Battery cover and electronic equipment

By setting a filler layer and an ink layer on the fiberglass layer of the battery cover, the marking problem caused by the shrinkage of the resin material is solved, and the aesthetics of the battery cover is improved and the process simplified is simplified, avoiding the difficulty of covering a large amount of ink.

CN119069932APending Publication Date: 2024-12-03HUAWEI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310639121.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-31
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the prior art, when making a battery cover, the appearance surface has a boss or pit feature mark due to the shrinkage of the resin material, and a large amount of ink is required to be sprayed to cover it, which is difficult to realize the process and affects the aesthetics and cost.

Method used

A laminated glass fiber assembly and filler layer structure is adopted, where one side of the glass fiber layer is provided with local characteristics, and the mark is covered by a filler layer (resin material and filler mixture). The filler layer is designed to be rough to reduce the marking effect, and If necessary, add the ink layer for further covering.

Benefits of technology

Effectively avoid or reduce the need to spray a large amount of ink, improve the appearance uniformity and aesthetics of the battery cover, simplify the process flow, and reduce costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069932A_ABST
    Figure CN119069932A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides a battery cover and electronic equipment. The battery cover at least comprises a glass fiber assembly and a filler layer which are stacked, the glass fiber assembly comprises a glass fiber layer and local features located on one face of the glass fiber layer. The filler layer is positioned on one surface, deviating from the local feature, of the glass fiber layer; the filler layer is configured as the appearance surface of the battery cover, and the material adopted by the filler layer is a mixture of a resin material and a filler. Therefore, the technical problems that a large amount of ink needs to be sprayed to cover the marks and the process is difficult to implement when the battery cover is manufactured in the prior art can be avoided or relieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present application relate to the field of terminal technology, and in particular to a battery cover and an electronic device. Background Art

[0002] Mobile phones, computers and other electronic devices have become inseparable from our lives. They can be seen everywhere in our lives and have greatly improved people's living standards. The aesthetics of electronic devices, such as the aesthetics of electronic device shells, directly affects consumers' purchasing desire.

[0003] Taking the mobile phone as an example of an electronic device, in the related art, in order to match the overall structure of the mobile phone, the inner surface of the battery cover (that is, the side of the battery cover facing the battery) is usually designed with boss features or pit features in local positions. After the battery cover is manufactured and formed, due to the shrinkage of the resin material, the appearance surface of the battery cover (that is, the side of the battery cover facing away from the battery) will have corresponding boss features or pit features. Generally, ink needs to be sprayed to cover the marks to reduce the impact on the aesthetics of the appearance of the battery cover.

[0004] However, when the above solution is adopted, a large amount of ink needs to be sprayed to cover the mark, which makes the process difficult to implement. Summary of the invention

[0005] The present application provides a battery cover and an electronic device, which can avoid or alleviate the technical problem in the prior art that a large amount of ink needs to be sprayed to cover the mark when making the battery cover, and the process is difficult to implement.

[0006] In a first aspect, an embodiment of the present application provides a battery cover, the battery cover at least comprising: a glass fiber component and a filler layer arranged in layers; the glass fiber component comprises: a glass fiber layer and a local feature located on one side of the glass fiber layer; the filler layer is located on a side of the glass fiber layer away from the local feature;

[0007] The filler layer is configured as the appearance surface of the battery cover, and the material used for the filler layer is a mixture of resin material and filler.

[0008] The battery cover provided by the embodiment of the present application has a local feature on one side of the glass fiber layer. During the manufacturing process, the side of the glass fiber layer that is away from the local feature will show a corresponding mark. A filler layer is provided on the side of the glass fiber layer that is away from the local feature, wherein the material used for the filler layer is a resin material and a filler mixture, and the resin material and the filler mixture are combined with each other to effectively cover the mark presented by the side of the glass fiber layer that is away from the local feature. In this way, compared with the prior art, the embodiment of the present application can avoid or alleviate the technical problem that a large amount of ink needs to be sprayed to cover the mark when manufacturing the battery cover in the prior art, and the process is difficult to implement.

[0009] In a possible implementation manner, in the filler layer, the proportion of the filler mixture is 1-20%.

[0010] In the filler layer, the filler mixture can play a good covering role, the proportion of the resin material is relatively high, the resin material has good fluidity, and the filler layer serves as the appearance surface of the battery cover. The resin material can make the filler layer fuller, thereby better playing the role of reducing the mark.

[0011] In a possible implementation manner, the resin material is epoxy resin or acrylic resin.

[0012] Epoxy resin is a high molecular polymer with the molecular formula (C11H12O3)n. It is a general term for a class of polymers containing two or more epoxy groups in the molecule. Epoxy resin is the polycondensation product of epichlorohydrin and bisphenol A or polyol. Due to the chemical activity of the epoxy group, it can be opened with a variety of compounds containing active hydrogen, cured and cross-linked to form a network structure. Therefore, epoxy resin is a thermosetting resin that can be used to prepare thermosetting composite materials or adhesives.

[0013] Acrylic resin, also known as acrylic resin emulsion in Chinese, has a molecular formula of (C3H4O2)n. Acrylic resin is light in color, water-white and transparent. The coating has excellent properties, including good light resistance, weather resistance, heat resistance, over-baking resistance, chemical resistance and corrosion resistance.

[0014] In a possible implementation, the filler mixture is titanium dioxide.

[0015] The scientific name of titanium dioxide is titanium dioxide, and its molecular formula is TiO2. Titanium dioxide is the strongest tinting power among white pigments, with excellent hiding power and color fastness.

[0016] In a possible implementation manner, a surface of the filler layer facing away from the glass fiber layer is rough.

[0017] By designing the side of the filler layer facing away from the glass fiber layer to be rough, the rough filler layer has a frosted effect, which can visually weaken the mark of the local features on the side of the filler layer facing away from the glass fiber layer, that is, it can weaken or completely hide the outline of the local features on the side of the filler layer facing away from the glass fiber layer, thereby weakening the impact of the local features on the appearance of the battery cover, which helps to make the appearance of the battery cover uniform.

[0018] In a possible implementation manner, the roughness of a side of the filler layer facing away from the glass fiber layer is between 0.5 um and 10 um.

[0019] In a possible implementation, the material used for the glass fiber layer is a mixture of resin material and glass fiber.

[0020] The resin material and the glass fiber mixture are combined to make the glass fiber layer, and the glass fiber layer serves as the inner surface of the battery cover. The combination of the resin material and the glass fiber mixture can ensure the structural stability and material gloss of the glass fiber layer, while also ensuring that the glass fiber layer has a certain drop resistance.

[0021] Among them, glass fiber is an inorganic non-metallic material with excellent performance, and its advantages are good insulation, strong heat resistance, good corrosion resistance and high mechanical strength. Glass fiber is made of six kinds of minerals, namely pyrophyllite, quartz sand, limestone, dolomite, colemanite and boraxite, through high-temperature melting, wire drawing, winding, weaving and other processes. The diameter of its monofilament is from several microns to more than twenty microns, and each bundle of fiber strands is composed of hundreds or even thousands of monofilaments. Glass fiber can be used as reinforcing material in composite materials, electrical insulation material and thermal insulation material, circuit substrate, etc. Therefore, glass fiber has great performance advantages as glass fiber layer 111.

[0022] In a possible implementation manner, the resin material is epoxy resin or acrylic resin.

[0023] In a possible implementation, the glass fiber layer includes: a first glass fiber layer; or the glass fiber layer includes: a first glass fiber layer and a second glass fiber layer which are stacked; the textures of the first glass fiber layer and the second glass fiber layer are different;

[0024] Alternatively, the glass fiber layer includes: a first glass fiber layer, a second glass fiber layer, and a third glass fiber layer located between the first glass fiber layer and the second glass fiber layer; the textures of the first glass fiber layer and the third glass fiber layer are different, or the textures of the second glass fiber layer and the third glass fiber layer are different, or the textures of the first glass fiber layer, the second glass fiber layer, and the third glass fiber layer are all different.

[0025] In actual application scenarios, the number of layers of the glass fiber layer can be set according to different requirements. The glass fiber layer including the first glass fiber layer can ensure the performance of the glass fiber layer.

[0026] When the glass fiber layer includes a first glass fiber layer and a second glass fiber layer that are stacked, and the textures of the first glass fiber layer and the second glass fiber layer are different, that is, when the first glass fiber layer and the second glass fiber layer are stacked on each other, the texture of the first glass fiber layer and the texture of the second glass fiber layer will not overlap, but will be staggered, thereby improving the overall structural stability of the glass fiber layer.

[0027] When the glass fiber layer includes a first glass fiber layer, a second glass fiber layer and a third glass fiber layer stacked in sequence, that is, the third glass fiber layer is located between the first glass fiber layer and the second glass fiber layer, at this time, the textures of the two adjacent layers are different, that is, when the first glass fiber layer, the second glass fiber layer and the third glass fiber layer are stacked on each other, the textures of the two adjacent layers will not overlap, and the distribution is staggered, which can improve the overall structural stability of the glass fiber layer.

[0028] In a possible implementation manner, an ink layer is further provided on a side of the filler layer facing away from the glass fiber layer.

[0029] By providing an ink layer on the side of the filler layer away from the glass fiber layer, the ink layer can play a further covering role. In addition, ink layers of different colors and patterns can also help the appearance of the battery cover to present different appearance effects, thereby improving the aesthetics of the battery cover.

[0030] In a second aspect, an embodiment of the present application provides an electronic device, which at least includes: a display screen, a middle frame, and any of the battery covers described above, wherein the display screen and the battery cover are respectively located on two sides of the middle frame.

[0031] The electronic device provided in the embodiment of the present application includes at least a battery cover, in which a glass fiber layer has a local feature on one side, and during the manufacturing process, the side of the glass fiber layer that is away from the local feature will present a corresponding mark, by providing a filler layer on the side of the glass fiber layer that is away from the local feature, wherein the material used for the filler layer is a resin material and a filler mixture, and the resin material and the filler mixture are combined with each other to effectively cover the mark presented by the side of the glass fiber layer that is away from the local feature. In this way, compared with the prior art, the embodiment of the present application can avoid or alleviate the technical problem of the prior art that a large amount of ink needs to be sprayed to cover the mark when making the battery cover, and the process is difficult to implement. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 A schematic diagram of the overall structure of an electronic device provided in one embodiment of the present application;

[0033] Figure 2 A schematic diagram of a disassembled structure of an electronic device provided in an embodiment of the present application;

[0034] Figure 3 A schematic diagram of a disassembled structure of an electronic device provided in an embodiment of the present application;

[0035] Figure 4 A schematic diagram of the structure of a battery cover in an electronic device provided in an embodiment of the present application;

[0036] Figure 5 An electronic device provided in an embodiment of the present application is Figure 4A schematic diagram of a cross-sectional structure in the AA direction;

[0037] Figure 6 An electronic device provided in an embodiment of the present application is Figure 4 Schematic diagram of another cross-sectional structure in the AA direction.

[0038] Description of reference numerals:

[0039] 100-battery cover; 100a-appearance surface;

[0040] 100b-inner surface; 110-glass fiber component;

[0041] 111-glass fiber layer; 1111-first glass fiber layer;

[0042] 1112-second glass fiber layer; 1113-third glass fiber layer;

[0043] 112- local features; 120- packing layer;

[0044] 121- rough part; 130- ink layer;

[0045] 200-mobile phone; 210-display screen;

[0046] 211-opening; 220-middle frame;

[0047] 221-frame; 222-metal middle plate;

[0048] 230-circuit board; 240-battery;

[0049] 250a-front camera assembly; 250b-rear camera assembly;

[0050] 300-forming mold; 310-upper mold;

[0051] 320-lower mold. DETAILED DESCRIPTION

[0052] The terms used in the implementation method part of this application are only used to explain the specific embodiments of this application, and are not intended to limit this application. The implementation method of the embodiments of this application will be described in detail below with reference to the accompanying drawings.

[0053] The embodiment of the present application provides an electronic device, which may include but is not limited to a mobile phone, a tablet computer, a laptop computer, an ultra-mobile personal computer (UMPC), a handheld computer, a walkie-talkie, a netbook, a point of sales (POS) machine, a personal digital assistant (PDA), a wearable device, a virtual reality device, a wireless USB flash drive, a Bluetooth speaker / headphone, or a mobile or fixed terminal with a battery cover, such as a vehicle-mounted front-end device, a driving recorder, and a security device.

[0054] Among them, in the embodiment of the present application, the mobile phone 200 is taken as an example of the above-mentioned electronic device for description. The mobile phone 200 provided in the embodiment of the present application can be a curved screen mobile phone or a flat screen mobile phone. In the embodiment of the present application, the flat screen mobile phone is taken as an example for description.

[0055] Figure 1 and Figure 2 The overall structure and split structure of the mobile phone 200 are shown respectively. The display screen 210 of the mobile phone 200 provided in the embodiment of the present application can be a water drop screen, a notch screen, a full screen or a punch hole screen (see Figure 1 As shown), for example, a hole 211 is opened on the display screen 210, and the following description is explained using the hole-punch screen as an example.

[0056] See also Figure 2 As shown, the mobile phone 200 may include: a display screen 210 , a middle frame 220 and a battery cover 100 , wherein the display screen 210 and the battery cover 100 are respectively located on two sides of the middle frame 220 .

[0057] In addition, the mobile phone 200 may further include a battery 240 located between the middle frame 220 and the battery cover 100, wherein the battery 240 may be disposed on a side of the middle frame 220 facing the battery cover 100 (eg, Figure 2 As shown), or the battery 240 can be arranged on the side of the middle frame 220 facing the display screen 210. For example, the side of the middle frame 220 facing the battery cover 100 can have a battery compartment (not shown in the figure), and the battery 240 is installed in the battery compartment.

[0058] In some other examples, the mobile phone 200 may further include a circuit board 230, wherein the circuit board 230 may be disposed on the middle frame 220, for example, the circuit board 230 may be disposed on a side of the middle frame 220 facing the battery cover 100 (eg, Figure 2 As shown), or the circuit board 230 can be arranged on a side of the middle frame 220 facing the display screen 210, and the display screen 210 and the battery cover 100 are respectively located on both sides of the middle frame 220.

[0059] Among them, the battery 240 can be connected to the charging management module and the circuit board 230 through the power management module. The power management module receives the input of the battery 240 and / or the charging management module, and supplies power to the processor, internal memory, external memory, display screen 210, camera module and communication module. The power management module can also be used to monitor parameters such as the capacity of the battery 240, the number of cycles of the battery 240, and the health status of the battery 240 (leakage, impedance). In some other embodiments, the power management module can also be set in the processor of the circuit board 230. In some other embodiments, the power management module and the charging management module can also be set in the same device.

[0060] When the mobile phone 200 is a flat screen mobile phone, the display screen 210 may be an organic light-emitting diode (OLED) display screen or a liquid crystal display (LCD) display screen. When the mobile phone 200 is a curved screen mobile phone, the display screen 210 may be an OLED display screen. It should be understood that the display screen 210 may include a display and a touch control device, the display is used to output display content to the user, and the touch control device is used to receive touch events input by the user on the display screen 210.

[0061] Continue to refer to Figure 2 , the middle frame 220 may include a metal middle plate 222 and a frame 221, and the frame 221 is arranged around the outer periphery of the metal middle plate 222. Generally, the frame 221 may include a top frame, a bottom frame, a left frame and a right frame, and the top frame, the bottom frame, the left frame and the right frame form a frame of a square ring structure. Among them, the material of the metal middle plate 222 includes but is not limited to aluminum plate, aluminum alloy, stainless steel, steel-aluminum composite die-casting plate, titanium alloy or magnesium alloy. The frame 221 may be a metal frame, a ceramic frame, or a glass frame. When the frame 221 is a metal frame, the material of the metal frame is but is not limited to aluminum alloy, stainless steel, steel-aluminum composite die-casting plate or titanium alloy. Among them, the metal middle plate 222 and the frame 221 can be clamped, welded, bonded or integrally formed, or the metal middle plate 222 and the frame 221 can be fixedly connected by injection molding.

[0062] The top frame and the bottom frame are arranged opposite to each other, the left frame and the right frame are arranged opposite to each other, the top frame is connected to one end of the left frame and one end of the right frame with rounded corners, and the bottom frame is connected to the other end of the left frame and the other end of the right frame with rounded corners, thereby forming a rounded rectangular area together. The rear shell grounding surface is arranged in the rounded rectangular area and is connected to the top frame, the bottom frame, the left frame and the right frame respectively. It can be understood that the rear shell grounding surface can be the battery cover 100 of the mobile phone 200.

[0063] The battery cover 100 may be a metal back cover, a glass back cover, a plastic back cover, or a ceramic back cover. In the embodiment of the present application, the material of the battery cover 100 is not limited and is not limited to the above examples.

[0064] It should be noted that, in some examples, the battery cover 100 of the mobile phone 200 can be connected to the frame 221 to form an integrally formed (Unibody) back shell. For example, the mobile phone 200 may include: a display screen 210, a metal middle plate 222 and a back shell. The back shell can be a back shell formed by integrally forming (Unibody) the frame 221 and the battery cover 100, so that the circuit board 230 and the battery 240 are located in the space surrounded by the metal middle plate 222 and the back shell.

[0065] In order to realize the shooting function, the mobile phone 200 may further include: a camera assembly, which may be arranged on the middle frame 220, and the camera of the camera assembly faces the display screen 210 or the battery cover 100. The camera assembly may be a front camera assembly 250a or a rear camera assembly 250b, or the number of camera assemblies may be two, one of which may be a front camera assembly 250a and the other may be a rear camera assembly 250b (see Figure 3 shown).

[0066] Specifically, the rear camera assembly 250b can be arranged on the side of the metal middle plate 222 facing the battery cover 100, the display screen 210 is provided with an opening 211, and the lens of the rear camera assembly 250b corresponds to the opening 211. The battery cover 100 can be provided with a mounting hole (not shown in the figure) for mounting a partial area of ​​the rear camera assembly 250b.

[0067] Of course, the rear camera assembly 250b can also be installed on the side of the battery cover 100 facing the metal middle plate 222. The front camera assembly 250a can be arranged on the side of the metal middle plate 222 facing the display screen 210, or the front camera assembly 250a can be arranged on the side of the metal middle plate 222 facing the battery cover 100, or the front camera assembly 250a can also be arranged on the side of the battery cover 100 facing the display screen 210, and the metal middle plate 222 is provided with an opening for exposing the lens end of the front camera assembly 250a.

[0068] In the embodiment of the present application, the location of the front camera assembly 250a and the rear camera assembly 250b may include but is not limited to the above description. In some embodiments, the number of the front camera assembly 250a and the rear camera assembly 250b provided in the notebook computer 300 may be 1 or N, where N is a positive integer greater than or equal to 1.

[0069] It is to be understood that the structure illustrated in the embodiment of the present application does not constitute a specific limitation on the mobile phone 200. In other embodiments of the present application, the mobile phone 200 may include more or fewer components than shown in the figure, or combine some components, or split some components, or arrange the components differently. The components shown in the figure may be implemented in hardware, software, or a combination of software and hardware.

[0070] In the related art, in order to match the overall structure of the mobile phone 200, a boss feature or a pit feature is usually designed at a local position on the side of the battery cover 100 facing the battery 240. After the battery cover 100 is manufactured and formed, due to the shrinkage of the resin material, a corresponding boss feature contour or pit feature contour mark will appear on the side of the battery cover 100 facing away from the battery 240. Generally, a large amount of ink needs to be sprayed to cover the mark, so as to reduce the impact on the aesthetics of the exterior surface of the battery cover 100.

[0071] However, spraying a large amount of ink to cover the mark is difficult to completely eliminate the mark presented by the boss feature profile or the pit feature profile, and the process is relatively difficult to implement. Moreover, spraying a large amount of ink on the appearance surface of the battery cover 100 not only affects the thinness of the battery cover 100, but also wastes costs.

[0072] Based on this, the embodiments of the present application provide a new battery cover and an electronic device having the battery cover, which can be applied to electronic devices (such as mobile phones or computers, etc.) to solve the above technical problems. Specifically, the embodiments of the present application provide a battery cover and an electronic device, wherein the battery cover at least includes: a glass fiber component and a filler layer stacked; the glass fiber component includes: a glass fiber layer and a local feature located on one side of the glass fiber layer; the filler layer is located on the side of the glass fiber layer away from the local feature; the filler layer is configured as the appearance surface of the battery cover, and the material used for the filler layer is a mixture of resin material and filler. In this way, the technical problem that a large amount of ink needs to be sprayed to cover the mark when making the battery cover in the prior art, and the process is difficult to implement, can be avoided or alleviated.

[0073] The specific structure of the battery cover is described in detail below with reference to specific drawings and taking different embodiments as examples.

[0074] Reference Figure 4 As shown, the present application embodiment provides a battery cover 100, which can be applied to an electronic device (such as a mobile phone 200). Specifically, referring to Figure 5 and Figure 6As shown, the battery cover 100 may include at least a stacked arrangement of: a glass fiber component 110 and a filler layer 120, wherein the glass fiber component 110 may include: a glass fiber layer 111 and a local feature 112, the local feature 112 is located on one side of the glass fiber layer 111, and the filler layer 120 is located on the side of the glass fiber layer 111 away from the local feature 112.

[0075] It can be understood that, in the embodiment of the present application, the filler layer 120 is configured as the appearance surface 100 a of the battery cover 100 , and the material used for the filler layer 120 can be a mixture of resin material and filler.

[0076] In the battery cover 100, one side of the glass fiber layer 111 has a local feature 112. In the manufacturing process, specifically, see Figure 5 As shown, the battery cover 100 is generally pressed and formed by a molding mold 300, the upper mold 310 is in contact with the appearance surface 100a of the battery cover 100, that is, the filler layer 120, and the lower mold 320 is in contact with the inner surface 100b of the battery cover 100, that is, the glass fiber component 110. During the actual pressing process, the side of the glass fiber layer 111 that is away from the local feature 112 will show an imprint corresponding to the local feature 112.

[0077] In the embodiment of the present application, a filler layer 120 is provided on the side of the glass fiber layer 111 away from the local feature 112, wherein the material used for the filler layer 120 is a resin material and a filler mixture, and the resin material and the filler mixture are combined to effectively cover the mark presented on the side of the glass fiber layer 111 away from the local feature 112. In this way, compared with the prior art, the embodiment of the present application can avoid or alleviate the technical problem of the prior art that a large amount of ink needs to be sprayed to cover the mark when making the battery cover 100, which makes the process difficult to implement.

[0078] It should be noted that the local feature 112 may be a boss feature, a pit feature or other pattern features, which is not limited in the embodiment of the present application.

[0079] In the embodiment of the present application, the proportion of the filler mixture in the filler layer 120 of the battery cover 100 may be 1-20%. For example, the proportion of the filler mixture in the filler layer 120 may be 1%, 5%, 10%, 15% or 20%, etc., and the embodiment of the present application is not limited to this, nor is it limited to the above examples.

[0080] In the filling layer 120, the filling mixture can play a good covering role, the proportion of the resin material is relatively high, and the resin material has good fluidity. The filling layer 120 serves as the appearance surface 100a of the battery cover 100, and the resin material can make the filling layer 120 filled more fully, thereby better playing the role of reducing the mark.

[0081] In the embodiment of the present application, the resin material may be epoxy resin.

[0082] Epoxy resin is a high molecular polymer with the molecular formula (C11H12O3)n. It is a general term for a class of polymers containing two or more epoxy groups in the molecule. Epoxy resin is the polycondensation product of epichlorohydrin and bisphenol A or polyol. Due to the chemical activity of the epoxy group, it can be opened with a variety of compounds containing active hydrogen, cured and cross-linked to form a network structure. Therefore, epoxy resin is a thermosetting resin that can be used to prepare thermosetting composite materials or adhesives.

[0083] Among them, epoxy resin can be classified into pure epoxy resin and modified epoxy resin according to its main components. That is to say, the resin material used in the filler layer 120 in the embodiment of the present application can be pure epoxy resin or modified epoxy resin, and the embodiment of the present application does not limit this.

[0084] Alternatively, in some embodiments, the resin material may also be acrylic resin.

[0085] Acrylic resin, also known as acrylic resin emulsion in Chinese, has a molecular formula of (C3H4O2)n. Acrylic resin is light in color, water-white and transparent. The coating has excellent properties, including good light resistance, weather resistance, heat resistance, over-baking resistance, chemical resistance and corrosion resistance.

[0086] Among them, acrylic resin can generally be divided into solvent-based thermoplastic acrylic resin, solvent-based thermosetting acrylic resin, water-based acrylic resin, high-solid acrylic resin, radiation-curable acrylic resin, acrylic resin for powder coating, etc. That is to say, the resin material used in the filler layer 120 in the embodiment of the present application can be solvent-based thermoplastic acrylic resin, solvent-based thermosetting acrylic resin, water-based acrylic resin, high-solid acrylic resin, radiation-curable acrylic resin, acrylic resin for powder coating, or other types of acrylic resin, and the embodiment of the present application is not limited to this, nor is it limited to the above examples.

[0087] In the embodiment of the present application, the filler mixture may be titanium dioxide.

[0088] The scientific name of titanium dioxide is titanium dioxide, and its molecular formula is TiO2. Titanium dioxide is the strongest tinting power among white pigments, with excellent hiding power and color fastness.

[0089] Specifically, the filler mixture can be nano-scale ultrafine titanium dioxide, which has semiconductor properties, high stability, high transparency, high activity and high dispersibility, and no toxicity and color effect.

[0090] In the embodiment of the present application, the side of the filler layer 120 facing away from the glass fiber layer 111 may be rough. Figure 6 In the embodiment, a surface of the filler layer 120 facing away from the glass fiber layer 111 has a rough portion 121 .

[0091] By designing the side of the filler layer 120 facing away from the glass fiber layer 111 to be rough, the rough filler layer 120 has a frosted effect, which can visually weaken the mark of the local feature 112 on the side of the filler layer 120 facing away from the glass fiber layer 111, that is, it can weaken or completely hide the outline of the local feature 112 on the side of the filler layer 120 facing away from the glass fiber layer 111, thereby weakening the impact of the local feature 112 on the appearance surface 100a of the battery cover 100, which helps to make the appearance surface 100a of the battery cover 100 uniform.

[0092] It should be noted that, in the embodiment of the present application, the roughness of the side of the filler layer 120 away from the glass fiber layer 111 may be between 0.5 um and 10 um.

[0093] Exemplarily, the roughness of the side of the filler layer 120 facing away from the glass fiber layer 111 may be 0.5um, 2um, 4um, 6um, 8um or 10um, etc., which is not limited to the above examples in the embodiments of the present application.

[0094] It should be noted here that the numerical values ​​and numerical ranges involved in this application are approximate values. Due to the influence of the manufacturing process, there may be a certain range of errors, which can be considered negligible by those skilled in the art.

[0095] In the embodiment of the present application, the material used for the glass fiber layer 111 may be a mixture of resin material and glass fiber.

[0096] The resin material and the glass fiber mixture are combined to make the glass fiber layer 111, and the glass fiber layer 111 serves as the inner surface 100b of the battery cover 100. The combination of the resin material and the glass fiber mixture can ensure the structural stability and material gloss of the glass fiber layer 111, and can also ensure that the glass fiber layer 111 has a certain drop resistance.

[0097] In some embodiments, the resin material may be epoxy resin or acrylic resin.

[0098] Specifically, the resin material used for the glass fiber layer 111 in the embodiment of the present application may be pure epoxy resin or modified epoxy resin, which is not limited in the embodiment of the present application.

[0099] Alternatively, the resin material used for the glass fiber layer 111 in the embodiment of the present application may be a solvent-based thermoplastic acrylic resin, a solvent-based thermosetting acrylic resin, a water-based acrylic resin, a high-solid acrylic resin, a radiation-curable acrylic resin, an acrylic resin for powder coatings, or other types of acrylic resins, and the embodiment of the present application is not limited to this and is not limited to the above examples.

[0100] The glass fiber mixture, namely the glass fiber mixture, is used as the basic material of the glass fiber layer 111 and provides the glass fiber layer 111 with better structural strength.

[0101] Specifically, glass fiber is an inorganic non-metallic material with excellent performance, and its advantages are good insulation, strong heat resistance, good corrosion resistance and high mechanical strength.

[0102] Glass fiber is made of six kinds of minerals, namely pyrophyllite, quartz sand, limestone, dolomite, colemanite and magnesia stone, through high temperature melting, wire drawing, winding, weaving and other processes. The diameter of its single filament is several microns to more than 20 microns, and each bundle of fiber raw filaments is composed of hundreds or even thousands of single filaments. Glass fiber can be used as reinforcing material in composite materials, electrical insulation material and thermal insulation material, circuit substrate, etc. Therefore, glass fiber has great performance advantages as glass fiber layer 111.

[0103] In addition, it can be understood that the embodiment of the present application does not limit the distribution ratio of the resin material and the glass fiber mixture in the glass fiber layer 111 of the battery cover 100, and the material composition can be the same or similar to that of the conventional glass fiber layer 111, which will not be repeated here.

[0104] It should be noted that, in the embodiment of the present application, the specific structure of the glass fiber layer 111 may include but is not limited to the following possible implementations:

[0105] A possible implementation is that the glass fiber layer 111 may include: a first glass fiber layer 1111, wherein the material used for the first glass fiber layer 111 may be a mixture of resin material and glass fiber. The glass fiber layer 111 includes the first glass fiber layer 1111 to ensure the performance of the glass fiber layer 111.

[0106] Another possible implementation is that the glass fiber layer 111 may include a first glass fiber layer 1111 and a second glass fiber layer 1112 which are stacked, and the first glass fiber layer 1111 and the second glass fiber layer 1112 have different textures.

[0107] When the glass fiber layer 111 may include a first glass fiber layer 1111 and a second glass fiber layer 1112 that are stacked, and the textures of the first glass fiber layer 1111 and the second glass fiber layer 1112 are different, that is, when the first glass fiber layer 1111 and the second glass fiber layer 1112 are stacked on each other, the texture of the first glass fiber layer 1111 and the texture of the second glass fiber layer 1112 will not overlap, but will be staggered, which can improve the overall structural stability of the glass fiber layer 111.

[0108] Another possible implementation is that the glass fiber layer 111 may include a first glass fiber layer 1111 , a second glass fiber layer 1112 , and a third glass fiber layer 1113 which are stacked, wherein the third glass fiber layer 1113 is located between the first glass fiber layer 1111 and the second glass fiber layer 1112 .

[0109] When the glass fiber layer 111 may include a first glass fiber layer 1111, a second glass fiber layer 1112 and a third glass fiber layer 1113 which are stacked in sequence, that is, the third glass fiber layer 1113 is located between the first glass fiber layer 1111 and the second glass fiber layer 1112, at this time, the textures of the two adjacent layers are different, that is, when the first glass fiber layer 1111, the second glass fiber layer 1112 and the third glass fiber layer 1113 are stacked on each other, the textures of the two adjacent layers will not overlap, but are staggered, which can improve the overall structural stability of the glass fiber layer 111.

[0110] Specifically, the texture of the first glass fiber layer 1111 and the texture of the third glass fiber layer 1113 can be different. In this case, the texture of the first glass fiber layer 1111 and the texture of the second glass fiber layer 1112 can be the same or different, and the texture of the second glass fiber layer 1112 and the texture of the third glass fiber layer 1113 can be the same or different.

[0111] Alternatively, in some embodiments, the textures of the second glass fiber layer 1112 and the third glass fiber layer 1113 may be different. In this case, the texture of the first glass fiber layer 1111 and the texture of the second glass fiber layer 1112 may be the same or different, and the texture of the first glass fiber layer 1111 and the texture of the third glass fiber layer 1113 may be the same or different.

[0112] Alternatively, in some other embodiments, the textures of the first glass fiber layer 1111 , the second glass fiber layer 1112 , and the third glass fiber layer 1113 may all be different.

[0113] It should be noted that in actual application scenarios, the number of layers that the glass fiber layer 111 can include can be set according to different needs. For example, the number of layers of the glass fiber layer 111 can also be four, five, six, seven or more layers, and the embodiments of the present application do not limit this.

[0114] It can be understood that, in the embodiment of the present application, an ink layer 130 may also be provided on the side of the filler layer 120 facing away from the glass fiber layer 111 .

[0115] By providing an ink layer 130 on the side of the filler layer 120 facing away from the glass fiber layer 111 , the ink layer 130 can play a further covering role. In addition, the ink layers 130 of different colors and patterns can also help the appearance surface 100a of the battery cover 100 to present different appearance effects, thereby improving the aesthetics of the battery cover 100.

[0116] In one possible implementation, the ink layer 130 may be a vacuum coating layer, a silk-screen ink layer, an ultraviolet (UV) transfer glue layer, or a UV coating layer, etc. The embodiment of the present application is not limited to this and is not limited to the above examples.

[0117] It should be noted that, in the embodiment of the present application, a texture structure may also be provided on the ink layer 130 .

[0118] It is easy to understand that the texture structure can be a plane texture, a three-dimensional pattern relief texture, or a combination of a plane texture and a three-dimensional pattern relief texture.

[0119] Among them, the planar texture structure can make the appearance surface 100a of the battery cover 100 have a texture effect that moves with the light and appears and disappears (such as the Kevlar texture effect), and the three-dimensional pattern relief texture structure can make the appearance of the battery cover 100 have a three-dimensional relief pattern, thereby enhancing the three-dimensional effect of the battery cover 100 and bringing a special visual experience to the user.

[0120] In addition, in the embodiment of the present application, the battery cover 100 may further include: a protective film layer (not shown in the figure), and the protective film layer may be located on a side of the ink layer 130 away from the filler layer 120 .

[0121] The protective film layer can protect the ink layer 130 , thereby preventing external conditions or factors from affecting the color of the ink layer 130 , that is, the appearance color of the battery cover 100 .

[0122] It should be noted that the protective film layer can be a transparent film layer. Exemplarily, the material used for the protective film layer can be polyethylene terephthalate (PET). The molecular structure of PET plastic is highly symmetrical and has a certain crystal orientation ability, so it has high film-forming property and formability. PET plastic has good optical properties and weather resistance, and amorphous PET plastic has good optical transparency. In addition, PET plastic has excellent wear resistance, friction resistance, dimensional stability and electrical insulation.

[0123] Alternatively, in some embodiments, the material used for the protective film layer may also be cycloolefin polymer (CycloOlefin Polymer, COP).

[0124] COP is a non-crystalline homopolymer formed by the ring-opening heteropolymerization of bicycloheptene (norbornene) under the action of a metallocene catalyst, followed by a hydrogenation reaction. It can be used in medical optical components and high-end pharmaceutical packaging materials. COP has the advantages of high transparency, low birefringence, low water absorption, high rigidity, high heat resistance and good water vapor airtightness.

[0125] Alternatively, in some other embodiments, the material used for the protective film layer may also be polyimide (PI). PI is one of the organic polymer materials with the best comprehensive performance, and PI has a high temperature resistance of more than 400° C. and high insulation performance.

[0126] It can be understood that in the embodiment of the present application, the protective film layer can also be a film layer formed by other materials with protective functions, and the embodiment of the present application is not limited here, nor is it limited to the above examples.

[0127] In the description of the embodiments of the present application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, or it can be an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the embodiments of the present application can be understood according to specific circumstances.

[0128] In the embodiments of the present application, the devices or elements referred to or implied must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the embodiments of the present application. In the description of the embodiments of the present application, the meaning of "multiple" is two or more, unless otherwise precisely and specifically specified.

[0129] The terms "first", "second", "third", "fourth", etc. (if any) in the specification and claims of the embodiments of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable where appropriate, so that the embodiments of the embodiments of the present application described herein can be implemented in an order other than those illustrated or described herein, for example. In addition, the terms "may include" and "have" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0130] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the embodiments of the present application, rather than to limit them. Although the embodiments of the present application have been described in detail with reference to the aforementioned embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents, and these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.

Claims

1. A battery cover, characterized in that: At least the cascade settings include: Glass fiber components and filler layers; The glass fiber component comprises: a glass fiber layer and a local feature located on one side of the glass fiber layer; the filler layer is located on a side of the glass fiber layer away from the local feature; The filler layer is configured as the appearance surface of the battery cover, and the material used for the filler layer is a mixture of resin material and filler.

2. The battery cover according to claim 1, characterized in that: In the filler layer, the proportion of the filler mixture is 1-20%.

3. The battery cover according to claim 1 or 2, characterized in that: The resin material is epoxy resin or acrylic resin.

4. The battery cover according to any one of claims 1 to 3, characterized in that: The filler mixture is titanium dioxide.

5. The battery cover according to any one of claims 1 to 4, characterized in that: The side of the filler layer facing away from the glass fiber layer is rough.

6. The battery cover according to claim 5, characterized in that: The roughness of the side of the filler layer away from the glass fiber layer is 0.5um-10um.

7. The battery cover according to any one of claims 1 to 6, characterized in that: The material used for the glass fiber layer is a mixture of resin material and glass fiber.

8. The battery cover according to claim 7, characterized in that: The resin material is epoxy resin or acrylic resin.

9. The battery cover according to any one of claims 1 to 8, characterized in that: The glass fiber layer comprises: a first glass fiber layer; Alternatively, the glass fiber layer includes: a first glass fiber layer and a second glass fiber layer which are stacked; the textures of the first glass fiber layer and the second glass fiber layer are different; Alternatively, the glass fiber layer includes: a first glass fiber layer, a second glass fiber layer, and a third glass fiber layer located between the first glass fiber layer and the second glass fiber layer; the textures of the first glass fiber layer and the third glass fiber layer are different, or the textures of the second glass fiber layer and the third glass fiber layer are different, or the textures of the first glass fiber layer, the second glass fiber layer, and the third glass fiber layer are all different.

10. The battery cover according to any one of claims 1 to 9, characterized in that: An ink layer is also arranged on the side of the filler layer facing away from the glass fiber layer.

11. An electronic device, characterized in that: At least: A display screen, a middle frame, and a battery cover as described in any one of claims 1 to 10, wherein the display screen and the battery cover are respectively located on two sides of the middle frame.