Chemical plating method
By using chemical deposition method to perform temperature control in nitrogen atmosphere in semiconductor device manufacturing, the problem of metal layer oxidation and temperature gradient control is solved, and the performance and reliability of the device are improved.
Patent Information
- Application Number
- CN202410601374.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-10-24
- Filing Date
- 2024-05-15
- Publication Date
- 2024-12-03
AI Technical Summary
In the existing semiconductor device manufacturing process, it is difficult to effectively prevent the metal layer from oxidizing during metal plating, and the temperature gradient control is not fine enough, affecting the device performance and reliability.
A metal layer, including metals such as nickel, palladium and gold, is formed on the flat surface of the semiconductor substrate by chemical deposition method, and is then heated from ambient temperature to 150C to 350C in a temperature gradient of less than or equal to 3C per minute in a nitrogen atmosphere, and The substrate is removed when cooled to less than 50C to avoid oxidation of the metal layer.
It effectively prevents the oxidation of the metal layer, improves the void structure of the device, avoids the phase shift problem of the metal layer, and improves the performance and reliability of the device.
Smart Images

Figure CN119069341A_ABST
Abstract
Description
[0001] Cross-references to related patent applications
[0002] This document claims the benefit of U.S. Provisional Patent Application 63 / 505,612, filed on June 1, 2023, to Noma et al., entitled “Electroless Metal Plating Semiconductor Device,” the disclosure of which is hereby incorporated by reference in its entirety. Technical Field
[0003] Aspects of this document generally relate to semiconductor device manufacturing processes, such as metal plating. More specific implementations relate to chemical metal plating systems and methods. Background Art
[0004] Semiconductor devices utilize semiconductor packages to establish electrical connections with a circuit board or motherboard to which the semiconductor package is coupled. Various semiconductor package designs have been devised that allow the associated semiconductor devices to be protected from moisture or shock and vibration. Summary of the invention
[0005] A specific implementation of the chemical deposition method may include providing a semiconductor substrate including a first maximum planar surface and a second maximum planar surface; forming a back metal layer on the second maximum planar surface; attaching a ribbon to the back metal layer; and chemically depositing a metal layer on a pad included on the first maximum planar surface. The method may include removing the ribbon after chemical deposition; and baking the semiconductor substrate after removing the ribbon.
[0006] Specific implementations of the chemical deposition method may include one, all, or any of the following:
[0007] The method may include dicing the semiconductor substrate to form a plurality of semiconductor dies.
[0008] The semiconductor substrate may include silicon carbide.
[0009] The metal layer may include one of: nickel, palladium and gold; nickel and copper, or copper.
[0010] Baking the semiconductor substrate may also include heating from ambient temperature to between 150C and 350C at a temperature gradient of less than or equal to 3C per minute.
[0011] The method may include removing the semiconductor substrate from the oven in which the baking is performed when the semiconductor substrate may have cooled to less than 50C.
[0012] Baking the semiconductor substrate may also include heating in a nitrogen atmosphere.
[0013] A specific implementation of the chemical deposition method may include providing a semiconductor substrate; chemically depositing a metal layer on a pad included on a maximum planar surface of the semiconductor substrate; and baking the semiconductor substrate after the chemical deposition.
[0014] Specific implementations of the chemical deposition method may include one, all, or any of the following:
[0015] The method may include dicing the semiconductor substrate to form a plurality of semiconductor dies.
[0016] The semiconductor substrate may include silicon carbide.
[0017] The metal layer may include one of: nickel, palladium and gold; nickel and copper, or copper.
[0018] Baking the semiconductor substrate may also include heating from ambient temperature to between 150C and 350C at a temperature gradient of less than or equal to 3C per minute.
[0019] The method may include removing the semiconductor substrate from the oven in which the baking is performed when the semiconductor substrate may have cooled to less than 50C.
[0020] Baking the semiconductor substrate may also include heating in a nitrogen atmosphere.
[0021] A specific implementation of the chemical deposition method may include providing a semiconductor substrate including a first maximum planar surface and a second maximum planar surface; coupling a carrier to the first maximum planar surface; thinning the semiconductor substrate from the second maximum planar surface to form an edge ring; and forming a back metal layer on the second maximum planar surface. The method may include removing the carrier from the first maximum planar surface; chemically depositing a metal layer on a pad included on the first maximum planar surface and on the back metal layer; and baking the semiconductor substrate.
[0022] Specific implementations of the chemical deposition method may include one, all, or any of the following:
[0023] The method may include mounting a semiconductor substrate to a dicing tape, removing an edge ring, and dicing the semiconductor substrate to form a plurality of semiconductor dies.
[0024] The semiconductor substrate may include silicon carbide.
[0025] The metal layer may include one of: nickel, palladium and gold; nickel and copper, or copper.
[0026] Baking the semiconductor substrate may also include heating from ambient temperature to between 150° C. and 350° C. in a nitrogen atmosphere at a temperature gradient of less than or equal to 3° C. per minute.
[0027] The method may include removing the semiconductor substrate from the oven in which the baking is performed when the semiconductor substrate may have cooled to less than 50C.
[0028] The foregoing and other aspects, features and advantages will be apparent to those skilled in the art from the detailed description and accompanying drawings, and from the claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Specific implementations will be described below in conjunction with the accompanying drawings, in which like reference numerals represent like elements, and:
[0030] Figure 1 is a cross-sectional view of a specific implementation of a first semiconductor substrate;
[0031] Figure 2 After the back metal layer is formed Figure 1 a cross-sectional view of a semiconductor substrate;
[0032] Figure 3 During the baking operation Figure 2 a cross-sectional view of a semiconductor substrate;
[0033] Figure 4 is a cross-sectional view of a second semiconductor substrate;
[0034] Figure 5 After chemical deposition on the top side Figure 4 a cross-sectional view of a semiconductor substrate;
[0035] Figure 6 After the baking process Figure 5 a cross-sectional view of a semiconductor substrate;
[0036] Figure 7 After the back metal layer is formed Figure 6 a cross-sectional view of a semiconductor substrate;
[0037] Figure 8 It is prepared for the subsequent thinning operation. Figure 6 a cross-sectional view of a semiconductor substrate;
[0038] Fig. 9 is a cross-sectional view of a third semiconductor substrate;
[0039] Fig.10 After the tape is applied to the back side of the semiconductor substrate Fig. 9 a cross-sectional view of a semiconductor substrate;
[0040] Fig.11 After the chemical deposition process Fig.10 a cross-sectional view of a semiconductor substrate;
[0041] Fig.12 After removing the strip Fig.11 a cross-sectional view of a semiconductor substrate;
[0042] Fig.13 After the baking process Fig.12 a cross-sectional view of a semiconductor substrate;
[0043] Fig.14 It is prepared for processing using various additional processes before chemical deposition. Fig.13 a cross-sectional view of a semiconductor substrate;
[0044] Fig.15 After additional preparation processes are completed before chemical deposition Fig.14 a cross-sectional view of a semiconductor substrate;
[0045] Fig.16 After double-sided chemical deposition Fig.15 a cross-sectional view of a semiconductor substrate;
[0046] Fig.17 After the baking process Fig.16 a cross-sectional view of a semiconductor substrate;
[0047] Fig.18 is a cross-sectional view of a fourth semiconductor substrate;
[0048] Fig.19 After mounting the slide and performing the thinning operation Fig.18 a cross-sectional view of a semiconductor substrate;
[0049] Fig. 20 After the back metal layer is applied Fig.19 a cross-sectional view of a semiconductor substrate;
[0050] Fig.21 After removing the slide Fig. 20 a cross-sectional view of a semiconductor substrate;
[0051] Fig. 22 After additional processing steps to prepare the semiconductor substrate for chemical deposition Fig.21 a cross-sectional view of a semiconductor substrate;
[0052] Fig.23 After double-sided chemical deposition Fig. 22 a cross-sectional view of a semiconductor substrate; and
[0053] Fig.24 After the edge ring has been removed and installed on the cutting strip in preparation for cutting Fig.23 A cross-sectional view of a semiconductor substrate. DETAILED DESCRIPTION
[0054] The present disclosure, its aspects, and specific implementations are not limited to the specific components, assembly processes, or method elements disclosed herein. Many additional components, assembly processes, and / or method elements known in the art that are consistent with the intended method of chemical deposition will obviously be used with specific specific implementations of the present disclosure. Thus, for example, although the present invention discloses specific specific implementations, such specific implementations and implementation components may include any shape, size, style, type, model, version, measurement, concentration, material, quantity, method element, step, etc. known in the art for such chemical deposition and implementation components and methods that are consistent with the intended operation and method.
[0055] refer to Figure 1 , shows a specific implementation of a cross-sectional view of a portion of a semiconductor substrate 2 at a point in the manufacturing process. Although a portion of the semiconductor substrate 2 is shown, it should be understood that for multiple semiconductor devices / die included in the semiconductor substrate, Figure 1 The specific structure shown in the cross section of can be repeated in various semiconductor tube cores across the surface of the semiconductor substrate. In various method implementations, the semiconductor substrate 2 can be a silicon carbide substrate. The semiconductor substrate may also be any of a variety of semiconductor material types, including, by way of non-limiting example, silicon, silicon on insulator, ruby, sapphire, gallium arsenide, gallium nitride, or any other semiconductor material type. Here, the semiconductor wafer already has semiconductor devices formed therein, and various material layers are subsequently formed as part of the trimming process, and then the semiconductor devices are cut for processing during the packaging operation. Figure 1 In the illustrated implementation, an aluminum pad 4 is shown surrounded by a passivation material 6 (nitride, polyimide, etc.) formed on the front side or first large planar side 12 of the semiconductor substrate 2. A back metal layer 8 of aluminum is shown formed on the back side or second large planar side 10 of the semiconductor substrate 2. A protective tape 14 is shown coupled to the aluminum to prevent other metals from being deposited thereon.
[0056] Shown after electroless plating of top side metallization Figure 1In a semiconductor substrate embodiment, in which the top side metallization is various layers of nickel, palladium and gold using a chemical deposition process called electroless nickel palladium gold (ENEPIG). The process forms metal layers including layers of nickel, palladium and gold. However, in this and other embodiments disclosed herein, other metals may be chemically deposited together or in layers on the top side and / or back side, including, by way of non-limiting example, nickel and copper; copper; palladium; gold; nickel and palladium; nickel and gold; copper, nickel and gold; copper, nickel, palladium and gold; any combination thereof, or any other metal capable of being chemically plated onto the surface of a pad or subsequently plated layer. Figure 2 The semiconductor substrate 2 is shown after an additional back metal layer 16 of titanium, nickel, vanadium, and silver is deposited thereon after removing the strip 14 from the back metal layer 8. In some implementations, the additional back metal layer 16 can be chemically deposited or can be deposited using another process such as sputtering or electroplating.
[0057] Reference Figure 3 , showing a baking operation / process performed using an oven or other thermal heating device capable of enclosing a semiconductor substrate Figure 2 As shown, during the baking operation, degassing of the remaining plating chemistry occurs, as indicated by arrow 18. In various implementations, nitrogen is used to maintain a substantially oxygen-free atmosphere (less than 20 ppm oxygen) during baking in the oven. In some implementations, the atmosphere in the oven is static during baking, and in other implementations, such as during convection heating, the atmosphere in the oven is evacuated, changed, or circulated.
[0058] During the baking operation, in various methods, the temperature rises from the ambient temperature to 250°C at a rate of 3°C per minute. However, in other methods, the maximum temperature may be in the range between 150°C and 300°C. In various methods, the baking time at the highest temperature point may be about 15 minutes. In various methods, after reaching the highest temperature in the baking, the semiconductor substrate 2 is then cooled using a cooling rate substantially the same as the heating rate until reaching below 50°C. This heating rate and cooling rate and removing the semiconductor substrate below 50°C help reduce / prevent oxidation of various metal layers on the semiconductor substrate 2. The maximum baking temperature and the time spent at the maximum baking temperature may help improve the gap and avoid phase shift of one or more metal layers. For example, when the maximum baking temperature is 250°C, the problem of nickel layer phase shift is avoided.
[0059] The above-mentioned baking process after chemically depositing the metal layer on the semiconductor substrate can be used for a variety of chemical plating layers, and by non-limiting example, a variety of chemical plating layers include titanium nickel vanadium silver (TiNiVAg), copper, copper nickel gold (CuNiAu), aluminum, tin, tin alloy, or nickel. During or after the baking process, an additional protective layer can be applied to the chemical plating layer, and by non-limiting example, the additional protective layer includes, for example, nickel gold, nickel palladium, palladium, tin, tin palladium, solder, organic material, organic solderability protectant, or any combination thereof. The protective layer can be deposited by electroplating, sputtering, evaporation, screen printing, spin coating, or other deposition processes consistent with the specific material used. The baking process can be used for semiconductor substrates of various thicknesses, including thinned wafers (less than 125 microns thick). The baking process can be used to process various types of semiconductor devices, and by non-limiting example, semiconductor devices include silicon carbide devices, gallium nitride devices, insulated gate bipolar transistors (IGBITs), metal oxide field effect transistors (MOSFETs), or any other type of semiconductor devices. In the case of a thinned semiconductor substrate, as further described herein, the wafer may be supported using a carrier or support, ground or polished, or thinned during the process of forming an edge ring. A variety of back metal metallizations may be used in various implementations of the methods disclosed herein, including, by way of non-limiting example, aluminum, titanium nickel vanadium silver, nickel palladium gold, copper, nickel, any combination thereof, or any other desired metal material.
[0060] Various method implementations involving baking processes / operations may be formed using the principles disclosed herein.The various implementations disclosed in this document are purely for exemplary purposes of the present disclosure.
[0061] See also Figure 4 , shows a specific implementation of a semiconductor substrate 20 having an aluminum pad 22 formed thereon. The type of semiconductor substrate used in this specific implementation can be any type disclosed in this document. Figure 4 The embodiment shown uses an aluminum pad 22, but in various embodiments any of a variety of pad metallizations may be employed, where, by way of non-limiting example, various other pad metals include copper, aluminum copper, aluminum silicon, silver, gold, any combination thereof, or any other pad metallization type.
[0062] refer to Figure 5, shows the semiconductor substrate 20 after chemically depositing a metal layer 24 on the pad 22. Here, in the case of nickel-palladium-gold or copper-nickel-gold, the metal layer 24 includes three different material layers. However, in various implementations, the metal layer 24 can be any chemically deposited metal layer disclosed herein, and can be protected using any type of protective layer disclosed herein in various method implementations. In such implementations, the method can include forming / applying a protective layer after or before a baking operation.
[0063] Reference Figure 6 , shows the semiconductor substrate 20 after a baking process is performed on the metal layer 24, the baking process is used to remove / degas the remaining plating chemicals from the chemical deposition operation. The baking process in this specific implementation can be any baking process disclosed in this document. After the baking step, Figure 7 The semiconductor substrate 20 is shown after a back metal layer 26 is applied to the second maximum flat surface 28. The back metal layer 26 can be any back metal layer disclosed in this document. In the case where the back metal layer is applied using a chemical deposition process, if it is desired to vent / remove the plating chemicals from the back metal layer, the order of the baking process can be changed to be performed after the back metal layer is applied. In some method implementations, the back metal layer may not be formed. Because Figures 4 to 6 The semiconductor substrate 20 in FIG. 1 does not have a back metal layer formed thereon, so no protective measures such as a coating of the second large planar side 28 are employed during the chemical deposition process. Figure 8 The semiconductor substrate 20 is shown without the application of a back metal, wherein the second largest planar surface 28 remains exposed.
[0064] In such Figure 8 In the case where no back metal is applied, an additional substrate thinning operation can be performed using a carrier or edge ring process to thin the semiconductor substrate 20. After thinning, a back metal can then be added to the thinned semiconductor substrate 20, which can be any back metal layer type disclosed herein.
[0065] exist Figures 4 to 7 or Figures 4 to 6 and Figure 8 After the process shown in , the method implementation includes cutting the semiconductor substrate into a plurality of semiconductor dies. Cutting can be performed using any of a variety of cutting methods, including, by way of non-limiting example, sawing, laser action, water jet cutting, scribing, breaking, plasma etching, wet etching, any combination thereof, or any other method of separating semiconductor materials. In various method implementations and in other method implementations disclosed in this document, the semiconductor dies can be prepared for further packaging / assembly / testing processes using a probing operation before cutting and a placement / tape-and-reel die sorting operation after cutting.
[0066] refer to Fig. 9 , shows a specific implementation of the semiconductor substrate 30 after forming a back metal layer 32 on the second maximum flat surface 38 and forming a pad 34 on the first maximum flat surface 36. Because of the presence of the back metal layer 32, if an additional metal layer is to be deposited, in order to avoid depositing it on the back metal layer, a tape 40 is applied, such as Fig.10 With the tape 40 in place, the method includes chemically depositing a metal layer 42 on the pads 34 . Fig.11 4 shows the semiconductor substrate 30 after the chemical deposition process. In various method implementations, the metal layer 42 can be any chemically deposited layer disclosed herein, as can the pads be any pad type disclosed herein. After chemical deposition, the strip 40 is removed and the semiconductor substrate 30 is revealed, as shown in FIG. Fig.12 Next, the resulting semiconductor substrate 30 is baked using any of the baking processes disclosed herein, such as Fig.13 , which shows a semiconductor substrate 30 after baking and now ready to be cut using any of the cutting processes disclosed herein. Because the back metal is applied before the chemical deposition process, in this method implementation, any thinning of the semiconductor substrate 30 occurs before forming / applying the back metal layer 32.
[0067] Other method implementations may employ a metal back layer but not protect the metal back layer during chemical processing operations. Fig.14 , a semiconductor substrate 42 is shown having a back metal layer 44 applied to a second maximum flat surface 46 and a pad 48 formed on a first maximum flat surface 50. The back metal in this implementation is aluminum copper. Because the semiconductor substrate 42 has an applied back metal layer 44, any thinning operations have been completed. In this method implementation, a wafer pre-cleaning process is used, followed by a back metal annealing process, and then a double-sided ashing process to prepare the pad 48 and back metal layer 44 for chemical deposition. Fig.15 The resulting semiconductor substrate 42 is shown.
[0068] Fig.16 The semiconductor substrate 42 is shown after double-sided chemical deposition of metal layers 52, 54 on the pad 48 and the back metal layer 44, respectively. Fig.16 In the implementation shown, the metal layer includes three metal layers as in a nickel-palladium-gold or copper-nickel-gold metallization. However, any of the metal layer implementations disclosed herein that are compatible with the materials chemically deposited to pads 48 and back metal layer 44 may be utilized in various method implementations.
[0069] Fig.17The semiconductor substrate 42 is shown after a bake process for removing the plated chemistry from the metal layers 52, 54 on both sides of the substrate. At this point, the semiconductor substrate 42 is ready for a subsequent sawing operation, such as any sawing operation disclosed in this document.
[0070] Various method implementations disclosed herein may be used to apply copper to one or both sides of a semiconductor substrate using chemical deposition. Figures 18 to 24 A specific implementation of the method for applying copper using chemical deposition is shown. Fig.18 A semiconductor substrate 56 is shown including a pad 58 surrounded with a nitride 60 and a photosensitive polyimide material 62 that acts as a passivation material. Fig.18 In the specific implementation, the material of the pad 58 is aluminum silicon copper. Fig.18 , semiconductor substrate 56 is at full thickness, or in other words, at the full thickness so far in the process for processing during manufacturing operations.
[0071] refer to Fig.19 , shows the semiconductor substrate 56 after mounting a carrier 64 to the photosensitive polyimide material 62 located on the first large surface 66 of the substrate. A thinning operation has been performed, which has formed an edge ring 68 in the material of the semiconductor substrate 56. Although Fig.19 The use of edge ring 68 to support thinned semiconductor substrate 56 is shown, but in other method implementations, an edge ring may not be used and mechanical support for thinned semiconductor substrate 56 may come solely from carrier 64 .
[0072] In various specific implementations of the method, such as Fig. 20 As shown in , after thinning the semiconductor substrate 56, additional processing steps may be performed depending on the type of devices formed in the semiconductor substrate 56 and / or the material of the semiconductor substrate 56. By way of non-limiting example, these additional processing steps may include stress relief etching, reverse ion implantation into the thinned material of the semiconductor substrate 56, laser annealing, back metal formation, or any other desired processing of or from the thinned side (the second large planar side 70) of the semiconductor substrate 56. Here, in Fig. 20 In the illustrated implementation, a back metal layer 72 in the form of aluminum copper has been applied via sputtering to the second large planar side 70 in the form of a two-layer material. Although sputtering has been shown herein to be used to apply the back metal layer, wherein double-sided chemical deposition is employed, sputtering or another metal deposition process may be used to form a seed or barrier layer on the second large planar side 70 prior to chemical deposition.
[0073] Reference Fig.21, shows the semiconductor substrate 56 after the carrier 64 is removed / separated from the photosensitive polyimide 62. After removing the carrier 64, in various method implementations, additional processing steps may be used to clean the pads 58 and / or the back metal layer 72 for subsequent chemical deposition. By way of non-limiting example, these additional steps may include pre-cleaning (wet or dry), metal annealing, single-sided or double-sided metal ashing, any combination thereof, or any other processing of the metal layer or exposed material of the semiconductor substrate. Fig. 22 Semiconductor substrate 56 is shown after these additional processing steps.
[0074] refer to Fig.23 , shows a semiconductor substrate 56 after double-sided chemical deposition of copper layers 74, 76 on pads 58 and back metal layer 72, respectively. The chemical deposition process can be performed using any method disclosed in this document. After the chemical deposition process, a baking process similar to that disclosed in this document is used to remove any remaining plating chemicals and prepare the semiconductor substrate 56 for additional processing.
[0075] Reference Fig.24 , shows the semiconductor substrate 56 after the edge ring 68 is removed and mounted to the cutting tape 78 attached to the frame 80. The semiconductor substrate 56 is now ready for cutting using a sawing process or a combination of laser action / sawing or water jet cutting / sawing processes. However, in various method implementations, sawing may not be used and any of the other cutting methods may be employed alone or in combination.
[0076] The foregoing examples of using a baking process with a chemical deposition process for a variety of metal layers are merely illustrative. One of ordinary skill will readily understand how to utilize these principles to form many different metal layer combinations for many different semiconductor substrates and many different device types.
[0077] A specific implementation of the chemical deposition method includes dicing a semiconductor substrate to form a plurality of semiconductor dies.
[0078] Specific implementations of the chemical deposition method include the case where the semiconductor substrate is silicon carbide.
[0079] Specific implementations of the chemical deposition method may include where the metal layer is one of: nickel, palladium, and gold; nickel and copper; or copper.
[0080] Where the above description relates to specific embodiments of chemical deposition methods and implementation components, sub-components, methods and sub-methods, it should be apparent that various modifications may be made without departing from the essence thereof, and that these specific embodiments, implementation components, sub-components, methods and sub-methods may be applied to other chemical deposition methods.
Claims
1. A chemical deposition method, comprising: providing a semiconductor substrate, the semiconductor substrate comprising a first maximum planar surface and a second maximum planar surface; forming a back metal layer on the second largest flat surface; attaching a tape to the metal back layer; chemically depositing a metal layer on pads included on the first largest planar surface; After chemical deposition, removing the strip; as well as After removing the ribbon, the semiconductor substrate is baked.
2. The method of claim 1, wherein baking the semiconductor substrate further comprises heating from ambient temperature to between 150°C and 350°C in a nitrogen atmosphere at a temperature gradient of less than or equal to 3°C per minute.
3. The method of claim 2, further comprising removing the semiconductor substrate from an oven in which the baking is performed when the semiconductor substrate has cooled to less than 50°C.
4. A chemical deposition method, the method comprising: providing a semiconductor substrate; chemically depositing a metal layer on a pad included on the largest planar surface of the semiconductor substrate; as well as After chemical deposition, the semiconductor substrate is baked.
5. The method of claim 4, wherein the metal layer comprises one of: nickel, palladium, and gold; Nickel and copper, or copper.
6. The method of claim 4, wherein baking the semiconductor substrate further comprises heating from ambient temperature to between 150C and 350C in a nitrogen atmosphere at a temperature gradient of less than or equal to 3C per minute. 7 . The method of claim 6 , further comprising removing the semiconductor substrate from an oven in which the baking is performed when the semiconductor substrate has cooled to less than 50° C.
8. A chemical deposition method, comprising: providing a semiconductor substrate, the semiconductor substrate comprising a first maximum planar surface and a second maximum planar surface; coupling a slide to the first largest planar surface; thinning the semiconductor substrate from the second maximum planar surface to form an edge ring; forming a back metal layer on the second largest flat surface; removing the slide from the first largest planar surface; chemically depositing a metal layer on pads included on the first largest planar surface and on the back metal layer; and The semiconductor substrate is baked. 9 . The method of claim 8 , further comprising mounting the semiconductor substrate to a dicing tape, removing the edge ring, and dicing the semiconductor substrate to form a plurality of semiconductor dies.
10. The method of claim 8, wherein baking the semiconductor substrate further comprises heating from ambient temperature to between 150°C and 350°C in a nitrogen atmosphere at a temperature gradient of less than or equal to 3°C per minute, and removing the semiconductor substrate from the oven in which the baking is performed when the semiconductor substrate has cooled to less than 50°C.