By using chemical crosslinking adhesives formed by chemically crosslinkable monomers in lithium-ion batteries, performance problems caused by changes in silicon-based anode volume are solved, and higher mechanical stability and capacity retention are achieved, which extends the The cycle life of the battery.
Patent Information
- Application Number
- CN202410615973.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-26
- Filing Date
- 2024-05-17
- Publication Date
- 2024-12-03
AI Technical Summary
Traditional adhesives cannot effectively adapt to the performance problems caused by volume expansion and contraction of silicon-based anodes in lithium-ion batteries, resulting in mechanical deterioration and capacity attenuation.
Chemically crosslinkable adhesives are formed using chemically crosslinkable monomers, allowing the electrode to expand volume during charging and shrink volume during discharge, forming an interconnect network structure to maintain the electrodes by mechanically bonding graphite and silicon-based particles. structural integrity and performance.
The mechanical stability and capacity retention rate of the electrode are improved, and the initial capacity retention rate in multiple charge and discharge cycles is 80%, extending the unit cycle life of the lithium-ion battery.
Smart Images

Figure CN119069702A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to electrode materials for lithium-ion batteries. Background Art
[0002] Anodes containing electrochemically active silicon particles have been studied because of their extremely high theoretical capacity. Silicon-based anodes are susceptible to volume expansion and contraction. To mitigate the problems associated with volume changes in silicon-based anodes, various approaches have been explored, including the use of binders that can accommodate the volume expansion and contraction of the anode material. Binders help maintain structural integrity by promoting good adhesion and cohesion in the electrode. Traditional binders, such as polyvinylidene fluoride (PVDF), may not be able to effectively accommodate the volume changes associated with silicon-based particles, leading to performance issues. Summary of the invention
[0003] In one example, a lithium-ion battery component includes a precured electrode including a current collector and a slurry applied to the current collector. The slurry includes graphite, silicon-based particles, and a chemically crosslinkable monomer. The chemically crosslinkable monomer is configured to chemically crosslink and form a chemically crosslinked adhesive in response to initiation, and the chemically crosslinked adhesive mechanically bonds the graphite and silicon-based particles together, thereby forming a coating that adheres to the current collector. The chemically crosslinked adhesive is also configured to allow the volume expansion of the coating during the charging of the electrode and promote the volume contraction of the coating during the discharge.
[0004] In another example, the precured electrode includes a current collector and a slurry on the current collector. The slurry includes an active material and a chemically crosslinkable monomer. The chemically crosslinkable monomer is configured to chemically crosslink upon initiation to form a chemically crosslinked adhesive that cohesively bonds the active material and other electrode components together to form a coating that adheres to the current collector. The chemically crosslinked adhesive also reduces mechanical degradation during volume expansion of the coating during charging of the electrode and promotes volume shrinkage of the coating during discharge.
[0005] In another example, the pre-cured electrode includes a current collector and a slurry on the current collector. The slurry contains graphite, silicon-based particles, and a chemically cross-linkable monomer having at least two functional groups. The chemically cross-linkable monomer is configured to be chemically cross-linked in response to the curing of the slurry to form a chemically cross-linked adhesive that mechanically bonds the graphite and silicon-based particles together, thereby forming an electrode having a coating adhered to the current collector. The chemically cross-linked adhesive is also configured to promote shrinkage of the coating during discharge of the electrode. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Figure 1 is a cross-sectional view showing an electrode having a chemically cross-linked binder;
[0007] Figure 2 is a flow chart of a cross-sectional view of an electrode charged and discharged without a chemically cross-linked binder; and
[0008] Figure 3 is a flow chart of a cross-sectional view of charging and discharging of an electrode with a chemically cross-linked binder. DETAILED DESCRIPTION
[0009] Embodiments are described herein. However, it should be understood that the disclosed embodiments are merely examples and that other embodiments may take various and alternative forms. The drawings are not necessarily drawn to scale. Some features may be enlarged or minimized to show details of particular components. Therefore, the specific structural details and functional details disclosed herein should not be interpreted as limiting, but merely as a representative basis for teaching those skilled in the art.
[0010] The various features shown and described with reference to any one of the accompanying drawings may be combined with features shown in one or more other drawings to produce embodiments not explicitly shown or described. The combinations of features shown provide representative embodiments for typical applications. However, for specific applications or implementations, various combinations and modifications of features consistent with the teachings of the present disclosure may be desired.
[0011] Graphite anodes blended with silicon-X (Si, SiOX, Si / C) can provide higher anode energy density than graphite-only anodes. Cycling is accompanied by high volume expansion of silicon (close to 300%), leading to potential capacity fading via silicon particle crushing and solid-electrolyte interface instability, volume changes during full-depth cycling, and loss of electrical contact between active materials and current collectors.
[0012] Styrene-butadiene rubber is an anode binder, commonly used for graphite or silicon-X-graphite anodes. When the silicon-X ratio is above 10%, this rubber binder may not effectively suppress anode swelling. Its lack of elasticity may make it difficult to prevent anode problems associated with high electrode expansion (e.g., volume expansion caused by charging / lithiation).
[0013] Electrodes used in battery cells are manufactured by a process involving coating a current collector with a slurry containing an active material (such as graphite or silicon) and a binder material. The precured electrode is then cured to produce a solid electrode. The curing process includes drying the precured electrode. This can be done by heating the precured electrode to a specific temperature to harden the slurry and form a durable electrode.
[0014] The present disclosure relates in one aspect to including chemically crosslinkable monomers in lithium ion battery components including precured electrodes. The chemically crosslinkable monomers form a chemically crosslinked binder in the electrode that enables volume expansion and contraction during charge and discharge cycles, thereby improving performance. The chemically crosslinked binder mechanically bonds the electrode materials together while allowing volume changes, resulting in increased capacity and size retention. In some embodiments, the chemically crosslinkable monomers may be present in an amount of 1% to 20% by weight relative to the graphite and silicon-based particles. In other embodiments, the chemically crosslinkable monomers may be present in an amount of 1% to 10% by weight relative to the graphite and silicon-based particles.
[0015] Reference now Figure 1 , in the first view 10, the pre-cured electrode 12 includes a current collector 14 and a slurry 16 applied to the current collector. It will be appreciated by those skilled in the art that a green anode represents an unprocessed anode that has not yet undergone the necessary process to realize its full potential in terms of functionality, durability and electrochemical performance. The current collector 14 may be a metal foil, such as but not limited to copper, aluminum or other suitable materials. The current collector 14 provides conductivity and a surface for adhering the slurry 14. The slurry 14 comprises graphite particles 18, silicon-based particles 20, a chemically cross-linkable monomer 22 and a binder material. The graphite particles 18 are used as an active material for lithium ion storage and provide good electronic conductivity. Compared with the graphite particles 18, the silicon-based particles 20 are also used as active materials and provide a higher theoretical capacity. The chemically cross-linkable monomer 22 is configured to be chemically cross-linked in response to initiation to form a chemically cross-linked binder 24. The binder material may be styrene-butadiene rubber (SBR) or any other known material suitable for the purpose. The initiator triggers a polymerization reaction between the crosslinkable monomer 22 and the adhesive, resulting in the formation of a chemically crosslinked adhesive 24. The initiator may be benzoyl peroxide (BPO), azobisisobutyronitrile (AIBN), or other suitable materials.
[0016] In the second view 26 at initiation, the chemically cross-linkable monomer 22 reacts to form a chemically cross-linked binder 24 that mechanically bonds the graphite particles 18 and the silicon-based particles 20 together. The formation of the chemically cross-linked binder 24 results in the formation of a coating that adheres to the current collector 14. The chemically cross-linked binder 24 is configured to allow the coating to expand in volume during the charging process of the electrode 28 and to facilitate the coating to shrink in volume during the discharging process of the electrode 28. Figure 1The chemically cross-linked binder 24 is shown to form a network structure that surrounds and interconnects the graphite particles 18 and the silicon-based particles 20, thereby providing mechanical stability and promoting adhesion of the slurry 16 to the current collector 14. The chemically cross-linked binder 24, due to its interconnected network structure, is also able to accommodate the volume changes experienced by the silicon-based particles 20 during the charge cycle and the discharge cycle, thereby maintaining the structural integrity and performance of the electrode. The increased mechanical stability provided by the interconnected network structure of the chemically cross-linked binder 24 also leads to better retention of the initial capacity during the charge cycle and the discharge cycle, with a retention rate of 80%. In the context of an electrode, capacity refers to the amount of charge that can be stored and released by the electrode during the charge cycle and the discharge cycle.
[0017] The weight percentage of the chemically cross-linked monomer 22 relative to the total weight of the graphite particles 18 and the silicon-based particles 20 can be in the range of 1 weight % to 20 weight %, or more specifically, in the range of 1 weight % to 10 weight %. The increase in the weight percentage of the cross-linkable monomer leads to a higher degree of chemical cross-linking, thereby leading to a more tightly interconnected network structure and further improving the mechanical properties. The weight percentages of the cross-linkable monomers and active materials disclosed herein have been determined to provide a desired balance between the weight percentage of the cross-linkable monomer required to achieve the best mechanical stability and adhesion of the electrode and the weight percentage of the active material required to achieve the desired electrochemical performance. It should be noted that these weight percentages have been proven to work well without reducing the capacity or other aspects of the electrode. The specific weight percentage can be adjusted based on the desired properties and performance requirements of the lithium-ion battery.
[0018] Reference now Figure 2 , in the first view, graphite particles, silicon-based particles, and a chemically cross-linked binder are shown under nominal conditions. The binder exists in its non-cross-linked state, providing limited mechanical stability and adhesion between the particles and the current collector. In the second view, the anode acquires lithium ions and charge, resulting in volume expansion of the silicon-based particles. Since there is no chemical cross-linking network, the binder cannot adapt to the volume change of the silicon-based particles, resulting in weakened structural integrity and reduced adhesion between the particles and the current collector. In the third view, the electrode has been discharged and lithium ions have been removed from the silicon-based particles. The volume of the silicon-based particles has shrunk, resulting in further wear of the slurry and degradation of the volume stability. This may affect the performance and capacity retention of the battery over time.
[0019] Reference now Figure 3, in the first view 30, the anode 32 comprises graphite particles 34, silicon-based particles 36 and a chemically cross-linked binder 38, which forms a network structure 40 surrounding and interconnecting the particles, thereby providing mechanical stability and adhesion between the particles and the current collector. In the second view 42, the anode acquires lithium ions and charges, resulting in volume expansion of the silicon-based particles 36. The chemically cross-linked binder 38 effectively accommodates the volume change of the silicon-based particles 36 due to its cross-linked network structure 40, thereby maintaining the structural integrity of the electrode and the adhesion between the particles and the current collector. In the third view 44, the anode 32 has been discharged and lithium ions have been removed from the silicon-based particles 36. The volume of the silicon-based particles 36 has shrunk, but the volume stability of the anode has been largely maintained due to the chemically cross-linked binder 38. This increased volume stability helps maintain the performance and capacity retention of lithium-ion batteries over multiple charge and discharge cycles. The increased volume stability provided by the interconnected network structure 40 of the chemically cross-linked binder 38 also results in an 80% retention of the initial capacity during the charge and discharge cycles.
[0020] Therefore, the present disclosure contemplates methods for constructing graphite / silicon X anodes containing elastomeric crosslinking binders to inhibit electrode swelling and promote recovery from volume expansion during lithium discharge. Crosslinkable monomers are crosslinked with anode binders (e.g., styrene-butadiene rubber) to form an elastomeric binder system. The resulting elastomeric forces increase the dimensional stability of the graphite / silicon X anode, thereby allowing for longer cell cycle life.
[0021] The use of a crosslinkable monomer can result in less calendaring by acting as a plasticizer prior to curing and mitigate anode springback after vacuum drying. The crosslinkable monomer and styrene butadiene rubber in the graphite / silicon X anode are thermally cured to an elastomer in the presence of a free radical initiator such as benzoyl peroxide.
[0022] The graphite / silicon X anode may comprise artificial or synthetic graphite, silicon (Si, SiOx, Si / C), a crosslinkable monomer, a free radical initiator, a conductive material, styrene-butadiene rubber and carboxymethyl cellulose. The crosslinkable monomer reacts with the vinyl and / or benzyl radicals of the styrene-butadiene rubber to produce an elastic binder system.
[0023] Crosslinkable monomers include, but are not limited to, multifunctional acrylics such as pentaerythritol tetraacrylate, ethoxylated pentaerythritol tetraacrylate, ditrimethylolpropane tetraacrylate, dipentaerythritol pentaacrylate, dipentaerythritol hexaacrylate or ethoxylated dipentaerythritol hexaacrylate, as a single or blended form. Curing is carried out in the presence of a free radical initiator via a heat beam, UV beam or electron beam. Curing initiators include, but are not limited to, peroxides, phosphorus compounds or sulfates.
[0024] Although exemplary embodiments are described above, these embodiments are not intended to describe all possible forms encompassed by the claims. The words used in the specification are words of description rather than limitation, and it should be understood that various changes can be made without departing from the spirit and scope of these disclosed materials.
[0025] As previously mentioned, the features of the various embodiments may be combined to form additional embodiments of the present invention that may not be explicitly described or shown. Although various embodiments may have been described as providing advantages or being preferred over other embodiments or prior art implementations with respect to one or more desired characteristics, it will be appreciated by those of ordinary skill in the art that one or more features or characteristics may be compromised to achieve desired overall system properties, depending on the specific application and implementation. These properties may include, but are not limited to, strength, durability, marketability, appearance, packaging, size, serviceability, weight, manufacturability, ease of assembly, and the like. Therefore, embodiments that are described as less desirable than other embodiments or prior art implementations with respect to one or more characteristics are within the scope of the present disclosure and may be desirable for a particular application.
Claims
1. A lithium ion battery component, comprising: A precured electrode comprising a current collector and a slurry on the current collector, the slurry comprising graphite, silicon-based particles and chemically cross-linkable monomers, the chemically cross-linkable monomers being configured to chemically cross-link in response to initiation to form a chemically cross-linked adhesive, the chemically cross-linked adhesive: (i) mechanically bonds the graphite and the silicon-based particles together, thereby resulting in the formation of a coating adhered to the current collector; and (ii) is configured to allow the coating to expand in volume during charging of the electrode and promote volume contraction of the coating during discharge.
2. The lithium-ion battery component of claim 1, wherein the chemically cross-linked binder is configured to allow the coating to expand in volume during charging of the electrode and to promote volume contraction of the coating during discharging of the electrode, such that the electrode retains 80% of its initial capacity.
3. The lithium ion battery component of claim 1, wherein the chemically cross-linkable monomer is 1 wt% to 20 wt% relative to the graphite and the silicon-based particles.
4. The lithium ion battery component of claim 3, wherein the chemically cross-linkable monomer is 1 wt% to 10 wt% relative to the graphite and the silicon-based particles.
5. The lithium ion battery component of claim 1, wherein the current collector is a metal foil.
6. A pre-cured electrode comprising: Current collector; as well as a slurry on the current collector and comprising an active material and a chemically cross-linkable monomer configured to chemically cross-link when initiated to form a chemically cross-linked binder that: (i) cohesively bonds the active material together to form a coating adhered to the current collector; (ii) enabling the coating to expand in volume during charging of the electrode; and (iii) promoting the coating to shrink in volume during discharge.
7. A pre-cured electrode as described in claim 6, wherein the chemically cross-linked binder is configured to allow the coating to expand in volume during charging of the electrode and promote the coating to shrink in volume during discharging of the electrode so that the electrode retains 80% of the initial capacity.
8. The precured electrode of claim 6, wherein the chemically cross-linkable monomer is 1 wt% to 20 wt% relative to the active material.
9. The precured electrode of claim 8, wherein the chemically cross-linkable monomer is 1 wt% to 10 wt% relative to the active material.
10. The precured electrode of claim 6, wherein the current collector is a metal foil.
11. A pre-cured electrode comprising: Current collector; as well as A slurry, the slurry being on the current collector and comprising graphite, silicon-based particles, and a chemically cross-linkable monomer having at least two functional groups, the chemically cross-linkable monomer being configured to chemically cross-link in response to curing of the slurry to form a chemically cross-linked binder, the chemically cross-linked binder mechanically bonding the graphite and the silicon-based particles together, thereby resulting in the formation of an electrode having a coating, the coating: (i) adhering to the current collector; and (ii) being configured to promote shrinkage of the coating during discharge of the electrode.
12. The pre-cured electrode of claim 11, wherein the chemically cross-linked binder is configured to allow the coating to expand in volume during charging of the electrode and to promote volume contraction of the coating during discharging of the electrode such that the electrode retains 80% of its initial capacity.
13. The precured electrode of claim 11, wherein the chemically cross-linkable monomer is 1 wt% to 20 wt% relative to the graphite and the silicon-based particles.
14. The precured electrode of claim 13, wherein the chemically cross-linkable monomer is 1 wt% to 10 wt% relative to the graphite and the silicon-based particles.
15. The precured electrode of claim 11, wherein the current collector is a metal foil.