Method for solving precipitation of shading material on surface of photomask

By using O2 surface treatment process to form a protective layer on the surface of the photocapsule, the problem of precipitation of light-shielding materials during lithography is solved, the service life of the photocapsule is extended and the rework frequency is reduced, and the surface stability and cost saving of the photocapsule are achieved.

CN119065196APending Publication Date: 2024-12-03SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411103586.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

During the lithography process, high-energy ArF exposure causes the precipitation of light-shielding material on the surface of the photomask, forming oxide defects, resulting in key size changes and a decrease in wafer yield. The existing technology can only temporarily solve the problem and requires frequent return to the factory to repair.

Method used

The O2 surface treatment process forms a protective layer on the side walls of the light-shielding material layer and the phase-shielding layer to prevent material precipitation. The thickness of the protective layer is 16% to 18% of the light-shielding material layer by using an oxygen plasma treatment process.

Benefits of technology

Effectively prevent the precipitation of light-shielding material on the surface of the photomask, extend the usage time of the photomask, reduce the rework frequency, save process costs, and maintain the stability of the key dimensions of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119065196A_ABST
    Figure CN119065196A_ABST
Patent Text Reader

Abstract

The invention provides a method for solving precipitation of a shading material on the surface of a photomask, which comprises the following steps of: providing a photomask plate which is divided into a shading area and a light-transmitting area and comprises a transparent substrate layer, a phase shift layer formed on the surface of the transparent substrate layer and a shading material layer formed on the upper surface of the phase shift layer, the phase shift layer and the shading material layer are located in the shading area, and the phase shift layer is exposed out of the side wall of the shading area; and forming a protective layer on the surface of the shading material layer and the side wall of the phase shift layer by using an O2 surface treatment process. According to the invention, the problem that a shading material is easy to separate out in the existing photomask plate is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor manufacturing, and in particular to a method for solving the problem of light shielding material precipitation on a mask surface. Background Art

[0002] Photolithography is the core technology of semiconductor manufacturing, and the mask is the mold of photolithography. Moreover, as the process nodes continue to advance, the requirements of photolithography for pattern line width are getting higher and higher.

[0003] When forming a contact hole (CT) or a through hole (Via), the exposure energy of the exposure light source Arf or Krf used in the photolithography process is relatively high (the exposure energy of Arf is 6.43eV, and the exposure energy of Krf is 5eV). Therefore, during the use of the mask, the higher energy ArF causes H2O to decompose into oxygen ions and generate oxides (such as Cr) with the light-shielding material (such as Cr). x O y ) causes migration and forms defects (such as Figure 1 Moreover, during the photolithography process, energy is concentrated, and the most serious energy concentration is at the center of the mask. As the exposure and cumulative exposure time increase, the cumulative exposure of the wafer exceeds 30,000 pieces. The mask cutting path diverges from the center to the outside, and covered oxide defects appear in the light-transmitting area, causing the critical dimension (CD) to continue to decline, reaching a deviation of 2nm in about half a year, and even showing a deteriorating trend, which ultimately affects the wafer yield.

[0004] The existing solution to the above problem is to return the mask to the factory, perform a similar double-scanning process, and perform etching again to remove the oxide in the light-transmitting area. However, this method can only temporarily solve the defect problem, and the returned mask needs to be returned to the factory again after being used for a period of time. Summary of the invention

[0005] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a method for solving the problem of light-shielding material precipitation on the surface of a photomask, so as to solve the problem that light-shielding material precipitation is easy to occur on the existing photomask.

[0006] To achieve the above-mentioned purpose and other related purposes, the present invention provides a method for solving the problem of light-shielding material precipitation on the surface of a photomask, the method comprising:

[0007] A photomask is provided, which is divided into a light-shielding area and a light-transmitting area, and includes a transparent substrate layer, a phase-shift layer formed on the surface of the transparent substrate layer, and a light-shielding material layer formed on the upper surface of the phase-shift layer, wherein the phase-shift layer and the light-shielding material layer are located in the light-shielding area, and the phase-shift layer leaks out of its side wall;

[0008] A protective layer is formed on the surface of the light shielding material layer and the sidewall of the phase shift layer by using an O2 surface treatment process.

[0009] Optionally, the O2 surface treatment process is an oxygen plasma surface treatment process.

[0010] Optionally, the thickness of the protective layer is 16% to 18% of the thickness of the light-shielding material layer.

[0011] Optionally, the thickness of the protective layer is 17% of the thickness of the light-shielding material layer.

[0012] Optionally, the light-shielding material layer is made of chromium.

[0013] Optionally, the phase-shift layer is made of MoSi or MoSiON.

[0014] Optionally, the material of the transparent substrate layer includes quartz glass.

[0015] As described above, the method of the present invention for solving the problem of precipitation of shading material on the surface of the mask forms a protective layer on the side wall of the phase shift layer and the surface of the shading material layer through an O2 surface treatment process, thereby solving the problem of precipitation of shading material (such as Cr), thereby preventing the key dimensions of the device from changing as the use time of the mask increases, and can enable the mask to be used for a longer time to avoid frequent rework, saving process costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 A schematic diagram showing a conventional photomask having oxide defects.

[0017] Figure 2 Shown is a schematic diagram of a photomask of the present invention.

[0018] Figure 3 It is a schematic diagram of a photomask for forming a protective layer according to the present invention.

[0019] Figure 4 The flowchart of the method for solving the problem of light shielding material precipitation on the surface of the photomask according to the present invention is shown. DETAILED DESCRIPTION

[0020] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0021] See also Figures 1 to 4It should be noted that the illustrations provided in this embodiment are only schematic illustrations of the basic concept of the present invention. Although the illustrations only show components related to the present invention and are not drawn according to the number, shape and size of components in actual implementation, the form, quantity and proportion of each component in actual implementation may be changed arbitrarily, and the component layout may also be more complicated.

[0022] like Figure 4 As shown, this embodiment provides a method for solving the problem of light shielding material precipitation on the surface of the mask, the method comprising:

[0023] A photomask is provided, which is divided into a light-shielding area and a light-transmitting area, and includes a transparent substrate layer, a phase-shift layer formed on the surface of the transparent substrate layer, and a light-shielding material layer formed on the upper surface of the phase-shift layer, wherein the phase-shift layer and the light-shielding material layer are located in the light-shielding area, and the phase-shift layer leaks out of its side wall;

[0024] A protective layer is formed on the surface of the light shielding material layer and the sidewall of the phase shift layer by using an O2 surface treatment process.

[0025] Specifically, the O2 surface treatment process is an oxygen plasma surface treatment process.

[0026] Specifically, the thickness of the protective layer is 16% to 18% of the thickness of the light-shielding material layer.

[0027] More specifically, the thickness of the protective layer is 17% of the thickness of the light shielding material layer. In this embodiment, the thickness of the light shielding material layer takes different values ​​according to different devices.

[0028] Specifically, the light-shielding material layer is made of chromium.

[0029] Specifically, the material of the phase-shift layer includes MoSi or MoSiON.

[0030] Specifically, the material of the transparent substrate layer includes quartz glass.

[0031] In summary, the method of solving the problem of light shielding material precipitation on the surface of the mask of the present invention forms a protective layer on the side wall of the phase shift layer and the surface of the light shielding material layer through the O2 surface treatment process, thereby solving the problem of light shielding material (such as Cr) precipitation, thereby preventing the key dimensions of the device from changing as the use time of the mask increases, and can make the mask use longer and avoid frequent rework, saving process costs. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0032] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for solving the problem of light shielding material precipitation on the surface of the mask, It is characterized in that The method comprises: A photomask is provided, which is divided into a light-shielding area and a light-transmitting area, and includes a transparent substrate layer, a phase-shift layer formed on the surface of the transparent substrate layer, and a light-shielding material layer formed on the upper surface of the phase-shift layer, wherein the phase-shift layer and the light-shielding material layer are located in the light-shielding area, and the phase-shift layer leaks out of its side wall; Using O 2 The surface treatment process forms a protective layer on the surface of the light shielding material layer and the side wall of the phase shift layer.

2. The method for solving the problem of light shielding material precipitation on the surface of the photomask according to claim 1, It is characterized in that The O 2 The surface treatment process is an oxygen plasma surface treatment process.

3. The method for solving the problem of light shielding material precipitation on the surface of the photomask according to claim 1, It is characterized in that The thickness of the protective layer is 16% to 18% of the thickness of the light-shielding material layer.

4. The method for solving the problem of light shielding material precipitation on the surface of the photomask according to claim 3, It is characterized in that The thickness of the protective layer is 17% of the thickness of the light shielding material layer.

5. The method for solving the problem of light shielding material precipitation on the surface of a photomask according to any one of claims 1 to 4, It is characterized in that The material of the light shielding material layer includes chromium.

6. The method for solving the problem of light shielding material precipitation on the surface of the photomask according to claim 1, It is characterized in that The material of the phase shift layer includes MoSi or MoSiON.

7. The method for solving the problem of light shielding material precipitation on the surface of the photomask according to claim 1, It is characterized in that The material of the transparent substrate layer includes quartz glass.

Citation Information

Patent Citations

  • Photoetching method

    CN106292186A

  • Attenuated phase shift mask and manufacturing method thereof

    CN106597803A

  • Mask blank, transfer mask, and methods of manufacturing the same

    US20110244373A1