Coating-integrated negative plate strip-shaped interval pre-lithiation device and method

By using a strip-shaped space prelithiation device for coating an integrated negative electrode sheet in a lithium-ion battery, the liquid metal lithium is coated into an ultra-thin lithium film and rolled onto the electrode sheet, the lithium-ion battery is solved for the first time charging. The problem of reducing energy density during discharge has achieved precise control of lithium supplementation and improved production efficiency.

CN119069649APending Publication Date: 2024-12-03CHINA ENERGY LITHIUM
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202310631507.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-31
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The solid electrolyte interface film formed by the lithium-ion battery during the first charging and discharging process consumes lithium ions, resulting in a decrease in energy density. In the prior art, excessive metal lithium film and uneven compression of the electrode sheet lead to a decrease in performance.

Method used

The liquid metal lithium is coated into an ultra-thin lithium film and is transferred to the electrode sheet by rolling the strip spacer to accurately control the lithium supplementation amount to avoid excessive metal lithium and Extreme sheet leaks.

Benefits of technology

It realizes precise control of lithium ion lithium replenishment, improves the energy density of lithium batteries, increases product qualification rate, and reduces production costs and waste of metal lithium.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069649A_ABST
    Figure CN119069649A_ABST
Patent Text Reader

Abstract

The invention discloses a coating integrated negative plate strip-shaped interval pre-lithiation device and method, and the device comprises a base film unwinding mechanism and a base film winding mechanism which are respectively used for unwinding and winding a base film; the coating assembly is used for producing a first lithium film and a second lithium film; the first pole piece unwinding mechanism, the second pole piece unwinding mechanism, the first pole piece winding mechanism and the second pole piece winding mechanism are respectively used for unwinding and winding the first pole piece and the second pole piece; the first film covering device is used for transferring and covering the metal lithium layers on the first lithium film and the second lithium film to the first pole piece in a striping and spaced manner; and the second film covering device is used for transferring and covering the residual metal lithium layers on the first lithium film and the second lithium film to the second pole piece. According to the invention, the coated lithium film can be pressed on the negative plate at intervals in a strip-shaped manner, so that the lithium supplementing amount is accurately controlled, and the problem of excessive metal lithium is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of battery manufacturing technology, in particular to the field of lithium battery technology, and specifically to a device and method for pre-lithiation of an integrally coated negative electrode strip interval. Background Art

[0002] Lithium-ion batteries have become one of the most widely used secondary batteries due to their advantages of high specific energy, small size and long cycle life. With the continuous development of high-power, high-energy devices such as electronic devices and electric vehicles, the demand for the energy density of lithium-ion batteries is getting higher and higher. During the first charge and discharge process of lithium-ion batteries, a layer of solid electrolyte interface (SEI) covering the surface of the electrode material will be formed. The production of the SEI film consumes part of the lithium ions from the positive electrode, which leads to an irreversible decrease in the energy density of the lithium-ion battery during the first charge and discharge process. In order to improve this problem, a layer of metal lithium film is usually pressed on the negative electrode in advance to increase the energy density of the lithium-ion battery.

[0003] At present, due to process problems, the thinnest metal lithium film usually produced is about 5μm, and there is a problem of excessive metal lithium when it is directly used in batteries for lithium replenishment. The patent application document with patent number CN114709374A discloses a press-coated integrated negative electrode sheet lithium replenishment device and lithium replenishment method. When the lithium strip is rolled, the oil is applied. The coated oil is inevitably introduced into the lithium-ion battery, which inevitably affects the battery performance; on the other hand, when the lithium strip is pressed on the pole piece, the two sides of the pole piece are laminated in batches, resulting in the pole piece being rolled twice, which increases the possibility of wrinkling of the pole ear and damage to the copper foil inside the pole piece.

[0004] In view of this, the present invention provides a negative electrode sheet strip-shaped pre-lithiation device and method with integrated coating, which avoids the problem of excessive metal lithium by pressing the lithium film formed after coating onto the negative electrode sheet in strip-shaped intervals. In addition, by controlling the lithium film base film, the metal lithium is easily peeled off from the base film and then transferred and coated onto the electrode sheet, avoiding the situation of electrode sheet leakage and greatly increasing the product qualification rate. Summary of the invention

[0005] The present invention provides a device and method for pre-lithiation of negative electrode strips with an integrated coating, through which liquid metal lithium can be coated on a base film to form an ultra-thin lithium film at the micron level, and the ultra-thin lithium film strips are transferred to two rolls of battery pole pieces, forming multiple lithium strips with strip spacing at the micron level on each pole piece, which can more accurately control the total amount of lithium replenishment to the negative electrode piece. The method and device of the present invention can be mass-produced, continuous, and roll-to-roll, and play a decisive role in accurately controlling the amount of lithium replenishment in the pre-lithiation process of the lithium battery industry.

[0006] The purpose of the present invention is to provide a device and method for pre-lithiation of negative electrode sheets with strip intervals coated in one piece, by rolling the ultra-thin metal lithium film formed after coating twice, and transferring the strip intervals to two rolls of electrode sheets to be pre-lithiated, so as to achieve the purpose of accurately controlling the amount of lithium replenished in the pre-lithiation process and improving production efficiency.

[0007] The purpose of the present invention can be achieved through the following technical solutions.

[0008] The present invention provides a negative electrode strip spacer pre-lithiation device with an integrated coating, comprising:

[0009] A base film unwinding mechanism, the base film unwinding mechanism includes a first base film unwinding mechanism and a second base film unwinding mechanism, which are respectively used to unwind the first base film and the second base film; a coating mechanism, the coating mechanism includes a first coating mechanism and a second coating mechanism, which are used to coat liquid metal lithium on the first base film and the second base film, respectively, to form a first lithium film and a second lithium film; a first pole piece unwinding mechanism, which is used to unwind the first pole piece; a first coating device, which is used to transfer and coat the metal lithium layers on the first lithium film and the second lithium film to the first pole piece in strips and intervals at the same time, to obtain a first pre-lithiation pole piece, wherein the metal lithium layer on the first lithium film and the metal lithium layer on the second lithium film are respectively transferred and coated on the upper and lower surfaces of the first pole piece On the surface; a first pole piece winding mechanism, used to wind up the first pre-lithiation pole piece after pre-lithiation; a second pole piece unwinding mechanism, used to unwind the second pole piece; a second coating device, used to transfer and laminate the remaining metal lithium layers on the first lithium film and the second lithium film to the second pole piece to obtain a second pre-lithiation pole piece, wherein the remaining metal lithium layer on the first lithium film and the remaining metal lithium layer on the second lithium film are transferred and laminated to the upper and lower surfaces of the second pole piece respectively; the second pole piece winding mechanism, used to wind up the second pre-lithiation pole piece; and a base film winding mechanism, the base film winding mechanism includes a first base film winding mechanism and a second base film winding mechanism, which are respectively used to wind up the first base film and the second base film after use.

[0010] Optionally, the coating mechanism includes a coating head and a backing roller.

[0011] Optionally, the back roller has a cooling function.

[0012] Optionally, the first coating device comprises a first coating roller and a second coating roller; wherein a working area of ​​at least one of the first coating roller and the second coating roller has a strip-shaped interval.

[0013] Optionally, the strip-shaped intervals are evenly distributed concave-convex intervals with clear boundaries, and the size of the concave-convex intervals is 1 mm-10 mm.

[0014] Optionally, only one of the first coating roller and the second coating roller has a concave-convex interval, and the width of the concave part and the convex part is 1mm-10mm, preferably 3-5mm.

[0015] Optionally, both the first coating roller and the second coating roller have concave-convex intervals, and the corresponding relationship between the two concave-convex intervals is convex to convex, and concave to concave.

[0016] Optionally, the cross-sectional shape of the concave portion of the laminating roller having the strip-shaped intervals is rectangular.

[0017] Optionally, the cross-sectional shape of the concave portion of the coating roller with the strip-shaped intervals is semicircular or groove-shaped with an arc-shaped bottom.

[0018] Optionally, at least one of a supporting roller mechanism, a tension detection mechanism, and a tension control mechanism is further arranged between the coating device and the first laminating device.

[0019] Optionally, at least one of a peeling mechanism, a supporting roller mechanism, a tension detection mechanism and a tension control mechanism is further provided downstream of the first laminating device and / or the second laminating device.

[0020] The present invention also provides a method for pre-lithiation of negative electrode strips, comprising: coating liquid metal lithium onto a base film through the above-mentioned integrated negative electrode strip pre-lithiation device to form an ultra-thin lithium film with a metal lithium layer of micrometer thickness, and transferring the metal lithium layer in strips to two rolled battery pole pieces, forming a plurality of lithium strips with strip spacings at micrometer level on each pole piece.

[0021] Optionally, first, liquid metal lithium is coated on the first base film and the second base film respectively to form two micron-level ultra-thin lithium films, and the thickness of the lithium layer on the ultra-thin lithium film is 3μm to 20μm; secondly, the ultra-thin lithium films formed by coating are respectively set on the two sides of the first pole piece, and a first coating device with a strip-spaced coating roller is used to roll the ultra-thin lithium film strips to the first pole piece; thirdly, a second coating device is used to roll the remaining lithium film (strip-spaced lithium film) and the second pole piece after the first coating device is rolled, so that the remaining strip-spaced lithium film is transferred to the second pole piece.

[0022] Optionally, the lithium film comprises a base film and a metallic lithium layer; wherein a side of the base film in contact with the metallic lithium layer is further provided with a coating, and the coating is provided on the base film so that the metallic lithium layer can be easily peeled off from the base film.

[0023] Optionally, the base film includes polyethylene terephthalate (PET), biaxially oriented polypropylene film (BOPP), polyimide (PI), or polytetrafluoroethylene (PTFE).

[0024] Optionally, the coating material includes silicone oil, fluoride, or mineral oil.

[0025] Optionally, the base film is subjected to plasma treatment or corona treatment before coating the coating material, and is heated and / or cured after coating, so that the coating material is firmly bonded to the base film and the coating material is prevented from detaching.

[0026] Optionally, the temperature of the liquid metal lithium is 180°C to 500°C, preferably 200°C to 260°C.

[0027] Optionally, when liquid metal lithium is coated to form a micron-sized ultra-thin lithium film, an inert gas (such as argon) is also mixed, so that the coated metal lithium layer has micropores, and the maximum size of the micropores is less than 1 mm, which is called a microporous lithium film; the lithium loading is further reduced.

[0028] The technical solution of the present invention has at least one of the following advantages:

[0029] 1. Maintaining the high temperature of liquid lithium metal reduces the tension of lithium metal, making the thickness of the lithium film formed after coating more uniform than that produced by conventional rolling scheme.

[0030] 2. The ultra-thin lithium film formed after coating is pressed onto the negative electrode sheet in the form of strip intervals, avoiding the problem of excessive metallic lithium.

[0031] 3. By controlling the type of lithium membrane base film coating material, metallic lithium can be easily peeled off from the base film and then transferred to the electrode, avoiding the leakage of the electrode and greatly increasing the product qualification rate.

[0032] 4. Liquid metal lithium is directly coated on the base film to form an ultra-thin lithium film, which is then transferred in strips and laminated on the two pole pieces. It has a high degree of automation, no waste of metal lithium, low production cost and high efficiency.

[0033] 5. The technical solution of the present invention has a simple and easy structure and adopts a roll-to-roll solution, which can be produced in batches quickly. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 is a schematic diagram of a specific embodiment of the present invention.

[0035] Figure 2 This is a specific embodiment in which the cross-sectional shape of the concave portion of the laminating roller having strip-shaped intervals is a rectangle.

[0036] Figure 3 This is a specific embodiment in which the cross-sectional shape of the concave portion of the laminating roller having strip-shaped intervals is an arc shape.

[0037] Figure 4 This is a picture of the strip-shaped spacer lithium film after being rolled by the first coating device.

[0038] Figure 5 This is a picture of the electrode after pre-lithiation using the method of the present invention.

[0039] Description of reference numerals:

[0040] 10 rack; 11 lithium source; 12 first feed pump; 13 first lithium liquid control valve; 14 second feed pump; 15 second lithium liquid control valve; 16 gas source; 17 first gas control valve; 18 second gas control valve; 19 first coating pipeline; 20 second coating pipeline; 21 first coating head; 22 second coating head; 23 first back roller; 24 second back roller; 25 first base film unwinding mechanism; 251 first base film unwinding shaft; 26 second base film unwinding mechanism; 261 second base film unwinding shaft; 27 first pole piece unwinding mechanism; 271 first pole piece unwinding shaft; 28 first pole piece rewinding mechanism; 281 first pole piece rewinding shaft; 29 second pole piece unwinding mechanism; 291 second pole piece Reel; 30 second pole piece reeling mechanism; 301 second pole piece reeling shaft; 31 first base film reeling mechanism; 311 first base film reeling shaft; 32 second base film reeling mechanism; 321 second base film reeling shaft; 33 first coating device; 331 first coating roller; 332 second coating roller; 333 concave portion; 334 convex portion; 34 second coating device; 341 third coating roller; 342 fourth coating roller; M10 first base film; M20 second base film; M11 first lithium film; M21 second lithium film; M12 first strip spacer lithium film; M22 second strip spacer lithium film; P1 first pole piece; P11 first pre-lithiation pole piece; P2 second pole piece; P21 second pre-lithiation pole piece. DETAILED DESCRIPTION

[0041] The specific embodiments of the present invention are described below. It should be understood that those skilled in the art can conceive of other various embodiments and can modify them according to the teachings of this disclosure without departing from the scope or spirit of the present invention. Therefore, the following specific embodiments are not intended to be limiting.

[0042] In the description of the present invention, it should be understood that the terms "first", "second", "upper", "lower", etc. are only used to facilitate the description of the present invention and simplify the description, and therefore cannot be understood as limiting the present invention.

[0043] A specific embodiment of the negative electrode strip spacer pre-lithiation device with integrated coating is described in detail below with reference to the accompanying drawings.

[0044] refer to Figures 1 to 3 In this embodiment, the integrated negative electrode strip spacer pre-lithiation device includes:

[0045] Frame 10; lithium source 11; gas source 16;

[0046] The first lithium film coating forming device includes: a first feed pump 12, a first lithium liquid control valve 13, a first gas control valve 17, a first coating pipeline 19, a first coating head 21, a first back roller 23 and a first base film unwinding mechanism 25; the first base film unwinding mechanism 25 also includes a first base film unwinding shaft 251, wherein the first base film M10 is installed on the first base film unwinding shaft 251, and is unwound by the first base film unwinding mechanism 25 and then bypasses the first back roller 23; the first feed pump 12 is used to pump the liquid metal lithium in the lithium source 11 into the first coating head 21 through the first coating pipeline 19, so as to coat it on the first base film M10; because the first base film M10 is tightly fitted with the first back roller 23, the first back roller 23 can quickly cool the liquid metal lithium coated on the first base film M10 to form an ultra-thin metal lithium layer, thereby forming a first lithium film M11. Optionally, an inert gas is mixed into the liquid metal lithium pumped into the first coating pipeline 19, and the gas is provided by a gas source 16. The content of the gas mixed in the liquid metal lithium can be adjusted by controlling the first feed pump 12, the first lithium liquid control valve 13 and the first gas control valve 17, so that the first lithium film M11 formed after coating has discontinuous micropores, further reducing the lithium loading per unit area.

[0047] The second lithium film coating forming device includes: a second feed pump 14, a second lithium liquid control valve 15, a second gas control valve 18, a second coating pipeline 20, a second coating head 22, a second back roller 24 and a second base film unwinding mechanism 26; the second base film unwinding mechanism 26 also includes a second base film unwinding shaft 261, wherein the second base film M20 is installed on the second base film unwinding shaft 261, and is unwound by the second base film unwinding mechanism 26 and then bypasses the second back roller 24; the second feed pump 14 is used to pump the liquid metal lithium in the lithium source 11 into the second coating head 22 through the second coating pipeline 20, so as to coat it on the second base film M20; because the second base film M20 is in close contact with the second back roller 24, the second back roller 24 can quickly cool the liquid metal lithium coated on the second base film M20 to form an ultra-thin metal lithium layer, thereby forming a second lithium film M21. Optionally, an inert gas is mixed into the liquid metal lithium pumped into the second coating pipeline 20, and the gas is provided by the gas source 16. The content of the gas mixed in the liquid metal lithium can be adjusted by controlling the second feed pump 14, the second lithium liquid control valve 15 and the second gas control valve 18, so that the second lithium film M21 formed after coating has discontinuous micropores, further reducing the lithium loading per unit area.

[0048] The first pole sheet unwinding mechanism 27 and the first pole sheet rewinding mechanism 28, wherein the first pole sheet unwinding mechanism 27 comprises a first pole sheet unwinding shaft 271 for unwinding the first pole sheet P1; the first pole sheet rewinding mechanism 28 comprises a first pole sheet rewinding shaft 281 for rewinding the first pre-lithiation pole sheet P11 formed after the first pole sheet P1 is pre-lithiation.

[0049] The second pole sheet unwinding mechanism 29 and the second pole sheet winding mechanism 30, the second pole sheet unwinding mechanism 29 includes a second pole sheet unwinding shaft 291, which is used for unwinding the second pole sheet P2; the second pole sheet winding mechanism 30 includes a second pole sheet winding shaft 301, which is used for winding the second pre-lithiation pole sheet P21 formed after the second pole sheet P2 is pre-lithiation.

[0050] The first base film winding mechanism 31 includes a first base film winding shaft 311 for winding the first base film M10.

[0051] The second base film winding mechanism 32 includes a second base film winding shaft 321 for winding the second base film M20.

[0052] The first coating device 33 comprises a first coating roller 331 and a second coating roller 332 which are arranged opposite to each other, and at least one of the first coating roller 331 and the second coating roller 332 has a concave-convex strip-shaped interval on its working surface, that is, a plurality of concave portions 333 and convex portions 334 are arrayed in the axial direction.

[0053] The second coating device 34 comprises a third coating roller 341 and a fourth coating roller 342 which are arranged opposite to each other, and the third coating roller 341 and the fourth coating roller 342 are both conventional cylindrical roller surfaces, that is, the roller surfaces have no concave-convex strip intervals.

[0054] In this embodiment, in the first coating device 33, preferably, only one of the first coating roller 331 and the second coating roller 332 has a concave-convex strip-shaped interval on its working surface, and the other coating roller is a conventional cylindrical roller surface (for example, the first coating roller 331 is a roller with a concave-convex strip-shaped interval, and the second coating roller 332 is a roller with a conventional cylindrical roller surface). The cross-sectional shape of the concave portion of the first coating roller 331 is preferably a rectangle (such as Figure 2 as shown) or arc-shaped (as Figure 3 As shown), the width of the concave portion is 1-10mm, the depth is not limited (can be 0.1-10mm), the width of the convex portion is 1-10mm, and preferably the width of the concave portion is the same as the width of the convex portion (for example, the width of the concave portion is 5mm, and the width of the convex portion is 5mm).

[0055] The specific working principle and process of the coated integrated negative electrode strip spacer pre-lithiation device of the present invention are as follows:

[0056] The first base film M10 is mounted on the first base film unwinding shaft 251 in the first base film unwinding mechanism 25, so that the first base film M10 is passed around the first back roller 23; the first back roller 23 has a cooling function, and the temperature of the first back roller 23 is controlled to be -50°C to 20°C, preferably -30°C to -10°C. The temperature of the liquid metal lithium in the lithium source 11 is controlled to be greater than 180°C, preferably 200°C to 260°C; the gas in the gas source 16 is an inert gas, preferably argon, and the output pressure is controlled to be less than 2MPa, preferably 0.2MPa to 0.5MPa. The first lithium liquid control valve 13 is adjusted, and the first feed pump 12 is started to pump the liquid metal lithium in the lithium source 11 into the first coating head 21 through the first coating pipe 19; the liquid metal lithium in the first coating head 21 is forced to be extruded from the slit and coated on the first base film M10 due to the pressure of the first feed pump 12, and the liquid metal lithium on the first base film M10 is instantly solidified on the first base film M10 due to the extremely low temperature of the first back roller 23, forming the first lithium film M11. The thickness of the metal lithium layer on the first lithium film M11 can be controlled by adjusting the size of the slit of the first coating head 21 and the tape speed of the first base film M10, and the thickness of the lithium layer can be controlled to be 3μm to 20μm. After stable coating, the first gas control valve 17 is opened and adjusted to allow a certain amount of argon to be mixed into the liquid metal in the first coating pipeline 19, thereby forming a number of micropores without lithium layer attached on the first lithium film M11 produced by coating. The maximum size of the micropores can be made less than 1 mm by controlling the pressure and flow rate of the argon.

[0057] The second base film M20 is mounted on the second base film unwinding shaft 261 in the second base film unwinding mechanism 26, so that the second base film M20 passes around the second back roller 24; the second back roller 24 has a cooling function, and the temperature of the second back roller 24 is controlled to be -50°C to 20°C, preferably -30°C to -10°C. The second lithium liquid control valve 15 is adjusted, and the second feed pump 14 is started to pump the liquid metal lithium in the lithium source 11 into the second coating head 22 through the second coating pipe 20; the liquid metal lithium in the second coating head 22 is forced to extrude and coat the second base film M20 from the slit due to the pressure of the second feed pump 14, and because the temperature of the second back roller 24 is extremely low, the liquid metal lithium on the second base film M20 is instantly solidified onto the second base film M20, forming a second lithium film M21. The thickness of the metal lithium layer on the second lithium film M21 can be controlled by adjusting the size of the slit of the second coating head 22 and the conveying speed of the second base film M20, and the thickness of the lithium layer can be controlled to be 3μm to 20μm. After stable coating, the second gas control valve 18 is opened and adjusted to allow a certain amount of argon gas to be mixed into the liquid metal in the second coating pipeline 20, so that a number of micropores without lithium layer attached are formed on the second lithium film M21 produced by coating, and the maximum size of the micropores can be controlled to be less than 1mm by controlling the pressure and flow rate of the argon gas.

[0058] The first coating roller 331 in the first coating device 33 is a roller having concave-convex strip intervals, and the second coating roller 332 is configured as a conventional cylindrical roller.

[0059] The first pole piece P1 is mounted on the first pole piece unwinding shaft 271, and after being unwound by the first pole piece unwinding mechanism 27, it enters between the first coating roller 331 and the second coating roller 332 of the first coating device 33; the first lithium film M11 formed after coating passes through the first coating device 33 between the second coating roller 332 and the first pole piece P1, and the side of the first lithium film M11 having the ultra-thin metal lithium layer is arranged opposite to the first pole piece P1, and the side of the first base film M10 on the first lithium film M11 is arranged opposite to the second coating roller 332. The second lithium film M21 formed after coating passes through the first coating device 33 between the first coating roller 331 and the first pole piece P1, and the side of the second lithium film M21 having the ultra-thin metal lithium layer is arranged opposite to the first pole piece P1, and the side of the second base film M20 on the second lithium film M21 is arranged opposite to the first coating roller 331. Since the first coating roller 331 in the first coating device 33 is a roller with concave-convex strip intervals, the portion corresponding to the convex portion 334 on the first coating roller 331 is rolled, so that the ultra-thin lithium layer of the corresponding portion on the first lithium film M11 and the second lithium film M21 is transferred and laminated on the first electrode P1, forming the first pre-lithiation electrode P11, as shown in FIG. Figure 5 As shown; the portion corresponding to the concave portion 333 on the first coating roller 331 is not rolled, and the ultra-thin lithium layer corresponding to the first lithium film M11 and the second lithium film M21 still remains on the first base film M10 and the second base film M20, forming a first strip-shaped spacer lithium film M12 and a second strip-shaped spacer lithium film M22, respectively, as shown Figure 4 The first pre-lithiation electrode P11 formed after rolling by the first coating device 33 is wound onto the first electrode winding shaft 281 and then rolled up by the first electrode winding mechanism 28 .

[0060] The second pole piece P2 is installed on the second pole piece unwinding shaft 291, and after being unwound by the second pole piece unwinding mechanism 29, enters between the third coating roller 341 and the fourth coating roller 342 of the second coating device 34; the first strip-shaped spacer lithium film M12 formed after rolling by the first coating device 33 passes through the second coating device 34 between the fourth coating roller 342 and the second pole piece P2, and the side of the first strip-shaped spacer lithium film M12 having a strip-shaped ultra-thin metal lithium layer is arranged opposite to the second pole piece P2, and the side of the first base film M10 on the first strip-shaped spacer lithium film M12 is arranged opposite to the fourth coating roller 342. The second strip-shaped spacer lithium film M22 formed by rolling by the first coating device 33 passes through the second coating device 34 between the third coating roller 341 and the second pole piece P2, and the side of the second strip-shaped spacer lithium film M22 having the strip-shaped ultra-thin metal lithium layer is arranged opposite to the second pole piece P2, and the side of the second base film M20 on the second strip-shaped spacer lithium film M22 is arranged opposite to the third coating roller 341. Since the third coating roller 341 and the fourth coating roller 342 in the second coating device 34 are conventional cylindrical rollers, the first strip-shaped spacer lithium film M12, the second pole piece P2, and the second strip-shaped spacer lithium film M22 are rolled, so that the strip-shaped spacer ultra-thin metal lithium layers on the first strip-shaped spacer lithium film M12 and the second strip-shaped spacer lithium film M22 are transferred and laminated onto the second pole piece P2, forming the second pre-lithiation pole piece P21. After rolling, the metal lithium on the first strip-shaped spacer lithium film M12 is completely transferred, and only the first base film M10 remains; the metal lithium layer on the second strip-shaped spacer lithium film M22 is completely transferred, and only the second base film M20 remains. The second pre-lithiation electrode P21 is wound onto the second electrode winding shaft 301 and wound by the second electrode winding mechanism 30; the first base film M10 and the second base film M20 after coating are respectively wound onto the first base film winding shaft 311 and the second base film winding shaft 321 and wound by the first base film winding mechanism 31 and the second base film winding mechanism 32.

[0061] In the present invention, the ultra-thin lithium film (the first lithium film M11 and the second lithium film M21) is directly formed by coating with liquid metal lithium, and then the strip-shaped intervals are transferred to the two negative electrode sheets (the first electrode sheet P1 and the second electrode sheet P2) after rolling by the specially arranged first coating device 33 and the second coating device 34. The width of the ultra-thin metal lithium layer on the pre-lithiation electrode sheet (the first pre-lithiation electrode sheet P11 and the second pre-lithiation electrode sheet P21) can be determined by pre-designing the width of the concave and convex strip-shaped intervals on the coating roller in the first coating device 33. For example, if the spacing of the ultra-thin metal lithium layer on the pre-lithiation electrode sheet is desired to be 3 mm, it can be achieved by only designing the width of the concave and convex parts in the first coating device 33 to be 3 mm. That is, the spacing distance of the ultra-thin lithium layer on the pre-lithiation electrode sheet can be controlled. On the other hand, assuming that the theoretical lithium replenishment requires a thickness of 3μm, the present invention only needs to coat the ultra-thin lithium layer to 6μm, and then transfer the strip-shaped intervals to the first pole piece P1 and the second pole piece P2, and the lithium loading is the same as the theoretical 3μm thick metal lithium content. This has a very big advantage, greatly reducing the difficulty of coating metal lithium (coating 3μm thick metal lithium is much more difficult than coating 6μm thick metal lithium), and greatly improving production efficiency (under the same coating speed, coating 6μm metal lithium is twice the output of coating 3μm metal lithium. In fact, due to the reduced difficulty, the production efficiency is improved by far more than 2 times).

[0062] Although the present invention has been disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A negative electrode strip spacer pre-lithiation device with an integrated coating, characterized in that: The device comprises: A base film unwinding mechanism, wherein the base film unwinding mechanism comprises a first base film unwinding mechanism and a second base film unwinding mechanism, which are used to unwind the first base film and the second base film respectively; A coating mechanism, comprising a first coating mechanism and a second coating mechanism, for coating liquid metal lithium onto the first base film and the second base film, respectively, to form a first lithium film and a second lithium film; A first pole piece unwinding mechanism, used for unwinding the first pole piece; A first coating device is used to transfer and coat the metal lithium layers on the first lithium film and the second lithium film onto the first electrode piece at intervals to obtain a first pre-lithiation electrode piece, wherein the metal lithium layer on the first lithium film and the metal lithium layer on the second lithium film are transferred and coated onto the upper and lower surfaces of the first electrode piece respectively; A first pole piece winding mechanism, used for winding the first pre-lithiation pole piece after pre-lithiation; A second pole piece unwinding mechanism, used for unwinding the second pole piece; A second coating device is used to transfer and coat the remaining metal lithium layers on the first lithium film and the second lithium film onto the second electrode piece at the same time to obtain a second pre-lithiation electrode piece, wherein the remaining metal lithium layer on the first lithium film and the remaining metal lithium layer on the second lithium film are respectively transferred and coated onto the upper and lower surfaces of the second electrode piece; A second pole piece winding mechanism, used for winding the second pre-lithiation pole piece; and The base film winding mechanism includes a first base film winding mechanism and a second base film winding mechanism, which are respectively used to wind up the first base film and the second base film after use.

2. The negative electrode strip-shaped pre-lithiation device coated as claimed in claim 1, characterized in that: The coating mechanism comprises a coating head and a backing roller.

3. The negative electrode strip-shaped pre-lithiation device coated as claimed in claim 2, characterized in that: The backing roller has a cooling function.

4. The negative electrode strip-shaped pre-lithiation device coated as claimed in claim 1, characterized in that: The first coating device comprises a first coating roller and a second coating roller, wherein a working area of ​​at least one of the first coating roller and the second coating roller has a strip-shaped interval.

5. The negative electrode strip-shaped pre-lithiation device coated as claimed in claim 4, characterized in that: The strip spacing is uniformly distributed and has a clear boundary line. The size of the concave-convex spacing is 1mm-IB232557 10mm; and when both the first coating roller and the second coating roller have strip-shaped intervals, the corresponding relationship between the strip-shaped intervals of the two coating rollers is convex to convex, and concave to concave.

6. The negative electrode strip-shaped pre-lithiation device coated as claimed in claim 1, characterized in that: At least one of a supporting roller mechanism, a tension detection mechanism and a tension control mechanism is also arranged between the coating mechanism and the first laminating device.

7. The negative electrode strip-shaped pre-lithiation device coated as claimed in claim 1, characterized in that: At least one of a peeling mechanism, a supporting roller mechanism, a tension detection mechanism and a tension control mechanism is further arranged downstream of the first laminating device and / or the second laminating device.

8. A method for pre-lithiation of a negative electrode strip interval, characterized in that: The method comprises: coating liquid metallic lithium onto a base film by means of a device as described in any one of claims 1 to 7 to form an ultra-thin lithium film having a metallic lithium layer with a thickness in the micrometer range, and transferring the metallic lithium layer in strip-shaped intervals onto two rolled battery pole pieces, thereby forming a plurality of lithium strips with strip-shaped intervals in the micrometer range on each pole piece.

9. The method according to claim 8, characterized in that The side of the base film in contact with the metal lithium layer is also provided with a coating.

10. The method according to claim 8, characterized in that When liquid metal lithium is coated to form an ultra-thin lithium film, an inert gas is mixed in, so that the coated metal lithium layer has micropores.

Citation Information

Cited By

  • A method for preparing an ultrathin and ultra-wide metal lithium composite material

    CN122918566A

  • Device for preparing ultra-thin and ultra-wide metal lithium composite material

    CN223951180U