Low-carbon clinker with hydration and carbonization performance as well as preparation method and application of low-carbon clinker

Through the use of high-magnesium limestone and siliceous raw material ingredients and modifiers, the problem of insufficient mold release and carbonization performance of low-carbon clinker after casting is solved, rapid mold release and high carbonization strength are achieved, and its application scope is broadened .

CN119059746APending Publication Date: 2024-12-03HUAXIN CEMENT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411188305.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Low-carbon clinker is difficult to release after casting and molding and has insufficient carbonization performance, which limits its application scope, especially in casting and molding occasions.

Method used

High-magnesium limestone and siliceous raw materials are used to prepare low-carbon clinker after decomposition and rotary kiln calcination, and MgSO4 and citric acid are added as modifiers to improve its hydration and carbonization properties, so that it can be quickly removed after casting and forming. and improve carbonization strength.

Benefits of technology

It realizes rapid release of low-carbon clinker after casting and forming, and significantly improves the carbonization strength and carbonization rate, broadens its application range, and is simple in preparation method, with low cost and energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005014207770000041
    Figure BDA0005014207770000041
  • Figure BDA0005014207770000042
    Figure BDA0005014207770000042
  • Figure BDA0005014207770000043
    Figure BDA0005014207770000043
Patent Text Reader

Abstract

The invention discloses a preparation method of low-carbon clinker with hydration and carbonization performance, which comprises the following steps: (1) obtaining high-magnesium limestone and siliceous raw materials, carrying out low-calcium batching, and then mixing and grinding; (2) adding the obtained mixture into a decomposing furnace for decomposing; (3) calcining in a rotary kiln after decomposition to prepare primary low-carbon clinker; and (4) mixing and grinding the low-carbon clinker obtained in the step (3) and a modifier to obtain the low-carbon clinker with hydration and carbonization properties. According to the low-carbon clinker disclosed by the invention, the low-calcium and high-magnesium limestone is taken as a main raw material, and the composite modifier, low-temperature calcination and grinding processes are combined, so that the obtained low-carbon clinker has good hydration performance and carbonization performance, rapid and effective demolding after pouring molding can be realized, meanwhile, excellent carbonization performance can be shown, and the application range of the low-carbon clinker is effectively widened.
Need to check novelty before this filing date? Find Prior Art