Synthetic method of isocaprylic acid rare earth salt
By using composite catalysts to react sodium isoctanoate with rare earth precursors in an ultrasonic environment of 30-40°C, the existing isoctanoate rare earth production process is solved, and efficient isoctanoate rare earth salt synthesis is achieved.
Patent Information
- Application Number
- CN202411120095.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-26
AI Technical Summary
The existing industrial production process of isocoustic rare earths is complex, and the catalytic performance is high and the synthesis method is complex, resulting in low production efficiency.
In an ultrasonic environment at 30-40°C, sodium isoctanoate reacts with a rare earth precursor to form isoctanoate rare earth salts by surface modification treatment and ultrasonic dispersion. The activity of the catalyst is enhanced by surface modification treatment and ultrasonic dispersion , reduce the reaction activation energy.
The energy consumption of industrial production of isoctanoic acid rare earth salt is reduced, the production efficiency is improved, and the reactants are fully mixed through an ultrasonic environment, which improves the catalytic activity of the composite catalyst.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical synthesis, and in particular to a method for synthesizing rare earth isooctanoate. Background Art
[0002] Rare earth 2-ethylhexanoate refers to a rare earth complex with 2-ethylhexanoate as a ligand. Rare earth elements refer to lanthanide elements and cerium elements in the periodic table. They have similar characteristics in chemical properties, while rare earth 2-ethylhexanoate maintains the coordination properties of rare earths, has certain stability and special chemical and physical properties, and has good compatibility with oil phases and organic polymers. Therefore, rare earth 2-ethylhexanoate has a variety of applications in chemistry and materials science. The special electronic structure of rare earth ions and the flexibility of 2-ethylhexanoate ligands make rare earth 2-ethylhexanoate used in the preparation of catalysts, coatings, plastics, rubber and other functional materials.
[0003] When synthesizing rare earth 2-octanoate, it is generally carried out by reacting 2-octanoic acid with rare earth metal oxide or hydroxide under an inert atmosphere, and heating and stirring are carried out under appropriate conditions so that the reaction can proceed smoothly. For example, the invention patent with publication number CN116621688A discloses a clean preparation method of rare earth 2-octanoate, firstly, saponifying 2-octanoic acid with sodium hydroxide solution to obtain a reaction solution containing sodium 2-octanoate, then adding solvent oil and rare earth chloride salt solution to the reaction solution, adding a composite catalyst, heating and stirring under light to carry out double decomposition reaction, and accompanying nuclear magnetic resonance treatment during the reaction process, separating the oil phase and concentrating and rectifying to obtain rare earth 2-octanoate.
[0004] However, when using the above method to synthesize rare earth isooctanoate, it is extremely dependent on the catalytic performance of the composite catalyst used. At the same time, the synthesis method of the composite catalyst is relatively complicated, and the production of rare earth isooctanoate needs to be carried out under complex environmental conditions, resulting in high complexity in the industrial production of rare earth isooctanoate and reduced production efficiency. Therefore, it is urgent to provide a solution to improve the above problems. Summary of the invention
[0005] The object of the present invention is to provide a method for synthesizing sodium 2-ethylhexanoate.
[0006] The invention provides a method for synthesizing sodium isooctanoate. In an ultrasonic environment at 30-40° C., sodium isooctanoate reacts with a rare earth precursor in the presence of a composite catalyst to generate isooctanoic acid rare earth salt; the composite catalyst comprises a porous carrier and nickel palladium oxide formed on the surface of the porous carrier.
[0007] Optionally, the preparation method of the composite catalyst comprises:
[0008] Performing surface modification on the porous carrier to obtain a modified carrier;
[0009] The modified carrier is ultrasonically dispersed in a nickel-palladium precursor solution and then separated to obtain a catalytic precursor;
[0010] The catalytic precursor is calcined in an oxygen-containing atmosphere to obtain a composite catalyst.
[0011] Optionally, when the porous carrier is subjected to surface modification treatment to obtain a modified carrier: the porous carrier includes at least one of carbon nitride and porous carbon.
[0012] Optionally, when the porous carrier is subjected to surface modification treatment to obtain a modified carrier: the porous carrier is ultrasonically dispersed in a modification solution to obtain the modified carrier, and preferably the solute of the modification solution includes at least one of KH-570, KH-560, and KH-550.
[0013] Optionally, when the porous carrier is subjected to surface modification treatment to obtain a modified carrier: the porous carrier is preheated at 80-100° C. for 1-2 hours, then cooled to 40-50° C., and then subjected to surface modification treatment.
[0014] Optionally, when the modified carrier is ultrasonically dispersed in a nickel-palladium precursor solution: the solute of the nickel-palladium precursor solution includes a nickel precursor and a palladium precursor, preferably the nickel precursor includes at least one of nickel sulfate, nickel chloride, nickel nitrate, and nickel acetate, and preferably the palladium precursor includes at least one of palladium nitrate, palladium chloride, and palladium sulfate.
[0015] Optionally, when the modified carrier is ultrasonically dispersed in a nickel-palladium precursor solution, the molar ratio of the nickel element to the palladium element in the nickel-palladium precursor solution is (2-3):1.
[0016] Optionally, when the modified carrier is ultrasonically dispersed in a nickel-palladium precursor solution, the mass ratio of the modified carrier to the nickel-palladium element in the nickel-palladium precursor solution is 1:(0.5-0.6).
[0017] Optionally, when the catalytic precursor is calcined and formed in an oxygen-containing atmosphere: the catalytic precursor is calcined and formed in an oxygen-containing atmosphere at 260-340°C.
[0018] Optionally, when the catalytic precursor is calcined and formed in an oxygen-containing atmosphere: the catalytic precursor is calcined in an oxygen-containing atmosphere for 1-2 hours to form the catalytic precursor.
[0019] Optionally, when the catalytic precursor is calcined and formed in an oxygen-containing atmosphere, the oxygen concentration in the oxygen-containing atmosphere is 10-100%.
[0020] Optionally, when the catalytic precursor is calcined and formed in an oxygen-containing atmosphere: the catalytic precursor is preheated in a non-oxidizing atmosphere at 260-340° C., then subjected to oxygen-containing atmosphere shock, and then calcined and formed at the same temperature.
[0021] Optionally, when sodium isooctanoate reacts with a rare earth precursor in the presence of a composite catalyst to generate isooctanoic acid rare earth salt: the molar ratio of sodium isooctanoate to the rare earth element in the rare earth precursor is 1:(0.5-0.8).
[0022] Optionally, when sodium isooctanoate reacts with a rare earth precursor in the presence of a composite catalyst to generate isooctanoic acid rare earth salt: the mass ratio of the sodium isooctanoate to the composite catalyst is 1:(0.01-0.03).
[0023] Optionally, when sodium isooctanoate reacts with a rare earth precursor in the presence of a composite catalyst to generate isooctanoic acid rare earth salt: the rare earth precursor includes at least one of rare earth chloride, rare earth nitrate, rare earth sulfate, and rare earth carbonate.
[0024] Optionally, the process comprises the following steps: keeping a mixed solution containing sodium isooctanoate and a rare earth precursor at 30-40° C., adding a composite catalyst into the mixed solution for ultrasonic mixing, separating the composite catalyst and adding an extracting liquid to extract an extracted oil phase, and concentrating the extracted oil phase to obtain isooctanoic acid rare earth salt.
[0025] Optionally, after the composite catalyst is separated, it is washed with a nickel-palladium mixed solution, and the composite catalyst is recycled after drying, wherein the nickel-cobalt mixed solution contains a nickel-palladium precursor.
[0026] Optionally, after the composite catalyst is separated, the composite catalyst is calcined and oxidized in an oxygen-containing atmosphere, and then cooled and the composite catalyst is recycled.
[0027] Optionally, when the extracting liquid is added to extract the extracted oil phase: the extracting liquid includes at least one of a mixture of tributyl phosphate and kerosene in a volume ratio of 1:1 and a mixture of trioctylphosphine oxide and toluene in a volume ratio of 1:1.
[0028] Optionally, when adding the extraction liquid to extract the extracted oil phase: adding the extraction liquid, shaking and mixing, and then separating to obtain the extracted oil phase.
[0029] Optionally, when adding the extracting liquid to extract the extracted oil phase: after adding the extracting liquid, oscillate and mix at 30-40°C.
[0030] Optionally, in the process of concentrating the extracted oil phase to obtain the isooctanoic acid rare earth salt, the extracted oil phase is evaporated to dryness at an evaporation temperature, and the extract is recovered and the isooctanoic acid rare earth salt is collected. DETAILED DESCRIPTION
[0031] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Unless otherwise defined, the technical terms or scientific terms used herein should be the common meanings understood by people with general skills in the field to which the present invention belongs.
[0032] The embodiment of the present invention provides a method for synthesizing rare earth isooctanoate, comprising reacting sodium isooctanoate with a rare earth precursor under a composite catalyst at 30-40° C. in an ultrasonic environment to generate rare earth isooctanoate. In fact, the present invention can greatly reduce the activation energy required for the reaction by introducing a composite catalyst, thereby reducing the energy consumption of industrial production of rare earth isooctanoate and improving production efficiency. In addition, by reacting in an ultrasonic environment, the reactants can be fully mixed, and the catalytic activity of the composite catalyst can be improved by utilizing the ultrasonic cavitation effect.
[0033] Specifically, the composite catalyst includes a porous carrier and nickel-palladium oxide formed on the surface of the porous carrier. In fact, the porous carrier itself has the characteristics of high specific surface area, which can provide sufficient active sites for the formation of nickel-palladium oxide, thereby increasing the loading amount of nickel-palladium oxide on the surface of the porous carrier, and nickel-palladium oxide can promote the double decomposition reaction of sodium isooctanoate and rare earth precursors to generate sodium salt and isooctanoic acid rare earth salt.
[0034] In fact, the preparation method of the composite catalyst comprises the following steps:
[0035] S1, performing surface modification treatment on the porous carrier to obtain a modified carrier;
[0036] S2, ultrasonically dispersing the modified carrier in a nickel-palladium precursor solution and separating the catalyst precursor;
[0037] S3. calcining the catalytic precursor in an oxygen-containing atmosphere to obtain a composite catalyst.
[0038] In fact, by modifying the porous carrier in step S1, the number of active sites on the surface of the porous carrier can be increased, thereby increasing the loading capacity of the porous carrier for nickel and palladium elements, and at the same time, the bonding strength between the porous carrier and nickel and palladium can be improved. In addition, during the ultrasonic dispersion process, the nickel-palladium precursor solution can be promoted to penetrate into the internal voids of the porous carrier, thereby improving the adhesion uniformity of nickel and palladium on the carrier surface, and calcination in an oxygen-containing atmosphere can oxidize the nickel and palladium, thereby forming a dense nickel-palladium oxide layer.
[0039] In some embodiments, when performing step S1, the porous carrier used includes at least one of carbon nitride and porous carbon. In fact, the specific surface area of the porous carrier is 100-200m 2 / g, by selecting porous materials with high specific surface area, the loading of the porous carrier on the nickel-palladium oxide layer can be effectively increased. In addition, the pores can be blocked during the calcination process due to the excessively large specific surface area causing the pores to be too narrow.
[0040] Specifically, when the porous carrier is carbon nitride during step S1, the preparation method of carbon nitride includes: using nitrogen-containing organic compounds such as melamine as a precursor, calcining the precursor at 500-600°C for 5-6h, cooling to room temperature, grinding, crushing, washing and drying to obtain a carbon nitride material. In fact, carbon nitride can also be a conventional commercial product, such as the graphite phase carbon nitride product numbered XFI10 of Jiangsu Xianfeng Nanomaterial Technology Co., Ltd.
[0041] In some embodiments, when performing step S1, the porous carrier is ultrasonically dispersed in the modification solution to obtain a modified carrier. In fact, by treating the porous carrier in the modification solution, the surface active sites of the porous carrier can be increased. In addition, the ultrasonic treatment can effectively utilize the ultrasonic cavitation effect to remove the bubbles blocked in the pore structure of the porous carrier, thereby improving the uniformity and integrity of the surface activation.
[0042] Specifically, when performing step S1, the solute in the modified solution includes at least one of KH-570, KH-560, and KH-550. In fact, KH-570, KH-560, and KH-550 are all silane coupling agents, which can introduce silicon-containing groups on the surface of the porous carrier, thereby effectively improving the binding ability to nickel and palladium elements.
[0043] In some embodiments, when executing step S1, the porous carrier is preheated at 80-100°C for 1-2h and then cooled to 40-50°C, and then the porous carrier is added to the modified solution for ultrasonic dispersion treatment. In fact, by preheating the porous carrier, the activity of the surface molecules of the porous carrier can be effectively improved, which is conducive to the surface modification of the porous carrier by the modified solution. At the same time, the preheating treatment can also cause cracks to appear in the closed pores in the porous carrier, thereby improving the pore connectivity of the porous carrier.
[0044] In some embodiments, when executing step S2, the solute of the nickel-palladium precursor solution includes a nickel precursor and a palladium precursor. After the modified carrier is immersed in the nickel-palladium precursor solution, the active sites and active groups present on the surface of the modified carrier can capture the nickel precursor and the palladium precursor, so that the nickel precursor and the palladium precursor are evenly attached to the surface of the modified carrier and the inner wall of the pores.
[0045] In fact, the nickel precursor includes at least one of nickel sulfate, nickel chloride, nickel nitrate, and nickel acetate, and the palladium precursor includes at least one of palladium nitrate, palladium chloride, and palladium sulfate. In fact, the solvent in the nickel-palladium precursor solution can be a commonly used solvent in the art, such as deionized water, so that the nickel precursor and the palladium precursor can be adaptively dissolved.
[0046] In some embodiments, the molar ratio of nickel to palladium in the nickel-palladium precursor solution is (2-3):1. In fact, by adjusting the molar ratio of nickel to palladium in the nickel-palladium precursor solution, the molar ratio of nickel to palladium on the surface of the porous support can be effectively adjusted to form a nickel-palladium oxide layer with different ratios, thereby adjusting the catalytic activity of the composite catalyst. Specifically, the mass ratio of the modified support to the nickel to palladium in the nickel-palladium precursor solution is 1:(0.5-0.6).
[0047] In some embodiments, when performing step S3, the catalytic precursor is calcined and formed in an oxygen-containing atmosphere at 260-340° C., so that the nickel precursor and the palladium precursor on the surface of the porous support can be fully oxidized and sintered to form a dense and stable cross-oxidation layer. Specifically, the catalytic precursor is calcined in an oxygen-containing atmosphere at 260-340° C. for 1-2 hours to form the oxidation layer.
[0048] In some embodiments, the oxygen concentration in the oxygen-containing atmosphere is 10-100%. Specifically, the oxygen-containing atmosphere can be a pure oxygen atmosphere or an air atmosphere, which is necessary to oxidize and shape the nickel precursor and the palladium precursor on the surface of the porous support.
[0049] In some embodiments, when performing step S3, the catalytic precursor is preheated in a non-oxidizing atmosphere at 260-340°C and then subjected to oxygen-containing atmosphere shock, and then calcined and formed after being kept at 260-340°C for 1-2 hours. In fact, by preheating the catalytic precursor in advance, the internal temperature uniformity of the catalytic precursor can be improved, so that after the oxygen-containing atmosphere thermal shock, the forming uniformity of the oxide layer can be improved. Specifically, the non-oxidizing atmosphere can be a nitrogen atmosphere or an inert atmosphere.
[0050] In fact, when sodium isooctanoate and a rare earth precursor are reacted in the presence of a composite catalyst to generate isooctanoic acid rare earth salt, the molar ratio of sodium isooctanoate to the rare earth element in the rare earth precursor is 1:(0.5-0.8). Specifically, by controlling the excess amount of sodium isooctanoate, the reaction can be effectively forwarded and the conversion rate of the rare earth element can be increased.
[0051] In fact, sodium isooctanoate can be synthesized using conventional products available on the market, or using conventional methods, such as saponifying isooctanoic acid with sodium hydroxide solution to produce sodium isooctanoate. In fact, in industrial production, the production of sodium isooctanoate can be combined with the production of isooctanoic acid rare earth salts, which can improve production efficiency and production line utilization.
[0052] In some embodiments, the mass ratio of sodium isooctanoate to the composite catalyst is 1:(0.01-0.03). In fact, by regulating the amount of the composite catalyst, the reaction cost can be reduced while maintaining the high reaction activity of the composite catalyst. In fact, in industrial production, the composite catalyst can be filled in a reaction bed or a reaction plate, thereby improving the convenience of application of the composite catalyst.
[0053] In some embodiments, the rare earth precursor includes at least one of rare earth chloride, rare earth nitrate, rare earth sulfate, and rare earth carbonate. The rare earth precursor is reacted with sodium isooctanoate to generate isooctanoic acid rare earth salt and corresponding sodium salt, such as sodium chloride, sodium nitrate, sodium sulfate, and sodium carbonate, so as to achieve the recycling of sodium ions.
[0054] In fact, the chloride rare earth salt includes at least one of lanthanum chloride (LaCl3), cerium chloride (CeCl3), neodymium chloride (NdCl3), gadolinium chloride (GdCl3), praseodymium chloride (PrCl3), yttrium chloride (YCl3), europium chloride (EuCl3), terbium chloride (TbCl3), dysprosium chloride (DyCl3), holmium chloride (HoCl3), erbium chloride (ErCl3), thulium chloride (TmCl3), ytterbium chloride (YbCl3), and lutetium chloride (LuCl3).
[0055] In fact, rare earth nitrates include at least one of lanthanum nitrate (La(NO3)3·6H2O), cerium nitrate (Ce(NO3)3·6H2O), neodymium nitrate (Nd(NO3)3·6H2O), yttrium nitrate (Y(NO3)3·6H2O), terbium nitrate (Tb(NO3)3·6H2O), praseodymium nitrate (Pr(NO3)3), gadolinium nitrate (Gd(NO3)3), dysprosium nitrate (Dy(NO3)3), europium nitrate (Eu(NO3)3), and holmium nitrate (Ho(NO3)3).
[0056] In fact, the rare earth sulfate salt includes at least one of lanthanum sulfate (La2(SO4)3), cerium sulfate (Ce2(SO4)3), neodymium sulfate (Nd2(SO4)3), praseodymium sulfate (Pr2(SO4)3), samarium sulfate (Sm2(SO4)3), europium sulfate (Eu2(SO4)3), gadolinium sulfate (Gd2(SO4)3), terbium sulfate (Tb2(SO4)3), dysprosium sulfate (Dy2(SO4)3), and holmium sulfate (Ho2(SO4)3).
[0057] In fact, rare earth carbonates include at least one of lanthanum carbonate (La2(CO3)3), cerium carbonate (Ce2(CO3)3), praseodymium carbonate (Pr2(CO3)3), samarium carbonate (Sm2(CO3)3), europium carbonate (Eu2(CO3)3), gadolinium carbonate (Gd2(CO3)3), terbium carbonate (Tb2(CO3)3), dysprosium carbonate (Dy2(CO3)3), holmium carbonate (Ho2(CO3)3), erbium carbonate (Er2(CO3)3), and lutetium carbonate (Lu2(CO3)3).
[0058] In fact, the synthesis method of rare earth isooctanoate provided by the present invention comprises the following steps: after keeping a mixed solution containing sodium isooctanoate and a rare earth precursor at 30-40° C., adding a composite catalyst into the mixed solution for ultrasonic mixing, separating the composite catalyst and adding an extracting liquid to extract an extracted oil phase, and concentrating the extracted oil phase to obtain rare earth isooctanoate.
[0059] Specifically, after the composite catalyst is separated from the mixed solution, the composite catalyst is washed with a nickel-palladium mixed solution, and the composite catalyst is recycled after being dried to a constant weight at 40-50° C., so that the composite catalyst can be used for a long time and the cycle stability is improved. In fact, a nickel-palladium precursor is dissolved in the nickel-palladium mixed solution, wherein the nickel-palladium precursor is a mixture of a nickel precursor and a palladium precursor.
[0060] In some embodiments, after the composite catalyst is separated from the mixed solution, the composite catalyst is calcined and oxidized in an oxygen-containing atmosphere and then cooled to room temperature, so that the composite catalyst can be reused. In fact, by calcining and oxidizing the composite catalyst, the structure of the nickel-palladium oxide layer in the composite catalyst can be restored, thereby improving the cycle performance stability.
[0061] In some embodiments, when the extracting liquid is added to extract the mixed solution, the extracting liquid includes at least one of a mixture of tributyl phosphate and kerosene in a volume ratio of 1:1 and a mixture of trioctylphosphine oxide and toluene in a volume ratio of 1:1. In fact, the extracting liquid can also be 200# solvent oil or aviation kerosene.
[0062] In some embodiments, the extracting liquid is added and then shaken and mixed to improve the extraction efficiency of the extracting liquid on the isooctanoic acid rare earth salt. In fact, the extracting liquid can be shaken and mixed at 30-40° C. After the extracting liquid is added, the extracting liquid is concentrated to obtain the isooctanoic acid rare earth salt. Specifically, in the process of concentrating the extracting oil phase to obtain the isooctanoic acid rare earth salt, the extracting oil phase is evaporated to dryness at the evaporation temperature, and the extracting liquid is recovered and the isooctanoic acid rare earth salt is collected.
[0063] Preparation Example 1
[0064] This preparation example 1 provides a method for preparing a composite catalyst, comprising the following steps:
[0065] S1, the specific surface area is 150m2 / g of carbon nitride was added into KH-560 silane coupling agent solution, ultrasonically dispersed at 45°C for 15 minutes, filtered and separated, washed with deionized water, and dried to constant weight to obtain a modified carrier;
[0066] S2, dispersing the modified support in a nickel-palladium precursor solution (solutes are nickel chloride and palladium chloride, the molar ratio of nickel element to palladium element is 2:1, and the mass ratio of the modified support to nickel-palladium is 1:0.5) by ultrasonic dispersion for 10 minutes, and then keeping the temperature at 50°C for 2 hours and filtering to separate the catalytic precursor;
[0067] S3. Place the catalytic precursor in an atmosphere furnace, raise the temperature of the atmosphere furnace to 300°C at 5°C / min under a nitrogen atmosphere to preheat the catalytic precursor, then transfer the catalytic precursor to an oxygen atmosphere at 300°C and calcine for 2 hours, then cool to room temperature to obtain a composite catalyst.
[0068] Preparation Example 2
[0069] This preparation example 2 provides a method for preparing a composite catalyst, comprising the following steps:
[0070] S1, the specific surface area is 150m 2 / g of carbon nitride was preheated for 2h in a nitrogen atmosphere at 100°C, naturally cooled to 45°C, and then added with a KH-560 silane coupling agent solution. After ultrasonic dispersion at 45°C for 15min, the modified carrier was separated by suction filtration, washed with deionized water, and dried to constant weight.
[0071] S2, dispersing the modified support in a nickel-palladium precursor solution (solutes are nickel chloride and palladium chloride, the molar ratio of nickel element to palladium element is 2:1, and the mass ratio of the modified support to nickel-palladium is 1:0.5) by ultrasonic dispersion for 10 minutes, and then keeping the temperature at 50°C for 2 hours and filtering to separate the catalytic precursor;
[0072] S3. Place the catalytic precursor in an atmosphere furnace, raise the temperature of the atmosphere furnace to 300°C at 5°C / min under a nitrogen atmosphere to preheat the catalytic precursor, then transfer the catalytic precursor to an oxygen atmosphere at 300°C and calcine for 2 hours, then cool to room temperature to obtain a composite catalyst.
[0073] Preparation Example 3
[0074] This preparation example 3 provides a method for preparing a composite catalyst, comprising the following steps:
[0075] S1, the specific surface area is 150m 2 / g of carbon nitride was preheated at 90°C in a nitrogen atmosphere for 2h, naturally cooled to 40°C, and then added with a KH-550 silane coupling agent solution. After ultrasonic dispersion at 40°C for 15min, the modified carrier was separated by suction filtration, washed with deionized water, and dried to constant weight.
[0076] S2, dispersing the modified support in a nickel-palladium precursor solution (solutes are nickel chloride and palladium chloride, the molar ratio of nickel element to palladium element is 1:2, and the mass ratio of the modified support to nickel-palladium is 1:0.5) by ultrasonic dispersion for 10 minutes, and then keeping the temperature at 50°C for 2 hours and filtering to separate the catalytic precursor;
[0077] S3. Place the catalytic precursor in an atmosphere furnace, raise the temperature of the atmosphere furnace to 300°C at 5°C / min under a nitrogen atmosphere to preheat the catalytic precursor, then transfer the catalytic precursor to an oxygen atmosphere at 300°C and calcine for 2 hours, then cool to room temperature to obtain a composite catalyst.
[0078] Preparation Example 4
[0079] This preparation example 4 provides a method for preparing a composite catalyst, comprising the following steps:
[0080] S1, the specific surface area is 150m 2 / g of carbon nitride was preheated for 1.5h in a nitrogen atmosphere at 100°C, naturally cooled to 45°C, and then added with a KH-550 silane coupling agent solution. After ultrasonic dispersion at 45°C for 10min, the modified carrier was separated by suction filtration, washed with deionized water, and dried to constant weight.
[0081] S2, dispersing the modified support in a nickel precursor solution (solute is nickel chloride, the mass ratio of the modified support to nickel is 1:0.5) by ultrasonic dispersion for 10 minutes, keeping the temperature at 50°C for 2 hours, and then filtering and separating to obtain a catalytic precursor;
[0082] S3. Place the catalytic precursor in an atmosphere furnace, raise the temperature of the atmosphere furnace to 300°C at 5°C / min under a nitrogen atmosphere to preheat the catalytic precursor, then transfer the catalytic precursor to an oxygen atmosphere at 300°C and calcine for 2 hours, then cool to room temperature to obtain a composite catalyst.
[0083] Preparation Example 5
[0084] This preparation example 5 provides a method for preparing a composite catalyst, comprising the following steps:
[0085] S1, the specific surface area is 150m 2 / g of carbon nitride was preheated for 1.5h in a nitrogen atmosphere at 100°C, naturally cooled to 45°C, and then added with a KH-550 silane coupling agent solution. After ultrasonic dispersion at 45°C for 10min, the modified carrier was separated by suction filtration, washed with deionized water, and dried to constant weight.
[0086] S2, dispersing the modified support in a palladium precursor solution (solute is palladium chloride, the mass ratio of the modified support to palladium is 1:0.5) by ultrasonic dispersion for 10 minutes, keeping the temperature at 50°C for 2 hours, and then filtering and separating to obtain a catalytic precursor;
[0087] S3. Place the catalytic precursor in an atmosphere furnace, raise the temperature of the atmosphere furnace to 300°C at 5°C / min under a nitrogen atmosphere to preheat the catalytic precursor, then transfer the catalytic precursor to an oxygen atmosphere at 300°C and calcine for 2 hours, then cool to room temperature to obtain a composite catalyst.
[0088] Preparation Example 6
[0089] This preparation example 6 provides a method for preparing a composite catalyst, comprising the following steps:
[0090] S1, the specific surface area is 150m 2 / g of carbon nitride was preheated at 90°C in a nitrogen atmosphere for 2h, naturally cooled to 40°C, and then added with a KH-550 silane coupling agent solution. After ultrasonic dispersion at 40°C for 15min, the modified carrier was separated by suction filtration, washed with deionized water, and dried to constant weight.
[0091] S2, dispersing the modified support in a nickel-cobalt precursor solution (solutes are nickel chloride and cobalt chloride, the molar ratio of nickel element to cobalt element is 2:1, and the mass ratio of the modified support to nickel-cobalt is 1:0.5) by ultrasonic dispersion for 10 minutes, and then keeping the temperature at 50°C for 2 hours and filtering to separate the catalytic precursor;
[0092] S3. Place the catalytic precursor in an atmosphere furnace, raise the temperature of the atmosphere furnace to 300°C at 5°C / min under a nitrogen atmosphere to preheat the catalytic precursor, then transfer the catalytic precursor to an oxygen atmosphere at 300°C and calcine for 2 hours, then cool to room temperature to obtain a composite catalyst.
[0093] Example 1
[0094] The present embodiment 1 provides a method for synthesizing rare earth isooctanoate, comprising the following steps: dissolving 1 mol of sodium isooctanoate and 0.8 mol of lanthanum chloride in deionized water, and mixing them in an ultrasonic environment at 35° C. for 15 minutes to obtain a mixed solution; adding 3.32 g of the composite catalyst prepared in preparation example 1 into the mixed solution, performing ultrasonic mixing, and stirring the mixture at 35° C. for 30 minutes to obtain a reaction solution; filtering the reaction solution to obtain a raffinate and the composite catalyst, adding aviation kerosene to the raffinate, oscillating and mixing the mixture at 35° C., and then standing to separate the layers, separating the extracted oil phase and the raffinate water phase, evaporating and concentrating the extracted oil phase to obtain lanthanum isooctanoate, and evaporating and concentrating the extracted water phase to obtain sodium chloride. The yield of lanthanum isooctanoate is calculated to be 98.46%.
[0095] Example 2
[0096] This Example 2 provides a method for synthesizing rare earth isooctanoate, comprising the following steps: dissolving 1 mol of sodium isooctanoate and 0.8 mol of lanthanum chloride in deionized water, and mixing them in an ultrasonic environment at 35°C for 15 minutes to obtain a mixed solution; adding 3.69 g of the composite catalyst prepared in Preparation Example 2 to the mixed solution, performing ultrasonic mixing, and stirring the mixture at 35°C for 30 minutes to obtain a reaction solution; filtering the reaction solution to obtain a raffinate and the composite catalyst, adding aviation kerosene to the raffinate, oscillating and mixing the mixture at 35°C, and then standing to separate the layers, separating the extracted oil phase and the raffinate water phase, evaporating and concentrating the extracted oil phase to obtain lanthanum isooctanoate, and evaporating and concentrating the extracted water phase to obtain sodium chloride. The yield of lanthanum isooctanoate is calculated to be 98.62%.
[0097] Example 3
[0098] This Example 3 provides a method for synthesizing rare earth isooctanoate, comprising the following steps: dissolving 1 mol of sodium isooctanoate and 0.8 mol of lanthanum chloride in deionized water, and mixing them in an ultrasonic environment at 35°C for 15 minutes to obtain a mixed solution; adding 3.48 g of the composite catalyst prepared in Preparation Example 3 to the mixed solution, performing ultrasonic mixing, and stirring the mixture at 35°C for 30 minutes to obtain a reaction solution; filtering the reaction solution to obtain a raffinate and the composite catalyst, adding aviation kerosene to the raffinate, oscillating and mixing the mixture at 35°C, and then standing to separate the layers, separating the extracted oil phase and the raffinate water phase, evaporating and concentrating the extracted oil phase to obtain lanthanum isooctanoate, and evaporating and concentrating the extracted water phase to obtain sodium chloride. The yield of lanthanum isooctanoate is calculated to be 95.34%.
[0099] Example 4
[0100] This Example 4 provides a method for synthesizing rare earth isooctanoate, comprising the following steps: dissolving 1 mol of sodium isooctanoate and 0.8 mol of lanthanum chloride in deionized water, and mixing them in an ultrasonic environment at 35°C for 15 minutes to obtain a mixed solution; adding 3.37 g of the composite catalyst prepared in Preparation Example 4 to the mixed solution, performing ultrasonic mixing, and stirring the mixture at 35°C for 30 minutes to obtain a reaction solution; filtering the reaction solution to obtain a raffinate and the composite catalyst, adding aviation kerosene to the raffinate, oscillating and mixing the mixture at 35°C, and then standing to separate the layers, separating the extracted oil phase and the raffinate water phase, evaporating and concentrating the extracted oil phase to obtain lanthanum isooctanoate, and evaporating and concentrating the extracted water phase to obtain sodium chloride. The yield of lanthanum isooctanoate is calculated to be 94.12%.
[0101] Example 5
[0102] This Example 5 provides a method for synthesizing rare earth isooctanoate, comprising the following steps: dissolving 1 mol of sodium isooctanoate and 0.8 mol of lanthanum chloride in deionized water, and mixing them in an ultrasonic environment at 35°C for 15 minutes to obtain a mixed solution; adding 3.71 g of the composite catalyst prepared in Preparation Example 5 to the mixed solution, performing ultrasonic mixing, and stirring the mixture at 35°C for 30 minutes to obtain a reaction solution; filtering the reaction solution to obtain a raffinate and the composite catalyst, adding aviation kerosene to the raffinate, oscillating and mixing the mixture at 35°C, and then standing to separate the layers, separating the extracted oil phase and the raffinate water phase, evaporating and concentrating the extracted oil phase to obtain lanthanum isooctanoate, and evaporating and concentrating the extracted water phase to obtain sodium chloride. The yield of lanthanum isooctanoate is calculated to be 91.64%.
[0103] Example 6
[0104] This Example 6 provides a method for synthesizing rare earth isooctanoate, comprising the following steps: dissolving 1 mol of sodium isooctanoate and 0.8 mol of lanthanum chloride in deionized water, and mixing them in an ultrasonic environment at 35°C for 15 minutes to obtain a mixed solution; adding 3.43 g of the composite catalyst prepared in Preparation Example 6 to the mixed solution, performing ultrasonic mixing, and stirring the mixture at 35°C for 30 minutes to obtain a reaction solution; filtering the reaction solution to obtain a raffinate and the composite catalyst, adding aviation kerosene to the raffinate, oscillating and mixing the mixture at 35°C, and then standing to separate the layers, separating the extracted oil phase and the raffinate water phase, evaporating and concentrating the extracted oil phase to obtain lanthanum isooctanoate, and evaporating and concentrating the extracted water phase to obtain sodium chloride. The yield of lanthanum isooctanoate is calculated to be 94.36%.
[0105] Example 7 to Example 18
[0106] Embodiments 7 to 18 of the present invention respectively provide a method for synthesizing rare earth isooctanoate, which is different from Embodiment 2 in that different types of rare earth are used, as shown in Table 1 below.
[0107] Table 1
[0108] Rare earth precursors Yield / % Rare earth precursors Yield / % Example 7 Cerium chloride 97.51 Example 13 Lanthanum Sulfate 98.23 Example 8 Neodymium chloride 98.12 Embodiment 14 Cerium Sulfate 97.98 Example 9 Gadolinium chloride 98.34 Embodiment 15 Lanthanum carbonate 98.56 Example 10 Yttrium chloride 97.67 Example 16 Cerium carbonate 97.71 Embodiment 11 Lanthanum Nitrate 98.78 Embodiment 17 Gadolinium carbonate 97.96 Example 12 Yttrium nitrate 97.89 Embodiment 18 Dysprosium carbonate 97.69
[0109] Comparative Example 1
[0110] The present comparative example 1 provides a method for synthesizing rare earth isooctanoate, comprising the following steps: dissolving 1 mol of sodium isooctanoate and 0.8 mol of lanthanum chloride in deionized water, mixing in an ultrasonic environment at 35° C. for 15 min to obtain a mixed solution, and stirring and reacting at 35° C. for 30 min to obtain a reaction solution; adding aviation kerosene to the reaction solution, oscillating and mixing at 35° C., standing to separate layers, separating an extracted oil phase and a raffinate water phase, evaporating and concentrating the extracted oil phase to obtain lanthanum isooctanoate, and evaporating and concentrating the extracted water phase to obtain sodium chloride. The yield of lanthanum isooctanoate is calculated to be 32.68%.
[0111] Cyclic catalytic performance test
[0112] The composite catalysts prepared in Preparation Examples 1 to 6 were subjected to cyclic catalytic tests. After each catalytic test, the composite catalysts were washed with deionized water and dried. The yields of rare earth isooctanoate after 5 cycles and 10 cycles were recorded as shown in Table 2 below.
[0113] The composite catalysts prepared in Preparation Examples 1 to 3 were subjected to a cyclic catalytic test. After each catalytic step, they were washed with the corresponding nickel-palladium precursor solution, transferred to an oxygen atmosphere at 300°C, calcined and dried, and then reused. The yield of rare earth isooctanoate after 5 cycles and 10 cycles is shown in Table 3 below.
[0114] Table 2
[0115] 5 times / % 10 times / % 5 times / % 10 times / % Preparation Example 1 94.35 89.61 Preparation Example 4 89.67 85.19 Preparation Example 2 94.96 91.22 Preparation Example 5 86.43 82.34 Preparation Example 3 90.37 86.54 Preparation Example 6 90.16 84.25
[0116] Table 3
[0117] 5 times / % 10 times / % Preparation Example 1 97.98 97.52 Preparation Example 2 98.12 97.91 Preparation Example 3 94.67 94.03
[0118] Although the embodiments of the present invention are described in detail above, it is obvious to those skilled in the art that various modifications and variations can be made to these embodiments. However, it should be understood that such modifications and variations are within the scope and spirit of the present invention as described in the claims. Moreover, the present invention described herein may have other embodiments and may be implemented or realized in a variety of ways.
Claims
1. A method for synthesizing rare earth isooctanoate, characterized in that: In an ultrasonic environment at 30-40° C., sodium isooctanoate and a rare earth precursor react in the presence of a composite catalyst to generate isooctanoic acid rare earth salt; the composite catalyst comprises a porous carrier and nickel palladium oxide formed on the surface of the porous carrier.
2. The synthesis method according to claim 1, characterized in that The preparation method of the composite catalyst comprises: Performing surface modification on the porous carrier to obtain a modified carrier; The modified carrier is ultrasonically dispersed in a nickel-palladium precursor solution and then separated to obtain a catalytic precursor; The catalytic precursor is calcined in an oxygen-containing atmosphere to obtain a composite catalyst.
3. The synthesis method according to claim 2, characterized in that When the porous carrier is subjected to surface modification to obtain a modified carrier: The porous support includes at least one of carbon nitride and porous carbon; and / or, preparing a modified carrier by ultrasonically dispersing the porous carrier in a modified solution, wherein the solute of the modified solution preferably comprises at least one of KH-570, KH-560 and KH-550; And / or, the porous carrier is preheated at 80-100° C. for 1-2 hours, then cooled to 40-50° C., and then subjected to surface modification treatment.
4. The synthesis method according to claim 2, characterized in that When the modified support is ultrasonically dispersed in the nickel-palladium precursor solution: The solute of the nickel-palladium precursor solution includes a nickel precursor and a palladium precursor, preferably the nickel precursor includes at least one of nickel sulfate, nickel chloride, nickel nitrate, and nickel acetate, and preferably the palladium precursor includes at least one of palladium nitrate, palladium chloride, and palladium sulfate; And / or, the molar ratio of nickel element to palladium element in the nickel-palladium precursor solution is (2-3):1; And / or, the mass ratio of the modified carrier to the nickel-palladium element in the nickel-palladium precursor solution is 1:(0.5-0.6).
5. The synthesis method according to claim 2, characterized in that When the catalytic precursor is calcined in an oxygen-containing atmosphere: Calcine the catalytic precursor in an oxygen-containing atmosphere at 260-340°C to form the catalyst; and / or, calcining the catalytic precursor in an oxygen-containing atmosphere for 1-2 hours to form the catalyst; And / or, the oxygen concentration in the oxygen-containing atmosphere is 10-100%; And / or, the catalytic precursor is preheated in a non-oxidizing atmosphere at 260-340° C., then subjected to oxygen-containing atmosphere shock, and then calcined at the same temperature to form the catalyst.
6. The synthesis method according to claim 1, characterized in that When sodium 2-ethylhexanoate reacts with a rare earth precursor in the presence of a composite catalyst to generate 2-ethylhexanoate rare earth salt: The molar ratio of sodium isooctanoate to the rare earth element in the rare earth precursor is 1:(0.5-0.8); And / or, the mass ratio of the sodium isooctanoate to the composite catalyst is 1:(0.01-0.03); And / or, the rare earth precursor includes at least one of rare earth chloride, rare earth nitrate, rare earth sulfate, and rare earth carbonate.
7. The synthesis method according to any one of claims 1 to 6, characterized in that The following steps are involved: After the mixed solution containing sodium isooctanoate and rare earth precursor is kept warm at 30-40°C, the composite catalyst is added into the mixed solution for ultrasonic mixing, the composite catalyst is separated and an extracting liquid is added to extract to obtain an extracted oil phase, and the extracted oil phase is concentrated to obtain isooctanoic acid rare earth salt.
8. The synthesis method according to claim 7, characterized in that After separating the composite catalyst, the composite catalyst is washed with a nickel-palladium mixed solution, and the composite catalyst is recycled after drying, wherein the nickel-cobalt mixed solution contains a nickel-palladium precursor; and / or, after separating the composite catalyst, the composite catalyst is calcined and oxidized in an oxygen-containing atmosphere, and then cooled and recycled.
9. The synthesis method according to claim 7, characterized in that: When the extraction liquid is added to extract the extracted oil phase: The extract comprises at least one of a mixture of tributyl phosphate and kerosene in a volume ratio of 1:1 and a mixture of trioctylphosphine oxide and toluene in a volume ratio of 1:1; and / or, adding the extracting liquid, shaking and mixing, and then separating to obtain the extracted oil phase; and / or, adding the extract and shaking the mixture at 30-40°C for mixing.
10. The synthesis method according to claim 7, characterized in that: In the process of concentrating the extracted oil phase to obtain the isooctanoic acid rare earth salt, the extracted oil phase is evaporated to dryness at an evaporation temperature, and the extract is recovered and the isooctanoic acid rare earth salt is collected.
Citation Information
Patent Citations
Method for preparing nontoxic rare-earth octoate
CN101628868A
Preparation method of rare earth drier and rare earth drier
CN117550965A
Stable concentrated rare earth carboxylate liquids
CN1303385A