Method for determining key factors causing layering of plastic package device

By formulating layered degradation test and simulation models, combined with statistical analysis, we determine the key factors for layering of plastic sealing devices, and solving the problem of difficulty in accurately identifying the causes of layering of plastic sealing devices in the existing technology, and improving the reliability of device design and manufacturing.

CN119066933APending Publication Date: 2024-12-03BEIHANG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411295526.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-18
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Plastic sealed devices are prone to stratification under high temperatures and environmental stresses, resulting in device failure, but it is difficult for the prior art to accurately determine the key factors leading to stratification.

Method used

By formulating a stratified degradation test plan, combining acoustic scanning microscopy detection and ANSYS simulation model, the influence of each sensitive factor of the plastic packaging device is quantitatively characterized, and the standardized regression coefficient is calculated through SPSS statistical software to sort out the key factors leading to stratification.

Benefits of technology

It has achieved accurate grasp of the layered degradation process of plastic sealing devices and determined key factors, providing new ideas for the reliability of plastic sealing devices, and improving the reference value of design and manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119066933A_ABST
    Figure CN119066933A_ABST
Patent Text Reader

Abstract

The invention provides a method for determining key factors causing layering of a plastic package device, and the method comprises the following steps: 1, analyzing a layering failure mechanism of the plastic package device, and determining a layering degradation test scheme; 2, carrying out a layering degradation test, obtaining a sound scanning image of each plastic package device after the layering degradation test, and recording the layering time; 3, carrying out a high-temperature storage and temperature cycle simulation test of the plastic package device, and correcting the simulation model in combination with the time required by layering of the plastic package device in the step 2; 4, simulating and calculating time required by complete layering of the device under different layering sensitive factors according to a variable control method; and 5, calculating a standardized regression coefficient of each sensitive factor, and determining key factors causing layering of the plastic package device. Through the above steps, each sensitive factor causing layering of the plastic package device can be quantitatively represented, and importance ranking is carried out, so that the key factor causing layering of the plastic package device is determined.
Need to check novelty before this filing date? Find Prior Art

Description

Technical field:

[0001] The invention provides a method for determining key factors leading to delamination of a plastic-encapsulated device, relates to a method for determining key factors leading to delamination of a plastic-encapsulated device, and belongs to the field of reliability failure analysis of electronic components. Background technology:

[0002] Plastic encapsulated devices have small characteristic dimensions, low cost, and excellent physical properties. They are gradually applied to high-tech fields such as military industry, aerospace, and submarine relay lines. However, due to the characteristics of plastic encapsulation materials, plastic encapsulated devices still have many reliability problems such as delamination, voids, and corrosion. Internal delamination is a failure mode that often occurs in the screening and identification of electronic components.

[0003] The connection between the internal materials of the plastic-encapsulated device is through intermolecular forces, which is an adhesive bonding structure. Under the influence of time and external forces, the interface between the internal plastic-encapsulated layer and other materials is prone to stratification. Although the thermal expansion coefficients of the plastic-encapsulated device substrate materials, chip materials, and adhesives have been optimized and improved in recent years, and the plastic-encapsulation technology has become more mature, the probability of stratification has been reduced, but the materials of the various parts of the plastic-encapsulated device cannot be completely matched, and the moisture intrusion caused by packaging defects and the hygroscopicity of the plastic itself can also cause stratification of the plastic-encapsulated device under high temperature. After stratification occurs, the internal stress between the originally stable internal structures increases. After the stratification expands to a certain extent, it will trigger a series of failures, and ultimately lead to device failure.

[0004] At present, the most commonly used detection method for delamination is to use acoustic microscope imaging detection technology (C-SAM) in the process of screening and identification of plastic-encapsulated microcircuits, and to detect and determine the unqualified criteria according to the destructive physical analysis method of military components GJB4027A-2006, so as to find delamination defects in the early stage of use and filter out problematic devices. However, there are many sensitive factors for the delamination failure of plastic-encapsulated devices, not only the delamination hidden dangers caused by the manufacturing design process and materials, but also environmental stress can cause delamination of plastic-encapsulated devices. There is no way to determine the key factors that cause delamination of plastic-encapsulated devices. Therefore, it is necessary to propose a method for determining the key factors that cause delamination of plastic-encapsulated devices with high credibility based on the process of delamination degradation of plastic-encapsulated devices.

[0005] The present invention proposes a method for determining the key factors that lead to the delamination of plastic-encapsulated devices. On the one hand, the process and influence of the delamination degradation of plastic-encapsulated devices can be more accurately grasped; on the other hand, the influence of sensitive factors such as plastic-encapsulated materials and environmental stress on the delamination of plastic-encapsulated devices can be quantitatively characterized, thereby determining the key factors that lead to the delamination of plastic-encapsulated devices, providing new ideas for the reliability research of plastic-encapsulated devices. Summary of the invention:

[0006] 1. Purpose: To address the deficiencies of the prior art, the present invention discloses a method for determining key factors leading to delamination of plastic-encapsulated devices, providing a new approach for the reliability research of plastic-encapsulated devices.

[0007] 2. Technical solution:

[0008] The present invention forms a method for determining key factors leading to delamination of plastic-encapsulated devices, quantitatively characterizes sensitive factors leading to delamination of plastic-encapsulated devices and sorts them by importance, thereby determining key factors leading to delamination of plastic-encapsulated devices.

[0009] The present invention provides a method for determining key factors leading to delamination of a plastic-encapsulated device, which comprises the following steps:

[0010] Step 1: Analyze the failure mechanism of plastic-encapsulated devices and formulate a delamination degradation test plan. The reasons for the delamination of plastic-encapsulated devices include the difference in thermal expansion coefficient, Poisson's ratio, density, thermal conductivity, elastic modulus, and specific heat capacity of the internal materials of the device; the external temperature change rate and the high and low temperature difference of the temperature cycle, etc. 8 delamination sensitive factors. The delamination degradation test is set to include high-temperature storage and temperature cycle tests. T1 is the upper limit of the operating temperature range specified in the product manual of the plastic-encapsulated device, and T2 is the working limit temperature specified in the product manual. 20 plastic-encapsulated devices with no obvious delamination and normal electrical performance parameters are selected and numbered, and divided into two groups for high-temperature storage test and temperature cycle test respectively. Devices numbered 1 to 5 are subjected to high-temperature storage test at temperature T1, devices numbered 6 to 10 are subjected to high-temperature storage test at temperature T2, and devices numbered 11 to 20 are subjected to -65℃~150℃ temperature cycle test. Refer to the relevant conditions in Method 1008 Stability Baking (High Temperature Storage) and Method 1010 Temperature Cycling in GJB548B, and set the high temperature storage time and temperature cycle times in combination with the detailed product specifications.

[0011] Step 2: Select 20 plastic-encapsulated devices that have passed the initial screening, conduct delamination degradation tests, and obtain acoustic scanning images of the plastic-encapsulated devices after the delamination degradation tests. After each delamination degradation test, use an acoustic scanning microscope to detect delamination of the plastic-encapsulated devices. Before the delamination test, bake them in a 125°C incubator for one hour. During the test, place the plastic-encapsulated devices on the acoustic scanning equipment test bench as required. After the test, take them out of the non-ionized water as soon as possible. After the test, clean the devices and then place them in a 125°C incubator to dry for one hour. For devices that have completely delaminated, record the delamination time t i (i=1,2…20); for the undelaminated device, repeat the delamination degradation test until the device image is completely delaminated, and record the delamination time t i .

[0012] Step 3: Establish ANSYS simulation model A of plastic-encapsulated components, and carry out high-temperature storage and temperature cycle simulation tests under the same conditions as step 1, namely, high-temperature storage test at temperature T1, high-temperature storage test at temperature T2, and temperature cycle test at -65℃~150℃, to obtain the strain energy W of each plastic-encapsulated component at each time node. t , calculate the strain energy density W a :

[0013]

[0014] In the formula, v t is the volume of the dangerous point at each time node in the simulation process;

[0015] The Darveaux model is used to calculate the number of temperature cycles or high temperature storage time t required for the simulation unit to be completely delaminated. a :

[0016]

[0017] In the formula, ΔW t =W t2 -W t1 , is the increment of average strain energy density, a is the critical length of delamination, K1, K2, K3, K4 are the delamination expansion correlation coefficients, and their values ​​are shown in the following table:

[0018]

[0019] Get the time t when each plastic encapsulated device is completely delaminated ai , adjust the mesh settings and solver parameters of simulation model A, including the density, type and size of the mesh, as well as the relaxation factor and iteration parameters of the solver, so that t ai With t i Equal, multiple iterations are performed to verify the corrected simulation model B.

[0020] Step 4: Based on simulation model B, simulate and calculate the time t required for the device to be completely delaminated under different delamination sensitivity factors mn (m=1,2…8,n=1,2…6). ANSYS finite element simulation software was used to carry out the simulation. Based on the simulation model B modified in step 4, according to the method of controlling variables, for 8 different sensitive factors, the parameter value of one delamination sensitive factor in the simulation model was changed, and the values ​​of other parameters were fixed unchanged. Six groups of simulation tests were set under each sensitive factor, and the time t when each plastic encapsulated device was completely delaminated was recorded. mn (m=1,2…8,n=1,2…6).

[0021] The specific method of "controlling variables" is: the thermal expansion coefficient value of the material with a larger thermal expansion coefficient value in the substrate and the plastic encapsulation material is set in a step-by-step manner, and the other method keeps the true value unchanged. The step value is 10% of the sum of the thermal expansion coefficients of the two, and the values ​​of other delamination sensitive factors are fixed unchanged. Six groups of simulation experiments are set up, and the time t when the plastic encapsulation device is completely delaminated is calculated in combination with the Darveaux model. mn In the same way, the individual effects of parameters such as Poisson's ratio, thermal conductivity, specific heat, and elastic modulus on delamination are simulated; for temperature, a delamination-sensitive factor, the upper and lower limits of the temperature cycle are set to -65℃~150℃, and the temperature change rate is adjusted. The initial value is 21.5℃ / min, the step value is 1.5℃ / min, and the temperature is adjusted to 30.5℃ / min. Other parameters remain unchanged and simulation is carried out; starting from T1 and +5℃ as the step value until T2, the temperature load is applied to the simulation model, and other parameters are kept unchanged. Simulation is carried out to calculate the time t when the plastic-encapsulated device is completely delaminated. mn (m=1,2…8,n=1,2…6).

[0022] Step 5: Use SPSS statistical software to calculate the standardized regression coefficient δ of each stratification sensitive factor on the stratification time of the plastic encapsulated device m (m=1,2…8), the larger the absolute value of the standardized regression coefficient, the stronger the correlation of the sensitive factor to the delamination of the plastic encapsulated device, that is, the greater the impact. By comparing the absolute values ​​of each standardized regression coefficient, the importance of each delamination sensitive factor is ranked to obtain the key factors that lead to the delamination of the plastic encapsulated device.

[0023] 3. Advantages and effects:

[0024] The present invention provides a method for determining key factors leading to delamination of a plastic-encapsulated device. The advantages of the present invention are:

[0025] (1) This method provides a method for determining the key factors that lead to delamination of plastic-encapsulated devices, which can quantitatively characterize the various sensitive factors of delamination of plastic-encapsulated devices and rank them by importance, thereby determining the key factors that lead to delamination of plastic-encapsulated devices.

[0026] (2) This method can provide a reference for the design, manufacture and selection of plastic encapsulated devices by determining the key factors of plastic encapsulated device stratification.

[0027] (3) This method designs a delamination degradation test for plastic-encapsulated devices and obtains acoustic scanning images of the device at different times, which can provide a reference for the study of delamination degradation and failure analysis of plastic-encapsulated devices. Description of the drawings:

[0028] In order to make the contents of the present invention more clearly understood, the present invention is further described in detail below based on specific embodiments of the present invention in conjunction with the accompanying drawings.

[0029] Figure 1 It is a flow chart of the method of the present invention.

[0030] Figure 2 It is a schematic diagram of substrate layering image and layering waveform.

[0031] Figure 3 This is a ranking chart of the importance of sensitive factors for stratification of plastic encapsulated components. Implementation method:

[0033] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.

[0034] The present invention provides a method for determining the key factors that lead to delamination of plastic-encapsulated devices. In a specific embodiment, a MAX708 monitoring circuit is selected, and its flow chart is as follows: Figure 1 As shown, the specific implementation steps are as follows:

[0035] Step 1: Analyze the failure mechanism of plastic-encapsulated devices and formulate a delamination degradation test plan. After investigation, it was found that the main reasons for the delamination of the MAX708 microprocessor monitoring circuit of the plastic-encapsulated device were the mismatch of the internal material coefficients of the device and the influence of external environmental stress, specifically the difference in thermal expansion coefficient, Poisson's ratio, density value, thermal conductivity, elastic modulus, and specific heat capacity of the device materials; the external temperature change rate and the high and low temperature difference of the temperature cycle, etc. 8 delamination sensitive factors. According to the detailed specifications of the MAX708 microprocessor monitoring circuit, the test plan is set as follows: 20 MAX708 microprocessor monitoring circuits without obvious delamination are selected and numbered, and divided into two groups for high-temperature storage test and temperature cycle test respectively. Devices numbered 1 to 5 are subjected to 70℃ high-temperature storage test, devices numbered 6 to 10 are subjected to 125℃ high-temperature storage test, and devices numbered 11 to 20 are subjected to -65℃~150℃ temperature cycle test. Refer to the relevant conditions in Method 1008 Stability Baking (High Temperature Storage) and Method 1010 Temperature Cycle in GJB548B, and set the high temperature storage time and temperature cycle times in combination with the detailed specifications of the MAX708 microprocessor monitoring circuit, as shown in the following table:

[0036]

[0037] Step 2: Select 20 plastic-encapsulated devices that have passed the initial screening, conduct delamination degradation tests, and obtain acoustic scanning images of the plastic-encapsulated devices after the delamination degradation tests. After each delamination degradation test, use an acoustic scanning microscope to detect delamination of the plastic-encapsulated devices. Before the delamination test, bake them in a 125°C incubator for one hour. During the test, place the plastic-encapsulated devices on the acoustic scanning equipment test bench as required. After the test, take them out of the non-ionized water as soon as possible. After the test, clean the devices and then place them in a 125°C incubator to dry for one hour. For devices that have completely delaminated, record the delamination time t i (i=1,2…20); for the undelaminated device, repeat the delamination degradation test until the device image is completely delaminated, and record the delamination time t i . Figure 2 This is a schematic diagram of the substrate layering image and layering waveform of a MAX708 microprocessor monitoring circuit.

[0038] Step 3: Establish ANSYS simulation model A of the plastic-encapsulated device and conduct high-temperature storage and temperature cycle simulation tests under the same conditions as step 1. Obtain the time t when each plastic-encapsulated device is completely delaminated ai , adjust the mesh settings and solver parameters of simulation model A, including the density, type and size of the mesh, as well as the relaxation factor and iteration parameters of the solver, so that t ai With t i Equal, multiple iterations are performed to verify the corrected simulation model B.

[0039] The device was scanned by X-ray equipment to obtain the actual internal structure characteristics and size of the device, and then the ANSYS simulation model A of the plastic packaged device was established. The simulation results of the MAX708ESA monitoring circuit under 70℃ high temperature storage test, 125℃ high temperature storage test and -65℃~150℃ temperature cycle test were obtained, and the strain energy W of each MAX708ESA monitoring circuit at each time node was further obtained. t , calculate the strain energy density W a :

[0040]

[0041] In the formula, v t is the volume of the dangerous point at each time node in the simulation process;

[0042] The Darveaux model is used to calculate the number of temperature cycles or high temperature storage time t required for the simulation unit to be completely delaminated. a :

[0043]

[0044] In the formula, ΔW t =Wt2 -W t1 , is the increment of average strain energy density, a is the critical length of delamination, K1, K2, K3, K4 are the delamination expansion correlation coefficients, and their values ​​are shown in the following table:

[0045]

[0046] Calculate the time t required for each plastic encapsulated device to completely delaminate ai , adjust the mesh settings and solver parameters of simulation model A, including the density, type and size of the mesh, as well as the relaxation factor and iteration parameters of the solver, so that t ai With t i Equal, multiple iterations are performed to verify the corrected simulation model B.

[0047] Step 4: For the corrected simulation model B, simulate and calculate the time t required for the device to be completely delaminated under different delamination sensitivity factors mn (m=1,2…8,n=1,2…6). ANSYS finite element simulation software was used to carry out the simulation. Based on the simulation model B modified in step 4, according to the method of controlling variables, for 8 different sensitive factors, the parameter value of one delamination sensitive factor in the simulation model was changed, and the values ​​of other parameters were fixed unchanged. Six groups of simulation tests were set under each sensitive factor, and the time t when each plastic encapsulated device was completely delaminated was recorded. mn (m=1,2…8,n=1,2…6).

[0048] In this example, the thermal expansion coefficient value of the material with a larger thermal expansion coefficient in the substrate and the plastic encapsulation material is set in a step-by-step manner, and the other one keeps the true value unchanged. The step value is 10% of the sum of the thermal expansion coefficients of the two. The values ​​of other delamination sensitive factors are fixed unchanged. Six groups of temperature cycle simulation tests from -65℃ to 150℃ are set. The time t when the plastic encapsulation device is completely delaminated is calculated in combination with the Darveaux model. mn In the same way, the individual effects of parameters such as Poisson's ratio, thermal conductivity, specific heat capacity, and elastic modulus on delamination are simulated to obtain the time t when the plastic encapsulated device is completely delaminated. mn .

[0049] Similarly, the upper and lower limits of the temperature cycle for the MAX708 monitoring circuit are set to -65℃~150℃, and the temperature change rate is adjusted. The initial value is 21.5℃ / min, the step value is 1.5℃ / min, and the temperature change rate is adjusted to 30.5℃ / min. Other parameters remain unchanged. The Darveaux model and the modified model in step 5 are used to obtain the time t when the substrate and plastic package simulation unit are completely delaminated. mn(m=1,2…8,n=1,2…6). ; Starting from 70℃ and increasing by +5℃ until 125℃, the simulation model is subjected to temperature load, and other parameters are kept unchanged to simulate the high temperature storage test, and then the time t when the plastic encapsulated device is completely delaminated is calculated. mn (m=1,2…8,n=1,2…6).

[0050] Step 5: Use SPSS statistical software to calculate the standardized regression coefficient δ of each stratified sensitive factor on stratification time m (m=1,2…8), the larger the absolute value of the standardized regression coefficient, the stronger the correlation of the sensitive factor to the delamination of the plastic encapsulated device, that is, the greater the impact. By comparing the absolute values ​​of each standardized regression coefficient, the importance of each delamination sensitive factor is ranked to obtain the key factors that lead to the delamination of the plastic encapsulated device.

[0051] In this example, the standardized regression coefficients of material parameters such as thermal expansion coefficient, Poisson's ratio, thermal conductivity, and temperature cycle limit temperature difference, temperature cycle temperature change rate, and storage temperature for the complete stratification of the MAX708 monitoring circuit are calculated using SPSS statistical software. The calculation results are shown in the following table:

[0052]

[0053] Compare the absolute values ​​of each standardized regression coefficient and rank the importance of each hierarchical sensitive factor to obtain the key factors that lead to the stratification of the MAX708ESA type monitoring circuit. Figure 3 This is the importance ranking diagram of the stratification sensitive factors of the plastic packaged device.

[0054] It is found that the material parameters that have a greater impact on delamination are thermal expansion coefficient, elastic modulus and thermal conductivity, etc.; the temperature factors that have a greater impact on delamination are the high and low temperature difference of the temperature cycle and the temperature change rate. Therefore, the key material factors that lead to delamination of the MAX708ESA type monitoring circuit are the difference in thermal expansion coefficient and elastic modulus between the plastic packaging material and the substrate, and the key temperature factor is the high and low temperature difference of the temperature cycle.

Claims

1. A method for determining key factors leading to delamination of a plastic packaged device, comprising the following steps: Step 1: Analyze the failure mechanism of plastic-encapsulated components and determine the delamination degradation test plan. The reasons for the delamination of plastic-encapsulated components include eight delamination-sensitive factors, including the difference in thermal expansion coefficient, Poisson's ratio, density, thermal conductivity, elastic modulus, specific heat capacity, external temperature change rate, and temperature cycle high and low temperature difference. Determine the delamination degradation test plan, where T1 is the upper limit of the operating temperature range specified in the product manual of the plastic-encapsulated device, and T2 is the operating limit temperature specified in the product manual. Select 5 plastic-encapsulated devices for high-temperature storage test at temperature T1, and 5 devices for high-temperature storage test at temperature T2; Ten devices were selected for -65°C to 150°C temperature cycle test. Step 2: Select 20 plastic-encapsulated devices that have passed the initial screening, conduct a delamination degradation test, and obtain the acoustic scanning images of the plastic-encapsulated devices after the delamination degradation test. For devices that have completely delaminated, record the delamination time t i (i=1, 2...20); for the undelaminated device, repeat the delamination degradation test until the device image is completely delaminated, and record the delamination time t i . Step 3: Establish ANSYS simulation model A of the plastic-encapsulated device, carry out high-temperature storage and temperature cycle simulation tests under the same conditions as step 1, and obtain the time t for each plastic-encapsulated device to be completely delaminated ai , adjust the mesh settings and solver parameters of simulation model A so that t ai With t i Equal, and the modified simulation model B is obtained. Step 4: Based on simulation model B, according to the method of controlling variables, for 8 different sensitive factors, change the parameter value of one delamination sensitive factor in the simulation model, keep the other parameter values ​​unchanged, set 6 groups of simulation tests under each sensitive factor, and record the time t when each plastic encapsulated device is completely delaminated mu (m=1, 2...8, n=1, 2...6). Step 5: Calculate the standardized regression coefficient δ of each delamination sensitive factor on the delamination time of the plastic packaged device m (m=1, 2...8), compare the absolute values ​​of each standardized regression coefficient, and rank the importance of each stratification sensitive factor to obtain the key factors that lead to stratification of plastic-encapsulated components.

2. The method for determining key factors leading to delamination of plastic-encapsulated components according to claim 1, characterized in that: The specific method of "correcting the simulation model" described in step 3 is as follows: based on the ANSYS finite element simulation software, a simulation model A of the plastic-encapsulated device is established, and the simulation results of the device under high-temperature storage tests at temperatures T1 and T2 and temperature cycle tests at -65°C to 150°C are obtained. The time t required for the plastic-encapsulated device to be completely delaminated is further calculated using the Darveaux model. ai , compared with t in step 3 i , change the mesh settings and solver parameters of simulation model A, including the density, type and size of the mesh, as well as the relaxation factor and iteration parameters of the solver, and obtain the modified simulation model B through multiple iterations.

3. The method for determining key factors leading to delamination of plastic-encapsulated components according to claim 1, characterized in that: The specific method of "controlling variables" in step 4 is: the thermal expansion coefficient value of the material with a larger thermal expansion coefficient value in the substrate and the plastic encapsulation material is set in a step-by-step manner, and the other one keeps the true value unchanged. The step value is 10% of the sum of the thermal expansion coefficients of the two. The values ​​of other delamination sensitive factors are fixed unchanged. Six groups of simulation experiments are set up, and the time t when the plastic encapsulation device is completely delaminated is calculated in combination with the Darveaux model. mn In the same way, the individual effects of parameters such as Poisson's ratio, thermal conductivity, specific heat capacity, and elastic modulus on delamination are simulated; For the temperature, a sensitive factor for stratification, the upper and lower limits of the temperature cycle are set to -65℃~150℃, and the temperature change rate is adjusted. The initial value is 21.5℃ / min, the step value is 1.5℃ / min, and the temperature is adjusted to 30.5℃ / min. Other parameters remain unchanged and simulation is carried out. Taking T1 as the starting point and +5℃ as the step value until T2, the simulation model is subjected to temperature load, and other parameters are kept unchanged and simulation is carried out to calculate the time t when the plastic encapsulated device is completely stratified. mn (m=1, 2...8, n=1, 2...6).