measure the weld bead produced in the weld. The disadvantage is that additional technical equipment is required for this and this measurement is slow and therefore expensive. In JP2019120650A, a transverse image of the welded hairpin is also proposed, i.e. when viewed in the plane of the end face. However, this also requires additional and expensive equipment. In addition, only one hairpin weld can be inspected at any one time. Finally, the measurement of process light during the welding process has been proposed. However, it is difficult to establish an exact correlation between the measured light signal and the welding result.

[0009] In summary, known quality control methods are disadvantageous in many respects; in particular, they are complex and expensive and are prone to errors.

[0010] The invention is based on the object of overcoming these and other disadvantages of the prior art and of providing a method and an apparatus with which a quality control of a weld seam between end sections of at least two elongated conductor elements can be performed in a simple, cost-effective, rapid and precise manner.

[0011] This object is achieved by a method according to claim 1 and a device according to claim 14 .

[0012] The method is therefore a method for evaluating the welding quality of a weld seam between end sections of at least two elongated conductor elements which are welded to one another by irradiating the end faces of the end sections, in particular by irradiating with the aid of a laser.

[0013] The method comprises at least the following steps:

[0014] (a) Capturing an image of the end faces of the conductor elements welded to each other by the weld. Here, the image is recorded from the end faces of the conductor elements and the area captured by the image includes at least the complete surface of the weld on the end faces of the conductor elements. Furthermore, the image is captured at a different intensity level for each pixel of the image. The intensity level is an indicator of the amount of light reflected locally by the recording location when the image was taken. The indicator or the amount of light is a measure of the local orientation of the surface of the weld. In particular, the weld is illuminated with light parallel to the direction in which the image was recorded.

[0015] (b) dividing the image into a first subset of pixels and a second subset of pixels, wherein the intensity level of the pixels in the first subset is greater than a predetermined intensity level threshold, and the intensity level of the pixels in the second subset is less than or equal to the intensity level threshold.

[0016] (c) evaluating the welding quality of the weld by comparing the number and / or position of pixels of the first subset and / or pixels of the second subset with at least one pixel target value and / or pixel target range of the number of pixels of the first subset and / or pixels of the second subset corresponding to a weld of desired quality.

[0017] Therefore, the present invention proposes a method for quality control of the end segments or ends of the welding of two or more conductor elements, by means of which the connection cross section of the weld is evaluated. Quality control is performed by comparing the number of recorded pixels or the recorded pixels of each subset and / or the position of the recorded pixels of each subset with a target value (pixel target value or pixel target range). The method is non-destructive, simple, cost-effective, fast and accurate. For example, quality control may require a certain number of pixels in a subset or a certain pixel spatial distribution in a subset. This will be discussed in more detail below.

[0018] The following explanations relate equally to the method and to the device according to the invention.

[0019] According to the invention, an image of the welded end face of the conductor element is captured, in particular by an image capture device, in particular a camera. The image is taken from the end face of the conductor element and thus shows the weld from above or when viewing the end face of the conductor element or conductor segment vertically.

[0020] From above here means positioned opposite to the end face. The image capture includes at least the entire weld or an area of ​​the size of the desired weld in the expected position. Portions of the surfaces or end faces of the conductor elements and, if applicable, their surroundings may also be part of the captured image.

[0021] The weld seam is usually formed in the shape of a (substantially hemispherical) weld bead. The weld bead is formed after a spherical or spherical weld pool is generated by (laser) irradiation at the end section of the conductor element. Therefore, the solidified weld bead also has a spherical or hemispherical shape.

[0022] The end section of the conductor element extends in the direction of the image capture device and the end face is perpendicular to this direction. The viewing direction of the image capture device is therefore perpendicular to the end face. Typically, the weld seam and its surroundings are illuminated from the direction of the image capture device or camera, i.e. parallel to the direction of its beam path, for which purpose an illumination device can be provided on a corresponding device or can be used as part of the method.

[0023] Illuminating light incident on the weld or the weld bead is reflected thereby and allows the weld bead or its spherical shape or the shape of the weld to be identified in the recorded image. When the illuminating light is reflected, for example if the shape of the weld is predominantly spherical or hemispherical, a different part of this light is reflected depending on the local position on the surface of the weld. Thus, a hemispherical weld bead appears bright in the center of the captured image and darker towards the edge of the captured image. Light directed perpendicularly onto the end face of the conductor element is reflected to a greater extent in the direction of the image capture device used to capture the image at a region of the weld extending parallel to the end face than light falling on adjacent angled regions of the weld.

[0024] Thus, the weld can be seen on the captured image by different intensity levels of the pixels of the image. Advantageously, the intensity levels are the gray levels of a grayscale image. The image can be recorded directly in grayscale or can be converted from a recorded color image into a grayscale image by image processing. As explained, the different intensity levels (in particular gray levels) of the individual pixels in the captured image are caused by different amounts of light reflected from the area where the weld is located and depicted by the image. Depending on the shape of the surface of the weld (in particular the weld bead), a smaller or larger amount of light is reflected back into the beam path of the image capture device at a specific point on the surface, which results in different exposures of the pixels of the image. Thus, the intensity level (or grayscale value) serves not only as an indicator of the amount of reflected light, but also as a measure of the local orientation of the surface of the weld via the amount of reflected light. The local orientation of the surface of the weld (in particular the weld bead) refers to the geometry or shape of the weld, i.e. its extension in different spatial directions.

[0025] Furthermore, according to the invention, the image is divided into a first subset of pixels and a second subset of pixels based on the intensity levels of the pixels and a comparison with previously defined intensity level thresholds, in particular based on reference measurements performed on welds that are considered good, i.e. welds that have a sufficient or satisfactory quality according to a desired criterion. The image can also be divided into further subsets of pixels by specifying a plurality of intensity level thresholds. The division of the image based on defined intensity level thresholds now enables only two (or more, but few) different types or numbers of pixels to be evaluated for evaluating the welding quality. This allows a simplified pixel data processing for simply, quickly and accurately evaluating the welding quality of the weld in subsequent steps of the method.

[0026] If the pixels are divided into multiple subsets, quality control can be performed by comparing the number and / or position of pixels in different subsets with a pixel target value or pixel target range. This can be done using the first subset and the second subset as described herein.

[0027] Preferably, grayscale is used as intensity level and grayscale threshold is used as intensity level threshold. For example, if grayscale is used as intensity level for a grayscale image with 8-bit color depth or 256 steps, each pixel of the grayscale image may have up to 256 different grayscale levels, each of which is caused by a different amount of light reflected onto the camera. By dividing the image into only a first subset of pixels (pixels with intensity levels above the threshold; the intensity levels may be grayscale) and a second subset of pixels (with intensity levels equal to or below the threshold; the intensity levels may be grayscale), each pixel is assigned only one of two (the number of subsets) values, instead of 256 possible grayscale values ​​(where 0 is the minimum value for black or no exposure and 255 is the maximum value for white, highest exposure), where this value is assigned to the first subset or the second subset. The grayscale is an exemplary but preferred choice of intensity level. However, hue may also be selected as intensity level. It is also possible to create subsets with their own thresholds for each color channel.

[0028] When subsets are formed, the captured image may be binarized. This produces a binary image that visualizes the division of the image into pixels of the first subset and pixels of the second subset. The intensity level thresholds may be adjusted individually for different processing parameters.

[0029] The binary image thus generated or the division of the image into the pixels of the first subset and the pixels of the second subset, which can be stored in a table or in a table, for example, now shows the local orientation of the surface of the weld seam (in particular the weld bead) produced by welding based on the number and position of the pixels of the first subset and / or the pixels of the second subset, and allows the welding quality to be evaluated by evaluating the number and / or position (in particular a combination of number and position) of the pixels of the first subset and / or the pixels of the second subset. The position of a pixel here refers to the spatial position in the image or the position of a pixel in the image. The position of a pixel can be specified, for example, by specifying the two-dimensional coordinates of the pixel in the image plane spanned by orthogonal axes or by specifying the quadrant in a grid superimposed on the image. For the evaluation, an optimal pixel range or a target pixel range for the number and / or position of the pixels, which is given in particular for a target weld seam or a weld seam with a high welding quality, is used for comparison with the number and / or position given for the pixels of the first subset and / or the pixels of the second subset in the binary image or in the table.

[0030] The pixel target value may be specified, for example, by a target number of pixels of the first subset or of the second subset, above or below which a properly formed weld is assumed. Thus, a single pixel target value, such as a target number of pixels of a certain subset, defines a quality criterion that can be easily verified. The target number may be a minimum number or a maximum number or an interval bounded by a minimum number and a maximum number.

[0031] The pixel target range may be a specific specification about the location of a subset of pixels in the image. For example, a criterion may be that more or less pixels of a subset must be present in a sub-region of an image.

[0032] A given weld is compared based on its first subset of pixels and / or second subset of pixels with an optimal target performance of these pixels. If there is a sufficiently large consistency as defined by the pixel target range, it can be assessed that the weld quality is sufficient. Otherwise, the weld quality can be judged to be insufficient or faulty.

[0033] For example, the number of pixels in the first subset may be compared with a target value. The number of pixels of the first subset within a certain area in the image may also be compared with a target value. Specifically, it may be provided that pixels in a certain specified area of ​​the image are not considered in the comparison, and for example only the number of pixels of a relevant subset outside this area is considered.

[0034] By evaluating the quality of the welds, it can be determined which welds are acceptable and which welds are not acceptable.

[0035] However, in addition, the proposed method also enables a more detailed specification of the quality based on the identification of other features, in particular the shape of the weld bead. For example, the shape of the weld bead and thus, for example, the symmetry or asymmetry can be determined based on the position and number of pixels of the first subset and / or of the second subset in the image.

[0036] Typically, an assessment of the weld quality of mutually welded conductor elements of a stator of an electric machine, in particular an electric motor, is performed as part of the method according to the invention.

[0037] In particular, the conductor element is a hairpin of a stator of an electric machine, in particular an electric motor. Considering the large number of welds caused by the large number of hairpins on the stator, the method according to the invention enables a particularly cost-effective, fast and reliable quality control of all welds.

[0038] It is possible, within the scope of the invention, that the image is a sub-region of a higher-level image comprising a plurality of welds. The evaluation can then be performed for each image (part of a higher-level image). In this way, a plurality of welds can be evaluated at once with one image.

[0039] A step of cropping the image to a region comprising the weld may be performed, and the evaluation may be performed only in this sub-region. Typically, this sub-region is an image of the end faces of the conductor elements and, if applicable, of the portions of the weld protruding beyond them. If a plurality of welds are present in the image or in a higher-level image, individual regions of each weld may be cropped. This reduces the amount of data to be processed and also allows the method to be performed only in the relevant region of the weld, thus avoiding errors in the evaluation.

[0040] As already explained, it can be provided that a specific area of ​​the image is not taken into account in the evaluation. For example, this can be a central area around the center of the weld (in the case of a spherical weld on two conductor elements). Here, it can generally be assumed that almost all pixels in this sub-area can be assigned to the first subset (strong reflection, bright) if the weld is formed as expected. For example, including these pixels when considering the set of pixels of the first subset can reduce its relative accuracy. For example, the area excluded from the evaluation can be defined as the following area: in this area, the surface of the weld formed as expected is essentially "flat", that is, orthogonal to the viewing direction of the image capture device. In simple terms, this is advantageous because the center of the weld bead appears bright in the image due to the reflection of the illumination light, and the weld bead mainly contains pixels of the first subset or pixels of the second subset assigned to the bright area. If individual pixels in this area are not assigned to the first subset (bright) for various reasons, this generally has no meaning for the surface inclination. If these pixels are taken into account in the analysis, this may make the result less accurate. In other words, by excluding from consideration areas in a weld formed as intended that are almost completely assigned to a subset, the sensitivity of the control in the critical area can be increased.

[0041] The central area is preferably a circular or elliptical area with a predetermined radius, for example, within which a predetermined minimum number of pixels of the first subset (bright) falls when the weld is properly formed, or in which there is a high degree of reflection. A properly formed weld is to be understood as a weld of a specified weld quality, in particular a weld of minimum quality. In welds connecting three or more conductor elements, the central area which is not taken into account in the evaluation is usually elliptical, since the weld is not circular, but elongated.

[0042] For example, a properly formed weld may have a certain number of pixels in the first subset or a certain number of pixels in the first subset outside of an area that is not considered in the evaluation.

[0043] A properly formed weld seam may also have, for example, a certain symmetry in the distribution of pixels of the first and second type (pixel target range).

[0044] A maximum number of pixels of the first subset or of the second subset can be specified, for example, absolutely or relatively with respect to the total number of pixels of the first subset or of the second subset. The maximum number can be determined based on a sample of properly formed welds or welds with sufficient welding quality. For example, in the case of a circular area, which is particularly useful in the case of two conductor elements welded to each other, the radius for the center area can be specified so that, based on the average value or the average of the sample, a minimum amount (e.g. 90%) of all pixels of the first subset or of all pixels of the second subset are located in the cutout center area. Alternatively, if more than two conductor elements are welded to each other and images of them are taken, the shape of the cutout area can be elliptical.

[0045] Preferably, the pixel target value for the number and / or the pixel target range for the position is determined by selecting a minimum connection cross section as a quality feature for the welding quality. This can be done by a separate determination step in the method. This step is based on the recognition that the number and / or the position of the pixels of the first subset and / or the pixels of the second subset are associated with the connection cross section and that the minimum connection cross section can therefore be determined via them.

[0046] Thus, the data by which the number and / or position of the pixels of the first subset and / or the pixels of the second subset are associated with the connection cross section of the weld can advantageously be used to determine a target value for the number of pixels and / or a target range for the positions of pixels. For example, the connection cross sections of different welds can be determined, for example, by cross-sectioning and set relative to the number and / or position of the pixels of the first subset and / or the pixels of the second subset to obtain a database that can be used to determine the target value for the number of pixels and / or the target range for the positions of pixels based on the desired minimum connection cross section.

[0047] In order to determine the quality of the weld, in principle only the number of pixels of the first subset and / or the second subset of pixels may be evaluated, only the position of the pixels of the first subset and / or the second subset of pixels may be evaluated or a combination of the number and the position may be evaluated. In the latter case, the number of pixels of the first subset of pixels and / or the second subset of pixels is taken into account depending on their position on the surface of the weld.

[0048] Advantageously, the weld symmetry of the weld seam can be determined based on the number and position of the pixels of the first subset and / or the pixels of the second subset. Weld symmetry means the symmetry of the weld seam, in particular the weld bead, with respect to one or more imaginary symmetry lines passing through the weld seam, in particular the weld bead. Due to a highly uneven distribution of the pixels of the first subset or the pixels of the second subset on each side of the symmetry line, an asymmetric weld bead shape can be detected. Excessive asymmetry indicates a poor weld quality.

[0049] It can be provided that the weld seam is re-welded as a function of the number and position of the pixels of the first subset and / or of the pixels of the second subset. For example, if an asymmetrical weld bead is detected due to an uneven energy input during welding, a targeted re-welding can be performed to produce a symmetrical weld bead. As a function of the number and position of the pixels of the first subset or of the pixels of the second subset, the geometry of the weld bead can be identified so that this geometry can be used for re-welding so that the desired spherical shape of the weld bead can be subsequently created. On the other hand, if the number of pixels of the first subset or of the pixels of the second subset is too high in the entire edge region of the weld bead, a weld bead that is too flat can be detected so that in this case re-welding can be performed in the entire edge region in order to rework the spherical shape of the weld bead and improve the weld quality. The edge region of the weld bead can be understood as the surface of the end faces of the conductor elements welded to each other minus the previously mentioned, in particular the center region of the cutout. This method not only enables quality control, but also enables simple, fast and precise post-processing of the components to avoid rejection.

[0050] Here, the welding power for the re-welding can be selected as a function of the number and / or position of the pixels of the first subset and / or the pixels of the second subset. This makes it possible to control not only the position but also the intensity of the energy input of the laser beam during the re-welding, thus enabling a weld seam of optimized quality to be produced precisely.

[0051] It is also advantageous if the welding quality of a weld seam on the same component with multiple conductor elements, in particular a stator, and the welding of a different weld seam are evaluated simultaneously. Parallel welding and evaluation enable further time savings in component production. Alternatively, it is also possible to alternate evaluation and welding.

[0052] The object mentioned at the outset is also achieved by a device for evaluating the welding quality of a weld seam between end sections of at least two elongated conductor elements, which are welded to one another by irradiating the end faces of the end sections. The device comprises an image capture device having a beam path. The image capture device is designed to perform step (a) of the method according to the invention.

[0053] Furthermore, the device has at least one data processing system which is configured to carry out steps (b) and (c) of the method according to the invention.

[0054] The apparatus comprises an illumination device configured to illuminate an end face of the conductor element from a direction along a beam path of the image capture device.

[0055] The device further comprises a laser beam source having a laser beam path for performing a welding process for connecting the conductor elements on the end faces of the conductor elements. In particular, the beam path of the image capture device and the beam path of the laser beam are coupled to each other, in particular by means of a beam splitter. Thus, the beam paths are identical. Thus, the image capture device enables an evaluation from the same "perspective" from which the laser also performs its processing.

[0056] When performing the method, the image is therefore preferably captured along the beam path of the laser used for the welding process. The illumination of the weld seam preferably takes place parallel to or along this beam path.

[0057] The device according to the present invention has the same advantages as explained in detail with reference to the method according to the present invention. In addition, the features described herein that have been explained about the method can be equally applied to the device. In particular, the device can be configured to perform the method described herein.

[0058] The invention is described in more detail hereinafter with reference to the drawings, wherein identical or functionally equivalent elements are designated only once with a reference numeral if necessary.

[0059] In the attached picture:

[0060] Figure 1 shows a schematic view of an exemplary embodiment of a device according to the invention;

[0061] Figure 2a , Figure 2b Shown before welding Figure 1 Schematic side view and plan view of two conductor units of a stator;

[0062] Figure 3a , 3b Shows the Figure 2a , Figure 2b Schematic side view and plan view of two conductor units;

[0063] Figure 4 The method for evaluating the Figure 1Schematic representation of the steps of an exemplary embodiment of a method for improving the welding quality of a weld seam on two conductor elements of a stator;

[0064] Figure 5 The method for evaluating the Figure 1 Schematic representation of the steps of an exemplary embodiment of a method for improving the welding quality of another weld seam of two conductor elements of a stator;

[0065] Figure 6 The binary images of the welds welded with different laser powers and the Figure 1 A schematic representation of a weld bead of a weld seam of two conductor elements of a stator of FIG. 1 ; and

[0066] Figure 7 Shown for Figure 1 Schematic representation of multiple welding beads of multiple pairs of conductor elements of a stator and the number of white pixels per welding bead.

[0067] Figure 1 An exemplary embodiment of an apparatus 200 for evaluating the welding quality of a weld 14 is shown (see Figure 3a In the present case, the device 200 is also designed to produce the weld seam 14 by laser beam welding with the aid of a laser beam source 102 and a scanner optics 100 .

[0068] In addition to the beam guide (beam path 114) of the laser beam source 102, the scanner optics 100 also comprises an image capture device 116, which is also referred to below as a camera 116. The beam path 118 of the camera 116 is used to detect the position of two (alternatively more) conductor elements 12 of the component 10 in the present case, which are welded before the actual laser beam welding and therefore before the precise laser beam welding of the free end sections of (in each case) two conductor elements 12 of the component 10 by the beam path 114 of the laser beam source 102.

[0069] In the present case, the component 10 is a stator 10 having a hairpin as a conductor element 12 of an electric motor (I-clips or other plug-in coils are also preferred conductor elements within the scope of the invention). For high electrical conductivity, the conductor element 12 can be made of copper or at least contain copper, for example.

[0070] The beam paths 114, 118 are coaxially superimposed or guided in a common beam path 120 at the beam splitter 106. Here, the beam path 114 of the laser 102 is collimated by the collimating lens 104 in front of the beam splitter 106. One or more movable deflection mirrors 108 of the scanner optical device 100 enable the coaxially combined beam path 120 to be displaced in a plane on the surface of the end section of the conductor element 12. In the beam direction behind the deflection mirror 108, a focusing lens 110 and an additional lighting device 112 of the device 200 are also arranged, which focusing lens can also be designed as a lens package for focusing the beam path 120 on the two end sections of the conductor element 12, and the additional lighting device 112 is used to illuminate the end section of the conductor element 12 for the camera 116.

[0071] The camera 116 of the scanner optical device 100 is not only used for process control of laser beam welding; instead, according to the method 40 described below (see Figure 4 ), which is also used for image recording in the context of assessing the welding quality of the weld seam 14. Alternatively, an additional camera (not shown) can also be used. In addition to the resulting advantages described in more detail below with respect to the method 40, this has the advantage that no additional and expensive equipment is required to implement the inspection of the welding quality; rather, the devices already provided for welding can be used. One or more data processing systems 202 of the device 200, also referred to as computers 202, can already exist or can be added, the function of which will be explained in more detail later.

[0072] Figure 2a Using a pair of elongated conductor elements 12 or hairpins that are still unsoldered, it is shown how light 118a of the beam path 118 of the camera 116 or the lighting device 112 is incident on the surface of the end face 13 of the unsoldered end section of the conductor element 12. This light 118a is reflected back perpendicularly at the end face 13 on the unsoldered end section as light 118b, because the end face 13 of the end section of the conductor element 12 is perpendicular to the direction of the light 118a. Figure 2b A schematic image 20 is shown which is recorded by a camera 116 and shows an illuminated end face 13 of an end section of a conductor element 12 .

[0073] on the other hand, Figure 3a A pair of welded end sections of an elongated conductor element 12 or hairpin is used to illustrate how the light 118a of the beam path 118 of the camera 116 is incident on the end face 13 of the welded end section of the conductor element 12. Figure 2a and Figure 2bIn contrast, the end faces 13 are no longer seen separately here, or have been connected to one another by welding (however, end faces 13 are still mentioned in this text). Here, light 118a irradiates a weld bead 16 of a weld seam 14, which was produced by laser welding using a laser beam source 102 and which connects two end sections of a conductor element 12 to one another at the end face 13. The weld bead 16 is spherical in shape. In this case, since the spherical shape of the weld bead 16 is uniform, a high welding quality can be presented and therefore a large connection cross section between the conductor elements 12 or their ends can be presented. Compared to the case of Figure 2a 16 is reflected back to the camera 116 and is otherwise mainly scattered outwards. The closer the shape of the weld bead 16 is to a spherical shape, the more the surface of the weld bead 16 is inclined towards the direction of incidence of the light 118a, so that less light 118b is reflected back to the camera 116 and is captured by the camera when the image 20 is taken. However, the flatter the weld bead 16 is, the weaker the weld bead and therefore the less stable it is. In the case of a flat weld bead 16, which indicates a poor weld quality due to the small connection cross section of the weld seam 14, more light 118b is reflected onto the camera 116 and captured when the image 20 is taken.

[0074] By means of different proportions or amounts of light reflection, conclusions can be drawn about the shape of the weld bead 16 and thus about the connection cross section of the weld seam 14 produced and thus the weld quality determined by the connection cross section. The method 40 described below utilizes this correlation between the shape of the weld bead 16 and the associated weld quality of the weld seam 14 and the light in the image 20 recorded by the camera 116. Figure 3b An image 20 recorded by camera 116 of end face 13 of a welded end section of conductor element 12 is shown, wherein weld bead 16 is clearly visible and the pixel density of image 20 decreases toward the outer or edge region of weld bead 16 .

[0075] Figure 4 The sequence of an exemplary method 40 according to the present invention for evaluating the welding quality of a pair of conductor elements 12 welded at the end sections of the pair of conductor elements 12 is now shown. The method 40 described here by way of example includes method steps 42, 44, 46, 48, 50, 52 and 54 (see Figure 7 ), wherein some of the method steps listed as previously described in this document are merely advantageous and not absolutely necessary.

[0076] In a first method step 42, an image 20 of the weld seam 14 is recorded by means of a camera 116, which is positioned with its beam path 118 above the weld bead 16 of the weld seam 14 or its weld bead 16. Although only one weld bead 16 or one weld seam 14 is mentioned here and hereinafter, it is also possible to record an image 20 of a larger area of ​​the component 10, which includes a plurality of weld beads 16 or weld seams 14, so that the plurality of weld beads 16 can be evaluated simultaneously at least temporarily with respect to the plurality of weld beads 16 and the method 40 can be carried out particularly quickly.

[0077] The recorded image 20 includes an area that is larger than the weld seam 14, so that the image 20 is cropped in the second method step 44 to obtain an image 22 cropped to the area of ​​the weld seam 14. From above (i.e. from the viewing direction of the camera 116 when the end face 13 is viewed perpendicularly), the individual conductor elements 12 and their end faces 13 are no longer visible, which are only indicated here; instead, the weld bead 16 can be seen from above.

[0078] In a third method step 46, an intensity level threshold is determined for the cropped image 22 in the form of grayscale values ​​(in the case of a color image, color values ​​are also possible); the image 20 is recorded as a grayscale image in method step 40. In the present example, this intensity level threshold determination is used for a subsequent binarization according to a thresholding method in a fourth method step 48.

[0079] Using the determined threshold, the pixels of the cropped image 22 are divided into two subsets. The pixels of the first subset 30 are pixels whose intensity level is greater than the determined intensity level threshold. In a grayscale image, these pixels are bright pixels, or pixels where a lot of light is reflected back toward the camera. The pixels of the second subset 32 ​​are pixels whose intensity level is less than or equal to the intensity level threshold.

[0080] In the threshold image 24, only pixels or regions 18 of the cropped image 22 that are above a determined intensity level threshold are marked for this purpose (pixels of the first subset 30). The remaining pixels in the threshold image 24 are below or at the threshold and belong to the second subset 32 ​​thereof.

[0081] In a fourth method step 48, a binary image 26 is generated having white pixels of the first subset 30 and black pixels of the second subset 32. The intensity level threshold, which in this case is a gray level threshold, can be adjusted individually for different lighting devices 112.

[0082] All pixels above the threshold are grouped as white pixels, while all pixels at or below the threshold are grouped as black pixels. Thus, the "color depth" is reduced. In addition, the colors can be inverted to improve visual recognition for a user monitoring the recognition process.

[0083] The images can also be evaluated without binarization and directly after the threshold analysis.

[0084] In a fifth method step 50, the central region 34 is cut out from the binary image 26 thus obtained, so that a binary image 28 is again cut out. The central region 34 can also be simply excluded from the subsequent evaluation and does not actually have to be cut out. This is because the central region 34 appears bright due to reflections and anyway contains mainly white pixels of the first subset 30, so that it generally does not provide any information about the welding quality of the weld seam 14. The cutout of the central region 34 can be circular here, thereby following the spherical shape of the weld bead 16. The radius of the circular cutout depends on the size of the conductor element 12 or its end section and the welding strategy. When more than 2 conductor elements are connected, an elliptical central region 34 is usually masked out instead of a circular central region. The radius (for the circular central region 34) can be defined in different ways. An example is to use an image 20 of a weld seam 14 with sufficient welding quality and consider how large the radius must be so that a certain amount (for example 90%) of all white pixels of the first subset 30 are located in the circular cutout. Thereby, an average value can be formed, which can then be defined as the radius of the circular center region 34. Advantageously, the amount of data to be processed by the method 40 can be reduced in this way.

[0085] Then, in a sixth method step 52, the number A of white pixels or pixels of the first subset 30 in the cropped binary image 28 can be counted. Figure 4 In this example of the weld 14 in the cropped binary image 28 of FIG. 5 , the number of white pixels in the first subset 30 is A=508.

[0086] Finally, in a seventh method step 54, if Figure 7 As shown in , the welding quality of the weld 14 is determined based on a comparison with a pixel target value or a pixel target range. For example, Figure 7 The pixel target value in is given particularly simply by a reference value R in the form of the number of white pixels of the first subset 30, which here is R=1500 white pixels, i.e. the pixels of the first subset 30. Therefore, for the number A=508 white pixels of the first subset 30, it can be concluded that the weld bead 16 is sufficiently spherical to ensure a sufficiently high weld quality, since in the edge region of the weld bead 16, less than 1500 white pixels of the first subset 30 are present, i.e. reflected back to the camera 116 in the form of light.

[0087] On the other hand, a number of more than 1500 white pixels in the first subset 30 would indicate that the weld bead 16 is flat rather than spherical, because too much light is reflected back to the camera 116 in the edge region of the weld seam 14, which is captured by binarization as white pixels of the first subset 30. Possible reasons for this could be, for example, incorrect positioning of the beam path 114 of the laser beam source 102, too low a power of the laser beam source 102, too short a welding time, and too large a gap between the end segments of the conductor element 12. Thus, it can be determined that the weld quality is poor.

[0088] In determining the quality of the weld seam, in addition to the quantitative determination based on the white pixels of the first subset 30 of high-quality or correctly formed weld seams 14 and incorrectly formed or poor-quality weld seams 14, further qualitative determinations, in particular position-dependent determinations, are also possible, such as, for example, from Figure 5 An embodiment of the method 40 is shown in FIG.

[0089] exist Figure 5 It can be seen in FIG. 2 that the solder bead 16 is formed asymmetrically, so that it is inclined toward one of the two conductor elements 12. This can be seen in addition to the very high number A=2550 white pixels of the first subset 30 in the cropped binary image 28, because the white pixels of the first subset 30 are only visible or very mainly visible on one side of the edge region of the solder bead 16 in the cropped binary image 28. It can be concluded from this that an asymmetrical solder bead 16 is present here, as well as Figure 5 . This can be detected, for example, by a target range test. For example, it can be checked whether a certain number of pixels of the first subset are present in each of the respective quadrants of the binary image 28. It is also possible to check a certain form of distribution of the pixels of the first subset.

[0090] The evaluation method 40 can be controlled by at least one computer 202 which is part of the device 200 and which, as shown, can be connected to the camera 116 in order to carry out the recording of the images 20 and further method steps of the method 40 in each case.

[0091] At least one computer 202 may also be connected to a control device (not shown) of the laser beam source 102 to transmit thereto information about the weld bead 16 obtained according to the method 40 and / or to control the laser beam source 102. Thus, the laser beam source 102 may be given information about, for example, an asymmetric weld bead 16, so that the device 200 may then perform re-welding in an insufficiently welded area that was identified based on the missing white pixels of the first subset 30, so that the weld bead 16 becomes symmetrical and spherical as a result of the re-welding. In other words, the number A and the position of the white pixels of the first subset 30 determine the location of the energy input during re-welding by means of the laser beam source 102 and preferably also the level of this energy.

[0092] Figure 6 Cropped binary images 28 and associated weld beads 16 are shown at exemplary, different laser powers P (indicated in % of maximum power) of the laser beam source 102 with the same welding time. It can be seen that the selected laser power P and the duration have a considerable influence on the formation of the weld bead 16 and thus on the weld quality of the weld seam 14 during laser beam welding. As the laser power P decreases, the weld bead 16 becomes increasingly flatter and the number A of white pixels of the first subset 30 in the edge region of the weld seam 14 increases. The connection cross section of the weld seam 14 decreases accordingly and the weld seam 14 becomes unstable and may not be able to withstand the loads during operation of the stator 10 in the electric motor.

[0093] If the number of white pixels of the first subset 30 above the reference value R or the target value is fairly uniformly distributed around the central area 34, for example due to too low a laser power or too short a welding time, as can be seen in Figure 6 As can be seen in the figure, this can not only be detected by means of the method 40, but also the entire pair of conductor elements 12 can be welded again. This can be done, for example, via a pixel target area analysis or a separate analysis step to determine any necessary post-processing of the weld. Here, the local distribution of the individual pixels of the individual subsets can be analyzed in detail to draw more detailed conclusions about the shape and position of the existing weld and further determine the optimal position and the optimal level of the additional energy input. The number of remaining white pixels of the first subset 30 can determine the energy input during the re-welding.

[0094] Partially explained Figure 7 A plurality of pairs of conductor elements 12 on a stator 10 are shown which have been welded. Two outliers of welded conductor elements 12 are shown which have a significant difference Δ in the number A of white pixels of the first subset 30 compared to a reference value R. The associated weld beads 16 are also formed asymmetrically.

Claims

1. A method (40) for evaluating the welding quality of a weld seam (14), wherein end sections of at least two elongated conductor elements (12) are welded to one another through the weld seam by irradiating the end faces (13) of the end sections, wherein: The method (40) comprises the following steps: (a) capturing an image (20) of the end faces (13) of the conductor elements (12) welded to each other via the weld (14), wherein the image (20) is recorded from the end faces (13) of the conductor elements (12), and the environment recorded by the image (20) comprises at least the complete surface of the weld (14), and wherein the image (20) is recorded at different intensity levels in pixels of the image (20), wherein the intensity levels are indicators of the amount of light locally reflected from the recording location when the image (20) was recorded, and thus the indicator is the weld (14). a measure of the local orientation of a surface, in particular wherein the weld is illuminated with light parallel to the direction in which the image is recorded, (b) dividing the image (20) into at least one first subset (30) of pixels having an intensity level greater than a specified intensity level threshold and at least one second subset (32) of pixels having an intensity level less than or equal to the intensity level threshold, and The welding quality of the weld (14) is evaluated based on a comparison of the number and / or position of the pixels of the first subset (30) and / or the pixels of the second subset (32) with at least one pixel target value and / or pixel target range of the number of pixels of the first subset (30) and / or the pixels of the second subset (32) corresponding to a weld of desired quality.

2. The method (40) according to claim 1, wherein: The intensity level is a gray level, and the intensity level threshold is a gray level threshold.

3. The method (40) according to claim 1 or 2, wherein: The conductor element (12) is an inserted coil of the stator (10) of the electric machine, in particular a hairpin and / or an I-clip.

4. The method (40) according to one of the preceding claims, wherein: A higher-level image (20) is captured, the higher-level image (2) comprising in each case a plurality of weld seams (14) of at least two end sections of a conductor element (12), and a weld quality assessment is performed for each of the weld seams (14).

5. The method (40) according to one of the preceding claims, wherein: The welding quality of a weld seam (14) is evaluated, wherein end sections of at least three conductor elements (12) are welded to one another at their end faces via the weld seam (14).

6. The method (40) according to one of the preceding claims, wherein: A central region (34) of the image (20), which corresponds to the center of the weld seam, in particular to the expected position of the weld bead, is not taken into account in the evaluation according to step (c).

7. The method (40) according to claim 6, wherein: The central area (34) is a circular or elliptical area of ​​predetermined size within which a predetermined minimum number of pixels of the first subset (30) or the second subset (32) fall when the weld (14) is properly formed.

8. The method (40) according to one of the preceding claims, wherein: The target number of pixel values ​​and / or the target range of pixels for the positions are determined by selecting a minimum connection cross section as a quality feature for the weld quality.

9. The method (40) according to claim 8, wherein: Data relating to a plurality of welds considered good is used to determine the pixel target value for the number and / or the pixel target range for the position, so as to determine the pixel target value or the pixel target range by associating the position and / or number of the individual intensity levels of the pixels with the connection cross-section of the weld (14).

10. The method (40) according to one of the preceding claims, wherein: Evaluating the weld quality of the weld (14) includes evaluating the symmetry of the weld (14) based on the number and position of the pixels of the first subset (30) and / or the pixels of the second subset (32).

11. The method (40) according to one of the preceding claims, wherein: The weld (14) is re-welded based on the number and position of the pixels of the first subset (30) and / or the pixels of the second subset (32).

12. The method (40) of claim 11, wherein: A welding power for the re-welding is selected based on the number and / or position of the pixels of the first subset (30) and / or the pixels of the second subset (32).

13. The method (40) according to one of the preceding claims, wherein: The welding quality of a weld seam (14) and a different weld seam (14) on the same component (10) having a plurality of conductor elements (12) are evaluated simultaneously.

14. A device (200) for evaluating the quality of a weld (14) between end sections of at least two elongated conductor elements (12), said conductor elements being welded to one another by irradiating the end faces (13) of said end sections, said device (200) comprising: - an image capture device (116) having a beam path (118), the image capture device being designed to perform step (a) of the method according to the preceding claim - at least one data processing system (202) configured to perform steps (b) and (c).

15. The apparatus according to claim 14, wherein The apparatus comprises an illumination device (112) configured to illuminate an end face (13) of the conductor element (12) from a direction along a beam path (118) of the image capture device (116).

16. The apparatus according to claim 14 or 15, wherein The device further comprises a laser beam source (102) having a beam path (114) of a laser beam for performing a welding process for connecting the conductor elements (12) at their end faces (13), in particular wherein the beam path (118) of the image capture device (116) and the beam path (114) of the laser beam are coupled to one another, in particular via a beam splitter (106).

Citation Information

Patent Citations

  • Welding quality analysis device based on infrared vision and analysis method thereof

    CN104977305A

  • Monitoring laser-welded or -soldered seam for quality, welds series of points and takes images to assess heat dissipation from each

    DE102008062866A1

  • Method for determining quality of e.g. weld seam, for interconnecting conductor lugs of single cells for manufacture of cell block of motor car battery in automobile industry, involves determining quality based on image data density value

    DE102011102010A1

  • Method for process monitoring and control of a processing parameter in heat conduction welding, as well as associated processing machine and computer program product

    DE102020210419A1

  • Methods for testing welds