Display panel and preparation method thereof

By preparing grooves and two layers of cathodes in the OLED display panel, connecting them in parallel, combining filling and packaging structures, the brightness uneven problem caused by cathode pressure drop is solved, brightness uniformity and water-oxygen barrier ability are improved, and power consumption is reduced .

CN119031791APending Publication Date: 2024-11-26NANJING LUMICORE TECH LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411144462.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing OLED display panels have uneven brightness due to the large cathode pressure drop, and the existing compensation method increases power consumption, which is difficult to effectively solve.

Method used

By preparing grooves in a flat layer, two cathodes are arranged, connected in parallel, and there are cracks in the light emitting layer covering the grooves and the cathode, the filling structure is in the grooves, the encapsulation layer is between the cathodes, and an isolation structure is arranged to reduce the cathode pressure drop , improve brightness uniformity.

Benefits of technology

It effectively reduces the cathode pressure drop, improves the brightness uniformity of the display panel, reduces power consumption, and enhances the water and oxygen barrier capacity, extends the equipment life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119031791A_ABST
    Figure CN119031791A_ABST
Patent Text Reader

Abstract

The invention discloses a display panel and a preparation method thereof. The display panel comprises a flat layer, a plurality of anodes, a light-emitting layer and a cathode which are arranged in a laminated mode. The display panel further comprises a groove which at least partially penetrates through the flat layer, and the groove is located between the two adjacent anodes. The light-emitting layer covers the anode and the groove; the cathode comprises a first cathode and a second cathode which are arranged in a laminated mode, the first cathode covers the light-emitting layer and the groove, the second cathode is arranged on the side, away from the light-emitting layer, of the first cathode, and the second cathode is connected with the first cathode. According to the technical scheme, the two layers of cathodes are prepared on the basis of preparing the grooves in the flat layer to improve transverse crosstalk, the second cathode is connected with the first cathode in parallel, the problem that the brightness of the display panel is not uniform due to the fact that the voltage drop of the first cathode is large is solved, the voltage drop of the cathodes is reduced, and the brightness uniformity of the display panel is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of display technology, and in particular to a display panel and a method for preparing the same. Background Art

[0002] Silicon-based organic light-emitting diodes (OLEDs) generally have a resolution of at least 2K*2K, and the current maximum is 4K*4K. Due to the high resolution, a corresponding voltage drop will occur at the cathode, that is, the voltages at both ends of the anode and cathode of the OLED at different pixel locations vary greatly, resulting in a large change in the brightness uniformity of the product.

[0003] In order to solve the problem of brightness uniformity, the voltage is increased at the corresponding position for compensation, but this method indirectly increases the power consumption of the display panel. Summary of the invention

[0004] The present invention provides a display panel and a preparation method thereof, so as to solve the problems of large cathode voltage drop and uneven brightness of organic light emitting diodes in the prior art.

[0005] According to one aspect of the present invention, there is provided a display panel, comprising: a planar layer, a plurality of anodes, a light-emitting layer and a cathode arranged in a stacked manner;

[0006] The display panel further includes a groove that at least partially penetrates the planar layer, and the groove is located between two adjacent anodes;

[0007] The light emitting layer covers the anode and the groove;

[0008] The cathode comprises a first cathode and a second cathode which are stacked, the first cathode covers the light emitting layer and the groove, the second cathode is arranged on a side of the first cathode away from the light emitting layer, and the second cathode is connected to the first cathode.

[0009] Optionally, the light-emitting layer covering the groove has cracks in the groove;

[0010] The first cathode covering the groove has cracks in the groove.

[0011] Optionally, the display panel further includes a filling structure;

[0012] The filling structure is arranged in the groove and is located at a side of the first cathode away from the light-emitting layer.

[0013] Optionally, the display panel further includes a first encapsulation layer, and the first encapsulation layer is arranged between the first cathode and the second cathode;

[0014] The encapsulation layer includes an opening, and the first cathode and the second cathode are connected through the opening.

[0015] Optionally, the anode includes a central portion and a peripheral portion, the peripheral portion surrounding the central portion;

[0016] The orthographic projection of the opening on the plane where the anode is located overlaps with the peripheral portion.

[0017] Optionally, the opening area of ​​the opening is positively correlated with the depth of the groove.

[0018] Optionally, the display panel further includes an isolation structure;

[0019] The isolation structure includes a side wall covering at least one side of the anode close to the groove.

[0020] Optionally, the groove includes a connected bottom surface and side walls;

[0021] The angle between the side wall and the bottom surface is less than or equal to 90°.

[0022] According to another aspect of the present invention, a method for preparing a display panel is provided, which is used to prepare a display panel;

[0023] The preparation method comprises:

[0024] providing a flat layer and preparing an anode layer on one side of the flat layer;

[0025] etching the anode layer to form an anode and etching the flat layer corresponding to the gap between the anodes to form a groove;

[0026] A light-emitting layer is prepared on the side of the anode away from the flat layer; wherein the light-emitting layer covers the anode and the groove;

[0027] A first cathode is prepared on the side of the light-emitting layer away from the anode; wherein the first cathode covers the light-emitting layer and the groove;

[0028] A second cathode is prepared on a side of the first cathode away from the light-emitting layer; wherein the second cathode is connected to the first cathode.

[0029] Optionally, before preparing the second cathode on the side of the first cathode away from the light-emitting layer, the method further comprises:

[0030] A filling structure is prepared on a side of the first cathode away from the light-emitting layer to fill the groove.

[0031] The technical solution of the embodiment of the present invention is to prepare two layers of cathodes on the basis of preparing grooves in the flat layer to improve lateral crosstalk, and the second cathode is connected in parallel with the first cathode to improve the problem of large voltage drop of the first cathode, which leads to uneven brightness of the display panel, reduce the cathode voltage drop, and improve the brightness uniformity of the display panel.

[0032] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0034] Figure 1 is a schematic structural diagram of a first display panel provided according to an embodiment of the present invention;

[0035] Figure 2 is a schematic structural diagram of a second display panel provided according to an embodiment of the present invention;

[0036] Figure 3 is a schematic structural diagram of a third display panel provided according to an embodiment of the present invention;

[0037] Figure 4 is a flow chart of preparing a first display panel provided according to an embodiment of the present invention;

[0038] Figure 5 is a flow chart of preparing a second display panel provided according to an embodiment of the present invention;

[0039] Figure 6 is a structural diagram corresponding to a preparation process of a second display panel provided in an embodiment of the present invention;

[0040] Figure 7 is a flow chart of preparing a second display panel provided according to an embodiment of the present invention;

[0041] Figure 8 It is a structural diagram corresponding to the preparation process of the second display panel provided according to an embodiment of the present invention. DETAILED DESCRIPTION

[0042] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0043] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0044] Figure 1 is a schematic structural diagram of a first display panel provided according to an embodiment of the present invention, Figure 2 is a schematic diagram of the structure of a second display panel provided according to an embodiment of the present invention. Figure 1 and Figure 2 As shown, the display panel includes:

[0045] A flat layer 1, a plurality of anodes 2, a light-emitting layer 3 and a cathode 4 are stacked;

[0046] The display panel further includes a groove 10 at least partially penetrating the flat layer 1 , and the groove 10 is located between two adjacent anodes 2 ;

[0047] The light-emitting layer 3 covers the anode 2 and the groove 10;

[0048] The cathode 4 includes a first cathode 41 and a second cathode 42 which are stacked. The first cathode 41 covers the light emitting layer 3 and the groove 10 . The second cathode 42 is arranged on a side of the first cathode 41 away from the light emitting layer 3 , and the second cathode 42 is connected to the first cathode 41 .

[0049] The organic light-emitting diode is prepared on the flat layer 1, and includes an anode 2, a light-emitting layer 3 and a cathode 4. The light-emitting layer 3 can be controlled to emit light by applying an electrical signal to the anode 2 and the cathode 4. In some embodiments, a connection structure can be prepared in the flat layer 1, and the connection structure penetrates the flat layer 1 and connects the electrode in the organic light-emitting diode to the driving substrate, and the driving substrate controls the operation of the organic light-emitting diode.

[0050] Among them, the anode 2 is arranged on one side of the flat layer 1, and multiple anodes 2 are arranged in an array with gaps between the anodes 2 and the anodes 2. The light-emitting layer 3 includes light-emitting units corresponding to the anodes 2, and the corresponding light-emitting units are controlled to emit light by applying electrical signals to different anodes 2 and cathodes 4. In the prior art, since the light-emitting layer 3 is set as a whole layer and the charge has good conductivity, the carriers are easily transferred between two adjacent light-emitting units, thereby causing the problem of lateral crosstalk in the display panel. In order to improve this, a groove 10 is set in the flat layer 1 corresponding to the adjacent anodes 2. The preparation of the groove 10 can be prepared after etching to generate the anode 2. When the light-emitting layer 3 is prepared subsequently, the light-emitting layer 3 prepared as a whole layer will be broken or unevenly distributed in the groove 10 due to the unevenness of the groove 10, thereby increasing the limitation of the lateral transmission of the carriers, thereby improving the lateral crosstalk of the light-emitting layer 3 and improving the color gamut of the display panel.

[0051] However, in the display panel, since the cathode 4 is a common cathode 4, the groove 10 improves the lateral crosstalk while also increasing the unevenness of the cathode 4 or the problem of material breaking, which results in a large change in the anode 2 and cathode 4 at both ends of the light-emitting unit at different positions, which results in the problem of uneven brightness of the display panel. Therefore, two layers of cathode 4 are provided in the embodiment of the present invention, namely the first cathode 41 and the second cathode 42. The first cathode 41 can be prepared on the basis of the light-emitting layer 3 covering the groove 10. Since the groove 10 also exists on the surface of the display panel after covering, after preparing the entire layer of the first cathode 41, the first cathode 41 is distributed in the groove 10 and on the surface of the light-emitting layer 3 corresponding to the anode 2. This increases the surface area of ​​the uneven first cathode 41 relative to the flat first cathode 41, and thus the resistance of the first cathode 41 becomes larger, making the voltage drop problem more obvious. At the same time, the first cathode 41 may also have the problem of material breaking, further affecting the normal operation of the display panel. Therefore, a second cathode 42 is prepared based on the first cathode 41. The second cathode 42 is connected to the first cathode 41. On the one hand, the disconnected first cathode 41 can be connected. On the other hand, being connected in parallel with the first cathode 41 can reduce the resistance of the cathode 4, improve the voltage drop problem of the cathode 4, and improve the brightness uniformity.

[0052] It is understandable that the materials of the first cathode 41 and the second cathode 42 may be the same or different. The first cathode 41 may be indium tin oxide or silver, and the second cathode 42 may be indium tin oxide to ensure the performance of the display panel.

[0053] The technical solution of the embodiment of the present invention is to prepare two layers of cathodes on the basis of preparing grooves in the flat layer to improve lateral crosstalk, and the second cathode is connected in parallel with the first cathode to improve the problem of large voltage drop of the first cathode, which leads to uneven brightness of the display panel. While solving the lateral crosstalk of the light-emitting layer, it reduces the cathode voltage drop and improves the brightness uniformity of the display panel.

[0054] Optional, continue to refer to Figure 2 As shown, the light emitting layer 3 covering the groove 10 has cracks in the groove 10;

[0055] The first cathode 41 covering the groove 10 has cracks in the groove 10 .

[0056] Among them, by preparing the shape and size of the groove 10, the light-emitting layer 3 covering the groove 10 can have cracks in the groove 10, thereby fundamentally changing the problem of lateral crosstalk of the light-emitting layer 3. For example, the depth of the groove 10 can be increased, so that when preparing the light-emitting layer 3, the light-emitting layer 3 can be divided by using the problem of difficulty in connecting the side wall and the bottom surface, ensuring that the light-emitting layer 3 is disconnected and eliminating the problem of lateral crosstalk of the light-emitting layer 3; the angle between the side wall and the bottom surface of the groove 10 can also be reduced, so that the light-emitting layer 3 can only cover the bottom surface during preparation, reducing the coverage of the side wall, and thus achieving the purpose of having cracks in the groove 10.

[0057] Among them, when preparing the first cathode 41, since the first cathode 41 is prepared above the light-emitting layer 3, when the depth of the groove 10 is deeper or the angle between the side wall of the groove 10 and the bottom surface is smaller, the first cathode 41 covering the groove 10 also has cracks in the groove 10. At this time, a whole layer of the second cathode 42 is arranged above the first cathode 41, and the second cathode 42 is connected in parallel with each disconnected first cathode 41, thereby reducing the overall resistance of the cathode 4, further reducing the voltage drop of the cathode 4, and ensuring the normal operation of the display panel.

[0058] It can be understood that the presence of cracks in the light-emitting layer 3 covering the groove 10 can eliminate the problem of lateral crosstalk of the light-emitting layer 3; the presence of cracks in the first cathode 41 covering the groove 10 can further reduce the resistance of the cathode 4 and reduce the voltage drop of the cathode 4 when the second cathode 42 is connected in parallel with the first cathode 41.

[0059] The technical solution of the embodiment of the present invention eliminates the problem of lateral crosstalk of the light-emitting layer and greatly reduces the cathode voltage drop, thereby improving the uniformity of the brightness of the display panel by arranging a crack in the light-emitting layer covering the groove and a crack in the first cathode covering the groove.

[0060] Optional, continue to refer to Figure 1 As shown, the display panel further includes a filling structure 5;

[0061] The filling structure 5 is disposed in the groove 10 and is located on a side of the first cathode 41 away from the light-emitting layer 3 .

[0062] Among them, since the display panel surface is still uneven after the first cathode 41 is prepared in the groove 10, that is, the groove 10 still exists, the filling structure 5 is prepared before preparing the second cathode 42, and the filling structure 5 can be OC glue. The filling structure 5 is arranged in the groove 10, so that the display panel surface is flat before preparing the second cathode 42, which increases the flatness of the second cathode 42. At the same time, when the second cathode 42 is connected in parallel with the first cathode 41, the resistance of the cathode 4 can be further reduced, the voltage drop of the cathode 4 can be reduced, and the uniformity of the brightness of the display panel can be improved.

[0063] Optional, continue to refer to Figure 1 As shown, the display panel further includes a first encapsulation layer 61, and the first encapsulation layer 61 is disposed between the first cathode 41 and the second cathode 42;

[0064] The encapsulation layer includes an opening 610 through which the first cathode 41 and the second cathode 42 are connected.

[0065] Among them, the first encapsulation layer 61 can be an organic thin film encapsulation layer, and the first encapsulation layer 61 can have the function of preventing water vapor. Setting the first encapsulation layer 61 between the first cathode 41 and the second cathode 42 can protect the light-emitting layer 3 under the first encapsulation layer 61 from being corroded by water vapor, enhance the water and oxygen barrier ability of the display panel, and ensure the life of the display panel.

[0066] Specifically, since the first cathode 41 and the second cathode 42 need to be connected, the opening 610 needs to be etched when preparing the first encapsulation layer 61 , so that the first cathode 41 and the second cathode 42 are connected through the opening 610 .

[0067] In some embodiments, the first encapsulation layer 61 can also be arranged in the groove 10. Since the light-emitting layer 3 also exists in the groove 10, the water and oxygen barrier capability of the display panel can be further improved by arranging the first encapsulation layer 61 in the groove 10. At the same time, a glue layer can be prepared on the basis of the first encapsulation layer 61, and an opening 610 is prepared on the surface of the first encapsulation layer 61 by exposure, development, etc., and the glue layer on the surface of the display panel is removed, leaving only the glue layer in the groove 10, that is, forming a filling structure 5, which ensures both the preparation of the first encapsulation layer 61 and the flatness of the surface of the display panel.

[0068] In some embodiments, after the second cathode 42 is prepared, a second encapsulation layer 62 is further prepared on a side of the second cathode 42 away from the first encapsulation layer 61 to complete the encapsulation of the display panel and ensure the reliability of the display panel.

[0069] The technical solution of the embodiment of the present invention is to prepare a first encapsulation layer between the first cathode and the second cathode, so that the first encapsulation layer can protect the light-emitting layer from being corroded by water vapor, thereby improving the water and oxygen barrier capacity of the display panel and ensuring the life of the display panel.

[0070] Optional, continue to refer to Figure 1 As shown, the anode 2 includes a central portion 21 and a peripheral portion 22, and the peripheral portion 22 surrounds the central portion 21;

[0071] The orthographic projection of the opening 610 on the plane where the anode 2 is located overlaps with the peripheral portion 22 .

[0072] Among them, the outer portion 22 of the anode 2 is connected to the groove 10 of the flat layer 1, and the outer portion 22 of the anode 2 is also connected to the central portion 21 of the anode 2. Since the light-emitting layer 3 is prepared as a whole layer, there will be problems of material breakage or uneven preparation from the edge of the anode 2 to the groove 10, so the anode 2 is divided into a central portion 21 and a peripheral portion 22. Since the light-emitting layer 3 corresponding to the central portion 21 has better preparation flatness, the central portion 21 of the anode 2 can be the main working area; since the light-emitting layer 3 corresponding to the peripheral portion 22 has poor flatness, the opening 610 of the first encapsulation layer 61 is set at a position corresponding to the outer portion 22 of the anode 2, that is, the orthographic projection of the opening 610 on the plane where the anode 2 is located overlaps with the peripheral portion 22, so that even if the opening 610 of the first encapsulation layer 61 is eroded by water vapor, the impact on the light-emitting layer 3 corresponding to the working area will be reduced, thereby ensuring the normal operation of the display panel.

[0073] In the embodiment of the present invention, by arranging the opening of the first encapsulation layer in the area where its orthographic projection overlaps with the outer periphery of the anode, even if water vapor erosion occurs at the opening of the first encapsulation layer, the impact on the light-emitting layer corresponding to the working area can be reduced, thereby ensuring the normal operation of the display panel.

[0074] Optional, continue to refer to Figure 1 As shown, the area of ​​the opening 610 is positively correlated with the depth of the groove 10 .

[0075] Among them, since the depth of the groove 10 is deeper, the resistance of the first cathode 41 is greater while it is continuously connected, which in turn causes a greater voltage drop at the cathode 4; the larger the area of ​​the opening 610, the smaller the resistance of the first cathode 41 and the second cathode 42 after being connected in parallel. Therefore, when the depth of the groove 10 is greater, the area of ​​the opening 610 can be increased, so that the connection area between the first cathode 41 and the second cathode 42 is increased, and the second cathode 42 neutralizes the large resistance of the first cathode 41, reduces the voltage drop of the cathode 4, and ensures the uniformity of the brightness of the display panel.

[0076] Optional, continue to refer to Figure 1 As shown, the display panel further includes an isolation structure 7;

[0077] The isolation structure 7 includes a side wall covering at least one side of the anode 2 close to the groove 10 .

[0078] Among them, the isolation structure 7 can be used to prevent the cathode 4 from being short-circuited with the anode 2. The isolation structure 7 can be an insulating material. Since the light-emitting layer 3 covers the anode 2 and the groove 10, and the groove 10 is arranged between the anode 2 and the anode 2, the light-emitting layer 3 is prone to be disconnected at the side wall of the anode 2 close to the groove 10, or the side wall and the bottom surface are disconnected. Therefore, the isolation structure 7 is arranged to at least cover the side wall of the anode 2 close to the groove 10, so that when the first cathode 41 is prepared on one side of the light-emitting layer 3, the first cathode 41 will not be connected to the anode 2 through the disconnected area of ​​the light-emitting layer 3, affecting the normal operation of the display panel.

[0079] In some embodiments, in order to further ensure the isolation effect of the isolation structure 7, the isolation structure 7 is provided on the bottom of the groove 10, the side wall of the groove 10, the side wall of the anode 2, and the upper surface of the part connected to the side wall of the anode 2, so as to ensure that the isolation structure 7 fully isolates the first cathode 41 from the anode 2. On this basis, the opening 610 can also be set at the position corresponding to the upper surface of the anode 2 covered by the isolation structure 7, because the light-emitting layer 3 corresponding to the position cannot be driven to work due to the isolation structure 7 being set on the upper surface of the anode 2. The opening 610 is set at the corresponding position of the isolation structure 7, which ensures the normal connection between the first cathode 41 and the second cathode 42, and does not affect the normal operation of other positions of the light-emitting layer 3.

[0080] The technical solution of the embodiment of the present invention provides an isolation structure in the display panel, so that the isolation structure includes a side wall at least covering the anode on one side close to the groove, thereby avoiding the connection between the anode and the cathode and ensuring the normal operation of the display panel.

[0081] Optional, Figure 3 is a schematic diagram of the structure of a third display panel provided according to an embodiment of the present invention. Figure 1 and Figure 3 As shown, the groove 10 includes a bottom surface 101 and a side wall 102 connected;

[0082] The angle between the side wall 101 and the bottom surface 102 is less than or equal to 90°.

[0083] Among them, the groove 10 includes a connected bottom surface 101 and a side wall 102. The angle between the side wall 101 and the bottom surface 102 is set to be less than or equal to 90° because when the angle between the side wall 101 and the bottom surface 102 is greater than 90° or closer to 180°, the corresponding interior of the groove 10 is flatter, and the probability of the light-emitting layer 3 being disconnected in the groove 10 is smaller, which cannot prevent lateral crosstalk.

[0084] For example, when the angle between the side wall 101 and the bottom surface 102 is equal to 90°, Figure 1 As shown, the right angle between the side wall and the bottom surface is most likely to cause disconnection; when the angle between the side wall 101 and the bottom surface 102 is less than 90°, such as Figure 3 As shown, disconnection will inevitably occur at the corresponding angle between the side wall 101 and the bottom surface 102, thereby eliminating the problem of lateral crosstalk.

[0085] In some embodiments, since the groove 10 is prepared after the anode 2 is prepared, in order to ensure the preparation effect of the groove 10, the angle between the side wall and the lower surface of the anode 2 can be etched into an acute angle, such as 60°, to ensure that there is enough space to prepare the groove 10 later.

[0086] The technical solution of the embodiment of the present invention ensures the performance of the groove in preventing lateral crosstalk of the light-emitting layer by setting the angle between the side wall and the bottom surface to be less than or equal to 90°.

[0087] Based on the same inventive concept, Figure 4 is a flow chart of preparing a first display panel according to an embodiment of the present invention, such as Figure 4 As shown, an embodiment of the present invention provides a method for preparing a display panel, which is used to prepare a display panel;

[0088] The preparation method comprises:

[0089] S10, providing a planar layer and preparing an anode layer on one side of the planar layer.

[0090] The organic light emitting diode is prepared on the flat layer 1 , and an anode layer 20 is prepared on one side of the flat layer 1 . The anode layer is a metal layer, and the sum of the thickness of the flat layer and the anode layer may be no less than 500 nm.

[0091] S11, etching the anode layer to form an anode and etching the flat layer corresponding to the gap between the anodes to form a groove.

[0092] The anode 2 layer is etched to form a plurality of anodes 2 arranged in an array on the surface of the flat layer 1, and the anodes 2 are not connected to each other and there are gaps between the anodes 2. After the anodes 2 are prepared, the flat layer 1 corresponding to the gaps is etched to form grooves 10 between the anodes 2 and the anodes 2.

[0093] In some embodiments, the angle between the bottom surface of the groove 10 and the side wall may be 90°, and the angle between the lower surface of the anode 2 and the side wall may be 60°.

[0094] S12, preparing a light-emitting layer on the side of the anode away from the flat layer, wherein the light-emitting layer covers the anode and the groove.

[0095] Wherein, the light-emitting layer 3 is prepared on the side of the anode 2 away from the flat layer 1. The light-emitting layer 3 may be disconnected or unevenly distributed in the groove 10 due to the presence of the groove 10, thereby increasing the limitation of the lateral transport of carriers, thereby improving the lateral crosstalk of the light-emitting layer 3 and improving the color gamut of the display panel. The figure shows a schematic diagram of the light-emitting layer 3 without disconnection. It can be understood that even if the light-emitting layer 3 is not disconnected, the effect of the groove 10 will increase the difficulty of lateral crosstalk of carriers.

[0096] S13, preparing a first cathode on the side of the light-emitting layer away from the anode, wherein the first cathode covers the light-emitting layer and the groove.

[0097] Among them, the first cathode 41 can be prepared on the basis of the light-emitting layer 3 covering the groove 10, and the material of the first cathode 41 can be indium tin oxide, and the thickness can be 10 to 30nm; or the material of the first cathode 41 can be silver, and the thickness can be 10 to 15nm. Since the groove 10 also exists on the surface of the display panel after covering, after preparing the whole layer of the first cathode 41, the first cathode 41 is distributed in the groove 10 and on the surface of the light-emitting layer 3 corresponding to the anode 2, which makes the surface area of ​​the uneven first cathode 41 increase relative to the flat first cathode 41, and then the resistance of the first cathode 41 becomes larger, making the voltage drop problem more obvious. At the same time, the first cathode 41 may also have the problem of material breaking, further affecting the normal operation of the display panel. Therefore, the second cathode 42 is prepared on the basis of the first cathode 41.

[0098] S14, preparing a second cathode on a side of the first cathode away from the light-emitting layer, wherein the second cathode is connected to the first cathode.

[0099] The second cathode 42 may be made of indium tin oxide or silver. When the indium tin oxide material is used, the thickness may be 100 to 300 nm. When the silver material is used, the thickness may be 10 to 15 nm. The second cathode 42 is connected to the first cathode 41. On the one hand, the disconnected first cathode 41 can be connected. On the other hand, the second cathode 42 can be connected in parallel with the first cathode 41 to reduce the resistance of the cathode 4, improve the voltage drop of the cathode 4, and improve the brightness uniformity.

[0100] The technical solution of the embodiment of the present invention is to prepare two layers of cathodes on the basis of preparing grooves in the flat layer to improve lateral crosstalk, and the second cathode is connected in parallel with the first cathode to improve the problem of large voltage drop of the first cathode, which leads to uneven brightness of the display panel. While solving the lateral crosstalk of the light-emitting layer, it reduces the cathode voltage drop and improves the brightness uniformity of the display panel.

[0101] Based on the above embodiments, Figure 5 is a flow chart of preparing a second display panel according to an embodiment of the present invention, Figure 6is a structural diagram corresponding to the preparation process of the second display panel provided in an embodiment of the present invention, such as Figure 5 and Figure 6 As shown, the preparation method comprises:

[0102] S20, providing a flat layer and preparing an anode layer on one side of the flat layer. Figure 6 Middle f step.

[0103] S21, etching the anode layer to form an anode and etching the flat layer corresponding to the gap between the anodes to form a groove. Figure 6 Middle g step.

[0104] S22, preparing a light-emitting layer on the side of the anode away from the flat layer, wherein the light-emitting layer covers the anode and the groove. Figure 6 Middle h step.

[0105] S23, preparing a first cathode on the side of the light-emitting layer away from the anode. The first cathode covers the light-emitting layer and the groove. Figure 6 Step i.

[0106] S24, preparing a filling structure on the side of the first cathode away from the light-emitting layer to fill the groove. Figure 6 Middle j step.

[0107] Among them, since the display panel surface is still uneven after the first cathode 41 is prepared in the groove 10, that is, the groove 10 still exists, the filling structure 5 is prepared before preparing the second cathode 42, and the filling structure 5 can be OC glue. The filling structure 5 is arranged in the groove 10, so that the display panel surface is flat before preparing the second cathode 42, which increases the flatness of the second cathode 42. At the same time, when the second cathode 42 is connected in parallel with the first cathode 41, the resistance of the cathode 4 can be further reduced, the voltage drop of the cathode 4 can be reduced, and the uniformity of the brightness of the display panel can be improved.

[0108] S25, preparing a second cathode on the side of the first cathode away from the light-emitting layer. The second cathode is connected to the first cathode. Figure 6 Middle k steps.

[0109] The technical solution of the embodiment of the present invention prepares a filling structure filling groove on the side of the first cathode away from the light-emitting layer, so that the second cathode has better flatness after preparation, which can further reduce the resistance of the cathode, reduce the voltage drop of the cathode, and improve the uniformity of the brightness of the display panel.

[0110] Based on the above embodiments, Figure 7 is a flow chart of preparing a second display panel according to an embodiment of the present invention, Figure 8 is a structural diagram corresponding to the preparation process of the second display panel provided in an embodiment of the present invention, such as Figure 7 and Figure 8 As shown, the preparation method comprises:

[0111] S30, providing a flat layer and preparing an anode layer on one side of the flat layer. Figure 8 Middle step.

[0112] S31, etching the anode layer to form an anode and etching the flat layer corresponding to the gap between the anodes to form a groove. Figure 8 Middle m step.

[0113] S32, preparing an isolation structure on the bottom surface of the groove, the side wall of the groove, the side wall of the anode and a portion of the upper surface of the anode. Figure 8 The thickness of the isolation structure 7 may be 10-30 nm.

[0114] S33, preparing a light-emitting layer on the side of the anode away from the flat layer, wherein the light-emitting layer covers the anode and the groove. Figure 8 Middle o step.

[0115] S34, preparing a first cathode on the side of the light-emitting layer away from the anode. The first cathode covers the light-emitting layer and the groove. Figure 8 Middle p step.

[0116] S35, preparing a first encapsulation layer on the side of the first cathode away from the light-emitting layer. The first encapsulation layer may include an aluminum oxide material with a thickness greater than or equal to 5 nm. Figure 8 Middle q step.

[0117] S36, preparing a glue layer on the side of the first encapsulation layer away from the first cathode; and removing the glue layer on the surface of the display panel after the opening is prepared in the first encapsulation layer by exposure, development and etching, so that the glue layer fills the groove to form a filling structure. Figure 8 Middle r step.

[0118] S37, preparing a second cathode on a side of the first cathode away from the light-emitting layer, wherein the second cathode is connected to the first cathode. Figure 8 Middle s step.

[0119] The technical solution of the embodiment of the present invention is to prepare two layers of cathode on the basis of preparing grooves in the flat layer to improve lateral crosstalk, which is equivalent to forming a cathode ring around the light-emitting unit, which can greatly reduce the cathode voltage drop, improve the brightness uniformity, and reduce the overall power consumption of the display panel; at the same time, the presence of the grooves solves the problem of lateral crosstalk in the light-emitting layer; due to the presence of the first encapsulation layer, the water and oxygen barrier ability of the product is enhanced, so that its life is longer in a double 85 environment.

[0120] It should be understood that the various forms of processes shown above can be used to reorder, add or delete steps. For example, the steps described in the present invention can be executed in parallel, sequentially or in different orders, as long as the desired results of the technical solution of the present invention can be achieved, and this document does not limit this.

[0121] The above specific implementations do not constitute a limitation on the protection scope of the present invention. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A display panel, characterized in that: include: A planar layer, a plurality of anodes, a light-emitting layer and a cathode are stacked; The display panel further comprises a groove that at least partially penetrates the planar layer, and the groove is located between two adjacent anodes; The light-emitting layer covers the anode and the groove; The cathode comprises a first cathode and a second cathode which are stacked, wherein the first cathode covers the light emitting layer and the groove, and the second cathode is arranged on a side of the first cathode away from the light emitting layer, and the second cathode is connected to the first cathode.

2. The display panel according to claim 1, characterized in that: The light-emitting layer covering the groove has cracks in the groove; The first cathode covering the groove has cracks in the groove.

3. The display panel according to claim 1, characterized in that: The display panel further includes a filling structure; The filling structure is arranged in the groove and is located on a side of the first cathode away from the light-emitting layer.

4. The display panel according to claim 1, characterized in that: The display panel further includes a first encapsulation layer, wherein the first encapsulation layer is disposed between the first cathode and the second cathode; The encapsulation layer includes an opening, and the first cathode and the second cathode are connected through the opening.

5. The display panel according to claim 4, characterized in that: The anode includes a central portion and a peripheral portion, the peripheral portion surrounding the central portion; The orthographic projection of the opening on the plane where the anode is located overlaps with the peripheral portion.

6. The display panel according to claim 4, characterized in that: The opening area of ​​the opening is positively correlated with the depth of the groove.

7. The display panel according to claim 1, characterized in that: The display panel also includes an isolation structure; The isolation structure includes a side wall at least covering a side of the anode close to the groove.

8. The display panel according to claim 1, characterized in that: The groove includes a connected bottom surface and side walls; An included angle between the side wall and the bottom surface is less than or equal to 90°.

9. A method for preparing a display panel, characterized in that: Used to prepare a display panel according to any one of claims 1 to 8; The preparation method comprises: Providing a flat layer and preparing an anode layer on one side of the flat layer; etching the anode layer to form an anode and etching the anode and a flat layer corresponding to a gap between the anodes to form a groove; A light-emitting layer is prepared on the side of the anode away from the flat layer; wherein the light-emitting layer covers the anode and the groove; A first cathode is prepared on the side of the light-emitting layer away from the anode; wherein the first cathode covers the light-emitting layer and the groove; A second cathode is prepared on a side of the first cathode away from the light-emitting layer; wherein the second cathode is connected to the first cathode.

10. The preparation method according to claim 9, characterized in that: Before preparing the second cathode on the side of the first cathode away from the light-emitting layer, the method further comprises: A filling structure is prepared on a side of the first cathode away from the light-emitting layer to fill the groove.