Microanalysis chip
By designing the stacked porous substrate structure and capillary phenomenon in the micro-analysis chip, increasing the contact area between the sample and the ion selective film, the measurement accuracy and stability problems in the prior art are solved, and efficient electrolyte concentration measurement is achieved.
Patent Information
- Application Number
- CN202380035403.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-23
- Filing Date
- 2023-04-10
- Publication Date
- 2024-11-29
AI Technical Summary
In the electrolyte concentration measurement, existing micro-analytical chips have problems such as low measurement accuracy, poor ion selectivity and poor potential stability, which are mainly due to insufficient or unstable contact area between the sample and the ion selective film.
A micro-analytical chip composed of a laminated porous substrate is designed, by forming a first flow passage chamber and a second flow passage chamber in the first porous substrate, and a reference electrode and a working electrode are provided therein. The substrate overlaps the surface of the first porous substrate to increase the contact area, increase the sample flow using capillary phenomena, and reduce interference by the restriction member.
The high sensitivity, ion selectivity and time stability of the electrolyte concentration measurement are achieved, and the measurement accuracy and efficiency of the micro-analysis chip are improved.
Smart Images

Figure CN119053852A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a micro-analysis chip with a micro-flow path formed in a porous substrate. Background Art
[0002] In recent years, microanalysis chips that allow analysis in biochemistry to be efficiently performed in a single chip by using microscopic flow paths having microscopic dimensions have become the focus of attention in a wide range of fields. Specifically, microanalysis chips have become the focus of attention not only in biochemical research but also in the fields of medicine, innovative drug development, health care, environment, food, and the like.
[0003] In the first half of the 1990s, a microanalysis chip was developed in which a micro-channel with a micrometer size was formed on glass or silicon by photolithography using a metal mold, etc., and sample pretreatment, stirring, mixing, reaction, and detection were performed on a single chip. As a result, miniaturization of the inspection system, rapid analysis, reduction of samples and waste liquid, etc. were achieved.
[0004] Electrochemical analysis measures the potential between electrodes immersed in a sample to be analyzed and is widely used in the fields of medicine, environment, etc. Existing electrochemical analysis is performed by engineers on advanced instruments, so the field and resources of measurement are limited to a certain extent. However, for the purpose of use in developing countries with insufficient medical equipment, medical care in remote areas or disaster sites, and at airports where the spread of infectious diseases needs to be checked near water, etc., low-cost, easy-to-handle and disposable micro-analysis chips for electrochemical analysis are needed.
[0005] Non-patent document 1 proposes a filter paper-based device for measuring Na ion concentration and K ion concentration. The device is formed on a filter paper sheet and has a distribution portion for distributing a sample. The sample after distribution penetrates from the distribution portion into the region of the working electrode and the reference electrode to electrically connect the two electrodes, and as a result, a potential difference can be measured. In the device, KCl ion crystals are deposited on the reference electrode to obtain a stable potential at the reference electrode, and the KCl ion crystals are dissolved in the sample during measurement to maintain the Cl ions in the reference electrode region at a high concentration, and as a result, a stable potential of the reference electrode is obtained. In addition, the ions to be measured are selected only by the K ion selective membrane formed to cover the working electrode, thereby making it possible to perform measurement without being affected by other ions.
[0006] Patent document 1 proposes a micro-analysis chip for electrochemical analysis. The device has a two-layer structure. A distribution part for distributing a sample is provided at the upper layer. The distributed sample substantially penetrates through the thickness of the porous hydrophilic layer and penetrates into the upper surface of the electrode assembly on the lower substrate. Then, a plurality of electrodes are electrically connected, and electrochemical measurement is possible.
[0007] Prior art literature
[0008] Patent Literature
[0009] Patent Document 1: U.S. Patent Application Publication No. 2012 / 0181184
[0010] Non-patent literature
[0011] Non-patent document 1: Nipapan Ruecha, Orawon Chailapakul, Koji Suzuki, and Daniel Chitterio, "Potential ion sensing device based entirely on inkjet printing paper", Analytical Chemistry, 89, pp. 10608-10616, published on August 29, 2017 Summary of the invention
[0012] Problem that the invention aims to solve
[0013] However, in the case of the above configuration, an undesirable influence may be exerted on the measurement accuracy of the sample concentration. Specifically, an undesirable influence may be exerted on the measurement sensitivity of the electrolyte concentration, the ion selectivity of specific ions, the potential stability during measurement, etc. The above reason is that the contact area between the sample and the ion selective membrane is insufficient or the contact is unstable.
[0014] In the case of the configuration described in Non-Patent Document 1, in order to obtain high measurement accuracy, it is necessary to accurately control the formation conditions of the ion selective membrane. Specifically, the ion selective membrane needs to penetrate into the air gap of the porous substrate so that the contact area between the porous substrate and the ion selective membrane in the porous substrate increases. However, Non-Patent Document 1 does not describe the details of the method for controlling penetration. When the area of the ion selective membrane is increased to increase the area of the boundary surface between the ion selective membrane and the porous substrate, the flow path device is enlarged.
[0015] In the case of the configuration described in Patent Document 1, the porous hydrophilic layer is in contact with the upper surface of the electrode assembly to supply the sample. However, a flow path through which the sample can permeate is not provided in the substrate supporting the electrode assembly, so the sample flow rate caused by the capillary phenomenon is small, and the time period from dispensing to the end of measurement is sometimes extended. The sample contact sometimes becomes unstable on the side of the electrode assembly without a flow path, so the measurement potential may be undesirably affected.
[0016] The present disclosure has been made in view of the above inconveniences, and an object of the present disclosure is to provide a micro-analysis chip capable of quickly obtaining electrolyte concentration with high measurement sensitivity, ion selectivity, and potential stability.
[0017] Solutions for solving problems
[0018] In order to achieve the above-mentioned purpose, one aspect of the present disclosure provides a micro-analysis chip, which is composed of a first porous substrate and a second porous substrate stacked on each other, wherein a first flow path chamber, a second flow path chamber, and a first flow path connecting the first flow path chamber and the second flow path chamber are formed by a flow path wall in the first porous substrate, a reference electrode is arranged in the first flow path chamber, a working electrode is arranged in the second flow path chamber, and the second porous substrate is arranged to overlap with at least a portion of an area on the surface of the first porous substrate where the working electrode is formed.
[0019] Effects of the Invention
[0020] According to one aspect of the present disclosure, a micro-analysis chip excellent in measurement sensitivity of electrolyte concentration, ion selectivity, and temporal stability of potential can be provided. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 : is a schematic cross-sectional view showing the configuration of a micro-analysis chip P1 according to Embodiment 1.
[0022] Figure 2 Schematically shows the relative positional relationship and size relationship among the flow path chamber 1, flow path chamber 2, flow path 3, flow path wall 5, distribution portion 6, reference electrode 7, working electrode 8, ion selective membrane 9 and ion crystal 10 of the micro-analysis chip P1 according to Example 1.
[0023] Figure 3 is a schematic cross-sectional view showing the configuration of a micro-analysis chip P2 according to Comparative Example 1.
[0024] Figure 4A is an example of measurement results according to Example 1 and Comparative Example 1.
[0025] Figure 4B is an example of measurement results according to Example 1 and Comparative Example 1.
[0026] Figure 5A is an example of measurement results according to Example 1 and Comparative Example 1.
[0027] Figure 5B is an example of measurement results according to Example 1 and Comparative Example 1.
[0028] Figure 6 : is a schematic cross-sectional view showing the filtering effect of Example 1.
[0029] Figure 7 : is a schematic cross-sectional view showing the filtering effect of Comparative Example 1.
[0030] Figure 8is a schematic cross-sectional view showing the configuration of a micro-analysis chip P3 according to Comparative Example 2.
[0031] Fig. 9 is a conceptual diagram showing the temporal changes in the behavior of the samples after dispensing according to Example 1 and Comparative Example 1.
[0032] Fig.10 : is a schematic cross-sectional view showing the configuration of a micro-analysis chip P2 according to Modification 1 of Embodiment 1. DETAILED DESCRIPTION
[0033] In the specification, unless otherwise specified, the phrase "greater than or equal to XX and less than or equal to YY" or the phrase "XX to YY" indicating a numerical range means a numerical range including the lower limit and the upper limit as endpoints. In the case where numerical values are described in a stepwise manner, a selected combination of the upper limit and the lower limit of each numerical range is described.
[0034] A micro-analysis chip according to the present invention for solving the above-mentioned inconvenience will be described with reference to the following embodiments. The embodiments described below are illustrative and are not intended to limit the technical scope of the present invention to only those embodiments.
[0035] Figure 1 Schematically shows the Figure 2 A cross-sectional view of the micro-analysis chip P1 taken along line AA in FIG.
[0036] Figure 2 Schematically shows the relative positional relationship and size relationship among the flow path chamber 1, flow path chamber 2, flow path 3, flow path wall 5, distribution portion 6, reference electrode 7, working electrode 8, ion selective membrane 9 and ion crystal 10 of the micro-analysis chip P1 according to Example 1.
[0037] The micro-analysis chip P1 is composed of a porous substrate S1 and a porous substrate S2. The porous substrate S1 and the porous substrate S2 are stacked in the thickness direction.
[0038] The porous substrate S1 has a first flow path region surrounded by a flow path wall 5. The flow path pattern in the porous substrate S1 is composed of a flow path chamber 1 (first flow path chamber), a flow path chamber 2 (second flow path chamber), and a flow path 3. The flow path 3 (first flow path) connects the flow path chamber 1 (first flow path chamber) and the flow path chamber 2 (second flow path chamber).
[0039] The reference electrode 7 is arranged in the flow path chamber 1. An ion crystal 10 having sample solubility is arranged on the surface of the reference electrode 7.
[0040] The working electrode 8 is arranged in the flow path chamber 2 .
[0041] The porous substrate S2 includes a distributing portion 6 for distributing a sample and a flow path 4 (second flow path) connecting the distributing portion 6 and a region in which the working electrode 8 is formed.
[0042] The flow channel 4 is provided on the surface of the porous substrate S1 so as to overlap at least a part of the region where the working electrode 8 is formed.
[0043] The position connecting at least the dispensing portion 6 and the working electrode 8 on the upper surface of the porous substrate S2 is preferably covered with a limiting member 11 into which the sample does not penetrate. This is because, for example, in the case where filtering of interfering particles (described later) is advantageous or the influence of the outside air can be reduced by reducing the exposure area of the sample to the outside air, the measurement potential easily becomes stable.
[0044] Both the lower surface of the porous substrate S1 and the upper surface of the porous substrate S2 are preferably covered with a restricting member 11 .
[0045] <Porous Substrate>
[0046] In the following examples, a paper material is used as a porous substrate; however, the material of the porous substrate is not limited to a paper material. The porous substrate may be made of any material that causes liquid capillary phenomenon, and may be a porous material of a grid-like structure, such as open-cell bubbles and nanofibers inside, or may be made of resin, glass, inorganic board, cloth, metal paper, etc. For example, a porous substrate having a large thickness or a high porosity is suitable for rapid measurement because the sample flow rate is high due to the capillary phenomenon.
[0047] In the following embodiments, the porous substrate S1 and the porous substrate S2 are each made of the same paper substrate one by one; however, the combination is not limited thereto. A flow path region equivalent to the flow path region of the present embodiment can be formed by folding a single porous substrate S1. The porous substrate S1 and the porous substrate S2 can be made of different materials. Depending on the combination of materials, effects of flow control of a sample, filtration of a sample, etc. can be imparted to the device.
[0048] <Flow path wall>
[0049] In the following embodiments, a hydrophobic resin is arranged and then a flow path pattern (flow path wall) is formed by heat fixing; however, the method of forming the flow path pattern is not limited thereto. The method of forming the flow path pattern only needs to form the flow path pattern. In addition to the method of cutting the paper porous substrate to leave only the flow path shape, the method can form the flow path wall using a wax printer.
[0050] <Restriction component>
[0051] The confinement member need only be made of a material that is impermeable to the sample.
[0052] Specifically, the restricting member may be a laminated film made of polyethylene terephthalate (PET).
[0053] The reference electrode 7 is arranged in the flow path chamber 1 (first flow path chamber). The upper surface and side surface of the reference electrode 7 are covered with ion crystals 10. The reference electrode 7 has a lead extending continuously from the inside of the flow path chamber 1 to above the flow path wall 5 as an electrode contact point during measurement.
[0054] The working electrode 8 is arranged in the flow path chamber 2 (second flow path chamber). The upper surface and side surface of the working electrode 8 are covered with an ion selective membrane 9, which includes a component having ion selectivity. The working electrode 8 has a lead extending continuously from the inside of the flow path chamber 2 to above the flow path wall 5.
[0055] In the following embodiments, the flow path chamber (first flow path chamber) for the reference electrode 7 and the flow path chamber (second flow path chamber) for the working electrode 8 are both one; however, the number of flow path chambers is not limited thereto. When the number of types of ions whose concentrations are to be measured is plural, working electrodes and flow path chambers may be increased according to the number of ion types.
[0056] The porous substrate S2 includes a distribution portion 6 and a flow path 4. The distribution portion 6 is arranged in a manner overlapping the flow path 3 of the porous substrate S1. The flow path 4 is arranged in a manner overlapping the flow path 3 and the ion selective membrane 9. The flow path 4 of the porous substrate S2 does not necessarily need to cover the entire upper surface of the working electrode 8. For example, in a working electrode having good wettability to a sample, when the flow path 4 covers a portion of the upper surface of the working electrode, an advantageous effect similar to that of the present embodiment is obtained.
[0057] [Example 1]
[0058] <Flow path structure>
[0059] In Example 1, a porous substrate S1 and a porous substrate S2 made of paper having a length L1 = 0.1 mm and a porosity of 50% were used.
[0060] The void ratio (%) was calculated by using the following formula.
[0061] Void ratio (%) = ((true density) - (apparent density)) / (true density) × 100
[0062] The apparent density (g / cm) was calculated by using the following formula 3 ).
[0063] (Apparent density)(g) / cm 3 )=(basis weight)(g / m 2 ) / Thickness(mm)×1000
[0064] After the hydrophobic resin is arranged on the surface of the porous substrate S1, a flow path pattern serving as a flow path wall 5 that is impermeable to the sample is formed by thermal fixing. The porous substrate S2 is arranged in such a manner as to overlap the flow path 3 and the ion selective membrane 9. The porous substrate S1 and the porous substrate S2 are covered with a limiting member that the sample does not penetrate. In this embodiment, a laminated film made of polyethylene terephthalate (PET) is used as the limiting member.
[0065] The dimensions of the flow path chamber 1 , the flow path chamber 2 , and the distribution portion 6 are as follows.
[0066] Flow path chamber 1: L11=6mm, L12=6mm
[0067] Flow path chamber 2: L21=6mm, L22=6mm
[0068] Distribution part 6: a circle with a diameter of 3 mm
[0069] The shortest distance L41 from the center of the distribution portion 6 to the ionic crystal 10: 7 mm
[0070] The shortest distance L42 from the center of the distribution portion 6 to the ion selective membrane 9: 6.5 mm
[0071] Width of channel 3 L31: 3 mm, width of channel 4 L43: 3 mm
[0072] <Sample>
[0073] The sample is an aqueous solution containing NaCl as the ion to be measured and KCl as the coexisting ion.
[0074] <Electrode formulation>
[0075] The formulation of the electrode according to Example 1 will be described.
[0076] A reference electrode 7 made of Ag / AgCl was provided in the flow path chamber 1 . 3.5 mg of KCl ion crystals were arranged on the reference electrode 7 as the ion crystals 10 .
[0077] The dimensions of the reference electrode 7 are as follows: Reference electrode 7: L71 = 4 mm, L72 = 4 mm.
[0078] On the other hand, a working electrode 8 mainly made of carbon as a main component is provided in the flow path chamber 2. Instead of the carbon electrode, a working electrode 8 made of a conductive polymer such as PEDOT:PSS (dispersion of polyethylene dioxythiophene and polystyrene sulfonate) may be used. A material such as Ag / AgCl used for the base of the reference electrode in the prior art may be used.
[0079] The dimensions of the working electrode 8 are as follows: Working electrode 8: L81 = 5.5 mm, L82 = 5.5 mm.
[0080] The Na ion selective membrane 9 is formed so as to cover the working electrode 8. The ion selective membrane 9 is formed of the following materials.
[0081] Ion selective material: Bis (12-crown-4) 3.0 mass%
[0082] Anion remover: Potassium tetrakis (tetrachlorophenyl) potassium borate 0.5 mass%
[0083] o-Nitrophenyl octyl ether 64.0 mass%
[0084] Polyvinyl chloride 32.5 mass%
[0085] In this embodiment, the reference electrode 7 , the working electrode 8 , and the ion selective membrane 9 are formed to have the shapes, sizes, materials, etc. as described above; however, the configuration is not limited thereto.
[0086] <Ionic Crystals>
[0087] The ionic crystal 10 is formed so as to cover the reference electrode 7 .
[0088] In this embodiment, KCl ion crystal is used as ion crystal 10. However, the material of ion crystal 10 only needs to include Cl ions and is not limited to KCl ion crystal. The mass of ion crystal 10 to be arranged falls within the mass range of KCl ion crystal that obtains a saturated solution when KCl ion crystal is dissolved in pure water of a volume equivalent to the solution in flow path chamber 1, but is not limited thereto.
[0089] In this embodiment, the ion selective membrane 9 is provided; however, in the case of measuring the total amount of ions in a sample, for example, the ion selective membrane 9 does not necessarily need to be provided.
[0090] <Permeation of Sample>
[0091] The penetration of the samples will be described.
[0092] The sample is dispensed on the porous substrate S2 by the dispensing section 6 and then permeates through the paper porous substrates S1 , S2 according to the flow path pattern simultaneously in both directions toward the flow path chamber 1 and toward the flow path chamber 2 due to the capillary phenomenon.
[0093] When the dispensed sample permeates into the flow path chamber 1 , ions included in the sample are selected by the ion selective membrane 9 in the flow path chamber 2 , and the measurement potential of the working electrode 8 required for measuring the electrolyte concentration becomes stable.
[0094] In the present embodiment, the position of the distribution portion 6 is the midpoint where the distance from the flow path chamber 1 is substantially equal to the distance from the flow path chamber 2; however, the position of the distribution portion 6 is not limited thereto. Depending on the position of the distribution portion relative to the ion selective membrane or the material of the porous substrate, the sensitivity, selectivity, etc. can be improved by imparting a filtering function to the device for a sample including fine particles of about several microns in the sample.
[0095] <Measurement of sample concentration>
[0096] The measurement of sample concentration will be described.
[0097] Once the sample permeates and reaches the ion crystal 10 covering the reference electrode 7, the KCl ion crystal dissolves in the sample, and the concentration of Cl ions in the solution in the flow path chamber 1 is saturated. At this time, when the measurement potential of the working electrode 8 is stable, the concentration of the sample can be measured, and the measurement of the sample concentration ends after a predetermined measurement time has passed. When the volume of the sample dispensed is greater than or equal to the volume of the sample that can reach the flow path chamber 1 and the flow path chamber 2 via the flow path 3 of the porous substrate S2, the sample concentration between the working electrode 8 and the reference electrode 7 can be measured with high accuracy by bringing a sufficient amount of the sample into contact with the ion selective membrane 9.
[0098] [Comparative Example 1]
[0099] In order to explain the advantageous effects of Example 1 in more detail, reference will be made to Figure 3 Comparative Example 1 will be described.
[0100] <Flow path structure>
[0101] The micro-analysis chip P2 includes the porous substrate S1, but does not include the porous substrate S2. In the micro-analysis chip P2, the shapes of the porous substrate S1 and the flow path wall are the same as those of Example 1. The configuration (shape and size) of each of the distributing portion 6, the reference electrode 7, the working electrode 8, the ion selective membrane 9, the ion crystal 10, etc. is also the same as that of Example 1. However, the distributing portion 6 is formed in the porous substrate S1. As described above, the porous substrate S2 is not used.
[0102] <Permeation of Sample>
[0103] The distributed sample starts to permeate from the distribution portion 6 in both directions, that is, the direction toward the flow path chamber 1 and the direction toward the flow path chamber 2 , and reaches the flow path chamber 1 and the flow path chamber 2 at the same time.
[0104] As in the case of Embodiment 1, the sample having reached the flow path chamber 1 dissolves the ion crystals 10 covering the reference electrode 7 and forms a Cl ion solution having a saturated concentration.
[0105] On the other hand, the sample that has reached the flow path chamber 2 is in contact with the ion selective membrane 9, but the portion where the sample is mainly in contact is at the boundary position between the porous substrate S1 and the ion selective membrane 9 in the cross section of the porous substrate S1. This boundary position corresponds to the side portion of the ion selective membrane 9 in Comparative Example 1. The sample is not in contact with the upper surface portion of the ion selective membrane 9. Therefore, there is a case where sufficient measurement sensitivity or ion selectivity is not obtained depending on the permeation state of the ion selective membrane 9 to the voids of the porous substrate S1 and the shape in which the ion selective membrane 9 is arranged in the porous substrate S1.
[0106] [Beneficial effects of embodiment 1]
[0107] [Superiority of Example 1 over Comparative Example 1]
[0108] Three superior points of Example 1 over Comparative Example 1 will be described.
[0109] <Measurement of sample concentration>
[0110] The measurement was performed using the mixed solution method for ion selective electrode method defined in JIS K0122 General Rules as the electrolyte concentration measurement method.
[0111] The solution containing the ions to be measured is NaCl, and KCl is selected as the solution containing the coexisting ions.
[0112] The concentration of KCl was fixed at 10 mmol / L, and then the concentration of NaCl was changed in five steps, namely 100 μmol / L, 1 mmol / L, 10 mmol / L, 100 mmol / L and 800 mmol / L. The sample distribution amount was set to 30 μL to 50 μL. Regarding this measurement, in order to compare the advantageous effect of the porous substrate S2 in the working electrode 8, a commercially available silver-silver chloride electrode (RE-1BP, BAS Corporation) was used for the reference electrode side.
[0113] Figure 4A and Figure 4B The measurement results are shown. Figure 4A and Figure 4B The logarithmic Na ion concentration (logCNa + ) and the measured potential (the potential after stabilization).
[0114] The sensitivity represents the slope of the region where the slope of the measured potential relative to the logarithmic Na ion concentration is constant and not negative. The ion selectivity represents how many orders of magnitude smaller the target ion can be detected relative to the coexisting K ion, and the larger it is in the negative direction, the more preferred it is.
[0115] like Figure 4AAs shown, the logarithmic Na ion concentration is close to -3 (mol / L) at the non-negative straight line rise point in Example 1. The logarithmic concentration of the coexisting ions in this example is -2, so the curve represents the expected Na ion that can be measured from a concentration that is one or more orders of magnitude smaller.
[0116] On the other hand, Figure 4B As shown, in Comparative Example 1, it is difficult to determine the region where the measurement potential rises, and therefore the determination of the ion selectivity and the sensitivity is also unstable.
[0117] like Figure 5A and Figure 5B As shown, there is a difference in performance between Example 1 and Comparative Example 1 in terms of the temporal stability of the measured potential. Figure 5A The stable time variation of the potential in Example 1 is shown; however, Figure 5B Both abrupt changes and continuous moderate changes in potential are shown.
[0118] This shows that, in Example 1, a sample required for measurement can be quickly and stably supplied to the ion selective membrane, Example 1 is excellent in measurement sensitivity, ion selectivity, and potential stability over time, and Example 1 is effective in electrolyte concentration measurement.
[0119] <Filtering of interfering particles>
[0120] The filtering of interfering particles will be described.
[0121] In the case of a sample including particles that may interfere with electrolyte concentration measurement, in order to perform stable potentiometric measurements, it is desirable that the interfering particles do not generally come into contact with the ion-selective membrane.
[0122] Figure 6 A schematic cross-sectional view is shown in the case where 30 μL to 50 μL of a sample containing particles 61 of styrene acrylic acid having a number average particle size of about 8 μm is used as a main component for the micro-analysis chip P1 used in Example 1. Figure 7 A schematic cross-sectional view is shown in the case where 30 μL to 50 μL of a sample containing particles 61 of styrene acrylic acid having a number average particle size of approximately 8 μm is used as a main component for the microanalysis chip P2 used in Comparative Example 1. It was observed that in both Example 1 and Comparative Example 1, the distributed interfering particles (particles 61) stagnated near the interface between the porous substrate having the distribution portion and the limiting member.
[0123] like Figure 6As shown, in the microanalysis chip P1 of Example 1, the interfering particles stagnate at the interface between the porous substrate S2 and the limiting member 11, so the interfering particles are difficult to diffuse into the interior of the porous substrate S1, and thus it is suitable as a structure for reducing the contact between the interfering particles and the ion selective membrane 9.
[0124] On the other hand, Figure 7 As shown, in the micro-analysis chip P2 of Comparative Example 1, depending on the distance between the dispensing portion 6 and the ion selective membrane 9, interfering particles may reach the surface of the ion selective membrane 9 by permeation, and thus may affect the electrochemical measurement.
[0125] Therefore, in the measurement of a sample containing particles that may interfere with electrochemical measurement, the interfering particles can be filtered without performing measurement pretreatment on the sample using the same configuration as in Example 1, and thus it is suitable for electrolyte concentration measurement.
[0126] [Comparative Example 2]
[0127] Figure 8 is a schematic cross-sectional view showing the configuration of a micro-analysis chip P3 according to Comparative Example 2. Figure 8 The structure of the micro-analysis chip P3 shown imitates the structure described in Patent Document 1.
[0128] <Flow path structure>
[0129] The micro-analysis chip P3 includes a porous substrate S1 and a porous substrate S2.
[0130] The porous substrate S1 is structured so that the region other than the region where the reference electrode 7 and the working electrode 8 are formed is buried with the flow path wall 5 which is impermeable to the sample.
[0131] The porous substrate S2 includes a distribution portion 6 and a flow path 4. The distribution portion 6 is arranged substantially directly above the midpoint between the reference electrode 7 and the working electrode 8 of the porous substrate S1. The flow path 4 is arranged so as to overlap the end portion of the ion crystal 10 on the distribution portion 6 side and the ion selective membrane 9 of the working electrode 8.
[0132] <Reduction of measurement time>
[0133] The reduction in measurement time will be described.
[0134] Fig. 9 The temporal changes in the behaviors of the samples after dispensing according to Example 1, Comparative Example 1, and Comparative Example 2 are shown.
[0135] ΔT1 represents the time period it takes for the dispensed sample to fill the flow path area when the dispensed sample reaches the working electrode, ΔT2 represents the time period it takes for the sample that has reached the working electrode to cover the surface of the working electrode and prepare to start measurement, and ΔT3 represents the time period it takes from the start of electrochemical measurement to the potential becoming stable and the measurement ends.
[0136] Table 1 shows the time-varying results of the sample behaviors in Example 1, Comparative Example 1 and Comparative Example 2. The results were measured during the above five-step concentration measurement (KCl concentration was fixed at 10 mmol / L, and then NaCl concentration was changed in five steps, i.e., 100 μmol / L, 1 mmol / L, 10 mmol / L, 100 mmol / L and 800 mmol / L), and the average value was taken.
[0137] In Example 1, the flow path volume can increase the amount of the flow path formed in the porous substrate S2, and the flow rate of the sample infiltrated into the flow path can be increased, compared with Comparative Example 1 or Comparative Example 2. This shows that, compared with Comparative Example 1 or Comparative Example 2, Example 1 achieves a reduction in time in all time periods ΔT1, ΔT2, and ΔT3, and the total measurement time T (=ΔT1+ΔT2+ΔT3) can be reduced.
[0138] [Table 1]
[0139] Table 1
[0140] Example 1 Comparative Example 1 Comparative Example 2 ΔT1 [seconds] 1 9 4 ΔT2 [seconds] 2 23 4 ΔT3 [seconds] 120 Unstable at 300 300
[0141] Table 2 summarizes the advantages of Example 1 over Comparative Examples 1 and 2.
[0142] High sensitivity and ion selectivity were obtained from the stable measured potential over time in Example 1. The sensitivity and ion selectivity were calculated according to the above-mentioned JIS K0122 general rules for ion selective electrode methods.
[0143] On the other hand, this suggests that in Comparative Example 1, the ion selectivity in the measurement of ion concentration changes (the KCl concentration was fixed at 10 mmol / L, and then the NaCl concentration was changed in five steps, i.e., 100 μmol / L, 1 mmol / L, 10 mmol / L, 100 mmol / L, and 800 mmol / L) was not constant, and the concentration measurement may be unstable.
[0144] In Comparative Example 2, compared with Example 1, the temporal change in potential was unstable and the total measurement time was prolonged.
[0145] In the configuration of Example 1, when the area of the ion selective membrane 9 in contact with the sample increases, a sufficient amount of the sample ( Figure 6 This shows that the construction of Example 1 is superior in terms of measurement sensitivity and ion selectivity ( Figure 4A and Figure 4B ) and the temporal stability of the measured potential ( Figure 5A and Figure 5B ) and is effective in accurately measuring the electrolyte concentration in a short time.
[0146] [Table 2]
[0147] Table 2
[0148] Example 1 Comparative Example 1 Comparative Example 2 Measurement sensitivity 86.2 Unstable 82.2 Ion selectivity -0.97 Unstable -0.91 Time stability Excellent bad good Filtration of interfering particles Excellent bad Excellent Total measurement time [seconds] Approximately 120 Unstable at 300 300
[0149] [Modification 1 of Embodiment 1]
[0150] A micro-analysis chip P4 according to Modification 1 of Embodiment 1 will be described.
[0151] Fig.10 is a cross-sectional view showing a schematic configuration of the micro-analysis chip P4. In this modification, the dispensing portion 6 is arranged on the upper surface of the working electrode 8 (substantially directly above).
[0152] Thereby, the distance between the reference electrode 7 and the working electrode 8 can be reduced while having high measurement performance such as sensitivity, ion selectivity and time stability, with the result that the device can be miniaturized.
[0153] The present invention is not limited to the above-described embodiments. Various changes or modifications are applicable without departing from the spirit and scope of the present invention. Therefore, the following claims are attached to show the scope of the present invention.
[0154] This application claims priority from Japanese Patent Application No. 2022-071207 filed on April 23, 2022, the entire contents of which are incorporated herein by reference.
Claims
1. A microanalysis chip, comprising a first porous substrate and a second porous substrate stacked on each other, wherein: A first flow path chamber, a second flow path chamber, and a first flow path connecting the first flow path chamber and the second flow path chamber are formed by a flow path wall in the first porous substrate. A reference electrode is arranged in the first flow path chamber, A working electrode is arranged in the second flow path chamber, and The second porous substrate is arranged to overlap at least a portion of a region on the surface of the first porous substrate where the working electrode is formed.
2. The micro-analysis chip according to claim 1, wherein: The working electrode is covered by an ion-selective membrane including a component having ion selectivity.
3. The micro-analysis chip according to claim 1, wherein: The second porous substrate has a dispensing portion for dispensing a sample.
4. The micro-analysis chip according to claim 1 or 2, further comprising a limiting member into which the sample does not penetrate, the limiting member being arranged at least at a position on the upper surface of the second porous substrate where the distributing portion and the working electrode are connected. 5 . The micro-analysis chip according to claim 1 , further comprising an ionic crystal having sample solubility, the ionic crystal being arranged on a surface of the reference electrode.