Manufacturing method of prism structure, exposure equipment and display panel
Through the digital exposure process, a high-precision prism structure is formed on the photocured glue layer, which solves the problems of low production accuracy of prism structure and mask plate alignment deviation in the prior art, and improves the effect of stereoscopic display.
Patent Information
- Application Number
- CN202410888460.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-03
- Publication Date
- 2024-11-29
AI Technical Summary
In the stereoscopic display technology, it is difficult for the prior art to effectively produce a high-precision prism structure, resulting in poor display effect, and the alignment deviation between the mask plate and the substrate affects the production accuracy.
The digital exposure process is used to perform preset exposure on the photocured glue layer to form a prism transition layer, and the interval distribution of prism parts are obtained by cleaning to avoid using a mask plate and improve position accuracy.
It realizes high-precision prism structure production, reduces production difficulty, avoids mask plate alignment deviation, and improves the display effect of the display panel.
Smart Images

Figure CN119045097A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of display technology, and in particular to a method for manufacturing a prism structure, an exposure device, and a display panel. Background Art
[0002] With the rapid development of stereoscopic display technology, there is an increasing demand for stereoscopic display devices. Among the many technologies for realizing three-dimensional stereoscopic display, naked-eye stereoscopic display is favored in the field of three-dimensional stereoscopic display because it does not require viewers to wear glasses. At present, the main way to realize naked-eye stereoscopic display technology is to set a grating in front of or behind the display panel, and divide the pixel units of the display panel into odd-numbered columns of pixels and even-numbered columns of pixels in the horizontal direction, so as to provide two different images for the left and right eyes of the viewer, respectively, and use the parallax effect of the viewer's left eye image and right eye image to form a depth of field, thereby producing a three-dimensional display effect. The grating includes two types: blocking type and spectroscopic type. The blocking type is divided into black and white parallax barrier grating and liquid crystal slit grating. The spectroscopic type is divided into cylindrical physical lens and switchable liquid crystal lens. There are three types of switchable liquid crystal lenses, including: switchable liquid crystal resin prism technology, switchable polarized liquid crystal lens technology, and switchable electrode liquid crystal lens. Among them, the liquid crystal resin prism technology is mature and has good display effect. It is the most widely used technical solution. In stereoscopic display products, how to make a prism structure is one of the topics that display product researchers are concerned about.
[0003] The above information disclosed in this section is only for understanding the background of the inventive concept of the present disclosure and therefore the above information may contain information that does not constitute the prior art. Summary of the invention
[0004] In one aspect, a method for manufacturing a prism structure is provided, comprising the following steps: forming a photocurable glue layer on a base substrate; imprinting a soft template on a side of the photocurable glue layer away from the base substrate; exposing a portion of the photocurable glue layer located in a preset exposure area using a digital exposure process, so that a portion of the photocurable glue layer located in an effective exposure area is cured to obtain a prism transition layer, wherein the preset exposure area includes a plurality of effective exposure areas distributed at intervals; peeling the soft template from the prism transition layer; and cleaning the prism transition layer to obtain a prism structure, wherein the prism structure includes a plurality of prism portions distributed at intervals.
[0005] According to some exemplary embodiments, the step of exposing a preset exposure area of a photocurable glue layer using a digital exposure process includes: modulating the propagation direction of the exposure light so that a portion of the exposure light is incident on a portion of the photocurable glue layer located in the effective exposure area, and another portion of the exposure light is incident on an area outside the photocurable glue layer.
[0006] According to some exemplary embodiments, the preset exposure area includes at least two exposure partitions, and exposing the portion of the photocurable glue layer located in the preset exposure area using a digital exposure process includes: sequentially exposing the portions of the photocurable glue layer located in each of the exposure partitions using a digital exposure process, so that the portions of the photocurable glue layer located in each of the exposure partitions and in the effective exposure area are cured in sequence.
[0007] According to some exemplary embodiments, the shape of the photocurable glue layer on the base substrate is approximately rectangular, two side edges of the photocurable glue layer extend along a first direction, and the other two side edges of the photocurable glue layer extend along a second direction, wherein the at least two exposure zones are arranged along the second direction.
[0008] According to some exemplary embodiments, at least one of the exposure partitions includes a first partition and a second partition, and the first partition and the second partition are arranged along the second direction; the first partition includes a plurality of first sub-partitions arranged at intervals along the first direction, and the second partition includes a plurality of second sub-partitions arranged at intervals along the first direction, the first sub-partition and the second sub-partition are both rectangular, and the plurality of first sub-partitions and the plurality of second sub-partitions are alternately arranged along the first direction; and in adjacent first sub-partitions and second sub-partitions, a side edge of the first sub-partition extending along the second direction is flush with a side edge of the second sub-partition extending along the second direction.
[0009] According to some exemplary embodiments, in the exposure partition, sides of the plurality of first sub-partitions close to the second partition are flush with sides of the plurality of second sub-partitions close to the first partition and are sequentially connected.
[0010] According to some exemplary embodiments, two adjacent exposure zones are connected complementarily.
[0011] According to some exemplary embodiments, the size of the first sub-partition along the first direction is 20-450 mm, and the size of the first sub-partition along the second direction is 20-450 mm; and / or the size of the second sub-partition along the first direction is 20-450 mm, and the size of the second sub-partition along the second direction is 20-450 mm.
[0012] According to some exemplary embodiments, the preset exposure area includes a first blank area located around the multiple effective exposure areas and a second blank area located between adjacent effective exposure areas, and the prism structure is formed in an area outside the first blank area and the second blank area.
[0013] On the other hand, an exposure device is provided, which is applied to any of the above-mentioned methods for manufacturing a prism structure, and the exposure device is used to perform the digital lithography process, and the exposure device includes: a light source for emitting exposure light; and a digital micromirror assembly, including a reflective mirror group, the reflective mirror group and the emitting direction of the exposure light form a preset angle, and the reflective mirror group is used to reflect a part of the exposure light to an effective exposure area, and reflect another part of the exposure light to an area outside the film layer to be exposed.
[0014] According to some exemplary embodiments, the digital micromirror assembly includes two rows of micromirror array units, each row of micromirror array units includes a plurality of micromirror array units arranged at intervals, and the plurality of micromirror array units in one row and the plurality of micromirror array units in another row are alternately arranged along the row direction.
[0015] According to some exemplary embodiments, the micromirror array unit includes a plurality of digital micromirror devices arranged in an array, the digital micromirror devices include a micromirror surface, the micromirror surface has a reset state and a deflection state, the micromirror surface in the deflection state is deflected by a preset angle compared to the micromirror surface in the reset state; and the micromirror surface in the reset state is used to reflect exposure light to an effective exposure area, and the micromirror surface in the deflection state is used to reflect exposure light to an area outside the film layer to be exposed.
[0016] According to some exemplary embodiments, an angle between the micro-reflection mirror surface in the reset state and the emission direction of the exposure light is 45°.
[0017] According to some exemplary embodiments, the exposure equipment also includes a light screening device, which is located on the light output side of the exposure light after being reflected by the micro-mirror surface, and the light screening device allows the exposure light reflected by the micro-mirror surface in the reset state to pass through, and absorbs the exposure light reflected by the micro-mirror surface in the deflection state.
[0018] On the other hand, a display panel is provided, which includes a display area and a peripheral area located around the display area, and the display panel includes: a first substrate; a second substrate, which is arranged opposite to the first substrate; a liquid crystal layer, which is arranged between the first substrate and the second substrate; and a frame glue layer, which is arranged between the first substrate and the second substrate, and the frame glue layer is arranged around the liquid crystal layer, and the frame glue layer is located in the peripheral area, wherein the second substrate includes a second base substrate and a prism portion arranged on a side of the second base substrate close to the liquid crystal layer, the prism portion covers the display area, and the prism portion and the frame glue layer are spaced apart.
[0019] According to some exemplary embodiments, the first substrate includes a first base substrate and a conductive layer located on a side of the first base substrate close to the liquid crystal layer; the second substrate also includes a second electrode layer located between the second base substrate and the prism portion; and the frame layer includes a frame glue body and conductive balls and first supporting balls doped in the frame glue body, the shape of the conductive balls is substantially the same as that of the first supporting balls, and the conductive balls are electrically connected to the first electrode layer and the conductive layer, respectively.
[0020] According to some exemplary embodiments, the liquid crystal layer includes liquid crystal molecules and second supporting balls, the size of the second supporting balls is smaller than the size of the first supporting balls, and the second supporting balls are in contact with the prism layer and the first substrate, respectively. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Other objects and advantages of the present disclosure will be apparent from the following description of the present disclosure with reference to the accompanying drawings, and will help to have a comprehensive understanding of the present disclosure.
[0022] Figure 1 The flowchart of the method for manufacturing a prism structure according to an embodiment of the present disclosure is schematically shown.
[0023] Figure 2A-2R The diagram schematically shows a process diagram of forming a prism structure according to some embodiments of the present disclosure.
[0024] Figure 3 The structure of an exposure device according to some embodiments of the present disclosure is schematically shown.
[0025] Figure 4 The structure of a digital micromirror device in an exposure device according to some embodiments of the present disclosure is schematically shown.
[0026] Figure 5 The structure of a micromirror array unit in an exposure device according to some embodiments of the present disclosure is schematically shown.
[0027] Figure 6 The structure of a micro-mirror in a reset state in an exposure device according to some embodiments of the present disclosure is schematically shown.
[0028] Figure 7 The structure of a micro-mirror in a deflected state in an exposure device according to some embodiments of the present disclosure is schematically shown.
[0029] Figures 8A-8B The diagram schematically shows a process of exposing a photocurable glue layer using the exposure equipment provided in an embodiment of the present disclosure.
[0030] Fig. 9The structure of an exposure device according to some embodiments of the present disclosure is schematically shown.
[0031] Fig.10 The planar structure diagram of a display panel according to some embodiments of the present disclosure is schematically shown.
[0032] Fig.11 Indicated along Fig.10 Cross-sectional view taken along the midline AA'.
[0033] It should be noted that, for the sake of clarity, in the drawings used to describe the embodiments of the present disclosure, the sizes of layers, structures or regions may be enlarged or reduced, that is, these drawings are not drawn according to the actual scale. DETAILED DESCRIPTION
[0034] In the following description, for the purpose of explanation, many specific details are set forth to provide a comprehensive understanding of various exemplary embodiments. However, it is apparent that various exemplary embodiments may be implemented without these specific details or with one or more equivalent arrangements. In other cases, well-known structures and devices are shown in block diagram form to avoid making various exemplary embodiments unnecessarily obscure. In addition, various exemplary embodiments may be different, but not necessarily exclusive. For example, the specific shape, configuration, and characteristics of an exemplary embodiment may be used or implemented in another exemplary embodiment without departing from the inventive concept.
[0035] In the accompanying drawings, the size and relative size of the elements may be exaggerated for the purpose of clarity and / or description. Thus, the size and relative size of the individual elements are not necessarily limited to the size and relative size shown in the drawings. When the exemplary embodiments may be implemented differently, the specific process sequence may be performed differently from the described sequence. For example, two processes described in succession may be performed substantially simultaneously or in an order opposite to the described sequence. In addition, the same reference numerals represent the same elements.
[0036] When an element is described as "on" another element, "connected to" another element or "coupled to" another element, the element may be directly on another element, directly connected to another element or directly coupled to another element, or there may be an intermediate element. However, when an element is described as "directly on" another element, "directly connected to" another element or "directly coupled to" another element, there is no intermediate element. Other terms and / or expressions used to describe the relationship between elements should be interpreted in a similar manner, for example, "between..." versus "directly between...", "adjacent" versus "directly adjacent" or "on..." versus "directly on...", etc. In addition, the term "connection" may refer to physical connection, electrical connection, communication connection and / or fluid connection. In addition, the X-axis, Y-axis and Z-axis are not limited to the three axes of the rectangular coordinate system, and can be interpreted in a broader sense. For example, the X-axis, Y-axis and Z-axis may be perpendicular to each other, or may represent different directions that are not perpendicular to each other. For the purpose of this disclosure, "at least one of X, Y, and Z" and "at least one selected from the group consisting of X, Y, and Z" may be interpreted as only X, only Y, only Z, or any combination of two or more of X, Y, and Z such as XYZ, XY, YZ, and XZ. As used herein, the term "and / or" includes any and all combinations of one or more of the listed associated items.
[0037] It should be understood that, although the terms first, second, etc. may be used herein to describe different elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. For example, without departing from the scope of the exemplary embodiment, a first element may be named a second element, and similarly, a second element may be named a first element.
[0038] Figure 1 The flowchart of the method for manufacturing a prism structure according to an embodiment of the present disclosure is schematically shown.
[0039] Reference Figure 1 The method for manufacturing the prism structure includes the following steps S10-S50.
[0040] In step S10, a light-curing glue layer is formed on the base substrate;
[0041] In step S20, the soft template is printed on a side of the photocurable glue layer away from the base substrate.
[0042] In step S30, a digital exposure process is used to expose the portion of the photocurable glue layer located in the preset exposure area, so that the portion of the photocurable glue layer located in the effective exposure area is cured to obtain a prism transition layer. The preset exposure area includes a plurality of effective exposure areas distributed at intervals.
[0043] In step S40, the soft template is peeled off from the prismatic transition layer.
[0044] In step S50, the prism transition layer is cleaned to obtain a prism structure, wherein the prism structure includes a plurality of prism portions distributed at intervals.
[0045] In the manufacturing method provided in the embodiment of the present disclosure, a digital exposure process is adopted, and the light-curing glue layer can be exposed without using a mask, so as to obtain a plurality of prism parts spaced apart on the substrate, and the difficulty of the manufacturing process is reduced. In addition, compared with the exposure process using a mask in the related art, the manufacturing method provided in the embodiment of the present disclosure does not need to use a mask, so it also avoids the problem of affecting the manufacturing accuracy due to the alignment deviation between the mask and the substrate, that is, the prism part manufactured by the manufacturing method provided in the embodiment of the present disclosure has a higher position accuracy.
[0046] It should be supplemented that the “position accuracy” mentioned in the embodiments of the present disclosure should be understood as the deviation distance between the actual position of the formed prism structure and the designed position.
[0047] Figure 2A-2R The diagram schematically shows a process diagram of forming a prism structure according to some embodiments of the present disclosure.
[0048] Reference Figure 2A , the surface of the base substrate 100 is cleaned and dried to ensure the cleanliness of the surface of the base substrate 100. The base substrate 100 may include a marking pattern for subsequent process alignment, for example, the marking pattern may be a "+" mark.
[0049] Reference Figure 2B and Figure 2C A tackifier layer 110 is formed on the surface of the base substrate 100 to increase the adhesion between the base substrate 100 and the subsequently formed prism structure 120. For example, the thickness of the tackifier layer 110 is 1-20 nanometers.
[0050] Reference Figure 2D , Figure 2E , Figure 2F and Figure 2G , the four corners of the base substrate 100 are optically aligned through the photosensitive device CCD, and then a photocurable glue layer 121 is formed on the side of the tackifier layer 110 away from the base substrate 100 .
[0051] For example, Figure 2G The plan view of the formed light-curing glue layer 121 is schematically shown, and the Figure 2F and Figure 2G The orthographic projection of the photocurable glue layer 121 on the base substrate 100 substantially covers the surface of the base substrate 100.
[0052] For example, the photocurable glue layer 121 may be formed by a full-surface coating process or a line coating process.
[0053] For example, the material of the light-curing glue layer 121 includes ultraviolet light-curing resin, and the refractive index of the ultraviolet light-curing resin may be 1.5-1.8. For another example, ultraviolet light-curing resin is a type of material that can be cured by ultraviolet laser, and different ultraviolet light-curing resins can be cured by ultraviolet lasers of different wavelength ranges, and the curing wavelength range may be 355nm to 425nm, and illustratively, the curing wavelength range is 365nm to 405nm.
[0054] Reference Figure 2H , providing a soft template 130, the soft template 130 having a specific microstructure, the microstructure of the soft template 130 being complementary to the prism structure 120 to be formed, fixing the soft template 130 above the imprinting device by a clamp or a roller, and accurately aligning the soft template 130 with the substrate 100 by a photosensitive device CCD.
[0055] Reference Fig.2I The roller is located on the side of the soft template 130 away from the base substrate 100 , and then the soft template 130 is pressed down so that the soft template 130 contacts the photocurable glue layer 121 , and the height is controlled to move slowly until the microstructure on the soft template 130 is completely imprinted on the photocurable glue layer 121 .
[0056] Reference Figure 2J , a digital exposure process is used to expose the portion of the photocurable glue layer 121 located in the preset exposure area, so that the portion of the photocurable glue layer 121 located in the effective exposure area is cured to obtain a prism transition layer.
[0057] Figure 2K The plan view of the preset exposure area is schematically shown, and the reference Figure 2J and Figure 2K The preset exposure area EA basically coincides with the area on the surface of the base substrate 100 close to the photocurable glue layer 121. The preset exposure area EA includes a plurality of effective exposure areas EEA distributed at intervals. The portion of the photocurable glue layer 121 located in each effective exposure area EEA is cured, and the portion of the photocurable glue layer 121 located outside the effective exposure area EEA is not cured.
[0058] Reference Figure 2M , peeling the soft template 130 from the prism transition layer 122 . Figure 2N The plan view of the prism transition layer is schematically shown. The prism transition layer 122 includes a plurality of prism portions 120 a distributed at intervals after solidification and an unsolidified glue layer 1221 to be removed located in an area other than the prism portions 120 a .
[0059] Reference Figure 2N , Fig.2O and Figure 2P , a cleaning process is performed on the prism transition layer 122 to remove the uncured glue layer 1221 to be removed, and dust and other particles are removed simultaneously, and then the multiple prism parts 120a retained on the base substrate 100 are baked to remove moisture, and the prism parts 120a obtained by light curing are further cured under heating conditions, so as to obtain the prism structure 120.
[0060] Figure 2Q The plan view of the prism structure is schematically shown, and the reference Figure 2K and Figure 2Q The prism structure 120 includes a plurality of prism portions 120 a distributed at intervals, and the plurality of prism portions 120 a are respectively formed in a plurality of effective exposure areas EEA.
[0061] According to some exemplary embodiments, after the prism structure 120 is manufactured, an optical inspection is performed on the prism structure 120. Figure 2R The prism structure 120 is measured at multiple points through a conjugate focus microscope to confirm that the prism parameters meet the design requirements. If there are any abnormalities, the problem points in the previous process are checked, and a new prism structure 120 is manufactured after adjustments and solutions are made.
[0062] According to some exemplary embodiments, referring to Figure 2K The step of exposing the preset exposure area EA of the photocurable glue layer 121 by using the digital exposure process includes: modulating the propagation direction of the exposure light so that a part of the exposure light is incident on the part of the photocurable glue layer 121 located in the effective exposure area EEA, and another part of the exposure light is incident on the area outside the photocurable glue layer 121, that is, by modulating the propagation direction of the exposure light, the area other than the effective exposure area EEA in the preset exposure area EA will not receive the exposure light, so that the part of the photocurable glue layer 121 located outside the effective exposure area EEA will not be cured.
[0063] According to some exemplary embodiments, referring to Figure 2K and Figure 2Q The preset exposure area EA includes a first blank area BA1 located around multiple effective exposure areas EEA and a second blank area BA2 located between adjacent effective exposure areas EEA. The prism structure 120 is formed in the area outside the first blank area BA1 and the second blank area BA2, that is, the first blank area BA1 and the second blank area BA2 will not form a prism structure 120.
[0064] For example, refer to Figure 2QThe base substrate 100 is a base substrate 100 used in the sixth generation (G6) production line. The size of the base substrate 100 along the first direction X is 1500 mm, and the size of the base substrate 100 along the second direction Y is 1850 mm. Twelve 27-inch prism portions 120a can be made on the base substrate 100. The 12 prism portions 120a are arranged in 3 rows × 4 columns. The size of the prism portion 120a along the first direction X is 348 mm, and the size of the prism portion 120a along the second direction Y is 608 mm. The spacing between adjacent prism portions 120a along the first direction X is 5 mm, and the spacing between adjacent prism portions 120a along the second direction Y is 5 mm, that is, the width of the second blank area BA2 is 5 mm. The width of the first blank area BA1 on both sides of the first direction X is 46.5 mm, and the width of the first blank area BA1 on both sides of the second direction Y is 8 mm.
[0065] In addition, refer to Figure 2K and Figure 2Q The first blank area BA1 and the second blank area BA2 where the prism structure 120 is not formed are used to form a plurality of frame glue structures, and the plurality of frame glue structures are respectively arranged around the plurality of prism portions 120a. After the base substrate 100 formed with the plurality of prism portions 120a is box-bonded with another substrate formed with a conductive layer, a plurality of display panels can be obtained by cutting, and each display panel includes a prism portion 120a in the prism structure 120.
[0066] For example, products of other sizes can be made on a substrate substrate of the size of a 6th generation production line. For example, 15.6-inch or 31.5-inch products can be made. According to the specific product size, the arrangement of the prism structure, the first blank area, and the second blank area and size are designed. For another example, it can also be made on a substrate substrate of other sizes. For example, the size of the substrate substrate can be 1100*1300mm (5th generation production line size) or 2200*2500mm (8.5th generation production line size), etc.
[0067] According to some exemplary embodiments, the width of the second blank area BA2 is 1-20 mm, for example, the width of the second blank area BA2 is 1-5 mm. The width of the first blank area BA1 is determined according to the size of the base substrate 100 and the product size, and the width of the first blank area BA1 can be 1-200 mm.
[0068] According to some exemplary embodiments, referring to Figure 2K and Figure 2LThe preset exposure area EA includes at least two exposure zones EAZ, and exposing the portion of the photocurable glue layer 121 located in the preset exposure area EA using a digital exposure process includes: sequentially exposing the portions of the photocurable glue layer 121 located in each exposure zone EAZ using a digital exposure process, so that the portions of the photocurable glue layer 121 located in each exposure zone EAZ and in the effective exposure area EEA are cured in sequence.
[0069] According to some exemplary embodiments, referring to Figure 2K and Figure 2L The shape of the photocurable glue layer 121 on the base substrate 100 is roughly rectangular, two side edges of the photocurable glue layer 121 extend along the first direction X, and the other two side edges of the photocurable glue layer 121 extend along the second direction Y, wherein at least two exposure zones EAZ are arranged along the second direction Y.
[0070] According to some exemplary embodiments, referring to Figure 2L , in the two exposure subareas EAZ located on both sides of the second direction Y, each exposure subarea EAZ includes a row of multiple third subareas EAZ3 spaced apart along the first direction X. In the other exposure subareas EAZ except the two exposure subareas EAZ located on both sides of the second direction Y, the exposure subareas EAZ include a first subarea EAZ1 and a second subarea EAZ2, and the first subarea EAZ1 and the second subarea EAZ2 are arranged along the second direction Y. The first subarea EAZ1 includes multiple first subareas EAZ11 spaced apart along the first direction X, and the second subarea EAZ2 includes multiple second subareas EAZ21 spaced apart along the first direction X. Both the first subarea EAZ11 and the second subarea EAZ21 are rectangular, and the multiple first subareas EAZ11 and the multiple second subareas EAZ21 are alternately arranged along the first direction X. In an adjacent first subarea EAZ11 and a second subarea EAZ21, a side edge of the first subarea EAZ11 extending along the second direction Y is flush with a side edge of the second subarea EAZ21 extending along the second direction Y.
[0071] In addition, Figure 2L In order to more clearly illustrate the range of each exposure partition, among two adjacent exposure partitions, one of the exposure partitions is filled with a "cross line" pattern, while the other exposure partition is not filled with a pattern.
[0072] According to some exemplary embodiments, referring to Figure 2L In other exposure zones EAZ except the two exposure zones EAZ located on both sides of the second direction Y, the sides of multiple first sub-zones EAZ11 close to the second zone EAZ2 are flush with the sides of multiple second sub-zones EAZ21 close to the first zone EAZ1 and are connected in sequence.
[0073] According to some exemplary embodiments, referring to Figure 2L , two adjacent exposure zones EAZ are complementarily connected, that is, multiple exposure zones EAZ are sequentially connected along the second direction Y to form a complete preset exposure area EA.
[0074] According to some exemplary embodiments, referring to Figure 2L , the size of the first sub-area EAZ11 along the first direction X is 20-450 mm, and the size of the first sub-area EAZ11 along the second direction Y is 20-450 mm. The size of the second sub-area EAZ21 along the first direction X is 20-450 mm, and the size of the second sub-area EAZ21 along the second direction Y is 20-450 mm. The size of the third sub-area EAZ3 along the first direction X is 20-450 mm, and the size of the third sub-area EAZ3 along the second direction Y is 20-450 mm.
[0075] On the other hand, an exposure device is provided. The exposure device is applied to any of the above-mentioned methods for manufacturing a prism structure, and the exposure device is used to perform a digital lithography process.
[0076] Figure 3 The structure of an exposure device according to some embodiments of the present disclosure is schematically shown.
[0077] Reference Figure 3 The exposure device includes: a light source 210 and a digital micromirror assembly 220. The light source 210 is used to emit exposure light; the digital micromirror assembly 220 includes a reflective mirror group MIR, which forms a preset angle with the emission direction of the exposure light. The reflective mirror group MIR can realize partition modulation of the exposure light, so that a part of the exposure light can be reflected to the effective exposure area of the film layer 300 to be exposed, and the remaining part of the exposure light can be reflected to the area outside the film layer 300 to be exposed.
[0078] For example, the light source 210 is an ultraviolet laser, and the light source 210 is used to emit ultraviolet light.
[0079] Figure 4 The structure of a digital micromirror device in an exposure device according to some embodiments of the present disclosure is schematically shown.
[0080] According to some exemplary embodiments, referring to Figure 4The digital micromirror assembly 220 includes two rows of micromirror array units 221, each row of micromirror array units 221 includes a plurality of micromirror array units 221 arranged at intervals, and the plurality of micromirror array units 221 in one row and the plurality of micromirror array units 221 in another row are alternately arranged along the row direction M. According to this arrangement, the exposure area of a micromirror array unit 221 in one row and the exposure area of an adjacent micromirror array unit 221 in another row can be continuous along the row direction M, so that the exposure areas of each micromirror array unit 221 in two rows are continuous along the row direction M.
[0081] Figure 5 The structure of a micromirror array unit in an exposure device according to some embodiments of the present disclosure is schematically shown.
[0082] Reference Figure 5 The micromirror array unit 221 includes a shell 2211 and a plurality of digital micromirror devices 2212 arranged in an array in the shell 2211. For example, the shape of the shell 2211 is roughly cylindrical, and a cylindrical cavity is provided in the shell 2211. The plurality of digital micromirror devices 2212 are arranged in a rectangular shape and embedded in the shell 2211. The shell 2211 has an opening, which exposes the plurality of digital micromirror devices 2212 arranged in the shell 2211, so that the digital micromirror devices 2212 can receive exposure light emitted by the light source 210.
[0083] According to some exemplary embodiments, in combination with reference Figure 4 and Figure 5 In a micromirror array unit 221 in one row and an adjacent micromirror array unit 221 in another row, a side edge of the multiple digital micromirror devices 2212 in one micromirror array unit 221 extending along the column direction N is substantially flush with a side edge of the multiple digital micromirror devices 2212 in another micromirror array unit 221 extending along the column direction N, so that the exposure area of a micromirror array unit 221 in one row and the exposure area of an adjacent micromirror array unit 221 in another row are continuous along the row direction M.
[0084] According to some exemplary embodiments, in combination with reference Figure 4 and Figure 5 In a micromirror array unit 221 in one row and an adjacent micromirror array unit 221 in another row, a side edge of the multiple digital micromirror devices 2212 in one micromirror array unit 221 extending along the row direction M is substantially flush with a side edge of the multiple digital micromirror devices 2212 in another micromirror array unit 221 extending along the row direction M.
[0085] According to some exemplary embodiments, referring to Figure 5The diameter of the housing 2211 in the micromirror array unit 221 is 50 mm-500 mm, the size of the multiple digital micromirror devices 2212 arranged in the array along the row direction M is 20-450 mm, the size of the multiple digital micromirror devices 2212 arranged in the array along the column direction N is 20-450 mm, and the size of the multiple digital micromirror devices 2212 along the row direction M and the size along the column direction N can be equal or unequal.
[0086] According to some exemplary embodiments, in combination with reference Figure 4 and Figure 5 The specific size and number of the micromirror array unit 221 can be set according to the size of the exposure area. For example, when applied to the 6th generation production line, the size of the area to be exposed is 1500*1850mm, and 20 micromirror array units 221 can be set. The 20 micromirror array units 221 are arranged in two rows, and one row includes 10 micromirror array units 221 arranged at intervals. The diameter of the housing 2211 in each micromirror array unit 221 is 106mm, and the size of the multiple digital micromirror devices 2212 arranged in the array along the row direction M is 75mm.
[0087] According to some exemplary embodiments, the main structure of the digital micro-mirror device is divided into four layers. The first layer is the micro-mirror surface MIR1, which is in a suspended state and is made of aluminum alloy. The material is relatively light and more convenient for deflection. The second layer is the torsion arm beam of the micro-mirror surface MIR1 and the addressing electrode of the micro-mirror surface MIR1. The third layer is a metal layer, including the addressing electrode of the torsion arm beam, the bias / reset electrode, and the landing platform of the micro-mirror surface MIR1 (limiting the deflection of the micro-mirror surface MIR1 by +12 degrees / -12 degrees or +10 degrees / -10 degrees). The fourth layer is a static memory (RAM), which can adopt a large-scale integrated circuit standard CMOS (complementary metal oxide semiconductor) process.
[0088] Figure 6 The structure of a micro-mirror in a reset state in an exposure device according to some embodiments of the present disclosure is schematically shown. Figure 7 The structure of a micro-mirror in a deflected state in an exposure device according to some embodiments of the present disclosure is schematically shown.
[0089] Combined with reference Figure 6 and Figure 7The digital micro-mirror device 2212 includes a micro-mirror surface MIR1, and the micro-mirror surface MIR1 has a reset state and a deflection state. Each micro-mirror surface MIR1 can be independently in a reset state or a deflection state. The micro-mirror surface MIR1 in the deflection state is deflected by a preset angle compared to the micro-mirror surface MIR1 in the reset state, for example, by 12 degrees. The micro-mirror surface MIR1 in the reset state is used to reflect the exposure light to the effective exposure area of the film layer 300 to be exposed, and the micro-mirror surface MIR1 in the deflection state is used to reflect the exposure light to the area outside the film layer 300 to be exposed.
[0090] According to some exemplary embodiments, the shape of the micro-reflection mirror surface MIR1 is square, and the size of the micro-reflection mirror surface MIR1 is 5-1000 microns. The smaller the size of the micro-reflection mirror surface MIR1, the higher the exposure accuracy can be achieved. For example, the size of the micro-reflection mirror surface MIR1 is 5-500 microns. Exemplarily, the size of the micro-reflection mirror surface MIR1 is 5 microns, and each micro-reflection mirror surface MIR1 can independently control the passage or blocking of light with a width of 5 microns.
[0091] The exposure device provided by the embodiment of the present disclosure can realize the digital exposure technology without mask. According to the pattern to be exposed, a digital layout is made in advance. When exposing, the control system in the exposure device will independently control each micro-mirror surface to be in a reset state or a deflection state according to the digital layout. The micro-mirrors corresponding to the areas that need light irradiation are in a reset state under the control of the control system, so that the exposure light can be reflected onto the film layer that needs to be exposed. The micro-mirrors corresponding to the areas that do not need light irradiation are in a deflection state under the control of the control system, so that the exposure light can be reflected outside the film layer that needs to be exposed. That is, the exposure device can realize the conversion of digital patterns into optical patterns, and can realize the exposure of specific patterns without the need for mask. By setting the size of the micro-mirrors, the exposure position accuracy of the exposure device can be 10-500um, for example, 10 to 200um.
[0092] According to some exemplary embodiments, the steps of exposing the aforementioned photocurable glue layer using the exposure device provided by the embodiments of the present disclosure may include the following:
[0093] Figures 8A-8B The diagram schematically shows a process of exposing a photocurable glue layer using the exposure equipment provided in an embodiment of the present disclosure.
[0094] Combined with reference Figure 2K and Fig. 8A, the digital micromirror assembly 220 is placed on the base substrate 100 formed with the photocurable glue layer 121, and the row direction of the digital micromirror assembly 220 is parallel to the first direction X, and the reflective mirror surface group of the digital micromirror assembly 220 faces the photocurable glue layer 121. The digital micromirror assembly 220 is moved along the second direction Y, so that the orthographic projection of each digital micromirror device 2212 in a row of micromirror array units 221 in the digital micromirror assembly 220 on the base substrate 100 covers the first exposure subarea EAZ located on one side of the second direction Y, that is, the orthographic projection of each digital micromirror device 2212 in a row of micromirror array units 221 on the base substrate 100 covers a row of multiple third subareas EAZ3 spaced apart along the first direction X, and the orthographic projection of each digital micromirror device 2212 in another row of micromirror array units 221 on the base substrate 100 is located outside the preset exposure area EA.
[0095] Combined with reference Figure 6 and Figure 7 The control system in the exposure device independently controls each micro-mirror surface MIR1 to be in a reset state or a deflection state according to the digital layout, that is, each micro-mirror surface MIR1 located in the effective exposure area EEA in the exposure zone EAZ is in a reset state, and each micro-mirror surface MIR1 located in the first blank area BA1 and the second blank area BA2 in the exposure zone EAZ is in a deflection state, and the light source 210 is turned on to realize the exposure of the first exposure zone EAZ.
[0096] Combined with reference Figure 2K and Figure 8B , move the digital micromirror assembly 220 along the second direction Y, so that the orthographic projection of each digital micromirror device 2212 in the digital micromirror assembly 220 on the substrate 100 covers the second exposure zone EAZ, that is, the orthographic projection of each digital micromirror device 2212 in a row of micromirror array units 221 on the substrate 100 covers each first sub-zone EAZ11 in the first zone EAZ1, and the orthographic projection of each digital micromirror device 2212 in another row of micromirror array units 221 on the substrate 100 covers each second sub-zone EAZ21 in the second zone EAZ2.
[0097] Combined with reference Figure 6 and Figure 7Similarly, the control system in the exposure equipment independently controls each micro-mirror surface MIR1 to be in a reset state or a deflection state according to the digital layout, that is, each micro-mirror surface MIR1 located in the effective exposure area EEA in the exposure zone EAZ is in a reset state, and each micro-mirror surface MIR1 located in the first blank area BA1 and the second blank area BA2 in the exposure zone EAZ is in a deflection state, and the light source 210 is turned on to realize the exposure of the second exposure zone EAZ.
[0098] Each exposure zone EAZ is exposed in sequence according to similar steps until the exposure of the entire preset exposure area is completed.
[0099] The exposure device adopts scanning mobile exposure to expose the photocurable glue layer 121 on the base substrate 100 to obtain a prism structure. The prism structure 120 includes a plurality of prism parts corresponding to a plurality of effective exposure areas EEA.
[0100] According to some exemplary embodiments, referring to Figure 5 In a micromirror array unit 221, the size of the multiple digital micromirror devices 2212 arranged in an array along the row direction M is 75 mm, the size of each digital micromirror device 2212 along the row direction M is 49 μm, and the spacing between two adjacent digital micromirror devices 2212 is 1 μm, that is, 1500 digital micromirror devices 2212 are arranged along the row direction M in a micromirror array unit 221, that is, 1500 columns of digital micromirror devices 2212 are included in a micromirror array unit 221.
[0101] Reference Figure 2K , Figure 4 and Figure 5 In order to form a first blank area BA1 ( Figure 2K The first blank area BA1 is marked with a in the figure. The width of the first blank area BA1 is 46.5 mm. The first micromirror array unit 221 ( Figure 4 The micro-mirror surfaces of the digital micro-mirror devices 2212 in the 1st to 930th columns in the micro-mirror array unit 221 (marked 1) are in a deflected state, so that the exposure light will not be projected to the first blank area BA1.
[0102] In order to form the first second blank area BA2 ( Figure 2K The width of the second blank area BA2 is 5 mm, and the size of the effective exposure area EEA along the first direction X is 348 mm. The sixth micromirror array unit 221 ( Figure 4The micro-mirror surfaces of the digital micro-mirror devices 2212 in the 391st to 490th columns in the micro-mirror array unit 221 (marked 6) are in a deflected state, so that the exposure light will not be projected to the second blank area BA2.
[0103] In order to form the second second blank area BA2 ( Figure 2K The second blank area BA2 marked with c in the figure), the width of the second blank area BA2 is 5 mm, then the tenth micromirror array unit 221 ( Figure 4 The micro-mirror surfaces of the digital micro-mirror devices 2212 in the 1451st to 150th columns of the micro-mirror array unit 221 (marked 10 in FIG. 10 ) are in a deflected state, and the eleventh micro-mirror array unit 221 ( Figure 4 The micro-mirror surfaces of the digital micro-mirror devices 2212 in the 1st to 50th columns in the micro-mirror array unit 221 (marked 11) are in a deflected state, so that the exposure light will not be projected to the second blank area BA2.
[0104] In order to form the first third blank area ( Figure 2K The width of the second blank area BA2 is 5 mm, and the size of the effective exposure area EEA along the first direction X is 348 mm. The fifteenth micromirror array unit 221 ( Figure 4 The micro-mirror surfaces of the digital micro-mirror devices 2212 in the 1011th to 1110th columns in the micro-mirror array unit 221 (marked 15) are in a deflected state, so that the exposure light will not be projected to the second blank area BA2.
[0105] In order to form a first blank area BA1 ( Figure 2K The width of the first blank area BA1 is 46.5 mm. The twentieth micromirror array unit 221 ( Figure 4 The micro-mirror surfaces of the digital micro-mirror devices 2212 in the 571st to 1500th columns in the micro-mirror array unit 221 (marked 20) are in a deflected state, so that the exposure light will not be projected to the first blank area BA1.
[0106] It is additionally noted that, only for the purpose of clearly explaining the above exposure process, Figure 4 In the figure, each micromirror array unit 221 is numbered, and the number does not indicate any other meaning.
[0107] According to some exemplary embodiments, referring to Figure 6The angle α between the micro-reflection mirror MIR1 in the reset state and the emission direction of the exposure light is 45°, and the angle β between the micro-reflection mirror MIR1 in the reset state and the surface of the film layer 300 to be exposed is 45°. Therefore, the exposure light reflected by the micro-reflection mirror MIR1 in the reset state can be vertically incident on the film layer 300 to be exposed.
[0108] Fig. 9 The structure of an exposure device according to some embodiments of the present disclosure is schematically shown.
[0109] According to some exemplary embodiments, referring to Fig. 9 The exposure device also includes a light screening device 230, which is located on the light output side of the exposure light after it is reflected by the micro-reflection mirror MIR1. The light screening device 230 allows the exposure light reflected by the micro-reflection mirror MIR1 in the reset state to pass through, and absorbs the exposure light reflected by the micro-reflection mirror MIR1 in the deflection state.
[0110] Fig.10 The planar structure diagram of a display panel according to some embodiments of the present disclosure is schematically shown. Fig.11 Indicated along Fig.10 Cross-sectional view taken along the midline AA'.
[0111] Combined with reference Fig.10 and Fig.11 The display panel includes a display area AA and a peripheral area NA located around the display area AA. The display panel includes a first substrate 500, a second substrate 600, a liquid crystal layer 700 and a sealant layer 400. The second substrate 600 is arranged opposite to the first substrate 500, the liquid crystal layer 700 is arranged between the first substrate 500 and the second substrate 600, the sealant layer 400 is arranged between the first substrate 500 and the second substrate 600, and the sealant layer 400 is arranged around the liquid crystal layer 700, and the sealant layer 400 is located in the peripheral area NA.
[0112] The first substrate 500 includes a first base substrate 510, a conductive layer 520 and a first electrode layer 530 located on the side of the first base substrate 510 close to the liquid crystal layer 700, and a flexible circuit board FPC is electrically connected to the side of the conductive layer 520 located in the peripheral area NA, and the flexible circuit board FPC is used to input a driving signal to the display panel. The second substrate 600 includes a second base substrate 610, a second electrode layer 620 located on the side of the second base substrate 610 close to the liquid crystal layer 700, and a prism portion 120a located on the side of the second electrode layer 620 close to the liquid crystal layer 700. In order to ensure that the prism portion 120a can completely cover the display area AA, the prism portion 120a is set slightly larger than the display area AA, and the prism portion 120a is spaced apart from the frame glue layer 400.
[0113] The conductive layer 520 includes a first conductive structure and a second conductive structure, the first conductive structure is electrically connected to the flexible circuit board and the first electrode layer 530, respectively, so as to connect the first voltage signal to the first electrode layer 530. The sealant layer 400 includes a sealant body 410 and a conductive ball 420 doped in the sealant body 410, the second conductive structure is electrically connected to the flexible circuit board, and is electrically connected to the second electrode layer 620 through the conductive ball 420 in the sealant layer 400, so as to connect the second voltage signal to the second electrode layer 620.
[0114] The display panel can be used in 2D reality scenes or 3D display scenes. When applied to 2D display scenes, the flexible circuit board does not input voltage signals, and the long axes of the liquid crystal molecules in the liquid crystal layer 700 are parallel to the first base substrate 510. At this time, the refractive index of the liquid crystal layer 700 is consistent with the refractive index of the prism portion 120a, and the light will not be refracted or split when passing through the interface between the prism portion 120a and the liquid crystal layer 700. When applied to a 2D display scenario, the flexible circuit board inputs a first voltage signal to the first electrode layer 530 and inputs a second voltage signal to the second electrode layer 620. For example, the first voltage signal is 0V, and the second voltage signal is -10 to -15V or 10 to 15V. An electric field is formed between the first electrode layer 530 and the second electrode layer 620, so that the liquid crystal molecules in the liquid crystal layer 700 are deflected, and the long axis of the liquid crystal molecules is perpendicular to the first base substrate 510. At this time, there is a difference between the refractive index of the liquid crystal layer 700 and the refractive index of the prism portion 120a. When the light passes through the interface between the prism portion 120a and the liquid crystal layer 700, it is refracted and split, forming a lens effect. The light is respectively transmitted to the left eye and the right eye of the viewer, and the display image with binocular parallax is combined to achieve a naked-eye 3D display effect.
[0115] In the display panel in the embodiment of the present disclosure, the prism portion 120a is manufactured by the manufacturing method provided in the above embodiment. Therefore, the prism portion 120a has a high position accuracy, which can effectively avoid the overlap of the prism portion 120a with the frame glue layer 400 due to the position offset, thereby causing the second voltage signal to be unable to be effectively transmitted to the second electrode portion through the conductive ball 420 in the frame glue layer 400.
[0116] According to some exemplary embodiments, referring to Fig.11 The frame layer also includes a first support ball 430 doped in the frame glue body 410. The shape of the conductive ball 420 is substantially the same as that of the first support ball 430. The conductive ball 420 and the first support ball 430 are mixed and doped in the frame glue body 410. The first support ball 430 plays a supporting role and is used to improve the uniformity of the gap thickness between the first substrate 500 and the second substrate 600.
[0117] According to some exemplary embodiments, referring to Fig.11 The liquid crystal layer 700 includes liquid crystal molecules and second support balls 710. The size of the second support balls 710 is smaller than that of the first support balls 430. The second support balls 710 are in contact with the prism layer and the first substrate 500 respectively. The second support balls 710 also play a supporting role. The second support balls 710 cooperate with the first support balls 430 to further improve the uniformity of the gap thickness between the first substrate 500 and the second substrate 600.
[0118] According to some exemplary embodiments, the material of the conductive balls 420 includes gold, the material of the first supporting balls 430 includes silicon, and the material of the second supporting balls 710 includes silicon.
[0119] It should be understood that the display device according to some exemplary embodiments of the present disclosure has all the features and advantages of the above-mentioned display substrate, and these features and advantages can be referred to the above description of the display substrate, which will not be repeated here.
[0120] As used herein, the terms "substantially," "approximately," "approximately," and other similar terms are used as terms of approximation rather than as terms of degree, and they are intended to account for the inherent deviations in measured or calculated values that would be recognized by one of ordinary skill in the art. Taking into account factors such as process fluctuations, measurement problems, and errors associated with the measurement of a particular quantity (i.e., limitations of the measurement system), "approximately" or "approximately" as used herein include the stated value and mean that the particular value is within an acceptable range of deviation as determined by one of ordinary skill in the art. For example, "approximately" can mean within one or more standard deviations, or within ±10% or ±5% of the stated value.
[0121] Although some embodiments according to the general inventive concept of the present disclosure have been illustrated and described, it will be appreciated by those skilled in the art that changes may be made to these embodiments without departing from the principles and spirit of the general inventive concept of the present disclosure, the scope of which is defined by the claims and their equivalents.
Claims
1. A method for manufacturing a prism structure, wherein: The production method comprises the following steps: forming a light-curing glue layer on the substrate; Imprinting a soft template on a side of the photocurable glue layer away from the substrate; The portion of the photocurable glue layer located in the preset exposure area is exposed by a digital exposure process, so that the portion of the photocurable glue layer located in the effective exposure area is cured to obtain a prism transition layer, wherein the preset exposure area includes a plurality of the effective exposure areas distributed at intervals; peeling the soft template from the prismatic transition layer; and The prism transition layer is cleaned to obtain a prism structure, wherein the prism structure includes a plurality of prism parts distributed at intervals.
2. The method for manufacturing a prism structure according to claim 1, wherein: The steps of exposing a preset exposure area of the photocurable glue layer using a digital exposure process include: The propagation direction of the exposure light is modulated so that a portion of the exposure light is incident on the portion of the photocurable glue layer located in the effective exposure area, and another portion of the exposure light is incident on an area outside the photocurable glue layer.
3. The method for manufacturing a prism structure according to claim 1 or 2, wherein: The preset exposure area includes at least two exposure subareas, and exposing the portion of the photocurable glue layer located in the preset exposure area using a digital exposure process includes: The portions of the photocurable glue layer located in each exposure zone are sequentially exposed using a digital exposure process, so that the portions of the photocurable glue layer located in each exposure zone and in the effective exposure area are sequentially cured.
4. The method for manufacturing a prism structure according to claim 3, wherein: The shape of the photocurable glue layer on the base substrate is roughly rectangular, two side edges of the photocurable glue layer extend along a first direction, and the other two side edges of the photocurable glue layer extend along a second direction, wherein the at least two exposure partitions are arranged along the second direction.
5. The method for manufacturing a prism structure according to claim 4, wherein: At least one of the exposure subareas includes a first subarea and a second subarea, and the first subarea and the second subarea are arranged along the second direction; The first partition includes a plurality of first sub-partitions arranged at intervals along the first direction, the second partition includes a plurality of second sub-partitions arranged at intervals along the first direction, the first sub-partitions and the second sub-partitions are both rectangular, and the plurality of first sub-partitions and the plurality of second sub-partitions are alternately arranged along the first direction; and In an adjacent first sub-region and an adjacent second sub-region, a side edge of the first sub-region extending along the second direction is flush with a side edge of the second sub-region extending along the second direction.
6. The method for manufacturing a prism structure according to claim 5, wherein: In the exposure partition, sides of the plurality of first sub-partitions close to the second partition are flush with sides of the plurality of second sub-partitions close to the first partition and are sequentially connected.
7. The method for manufacturing a prism structure according to claim 6, wherein: Two adjacent exposure partitions are connected in a complementary manner.
8. The method for manufacturing a prism structure according to any one of claims 5 to 7, wherein: The size of the first sub-partition along the first direction is 20-450 mm, and the size of the first sub-partition along the second direction is 20-450 mm; and / or A size of the second sub-partition along the first direction is 20-450 mm, and a size of the second sub-partition along the second direction is 20-450 mm.
9. The method for manufacturing a prism structure according to any one of claims 1 to 8, wherein: The preset exposure area includes a first blank area located around the multiple effective exposure areas and a second blank area located between adjacent effective exposure areas, and the prism structure is formed in an area outside the first blank area and the second blank area.
10. An exposure device, wherein: The exposure device is applied to the method for manufacturing a prism structure according to any one of claims 1 to 9, and the exposure device is used to perform the digital lithography process, and the exposure device includes: a light source for emitting exposure light; and The digital micromirror assembly comprises a reflective mirror group, wherein the reflective mirror group forms a preset angle with the emitting direction of the exposure light, and the reflective mirror group is used to reflect a part of the exposure light to an effective exposure area, and reflect another part of the exposure light to an area outside the film layer to be exposed.
11. The exposure apparatus according to claim 10, wherein The digital micromirror assembly includes two rows of micromirror array units, each row of micromirror array units includes a plurality of micromirror array units arranged at intervals, and the plurality of micromirror array units in one row and the plurality of micromirror array units in another row are alternately arranged along the row direction.
12. The exposure apparatus according to claim 11, wherein The micromirror array unit includes a plurality of digital micromirror devices arranged in an array, wherein the digital micromirror device includes a micromirror surface, wherein the micromirror surface has a reset state and a deflection state, and the micromirror surface in the deflection state is deflected by a preset angle compared to the micromirror surface in the reset state; as well as The micro-reflection mirror surface in the reset state is used to reflect the exposure light to the effective exposure area, and the micro-reflection mirror surface in the deflection state is used to reflect the exposure light to the area outside the film layer to be exposed.
13. The exposure apparatus according to claim 12, wherein: The angle between the micro-reflection mirror surface in the reset state and the emitting direction of the exposure light is 45°.
14. The exposure apparatus according to claim 12 or 13, wherein: The exposure equipment also includes a light screening device, which is located on the light output side of the exposure light after it is reflected by the micro-reflection mirror. The light screening device allows the exposure light reflected by the micro-reflection mirror in the reset state to pass through, and absorbs the exposure light reflected by the micro-reflection mirror in the deflection state.
15. A display panel, wherein: The display panel includes a display area and a peripheral area located around the display area, and the display panel includes: a first substrate; a second substrate, arranged opposite to the first substrate; a liquid crystal layer disposed between the first substrate and the second substrate; and A sealant layer is disposed between the first substrate and the second substrate. The sealant layer surrounds the liquid crystal layer and is located in the peripheral area. The second substrate includes a second base substrate and a prism portion disposed on a side of the second base substrate close to the liquid crystal layer, the prism portion covers the display area, and the prism portion is spaced apart from the frame glue layer.
16. The display panel according to claim 15, wherein: The first substrate comprises a first base substrate and a conductive layer located on a side of the first base substrate close to the liquid crystal layer; The second substrate further includes a second electrode layer located between the second base substrate and the prism portion; and The frame layer includes a sealant body, conductive balls and first supporting balls doped in the sealant body. The shape of the conductive balls is substantially the same as that of the first supporting balls. The conductive balls are electrically connected to the first electrode layer and the conductive layer, respectively.
17. The display panel according to claim 16, wherein: The liquid crystal layer includes liquid crystal molecules and second supporting balls. The size of the second supporting balls is smaller than that of the first supporting balls. The second supporting balls are in contact with the prism layer and the first substrate respectively.