Thermal barrier coating internal stress detection system
Through three-dimensional reconstruction and spectral measurement technology, combined with data processing and robot control, stress detection on curved blades is realized, solving the difficulty of obtaining data in existing systems during curved blade detection and improving detection accuracy and efficiency.
Patent Information
- Application Number
- CN202411232626.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-11-29
AI Technical Summary
The existing internal stress detection system for thermal barrier coatings is difficult to adapt to the stress detection of curved blades, and it is impossible to obtain the complete spectrum data of curved blades.
The three-dimensional reconstruction unit is used to obtain the three-dimensional model of the blade to be tested, combined with the spectral measurement unit and the data processing unit, spectral measurement of specific areas is performed by excitation laser, stress data is calculated using the correspondence between historical stress and spectral peak position, and through the robot The control unit realizes the three-dimensional movement of the curved blade and the tangent plane of the excitation point perpendicular to the direction of the excitation laser incident.
Complete stress detection of curved blades is achieved, which solves the problem that existing systems need to expand the spectral detection range when detecting curved blades, and improves the detection accuracy and efficiency.
Smart Images

Figure CN119043540A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of internal stress field detection of thermal barrier coatings, and in particular relates to an internal stress detection system for thermal barrier coatings. Background Art
[0002] The service temperature of high-pressure turbine blades is generally very high. Therefore, in order to extend the service life of high-pressure turbine blades, it is necessary to provide thermal protection for high-pressure turbine blades. Generally, the thermal protection capability of high-pressure turbine blades is improved from three aspects: high-temperature resistant alloy substrate materials, performance cooling channel design, and advanced thermal barrier coating (TBC) system. Since the thermal barrier coating system has strong designability, the thermal protection capability of high-pressure turbine blades is generally improved from this aspect.
[0003] Thermal barrier coating systems often crack and peel off without warning in complex service environments. Failure factors of thermal barrier coatings include high-temperature oxidation, thermal shock fatigue, high-temperature creep, high-temperature sintering, phase change, high-temperature corrosion, high-temperature particle erosion and impact, etc. The influence of these factors often causes the accumulation of residual stress near the interface. When the accumulated residual stress in the coating, especially near the interface, exceeds its own strength, it will induce the initiation and expansion of cracks and eventually lead to the failure of the coating to peel off. Therefore, the degree of damage to the coating is evaluated by measuring the residual stress inside the coating.
[0004] In order to facilitate the detection of stress of the coating, the patent document with publication number CN110231325A discloses an interface stress detection system and method for thermal barrier coating structure, which includes a laser light source, a first dichroic mirror, a focusing lens and a fluorescence spectrometer; the focusing lens and the fluorescence spectrometer are respectively arranged on both sides of the first dichroic mirror; to obtain rare earth fluorescence spectrum and ruby fluorescence spectrum, and to fully measure the stress distribution characteristics at the key interface inside the thermal barrier coating based on the double fluorescence method. However, the surface of the object to be tested in this system is a plane. When the object to be tested is a curved object, the direction of the fluorescence generated by the object to be tested after laser excitation is diverse. When the direction of the excitation laser is basically unchanged, the range of the detection spectrum needs to be expanded to obtain complete spectral data, that is, it is difficult for the system to perform comprehensive scanning detection of the fluorescence after excitation.
[0005] In summary, the existing blade stress detection system cannot complete the detection of curved blade stress. Summary of the invention
[0006] The technical problem to be solved by the present invention is to provide a thermal barrier coating internal stress detection system in view of the above-mentioned deficiencies in the prior art, which can be adapted to the coating stress detection of curved blades and is easy to promote and use.
[0007] In order to solve the above technical problems, the technical solution adopted by the present invention is: A thermal barrier coating internal stress detection system comprises a three-dimensional reconstruction unit, a spectrum measurement unit and a data processing unit, wherein the three-dimensional reconstruction unit, the spectrum measurement unit and the data processing unit are communicatively connected in sequence; the three-dimensional reconstruction unit is used to obtain three-dimensional coordinate data of a blade to be measured by using a laser rangefinder, thereby performing three-dimensional reconstruction to obtain a three-dimensional model of the blade to be measured; the surface of the blade to be measured is a curved surface; the spectrum measurement unit is used to control an excitation laser to excite a region to be measured selected from the three-dimensional model on the blade to be measured, and obtain spectrum data of the region to be measured; the data processing unit is used to compare the spectrum peak position of the obtained spectrum data with the spectrum peak position of normal spectrum data, thereby determining the spectrum peak position deviation, and calculating the stress data of the blade to be measured in combination with the corresponding relationship between historical stress and spectrum peak position.
[0008] Furthermore, it also includes a robot control unit that is communicatively connected to the three-dimensional reconstruction unit and is used to control the three-dimensional movement of a fixture device, wherein the fixture device is used to clamp the blade to be measured to achieve three-dimensional movement control of the blade to be measured.
[0009] Furthermore, the robot control unit is also used to control the tangent plane of the excitation point of the blade to be measured to be perpendicular to the incident direction of the excitation laser when the excitation laser excites the blade to be measured.
[0010] Furthermore, the process of the three-dimensional reconstruction unit obtaining the three-dimensional model of the blade to be measured is: performing laser ranging scanning on the outer surface of the blade to be measured to obtain the undulating distance data of the outer surface, converting the undulating distance data into three-dimensional coordinate data, and using the three-dimensional coordinate data to establish the three-dimensional model of the blade to be measured.
[0011] Furthermore, the process of selecting the area to be tested is: respectively selecting test areas from the concave surface, the leading edge surface and the convex surface of the blade to be tested, and using the three selected test areas as the area to be tested.
[0012] Furthermore, the spectral data of the area to be measured includes spectral data of a concave surface, a leading edge surface and a convex surface; the data processing unit is used to compare the spectral peaks of the acquired spectral data of the concave surface with the spectral data of the normal concave surface, so as to determine the spectral peak deviation of the concave surface, and calculate the average stress data of the concave surface in combination with the correspondence between the historical stress and the spectral peak of the concave surface; compare the spectral peaks of the acquired spectral data of the leading edge surface with the spectral peaks of the normal leading edge surface, so as to determine the spectral peak deviation of the leading edge surface, and calculate the average stress data of the leading edge surface in combination with the correspondence between the historical stress and the spectral peak of the leading edge surface; compare the spectral peaks of the acquired spectral data of the convex surface with the spectral peaks of the normal convex surface, so as to determine the spectral peak deviation of the convex surface, and calculate the average stress data of the convex surface in combination with the correspondence between the historical stress and the spectral peak of the convex surface; and take the average of the concave surface average stress data, the leading edge surface average stress data and the convex surface average stress data as the stress data of the blade to be measured.
[0013] Furthermore, the spectrum types of the above-mentioned spectrum data include Raman spectrum and fluorescence spectrum. The above-mentioned Raman spectrum is used to calculate the stress data of the ceramic layer, and the above-mentioned fluorescence spectrum is used to calculate the stress data of the oxide layer.
[0014] Furthermore, the excitation laser is emitted by a high-power continuous laser, and the spectrum data is acquired by a line scanning method of a high-speed scanning galvanometer.
[0015] Furthermore, the process of establishing the correspondence between the historical stress and the spectral peak position is as follows: obtain the stress data and spectral peak data at each sampling time before and after use of the blade with the same ambient temperature as the blade to be tested, and establish a linear relationship between stress and spectral peak position in combination with the corresponding frequency shift coefficient, and use it as the correspondence between the historical stress and the spectral peak position.
[0016] Furthermore, the corresponding relationship between historical stress and spectral peak position is expressed as follows:
[0017] in, is the historical stress, is the average stress on the x-axis, is the average stress on the y-axis, It is the spectral peak position of the luminescent ions after the leaves are used. The spectral peak position of the luminescent ion before the leaf is used. is the frequency shift coefficient corresponding to the uniaxial stress state.
[0018] Compared with the prior art, the present invention has the following advantages: The thermal barrier coating internal stress detection system of the present invention obtains the three-dimensional model of the blade to be tested through the three-dimensional reconstruction unit, and the spectrum measurement unit excites the blade to be tested according to the test area selected from the three-dimensional model, and obtains the spectrum data of the test area; in this way, the spectrum detection unit can know the direction of the spectrum after excitation, which is convenient for the spectrum measurement unit to completely obtain the spectrum data. The existing situation that the spectrum detection range needs to be expanded when detecting the stress of the blade with a curved surface is solved, and the stress detection of the coating of the curved blade is realized.
[0019] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the coating structure of a turbine blade in the prior art; Figure 2 It is a structural stereoscopic schematic diagram of an embodiment of a thermal barrier coating internal stress detection system of the present invention; Figure 3 It is a schematic diagram of the structure of an embodiment of a thermal barrier coating internal stress detection system of the present invention; Figure 4 It is a schematic diagram of the structure of a right side view of an embodiment of a thermal barrier coating internal stress detection system of the present invention; Figure 5 A schematic cross-sectional diagram of a three-dimensional topographic image of a blade to be tested according to an embodiment of a thermal barrier coating internal stress detection system of the present invention; Figure 6 A schematic diagram of a concave test area of a blade to be tested in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Figure 7 A schematic diagram of a leading edge test area of a blade to be tested in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Figure 8 A schematic diagram of a convex surface test area of a blade to be tested in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Fig. 9 A schematic diagram of the morphology of a ceramic layer of a blade to be tested in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Fig.10 A schematic diagram of the morphology of the oxide layer of a blade to be tested according to an embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.11 A schematic diagram of spectrum shift of a blade to be tested in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Fig.12 A schematic diagram of the structure of a fixture device of an embodiment of a thermal barrier coating internal stress detection system of the present invention; Fig.13A stress cloud diagram of a ceramic layer of a blade to be tested that changes with service time in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Fig.14 A graph showing the evolution of the average stress of the ceramic layer of a blade to be tested versus the service time in an embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.15 A graph showing the evolution of the stress of the ceramic layer on the leading edge of a blade to be tested versus the service time in an embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.16 A stress cloud diagram showing changes in the oxide layer of a blade to be tested with service time in an embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.17 A graph showing the evolution of the average stress of the oxide layer of a blade to be tested versus the service time in an embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.18 A graph showing the evolution of the stress of the oxide layer on the leading edge of a blade to be tested versus the service time in an embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.19 It is a schematic diagram of the reconstruction result of the bottom surface of the blade to be tested in the embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig. 20 A schematic diagram of the stress detection result of the oxide layer without using the galvanometer technology according to the embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.21 A schematic diagram of the stress detection result of the oxide layer using the galvanometer technology in the embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig. 22 A stress cloud diagram of the oxide layer of a blade to be tested in an embodiment of the thermal barrier coating internal stress detection system of the present invention; Fig.23 A schematic diagram of the stress detection result of a ceramic layer using a galvanometer in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Fig.24 A stress cloud diagram of a ceramic layer of a blade to be tested in an embodiment of a thermal barrier coating internal stress detection system of the present invention; Description of reference numerals: 1. Robot control unit; 2. Three-dimensional reconstruction unit; 3. Spectral measurement unit; 4. Optical platform; 5. Distance measuring baffle. DETAILED DESCRIPTION
[0021] Thermal barrier coating internal stress detection system example: like Figure 1As shown, the thermal barrier coating of the high-pressure turbine blade includes a high-temperature alloy substrate, a ceramic coating, a metal bonding layer between the two layers that acts as an oxygen isolation and stress buffer, and a thermally grown oxide layer generated due to oxidation service.
[0022] With the use of high-pressure turbine blades, the coating will produce peeling failure phenomenon; the peeling of the coating not only makes the metal substrate lose its protective effect, but the collision of coating fragments may also pose a fatal threat to the high-speed rotating turbine blades, and even cause the overall failure of the heavy-duty gas turbine. In order to avoid this phenomenon, the blades need to be inspected. If they have reached the failure stage, they must be replaced with new blades. The existing method generally evaluates whether the blades will peel off and fail by detecting the residual stress of the high-pressure turbine blades. However, the existing method of detecting stress does not use the detection of curved blades. Therefore, the internal stress detection system of the thermal barrier coating of the present application is used to perform stress detection on the curved blade high-pressure turbine blades. The details are as follows: like Figure 2-Figure 4 As shown, the thermal barrier coating internal stress detection system includes a three-dimensional reconstruction unit 2, a spectrum measurement unit 3 and a data processing unit, which are sequentially connected in communication. The system is used to detect the stress of the blade to be tested, so as to evaluate the damage degree of the blade through the stress. Figure 2-Figure 4 The unmarked cube blocks are irrelevant to the solution of this embodiment and can be ignored when understanding this solution. Specifically, the detailed functions of each unit are as follows: 1) Three-dimensional reconstruction unit 2.
[0023] The three-dimensional reconstruction unit 2 is used to obtain the three-dimensional coordinate data of the blade to be measured by using the laser rangefinder, so as to perform three-dimensional reconstruction to obtain the three-dimensional model of the blade to be measured. In order to facilitate modeling, the system also includes a robot control unit 1 that is connected to the three-dimensional reconstruction unit 2 for controlling the position of the fixture device to achieve control of the position of the blade to be measured. That is, the position of the laser rangefinder is fixed, and the robot control unit 1 is used to control the forward and backward, up and down, and rotational movement of the mechanical arm, thereby driving the forward and backward, up and down, and rotational movement of the fixture device at the front end of the mechanical arm, so as to ensure that the three-dimensional reconstruction unit 2 can achieve three-dimensional reconstruction of the blade using the data obtained by the laser rangefinder.
[0024] The process of obtaining the three-dimensional model of the blade to be measured is as follows: the outer surface of the blade to be measured is scanned by laser ranging to obtain the undulating distance data of the outer surface, that is, the outer surface of the blade to be measured is emitted with ranging laser, and the undulating distance data is obtained according to the difference between the received laser and the emitted laser in cooperation with the ranging baffle 5; the undulating distance data is converted into three-dimensional coordinate data, and the three-dimensional coordinate data is used to establish the three-dimensional model of the blade to be measured. Specifically, the outer surface includes a bottom surface, an upper surface, a left side surface and a right side surface. Fig.19As shown, taking the current test surface as the bottom surface as an example, the robot moves to the front of the ranging baffle, and then pushes the ranging baffle backward to make a translational movement. The length data of the blade to be measured can be obtained according to the moving distance of the ranging baffle; when the robot drives the ranging baffle to move to the rear boundary of the slide rail, the rear translational movement ends, and the slide rail refers to the slide rail of the ranging baffle; the robot moves to the rear of the ranging baffle again, and pushes the ranging baffle forward to make a translational movement. The distance of the translational movement refers to the length data of the blade to be measured obtained above; when the blade passes through the laser ranging module at the bottom, the corresponding bottom surface distance information is recorded, and the bottom surface distance information is the undulating distance data; when the robot moves to the front boundary of the slide rail, the three-dimensional reconstruction process of the bottom surface of the blade is completed. If the current test surface is the top, left side or right side, the robot control unit 1 adjusts the test of the page to be tested to a position that is convenient for the laser rangefinder of the three-dimensional reconstruction unit 2 to scan, and the remaining steps for obtaining the corresponding undulating distance data are similar to the above-mentioned process of obtaining the bottom surface undulating distance data, which will not be repeated here.
[0025] 2) Robot control unit 1.
[0026] In order to ensure that the spectral data can be easily obtained, the robot control unit 1 is also used to control the tangent plane of the excitation point of the blade to be measured to be perpendicular to the incident direction of the excitation laser when the excitation laser emits the excitation laser to excite the blade to be measured; further, the robot control unit 1 controls each excitation point of the blade to be measured to be consistent with the excitation laser, so as to ensure the accuracy of stress measurement. Specifically, the direction of the laser in the spectrum measurement unit 3 is fixed, and the detection range of the multi-channel optical fiber probe used to obtain spectral data is also fixed. Therefore, the robot control unit 1 controls the movement of the blade to be measured to ensure that the tangent plane of the excitation point of the blade to be measured is perpendicular to the incident direction of the excitation laser, which is convenient for the excitation laser to excite the blade to be measured and also convenient for the multi-channel optical fiber probe to detect. The robot control unit 1 can realize the precise movement of the blade to be measured in three-dimensional space; the three-dimensional reconstruction unit 2 based on laser ranging can realize the morphology reconstruction of the three-dimensional blade to be measured. The combination of the two can realize the stress measurement of the curved surface area of the three-dimensional blade, ensuring that each measured point in the measurement area is perpendicular to the probe and the distance is consistent, and ensuring the stress measurement accuracy of the measured point.
[0027] The robot control unit 1 controls an Epson VT6L robot arm, which has a rated load of 3kg and a maximum load of 6kg, sufficient to support the load of a 50MW heavy-duty gas turbine secondary blade. The weight of a 50MW gas turbine secondary blade is generally no more than 3kg. In a specific implementation, the robot arm is mounted on a fixed frame, which allows the robot arm to be suspended 30cm in the air. The size and structure of the fixture device are determined according to the actual blade object to be tested.
[0028] 3) Spectral measurement unit 3.
[0029] like Figure 2 As shown, the spectrum measurement unit 3 is used to control the excitation laser to excite the blade to be measured according to the area to be measured selected from the three-dimensional model, and obtain the spectrum data of the area to be measured; in order to ensure that the excitation laser can reach the oxide layer, the excitation laser is emitted by a high-power continuous laser, and the excitation laser can penetrate a ceramic layer with a thickness of not less than 0.3mm; the spectrum data is obtained by line scanning using a high-speed scanning galvanometer. The spectrum data includes Raman spectrum and fluorescence spectrum, the Raman spectrum is used to calculate the stress data of the ceramic layer, and the fluorescence spectrum is used to calculate the stress data of the oxide layer.
[0030] The process of selecting the test area is to select the test area from the concave surface, the leading edge surface and the convex surface of the blade to be tested respectively, and use the three selected test areas as the test area. Preferably, the test area is less than or equal to 50 mm×50 mm.
[0031] The rated power of this high-power continuous laser can reach 300mW; the monochromatic light emitted can successfully penetrate a ceramic layer with a thickness of not less than 0.3mm, and the excited fluorescence can be measured with a high signal-to-noise ratio. Fig. 20 As shown in the figure, the high-power continuous laser is used to excite the blade to be tested, and the fluorescence spectrum of the oxide layer near the inner interface is obtained when the single-point integration time is 2 seconds. Fig. 20 The two typical fluorescence peaks of Cr ions can be clearly seen in the figure, which are 693nm and 695nm. Compared with the initial peaks of 692nm and 694nm, there is an obvious peak shift phenomenon, so there is obvious residual stress in the oxide layer. Therefore, by using a high-power continuous laser, the goal of penetrating the ceramic layer to measure the fluorescence spectrum of the oxide layer in the interface area was successfully achieved.
[0032] This application not only uses the high-power continuous laser, but also adds a galvanometer. Without the galvanometer, in single-point test mode, the total test time required to measure an area of 50×50 points (the test area size is 50 mm×50 mm) is 2.08 hours, so the test time for each point is 3 seconds. Fig.13 As shown in the figure, when the galvanometer is added, the total test time required for testing an area with a test array of 50×50 points (area size is 50 mm×50 mm) is 0.36 hours, and the test time for each point is 0.52 seconds; therefore, the test time can be greatly shortened by adding the galvanometer technology.
[0033] 4) Data processing unit.
[0034] The data processing unit is used to compare the spectrum peaks of the acquired spectrum data with the normal spectrum data to determine the spectrum peak deviation, and calculate the stress data of the blade to be tested in combination with the corresponding relationship between the historical stress and the spectrum peak. Specifically, the spectrum data includes spectrum data of the concave surface, the leading edge surface and the convex surface. Furthermore, the process of calculating the stress data of the blade to be tested is as follows: comparing the spectral peaks of the acquired spectral data of the concave surface with the spectral peaks of the normal concave surface to determine the spectral peak deviation of the concave surface, and calculating the average stress data of the concave surface in combination with the correspondence between the historical stress and the spectral peak of the concave surface; comparing the spectral peaks of the acquired spectral data of the leading edge surface with the spectral peaks of the normal leading edge surface to determine the spectral peak deviation of the leading edge surface, and calculating the average stress data of the leading edge surface in combination with the correspondence between the historical stress and the spectral peak of the leading edge surface; comparing the spectral peaks of the acquired spectral data of the convex surface with the spectral peaks of the normal convex surface to determine the spectral peak deviation of the convex surface, and calculating the average stress data of the convex surface in combination with the correspondence between the historical stress and the spectral peak of the convex surface; and taking the average of the concave surface average stress data, the leading edge surface average stress data and the convex surface average stress data as the stress data of the blade to be tested.
[0035] The process of establishing the correspondence between historical stress and spectral peak position is as follows: obtain the stress data and spectral peak data at each sampling time before and after the blade is used in the same usage scenario as the blade to be tested, and establish the linear relationship between stress and spectral peak position in combination with the corresponding frequency shift coefficient, and use it as the correspondence between historical stress and spectral peak position. Since the thermal barrier coating of the blade to be tested is subjected to stress under plane equiaxial stress conditions, the stresses of the x-axis, y-axis, and z-axis have the following relationship, namely: , Specifically, the corresponding relationship between stress and spectral peak position is expressed as:
[0036] in, is the blade stress, is the average stress on the x-axis, is the average stress on the y-axis, It is the spectral peak position of the luminescent ions after the leaves are used. The spectral peak position of the luminescent ion before the leaf is used. is the frequency shift coefficient under uniaxial stress state; when calculating the stress of oxide layer, the luminescent ion is Cr ion; when calculating the stress of ceramic layer, the luminescent ion is Zr ion. The initial peak position of Zr ion in ceramic layer 645.0cm -1 The frequency shift coefficient of Zr ions under uniaxial stress is 25.0 cm -1 / GPa; Correspondingly, the initial peak position of Cr ions in the oxide layer 694.3 cm -1 The frequency shift coefficient of Cr ions under uniaxial stress is 2.04 cm -1 / GPa.
[0037] In order to ensure the accuracy of the detection, the equipment and devices involved in the thermal barrier coating internal stress detection system are installed on an absolutely horizontal optical platform 4 and fixed to the corresponding position of the optical platform 4 by bolts. The mechanical arm must be placed on a stainless steel frame higher than the optical platform 4 to ensure that there is no interference with the optical platform 4 within the effective range of motion of the mechanical arm.
[0038] This embodiment uses the test of the secondary blade of a domestic 50MW gas turbine as an example for explanation. The overall length of the blade is 20cm, the blade body length is 14cm, the blade body width is 7cm, and the overall weight is 3.0kg. The blade substrate is made of a nickel-based high-temperature alloy, and the substrate thickness is not less than 1.0mm; a NiCoCrAlY alloy bonding layer is coated in the middle, and the bonding layer thickness is 0.1mm; the surface is sprayed with a YSZ ceramic layer using atmospheric plasma technology, and the ceramic layer thickness is 0.3mm. The system can test both the ceramic layer stress and the oxide layer stress. The specific steps for testing stress using the system are as follows: (1) Fix the blade to the fixture system with bolts, and fix the fixture system to the front end of the robot arm; start the three-dimensional structural reconstruction scanning of the blade.
[0039] (2) If Figure 5-Figure 11 As shown, Figure 6 , Figure 7 , Figure 8 The points in the table refer to the number of measurement points. Fig. 9 Holes in the word means pores. Fig.10 Mixed Oxide in is oxidation, Fig.11 Wavenumber is the wave number, Raman for Zr 4+ inYSZ for Raman spectroscopy, Luminescence for Cr 3+ in TGO is the fluorescence spectrum, Compressed State is the stress state, and Unstressed State is the stress-free state. Select the measured area on three typical cross sections of the three-dimensionally reconstructed blade surface, set the number of measurement points and measurement parameters, and measure the measured area; for the ceramic layer, select the Raman spectrum measurement range of 500nm to 800nm, and for the oxide layer, select the fluorescence spectrum measurement range of 680nm to 710nm; process the measured spectral information to obtain the spectral peak position data.
[0040] (3) The data processing unit compares the spectral peak with the normal spectral peak to determine the spectral peak deviation, and calculates the stress data of the blade to be tested based on the spectral peak deviation using the correspondence between the historical stress and the spectral peak. The normal spectral peak refers to the spectral peak of the blade to be tested before use, or the spectral peak of the blade to be tested without grinding. When calculating the stress of the ceramic layer, the correspondence between the historical stress and the spectral peak refers to the correspondence between the historical ceramic layer stress and the spectral peak; when calculating the stress of the oxide layer, the correspondence between the historical stress and the spectral peak refers to the correspondence between the historical oxide layer stress and the spectral peak.
[0041] The specific ion of the ceramic layer is Zr ion, and its excitation spectrum is Raman spectrum, with a typical peak wave number of 640 cm -1 The specific ion of the oxide layer is Cr ion, and its excitation spectrum is a fluorescence spectrum with two typical peaks. The wavelength of one peak is 692nm, and the corresponding wave number is 14450.9cm -1 ; The wavelength of the other peak is 694nm, and the corresponding wave number is 14409.2cm -1 .
[0042] The ceramic layer stress of the blade is detected, the historical ceramic layer stress data is obtained, the corresponding relationship between the historical ceramic layer stress and the spectral peak is established, and the stress data of the ceramic layer of the blade to be tested is calculated based on the corresponding relationship between the historical ceramic layer stress and the spectral peak according to the spectral peak deviation currently measured. Specifically, Figure 4 The following are the appearance pictures of the blade at different temperatures before and after use at different sampling times; Figure 5 The stress cloud diagram of the blade ceramic layer at each sampling time before and after use is shown. The sampling times after use are: 40h, 80h, 120h, 160h, 200h, 300h, 400h, 500h, 600h, 700h. Figure 5 It can be seen that the stress dispersion in the ceramic layer is very large when not in service, and the tensile stress state and the compressive stress state coexist and show random distribution characteristics. Figure 6 , Figure 7As shown in the figure, when the service time of the blade reaches 40h at high temperature, the stress of the ceramic layer on the blade surface shifts to tensile stress as a whole, and the dispersion decreases sharply. This is because the tensile stress generated by the oxidation of the matrix during the service process exceeds the compressive stress caused by the oxidation of the oxide layer, causing the stress of the ceramic layer to shift to the tensile stress direction as a whole. At the same time, it can be found that when the service time is between 0h and 160h, the residual stress of the ceramic layer is in a continuous deflection state, that is, it shifts to the tensile stress direction from 0h to 80h, and shifts to the compressive stress direction from 80h to 160h. When the service time of the blade is between 160h and 600h, although the stress of the ceramic layer has a slight deflection, the magnitude of the overall average stress has not changed significantly. The oxidation growth of the oxide layer and the oxidation growth of the matrix are slowed down, and the corresponding induced stress is also reduced, resulting in the stability of the overall stress of the ceramic layer. When the service time of the blade is between 600h and 720h, the average stress of the ceramic layer drops rapidly, and the blade fails at 720h.
[0043] The oxide layer stress of the blade is detected, the historical oxide layer stress data is obtained, the corresponding relationship between the historical oxide layer stress and the spectral peak is established, and the stress data of the oxide layer of the blade to be tested is calculated based on the corresponding relationship between the historical oxide layer stress and the spectral peak according to the spectral peak deviation currently measured. Specifically, Fig.16 As shown in the figure, from the stress cloud diagram of the blade interface oxide layer after different oxidation service times, it can be seen that the stress dispersion in the oxide layer is large when not in service, and there is a phenomenon of coexistence of tensile stress state and compressive stress state. Fig.17 , Fig.18 As shown in the figure, when the oxidation service time is between 40h and 120h, the stress of the oxide layer at the blade interface shifts toward tensile stress as a whole, and the dispersion decreases sharply, and the stress concentration phenomenon disappears. When the oxidation service time is between 120h and 200h, the residual stress of the oxide layer shifts toward compressive stress as a whole. When the blade service time is between 200h and 600h, the stress of the oxide layer shows a slight deflection, but the magnitude of the overall average stress has not changed significantly. When the blade service time is between 600h and 720h, the average stress of the oxide layer also drops rapidly.
[0044] Among them, Figure 14-Figure 24 In the figure, Deflecting Stage is the deflection stage, Steady Stage is the stable stage, Failure Stage is the failure stage, YSZ Residual Stress is the residual stress of the ceramic layer, Oxidation Tims is the oxidation time, and TGO Residual Stress is the residual stress of the oxide layer.
[0045] In summary, based on the galvanometer technology and high-power continuous laser, the scanning time of Raman and fluorescence spectrum tests can be greatly shortened. For the Cr ion fluorescence spectrum with a strong signal, the limit scanning time can be compressed to 50ms, and for the Zr ion Raman spectrum with a weak signal, the limit scanning time can be compressed to 500ms. The stress detection of any area of the complex curved three-dimensional blade is realized through the three-dimensional reconstruction unit 2, the spectrum measurement unit 3 and the data processing unit.
[0046] The system obtains the three-dimensional model of the blade to be tested through the three-dimensional reconstruction unit 2, and the spectrum measurement unit 3 excites the blade to be tested according to the area to be tested selected from the three-dimensional model, and obtains the spectrum data of the area to be tested; in this way, the spectrum detection unit can know the direction of the spectrum after excitation, which is convenient for the spectrum measurement unit 3 to completely obtain the spectrum data. The existing situation that the spectrum detection range needs to be expanded when detecting the stress of the blade with a curved surface is solved, and the coating stress of the curved blade is detected.
[0047] In addition, the robot control unit 1 is used to realize three-dimensional movement of the blade to be measured, and the tangent plane of the excitation point of the blade to be measured is controlled to be perpendicular to the incident direction of the excitation laser, so that the probe for detecting the spectrum in the spectral detection unit can be set in only one plane. Because by controlling the tangent plane of the excitation point of the blade to be measured to be perpendicular to the incident direction of the excitation laser, the spectral direction of the blade to be measured is also basically determined, and it is only necessary to set the spectral detection equipment at the corresponding position, which further reduces the cost of spectral detection.
[0048] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any simple modification, change and equivalent structural change made to the above embodiment based on the technical essence of the present invention still falls within the protection scope of the technical solution of the present invention.
Claims
1. A thermal barrier coating internal stress detection system, characterized in that: The system comprises a three-dimensional reconstruction unit, a spectrum measurement unit and a data processing unit, wherein the three-dimensional reconstruction unit, the spectrum measurement unit and the data processing unit are sequentially connected in communication; The three-dimensional reconstruction unit is used to obtain the three-dimensional coordinate data of the blade to be measured by using a laser rangefinder, and to perform three-dimensional reconstruction to obtain a three-dimensional model of the blade to be measured; the surface of the blade to be measured is a curved surface; The spectrum measurement unit is used to control the excitation laser to excite the area to be measured selected from the three-dimensional model on the blade to be measured, and obtain spectrum data of the area to be measured; The data processing unit is used to compare the spectrum peaks of the acquired spectrum data with the normal spectrum data to determine the spectrum peak deviation, and calculate the stress data of the blade to be tested in combination with the corresponding relationship between the historical stress and the spectrum peak.
2. The thermal barrier coating internal stress detection system according to claim 1, characterized in that: It also includes a robot control unit that is communicatively connected to the three-dimensional reconstruction unit and is used to control the three-dimensional movement of a fixture device, wherein the fixture device is used to clamp the blade to be measured to achieve three-dimensional movement control of the blade to be measured.
3. The thermal barrier coating internal stress detection system according to claim 2, characterized in that: The robot control unit is also used to control the tangent plane of the excitation point of the blade to be measured to be perpendicular to the incident direction of the excitation laser when the excitation laser excites the blade to be measured.
4. The thermal barrier coating internal stress detection system according to claim 2, characterized in that: The process of the three-dimensional reconstruction unit obtaining the three-dimensional model of the blade to be measured is as follows: performing laser ranging scanning on the outer surface of the blade to be measured to obtain the undulating distance data of the outer surface, converting the undulating distance data into three-dimensional coordinate data, and using the three-dimensional coordinate data to establish the three-dimensional model of the blade to be measured.
5. The thermal barrier coating internal stress detection system according to claim 1, characterized in that: The process of selecting the area to be tested is as follows: test areas are respectively selected from the concave surface, the leading edge surface and the convex surface of the blade to be tested, and the three selected test areas are used as the area to be tested.
6. The thermal barrier coating internal stress detection system according to claim 5, characterized in that: The spectral data of the area to be measured include spectral data of a concave surface, a leading edge surface and a convex surface; The data processing unit is used to compare the spectrum peaks of the acquired spectrum data of the concave surface with the spectrum data of the normal concave surface, so as to determine the spectrum peak deviation of the concave surface, and calculate the average stress data of the concave surface in combination with the corresponding relationship between the historical stress and the spectrum peak of the concave surface; Compare the spectral peaks of the acquired spectral data of the leading edge surface with those of the spectral data of the normal leading edge surface, thereby determining the spectral peak deviation of the leading edge surface, and calculate the average stress data of the leading edge surface in combination with the corresponding relationship between the historical stress and the spectral peak of the leading edge surface; Compare the spectral peaks of the acquired convex surface spectral data with those of the normal convex surface spectral data to determine the spectral peak deviation of the convex surface, and calculate the average stress data of the convex surface in combination with the corresponding relationship between the historical stress and the spectral peak of the convex surface; The average of the concave surface average stress data, the leading edge surface average stress data and the convex surface average stress data is taken as the stress data of the blade to be tested.
7. The thermal barrier coating internal stress detection system according to claim 1, characterized in that: The spectrum types of the spectrum data include Raman spectrum and fluorescence spectrum. The Raman spectrum is used to calculate the stress data of the ceramic layer, and the fluorescence spectrum is used to calculate the stress data of the oxide layer.
8. The thermal barrier coating internal stress detection system according to claim 1, characterized in that: The excitation laser is emitted by a high-power continuous laser, and the spectrum data is acquired by a line scanning method of a high-speed scanning galvanometer.
9. The thermal barrier coating internal stress detection system according to claim 1, characterized in that: The process of establishing the correspondence between the historical stress and the spectral peak position is as follows: obtaining the stress data and spectral peak data at each sampling time before and after use of a blade with the same ambient temperature as the blade to be tested, establishing a linear relationship between stress and spectral peak position in combination with the corresponding frequency shift coefficient, and using it as the correspondence between the historical stress and the spectral peak position.
10. The thermal barrier coating internal stress detection system according to claim 1, characterized in that: The corresponding relationship between the historical stress and the spectral peak position is expressed by the formula: in, is the historical stress, is the average stress on the x-axis, is the average stress on the y-axis, It is the spectral peak position of the luminescent ions after the leaves are used. The spectral peak position of the luminescent ion before the leaf is used. is the frequency shift coefficient corresponding to the uniaxial stress state.
Citation Information
Patent Citations
Nondestructive testing method of residual stress of thermally grown oxide layers in thermal barrier coatings
CN106066319A
Turbine blade thermal barrier coating working condition simulation experiment test system
CN109682702A
Raman spectrum method for simultaneously measuring temperature and thermal stress of two-dimensional thin film material in situ
CN110736499A
Thermal barrier coating and preparation method and application thereof
CN111394702A
Space suit helmet face window internal stress lossless tracking detection method
CN114777971A
Cited By
System and method for detecting splicing and welding residual stress of multi-curve stretch-bending oversized aluminum plate