Method for producing periodate via anodic oxidation in steady-state reactor
By anodizing the iodine compound with an oxidation state of -1 to +V in the electrolytic cell, and preparing metal secondary periodate is performed using a continuous stirred tank reactor, the blockage and blockage in the production of secondary periodate are solved. The problem of low efficiency has achieved stable and efficient production.
Patent Information
- Application Number
- CN202380031187.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-05
- Filing Date
- 2023-04-05
- Publication Date
- 2024-11-26
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The prior art is prone to clogging when producing secondary periodates, which damages the electrolytic cell efficiency and leads to damage to the anode, and is difficult to scale up and continuously produce.
By anodizing the iodine compound with an oxidation state of -1 to +V in an electrolytic cell, the preparation of metal secondary periodate is performed using a continuous stirred tank reactor, so as to realize the recycling of the anolyte and steady-state molar ratio control of the anolyte electrolyte and the control of the steady-state molar ratio , avoid blockage.
Continuous or semi-continuous production of secondary periodates is achieved, avoiding or reducing clogging, improving the stability and production efficiency of the electrolytic cell, and is suitable for various iodine starting materials.
Smart Images

Figure HDA0005063780940000011 
Figure HDA0005063780940000021
Abstract
Description
[0001] The present invention relates to a process for preparing secondary metal periodates by anodic oxidation of iodine compounds in oxidation states ranging from -I to +V in an electrolytic cell under specific conditions, and to an apparatus for carrying out the reaction. Technical Background
[0002] Periodates are strong oxidizing agents widely used in chemical syntheses. There is a continuous need for economical processes for their production and production methods that comply with specific regulations, especially if periodates are used at some point in the synthesis of products for the pharmaceutical, cosmetic or nutritional fields.
[0003] Periodate or periodic acid can be produced electrochemically by anodic oxidation starting from elemental iodine or from iodine salts in which the iodine is in an oxidation state below +VII.
[0004] A common challenge in the production of periodate is the different solubility of iodine-containing species, which severely hinders electrolytic performance. Iodine is converted into iodide ions (I -– ) and hypoiodite (HIO) and are soluble in alkaline media, but they are insoluble in neutral to acidic media. In contrast, periodate is soluble in aqueous acids that form orthoperiodic acid (H5IO6), but is insoluble in alkaline media because it forms secondary periodate (Na3H2IO6). If iodine and secondary periodate are separated out, this damages the efficiency of electrolysis due to coating anode surfaces and separators. In addition, the blocking of the flow electrolytic cell may occur, which immediately interrupts electrolysis and may cause damage to the electrolytic cell.
[0005] WO 2021 / 110928 relates to a method for preparing metal periodates by anodizing metal iodides using carbon-based anodes. The method is preferably carried out under alkaline conditions. Similarly, S.Arndt et al. describe the electrochemical synthesis of sodium periodate by anodizing sodium iodide using boron-doped diamond (boron-doped diamond, BDD) electrodes under alkaline conditions in Angew.Chem.2020,132,8112-8118. In these documents, secondary periodates are obtained in high yield and high purity. However, the inventors found that when the reaction is scaled up under the conditions of these documents, due to the formation of solid periodate precipitates in the electrolytic cell, blockage may occur to an undesirable extent. Blockage is not only a maintenance problem that requires disassembly and cleaning of the electrolytic cell, but may also cause high back pressure and even damage to the anode.
[0006] US 4,687,565 relates to an electrolytic cell for producing periodate, the electrolytic cell comprising: a plurality of cathodes mounted vertically parallel to the long sides of the cell body and spaced apart from each other at equal intervals, a plurality of open anode compartment boxes having plate separators suitable for maintaining equal intervals between the cathodes, one or more anodes inserted into the anode compartment boxes, a plurality of polyvinyl chloride (PVC) diaphragms mounted on both sides of the anode compartment box parallel to the cathodes, an anode electrolyte inlet mounted at the lower part of the anode compartment box, an anode electrolyte outlet at the upper part of the opposite side of the box, a cell cover mounted on the cell body with an air inlet hole and a cell gas exhaust pipe, and a perforated PVC cover for the cathode compartment located between the cell cover and the upper liquid surface of the cathode electrolyte.
[0007] US 5,074,975 relates to a process for the simultaneous electrosynthesis of alkaline peroxides and oxygen-containing halogen salts of alkali metals, and to a reactor for carrying out said reaction. The reactor comprises an oxygen-reducing cathode (which is advantageously porous) and a halogen-generating anode separated by an anion-permeable wall (which is advantageously an anion exchange membrane).
[0008] The object of the invention is to provide a method for producing secondary periodate, which allows easy scaling up, can be carried out continuously or semi-continuously, and avoids or at least reduces blocking. In addition, the method should not be limited to the oxidation of metal iodides, but should be applicable to all types of iodine starting materials. In a specific embodiment, the method should also allow the use of starting materials in dispersed form (e.g., dissolved or suspended) or in solid form, online separation of desired products and / or recycling of electrolyte. Summary of the invention
[0009] The inventors have found that clogging can be avoided or at least significantly reduced if, in the anodic oxidation of the iodine compound to the desired (secondary) periodate, an anode electrolyte comprising a metal periodate and an iodine compound in an oxidation state of -I to +V is recycled to the anode compartment via an anode electrolyte loop, and the anode electrolyte loop comprises a continuously stirred tank reactor operating in a steady-state mode relative to the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +V in the anode electrolyte. In particular, when the anode electrolyte is reintroduced into the anode compartment, the anode electrolyte recycled through the anode compartment is not completely depleted of the target secondary periodate or any periodate (i.e., any iodine salt having an iodine atom in an oxidation state of +VII; a more detailed definition is given below), but rather contains a large amount of the target secondary periodate or any periodate.
[0010] The present invention therefore relates to a method for preparing a metal secondary periodate by anodic oxidation of an iodine compound having an oxidation state ranging from -I to +V in an electrolytic cell comprising an anodic compartment having one or more anodes, a cathodic compartment having one or more cathodes, and a separator arranged between the anodic compartment and the cathodic compartment, the method comprising:
[0011] recirculating the cathode electrolyte to the cathode compartment via a cathode electrolyte loop,
[0012] recirculating an anolyte to the anode compartment via an anolyte loop, the anolyte comprising a metal periodate and an iodine compound in an oxidation state ranging from -I to +V, the iodine compound being selected from an iodine salt (in an oxidation state ranging from -I to +V, of course), elemental iodine, a mixture of different iodine salts (in an oxidation state ranging from -I to +V, of course), or a mixture of iodine and one or more iodine salts (in an oxidation state ranging from -I to +V, of course),
[0013] The anodic oxidation of the iodine compound is carried out at a pH of at least 10, wherein the anode electrolyte loop comprises at least one continuously stirred tank reactor operated in a steady-state mode relative to the total molar ratio of metal periodate to iodine compound with oxidation states ranging from -I to +V in the anode electrolyte, wherein the continuously stirred tank reactor is operated in a "steady-state" mode by continuously or periodically feeding the iodine compound with oxidation states ranging from -I to +V into the continuous stirred tank reactor and continuously or periodically removing the metal periodate from the continuous stirred tank reactor.
[0014] Furthermore, the present invention relates to an apparatus configured to prepare a metal secondary periodate by the method of the present invention, i.e. preparing a metal secondary periodate by continuous anodic oxidation of an iodine compound, the apparatus comprising:
[0015] An electrolytic cell comprising an anode compartment having one or more anodes, a cathode compartment having one or more cathodes, and a separator arranged between the anode compartment and the cathode compartment,
[0016] a cathode electrolyte loop for recirculating cathode electrolyte through the cathode compartment, the cathode electrolyte loop comprising a cathode electrolyte reservoir,
[0017] An anode electrolyte loop for circulating the anode electrolyte through the anode compartment, the anode electrolyte loop comprising at least one continuously stirred tank reactor, the at least one continuously stirred tank reactor being provided with a feeding device for feeding an iodine compound with an oxidation state of -I to +V selected from an iodine salt (of course, with an oxidation state of -I to +V), elemental iodine, a mixture of different iodine salts (of course, with an oxidation state of -I to +V) or a mixture of iodine and one or more iodine salts (of course, with an oxidation state of -I to +V) into the at least one continuously stirred tank reactor, and a discharge device for discharging the metal periodate reaction product from the at least one continuously stirred tank reactor. DETAILED DESCRIPTION
[0018] definition
[0019] Metal periodates are metal salts of various periodic acids. In periodic acid, the corresponding anion is composed of iodine in oxidation state +VII and oxygen (oxygen in oxidation state -II). Periodates especially include orthoperiodate (IO6 5- ; Thus, the molecular formula of metal periodate is M5IO6), metaperiodate (IO4 - ; Therefore, the molecular formula of metal metaperiodate is MIO4), dimesoperiodate (I2O9 4- ; The molecular formula of the metal diperiodate is M4I2O9), mesoperiodate (IO5 3- ; Thus, the molecular formula of the periodate in the metal is M3IO5) and secondary periodate. Secondary periodate is a salt with the molecular formula M3H2IO6, and is also called the corresponding double salt MIO4*2MOH. The M in the above molecular formula is the metal equivalent [(M n + ) 1 / n , where n is the charge number]; in the case of, for example, an alkali metal periodate, M is thus an alkali metal cation; and in the case of an alkaline earth metal periodate, M is (M 2+ ) 1 / 2 . In periodates with more than one negative charge, the M of more than one metal equivalent may have the same or different meanings. For example, in the secondary periodate M3H2IO6 or MIO4*2MOH, all three metal equivalents M may have the same meaning, or may be from different metals; this may occur, for example, if the starting material is an iodide salt (e.g., iodide or iodate) in which the counter cation is different from the counter cation present during the anodization or in the base used during the post-treatment of the reaction product. See below for further details.
[0020] In the terminology of the present invention, an iodine compound in an oxidation state of -1 to +V is an inorganic iodine compound in which the iodine atom has a specified oxidation state, i.e., an iodine salt or elemental iodine in an oxidation state of -1 to +V. An inorganic iodine salt in an oxidation state of -1 to +V is, for example, an iodide [(M n+ ) 1 / n (I - ); the oxidation state of the iodine atom is -I], hypoiodite [(M n+ ) 1 / n (IO - ); the oxidation state of the iodine atom is +I], iodite [(M n+ ) 1 / n (IO2 - ) - ; the oxidation state of the iodine atom is +III], and iodate [(M n+ ) 1 / n (IO3 - ) - ; The oxidation state of the iodine atom is +V], where M is a cation, usually a metal cation or an ammonium cation, and n is the charge number.
[0021] The anolyte is the liquid medium in the anode compartment; the catholyte is the liquid medium in the cathode compartment.
[0022] In the terminology of the present invention, a dispersion is a solution or a suspension. Similarly, "dispersed" means dissolved or suspended.
[0023] Operating the continuous stirred tank reactor in a "steady state mode" with respect to the total molar ratio of metal periodate to iodine compound in oxidation state -I to +V in the anode electrolyte means: selecting a predetermined molar ratio so that during operation, the actual molar ratio of metal periodate to iodine compound remains at a predetermined molar ratio (range) or close to a preselected molar ratio (range), wherein "close" means that the actual molar ratio (range) deviates from the preselected molar ratio (range) by at most ±20%, preferably at most ±10%. Since metal periodate is continuously formed during the anodic oxidation of the iodine compound in the electrolytic cell, resulting in a decrease in iodine compound in a lower oxidation state (i.e. -I to +V) and an increase in metal periodate in the anode electrolyte, steady state mode operation can only be maintained by adding iodine compound in a lower oxidation state (i.e. oxidation state -I to +V) and / or removing metal periodate. In order to keep the actual ratio within the range defined above, up to 20 mol%, preferably up to 10 mol%, more or less iodine compound in a lower oxidation state can be added to the anode electrolyte when the metal periodate is removed. The predetermined molar ratio is conveniently defined for a certain point in time in the electrolysis, for example for the anolyte prior to entering the anode compartment.
[0024] The following description of the preferred embodiments of the present invention is valid per se and preferably in any combination with each other. Unless expressly provided otherwise, the description made in the context of the preferred embodiments of the method of the present invention also applies to the device of the present invention, as long as applicable; and vice versa.
[0025] Embodiment of the invention (Ex)
[0026] General and preferred embodiments Ex are summarized in the following non-exhaustive list. Other preferred embodiments become apparent from the paragraphs following this list.
[0027] E.1. A method for preparing a metal secondary periodate by anodic oxidation of an iodine compound having an oxidation state of -I to +V in an electrolytic cell, the electrolytic cell comprising an anodic compartment having one or more anodes, a cathodic compartment having one or more cathodes and a separator arranged between the anodic compartment and the cathodic compartment, the method comprising:
[0028] recirculating the cathode electrolyte to the cathode compartment via a cathode electrolyte loop, recirculating the anode electrolyte to the anode compartment via an anode electrolyte loop, the anode electrolyte comprising a metal periodate and an iodine compound in an oxidation state of -I to +V, the iodine compound being selected from an iodine salt (in an oxidation state of -I to +V, of course), elemental iodine, a mixture of different iodine salts (in an oxidation state of -I to +V, of course), or a mixture of iodine and one or more iodine salts (in an oxidation state of -I to +V, of course),
[0029] said anodic oxidation of said iodine compound is carried out at a pH of at least 10,
[0030] wherein the anode electrolyte loop comprises at least one continuously stirred tank reactor operating in a steady-state mode relative to the total molar ratio of metal periodate to iodine compound with oxidation states ranging from -I to +V in the anode electrolyte, wherein the continuously stirred tank reactor operates in a "steady-state" mode by continuously or periodically feeding the iodine compound with oxidation states ranging from -I to +V into the continuous stirred tank reactor and continuously or periodically removing metal periodate from the continuous stirred tank reactor.
[0031] E.2. A method according to embodiment E.1, wherein the metal periodate contained in the recycled anode electrolyte is primarily metal secondary periodate.
[0032] E.3. A method according to any of the preceding embodiments, wherein in order to operate a continuous stirred tank reactor in a steady-state mode relative to the total molar ratio of metal periodate to iodine compounds with oxidation states ranging from -I to +V in the anode electrolyte, a molar ratio or molar ratio range is defined so that during operation, the actual molar ratio or molar ratio range of metal periodate to iodine compounds remains within the defined molar ratio or molar ratio range or is close to the defined molar ratio or molar ratio range, wherein "close" means that the actual molar ratio or molar ratio range may deviate from the defined molar ratio or molar ratio range by up to ±20%, wherein the molar ratio is calculated based on the iodine atoms present in the metal periodate and the iodine compound.
[0033] E.4. A method according to embodiment E.3, wherein the defined molar ratio or molar ratio range is related to the molar ratio or molar ratio range in the anode electrolyte before entering the anode compartment.
[0034] E.5. A method according to any of the preceding embodiments, wherein in the recycled anode electrolyte, the total molar ratio of the metal periodate to the iodine compounds with an oxidation state of -I to +V is 1:>0 to 1:5 (meaning that there must be some iodine compounds with an oxidation state of -I to +V; but the total amount of iodine compounds with an oxidation state of -I to +V cannot exceed the amount of metal periodate by more than 5 times its amount); wherein in the case of iodine compounds with an oxidation state of -I to +III, the total molar ratio of metal periodate to iodine compounds with an oxidation state of -I to +III is 1:0 to 8:1 (meaning that the metal periodate exceeds the total amount of iodine compounds with an oxidation state of -I to +III by at least 8 times its amount - if the latter does exist); and wherein in the case of iodine compounds with an oxidation state of +V, the total molar ratio of metal periodate to iodine compounds with an oxidation state of +V is 1:0 to 1:5 (meaning that the total amount of iodine compounds with an oxidation state of +V (if they do exist) cannot exceed the amount of metal periodate by more than 5 times its amount).
[0035] E.6. A method according to embodiment E.5, wherein the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 1:>0 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 1:0 to 1:4.
[0036] E.7. A method according to embodiment E.6, wherein the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 200:1 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 200:1 to 1:4.
[0037] E.8. A method according to any one of embodiments E.1 to E.4, wherein in the recirculating anode electrolyte, when fed to the anode compartment, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 1:>0 to 1:5 (meaning that there must be some iodine compounds with an oxidation state of -I to +V; but the total amount of iodine compounds with an oxidation state of -I to +V cannot exceed the amount of metal periodate to more than 5 times its amount); wherein in the case of the iodine compound with an oxidation state of -I to +III , the total molar ratio of metal periodate to iodine compounds in oxidation state -I to +III is from 1:0 to 8:1 (meaning that the metal periodate exceeds the total amount of iodine compounds in oxidation state -I to +III by at least 8 times their amount); and wherein in the case where the iodine compounds are in oxidation state +V, the total molar ratio of metal periodate to iodine compounds in oxidation state +V is from 1:0 to 1:5 (meaning that the total amount of iodine compounds in oxidation state +V (if present) cannot exceed the amount of metal periodate by more than 5 times their amount).
[0038] E.9. A method according to embodiment E.8, wherein the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 1:>0 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 1:0 to 1:4.
[0039] E.10. A method according to embodiment E.9, wherein the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 200:1 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 200:1 to 1:4.
[0040] E.11. A method according to any one of embodiments E.1 to E.4 and E.8 to E.10, wherein in order to operate the continuous stirred tank reactor in a steady-state mode with respect to the total molar ratio of metal periodate to iodine compound having an oxidation state of -I to +V, a molar ratio or a molar ratio range is defined for the anode electrolyte before entering the anode compartment, so that during operation, the actual molar ratio or molar ratio range of metal periodate to iodine compound in the anode electrolyte before entering the anode compartment is maintained within the defined molar ratio or molar ratio range ±20%;
[0041] wherein the defined molar ratio or molar ratio range is thereby selected such that in the anode electrolyte, before entering the anode compartment (i.e. when fed to the anode compartment), the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +V is from 1:>0 to 1:5; wherein in the case where the iodine compound has an oxidation state of -I to +III, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +III is from 1:0 to 8:1; and wherein in the case where the iodine compound has an oxidation state of +V, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of +V is from 1:0 to 1:5;
[0042] wherein the molar ratio is calculated based on the iodine atoms present in the metal periodate and the iodine compound.
[0043] E.12. A method according to embodiment E.11, wherein the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 1:>0 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 1:0 to 1:4.
[0044] E.13. A method according to embodiment E.12, wherein the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 200:1 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 200:1 to 1:4.
[0045] E.14. A method according to any one of the preceding embodiments, for the preparation of alkali metal secondary periodate, wherein the iodine compound having an oxidation state of -I to +V is an alkali metal iodide, an alkali metal iodate, iodine or a mixture thereof.
[0046] E.15. A method according to embodiment E.14, for preparing sodium paraperiodate or potassium paraperiodate, wherein the iodine compound with an oxidation state of -I to +V is sodium iodide, potassium iodide, sodium iodate, potassium iodate, iodine or a mixture thereof.
[0047] E.16. The method according to any of the preceding embodiments, wherein the anodizing is performed at a pH of at least 11.
[0048] E.17. The method according to embodiment E.16, wherein the anodizing is performed at a pH of at least 12.
[0049] E.18. The method according to embodiment E.17, wherein the anodizing is performed at a pH of at least 13.
[0050] E.19. The method according to any of the preceding embodiments, wherein the anodization is performed in the presence of a base, wherein the base is selected from the group consisting of metal hydroxides, metal oxides and metal carbonates.
[0051] E.20. A method according to embodiment E.19, wherein the anodization is carried out in the presence of a metal hydroxide, wherein, in the case where the iodine compound having an oxidation state of -I to +V is an alkali metal iodine salt, the metal of the alkali corresponds to the metal in the metal iodine salt.
[0052] E.21. A method according to any of the preceding embodiments, wherein the cathode electrolyte comprises an aqueous medium having a pH of at least 10.
[0053] E.22. A method according to embodiment E.21, wherein the cathode electrolyte comprises an aqueous medium with a pH of at least 11.
[0054] E.23. A method according to embodiment E.22, wherein the cathode electrolyte comprises an aqueous medium with a pH of at least 12.
[0055] E.24. A method according to embodiment E.23, wherein the cathode electrolyte comprises an aqueous medium with a pH of at least 13.
[0056] E.25. A method according to any one of the preceding embodiments, wherein the anodizing 2 Up to 1000mA / cm 2 The current density is within the range of .
[0057] E.26. A method according to embodiment E.25, wherein the anodizing is carried out at 100 mA / cm 2 Up to 750mA / cm 2 The current density is within the range of .
[0058] E.27. A method according to embodiment E.26, wherein the anodizing is carried out at 250 mA / cm 2 Up to 500mA / cm 2 The current density is within the range of .
[0059] E.28. A method according to embodiment E.27, wherein the anodizing is carried out at 400 mA / cm 2 Up to 430mA / cm 2 carried out at a current density of .
[0060] E.29. A method according to any of the preceding embodiments, wherein the iodine compound with an oxidation state of -I to +V is continuously or periodically introduced into the continuous stirred tank reactor at a rate substantially the same as the metal periodate is continuously or periodically removed from the anode compartment, "substantially the same rate" means that the molar ratio of the metal periodate to the iodine compound is maintained within the above-mentioned predetermined range.
[0061] E.30. A method according to any of the preceding embodiments, wherein the metal periodate formed in the anode compartment is separated from the anode electrolyte removed from the anode compartment, and the remaining portion of the anode electrolyte is transferred to the continuous stirred tank reactor.
[0062] E.31. A method according to embodiment E.30, wherein, in the case where the separated periodate is not composed of or is not entirely composed of metal secondary periodate, a periodate other than secondary periodate is converted to secondary periodate (for example, by adding a base that converts a periodate other than secondary periodate to secondary periodate).
[0063] E.32. The method according to any of the preceding embodiments, wherein the separator arranged between the cathode compartment and the anode compartment is selected from the group consisting of a semipermeable membrane, a diaphragm, and a frit.
[0064] E.33. The method of embodiment E.32, wherein the separator disposed between the cathode compartment and the anode compartment is an ion exchange membrane.
[0065] E.34. The method according to any of the preceding embodiments, wherein the one or more anodes comprises a carbon-based active layer.
[0066] E.35. The method of embodiment E.34, wherein the one or more anodes comprises a diamond layer doped with one or more elements from Group 13, Group 15, or Group 16 of the IUPAC Periodic Table of Elements.
[0067] E.36. The method of embodiment E.35, wherein the one or more anodes comprises a boron-doped diamond layer.
[0068] E.37. The method according to any one of the preceding embodiments, wherein the iodine compound in an oxidation state of -I to +V is fed into the continuous stirred tank reactor in the form of an aqueous dispersion or in solid form.
[0069] E.38. An apparatus for preparing metal periodates, in particular metal secondary periodates, by continuous anodic oxidation of iodine compounds having oxidation states ranging from -I to +V, in particular an apparatus configured to carry out the method according to any one of the embodiments E.1 to E.37, comprising:
[0070] An electrolytic cell comprising an anode compartment having one or more anodes, a cathode compartment having one or more cathodes, and a separator arranged between the anode compartment and the cathode compartment,
[0071] a cathode electrolyte loop for recirculating cathode electrolyte through the cathode compartment, the cathode electrolyte loop comprising a cathode electrolyte reservoir,
[0072] An anode electrolyte loop for circulating an anode electrolyte through the anode compartment, the anode electrolyte loop comprising at least one continuously stirred tank reactor, the at least one continuously stirred tank reactor being provided with a feeding device for feeding the iodine compound with an oxidation state of -I to +V selected from iodine salts, elemental iodine, a mixture of different iodine salts or a mixture of iodine and one or more iodine salts into the at least one continuously stirred tank reactor, and a discharging device for discharging the metal periodate reaction product from the at least one continuously stirred tank reactor.
[0073] E.39. An apparatus according to embodiment E.38, wherein the feeding device for feeding the iodine compound with an oxidation state of -I to +V includes a starting material kettle connected to the continuous stirred tank reactor for containing a solution of the iodine compound with an oxidation state of -I to +V.
[0074] E.40. Apparatus according to any one of embodiments E.38 and E.39, wherein the discharge device comprises a collecting vessel connected to the continuous stirred tank reactor via a discharge line.
[0075] E.41. The apparatus according to embodiment E.40, wherein the feeding device for feeding the iodine compound comprises a feeding device for a solid iodine compound connected to the continuous stirred tank reactor.
[0076] E.42. An apparatus according to embodiment E.41, wherein the discharge device comprises a collecting vessel connected to the continuous stirred tank reactor via a discharge line and a recirculation line.
[0077] E.43. An apparatus according to any one of embodiments E.38 to E.42, wherein the cathode electrolyte loop comprises a cathode electrolyte kettle connected to the anode electrolyte loop via a transfer line for transferring a portion of the cathode electrolyte into the anode electrolyte loop.
[0078] E.44. An apparatus according to any one of embodiments E.38 to E.43, wherein the electrolytic cell comprises a cooling water system for controlling the temperature of the anode compartment and / or the cathode compartment of the electrolytic cell.
[0079] E.45. An apparatus according to any one of embodiments E.38 to E.44, wherein the apparatus comprises a measurement system for determining the ratio of metal periodate to iodine compounds having oxidation states ranging from -I to +V in the anode electrolyte.
[0080] E.46. An apparatus according to embodiment E.45, wherein the measurement system comprises a potentiometer, an ammeter, a pH probe, or a combination thereof.
[0081] The material to be subjected to anodization is an iodine compound in an oxidation state of -I to +V. The iodine compound in an oxidation state of -I to +V is in fact an iodine compound in an oxidation state of -I, O (elemental iodine), +I, +III or +V. The iodine compound in an oxidation state of -I to +V is selected from an iodine salt, elemental iodine, a mixture of different iodine salts or a mixture of iodine and one or more iodine salts.
[0082] As explained above, the iodine salt is an inorganic iodine salt. Examples of suitable inorganic iodine salts having an oxidation state of -I to +V (of the iodine atom) are iodides [(M n+ ) 1 / n (I - ); the oxidation state of the iodine atom is -I], hypoiodite [(M n+ ) 1 / n (IO - ); the oxidation state of the iodine atom is +I], iodite [(M n+ ) 1 / n (IO2 - ) - ; The oxidation state of the iodine atom is +III] and iodate [(M n+ ) 1 / n (IO3 - ) - ; the oxidation state of the iodine atom is +V], wherein M is a cation, typically a metal cation or an ammonium cation, and n is the charge number. Among them, preferred are metal salts, i.e. metal iodides, metal hypoiodites, metal iodites and metal iodates. Ideally, the metal counter cation corresponds to the metal counter cation expected by the target metal secondary periodate, so that cation exchange can be avoided.
[0083] Suitable metal counter cations for the iodonium salts and for the target metal paraperiodates are alkali metal cations, alkaline earth metal cations and transition metal cations.
[0084] Suitable alkali metal countercations are, for example, lithium, sodium, potassium or cesium cations.
[0085] Suitable alkaline earth metal countercations are, for example, magnesium cations or calcium cations.
[0086] Suitable transition metal iodide salts used as starting material in the method for the present invention are those that are stable under atmospheric conditions (air, moisture) and at least partially soluble in the reaction medium with the concentration of the expectation. Usually, the reaction medium for anodization is aqueous. However, low solubility in pure water does not necessarily make transition metal iodide salts unqualified, because the reaction (anodization) is carried out under alkaline conditions, which can greatly improve the solubility in the reaction medium. For example, CuI (which is substantially insoluble in water of about 7 pH) remains a suitable starting compound in an alkaline reaction medium, and particularly if the reaction medium comprises an inorganic basic salt in which a cation forms a water-soluble iodide as a base, such as the situation of NaOH or KOH.
[0087] Suitable transition metal counter cations are Sc (III) cations, Y (III) cations, La (III) cations, Co (II) cations, Ni (II) cations, Cu (I) cations and Zn (II) cations. Among them, considering their economic benefits and availability, Cu (I) cations and Zn (II) cations are preferred.
[0088] Among the starting iodine compounds listed above in which the oxidation state of the iodine atom is -I to +V, preferred are iodides, iodates, elemental iodine and mixtures thereof. More preferred are alkali metal iodides, alkali metal iodates, alkaline earth metal iodides, alkaline earth metal iodates, scandium (III) iodide, scandium (III) iodate, yttrium (III) iodide, yttrium (III) iodate, lanthanum (III) iodide, lanthanum (III) iodate, cobalt (II) iodide, cobalt (II) iodate, nickel (II) iodide, nickel (II) iodate, copper (I) iodide, copper (I) iodate, zinc (II) iodide, zinc (II) iodate, elemental iodine and mixtures thereof. Even more preferred are alkali metal iodides, in particular LiI, NaI, KI and CsI; alkali metal iodates, in particular Li(IO3), Na(IO3), K(IO3) and Cs(IO3); alkaline earth metal iodides, in particular MgI2 and CaI2; alkaline earth metal iodates, in particular Mg(IO3)2 and Ca(IO3)2; CuI; Cu(IO3); ZnI2; Zn(IO3)2; elemental iodine and mixtures thereof. Particularly preferred are alkali metal iodides, in particular LiI, NaI, KI and CsI; alkali metal iodates, in particular Li(IO3), Na(IO3), K(IO3) and Cs(IO3); alkaline earth metal iodides, in particular MgI2 and CaI2; alkaline earth metal iodates, in particular Mg(IO3)2 and Ca(IO3)2; elemental iodine and mixtures thereof. More particularly preferred are alkali metal iodides, in particular LiI, NaI, KI and CsI; alkali metal iodates, in particular Li(IO3), Na(IO3), K(IO3) and Cs(IO3); elemental iodine and mixtures thereof. Specifically, NaI, KI, Na(IO3), K(IO3), iodine or mixtures thereof are used.
[0089] Therefore, the method of the present invention is preferably used to prepare an alkali metal secondary periodate, an alkaline earth metal secondary periodate or a secondary periodate of Sc(III), Y(III), La(III), Co(II), Ni(II), Cu(I) or Zn(II); or a mixture thereof. More preferably, the method of the present invention is used to prepare an alkali metal secondary periodate, in particular lithium, sodium or potassium secondary periodate; an alkaline earth metal secondary periodate, in particular magnesium or calcium secondary periodate; copper(I) secondary periodate, zinc(II) secondary periodate; or a mixture thereof. Even more preferably, the method of the present invention is used to prepare an alkali metal secondary periodate, in particular lithium, sodium or potassium secondary periodate; or an alkaline earth metal secondary periodate, in particular magnesium or calcium secondary periodate; or a mixture thereof. Specifically, the method of the present invention is used to prepare an alkali metal secondary periodate, in particular sodium or potassium secondary periodate; in particular sodium secondary periodate.
[0090] In the method according to the invention, the anolyte is recycled to the anode compartment via the anolyte loop. According to the invention, the anolyte comprises a metal periodate and an iodine compound in an oxidation state of -I to +V, the iodine compound in an oxidation state of -I to +V being selected from an iodine salt, elemental iodine, a mixture of different iodine salts or a mixture of iodine and one or more iodine salts.
[0091] In the method according to the present invention, a continuous stirred tank reactor is operated in a steady-state mode relative to the total molar ratio of metal periodate to iodine compound with oxidation state of -I to +V in the anode electrolyte by continuously or periodically feeding the iodine compound with oxidation state of -I to +V into the continuous stirred tank reactor and continuously or periodically removing metal periodate from the continuous stirred tank reactor. Operating in a steady-state mode relative to the total molar ratio means: specifying a suitable molar ratio or more generally, specifying a suitable molar ratio range, so that during operation, the actual molar ratio or molar ratio range of metal periodate to iodine compound remains within the specified molar ratio or within the specified molar ratio range or is close to the specified molar ratio or molar ratio range, wherein "close" means that the actual molar ratio or molar ratio range (limit) can deviate from the specified molar ratio or molar ratio range by up to ±20%. In this article, the molar ratio (range) is calculated based on the iodine atoms present in the metal periodate and iodine compound. The values of suitable and preferred molar ratios or molar ratio ranges are defined below. Conveniently define the molar ratio or molar ratio range at a certain time point in the electrolysis. A suitable time point in the electrolysis is the composition of the anode electrolyte before the anode electrolyte is fed to the anode compartment. Therefore, in a preferred embodiment, the molar ratio or molar ratio range is related to the molar ratio or molar ratio range in the anode electrolyte before entering the anode compartment. Therefore, preferably, operating in a steady-state mode relative to the total molar ratio means: a suitable total molar ratio (range) of metal periodate to iodine compounds with oxidation states of -I to +V is defined for the anode electrolyte before entering the anode compartment, so that during operation, the actual molar ratio (range) of metal periodate to iodine compounds in the anode electrolyte before entering the anode compartment is maintained within the defined molar ratio or within the defined molar ratio range or close to the defined molar ratio or molar ratio range, wherein "close" means that the actual molar ratio or molar ratio range may deviate from the specified molar ratio or molar ratio range by up to ±20%.
[0092] It was found that clogging can be reduced or even inhibited if the amount of metal periodate in the anode electrolyte is present in large amounts. Clogging is primarily avoided in the anode compartment, and it is therefore important that the metal periodate is present in large amounts in the anode electrolyte before the anode electrolyte enters the anode compartment (and of course also in the compartment, but the amount of periodate is adjusted before the anode electrolyte is fed to the anode compartment). Thus, in a preferred embodiment, in the recirculating anode electrolyte, the total molar ratio of metal periodate to iodine compounds in oxidation states of -I to +V as fed to the anode compartment is from 1:>0 to 1:5 (meaning that some iodine compounds in oxidation states of -I to +V must be present; but the total amount of iodine compounds in oxidation states of -I to +V cannot exceed the amount of metal periodate by more than 5 times its amount); wherein in the case of iodine compounds in oxidation states of -I to +III, the total molar ratio of metal periodate to iodine compounds in oxidation states of -I to +III is from 1:0 to 8:1 (meaning that the metal periodate exceeds the total amount of iodine compounds in oxidation states of -I to +III (if the latter do exist) by at least 8 times its amount); and wherein in the case of iodine compounds in oxidation state of +V, the total molar ratio of metal periodate to iodine compounds in oxidation state of +V is from 1:0 to 1:5 (meaning that the total amount of iodine compounds in oxidation state of +V (if they do exist) cannot exceed the amount of metal periodate by more than 5 times its amount).
[0093] More preferably, the total molar ratio of metal periodate to iodine compounds with oxidation states of -I to +V is from 1:>0 to 1:4; even more preferably from 200:1 to 1:4; wherein in the case where the oxidation state of the iodine compound is from -I to +III, the total molar ratio of metal periodate to iodine compounds with oxidation states of -I to +III is from 1:0 to 10:1, and wherein in the case where the oxidation state of the iodine compound is +V, the total molar ratio of metal periodate to iodine compounds with oxidation state of +V is from 1:0 to 1:4, preferably from 200:1 to 1:4.
[0094] Preferably, the total molar ratio given above is not limited to the anode electrolyte before the anode electrolyte enters the anode compartment, but is generally applicable to the (re)circulating anode electrolyte. Thus, preferably, the total molar ratio of metal periodate to iodine compounds in oxidation states of -I to +V is from 1:>0 to 1:5; wherein in the case of iodine compounds in oxidation states of -I to +III, the total molar ratio of metal periodate to iodine compounds in oxidation states of -I to +III is from 1:0 to 8:1; and wherein in the case of iodine compounds in oxidation state of +V, the total molar ratio of metal periodate to iodine compounds in oxidation state of +V is from 1:0 to 1:5.
[0095] More preferably, the total molar ratio of metal periodate to iodine compounds with oxidation states of -I to +V is from 1:>0 to 1:4; even more preferably from 200:1 to 1:4; wherein in the case where the oxidation state of the iodine compound is from -I to +III, the total molar ratio of metal periodate to iodine compounds with oxidation states of -I to +III is from 1:0 to 10:1, and wherein in the case where the oxidation state of the iodine compound is +V, the total molar ratio of metal periodate to iodine compounds with oxidation state of +V is from 1:0 to 1:4, preferably from 200:1 to 1:4.
[0096] The molar ratio of metal periodate to iodine compound in oxidation state -I to +V will vary depending on the location of the anolyte (by way of example only, the anolyte will of course contain more periodate after leaving the anolyte compartment than before entering the anolyte compartment), but the indicated molar ratio conditions will preferably apply independently of the location of the anolyte. As indicated above, the given molar ratios are particularly applicable to the anolyte before the anolyte enters the anolyte compartment. The molar ratio of the anolyte at this location can be adjusted, for example, by the amount of iodine compound in oxidation state -I to +V added to the stirred tank reactor and / or by the amount of periodate removed after passing through the anolyte compartment.
[0097] The process allows a certain degree of tolerance for deviations from the molar ratios given above, in particular during the initial phase at the start of the electrolysis, since the steady state is generally reached only after a certain start time.
[0098] A molar ratio of 1:>0 means that a minimum amount of iodine compounds in oxidation states from -I to +V are present.
[0099] Elemental iodine in the case of the above molar ratios is calculated to contain 2 moles of I (i.e., for determining the above molar ratios, 1 mol of I2 is calculated as 2 mol). In fact, in an alkaline medium of an anolyte having a pH of at least 10 as used in the process of the present invention, elemental iodine disproportionates into iodide ions and hypoiodite, thereby obtaining two iodine species:
[0100] I2+2OH - →I - +IO - +H2O.
[0101] In addition, the salt contains x iodine atoms of periodate (e.g., diperiodate (I2O9 4- ), each diperiodate anion contains two iodine atoms) is calculated herein as containing x moles of I (e.g., for determining the molar ratio of the metal periodate to the iodine compound in the lower oxidation state above, 1 mol of I2O9 4- Calculated as 2 mol).
[0102] The total molar ratio of metal periodate and iodine compounds with oxidation states of -I to +V can be determined and adjusted, for example, by continuously or periodically analyzing the composition of the anolyte and feeding iodine compounds with oxidation states of -I to +V in such an amount that the desired periodate / iodine (-I to +V) material ratio is obtained. The anolyte can be quantitatively analyzed, for example, by LC-PDA or titration. If LC-PDA is used, the influence factor of the analyzed iodine species must be determined to take into account the different sensitivities of the method to different iodine species. In fact, if the anolyte discharged in or from the anolyte compartment is analyzed, it is usually sufficient to determine the ratio of periodate to iodate. As will be explained below, the oxidation of iodine species with oxidation states of -I to +III to periodate is carried out via iodate by stepwise anodic oxidation or by anti-disproportionation. Compared with the oxidation of iodate to periodate, the intermediate reaction rate to iodate is fast, so that iodine species with oxidation states of -I to +III are often included in an amount below the detection threshold. To analyze the anolyte via LC-PDA, the alkaline anolyte is advantageously neutralized or acidified to convert any secondary periodate present in the anolyte (which is poorly soluble in water) to water-soluble metaperiodate and thereby ensure proper quantitative detection of all periodate species formed.
[0103] Alternatively, the composition can be calculated. When electrolysis begins, the composition of the anolyte is known. The periodate removed continuously or periodically is separated and weighed, and the amount of iodine compounds with oxidation states of -I to +V consumed can be calculated from this. The amount required for the desired ratio is then substituted. Combinations of these methods are certainly possible.
[0104] The analysis / calculation of the composition is suitably carried out at least at the beginning of the electrolysis at suitable time intervals, for example a few minutes or about an hour, until a steady state is obtained.
[0105] The metal periodate contained in the recycled anode electrolyte may be any periodate in which the iodine atom is in the oxidation state +VII.
[0106] As explained above, metal periodates are metal salts of various periodic acids. In periodic acid, the corresponding anion is composed of iodine and oxygen in oxidation state +VII. Periodates particularly include orthoperiodate (IO6 5- ; Thus, the molecular formula of metal periodate is M5IO6), metaperiodate (IO4 - ; Therefore, the molecular formula of metal metaperiodate is MIO4), di-periodate (I2O9 4- ; Therefore, the molecular formula of the metal diperiodate is M4I2O9), mesoperiodate (IO5 3-; Thus, the molecular formula of the periodate in the metal is M3IO5) and secondary periodate. Secondary periodate is a salt with the molecular formula M3H2IO6, and is also called the corresponding double salt MIO4*2MOH. The M in the above molecular formula is the metal equivalent [(M n+ ) 1 / n , where n is the charge number]; in the case of, for example, an alkali metal periodate, M is thus an alkali metal cation; and in the case of an alkaline earth metal periodate, M is (M 2+ ) 1 / 2 In periodates with more than one negative charge, M for more than one metal equivalent may have the same or different meanings. For example, in the secondary periodate M3H2IO6 or MIO4*2MOH, M for all three metal equivalents may have the same meaning or may be from different metals; this may occur, for example, if the counter cation of the iodide salt used as starting material is different from the counter cation in the base present during anodization or used during post-treatment of the reaction product.
[0107] Preferably, the metal periodate contained in the recirculating anode electrolyte is an orthoperiodate, a metaperiodate, a secondary periodate or a mixture thereof. More preferably, the metal periodate contained in the recirculating anode electrolyte comprises a metal secondary periodate. Even more preferably, the metal periodate is the predominant metal periodate species in the anode electrolyte, i.e. it is contained in a higher (molar) amount than other metal periodate species. Preferably, at least 50 mol%, more preferably at least 70 mol% of the metal periodate contained in the recirculating anode electrolyte is a metal secondary periodate.
[0108] Anodic oxidation is carried out at a pH of at least 10, such as 10 to 14 or 10 to 13, preferably at least 11, such as 11 to 14 or higher, particularly at least 12, such as 12 to 14 or higher, and specifically at least 13, such as 13 to 14 or higher; that is, the pH of the anode electrolyte is at least 10, such as 10 to 14 or higher, preferably at least 11, such as 11 to 14 or higher, particularly at least 12, such as 12 to 14 or higher, and specifically at least 13, such as 13 to 14 or higher.
[0109] Therefore, the anodic oxidation is preferably carried out in the presence of a base. In view of the fact that aqueous media are usually used for anodic oxidation, suitable bases are all those that are water-soluble and form hydroxide ions in the aqueous phase. Preferred are inorganic bases such as metal hydroxides, metal oxides and metal carbonates.
[0110] In order to avoid any separation problems, in these bases, the counter cation preferably corresponds to the metal cation in the iodine salt used. If elemental iodine is used as the starting material, such a restriction is of course not required. However, the counter cation of the base preferably corresponds to the counter cation of the desired secondary periodate. In view of the fact that aqueous media are usually used for anodic oxidation, if the base whose cation corresponds to the metal cation in the iodine salt is not (sufficiently) water-soluble, such a preferred exception is required. For example, CuO, Cu(OH)2 and CuCO3 are substantially insoluble in water. Therefore, if CuI or other iodine salts of Cu are used as the starting iodine salt, it is indicated to use a water-soluble base that is not based on Cu; for example, NaOH or KOH. If certain alkaline earth metal iodine salts are used as starting materials, particularly MgI2 or CaI2 or other iodine salts of Mg or Ca, the same is true because the corresponding hydroxides, oxides and carbonates are almost insoluble in water. In this case, it is also indicated to use a water-soluble base that is not based on Mg or not based on Ca, such as NaOH or KOH. "Not sufficiently water-soluble" means that the base is insoluble at the concentration required to obtain the pH.
[0111] Preferably, the base is a metal hydroxide. More preferably, the base is a metal hydroxide in which the metal of the base corresponds to the metal in the metal iodide salt if it is used as the starting material (instead of elemental iodine); except for the above-mentioned case in which the corresponding base is not (sufficiently) water-soluble. In view of the preference for using alkali metal iodide salts, alkaline earth metal iodide salts and certain transition metal iodide salts as starting materials, and in view of the solubility of the corresponding hydroxide in the aqueous reaction medium, it is preferred to use an alkali metal hydroxide as the base. In the case of using an alkali metal iodide salt as the starting material, the metal of the base preferably corresponds to the metal in the alkali metal iodide salt used.
[0112] The process according to the invention preferably comprises subjecting an aqueous dispersion comprising an iodine compound in oxidation states of −I to +V and a base as anolyte to anodic oxidation. With regard to suitable and preferred iodine compounds and suitable and preferred bases, reference is made to the above.
[0113] More precisely, the method of the present invention preferably comprises subjecting an anolyte, which is an aqueous dispersion comprising an iodine compound in an oxidation state of -I to +V mixed with a metal periodate and a base. In the anolyte, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +V is from 1:>0 to 1:5; wherein in the case of the iodine compound in an oxidation state of -I to +III, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +III is from 1:0 to 8:1; and wherein in the case of the iodine compound in an oxidation state of +V, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of +V is from 1:0 to 1:5. More preferably, the total molar ratio of metal periodate to iodine compounds in oxidation state -I to +V is from 1:>0 to 1:4; even more preferably from 200:1 to 1:4; wherein in the case of iodine compounds in oxidation state -I to +III, the total molar ratio of metal periodate to iodine compounds in oxidation state -I to +III is from 1:0 to 10:1, and wherein in the case of iodine compounds in oxidation state +V, the total molar ratio of metal periodate to iodine compounds in oxidation state +V is from 1:0 to 1:4, preferably from 200:1 to 1:4. As described above, this molar ratio is present in the anode electrolyte at least before the anode electrolyte enters the anode compartment.
[0114] The processes in the anode compartment depend on the starting materials, are partly interconnected and complex. Theoretically, in a simplified model, the following processes occur under alkaline conditions, depending on the iodine species to be oxidized:
[0115] I - +8OH - →IO4 - +4H2O+8e -
[0116] I - +8OH - →IO4 - +4H2O+6e -
[0117] I2+16OH - →2IO4 - +8H2O+14e -
[0118] IO - +6OH - →IO4 - +3H2O+6e -
[0119] IO3 - +2OH - →IO4 - +H2O+2e -
[0120] The first four starting iodine species are usually converted to periodate salts via subsequent higher order oxidation species.
[0121] Furthermore, as explained above, elemental iodine disproportionates into iodide ion and hypoiodite under alkaline conditions, thereby obtaining two iodine species:
[0122] I2+2OH - →I - +IO - +H2O
[0123] Instead of the above third reaction scheme, the first reaction scheme and the fourth reaction scheme occur at least partially.
[0124] In addition, iodine species can also undergo a reverse disproportionation with periodate which is also present. For example, the reaction of iodide and elemental iodine is shown:
[0125] 3I2+6OH - →IO3 - +5I - +3H2O
[0126] I - +3IO4 - →4IO3 -
[0127] This means that at least a portion of the iodine or iodide starting material is not itself oxidized, but rather undergoes back disproportionation with periodate which is also present, such that iodate is the species that is actually oxidized.
[0128] Then, orthoperiodate IO4 - It can further react with hydroxide ion to form paraperiodate:
[0129] IO4 - +2OH - →H2IO6 3- .
[0130] The total concentration of metal periodates and iodine compounds in oxidation states from -I to +V in the anode electrolyte is preferably from 0.01 mol / l to 12 mol / l, more preferably from 0.05 mol / l to 5 mol / l, even more preferably from 0.1 mol / l to 2 mol / l, in particular from 0.1 mol / l to 1 mol / l, specifically from 0.1 mol / l to 0.5 mol / l, and very specifically from 0.1 mol / l to 0.3 mol / l; wherein the concentration refers to the amount of iodine atoms, for example iodide anions in the case of metal iodide starting materials, iodate anions in the case of metal iodate starting materials, and two I atoms in the case of elemental iodine as starting material (because of disproportionation to iodide ions and hypoiodite in alkaline media).
[0131] The base is used in a concentration that provides the desired pH.
[0132] The cathode electrolyte is typically an aqueous solution comprising an electrolyte. Preferably, the electrolyte is an alkali. Preferably, the alkali corresponds to the alkali used in the anode electrolyte. In the case where the electrolyte is an alkali, the pH is preferably at least 8, more preferably at least 10, even more preferably at least 11, and in particular at least 12. Suitably, an inorganic base is used to obtain an alkaline pH in the aqueous medium in the cathode compartment. Suitable and preferred inorganic bases have been described above with respect to the anode electrolyte; i.e. they are therefore preferably selected from metal hydroxides, metal oxides and metal carbonates. Preferred are hydroxides. More preferred are alkali metal hydroxides, in particular sodium hydroxide and potassium hydroxide. Preferably, the alkali used in the cathode electrolyte is the same as the alkali used in the anode electrolyte.
[0133] The reaction at the cathode will of course depend on the catholyte present in the cathode compartment. As mentioned above, the catholyte is typically an aqueous medium. In this case, the reaction occurring at the cathode is the reduction of water to hydrogen (with the formation of hydroxide anions):
[0134] 2H2O+2e - →H2+2OH - .
[0135] The anolyte circuit comprises at least one continuously stirred tank reactor operating in steady state mode with respect to the total molar ratio of metal periodate to iodine compound in oxidation states from -I to +V in said anolyte. As indicated above, the term "steady state" in the present invention includes deviations from the absolute limit value by up to 20%.
[0136] The anolyte circulates between the anode compartment and the stirred tank reactor.
[0137] The stirred tank reactor is fed with materials for obtaining the desired composition and concentration of the anolyte to be fed to the anode compartment. For this purpose, the iodine compound in the oxidation state of -I to +V which has been converted into the periodate during the anodic oxidation process must be replenished; if water and / or alkali are consumed during the reaction or during the product separation process, water and / or alkali must be replenished (see below), and if desired, also additional additives or promoters are added (however, their use is not preferred). In addition, the anolyte from which a portion of the formed periodate has been removed (see details below) is of course also returned to the stirred tank reactor.
[0138] At the beginning of electrolysis, the stirred tank reactor is also fed with metal periodate, preferably metal secondary periodate. The amount of metal (secondary) periodate is such that the desired ratio of metal (secondary) periodate to iodine compounds with oxidation states of -I to +V is obtained at the desired concentration. However, after the electrolysis begins, unless the desired ratio of metal (secondary) periodate to iodine compounds with oxidation states of -I to +V must be adjusted due to, for example, separation of too much (secondary) periodate from the anode electrolyte returned by the anode compartment, it is no longer necessary to add metal (secondary) periodate.
[0139] After the electrolysis starts, the metal periodate is formed at the anode from an iodine compound in an oxidation state of -I to +V and is transported to the stirred tank reactor via the circulating anode electrolyte, from which it is partially removed. Under given conditions, in particular due to an alkaline pH of at least 10, the periodate is at least partially composed of the desired secondary periodate. Typically, secondary periodate is even the main periodate species in the recirculating anode electrolyte; in particular at higher pH values. In view of the rather low water solubility of the metal secondary periodate, its main amount is usually present in the form of a solid suspended in the anode electrolyte and can be simply removed from the anode electrolyte by precipitation; if necessary, removed after concentration. Concentration (if necessary) can be carried out by conventional methods, such as evaporation of part of the solvent (if desired, carried out under reduced pressure), partial freeze drying, partial reverse osmosis, etc.
[0140] For this purpose, preferably, a portion of the anolyte that is recycled to the stirred tank reactor is removed from the stirred tank reactor, and at least a portion of the metal secondary periodate is removed from the anolyte. If at least a portion of the secondary periodate is already present in the removed anolyte in solid form, then its separation can be carried out by conventional methods, such as filtering or decantation of the supernatant. If the anolyte needs to be first concentrated to produce enough solid matter for separation, the anolyte is usually transferred to a suitable device wherein, for example, by evaporation (removing under reduced pressure if desired) to remove part of the solvent, or the anolyte is subjected to partial freeze drying, partial reverse osmosis, etc. The precipitate obtained is separated as described above.
[0141] If the anolyte is not alkaline enough so that secondary periodate is not the main periodate species, secondary periodate can also be obtained after adding other bases. This converts metaperiodate and other periodate species into the desired secondary periodate, which forces precipitation to occur. Subsequent removal and post-processing can be carried out as described above.
[0142] Alternatively, to isolate the secondary periodate, the water can be removed more or less completely from the anolyte, for example by evaporation of the solvent (if desired under reduced pressure), freeze drying, reverse osmosis, with subsequent evaporation of residual water if necessary, etc., and the remainder can be purified if desired.
[0143] If desired, in order to remove unreacted iodine starting compound, excessive alkali, undesirable by product etc. (if any), the separated secondary periodate can be subjected to further purification step, for example, washing with water or aqueous solvent mixture, impregnating with water or aqueous solvent mixture or recrystallization. However, according to the intended use of secondary periodate, it is not necessary to subject it to purification step. In many cases, if particularly secondary periodate is used as oxygenant, then from the aqueous medium obtained after neutralization, water evaporation is just enough. In some cases, even do not need to evaporate residual water (i.e. the aqueous medium obtained from the anode compartment can be used as it is for subsequent oxidation process), or at least do not need to be dried.
[0144] The anolyte of the consumed (secondary) periodate is then returned to the stirred tank reactor. Before, during or after the consumed anolyte is returned to the stirred tank reactor, it is supplemented with an iodine compound in an oxidation state of -1 to +V. The iodine compound in an oxidation state of -1 to +V is added in an amount substantially equimolar to the amount of secondary periodate removed. Preferably, the iodine compound in an oxidation state of -1 to +V is fed to the stirred tank reactor.
[0145] The iodine compound with an oxidation state of -I to +V can be added in a dispersed state (usually an aqueous dispersion) or in solid form. If the iodine compound is added in a dispersed form (usually in water), the loss of water that may occur during the removal of the (secondary) periodate is at least partially compensated at the same time. If the iodine compound is added in solid form, the water that may be lost is usually compensated by preferably also adding water to the stirred tank reactor. This can be done simultaneously with the addition of the solid iodine compound or independently in time.
[0146] Removing (secondary) periodate may also result in a consumption of alkali. This may also be compensated by adding alkali, and may also be done simultaneously with the addition of the solid iodine compound or independently in time. The added alkali may be a "fresh" material. However, in a particular embodiment, the alkali is added in the form of a portion of the cathode electrolyte from the cathode compartment. Since hydroxide ions are formed at the cathode during electrolysis (by reduction of water), the cathode electrolyte does not need to be supplemented with fresh alkali to compensate for the amount transferred. It is only necessary to supplement the cathode compartment with water transferred to the stirred tank reactor.
[0147] The removal of the anolyte from the anode compartment and from the stirred tank reactor and the addition of the iodine compound having an oxidation state of -I to +V to the anolyte depleted of (secondary) periodate may be performed continuously or periodically.
[0148] The removal of the anolyte from the anode compartment and from the stirred tank reactor and the addition of the iodine compound in the oxidation state of -I to +V to the anolyte from which the secondary periodate is depleted are preferably carried out at substantially the same rate so that the electrolysis occurs in a substantially steady-state mode. This can be achieved simultaneously by adding the iodine compound in the lower oxidation state and removing the metal periodate, and can also be achieved intermittently by adding the iodine compound in the lower oxidation state and removing the metal periodate, i.e., adding the iodine compound during certain time intervals and removing the metal periodate during other time intervals, as long as the molar ratio is maintained within a predetermined range.
[0149] The addition of the iodine compound in the oxidation state of -I to +V is preferably carried out at a rate and concentration such that the periodate is the predominant iodine species in the anode electrolyte present in the stirred tank reactor, and of course the predominant iodine species in the anode compartment. Preferably, the addition is preferably carried out at a rate and at a concentration such that the total molar ratio of all metal periodates to all iodine compounds in the oxidation state of -I to +V in the stirred tank reactor is from 1:>0 to 1:5; wherein in the case of iodine compounds in the oxidation state of -I to +III, the total molar ratio of metal periodates to iodine compounds in the oxidation state of -I to +III is from 1:0 to 8:1; and wherein in the case of iodine compounds in the oxidation state of +V, the total molar ratio of metal periodates to iodine compounds in the oxidation state of +V is from 1:0 to 1:5. More preferably, the total molar ratio of metal periodate to iodine compounds in oxidation state -I to +V is from 1:>0 to 1:4; even more preferably from 200:1 to 1:4; wherein in the case of iodine compounds in oxidation state -I to +III, the total molar ratio of metal periodate to iodine compounds in oxidation state -I to +III is from 1:0 to 10:1, and wherein in the case of iodine compounds in oxidation state +V, the total molar ratio of metal periodate to iodine compounds in oxidation state +V is from 1:0 to 1:4, preferably from 200:1 to 1:4. As described above, this molar ratio is present in the anode electrolyte at least before the anode electrolyte enters the anode compartment.
[0150] In the method of the present invention, anodization is preferably carried out in the absence of promoters and additives. The promoter in the term of the present invention is understood to be an anti-reducing agent and an oxidation promoter, such as a polarizing substance. Additives are understood to refer to any substance other than the starting compound, the product formed during the reaction, the acid, the base, the electrolyte medium (usually water) and the promoter. In the methods of the prior art, in order to obtain periodate with a satisfactory yield, the presence of a promoter or an additive is often necessary. For example, the method of Nam et al., as described in Journal of the Korean Chemical Society 1974,18,373, requires the presence of potassium dichromate as an anti-reducing agent. Obviously, chromium should be avoided in certain applications, such as health, personal care or nutrition. Fluorides such as lithium fluoride or silicon fluoride are also often used; it is believed that they increase the overpotential of oxygen at the anode and improve the oxidation efficiency. In particular, in the method of the present invention, anodization is preferably carried out in the absence of any promoter, and in particular in the absence of any chromium salt and any fluoride such as lithium fluoride or silicon fluoride.
[0151] Anode material can be any one of the oxidations known in the art for this type in principle. However, if the desired product is used for a specific purpose that does not allow specific impurities such as heavy metals, particularly lead, such as the situation of pharmaceutical processes, then the anode material preferably does not include such material. Therefore, in a preferred embodiment, the anode includes an active layer based on carbon. Anodes (or more generally, electrodes) comprising carbon or anodes / electrodes based on carbon (they are also referred to as such hereinafter) are well known in the art, and include for example graphite electrodes, glassy carbon (glassy carbon) electrodes, meshed glassy carbon electrodes, carbon fiber electrodes, electrodes based on carbonized composite materials, electrodes based on carbon-silicon composite materials, electrodes based on graphene and electrodes based on diamond.
[0152] Anodes comprising carbon need not be composed entirely of carbonaceous materials. Although graphite electrodes are often composed only of graphite or as the main material, other carbonaceous materials may be present only as the outer layer of the electrode or as part of the outer layer of the electrode (i.e., the part that is in direct contact with the electrolyte). Further details are given below.
[0153] Among the above anodes, diamond based electrodes are preferred. Such electrodes are characterized by very high overpotentials for both oxygen and hydrogen evolution, resulting in a wide potential window.
[0154] Diamond itself is generally an electrical insulator due to its large band gap of greater than 5 eV and is therefore not suitable as an electrode material. However, diamond can be made conductive by doping with certain elements. Another alternative method to make diamond conductive is to anneal an undoped diamond film at temperatures above 1550°C in a vacuum. These harsh conditions may cause a network of conductive carbon phases to form within the diamond film.
[0155] However, the former method is more practical and reliable. Therefore, the diamond-based electrode is preferably an electrode comprising conductively doped diamond.
[0156] Suitable dopants are selected from elements of Group 13, Group 15 or Group 16 of the IUPAC Periodic Table of Elements.
[0157] Thus, in a preferred embodiment, the one or more anodes used in the method of the present invention comprise diamond doped with one or more elements of Group 13, Group 15 or Group 16 of the IUPAC Periodic Table of Elements.
[0158] Suitable dopants of group 13 are boron. Suitable dopants of group 15 are nitrogen and phosphorus. Suitable dopants of group 16 are sulfur. Boron doping produces p-type semiconductors, while nitrogen doping, phosphorus doping and sulfur doping produce n-type conductivity. It is also possible to use two or more different dopants, producing, for example, boron-nitrogen co-doping or boron-sulfur co-doping. If, in the case of co-doping, the two or more dopants have different conductivities, such as in the case of BN co-doping or BS co-doping, the type of conductivity obtained in the co-doped diamond depends inter alia on the concentration of the individual dopants and can be adjusted to the desired type.
[0159] Among the above dopants, boron doping is preferred. Thus, in a more preferred embodiment, the one or more anodes used in the method of the present invention comprise boron doped diamond (BDD).
[0160] The boron doped diamond comprises boron in an amount of preferably 0.02 to 1 wt% (200 ppm to 10,000 ppm), more preferably 0.04 to 0.2 wt%, especially 0.06 to 0.09 wt%, relative to the total weight of the doped diamond.
[0161] As already indicated above, such electrodes are usually not composed of doped diamond alone. Instead, the doped diamond is attached to a substrate. Most commonly, the doped diamond is present as a layer on a conductive substrate, but diamond particle electrodes in which the doped diamond particles are embedded in a conductive or non-conductive substrate are also suitable. However, preference is given to anodes in which the doped diamond is present as a layer on a conductive substrate.
[0162] Thus, in particular, one or more anodes used in the method of the invention comprise a boron doped diamond layer.
[0163] Suitable support materials for an electrode comprising a boron doped diamond layer are silicon, self-passivating metals, metal carbides, graphite, glassy carbon, carbon fibers and combinations thereof.
[0164] Suitable self-passivating metals are, for example, germanium, zirconium, niobium, titanium, tantalum, molybdenum and tungsten.
[0165] Suitable combinations are, for example, metal carbide layers on the corresponding metals (such an intermediate layer can be formed in situ when the diamond layer is applied to the metal support), composites of two or more of the support materials listed above, and combinations of carbon with one or more of the other elements listed above. Examples of composite materials are siliconized carbon fiber carbon composites (carbon fiber carbon, CFC) and partially carbonized composite materials.
[0166] Preferably, the support material is selected from elemental silicon, germanium, zirconium, niobium, titanium, tantalum, molybdenum, tungsten, carbides of the eight aforementioned metals, graphite, glassy carbon, carbon fiber and combinations thereof (particularly composite materials).
[0167] More preferred are elemental silicon, germanium, zirconium, niobium, titanium, tantalum, molybdenum, tungsten, and a combination of one of the seven aforementioned metals and a corresponding metal carbide.
[0168] Doped diamond electrodes and methods for preparing them are known in the art and are described, for example, in NL1013348C2 (Electrochimica Acta 2003, 48, 3959-3964) by LJJ Janssen et al. and in the references cited therein. Suitable preparation methods include, for example, chemical vapour deposition (CVD), such as hot filament CVD or microwave plasma CVD, for preparing electrodes with doped diamond films; and high temperature high pressure (HTHP) methods for preparing electrodes with doped diamond particles. Doped diamond electrodes are commercially available.
[0169] The cathode material is not very critical and any commonly used material is suitable, such as stainless steel, chromium-nickel steel, platinum, nickel, bronze, tin, zirconium or carbon. In a specific embodiment, a stainless steel electrode is used as the cathode.
[0170] The separation of the anode compartment and the cathode compartment can be achieved by conventional separation means (separators), such as semipermeable membranes or diaphragms or glass frits. Alternatively stated, the electrolytic cell is a separation cell. The separator separates the anode electrolyte [liquid medium in the anode compartment] from the cathode electrolyte [liquid medium in the cathode compartment], but allows charge balance. The diaphragm is a separator of an oxidizing material comprising a porous structure, such as a silicate in the form of porcelain (porcelain) or ceramic (ceramic). However, due to the sensitivity of the diaphragm material to harsher conditions, semipermeable membranes are generally preferred, especially if the reaction is carried out at an alkaline pH (because alkaline pH is preferred). The semipermeable membrane is preferably a semipermeable membrane that resists such conditions, especially alkaline pH. Suitable semipermeable membranes are, for example, ion exchange membranes, particularly cation exchange membranes, i.e., membranes composed of materials that allow cations [and fluids (which are generally water)] to pass but do not allow anions to pass. More specifically, the semipermeable membrane is a proton exchange membrane (proton exchange membrane, PEM). Membrane materials that resist harsher conditions, especially alkaline pH, are based on fluorinated polymers. Examples of suitable materials for this type of membrane are fluoropolymer copolymers based on sulfonated tetrafluoroethylene, such as SULFONATE® from DuPont de Nemours. Trademarks or trademarks of WL Gore & Associates, Inc. Trademark. However, in the case of using iodides with divalent or higher valent counter cations, it is preferred to use a separator of a different semipermeable membrane that is permeable only to monovalent cations. In this case, a diaphragm is preferred.
[0171] The electrolytic cell for practicing the method of the present invention comprises one or more anodes in one or more anode compartments and one or more cathodes in one or more cathode compartments, wherein the anode compartment is separated from the cathode compartment.
[0172] If more than one anode is used, two or more anodes may be arranged in the same anode compartment or in separate compartments. If two or more anodes are present in the same compartment, they may be arranged adjacent to each other or on top of each other. If one or more anode compartments are used, they may also be arranged adjacent to each other or on top of each other.
[0173] The same applies when one or more cathodes are used.
[0174] Alternatively, if the electrolysis device comprises more than one anode and more than one cathode, the electrolysis device may comprise more than one electrolysis cell, each cell comprising an anode compartment and a cathode compartment.The electrolysis cells may be arranged adjacent to each other or on top of each other.
[0175] Suitable geometries and arrangements of electrolysis devices comprising more than one anode and / or cathode are known to those skilled in the art.
[0176] The method of the present invention is suitable for laboratory-scale as well as industrial-scale reactions.
[0177] The process of the present invention can be carried out as a semi-continuous process or as a continuous process.
[0178] In a continuous process design, the electrolyte is passed continuously through the electrolytic cell, i.e., the electrolyte containing the iodine compound to be oxidized is continuously added and reacted, and the resulting reaction mixture is continuously removed from the process. A semi-continuous process design contains elements of both batch and continuous forms: the process is primarily continuous, but at some point in time an anolyte containing the iodine compound to be oxidized is added, and at some point in time the resulting reaction mixture is removed.
[0179] For semi-continuous or continuous process designs, the anode and cathode compartments are typically designed as flow cells.
[0180] Various designs and geometries of flow cells are known in the art and can be applied to the present methods.
[0181] Typically, the electrolysis device is equipped with a heat exchanger, a thermometer, a mixing device, and a gas outlet away from the cathode compartment and the anode compartment. In addition, a device for continuous supply and removal is provided, for example in the form of a recirculation loop equipped with a pump. The stirred tank reactor is part of the anolyte loop, and typically also includes a loop for removing a portion of the formed product and returning the remaining anolyte, and a connector for a supply system for replenishing the consumed starting materials, water and alkali, and any other desired components of the anolyte. As already explained above, the starting materials can be supplemented in a stirred tank reactor in a dispersed form or as a solid. In the latter case, a suitable supply system for solids, such as a screw conveyor, etc., is required.
[0182] The device according to the present invention is a preferred form of electrolysis device suitable for carrying out the method of the present invention. Therefore, the device configured to prepare metal paraperiodate by the method of the present invention, i.e., to prepare metal paraperiodate by continuous anodic oxidation of iodine compounds, comprises: an electrolytic cell, the electrolytic cell comprising an anode compartment having one or more anodes, a cathode compartment having one or more cathodes, and a separator arranged between the anode compartment and the cathode compartment; a cathode electrolyte loop for recycling cathode electrolyte through the cathode compartment, the cathode electrolyte loop comprising a cathode electrolyte reservoir; an anode electrolyte loop for circulating anode electrolyte through the anode compartment, the anode electrolyte loop comprising at least one continuous stirred tank reactor, the at least one continuous stirred tank reactor being provided with a feeding device for feeding an iodine compound having an oxidation state of -I to +V selected from an iodine salt, elemental iodine, a mixture of different iodine salts, or a mixture of iodine and one or more iodine salts into the at least one continuous stirred tank reactor, and a discharge device for discharging the metal periodate reaction product from the at least one continuous stirred tank reactor.
[0183] For a given device according to the invention, calibration tests can be carried out to determine the operating conditions under which the reactor operates in steady-state mode with respect to the molar ratio of metal periodate to iodine compound in oxidation states ranging from -I to +V in the anolyte, for example by using LC-PDA data or data obtained by other analytical or computational methods. Thus, by choosing appropriate operating conditions, in particular with respect to the concentration of iodine compound (feed rate), the concentration of metal periodate (exhaust rate), the temperature, the flow rate of the anolyte through the electrolytic cell, the pH of the anolyte, the operating current density of the electrolytic cell, the reactor can be maintained in steady-state mode.
[0184] Preferably, the apparatus of the present invention comprises a suitable measurement system for determining and / or controlling the operating conditions of the apparatus. The measurement system typically comprises a potentiometer and / or an ammeter, a pH meter (typically an online pH meter), a temperature sensor and a flow sensor. Typically, there is a linear relationship between flow and current density, i.e., an increase in flow by a certain factor results in a similar increase in current density while still maintaining steady-state conditions.
[0185] The electrolysis may be performed under galvanostatic control (the applied current is controlled; the voltage may be measured, but not controlled) or potentiostatic control (the applied voltage is controlled; the current may be measured, but not controlled), the former being preferred.
[0186] When measuring voltage under constant current control, reaction conditions can be adjusted so that voltage is basically maintained at desired value, thus ensuring that reactor operates under steady state mode. Similarly, under constant potential control, current is maintained at desired value and reactor can also be ensured to operate in steady state mode. Electrolysis system can be calibrated by measuring various electrolytes with known composition, particularly metal periodates of known composition and oxidation state being-I to+V iodine compound current / voltage relationship. Based on calibration data, electrolysis can be carried out under the desired ratio of metal periodates and oxidation state being-I to+V iodine compound by setting up and keeping suitable current / voltage value during electrolysis.
[0187] Under constant current control, an increase in the cell voltage indicates that more metal periodate is produced. Therefore, in order to maintain a steady state in the reactor, more iodine compounds with an oxidation state of -I to +V should be added. Similarly, under constant potential control, a decrease in current density indicates an increase in the production of metal periodate, so it is also necessary to add iodine compounds with an oxidation state of -I to +V to maintain a steady state.
[0188] In the case of the preferred constant current control, the voltage observed is typically in the range of 0V to 30V, more often 1V to 20V, and especially 1V to 10V.
[0189] In the case of constant potential control, the applied voltage is generally in the same range, ie 1 V to 30 V, preferably 1 V to 20 V, in particular 2 V to 10 V. The voltage can be adjusted precisely to the redox potential of the iodine species to be oxidized.
[0190] Anodic oxidation is preferably carried out at 10 mA / cm 2 Up to 1000mA / cm 2 , more preferably 100mA / cm 2 Up to 750mA / cm 2 , especially 250mA / cm 2 Up to 500mA / cm 2 , and specifically 400mA / cm 2 Up to 430mA / cm 2 These values apply to a flow rate of about 7.5 L / hour. If the flow rate is reduced or increased by a certain factor, the current density can be reduced or increased by the same factor.
[0191] Anodization is preferably performed at a temperature of 5°C to 80°C, more preferably 10°C to 60°C, particularly 20°C to 45°C, and specifically 30°C to 40°C.
[0192] The reaction pressure is not critical. Therefore, anodization is usually carried out at ambient pressure. However, in order to avoid boiling, higher pressures may be required if the reaction is carried out at a temperature above the normal boiling point of the aqueous medium.
[0193] Furthermore, the present invention relates to an apparatus for preparing a metal secondary periodate by continuous anodic oxidation of an iodine compound, and more precisely to an apparatus configured to prepare a metal secondary periodate by the method of the present invention, comprising:
[0194] An electrolytic cell comprising an anode compartment having one or more anodes, a cathode compartment having one or more cathodes, and a separator arranged between the anode compartment and the cathode compartment,
[0195] a cathode electrolyte loop for recirculating cathode electrolyte through the cathode compartment, the cathode electrolyte loop comprising a cathode electrolyte reservoir,
[0196] An anode electrolyte loop for circulating an anode electrolyte through the anode compartment, the anode electrolyte loop comprising at least one continuously stirred tank reactor, the at least one continuously stirred tank reactor being provided with a feeding device for feeding an iodine compound with an oxidation state of -I to +V selected from an iodine salt, elemental iodine, a mixture of different iodine salts or a mixture of iodine and one or more iodine salts into the at least one continuously stirred tank reactor, and a discharging device for discharging a metal periodate reaction product from the at least one continuously stirred tank reactor.
[0197] Preferably, the feeding means comprises a starting material tank connected to the continuous stirred tank reactor for containing a solution of an iodine compound having an oxidation state ranging from -I to +V.
[0198] The discharge device preferably comprises a collecting vessel which is connected to the continuous stirred tank reactor via a discharge line.
[0199] In a particular embodiment, the feed device for feeding the iodine compound in the oxidation state -I to +V comprises a feed device for solid starting materials, here in particular for solid iodine compounds in the oxidation state -I to +V, connected to a continuous stirred tank reactor.
[0200] In another particular embodiment, the discharge device comprises a collecting vessel connected to the continuous stirred tank reactor via a discharge line and a recirculation line.
[0201] Specifically, the apparatus comprises a feed device for solid starting materials connected to a continuous stirred tank reactor and a collecting vessel connected to the continuous stirred tank reactor via a discharge line and a recirculation line.
[0202] The cathode electrolyte loop preferably comprises a cathode electrolyte kettle connected to the cathode electrolyte loop via a transfer line for transferring a portion of the cathode electrolyte into the cathode electrolyte loop.
[0203] Specifically, the apparatus comprises a feeding device for solid starting materials connected to a continuous stirred tank reactor, a collecting container connected to the continuous stirred tank reactor via a discharge line and a recirculation line, and a cathode electrolyte kettle connected to an anode electrolyte loop via a transfer line for transferring a portion of the cathode electrolyte into the anode electrolyte loop.
[0204] The electrolytic cell preferably comprises a cooling water system for controlling the temperature of the anode compartment and / or cathode compartment of the electrolytic cell.
[0205] Further preferred embodiments of the apparatus of the present invention will become apparent in the context of the following description of the drawings.
[0206] The method of the present invention combines the concepts of circulating flow electrolysis and a continuous stirred tank reactor (e-CSTR) (which operates in a steady-state mode, enabling full continuous operation if desired). The product can be separated online, and the remaining anolyte can be recycled to the process. The method allows the production of secondary periodate in a quality suitable for high-demand applications such as pharmaceuticals, cosmetics and nutritional products. The method is universal with respect to starting materials, allowing any inorganic iodine compound as a starting compound, including starting from readily available, economical and problem-free, easy-to-handle iodide in a single step, and can also start from other iodine substances, such as iodate (which is usually provided for recycling in an oxidation process in which periodate is used as an oxidant, and is therefore also readily available) or iodine. The method is also universal with respect to the physical form in which the starting material is added, allowing not only a dispersed state, but also a solid form of supply. High conversion and high space-time yields coupled with high atom economy and the absence of promoters and additives make the method particularly attractive. However, most importantly, blockages can be significantly reduced. Furthermore, the method can be easily scaled up to industrial designs.
[0207] The method will now be further described with reference to the illustrative embodiments shown in the accompanying drawings and with reference to the examples described below.
[0208] In the attached picture:
[0209] Figure 1 A first embodiment of an apparatus for carrying out the invention is shown; and
[0210] Figure 2 A second embodiment of an apparatus for carrying out the invention is shown.
[0211] exist Figure 1 In the first embodiment of the apparatus for preparing metal periodate according to the method of the present invention, the whole is indicated by the reference numeral 10. The apparatus 10 comprises an electrolytic cell 11 having an anode compartment 12 in which an anode 13 is arranged and a cathode compartment 14 in which a cathode 15 is arranged. A separator 16 (e.g. a semipermeable membrane, a diaphragm or a glass frit) is arranged between the anode compartment 12 and the cathode compartment 14. The two compartments are respectively provided with an anode cooling water system 17 and a cathode cooling water system 18 to allow temperature regulation of the respective units. The cathode compartment 14 is part of a cathode electrolyte loop 19, which includes a cathode electrolyte kettle 20 and a cathode electrolyte recirculation pump 21. The anode electrolyte compartment is part of an anode electrolyte loop 22, which includes a continuous stirred tank reactor 23 used as an anode electrolyte kettle and an anode electrolyte recirculation pump 24. In the continuous stirred tank reactor 23, a predetermined molar ratio of metal periodate to iodine compound with an aggregation state of -I to +V is maintained. To this effect, the continuous stirred tank reactor 23 is fed with a starting material solution from a starting material tank 25 via a feed pump 26 and a feed line 27. The anolyte can be discharged from the continuous stirred tank reactor 23 via a discharge line 28 and a discharge pump 29 that discharge a portion of the anolyte into a product collection vessel 30. In this embodiment, the rate at which the iodine compound is fed from the starting material tank 25 into the continuous stirred tank reactor 23 corresponds to the rate at which the metal periodate is produced via electrolysis in the anode compartment 12, which in turn determines the rate at which the metal periodate is removed from the continuous stirred tank reactor 23 into the product collection vessel 30 via the discharge line 28.
[0212] Figure 2 A second embodiment of the device according to the invention is shown. Figure 2 In combination with Figure 1 Elements that are the same or similar to the elements described are denoted by the same reference numerals increased by 100.
[0213] Thus, an apparatus for preparing metal periodates is indicated by reference numeral 110 and comprises an electrolytic cell 111 having an anode compartment 112 with an anode 113 and a cathode compartment 114 with a cathode 115. Again, a separator 116 is arranged between the anode compartment 112 and the cathode compartment 114. The two compartments are provided with an anode cooling water system 117 and a cathode cooling water system 118, respectively. The cathode compartment 114 is part of a cathode electrolyte loop 119, which comprises a cathode electrolyte kettle 120 and a cathode electrolyte recirculation pump 121. The anode electrolyte compartment 112 is part of an anode electrolyte loop 122, which comprises a continuous stirred tank reactor 123 and an anode electrolyte recirculation pump 124.
[0214] Figure 2 Equipment and Figure 1 The difference of the device is that the starting material (especially the iodine compound) is fed directly into the continuous stirred tank reactor 123 as a solid. To this effect, a container 131 and a supply line 132 for the solid starting material are provided. The container 131 can be provided with a motorized feeder, such as a screw conveyor 133 driven by a motor 134. In this embodiment, the collecting tank 130 is not a batch collecting tank, but a collecting tank that allows the removal of metal periodate from the anode electrolyte fed into the collecting container 130 via a discharge line 128 and a discharge pump 129. The consumed anode electrolyte is recycled to the continuous stirred tank reactor 123 via a recirculation line 135 and a recirculation pump 136. As with Figure 1 Compared to another variant of the implementation, Figure 2 The device 110 is provided with a transfer line 137 and a transfer pump 138, which allow a certain amount of cathode electrolyte to be transferred to the continuous steel tank reactor 123 to allow the pH of the anode electrolyte to be adjusted during long-term operation. When a certain amount of cathode electrolyte is transferred to the anode electrolyte loop, the cathode electrolyte loop must be re-supplied with water (H2O) via a water supply line 139.
[0215] Example
[0216] Example 1 Anodic oxidation of sodium iodide to sodium paraperiodate - replenishment of sodium iodide in solid form
[0217] In such Figure 2 In the apparatus 110 for preparing metal periodate schematically depicted in FIG. 1 , the flow electrolysis cell 111 is equipped with 48 cm 2 The cell was separated by a 1 mm EPDM spacer (the anode compartment and the cathode compartment were separated by a cation exchange membrane 116 (from DuPont N 324) separated from each other) and confined. Boron-doped diamond electrodes (from Condias GmbH) were used. electrode; 10 μm BDD on silicon support (3 mm thickness); about 800 ppm of boron) as anode 113. Stainless steel was used as cathode 115. Each compartment is part of a respective electrolyte loop 119, 122, which includes respective reservoirs for anolyte (V=5 L) and cathode electrolyte (V=2.5 L), and each loop is powered by a membrane pump 121, 124 (Ritmo R033 from Fink). The anolyte loop includes a continuous stirred tank reactor (CSTR) 123, which serves as an anolyte reservoir and is stirred at 350 rpm, and is further connected via a discharge line 128 to a collection vessel 130 for separating a portion of the formed periodate from the anolyte by sedimentation and decantation. The supernatant anolyte from the collection vessel 130 is returned to the CSTR 123 via a recirculation line 135. The discharge line 128 and the recirculation line 135 are powered by peristaltic pumps 129, 136 (RegloICC from Ismatec), respectively. In addition, the CSTR 123 is connected to the feed of solid starting material to replenish the consumed iodine compound (here sodium iodide), Figure 2 In the figure, the cathode electrolyte reservoir 120 is represented by reference numerals 131 to 134, and is connected to the cathode electrolyte reservoir 120 to replenish the consumed alkali. In addition, the cathode electrolyte reservoir 120 is connected to the feed 139 to replenish the water lost in the transfer of the cathode electrolyte and consumed in the electrolysis at the cathode. During electrolysis using water, the cell is cooled by a thermostatically controlled anode cooling water system 117 and a cathode cooling water system 118.
[0218] For electrolysis, the secondary periodate from the previous electrolysis is suspended in caustic soda (4M NaOH) and added to the anolyte reservoir. The pH of the anolyte is>12. The cathode electrolyte consists of caustic soda of the same concentration. In addition, solid NaI is continuously fed to the anolyte at an addition rate of 3.5g / hour NaI. The anolyte and cathode electrolyte are pumped through the electrolytic cell 111 at a flow rate of fr (anolyte / cathode electrolyte) = 7.5L / hour. The suspension is removed from the anolyte by decantation in the secondary circulation (fr (decantation) = multiple). The composition of the anolyte is often controlled by LC-PDA analysis. After electrolysis, the removed suspension is filtered, the filter residue is washed with acetone, dried under reduced pressure, and the quality of the product is determined to obtain productivity.
[0219] After 29 hours of electrolysis and after adding a total amount of 103 g of NaI (0.68 mol), the secondary periodate precipitated in the collector was filtered out, the filter residue was washed with water and acetone, and dried under reduced pressure to obtain a product (497 g, 1.69 mol, purity 99.1%, determined by LC-PDA) with a yield of 94% (considering the initial amount of 309 g (1.05 mol) of secondary periodate). The productivity was calculated to be 6.5 g / hour, and the current efficiency was calculated to be 24%. The IR spectrum was consistent with the literature.
[0220] The total molar ratio of sodium periodate to sodium iodate in the anolyte contained in the anolyte reservoir is about 1:2 to 1:3 as determined by LC-PDA analysis of the anolyte returned to the CSTR. The iodide content in the anolyte returned to the CSTR is below the detection threshold of the LC-PDA. The amount of iodide added is such that the total molar ratio of sodium periodate to sodium iodide (prior to entering the analysis compartment) is at least 15:1.
[0221] No blockage occurred.
[0222] Example 2 Anodic oxidation of sodium iodide to sodium paraperiodate - replenishment of sodium iodide in solid form
[0223] The procedure of Example 1 was repeated; however, the addition rate of NaI was increased to 14.2 g / hour. This increased the productivity to 16.8 g / hour and the current efficiency to 61%. However, after 29 hours of electrolysis and after a total of 411 g of NaI had been added, the yield of sodium paraperiodate dropped to 61%. However, this yield is still very satisfactory for a steady-state reaction. The purity is 98.7%
[0224] No blockage occurred here either.
[0225] Example 3 Anodic oxidation of sodium iodide to sodium paraperiodate - replenishment of sodium iodide in solid form
[0226] The procedure of Example 1 was repeated; however, the flow rate fr (anolyte / catholyte) was increased to 700 L / hour (using a Flujo01 pump from Fink), and the addition rate of NaI was 8.5 g / hour. This increased the productivity to 15.6 g / hour and the current efficiency to 57%. After 29 hours of electrolysis and after adding a total amount of 247 g of NaI, the productivity of sodium paraperiodate was 94% and the purity was 98.7%.
[0227] No blockage occurred here either.
[0228] Example 4 Anodic oxidation of sodium iodide to sodium paraperiodate - replenishment of sodium iodide in solid form
[0229] The procedure of Example 1 was repeated, however using only 1 M NaOH. After 71 hours of electrolysis and after adding a total of 245 g of NaI at a feed rate of 24 mmol / hour (3.45 g / hour), the yield of sodium paraperiodate was 64% with a purity of 99.7%. The productivity was 4.3 g / hour and the current efficiency was 16%.
[0230] No blockage occurred.
[0231] Example 5 Anodic oxidation of sodium iodate to sodium paraperiodate - replenishment of sodium iodate in solid form
[0232] The procedure of Example 4 was repeated, however sodium iodate was used as the starting material. After 44 hours of electrolysis and after adding a total of 754 g of NaIO at a feed rate of 86 mmol / hour (17 g / hour), the productivity of sodium paraperiodate was 70% and the purity was 99.9%. The productivity was 17.9 g / hour and the current efficiency was 16%. Similar results were obtained when the addition rate was increased to 168 mmol / hour (33 g / hour).
[0233] The overall molar ratio of sodium periodate to sodium iodate in the anolyte contained in the anolyte reservoir is about 1 :1 to 1 :2 as determined by LC-PDA.
[0234] No blockage occurred.
[0235] Example 6 Anodic oxidation of elemental iodine to sodium paraperiodate - replenishment of iodine in solid form
[0236] The procedure of Example 4 was repeated, however using iodine as the starting material. After 75 hours of electrolysis and after adding a total of 283 g of I2, the yield of sodium paraperiodate was 44% with a purity of 99.6%. The productivity was 3.9 g / hour and the current efficiency was 12%.
[0237] No blockage occurred.
[0238] In the anode electrolyte contained in the anode electrolyte reservoir, the total molar ratio of sodium periodate to sodium iodate is about 1:1 to 1:2 as determined by LC-PDA. The amount of iodine added is such that the total molar ratio of sodium periodate to iodine (before entering the analysis compartment) is at least 14:1.
[0239] Example 7 Anodic oxidation of sodium iodide to sodium paraperiodate - replenishment of sodium iodide in dissolved form
[0240] The setup is simpler than in Examples 1 to 6, including no cathode electrolyte feed to the CSTR, and no return of the anolyte from the collector to the CSTR:
[0241] In such Figure 1In the apparatus 10 for preparing metal periodate schematically depicted in FIG. 1 , the flow electrolysis cell 11 is equipped with 48 cm 2 The cell was separated by a 1 mm EPDM spacer (the anode compartment and the cathode compartment were separated by a cation exchange membrane 16 (from DuPont N324) are separated from each other) and confined. Boron-doped diamond electrodes (from Condias GmbH) were used. electrode; 10 μm BDD on silicon support (3 mm thickness); about 800 ppm of boron) as anode 13. Stainless steel was used as cathode 14. Each compartment is part of a respective electrolyte loop 19, 22, which includes respective reservoirs for anolyte (V=5 L) and catholyte (V=2.5 L), and each loop is powered by a respective membrane pump 21, 24 (Ritmo R033 from Fink). The anolyte loop includes a continuous stirred tank reactor (CSTR) 23, which serves as anolyte reservoir and is stirred at 300 rpm, and is further connected to the feed solution (starting material tank 25) via line 27 and to the collection container 30 via line 28. The two lines 27, 28 are powered by respective peristaltic pumps 26, 28 (RegloICC from Ismatec). During electrolysis using water, the cell is cooled by thermostatically controlled anode cooling water systems 17 and cathode cooling water systems 18 .
[0242] For electrolysis, the anolyte container is loaded with a suspension of paraperiodate suspended in caustic soda (1M NaOH) from a previous electrolysis. The pH of the anolyte is >10. The catholyte consists of caustic soda at the same concentration. The anolyte and catholyte are pumped through the electrolyzer at a flow rate of fr (anolyte / cathode electrolyte) = 7.5 L / hour. The suspension is removed from the anolyte while the feed solution is added at the same flow rate (fr (in / out) = multiple). The composition is typically controlled by LC-PDA analysis. After electrolysis, the removed suspension is filtered, the filter residue is washed with acetone, dried under reduced pressure, and the quality of the product is determined to obtain productivity.
[0243] The electrolysis was carried out at a current of 20 A. NaI was added as an aqueous solution at an addition rate of 24 mmol / hour. After 101 hours of electrolysis and after adding a total amount of 375 g of NaI, the yield of sodium paraperiodate was 52% with a purity of 99.6%. The productivity was 3.8 g / hour and the current efficiency was 14%.
[0244] No blockage occurred.
[0245] Example 8 Anodic oxidation of sodium iodate to sodium paraperiodate - replenishment of sodium iodate in dissolved form
[0246] The procedure of Example 7 was repeated, however sodium iodate was used as the starting material. After 109 hours of electrolysis and after adding a total of 950 g of NaIO3 at an addition rate of 44 mmol / hour, the yield of sodium paraperiodate was 68% with a purity of 99.9%. The productivity was 8.8 g / hour and the current efficiency was 8%.
[0247] No clogging occurred. Under otherwise similar conditions, when the addition rate of sodium iodate was increased to 179 mmol / hour, no clogging occurred either.
[0248] Description of reference numerals:
[0249] 10,110 Equipment for preparing metal periodates
[0250] 11,111 Electrolytic Cell
[0251] 12, 112 Anode compartment
[0252] 13,113 Anode
[0253] 14,114 Cathode compartment
[0254] 15,115 cathode
[0255] 16,116 Separator
[0256] 17,117 Anode cooling water system
[0257] 18,118 Cathode cooling water system
[0258] 19, 119 Catholyte loop
[0259] 20,120 cathode electrolyte kettle
[0260] 21,121 Catholyte recirculation pump
[0261] 22,122 Anode electrolyte loop
[0262] 23,123 Continuous Stirred Tank Reactor
[0263] 24,124 Anolyte recirculation pump
[0264] 25 Starting material kettle
[0265] 26 Feed pump
[0266] 27 Feed line
[0267] 28,128 Discharge line
[0268] 29,129 Discharge pump
[0269] 30,130 Product collection container
[0270] 131 Starting material container
[0271] 132 Supply lines
[0272] 133 Screw Conveyor
[0273] 134 Motor
[0274] 135 Recirculation line
[0275] 136 Recirculation pump
[0276] 137 Cathode electrolyte transfer line
[0277] 138 Transfer Pump
[0278] 139 Water supply line
Claims
1. A method for preparing a metal secondary periodate by anodic oxidation of an iodine compound having an oxidation state of -I to +V in an electrolytic cell, the electrolytic cell comprising an anodic compartment having one or more anodes, a cathodic compartment having one or more cathodes, and a separator arranged between the anodic compartment and the cathodic compartment, the method comprising: include: recirculating the cathode electrolyte to the cathode compartment via a cathode electrolyte loop, recirculating an anolyte to the anode compartment via an anolyte loop, the anolyte comprising a metal periodate and an iodine compound having an oxidation state of -I to +V, the iodine compound being selected from an iodine salt, elemental iodine, a mixture of different iodine salts, or a mixture of iodine and one or more iodine salts, said anodic oxidation of said iodine compound is carried out at a pH of at least 10, wherein the anode electrolyte loop comprises at least one continuously stirred tank reactor operating in a steady-state mode relative to the total molar ratio of metal periodate to iodine compound with oxidation states ranging from -I to +V in the anode electrolyte, wherein the continuously stirred tank reactor is operated in a steady-state mode by continuously or periodically feeding the iodine compound with oxidation states ranging from -I to +V into the continuously stirred tank reactor and continuously or periodically removing the metal periodate from the continuously stirred tank reactor.
2. The method of claim 1, wherein the metal periodate contained in the recycled anode electrolyte is primarily a metal secondary periodate.
3. A method according to any one of claims 1 or 2, wherein operating the continuous stirred tank reactor in steady-state mode relative to the total molar ratio of metal periodate to iodine compounds with oxidation states ranging from -I to +V in the anode electrolyte means: selecting a predetermined molar ratio or molar ratio range so that during operation, the actual molar ratio or molar ratio range of metal periodate to iodine compound remains within the predetermined molar ratio or molar ratio range or close to a preselected molar ratio or molar ratio range, wherein "close" means that the actual molar ratio or molar ratio range may deviate from the selected molar ratio or molar ratio range by up to ±20%, wherein the molar ratio is calculated based on the iodine atoms present in the metal periodate and the iodine compound.
4. The method of claim 3, wherein the predetermined molar ratio or molar ratio range is related to the molar ratio or molar ratio range in the anode electrolyte before entering the anode compartment.
5. The method according to any one of claims 1 to 3, wherein in the recirculating anode electrolyte, the total molar ratio of the metal periodate to the iodine compound in the oxidation state of -I to +V is from 1:>0 to 1:5; wherein in the case where the oxidation state of the iodine compound is from -I to +III, the total molar ratio of the metal periodate to the iodine compound in the oxidation state of -I to +III is from 1:0 to 8:1; and wherein in the case where the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound in the oxidation state of +V is from 1:0 to 1:5; Preferably, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 1:>0 to 1:4; more preferably 200:1 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 1:0 to 1:4, preferably 200:1 to 1:
4.
6. A method according to any one of claims 1 to 4, wherein in the recirculating anode electrolyte, when fed to the anode compartment, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +V is from 1:>0 to 1:5; wherein in the case where the oxidation state of the iodine compound is from -I to +III, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +III is from 1:0 to 8:1; and wherein in the case where the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of +V is from 1:0 to 1:5; Preferably, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +V is 1:>0 to 1:4; more preferably 200:1 to 1:4; wherein when the oxidation state of the iodine compound is -I to +III, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of -I to +III is 1:0 to 10:1, and wherein when the oxidation state of the iodine compound is +V, the total molar ratio of the metal periodate to the iodine compound with an oxidation state of +V is 1:0 to 1:4, more preferably 200:1 to 1:
4.
7. A method according to any one of claims 1 to 4 or 6, wherein in order to operate the continuous stirred tank reactor in steady state mode with respect to the total molar ratio of metal periodate to iodine compound having an oxidation state of -I to +V, a predetermined molar ratio or molar ratio range is selected for the anolyte before entering the anode compartment, so that during operation, the actual molar ratio of metal periodate to iodine compound in the anolyte before entering the anode compartment is maintained within the predetermined molar ratio or molar ratio range ±20%; wherein the predetermined molar ratio or range of molar ratios is thereby selected such that in the anode electrolyte, prior to entry into the anode compartment (i.e. when fed to the anode compartment), the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +V is from 1:>0 to 1:5; wherein in the case where the iodine compound has an oxidation state of -I to +III, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of -I to +III is from 1:0 to 8:1; and wherein in the case where the iodine compound has an oxidation state of +V, the total molar ratio of the metal periodate to the iodine compound in an oxidation state of +V is from 1:0 to 1:5; wherein the molar ratio is calculated based on the iodine atoms present in the metal periodate and the iodine compound.
8. A process according to any one of the preceding claims, for the preparation of an alkali metal paraperiodate, preferably sodium paraperiodate or potassium paraperiodate, wherein the iodine compound having an oxidation state of -I to +V is an alkali metal iodide, an alkali metal iodate, iodine or a mixture thereof, preferably sodium iodide, potassium iodide, sodium iodate, potassium iodate, iodine or a mixture thereof. 9 . The method according to claim 1 , wherein the anodizing is carried out at a pH of at least 11, in particular at least 12.
10. The method according to any one of the preceding claims, wherein the anodization is carried out in the presence of a base, wherein the base is selected from metal hydroxides, metal oxides and metal carbonates.
11. The method according to claim 10, wherein the anodization is carried out in the presence of a metal hydroxide, wherein in the case where the iodine compound having an oxidation state of -I to +V is an alkali metal iodine salt, the metal of the alkali corresponds to the metal in the metal iodine salt. 12 . The method according to claim 1 , wherein the cathode electrolyte comprises an aqueous medium having a pH of at least 10, preferably at least 11, in particular at least 12.
13. The method according to any one of the preceding claims, wherein the anodizing is carried out at 10 mA / cm 2 Up to 1000mA / cm 2 , preferably 100mA / cm 2 Up to 750mA / cm 2 , especially 250mA / cm 2 Up to 500mA / cm 2 , and specifically 400mA / cm 2 Up to 430mA / cm 2 The current density is within the range of .
14. The method according to any of the preceding claims, wherein the separator arranged between the cathode compartment and the anode compartment is selected from a semipermeable membrane, a diaphragm and a glass frit, and is in particular an ion exchange membrane.
15. The method according to any one of the preceding claims, wherein the one or more anodes comprises a carbon-based active layer.
16. The method of claim 15, wherein the one or more anodes comprise a diamond layer doped with one or more elements from Group 13, Group 15, or Group 16 of the IUPAC Periodic Table of Elements.
17. The method of claim 16, wherein the one or more anodes comprise a boron doped diamond layer.
18. The process according to any one of the preceding claims, wherein the iodine compound in an oxidation state of -I to +V is fed to the continuous stirred tank reactor in the form of an aqueous solution, an aqueous suspension or in solid form.
19. An apparatus configured to prepare a metal secondary periodate by the method according to any one of claims 1 to 18, the apparatus include: The electrolytic cell comprises an anode compartment having one or more anodes, a cathode compartment having one or more cathodes, and a separator disposed between the anode compartment and the cathode compartment, the cathode electrolyte loop for recirculating cathode electrolyte through the cathode compartment, the cathode electrolyte loop comprising a cathode electrolyte reservoir, The anode electrolyte loop is used to circulate the anode electrolyte through the anode compartment, and the anode electrolyte loop includes at least one continuously stirred tank reactor. The at least one continuously stirred tank reactor is provided with a feeding device and a discharging device, the feeding device is used to feed the iodine compound with an oxidation state of -I to +V selected from iodine salt, elemental iodine, a mixture of different iodine salts or a mixture of iodine and one or more iodine salts into the at least one continuously stirred tank reactor, and the discharging device is used to discharge the metal periodate reaction product from the at least one continuously stirred tank reactor.
Citation Information
Patent Citations
method for preparing periodate by oxidation of iodate in an electrolysis cell.
NL1013348A
Electrolytic cell for producing periodates
US4687565A
Electrochemical cogeneration of alkali metal halate and alkaline peroxide solutions
US5074975A
Method for preparing periodates
WO2021110928A1