Preparation method of flip chip and flip chip

By using the surface-defining components in flip chip welding to accept welding pressure, the circuit structure of the intermediate substrate is protected, the problem of the circuit being affected by pressure during flip chip welding is solved, and the consistency of the substrate spacing and chip performance are achieved. stability.

CN119069366AActive Publication Date: 2024-12-03ORIGIN QUANTUM COMPUTING TECH (HEFEI) CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202310640015.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-31
Publication Date
2024-12-03
Estimated Expiration
2043-05-31

Smart Images

  • Figure CN119069366A_ABST
    Figure CN119069366A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of a flip chip and the flip chip, and belongs to the technical field of flip chips. According to the flip chip preparation method provided by the invention, a first interconnection element is formed on a first substrate, a first sub-interconnection element is formed on a first surface of a middle substrate, a second sub-interconnection element and an acting surface limiting element are formed on a second surface of the middle substrate, and the height of the second sub-interconnection element does not exceed that of the acting surface limiting element; the second substrate forms a second interconnection element, and when the first surface of the middle substrate and the first substrate are welded and interconnected, the height of the second sub-interconnection element does not exceed the height of the acting surface limiting element, so that the acting surface limiting element receives pressure applied in the flip-chip bonding process; therefore, the circuit structure on the second surface can be prevented from being damaged or destroyed under the influence of pressure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of flip chip technology, especially the field of superconducting quantum chip technology. In particular, the present application relates to a method for preparing a flip chip and a flip chip. Background Art

[0002] Flip chip welding technology is a microelectronic circuit interconnection technology that interconnects the circuit structure located on the lower surface of a substrate with the circuit structure located on the upper surface of another substrate using solder to form a stable and reliable mechanical and electrical connection. The main process methods for flip chip welding are hot pressing welding.

[0003] The qubits on the quantum chip are the basic units for performing quantum computing. To achieve large-scale expansion of qubits, it is usually necessary to stack and interconnect the quantum circuits on the substrate through flip-chip welding technology. When three or more layers of substrates are flip-chip interconnected, the substrate in the middle needs to be welded twice to interconnect with the adjacent substrates. Since the circuit structure is formed on both surfaces of the substrate in the middle, how to apply pressure during the flip-chip welding process while avoiding the impact on the circuit needs to be solved urgently. Invention content

[0004] The purpose of the present application is to provide a method for preparing a flip chip and a flip chip to solve the deficiencies in the prior art.

[0005] An embodiment of the present application provides a method for preparing a flip chip, comprising:

[0006] forming a first interconnection element on a first substrate;

[0007] forming a first sub-interconnection element on a first surface of the intermediate substrate, and forming a second sub-interconnection element and an active surface defining element on a second surface of the intermediate substrate, wherein the height of the second sub-interconnection element does not exceed the active surface defining element;

[0008] forming a second interconnection element on the second substrate;

[0009] placing the first interconnection element opposite to the first interconnection element, and engaging the first interconnection element to the first interconnection element based on applying a force to the first substrate and the surface defined by the active surface defining element;

[0010] The second sub-interconnection element and the second interconnection element are opposed to each other, and the second sub-interconnection element and the second interconnection element are joined based on applying a force to the first substrate and the second substrate.

[0011] In the method described above, in some embodiments, the step of placing the second sub-interconnection element and the second interconnection element opposite to each other and bonding the second sub-interconnection element and the second interconnection element by applying force to the first substrate and the second substrate comprises:

[0012] Heating the second interconnection element at a first temperature and heating the second sub-interconnection element at a second temperature, wherein the first temperature is higher than the second temperature, and the second temperature is more than 10° C. lower than the melting point of both the first sub-interconnection element and the first interconnection element;

[0013] Applying a force engages the second sub-interconnection element and the second interconnection element.

[0014] In the method described above, in some embodiments, the first temperature is within 10° C. lower than the melting point of the second interconnection element.

[0015] In the method described above, in some embodiments, the second temperature is at least 10° C. lower than the melting point of the second interconnection sub-element and the first temperature.

[0016] In some embodiments of the method described above, the second interconnection element, the second sub-interconnection element, the first sub-interconnection element and the first interconnection element are all indium, and the first temperature is 150°C to 155°C, and the second temperature is 20°C to 30°C.

[0017] In some embodiments of the method described above, at least one of the following parameters of the first interconnection sub-element and the first interconnection element is greater than that of the second interconnection sub-element and the second interconnection element: cross-sectional area, quantity.

[0018] In some embodiments of the method described above, the step of placing the first interconnection sub-element opposite to the first interconnection element and bonding the first interconnection element to the first interconnection sub-element based on applying a force to the first substrate and the surface defined by the active surface defining element comprises:

[0019] heating the first sub-interconnection element and the first interconnection element at a third temperature;

[0020] Applying a force engages the first sub-interconnection element and the first interconnection element.

[0021] In the method described above, in some embodiments, the first interconnection element and the first interconnection element have the same melting point, and the third temperature is within 10° C. lower than the melting point.

[0022] Another embodiment of the present application provides a flip chip prepared according to the method as described above, comprising:

[0023] a first substrate formed with a first interconnection element;

[0024] An intermediate substrate, wherein a first sub-interconnection element is formed on a first surface of the intermediate substrate, a second sub-interconnection element and an active surface defining element are formed on a second surface of the intermediate substrate, the height of the second sub-interconnection element does not exceed the active surface defining element, and the first sub-interconnection element is oppositely engaged with the first interconnection element;

[0025] The second substrate is formed with a second interconnection element, and the second interconnection element is oppositely combined with the second sub-interconnection element.

[0026] Compared with the prior art, the present application provides a flip chip preparation method, in which the first substrate forms a first interconnection element, the first surface of the intermediate substrate forms a first sub-interconnection element, and the second surface of the intermediate substrate forms a second sub-interconnection element and an active surface defining element, and the height of the second sub-interconnection element does not exceed the active surface defining element, and the second substrate forms a second interconnection element. When the first surface of the intermediate substrate is welded and interconnected with the first substrate, since the height of the second sub-interconnection element does not exceed the active surface defining element, the active surface defining element receives the pressure applied during the flip-chip welding process, which helps to prevent the circuit structure on the second surface from being damaged or destroyed by the pressure. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 A schematic diagram of the structure of a three-layer substrate to be flip-chip welded in an embodiment provided in the present application;

[0028] Figure 2 A schematic diagram of the first flip chip bonding in an embodiment provided in the present application;

[0029] Figure 3 A schematic diagram of the second flip chip bonding in an embodiment provided in the present application;

[0030] Figure 4 A structural diagram of a flip chip in an embodiment provided in the present application.

[0031] Description of reference numerals:

[0032] 1-first substrate, 11-first interconnection element;

[0033] 2 - intermediate substrate, 21 - first sub-interconnection element, 22 - second sub-interconnection element, 23 - active surface defining element;

[0034] 3 - second substrate, 31 - second interconnection element. DETAILED DESCRIPTION

[0035] The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present application, and should not be construed as limiting the present application.

[0036] To make the purpose, technical scheme and advantages of the embodiments of the present application clearer, one or more embodiments are now described with reference to the accompanying drawings, wherein similar reference numerals throughout the text are used to refer to similar components. In the following description, for the purpose of explanation, many specific details are set forth in order to provide a more thorough understanding of one or more embodiments. However, it is clear that in various cases, one or more embodiments can be practiced without these specific details, and the various embodiments can be combined and referenced to each other without contradiction.

[0037] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable where appropriate, so that the embodiments of the present application described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0038] In addition, it should be understood that when a layer (or film), region, pattern or structure is referred to as being "on" a substrate, layer (or film), region and / or pattern, it can be directly on another layer or substrate, and / or there can also be intervening layers. In addition, it should be understood that when a layer is referred to as being "under" another layer, it can be directly under another layer, and / or there can also be one or more intervening layers. In addition, references to being "on" and "under" each layer can be made based on the accompanying drawings.

[0039] A quantum chip is a processor that performs quantum computing in a quantum computer. The circuit structure of the processing unit of the processor is usually called a quantum bit. A quantum bit can be understood as a two-level system that follows the laws of quantum mechanics. It can be in any superposition state of 0 and 1. There are many circuit structures with different functions around the quantum bit, such as the drive control signal line (xy-control line, also known as xy control line or pulse control signal line) for XY rotation of the quantum bit, the flux control signal line (z-control line, also known as z control signal line or frequency control signal line) for Z rotation of the quantum bit, the reading resonant cavity, and the coupler used for coupling connection between quantum bits. In a quantum chip, the circuit structure described above is generally referred to as a quantum circuit.

[0040] Traditional quantum circuits are all prepared on the same substrate, which results in very limited space on the substrate for forming quantum bits, making it difficult to expand the number of quantum bits on a large scale. In order to achieve large-scale expansion of quantum bits, the relevant technology classifies the quantum circuits located on the substrate and prepares them on different substrates, and then realizes stacking interconnection through flip chip welding technology. Flip chip welding (Flip Chip) technology is a microelectronic circuit interconnection technology that interconnects the circuit structure located on the lower surface of the substrate with the circuit structure located on the upper surface of another substrate with solder to form a stable and reliable mechanical and electrical connection. Compared with traditional wire bonding interconnection technology, flip chip welding technology has a higher density and can increase the number of I / Os per unit area. The preparation of flip chip bumps is basically based on wafers and chips. Compared with wire bonding interconnection based on a single wire, it has high production efficiency and reduces the cost of batch packaging.

[0041] When using flip-chip welding technology to stack and interconnect three or more substrates to expand the number of quantum bits, it is generally necessary to perform multiple welding to sequentially realize the stacking and interconnection between different layers, and the substrate in the middle needs to be welded twice to achieve interconnection with the adjacent substrate. However, circuit structures are formed on both surfaces of the middle substrate. How to apply pressure during the flip-chip welding process while avoiding affecting the circuit, such as causing deformation of the interconnection components or damage to other circuit structures, etc. These influences will further change the chip performance parameters. Therefore, it is urgent for technical personnel in this field to solve.

[0042] For a chip stacked by flip-chip welding of three or more substrates, in order to ensure that the circuit in the middle substrate is not affected by the pressure applied during the flip-chip welding process, the present application provides a method for preparing a flip-chip and a flip-chip.

[0043] Figure 1 A schematic diagram of the structure of a three-layer substrate to be flip-chip welded in an embodiment provided in the present application;

[0044] Figure 2 A schematic diagram of the first flip chip bonding in an embodiment provided in the present application;

[0045] Figure 3 A schematic diagram of the second flip chip bonding in an embodiment provided in the present application;

[0046] Figure 4 A structural diagram of a flip chip in an embodiment provided in the present application.

[0047] Combination Figures 1 to 4 As shown, an embodiment of the present application provides a method for preparing a flip chip, comprising the following steps:

[0048] A first interconnection element 11 is formed on the first substrate 1; a first sub-interconnection element 21 is formed on the first surface of the intermediate substrate 2, and a second sub-interconnection element 22 and an active surface defining element 23 are formed on the second surface of the intermediate substrate 2, and the height of the second sub-interconnection element 22 does not exceed the active surface defining element 23; a second interconnection element 31 is formed on the second substrate 3; it should be noted that the substrates can be made of dielectric materials such as silicon or sapphire, and the interconnection elements can be directly formed on the surface of the substrate or on the surface of the circuit structure located on the substrate, combined with Figure 1 As shown, the first interconnection element 11 is located on the top surface of the first substrate 11, the first sub-interconnection element 21 is located on the bottom surface of the intermediate substrate 2, the second sub-interconnection element 22 and the action surface defining element 23 are located on the top surface of the intermediate substrate 2, and the second interconnection element 31 is located on the bottom surface of the second substrate 3. It can be understood that the bottom and the top here are relative to the embodiment drawings provided in the present application. The height of the second sub-interconnection element 22 does not exceed the action surface defining element 23, and the height of the action surface defining element 23 does not affect the engagement of the second sub-interconnection element 22 and the second interconnection element 31. Therefore, the action surface defining element 23 can define a force action surface, which is higher than the second sub-interconnection element 22; and,

[0049] First, the first sub-interconnection element 21 and the first interconnection element 11 are placed one by one, and based on the force applied to the first substrate 1 and the surface defined by the active surface defining element 23, the first interconnection element 11 and the first sub-interconnection element 21 are joined; then, the second sub-interconnection element 22 and the second interconnection element 31 are placed one by one, and based on the force applied to the first substrate 1 and the second substrate 3, the second sub-interconnection element 22 and the second interconnection element 31 are joined.

[0050] A flip chip is a device that realizes stacked interconnection by using flip-chip welding technology, which includes at least three layers of stacked interconnected substrates, and the circuit structures on the two adjacent layers of substrates realize circuit interconnection by bonding interconnection elements. Therefore, the substrate in the middle position and the substrates above and below it all need to realize the interconnection of the circuit structure through interconnection elements. The flip chip preparation method provided by the present application, the first substrate 1 forms a first interconnection element 11, the first surface of the intermediate substrate 2 (the bottom surface of the intermediate substrate 2 as shown in the figure) forms a first sub-interconnection element 21 and the second surface of the intermediate substrate 2 (the top surface of the intermediate substrate 2 as shown in the figure) forms a second sub-interconnection element 22 and an action surface defining element 23, and the height of the second sub-interconnection element 22 does not exceed the action surface defining element 23, and the second substrate 3 forms a second interconnection element 31. When the first surface of the intermediate substrate 2 is welded and interconnected with the first substrate 1, since the height of the second sub-interconnection element 22 does not exceed the action surface defining element 23, the action surface defining element 23 receives the pressure applied during the flip-chip welding process, which helps to avoid the circuit structure on the second surface from being damaged or destroyed by the pressure.

[0051] It should be noted that, in the embodiment of the present application, in order to protect the second sub-interconnection element 22 from the influence of the pressure applied during the flip-chip welding process, the height of the second sub-interconnection element 22 can be set to be lower than the height of the action surface defining element 23, so the action surface defining element 23 can be a convex structure of any form. Exemplarily, the action surface defining element 23 can be a hole-shaped structure, and the second sub-interconnection element 22 is formed in the hole, and the height of the hole wall is higher than the second sub-interconnection element 22. In specific implementation, the hole can be formed by deep silicon etching on the silicon substrate, and then the second sub-interconnection element 22 is formed in the hole. When the pressure is applied during the flip-chip welding, the second sub-interconnection element 22 formed in the hole is not squeezed by force, so the integrity of the morphology can be maintained.

[0052] In some embodiments, the step of placing the second sub-interconnection element 22 and the second interconnection element 31 opposite to each other and joining the second sub-interconnection element 22 and the second interconnection element 31 based on the force applied to the first substrate 1 and the second substrate 3 includes: heating the second interconnection element 31 at a first temperature and heating the second sub-interconnection element 22 at a second temperature, wherein the first temperature is higher than the second temperature, and the second temperature is more than 10°C lower than the melting point of the first sub-interconnection element 21 and the first interconnection element 11, for example, the second temperature is 10°C, 11°C, 12°C, 12.5°C, 14°C... etc. lower than the melting point; applying force to join the second sub-interconnection element 22 and the second interconnection element 31.

[0053] See also Figure 3 And compare Figure 2 , Figure 1 As shown (relative to Figure 2 , Figure 1 , Figure 3 The end of the second interconnection element 31 is heated and wetted under the first temperature heating state, so it is distinguished in the figure). Since the heat provided by the first temperature can ensure that the second interconnection element 31 is heated and wetted, the wetting makes a part of the second interconnection element 31 close to the end tend to melt and have adhesion and atomic penetration ability, so that the second interconnection element 31 has the ability to bond with the second sub-interconnection element 22. The second interconnection element 31 and the second sub-interconnection element 22 are in contact with each other under the action of external force and generate friction. Due to the bonding ability described above, the second interconnection element 31 and the second sub-interconnection element 22 are bonded. In this process, the second temperature used is far away from the melting point of the first interconnection element 11 and the first sub-interconnection element 21, and is lower than the melting point by more than 10°C, which ensures that the conducted heat will not cause the first interconnection element 11 and the first sub-interconnection element 21 to soften and deform, and the bonding structure of the first interconnection element 11 and the first sub-interconnection element 21 still has a certain rigidity. Therefore, the preparation method of this embodiment avoids the morphological structure change of the bonding structure of the previous interconnection during flip-chip welding, which affects the performance parameters of the chip.

[0054] It should be noted that the method of providing the first temperature or the second temperature can be ultrasonic heating, or it can be flat plate heating, hot air heating, laser heating, etc. The specific implementation is not limited to the method described above, as long as it can achieve heating the second interconnection element 31 at the required first temperature and heating the second sub-interconnection element 22 at the required second temperature.

[0055] A commonly used process for flip chip welding is hot pressing welding. Figure 2 , Figure 3 As shown, the relative direction (such as Figure 2 , Figure 3 The working principle of hot-press flip-chip welding is: under certain pressure and temperature, ultrasonic energy is applied to the protruding element on one substrate (i.e., the interconnecting element described above), and within a certain period of time, the protruding element generates a binding force with the protruding element on the other substrate, thereby realizing the interconnection of the protruding elements of the two substrates. The interface bonding of the protruding elements in the hot-press welding method is a friction process, which first involves interface contact and pre-deformation, that is, under a given pressure, the protruding elements are in contact and are flattened and deformed to a certain extent; then, ultrasonic action is applied to remove the oxide and contamination layer on the surface of the protruding elements, and then the temperature rises sharply, the protruding elements are deformed, and the atoms of the protruding elements penetrate each other until they are within a certain range. Therefore, the key process parameters of hot-press flip-chip welding are pressure, temperature, ultrasonic power, and welding time.

[0056] The operation method of hot-press flip-chip welding is to place a substrate to be flip-chip welded on a wafer table, pick up another substrate with a protruding element with a pick-up welding head, and place the surface with the protruding element facing down to the substrate, and adjust the position so that the two substrates are parallel to each other and the welding positions are aligned. During flip-chip welding, the parallelism between the substrates is very important. If they are not parallel, the deformation of the protruding elements after welding will be large or small, resulting in high or low tensile strength, and some solder joints may not meet the use requirements. Therefore, parallelism is crucial to welding quality. During the ultrasonic hot pressing process, under the action of temperature and pressure, the protruding elements tend to melt, and the deformation that occurs in this process is very likely to tilt, which also causes the ultrasonic hot pressing flip-chip welding method to have a particularly serious impact on the consistency of the chip spacing.

[0057] In order to ensure that the second interconnection element 31 can achieve effective wetting when receiving the heat provided by the first temperature, in some embodiments of the present application, the first temperature is lower than the melting point of the second interconnection element 31 and is within 10°C lower, for example, 10°C, 9°C, 8°C, 8.5°C, 7°C, etc. lower than the melting point. A temperature close to the melting point but not reaching the melting point can make the second interconnection element 31 wetted and tend to melt. It should be noted that wetting means that the part close to the surface has melted and forms an adhesion layer on the surface of the parent material with the help of capillary force, and the atoms of the melted part and the parent material are close to each other and reach a distance where the atomic attraction acts.

[0058] In some embodiments, when the preparation method described above is implemented, the second temperature is lower than the melting point of the second sub-interconnection element 22 and the first temperature, and is more than 10°C lower. In specific implementation, it can be 10°C, 11°C, 12°C, 12.5°C, 14°C, etc. lower than the melting point and the first temperature of the second sub-interconnection element 22, thereby forming a sufficiently large temperature gradient in the direction from the second sub-interconnection element 22 to the first interconnection element 11. The sufficiently large temperature gradient further ensures that the bonding structure formed by the interconnection of the first interconnection element 11 and the first sub-interconnection element 21 does not deform.

[0059] In some embodiments, the second interconnection element 31, the second sub-interconnection element 22, the first sub-interconnection element 21, and the first interconnection element 11 are all superconductors. The superconductor may be formed of a superconductor material that exhibits superconducting properties at a temperature equal to or lower than a critical temperature, such as about 10-100 millikelvin (mK) or about 4K, such as aluminum, niobium, tantalum, or titanium nitride, etc., and is not limited to these materials in specific implementations. Any material that exhibits superconducting properties at a temperature equal to or lower than the critical temperature can be used to form the superconductor. In some implementation examples, the second interconnection element 31, the second sub-interconnection element 22, the first sub-interconnection element 21 and the first interconnection element 11 are all indium (the melting point is 157°C), and the first temperature is 150°C to 155°C (in specific implementation, one of the values ​​of 150°C, 151°C, 152°C, 153°C, 154°C, 155°C, etc. can be selected), and the second temperature is 20°C to 30°C (in specific implementation, one of the values ​​of 20°C, 21°C, 23°C, 25°C, 28°C, 30°C, etc. can be selected). In a preferred example, the first temperature is selected as 155°C and the second temperature is selected as 20°C. At this time, the second sub-interconnection element 22 and the second interconnection element 31, which are both indium, can be bonded with high quality, and in this process, the bonding structure formed by the interconnection of the first interconnection element 11 and the first sub-interconnection element 21 is not deformed.

[0060] In order to prevent the substrate from being tilted relative to each other due to the pressing force in the subsequent flip-chip welding process. In some embodiments, at least one of the following parameters of the first interconnection element 21 and the first interconnection element 11 is greater than that of the second interconnection element 22 and the second interconnection element 31: cross-sectional area, quantity. In one example, specifically, the cross-sectional area of ​​the first interconnection element 21 and the first interconnection element 11 at any point is greater than that of the second interconnection element 22 and the second interconnection element 31, so as to increase the compressive strength of the interconnection element previously joined. It should be noted that the cross section is perpendicular to the joining direction of the first interconnection element 11 and the first interconnection element 21, and the cross-sectional area of ​​the first interconnection element 11 is greater than that of the second interconnection element 22 and the second interconnection element 31. Figure 1 , Figure 2 and Figure 3 In one example, specifically, the number of the first interconnection elements 21 and the first interconnection elements 11 is greater than the number of the second interconnection elements 22 and the second interconnection elements 31, so as to increase the overall compressive strength of the interconnection elements previously joined to ensure the stability of the spacing between the first substrate 1 and the intermediate substrate 2.

[0061] In some embodiments, the step of placing the first interconnection element 21 and the first interconnection element 11 opposite to each other and bonding the first interconnection element 11 and the first interconnection element 21 based on applying force to the first substrate 1 and the surface defined by the action surface defining element 23 is a step of prior flip-chip welding, which includes: heating the first interconnection element 21 and the first interconnection element 11 at a third temperature; applying force to bond the first interconnection element 21 and the first interconnection element 11. In the specific implementation of the step of prior flip-chip welding, the first interconnection element 21 and the first interconnection element 11 can be made of a material different from the second interconnection element 22 and the second interconnection element 31, so as to facilitate heating at a third temperature different from the first temperature during flip-chip welding, as long as the third temperature is lower than the melting point of the first interconnection element 21 and the first interconnection element 11, and is within 10°C lower. In some embodiments, the first interconnection element 21 and the first interconnection element 11 have the same melting point.

[0062] Another embodiment of the present application provides a flip chip prepared according to the method described above, see Figure 4 The flip chip comprises: a first substrate 1, formed with a first interconnection element 11; an intermediate substrate 2, a first surface of the intermediate substrate 2 is formed with a first sub-interconnection element 21, a second surface of the intermediate substrate 2 is formed with a second sub-interconnection element 22 and an active surface defining element 23, the height of the second sub-interconnection element 22 does not exceed the active surface defining element 23, and the first sub-interconnection element 21 is oppositely bonded to the first interconnection element 11; a second substrate 3, formed with a second interconnection element 31, and the second interconnection element 31 is oppositely bonded to the second sub-interconnection element 22.

[0063] The above flip chip has a multi-layer stacked substrate, and the spacing consistency of the substrate is high, the performance parameters of the chip are stable, and the process is easy to prepare, and has the same or similar beneficial effects as the above preparation method embodiment, so it is not repeated here. For the technical details not disclosed in the flip chip embodiment of this application, technicians in this field please refer to the description of the above preparation method for understanding, and in order to save space, it will not be repeated here.

[0064] The above describes in detail the structure, features and effects of the present application based on the embodiments shown in the drawings. The above is only a preferred embodiment of the present application, but the present application does not limit the scope of implementation to what is shown in the drawings. Any changes made in accordance with the concept of the present application, or modifications to equivalent embodiments with equivalent changes, which still do not exceed the spirit covered by the description and drawings, should be within the protection scope of the present application.

Claims

1. A method for preparing a flip chip, characterized in that: include: forming a first interconnection element on a first substrate; forming a first sub-interconnection element on a first surface of the intermediate substrate, and forming a second sub-interconnection element and an active surface defining element on a second surface of the intermediate substrate, wherein the height of the second sub-interconnection element does not exceed the active surface defining element; forming a second interconnection element on the second substrate; placing the first interconnection element opposite to the first interconnection element, and engaging the first interconnection element to the first interconnection element based on applying a force to the first substrate and the surface defined by the active surface defining element; The second sub-interconnection element and the second interconnection element are opposed to each other, and the second sub-interconnection element and the second interconnection element are joined based on applying a force to the first substrate and the second substrate.

2. The method according to claim 1, characterized in that The step of placing the second sub-interconnection element and the second interconnection element opposite to each other and bonding the second sub-interconnection element and the second interconnection element based on applying force to the first substrate and the second substrate comprises: Heating the second interconnection element at a first temperature and heating the second sub-interconnection element at a second temperature, wherein the first temperature is higher than the second temperature, and the second temperature is more than 10° C. lower than the melting point of both the first sub-interconnection element and the first interconnection element; Applying a force engages the second sub-interconnection element and the second interconnection element.

3. The method according to claim 2, characterized in that The first temperature is within 10° C. lower than a melting point of the second interconnect element.

4. The method according to claim 2 or 3, characterized in that: The second temperature is lower than both the melting point of the second interconnection sub-element and the first temperature by more than 10°C.

5. The method according to claim 2 or 3, characterized in that: The second interconnection element, the second sub-interconnection element, the first sub-interconnection element and the first interconnection element are all indium, and the first temperature is 150°C to 155°C, and the second temperature is 20°C to 30°C.

6. The method according to claim 1, characterized in that At least one of the following parameters of the first sub-interconnection element and the first interconnection element is greater than that of the second sub-interconnection element and the second interconnection element: cross-sectional area, quantity.

7. The method according to claim 1, characterized in that The step of placing the first interconnection sub-element opposite to the first interconnection element and bonding the first interconnection element to the first interconnection sub-element based on applying force to the first substrate and the surface defined by the active surface defining element comprises: heating the first sub-interconnection element and the first interconnection element at a third temperature; Applying a force engages the first sub-interconnection element and the first interconnection element.

8. The method according to claim 7, characterized in that The first sub-interconnection element and the first interconnection element have the same melting point, and the third temperature is within 10° C. lower than the melting point.

9. A flip chip prepared according to the method according to any one of claims 1 to 8, characterized in that: include: a first substrate formed with a first interconnection element; An intermediate substrate, wherein a first sub-interconnection element is formed on a first surface of the intermediate substrate, a second sub-interconnection element and an active surface defining element are formed on a second surface of the intermediate substrate, the height of the second sub-interconnection element does not exceed the active surface defining element, and the first sub-interconnection element is oppositely engaged with the first interconnection element; The second substrate is formed with a second interconnection element, and the second interconnection element is oppositely combined with the second sub-interconnection element.

Citation Information

Patent Citations

  • Chip for double-sided indium inverted pile interconnection and preparation method thereof

    CN114783896A

  • Semiconductor element fixing method

    JP1998270497A

  • Semiconductor device manufacturing method, semiconductor wafer with adhesive layer manufacturing method, semiconductor wafer with semiconductor element manufacturing method and semiconductor wafer laminate manufacturing method

    JP2012238704A

  • Manufacturing method for semiconductor device

    JP2021129052A

  • Microelectronic packages and methods therefor

    US20050181544A1