Device and method for detecting bonding failure between rubber material and base material

Through aging test and data analysis, a rubber-substrate combination aging impact evaluation index was generated, which solved the problem of changes in the bonding density between rubber support and substrate, and achieved accurate evaluation and safety guarantee of the bonding density between rubber and substrate. .

CN119044463APending Publication Date: 2024-11-29SUZHOU IND PARK YUANRONG KECHUANG ELECTROMECHANICAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411245840.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-06
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

During use, the bonding density between the rubber support and the substrate changes lead to loosening and offset, which poses safety risks. It is difficult for the prior art to effectively judge the bonding density between the rubber and the substrate.

Method used

The friction coefficient and volume change of rubber surface are recorded through the aging test, and the aging friction coefficient and volume change coefficient are generated, the impact evaluation index of rubber-substrate bond aging is calculated, and the bond density level is judged.

Benefits of technology

The accurate evaluation of the bonding density between rubber and substrate is achieved, providing confidence in the bonding density level between rubber and substrate, ensuring safety and product performance maintenance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119044463A_ABST
    Figure CN119044463A_ABST
Patent Text Reader

Abstract

The invention provides a device and a method for detecting bonding failure between a rubber material and a base material, and relates to the technical field of rubber detection.The method comprises the steps of collecting data, analyzing and processing the data and outputting the compactness grade. Friction coefficient change and volume change of the rubber surface subjected to aging test are collected for analysis and are correspondingly converted into effective use time at normal temperature, so that correlation analysis is performed on the change quantity of the friction coefficient of the rubber surface along with time, and the aging friction coefficient is generated; a rubber aging volume change coefficient is generated by performing correlation analysis on the volume change of rubber subjected to aging test, the rubber aging volume change coefficient and the aging friction coefficient are further comprehensively analyzed, and a rubber-base material bonding aging influence evaluation index is output. Therefore, the combination tightness grade of the rubber and the base material is judged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of rubber detection, and in particular to a device and method for detecting failure of bonding between a rubber material and a substrate. Background Art

[0002] The combination of rubber and substrate is a very important project in many industries, especially in manufacturing. This involves how to effectively combine rubber with substrate to improve the performance and durability of the product. Rubber is a highly elastic polymer material. Natural rubber is mainly extracted from the latex collected from rubber trees, while synthetic rubber is made by chemical synthesis. The main feature of rubber is its excellent elasticity and its ability to return to its original shape after being subjected to force. Rubber has a wide range of uses, including tires, seals, shockproof components, etc. Substrate refers to any material used in combination with rubber, which can be metal, plastic, textiles, etc. The choice of substrate depends on the application requirements of the final product, such as strength, toughness, heat resistance or conductivity. In the bridge system, the bearing is an important component of the bridge system. It is a key part connecting the superstructure and the substructure of the bridge. The rubber bearing has good performance and can meet the rotation of the beam end. In addition, it also has large shear deformation.

[0003] However, during the use of rubber bearings, as the use time increases, its performance is bound to change to a certain extent, and cause a certain change in the bonding tightness between the rubber and the bearing substrate. Poor bonding tightness will cause loosening and deviation between the rubber and the substrate, which is dangerous. Therefore, it is very important to judge the bonding tightness between the rubber and the substrate.

[0004] The above information disclosed in this Background section is only for enhancement of understanding of the background of the present disclosure and therefore it may contain information that does not constitute the prior art that is already known to one of ordinary skill in the art. Summary of the invention

[0005] The object of the present invention is to provide a device and method for detecting failure of bonding between a rubber material and a substrate, so as to solve the problems raised in the above-mentioned background technology.

[0006] To achieve the above object, the present invention provides the following technical solutions:

[0007] A method for detecting failure of bonding between a rubber material and a substrate, the specific steps comprising:

[0008] S1. Set aging test parameters, place n round rubbers in an aging box for aging test, and record the average friction coefficient, average radius, and average thickness of the round rubber surface every hour;

[0009] S2, preprocessing the aging test parameters to generate an equivalent time expression;

[0010] S3, performing correlation analysis on the average value of the circular rubber surface friction coefficient and the aging time, and generating an aging friction coefficient by the least square method, wherein the aging friction coefficient is used to reflect the surface friction coefficient of the circular rubber after aging over time;

[0011] S4, pre-processing the average radius and average thickness of the circular rubber in the aging test to generate a volume coefficient, wherein the volume coefficient is used to reflect the volume value of the circular rubber that changes with time during the aging test;

[0012] S5, pre-processing the volume coefficient and initial volume of the circular rubber after the aging test to generate a rubber aging volume change coefficient, wherein the rubber aging volume change coefficient is used to reflect the volume value change degree of the circular rubber as it ages over time;

[0013] S6, pre-processing the rubber aging volume change coefficient and the aging friction coefficient to generate a rubber-substrate combination aging impact evaluation index, wherein the rubber-substrate combination aging impact evaluation index is used to reflect the degree of bonding between the rubber and the substrate;

[0014] S7. Compare the rubber-substrate bonding aging impact evaluation index with the bonding threshold, and output the bonding tightness level of the rubber and the substrate.

[0015] Furthermore, in S1, n is not less than 10, the radius of the circular rubber is 10 cm, and the thickness is 5 cm. The aging test parameters include test temperature and aging time. The test temperature is 100 degrees Celsius, and the aging time is 100 hours.

[0016] Furthermore, in S2, according to the Arrhenius formula, it can be obtained that:

[0017]

[0018] Where t is the aging time, T is the test temperature, A is a constant term, E is the surface activation energy, R is the molar gas constant, the equivalent aging time of the round rubber at the equivalent temperature T1 is t1, and the aging time of the round rubber at the aging temperature T2 is t2. For the equivalent temperature T1, equivalent time t1, aging temperature T2, aging time t2 and equation: Perform correlation analysis and generate an expression for the equivalent time t1 as follows:

[0019]

[0020] Among them, the aging temperature T2 is 100 degrees Celsius, the equivalent temperature T1 is 20 degrees Celsius, and the equivalent time t1 can be output according to the aging time t2.

[0021] Furthermore, during the aging test, the aging time t2 is set to 1, 2, 3, ..., N hours, N is not less than 50, and the friction coefficient function is set to:

[0022]

[0023] Among them, μ is the friction coefficient of the rubber surface, a, b, c are constant terms, t2 is the aging time, and the values ​​of a, b, c are generated by least squares fitting based on the aging time-average circular rubber friction coefficient scatter plot per hour. The expression of equivalent time and the friction coefficient function are analyzed for correlation, and the equivalent time t1 expression is substituted into the friction coefficient function, and the time unit is converted to generate the aging friction coefficient LMX. The formula is as follows:

[0024]

[0025] Wherein, e is a natural constant, t is the service life of the rubber, i.e., the equivalent time, in years. The equivalent time is used to reflect the equivalent service life of the circular rubber after aging test at room temperature, where the room temperature is 20 degrees Celsius. α is the influencing factor of the friction coefficient of the circular rubber, and its value range is [0.1, 0.95].

[0026] Furthermore, during the aging test, the average radius at the jth hour is d j , the average thickness at the jth hour is s j , perform correlation analysis on the average radius and average thickness to generate the volume factor TX at the jth hour j , the formula based on is:

[0027] TX j =π*d j 2 *s j

[0028] Among them, π is the ratio of a circle to its circumference.

[0029] Furthermore, the correlation analysis is performed on the radius and thickness of the circular rubber to generate the initial volume V of the circular rubber, and the formula used is: V = 5*10 2 *π.

[0030] Furthermore, for the expression of equivalent time, volume coefficient TX j The correlation analysis is performed with the initial volume V to generate the rubber aging volume change coefficient XTX, based on the formula:

[0031]

[0032] Wherein, t is the service life of rubber, in years, and β is the influencing factor of the friction coefficient of circular rubber, with a value range of [0.16, 1.98].

[0033] Furthermore, the correlation analysis of the rubber aging volume change coefficient XTX and the aging friction coefficient LMX was performed to generate the rubber-substrate combined aging impact evaluation index XJP, based on the formula:

[0034]

[0035] The bonding threshold is θ, and the rubber-substrate bonding aging impact evaluation index is XJP. When XJP ≥ θ, it means that the bonding tightness level of the rubber and the substrate is level three, and the bonding tightness confidence of the rubber and the substrate is 0%; when When , it means that the bonding tightness level between rubber and substrate is level 2, and the bonding tightness confidence level between rubber and substrate is 70%; when When , it means that the bonding tightness level between the rubber and the substrate is level one, and the confidence level of the bonding tightness between the rubber and the substrate is 95%.

[0036] The present invention also provides a bonding failure detection device between a rubber material and a substrate, comprising a mounting mechanism and a debonding test assembly:

[0037] The mounting mechanism comprises a bottom plate, a support column and a top plate, wherein the support column is fixedly connected to the bottom plate, and the top plate is fixedly connected to the top end of the support column;

[0038] The degumming test assembly includes an electric cylinder, a pressure sensor protective cover, a hardened block, a pressure sensor, a connecting plate and a pressure head. The electric cylinder is installed at the top center of the top plate, the bottom output shaft of the electric cylinder is fixedly connected to the pressure sensor protective cover, the bottom of the pressure sensor protective cover is fixedly connected to the hardened block, the pressure sensor is arranged on the lower side of the hardened block, the pressure sensor is installed on the top of the connecting plate, the pressure head is installed at the bottom center of the connecting plate, a protective block is installed on the outside of the pressure sensor protective cover, and the pressure sensor is slidably connected to the inner side wall of the protective block.

[0039] Furthermore, a slide rail is fixedly connected between the bottom plate and the top plate, a slider is slidably connected to one side of the slide rail, a connecting block is welded to one side of the slider, and the connecting block is fixedly connected to the connecting plate.

[0040] Compared with the prior art, the present invention has the following beneficial effects:

[0041] The present invention analyzes the degree of bonding between rubber and substrate, conducts targeted detection on the performance change of the rubber side, collects the friction coefficient change and volume change of the rubber surface in the aging test for analysis, and converts them into the effective use time at room temperature, thereby performing a correlation analysis on the amount of change of the friction coefficient of the rubber surface over time to generate an aging friction coefficient, and performs a correlation analysis on the change in volume of the rubber in the aging test to generate a rubber aging volume change coefficient. The present invention further conducts a comprehensive analysis on the rubber aging volume change coefficient and the aging friction coefficient, outputs a rubber-substrate bonding aging impact evaluation index, and thus judges the bonding tightness level of the rubber and the substrate. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 It is a schematic diagram of the overall method flow of the present invention;

[0043] Figure 2 It is a schematic diagram of the structure of the bonding failure detection device between the rubber material and the substrate of the present invention;

[0044] Figure 3 It is a structural schematic diagram of the degumming test assembly of the present invention.

[0045] In the figure: 11, bottom plate; 12, support; 13, top plate; 21, electric cylinder; 22, pressure sensor protection cover; 23, hardening block; 24, pressure sensor; 25, connecting plate; 26, pressure head; 27, protective block; 31, slide rail; 32, slider; 33, connecting block. DETAILED DESCRIPTION

[0046] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments.

[0047] It should be noted that, unless otherwise defined, the technical terms or scientific terms used in the present invention should be understood by people with ordinary skills in the field to which the present invention belongs. The words "first", "second" and similar words used in the present invention do not indicate any order, quantity or importance, but are only used to distinguish different components. "Include" or "comprise" and similar words mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connect" or "connected" and similar words are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0048] Example:

[0049] See also Figure 1 , the present invention provides a technical solution:

[0050] A method for detecting failure of bonding between a rubber material and a substrate. When the rubber and the substrate are bonded, one side of the rubber is analyzed. When the performance of the rubber changes, the bonding tightness between the rubber and the substrate will change. The causes involved are analyzed. Under normal circumstances, when the surface friction coefficient of the rubber changes, the bonding tightness between the rubber and the substrate will change. The smaller the friction coefficient, the worse the bonding tightness between the two under the same conditions. In addition, after the rubber and the substrate are bonded, the rubber itself deforms over time, which will cause the bonding tightness with the substrate to change. Therefore, the present invention analyzes the friction coefficient of the rubber surface and the volume change factor to judge the bonding tightness level between the rubber and the substrate. The specific steps include:

[0051] Step 1: Set the aging test parameters, place n round rubbers in the aging box for aging test, and record the average friction coefficient, average radius, and average thickness of the round rubber surface every hour; in order to make the results more accurate, multiple groups are tested simultaneously, and the average values ​​are averaged. The aging box is a rubber aging test box that can perform aging tests on rubber at set temperature and time.

[0052] In step 1, n is not less than 10, the radius of the circular rubber is 10 cm, the thickness is 5 cm, and the aging test parameters include test temperature and aging time. The test temperature is 100 degrees Celsius and the aging time is 100 hours.

[0053] Step 2: Preprocess the aging test parameters and generate equivalent time expressions, as follows:

[0054] According to the Arrhenius formula, we can get:

[0055]

[0056] Where t is the aging time, T is the test temperature, A is a constant term, E is the surface activation energy, R is the molar gas constant, the equivalent aging time of the round rubber at the equivalent temperature T1 is t1, and the aging time of the round rubber at the aging temperature T2 is t2. For the equivalent temperature T1, equivalent time t1, aging temperature T2, aging time t2 and equation: Perform correlation analysis by substituting T1, t1, T2, and t2 into the equation: Finally, combine similar terms to generate an expression for the equivalent time t1, as follows:

[0057]

[0058] Among them, the aging temperature T2 is 100 degrees Celsius, the equivalent temperature T1 is 20 degrees Celsius, and the equivalent time t1 can be output according to the aging time t2.

[0059] Step 3: Perform a correlation analysis on the average value of the circular rubber surface friction coefficient and the aging time, and generate the aging friction coefficient by the least square method. The aging friction coefficient is used to reflect the surface friction coefficient of the circular rubber after aging over time;

[0060] During the aging test, the aging time t2 is set to 1, 2, 3, ..., N hours, N is not less than 50, and the friction coefficient function is set as follows:

[0061]

[0062] Among them, μ is the friction coefficient of the rubber surface, a, b, c are constant terms, t2 is the aging time, and the values ​​of a, b, c are generated by least squares fitting based on the aging time-average circular rubber friction coefficient scatter plot per hour. The expression of equivalent time and the friction coefficient function are analyzed for correlation, and the equivalent time t1 expression is substituted into the friction coefficient function, and the time unit is converted to generate the aging friction coefficient LMX. The formula is as follows:

[0063]

[0064] Among them, e is a natural constant, t is the rubber usage time, that is, the equivalent time, in years. The equivalent time is used to reflect the equivalent usage time of the circular rubber that has undergone aging test at room temperature. The normal temperature is 20 degrees Celsius. α is the influencing factor of the circular rubber friction coefficient, and the value range is [0.1, 0.95]. a, b, and c are constant terms, and each type of rubber corresponds to a different value. The aging friction coefficient LMX is positively correlated with the rubber usage time t.

[0065] The larger the value of the aging friction coefficient LMX, the greater the change in the surface friction coefficient of the round rubber after aging over time, indicating that the bonding tightness between the rubber and the substrate is better;

[0066] Step 4: Preprocess the average radius and average thickness of the circular rubber in the aging test to generate a volume coefficient. The volume coefficient is used to reflect the volume value of the circular rubber that changes with time during the aging test. The preprocessing process is as follows:

[0067] During the aging test, the average radius at the jth hour is d j , the average thickness at the jth hour is s j , perform correlation analysis on the average radius and average thickness to generate the volume factor TX at the jth hour j , the formula based on is:

[0068] TX j =π*d j 2 *s j

[0069] Among them, π is the ratio of a circle to its circumference.

[0070] Step 5: Pre-process the volume coefficient and initial volume of the circular rubber after aging test to generate the rubber aging volume change coefficient. The rubber aging volume change coefficient is used to reflect the volume value change degree of the circular rubber with aging over time. The pre-processing process is as follows:

[0071] The radius and thickness of the circular rubber are analyzed for correlation to generate the initial volume V of the circular rubber. The formula is: V = 5*10 2 *π.

[0072] Expression for equivalent time, volume factor TX j The correlation analysis is performed with the initial volume V to generate the rubber aging volume change coefficient XTX, based on the formula:

[0073]

[0074] Among them, t is the rubber usage time, in years, β is the influencing factor of the circular rubber friction coefficient, and its value range is [0.16, 1.98]. The rubber aging volume change coefficient XTX is positively correlated with the rubber usage time t.

[0075] The larger the value of the rubber aging volume change coefficient XTX, the greater the volume change of the rubber over time, which in turn makes the bonding tightness between the rubber and the substrate worse.

[0076] Step 6: Pre-process the rubber aging volume change coefficient and aging friction coefficient to generate a rubber-substrate bonding aging impact evaluation index, which is used to reflect the degree of bonding between the rubber and the substrate as the rubber ages;

[0077] The correlation analysis of the rubber aging volume change coefficient XTX and the aging friction coefficient LMX is performed to generate the rubber-substrate combined aging impact evaluation index XJP, based on the formula:

[0078]

[0079] The rubber-substrate bonding aging impact evaluation index XJP is a comprehensive evaluation index of the comprehensive rubber surface friction coefficient and the rubber volume change, which is used to comprehensively evaluate the bonding effect between rubber and substrate. The larger the value, the worse the bonding effect. The rubber-substrate bonding aging impact evaluation index XJP is positively correlated with the rubber aging volume change coefficient XTX, and the rubber-substrate bonding aging impact evaluation index XJP is negatively correlated with the aging friction coefficient LMX. In the rubber-substrate bonding process, the effect of rubber deformation on the bonding effect is greater than the effect of the friction coefficient change on the bonding effect.

[0080] Step 7: Compare the rubber-substrate bonding aging impact evaluation index with the bonding threshold, and output the bonding tightness level of the rubber and the substrate.

[0081] The bonding threshold is θ, and the value of θ is 52.5-6.4. The rubber-substrate bonding aging impact evaluation index is XJP. When XJP ≥ θ, it means that the bonding tightness level of the rubber and the substrate is level three, and the bonding tightness confidence of the rubber and the substrate is 0%, indicating that the bonding effect between the rubber and the substrate is very poor and needs to be replaced; when When , it means that the bonding tightness level between rubber and substrate is level 2, and the bonding tightness confidence between rubber and substrate is 70%, which means that the bonding effect between rubber and substrate is general and needs to be repaired; when When , it means that the bonding tightness level between the rubber and the substrate is level one, and the confidence level of the bonding tightness between the rubber and the substrate is 95%, indicating that the bonding effect between the rubber and the substrate is very good.

[0082] The bonding threshold is θ, and the rubber-substrate bonding aging impact evaluation index is XJP. When XJP ≥ θ, it means that the bonding tightness level of the rubber and the substrate is level three, and the bonding tightness confidence of the rubber and the substrate is 0%; when When , it means that the bonding tightness level between rubber and substrate is level 2, and the bonding tightness confidence level between rubber and substrate is 70%; when When , it means that the bonding tightness level between the rubber and the substrate is level one, and the confidence level of the bonding tightness between the rubber and the substrate is 95%.

[0083] Reference Figure 2-3 The present invention also discloses a bonding failure detection device between a rubber material and a substrate, including a mounting mechanism and a degumming test component. The mounting mechanism is a mounting frame for mounting the degumming test component, and the degumming test component is used to test the degumming stress of the rubber.

[0084] The mounting mechanism includes a bottom plate 11, a support column 12 and a top plate 13, wherein the support column 12 is fixedly connected to the bottom plate 11, and the top plate 13 is fixedly connected to the top of the support column 12;

[0085] The degumming test assembly includes an electric cylinder 21, a pressure sensor protection cover 22, a hardening block 23, a pressure sensor 24, a connecting plate 25 and a pressure head 26. The electric cylinder 21 is installed at the top center of the top plate 13. The bottom output shaft of the electric cylinder 21 is fixedly connected to the pressure sensor protection cover 22. The bottom of the pressure sensor protection cover 22 is fixedly connected to the hardening block 23. The pressure sensor 24 is arranged on the lower side of the hardening block 23. The pressure sensor 24 is installed on the top of the connecting plate 25. The pressure head 26 is installed at the bottom center of the connecting plate 25. A protective block 27 is installed on the outer side of the pressure sensor protection cover 22. The pressure sensor 24 is slidably connected to the inner wall of the protective block 27. The protective block 27 is used to protect the pressure sensor 24 as a whole and provide a detection displacement space for the pressure sensor 24. The electric cylinder 21 is used to push the pressure sensor protective cover 22, the hardening block 23, the pressure sensor 24, the connecting plate 25, and the pressure head 26 downward. After the pressure head 26 is subjected to force, the force is transmitted to the connecting plate 25, and then squeezes the pressure sensor 24 together with the hardening block 23 to test the rubber debonding force.

[0086] A slide rail 31 is fixedly connected between the bottom plate 11 and the top plate 13, a slider 32 is slidably connected to one side of the slide rail 31, a connecting block 33 is welded to one side of the slider 32, and the connecting block 33 is fixedly connected to the connecting plate 25. The slider 32 is used to guide the auxiliary connecting plate 25 to slide and move.

[0087] The above formulas are all dimensionless and numerical calculations. The formula is a formula for the most recent real situation obtained by collecting a large amount of data and performing software simulation. The preset parameters in the formula are set by technicians in this field according to actual conditions.

[0088] The above embodiments may be implemented in whole or in part by software, hardware, firmware or any other combination thereof. When implemented by software, the above embodiments may be implemented in whole or in part in the form of a computer program product. Those skilled in the art may appreciate that the units and algorithm steps of each example described in conjunction with the embodiments disclosed herein may be implemented by electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are performed by hardware or software methods depends on the specific application and design constraints of the technical solution.

[0089] The units described as separate components may or may not be physically separated, and the components shown as units may or may not be physical units, and may be located in one place or distributed on multiple network units. Some or all of the units may be selected according to actual needs to achieve the purpose of the solution of this embodiment.

[0090] The above description is only a specific implementation manner of the present application, but the protection scope of the present application is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in the present application, which should be included in the protection scope of the present application.

Claims

1. A bonding failure detection device between a rubber material and a substrate, comprising a mounting mechanism and a debonding test assembly, characterized in that: The mounting mechanism comprises a bottom plate (11), a support column (12) and a top plate (13), wherein the support column (12) is fixedly connected to the bottom plate (11), and the top plate (13) is fixedly connected to the top end of the support column (12); The debonding test assembly comprises an electric cylinder (21), a pressure sensor protective cover (22), a hardening block (23), a pressure sensor (24), a connecting plate (25) and a pressure head (26); the electric cylinder (21) is mounted at the top center of the top plate (13); the bottom output shaft of the electric cylinder (21) is fixedly connected to the pressure sensor protective cover (22); the bottom of the pressure sensor protective cover (22) is fixedly connected to the hardening block (23); the pressure sensor (24) is arranged on the lower side of the hardening block (23); the pressure sensor (24) is mounted on the top of the connecting plate (25); the pressure head (26) is mounted at the bottom center of the connecting plate (25); a protective block (27) is mounted on the outer side of the pressure sensor protective cover (22); and the pressure sensor (24) is slidably connected to the inner side wall of the protective block (27).

2. The device for detecting failure of bonding between a rubber material and a substrate according to claim 1, characterized in that: A slide rail (31) is fixedly connected between the bottom plate (11) and the top plate (13); a slider (32) is slidably connected to one side of the slide rail (31); a connecting block (33) is welded to one side of the slider (32); and the connecting block (33) is fixedly connected to the connecting plate (25).

3. A method for detecting failure of bonding between a rubber material and a substrate, characterized in that: The specific steps include: S1. Set aging test parameters, place n round rubbers in an aging box for aging test, and record the average friction coefficient, average radius, and average thickness of the round rubber surface every hour; S2, preprocessing the aging test parameters to generate an equivalent time expression; S3, performing correlation analysis on the average value of the circular rubber surface friction coefficient and the aging time, and generating an aging friction coefficient by the least square method, wherein the aging friction coefficient is used to reflect the surface friction coefficient of the circular rubber after aging over time; S4, pre-processing the average radius and average thickness of the circular rubber in the aging test to generate a volume coefficient, wherein the volume coefficient is used to reflect the volume value of the circular rubber that changes with time during the aging test; S5, pre-processing the volume coefficient and initial volume of the circular rubber after the aging test to generate a rubber aging volume change coefficient, wherein the rubber aging volume change coefficient is used to reflect the volume value change degree of the circular rubber as it ages over time; S6, pre-processing the rubber aging volume change coefficient and the aging friction coefficient to generate a rubber-substrate combination aging impact evaluation index, wherein the rubber-substrate combination aging impact evaluation index is used to reflect the degree of bonding between the rubber and the substrate; S7. Compare the rubber-substrate bonding aging impact evaluation index with the bonding threshold, and output the bonding tightness level of the rubber and the substrate.

4. The method for detecting failure of bonding between a rubber material and a substrate according to claim 3, characterized in that: In S1, n is not less than 10, the radius of the circular rubber is 10 cm, and the thickness is 5 cm. The aging test parameters include test temperature and aging time. The test temperature is 100 degrees Celsius, and the aging time is 100 hours.

5. The method for detecting failure of bonding between a rubber material and a substrate according to claim 4, characterized in that: In S2, according to the Arrhenius formula, it can be obtained that: Where t is the aging time, T is the test temperature, A is a constant term, E is the surface activation energy, R is the molar gas constant, the equivalent aging time of the round rubber at the equivalent temperature T1 is t1, and the aging time of the round rubber at the aging temperature T2 is t2. For the equivalent temperature T1, equivalent time t1, aging temperature T2, aging time t2 and equation: Perform correlation analysis and generate an expression for the equivalent time t1 as follows: Among them, the aging temperature T2 is 100 degrees Celsius, the equivalent temperature T1 is 20 degrees Celsius, and the equivalent time t1 can be output according to the aging time t2.

6. The method for detecting failure of bonding between a rubber material and a substrate according to claim 5, characterized in that: During the aging test, the aging time t2 is set to 1, 2, 3, ..., N hours, N is not less than 50, and the friction coefficient function is set as follows: Among them, μ is the friction coefficient of the rubber surface, a, b, c are constant terms, t2 is the aging time, and the values ​​of a, b, c are generated by least squares fitting based on the aging time-average circular rubber friction coefficient scatter plot per hour. The expression of equivalent time and the friction coefficient function are analyzed for correlation, and the equivalent time t1 expression is substituted into the friction coefficient function, and the time unit is converted to generate the aging friction coefficient LMX. The formula is as follows: Wherein, e is a natural constant, t is the service life of the rubber, i.e., the equivalent time, in years. The equivalent time is used to reflect the equivalent service life of the circular rubber after aging test at room temperature, where the room temperature is 20 degrees Celsius. α is the influencing factor of the friction coefficient of the circular rubber, and its value range is [0.1, 0.95].

7. The method for detecting failure of bonding between a rubber material and a substrate according to claim 5, characterized in that: During the aging test, the average radius at the jth hour is d j , the average thickness at the jth hour is s j , perform correlation analysis on the average radius and average thickness to generate the volume factor TX at the jth hour j , the formula based on is: TX j =π*d j 2 *s j Among them, π is the ratio of a circle to its circumference.

8. The method for detecting failure of bonding between a rubber material and a substrate according to claim 7, characterized in that: The correlation analysis of the radius and thickness of the circular rubber is performed to generate the initial volume V of the circular rubber, and the formula based on which is: V = 5*10 2 *π.

9. The method for detecting failure of bonding between a rubber material and a substrate according to claim 8, characterized in that: Expression for equivalent time, volume factor TX j The correlation analysis is performed with the initial volume V to generate the rubber aging volume change coefficient XTX, based on the formula: Wherein, t is the service life of rubber, in years, and β is the influencing factor of the friction coefficient of circular rubber, with a value range of [0.16, 1.98].

10. A method for detecting failure of bonding between a rubber material and a substrate according to any one of claims 3 to 9, characterized in that: The correlation analysis of the rubber aging volume change coefficient XTX and the aging friction coefficient LMX is performed to generate the rubber-substrate combined aging impact evaluation index XJP, based on the formula: The bonding threshold is θ, and the rubber-substrate bonding aging impact evaluation index is XJP. When XJP ≥ θ, it means that the bonding tightness level of the rubber and the substrate is level three, and the bonding tightness confidence of the rubber and the substrate is 0%; when When , it means that the bonding tightness level between rubber and substrate is level 2, and the bonding tightness confidence level between rubber and substrate is 70%; when When , it means that the bonding tightness level between the rubber and the substrate is level one, and the confidence level of the bonding tightness between the rubber and the substrate is 95%.