Electricity storage unit
By placing a buffer material with a low elastic modulus at the uncoated part of the wound electrode body, the problem of concave and convexity caused by the thickness of the electrode lead is solved, local pressure is suppressed, and the stability and performance of the electrode body are improved.
Patent Information
- Application Number
- CN202410684047.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-31
- Filing Date
- 2024-05-30
- Publication Date
- 2024-12-03
AI Technical Summary
In the wound electrode body equipped with the ear leads, the lead thickness causes the formation of concave and convexity, and then locally applies pressure, affecting the stability and performance of the battery.
By configuring a buffer material, such as an adhesive material, at the uncoated site, to reduce the exposed area of the current collector and to make the elastic modulus of the buffer material lower than the tip leads, it ensures that the buffer material is more likely to deform, thereby reducing thickness Differentially inhibits the formation of concave and convexity.
The pressure applied locally in the wound electrode body is effectively suppressed, the stability and performance of the electrode body are improved, the formation of concave and convexity is reduced, and the service life of the battery is extended.
Smart Images

Figure CN119069825A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a power storage unit. Background Art
[0002] International Publication No. 2018 / 105398 discloses a secondary battery having an electrode body in which a positive electrode and a negative electrode are wound in a spiral shape with a separator interposed therebetween. A lead wire electrically connected to a positive electrode (negative electrode) terminal is joined to a current collector of the positive electrode (negative electrode). Summary of the invention
[0003] In the electrode body of the International Publication No. 2018 / 105398, the portion of the current collector where the lead is provided may be uneven due to the thickness of the lead. In this case, the unevenness of the wound electrode body will locally apply pressure to the wound electrode body when the wound electrode body is constrained by a shell or the like.
[0004] The present disclosure has been made to solve the above-mentioned problems, and an object of the present disclosure is to provide a power storage unit capable of suppressing local application of pressure in a wound electrode body in which a tab lead is arranged.
[0005] The storage unit of one aspect of the present disclosure comprises: a wound electrode body including a first electrode, a second electrode, and a separator arranged between the first electrode and the second electrode; and a shell that accommodates the wound electrode body. The wound electrode body is wound with the first electrode, the second electrode, and the separator in a manner that the first electrode, the second electrode, and the separator surround the winding axis. The first electrode includes a current collector, an electrode material layer applied to a portion of the current collector, a tab lead arranged in a manner protruding from the current collector in the axial direction of the wound electrode body, and a buffer material. The current collector includes an uncoated portion to which the electrode material layer is not applied. The tab lead is arranged in the uncoated portion. The buffer material is arranged in a position adjacent to the tab lead in the uncoated portion.
[0006] In the storage cell of one aspect of the present disclosure, as described above, the buffer material is arranged at a position adjacent to the tab lead in the uncoated portion. Thus, by arranging the buffer material in the uncoated portion where the tab lead is arranged, the area where the current collector is exposed in the uncoated portion can be reduced. As a result, it is possible to suppress the formation of unevenness between the portion where the tab lead is arranged and the portion where the tab lead is not arranged. Thus, it is possible to suppress the local application of pressure to the wound electrode body due to the unevenness.
[0007] In the above-mentioned storage unit of one aspect, it is preferred that the elastic modulus of the buffer material is lower than the elastic modulus of the tab lead. When the first electrode is expanded into a sheet-like state, the thickness of the buffer material in the orthogonal direction orthogonal to the collector is greater than the thickness of the tab lead in the orthogonal direction. If so configured, the buffer material is more easily deformed than the tab lead by making the elastic modulus of the buffer material lower than the elastic modulus of the tab lead. In addition, by making the thickness of the buffer material in the orthogonal direction greater than the thickness of the tab lead, when the buffer material and the tab lead are deformed due to winding the first electrode, the difference between the thickness of the buffer material and the thickness of the tab lead can be suppressed.
[0008] In this case, it is preferred that the elastic modulus of the electrode material layer is lower than the elastic modulus of the tab lead. When the first electrode is expanded into a sheet, the thickness of the electrode material layer in the orthogonal direction is greater than the thickness of the tab lead in the orthogonal direction. If so configured, the electrode material layer is more easily deformed than the tab lead by making the elastic modulus of the electrode material layer lower than the elastic modulus of the tab lead. In addition, by making the thickness of the electrode material layer in the orthogonal direction greater than the thickness of the tab lead, when the electrode material layer and the tab lead are deformed due to winding the first electrode, the difference between the thickness of the electrode material layer and the thickness of the tab lead can be suppressed.
[0009] In the storage unit in which the elastic modulus of the electrode material layer is lower than the elastic modulus of the tab lead, it is preferred that the elastic modulus of the buffer material is lower than the elastic modulus of the electrode material layer. When the first electrode is expanded into a sheet, the thickness of the buffer material in the orthogonal direction is greater than the thickness of the electrode material layer in the orthogonal direction. If so configured, the buffer material is more easily deformed than the electrode material layer by making the elastic modulus of the buffer material lower than the elastic modulus of the electrode material layer. In addition, by making the thickness of the buffer material in the orthogonal direction greater than the thickness of the electrode material layer, when the buffer material and the electrode material layer are deformed due to winding the first electrode, the difference between the thickness of the buffer material and the electrode material layer can be suppressed.
[0010] In the storage cell in which the elastic modulus of the buffer material is lower than the elastic modulus of the tab lead, it is preferred that, in a state in which the first electrode is wound together with the second electrode and the separator, the absolute value of the difference between the thickness of the buffer material in the radial direction of the wound electrode body and the thickness of the tab lead in the radial direction is less than the thickness of the collector in the radial direction. If so configured, the unevenness formed on the wound electrode body can be reduced compared to a case in which the difference is larger than the thickness of the collector.
[0011] In the above-mentioned power storage unit according to one aspect, the uncoated portion is preferably provided at an end portion of the current collector in the winding direction of the wound electrode body. With such a configuration, it is possible to suppress the formation of irregularities at the end portion of the wound electrode body.
[0012] In this case, the buffer material preferably includes an adhesive material. With this configuration, the first electrode can be easily bonded (fixed) to a member (eg, a separator) adjacent to the first electrode in the radial direction at the end of the wound electrode body.
[0013] In the above-mentioned storage battery cell, it is preferred that the uncoated portion extends in the axial direction along which the winding axis extends. The buffer material is provided so as to extend along the uncoated portion extending in the axial direction. If so configured, the buffer material is provided over a wider range in the axial direction, thereby further suppressing the formation of irregularities in the wound electrode body.
[0014] According to the present disclosure, it is possible to suppress the local application of pressure in the wound electrode body in which the tab lead is arranged.
[0015] The foregoing and other objects, features, aspects and advantages of the present invention will become more apparent from the following detailed description of the present invention when taken in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a cross-sectional view showing the structure of a power storage unit according to one embodiment.
[0017] Figure 2 It is a perspective view schematically showing the structure of a wound electrode body according to one embodiment.
[0018] Figure 3 It is a plan view showing the structure of a positive electrode plate according to one embodiment.
[0019] Figure 4 It is a plan view showing the structure of a negative electrode plate according to one embodiment.
[0020] Figure 5 It is a diagram showing the relationship between the elastic moduli of the positive electrode tab lead, the positive electrode mixture layer, and the adhesive material.
[0021] Figure 6 It is along Figure 3 A cross-sectional view taken along line VI-VI.
[0022] Figure 7 It is a partially enlarged cross-sectional view of the wound electrode body in a wound state.
[0023] Figure 8 FIG. 1 is a plan view showing the structure of a positive electrode plate according to a modified example of one embodiment.
[0024] Fig. 9 It is a plan view showing the structure of a negative electrode plate according to a modified example of one embodiment.
[0025] Fig.10 FIG. 2 is a plan view showing the structure of a positive electrode plate according to a modified example of one embodiment.
[0026] Fig.11 FIG. 3 is a plan view showing the structure of a positive electrode plate according to a modified example of one embodiment. DETAILED DESCRIPTION
[0027] Hereinafter, the embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. It should be noted that the same or corresponding parts in the drawings are denoted by the same reference numerals, and their description will not be repeated.
[0028] Figure 1 1 is a cross-sectional view showing the overall structure of the power storage unit 100 according to the embodiment of the present disclosure. The power storage unit 100 is, for example, a lithium-ion battery mounted on a vehicle. It should be noted that the use and type of the power storage unit 100 are not limited to the above example.
[0029] The power storage cell 100 includes a wound electrode body 1 , a case 2 , a CID (Current Interrupt Device) 3 , a positive insulating plate 4 , a negative insulating plate 5 , and an insulating layer 6 .
[0030] The wound electrode body 1 is accommodated in a case 2. The case 2 has a cylindrical shape. That is, the power storage unit 100 is a cylindrical battery. The case 2 is formed of, for example, copper or aluminum.
[0031] The wound electrode body 1 includes a positive electrode plate 10, a negative electrode plate 20 and a separator 30. The separator 30 is arranged between the positive electrode plate 10 and the negative electrode plate 20. The separator 30 enables ions (such as lithium ions) to travel back and forth between the positive electrode plate 10 (positive electrode active material) and the negative electrode plate 20 (negative electrode active material), and separates the positive electrode plate 10 from the negative electrode plate 20. The wound electrode body 1 is composed of an electrode plate group in which the positive electrode plate 10 and the negative electrode plate 20 are wound with the separator 30 interposed therebetween. It should be noted that the positive electrode plate 10 and the negative electrode plate 20 are examples of the "first electrode" and the "second electrode" of the present disclosure, respectively.
[0032] like Figure 2 As shown in FIG. 1 , the wound electrode body 1 is wound so that the positive electrode plate 10 , the negative electrode plate 20 , and the separator 30 surround the periphery of the winding axis α. Figure 2 In order to facilitate understanding of the wound state of the wound electrode body 1 , the wound electrode body 1 is shown in a state where it is slightly unwound.
[0033] The positive electrode plate 10 includes a positive electrode current collector 11 (see Figure 3 ), positive electrode mixture layer 12 (refer to Figure 3 ), a plurality of positive electrode tab leads 13 (five in this embodiment) and an adhesive material 14 (see Figure 3The negative electrode plate 20 includes a negative electrode current collector 21 (see Figure 4 ), negative electrode mixture layer 22 (refer to Figure 4 ) and the negative electrode tab lead 23. It should be noted that Figure 1 In the figure, only two positive electrode tab leads 13 are shown. In addition, the adhesive material 14 and the positive electrode tab lead 13 are examples of the "buffer material" and "tab lead" of the present disclosure, respectively. In addition, the positive electrode collector 11 and the positive electrode mixture layer 12 are examples of the "collector" and "electrode material layer" of the present disclosure, respectively.
[0034] Refer again Figure 1 The positive insulating plate 4 is accommodated in the case 2. The positive insulating plate 4 is provided to insulate the wound electrode body 1 (negative electrode plate 20 and separator 30) from the case 2. The positive insulating plate 4 is provided to cover the positive electrode collector 11, the negative electrode plate 20 and the separator 30 from the Z1 side.
[0035] The positive side insulating plate 4 has a through hole 4a. The positive electrode tab lead 13 passes through the through hole 4a and contacts the conductive film 3b described later. Thus, the positive electrode tab lead 13 and the conductive film 3b are electrically connected.
[0036] One of the plurality of positive tab leads 13 is in contact with (welded to) the conductive film 3b, and the remaining positive tab leads 13 are welded to the positive tab leads 13 in contact with the conductive film 3b. It should be noted that all of the plurality of positive tab leads 13 may be welded to the conductive film 3b.
[0037] The negative insulating plate 5 is housed in the case 2. The negative insulating plate 5 is provided to insulate the wound electrode body 1 (positive electrode plate 10 and separator 30) from the case 2. The negative insulating plate 5 is provided to cover the positive electrode plate 10, the negative electrode collector 21, and the separator 30 from the Z2 side.
[0038] The negative side insulating plate 5 has a through hole 5a. The negative electrode tab lead 23 passes through the through hole 5a and contacts the bottom 2a of the case 2. As a result, the negative electrode tab lead 23 is electrically connected to the bottom 2a of the case. As a result, the side surface 2b of the case 2 connected to the bottom 2a of the case 2 is negatively charged. It should be noted that the side surface 2b contacts the negative electrode collector 21 of the negative electrode plate 20 provided on the outermost periphery of the wound electrode body 1.
[0039] CID 3 is a device that cuts off the current path by utilizing the increase in cell internal pressure caused by gas generated by overcharging of the power storage cell 100. CID 3 is provided to seal the opening on the Z1 side of the case 2. CID 3 includes an external cover 3a, a conductive film 3b, a gasket 3c, and a chassis 3d.
[0040] The outer cover 3a functions as an external terminal by being electrically connected to an external bus bar (not shown). The outer cover 3a is provided with a fragile portion 3e (thin wall portion). When the internal pressure of the housing 2 rises, the outer cover 3a is easily damaged starting from the fragile portion 3e. As a result, the gas is quickly discharged to the outside of the housing 2.
[0041] The conductive film 3b is provided in a manner to seal the opening on the Z1 side of the shell 2. The conductive film 3b includes a protrusion 3f protruding toward the side (Z2 side) of the wound electrode body 1. The protrusion 3f is in contact with the positive electrode tab lead 13. Thus, the conductive film 3b is positively charged. In addition, the conductive film 3b is electrically connected to the external cover 3a. Thus, the external cover 3a is also positively charged. It should be noted that the protrusion 3f is provided in a manner to penetrate the gasket 3c and the chassis 3d respectively.
[0042] The conductive film 3b is provided with a fragile portion 3g (thin-walled portion) similarly to the external cover 3a. When the internal pressure of the housing 2 rises, the conductive film 3b is easily damaged starting from the fragile portion 3g. When the conductive film 3b is damaged due to the increase in internal pressure, the contact between the conductive film 3b and the positive electrode tab lead 13 is released. As a result, the positive charge of the conductive film 3b is eliminated, and the positive charge of the external cover 3a is eliminated. As a result, the charging and discharging of the storage cell 100 is stopped.
[0043] The housing 2 is provided with a caulking portion 2c caulked to the outer peripheral edge of the outer cover 3a. The insulating layer 6 is provided so as to insulate the caulking portion 2c from the outer cover 3a (and the conductive film 3b).
[0044] Figure 3 This is a diagram of the positive electrode plate 10 in a sheet-like state when viewed from the Y1 side. The Y direction is a direction orthogonal to the positive electrode current collector 11 that has been expanded into a sheet. The positive electrode current collector 11 has a rectangular shape consisting of a long side extending in the X direction and a short side extending in the Z direction. It should be noted that the X direction is an example of the "winding direction" of the present disclosure. In addition, the Z direction is an example of the "axial direction" of the present disclosure. In addition, the Y direction is an example of the "orthogonal direction" of the present disclosure. It should be noted that the Y direction is equivalent to Figure 1 The R direction is shown. In addition, the R direction is an example of the "radial direction" of the present disclosure.
[0045] like Figure 3 As shown, the positive electrode mixture layer 12 (shaded portion) is applied to a portion of the positive electrode current collector 11. That is, the positive electrode current collector 11 includes a coated portion 11a coated with the positive electrode mixture layer 12, and an uncoated portion 11b and an uncoated portion 11c not coated with the positive electrode mixture layer 12. It should be noted that the uncoated portion 11c is an example of the "uncoated portion" disclosed in the present invention.
[0046] exist Figure 3In the example shown, the uncoated portion 11c is provided at the end 11d on the X1 side and the end 11e on the X2 side of the positive electrode current collector 11. The three uncoated portions 11b are arranged between the end 11d and the end 11e in the X direction and separated from each other. The coated portions 11a are provided between the uncoated portion 11c and the uncoated portion 11b and between the uncoated portions 11b. In the present embodiment, the X1 side and the X2 side are respectively used as the winding end side and the winding start side of the wound electrode body 1.
[0047] The positive electrode current collector 11 is made of aluminum, for example. The positive electrode mixture layer 12 is formed by applying a positive electrode slurry to the surface of the positive electrode current collector 11 and drying it. The positive electrode slurry is a slurry prepared by kneading the materials (positive electrode active material, binder, etc.) of the positive electrode mixture layer 12 with a solvent. Figure 1 The thickness of the positive electrode mixture layer 12 is, for example, not less than 0.1 μm and not more than 1000 μm.
[0048] The three uncoated portions 11b and the two uncoated portions 11c are provided so as to extend in the Z direction. Each uncoated portion 11b has a width W1 in the X direction. Each uncoated portion 11c has a width W2 in the X direction. The width W2 of the uncoated portion 11c is greater than the width W1 of the uncoated portion 11b.
[0049] The positive electrode tab leads 13 are disposed on the three uncoated portions 11b and the two uncoated portions 11c. The positive electrode tab leads 13 are provided so as to protrude in the axial direction (Z1 side) from the positive electrode current collector 11. The positive electrode tab leads 13 are provided at the center of each uncoated portion 11b and each uncoated portion 11c in the X direction.
[0050] Here, in the conventional storage cells, the lead-provided portion of the current collector may have unevenness due to the thickness of the lead. In this case, the unevenness of the wound electrode body may locally exert pressure on the wound electrode body when the wound electrode body is constrained by a case or the like.
[0051] Therefore, in the present embodiment, the adhesive material 14 is arranged in the uncoated portion 11c at a position adjacent to the positive electrode tab lead 13. Specifically, in the uncoated portion 11c, the adhesive material 14 is arranged on the X1 side and the X2 side of the positive electrode tab lead 13. That is, the positive electrode tab lead 13 in the uncoated portion 11c is arranged so as to be sandwiched by two adhesive materials 14 in the X direction.
[0052] The adhesive material 14 is provided so as to extend along the uncoated portion 11 c (positive electrode tab lead 13 ) extending in the Z direction. That is, the adhesive material 14 is arranged on the surface of the uncoated portion 11 c so as to extend in the Z direction.
[0053] Specifically, the adhesive material 14 is provided so as to extend from the vicinity of the end 11f on the Z1 side of the positive electrode current collector 11 to the vicinity of the end 11g on the Z2 side of the positive electrode current collector 11. The length L1 of the adhesive material 14 in the Z direction is greater than the length L2 of the portion of the positive electrode tab lead 13 disposed in the uncoated portion 11c (overlapping with the uncoated portion 11c) in the Z direction. Figure 3 In the example shown, the length L1 is at least twice the length L2. It should be noted that the adhesive material 14 may extend to the position of the end 11f (11g).
[0054] Figure 4 20 is a diagram showing the negative electrode plate 20 in a sheet-like state when viewed from the Y1 side. Figure 4 As shown, the negative electrode current collector 21 has a rectangular shape including long sides extending in the X direction and short sides extending in the Z direction, similarly to the positive electrode current collector 11 .
[0055] The negative electrode current collector 21 is made of, for example, copper foil. The negative electrode mixture layer 22 is formed by applying a negative electrode slurry to the surface of the negative electrode current collector 21 and drying it. The negative electrode slurry is a slurry prepared by kneading the materials of the negative electrode mixture layer 22 (negative electrode active material and binder, etc.) with a solvent. The negative electrode mixture layer 22 and the separator 30 (see Figure 1 The thickness of the negative electrode mixture layer 22 is, for example, not less than 0.1 μm and not more than 1000 μm.
[0056] The negative electrode mixture layer 22 is applied to a portion of the negative electrode current collector 21. That is, the negative electrode current collector 21 includes a coated portion 21a coated with the negative electrode mixture layer 22 and an uncoated portion 21b not coated with the negative electrode mixture layer 22. The negative electrode tab lead 23 is disposed in the uncoated portion 21b. The negative electrode tab lead 23 is provided so as to protrude from the negative electrode current collector 21 in the axial direction (Z2 side).
[0057] Figure 5 1 is a diagram showing the relationship between the elastic modulus of the positive electrode tab lead 13, the positive electrode mixture layer 12, and the adhesive material 14. Figure 5 As shown, the elastic modulus increases in the order of the positive electrode tab lead 13, the positive electrode mixture layer 12, and the adhesive material 14. That is, the positive electrode tab lead 13, the positive electrode mixture layer 12, and the adhesive material 14 are less likely to deform in this order.
[0058] Figure 6 It is along Figure 3 The cross-sectional view of the VI-VI line. Figure 6As shown, the positive electrode current collector 11 has a thickness t11 in the Y direction. The positive electrode mixture layer 12 has a thickness t12 in the Y direction. The positive electrode tab lead 13 has a thickness t13 in the Y direction. The adhesive material 14 has a thickness t14 in the Y direction. It should be noted that the thickness t12 of the positive electrode mixture layer 12, the thickness t13 of the positive electrode tab lead 13, and the thickness t14 of the adhesive material 14 are respectively greater than the thickness t11 of the positive electrode current collector 11.
[0059] The thickness t14 of the adhesive material 14 is greater than the thickness t12 of the positive electrode mixture layer 12 (t14>t12). In addition, the thickness t12 of the positive electrode mixture layer 12 is greater than the thickness t13 of the positive electrode tab lead 13 (t12>t13). That is, the thickness increases in the order of the adhesive material 14, the positive electrode mixture layer 12, and the positive electrode tab lead 13 (t14>t12>t13). Therefore, the thickness is configured to increase in the order of elastic modulus from low to high (order of easy deformation).
[0060] The difference Δt between the thickness t14 of the adhesive material 14 and the thickness t13 of the positive electrode tab lead 13 is greater than the thickness t11 of the positive electrode collector 11 (Δt>t11). In addition, the difference Δt is less than the thickness t13 of the positive electrode tab lead 13 (Δt<t13). For example, the difference Δt is less than 1 / 3 of the thickness t13 of the positive electrode tab lead 13 (Δt≤t13 / 3). It should be noted that the difference Δt can also be less than the thickness t11 of the positive electrode collector 11. In addition, the above-mentioned value of 1 / 3 is just an example and is not limited to this example.
[0061] Figure 7 It is a cross-sectional view of a state in which the positive electrode plate 10 is wound together with the separator 30 and the negative electrode plate 20. In this state, due to the difference in elastic modulus, the deformation amount increases in the order of the adhesive material 14, the positive electrode mixture layer 12, and the positive electrode tab lead 13. Therefore, the difference between the radial thickness t24 of the adhesive material 14 (R direction) and the radial thickness t23 of the positive electrode tab lead 13 is smaller than the radial thickness t21 of the positive electrode collector 11.
[0062] exist Figure 7 In the example shown, the thickness t24 of the adhesive material 14, the thickness t23 of the positive electrode tab lead 13, and the radial thickness t22 of the positive electrode mixture layer 12 are substantially equal to each other. Therefore, the above difference is substantially 0. It should be noted that the above difference may also be greater than 0 and less than the thickness t21 of the positive electrode collector 11.
[0063] As described above, in the present embodiment, the adhesive material 14 is disposed in the uncoated portion 11c at a position adjacent to the positive electrode tab lead 13. It is possible to suppress the formation of a space where no member is disposed at a position adjacent to the positive electrode tab lead 13. As a result, it is possible to suppress the formation of irregularities at a position adjacent to the positive electrode tab lead 13. Thus, it is possible to suppress the application of local pressure to the wound electrode body 1 due to the irregularities.
[0064] In the above embodiment, an example is shown in which the adhesive material 14 is arranged on the uncoated portion 11c provided at the end 11d on the X1 side and the end 11e on the X2 side of the positive electrode current collector 11, but the present disclosure is not limited thereto. The uncoated portion 11c may also be provided at a location other than the end 11d and the end 11e of the positive electrode current collector 11. Figure 8 In the positive electrode plate 110 shown, an uncoated portion 11c on which a positive electrode tab lead 13 and an adhesive material 14 are arranged is provided between the end 11d and the end 11e of the positive electrode collector 11 (e.g., the central portion). In addition, although not shown in the figure, the uncoated portion 11c may be provided only on one of the end 11d on the X1 side and the end 11e on the X2 side of the positive electrode collector 11. It should be noted that the positive electrode plate 110 is an example of the "first electrode" of the present disclosure.
[0065] In the above embodiment, an example in which the adhesive material 14 is arranged on the uncoated portion 11c of the positive electrode current collector 11 is shown, but the present disclosure is not limited thereto. The adhesive material 14 may also be arranged on the negative electrode current collector plate. Fig. 9 In the example shown, in addition to the coated portion 21a and the uncoated portion 21b, an uncoated portion 21c is provided in the negative electrode collector 21 of the negative electrode plate 120. The negative electrode tab lead 23 and the adhesive material 14 are arranged in the uncoated portion 21c. The negative electrode tab lead 23 is sandwiched by two adhesive materials 14 in the uncoated portion 21c. It should be noted that the uncoated portion 21c is provided at the end 21d on the X1 side of the negative electrode collector 21 and the end 21e on the X2 side of the negative electrode collector 21, respectively. In addition, the negative electrode plate 120 is an example of the "second electrode" disclosed in the present invention.
[0066] In the above embodiment, an example is shown where the adhesive material 14 and the positive electrode tab lead 13 are adjacent to each other in the X direction, but the present disclosure is not limited thereto. Fig.10In the uncoated portion 11h of the positive electrode plate 210 shown, in addition to the adhesive material 14 on both sides of the positive electrode tab lead 13 in the X direction, the adhesive material 114 is arranged adjacent to the positive electrode tab lead 13 on the Z2 side of the positive electrode tab lead 13. In the uncoated portion 11i, the adhesive material 114 is arranged adjacent to the positive electrode tab lead 13 on the Z2 side of the positive electrode tab lead 13. It should be noted that in the uncoated portion 11h, the adhesive material 14 and the adhesive material 114 can also be combined and arranged as one adhesive material. In addition, the positive electrode plate 210 and the adhesive material 114 are examples of the "first electrode" and the "buffer material" of the present disclosure, respectively.
[0067] In the above embodiment, an example is shown in which the thickness t14 of the adhesive material 14 is greater than the thickness t13 of the positive electrode tab lead 13, but the present invention is not limited thereto. The thickness t14 of the adhesive material 14 may be equal to the thickness t13 of the positive electrode tab lead 13. In addition, the thickness t12 of the positive electrode mixture layer 12 may be equal to the thickness t13 of the positive electrode tab lead 13. The thickness t14 of the adhesive material 14 may be equal to the thickness t12 of the positive electrode mixture layer 12.
[0068] In the above embodiment, an example in which the adhesive material 14 is arranged on the uncoated portion 11c is shown, but the present disclosure is not limited thereto. A non-adhesive cushioning material (such as rubber) may be arranged on the uncoated portion 11c.
[0069] In the above embodiment, an example is shown in which the adhesive material 14 extends in the axial direction along the uncoated portion 11c, but the present disclosure is not limited thereto. Fig.11 In the positive electrode plate 310 shown, the adhesive material 214 is arranged only at the end of the uncoated portion 11j on the Z1 side. In addition, the adhesive material 214 is arranged only near the center of the uncoated portion 11k in the Z direction. It should be noted that the positive electrode plate 310 and the adhesive material 214 are examples of the "first electrode" and "buffer material" of the present disclosure, respectively.
[0070] In the above embodiment, an example in which a plurality of positive electrode tab leads 13 are provided is shown, but the present disclosure is not limited thereto. Only one positive electrode tab lead 13 may be provided.
[0071] In the above embodiment, an example in which two adhesive materials 14 are arranged in the uncoated portion 11 c is shown, but the present disclosure is not limited thereto. Only one adhesive material 14 may be arranged in the uncoated portion 11 c.
[0072] It should be noted that the structures of the above-mentioned embodiment and the above-mentioned modifications may be combined with each other.
[0073] Although the embodiments of the present invention have been described, the embodiments disclosed this time should be considered to be illustrative in all aspects and not restrictive. The scope of the present invention is indicated by the claims, and it is intended to include all modifications within the meaning and scope equivalent to the claims.
Claims
1. A power storage unit, wherein: The power storage unit has: A wound electrode body comprising a first electrode, a second electrode, and a separator disposed between the first electrode and the second electrode; as well as a casing for housing the wound electrode body, The wound electrode body is formed by winding the first electrode, the second electrode, and the separator so that the first electrode, the second electrode, and the separator surround a winding axis. The first electrode comprises: Current collector; An electrode material layer, applied to a portion of the current collector; a tab lead provided so as to protrude from the current collector in the axial direction of the wound electrode body; and Cushioning materials, The current collector includes an uncoated portion not coated with the electrode material layer, The tab lead is arranged at the uncoated portion, The buffer material is disposed at a position adjacent to the tab lead in the uncoated portion.
2. The power storage unit according to claim 1, wherein: The elastic modulus of the buffer material is lower than the elastic modulus of the tab lead. In a state where the first electrode is expanded into a sheet shape, a thickness of the buffer material in a direction perpendicular to the current collector is equal to or greater than a thickness of the tab lead in the perpendicular direction.
3. The power storage unit according to claim 2, wherein: The elastic modulus of the electrode material layer is lower than the elastic modulus of the tab lead. In a state where the first electrode is expanded into a sheet shape, the thickness of the electrode material layer in the orthogonal direction is equal to or greater than the thickness of the tab lead in the orthogonal direction.
4. The power storage unit according to claim 3, wherein: The elastic modulus of the buffer material is lower than the elastic modulus of the electrode material layer, In a state where the first electrode is expanded into a sheet shape, the thickness of the buffer material in the orthogonal direction is equal to or greater than the thickness of the electrode material layer in the orthogonal direction.
5. The power storage unit according to any one of claims 2 to 4, wherein: When the first electrode is wound together with the second electrode and the separator, an absolute value of a difference between a radial thickness of the buffer material of the wound electrode body and a radial thickness of the tab lead is less than a radial thickness of the collector.
6. The power storage unit according to any one of claims 1 to 4, wherein: The uncoated portion is provided at an end portion of the current collector in a winding direction of the wound electrode body.
7. The power storage unit according to claim 6, wherein: The buffer material includes an adhesive material.
8. The power storage unit according to any one of claims 1 to 4, wherein: The uncoated portion extends in the axial direction in which the winding axis extends, The buffer material is provided so as to extend along the uncoated portion extending in the axial direction.