Anode structure for increasing light polymerization and preparation method thereof
By providing a convex lens-type anode structure with an ITO film layer with a semicircular lens structure on the CMOS substrate, the serious light loss problem in traditional FMM technology is solved, high-brightness display is realized and light leakage is reduced, suitable for high-resolution display Device fabrication.
Patent Information
- Application Number
- CN202411040348.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-12-03
AI Technical Summary
Traditional FMM technology is difficult to achieve high resolution and color display, resulting in serious light loss in OLED display. Especially when PPI requirements are high in the field of silicon-based OLED, it is difficult to produce FMM and cannot achieve high brightness display.
The CMOS substrate is equipped with a pixel anode layer and an ITO film layer. The ITO film layer corresponding to the color filter is a semicircular lens structure. The convex lens anode structure is formed by etching, and the ITO film corresponding to red, green and blue light is formed. The layer thickness varies to reduce light loss.
Effectively reduce light loss, improve light output efficiency, reduce light leakage astigmatism, and achieve higher brightness display. It is suitable for the production of high-resolution display devices.
Smart Images

Figure CN119072153A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of microdisplay technology, and more specifically, relates to an anode structure for increasing light polymerization and a preparation method thereof. Background Art
[0002] As OLED technology continues to mature, OLED display is based on the principle of self-luminescence and has obvious advantages in display effect, response speed, lightness and thinness, and is applied to smart phones, TVs, laptops, smart wearable devices, etc. Compared with traditional AMOLED display technology, micro-OLED has been widely used in the fields of VR and AR. Currently, mainstream VR and AR products all use micro-OLED displays.
[0003] Especially for color display, it is difficult to achieve high-resolution screen production by relying on traditional FMM technology. At present, high-resolution and color display are mainly achieved through the combination of white light OLED and color filter. In this method, OLED light will lose more than 50% of light after passing through the color filter, and it is difficult for the product to achieve a higher brightness display. The panel industry (such as mobile phones) PPI (pixel density) of about 500 can meet the demand, and the production of FFM is feasible under this PPI and can be mass-produced. However, for silicon-based OLED, the minimum PPI requirement is above 2000. In this case, it is very difficult to use FMM (precision metal mask) to produce high-resolution screens and it cannot be produced accordingly. Summary of the invention
[0004] The purpose of the present invention is to solve the problems existing in the prior art and to provide an anode structure and a preparation method thereof which has a simple structure, can effectively reduce light loss, and achieve a higher brightness display and increase light polymerization.
[0005] In order to achieve the above-mentioned purpose, the technical solution adopted by the present invention is: the provided anode structure for increasing light polymerization includes a CMOS substrate, a pixel anode layer is provided on the CMOS substrate, and an ITO film layer is provided on the pixel anode layer, characterized in that: the ITO film layer corresponding to the color filter is a semicircular lens structure.
[0006] In order to make the above technical solution more detailed and specific, the present invention also provides the following further preferred technical solutions to obtain satisfactory practical effects:
[0007] The thickness of the ITO film layer corresponding to red light is greater than the thickness of the ITO film layer corresponding to green light, and the thickness of the ITO film layer corresponding to green light is greater than the thickness of the ITO film layer corresponding to blue light.
[0008] A method for preparing an anode structure for increasing light polymerization, characterized in that it comprises the following steps:
[0009] Step 1) forming a pixel anode layer (Anode) and a first ITO film layer on a CMOS substrate;
[0010] Step 2) providing a first HM layer on the surface of the first ITO film layer;
[0011] Step 3) performing multiple coating, exposure and etching on the first HM layer to form a first mask pattern with a semicircular lens morphology at a position corresponding to the first filter;
[0012] Step 4) forming a second ITO film layer on the structure after step 3);
[0013] Step 5) providing a second HM layer on the surface of the second ITO film layer;
[0014] Step 6) performing multiple coating, exposure and etching on the second HM layer to form a second mask pattern with a semicircular lens morphology at a position corresponding to the second filter;
[0015] Step 7) forming a third ITO film layer on the structure after step 6);
[0016] Step 8) providing a third HM layer on the surface of the third ITO film layer;
[0017] Step 9) performing multiple coating, exposure and etching on the third HM layer to form a third mask pattern with a semicircular lens morphology at a position corresponding to the third filter;
[0018] Step 10) etching is performed on the structure after step 9) to form the anode structure for increasing light polymerization.
[0019] The first ITO film layer is a blue light ITO film layer, the second ITO film layer is a green light ITO film layer, and the third ITO film layer is a red light ITO film layer.
[0020] In step 3), step 6) and step 9), negative photoresist is used for coating.
[0021] In step 3), the photoresist at the position corresponding to the first filter is retained in the first glue coating, and the rest is removed; the whole surface is etched, and the morphology of the retained part of the photoresist is transferred to the first HM layer; except for the first glue coating, glue is applied on the exposed first ITO film layer in each other glue coating, and the width of the photoresist in the middle is gradually reduced compared with the straight section width of the first HM layer retained in the previous time, and the two sides that have been etched into curved surfaces are retained in the next glue coating.
[0022] In step 6), the photoresist at the position corresponding to the second filter is retained in the first glue coating, and the rest is removed; the whole surface is etched, and the photoresist retained part of the morphology is transferred to the second HM layer; except for the first glue coating, glue is applied on the exposed second ITO film layer in each glue coating, and the width of the photoresist in the middle is gradually reduced compared with the straight section width of the second HM layer retained in the previous time, and the two sides that have been etched into curved surfaces are retained in the next glue coating.
[0023] In step 9), the photoresist at the position corresponding to the third filter is retained during the first glue coating, and the rest is removed; the entire surface is etched, and the photoresist retains the morphology of the part to be transferred to the third HM layer; except for the first glue coating, glue is applied on the exposed third ITO film layer for each glue coating, and the width of the photoresist in the middle is gradually reduced compared with the straight section width of the third HM layer retained in the previous time, and the two sides that have been etched into curved surfaces are retained during the next glue coating.
[0024] Compared with the prior art, the present invention has the following advantages: the present invention adds an anode structure for light polymerization and a preparation method thereof, which has a simple structure, can effectively reduce light loss, achieve higher brightness display, and has strong practicality and good application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] The following is a brief description of the contents and symbols in the drawings of this specification:
[0026] Figure 1 This is a schematic diagram of the structure of forming a pixel anode layer and a first ITO film layer on a CMOS substrate in step 1);
[0027] Figure 2 The schematic diagram of the structure of step 2) providing a first HM layer on the surface of the first ITO film layer;
[0028] Figure 3 , 4 , 5, 6, 7, 8, 9, and 10 are schematic diagrams of a first mask pattern structure in which, in step 3), multiple coating, exposure, and etching are performed on the first HM layer to form a semicircular lens morphology;
[0029] Fig.11 The schematic diagram of the structure of forming a second ITO film layer on the structure after step 3) in step 4);
[0030] Fig.12 The schematic diagram of the structure of step 5) providing a second HM layer on the surface of the second ITO film layer;
[0031] Fig.13 , 14 15, 16, 17, 18, 19, and 20 are schematic diagrams of a second mask pattern structure in which, in step 6), multiple coating, exposure, and etching are performed on the second HM layer to form a semicircular lens morphology;
[0032] Fig.21 The schematic diagram of the structure of forming a third ITO film layer on the structure after step 6) in step 7);
[0033] Fig. 22 In step 8), a third HM layer is provided on the surface of the third ITO film layer;
[0034] Fig.23 , 24 25, 26, 27, 28, 29, and 30 are schematic diagrams of a third mask pattern structure in step 9) performing multiple coating, exposure, and etching on the third HM layer to form a semicircular lens morphology;
[0035] Fig.31 A schematic diagram of the anode structure for adding light polymerization to the present invention;
[0036] Fig.32 Schematic diagram of light reflection in a non-convex mirror structure;
[0037] Fig.33 Schematic diagram of light reflection in a convex mirror structure.
[0038] Reference numerals:
[0039] 1. First mask pattern; 2. Second mask pattern; 3. Third mask pattern. DETAILED DESCRIPTION
[0040] The specific implementation modes of the present invention will be further explained in detail below through the description of embodiments with reference to the accompanying drawings.
[0041] In the description of the present invention, it should be noted that the directions or positional relationships indicated by terms such as “upper”, “lower”, “front”, “back”, “left”, “right”, “vertical”, “inside” and “outside” are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.
[0042] The present invention increases the anode structure of light polymerization such as Fig.31 As shown in , it includes a CMOS substrate, a pixel anode layer is provided on the CMOS substrate, an ITO film layer is provided on the pixel anode layer, and the ITO film layer corresponding to the color filter is a semicircular lens structure.
[0043] In the present invention, the thickness of the ITO film layer corresponding to red light is greater than the thickness of the ITO film layer corresponding to green light, and the thickness of the ITO film layer corresponding to green light is greater than the thickness of the ITO film layer corresponding to blue light.
[0044] The present invention adds an anode structure for light polymerization, which is an anode structure suitable for manufacturing high-resolution display devices. By etching, the indium tin oxide conductive film (ITO) structure is transformed into a convex lens form, so that the light coming down through the light-emitting layer can be polymerized when it is reflected by the AL of the Anode, thereby achieving the purpose of reducing light loss. Fig.32 , 33 As shown in . Due to the current method of using white light plus color filters, the light emitting position is far away from the light output point, and the light output loss is high. This solution can effectively reduce the light output loss.
[0045] The present invention provides a convex lens anode structure, which has the following beneficial technical effects: 1. Increase light aggregation and improve light extraction efficiency; since the refractive index of ITO is between 1.8 and 2.1, the lens form can aggregate the irregular light reflected from the anode AL to the upper part of ITO, and then transmit it upward. Therefore, this solution can improve light extraction efficiency; 2. Reduce light leakage and astigmatism; the special ITO structure can collect and aggregate scattered light, reducing light leakage and astigmatism.
[0046] A method for preparing an anode structure for light polymerization includes the following steps:
[0047] Step 1) forming a pixel anode layer (Anode) and a first ITO film layer on a CMOS substrate;
[0048] Step 2) providing a first HM layer on the surface of the first ITO film layer;
[0049] Step 3) performing multiple coating, exposure and etching on the first HM layer to form a first mask pattern 1 with a semicircular lens morphology at a position corresponding to the first filter;
[0050] Step 4) forming a second ITO film layer on the structure after step 3);
[0051] Step 5) providing a second HM layer on the surface of the second ITO film layer;
[0052] Step 6) performing multiple coating, exposure and etching on the second HM layer to form a second mask pattern 2 with a semicircular lens morphology at a position corresponding to the second filter;
[0053] Step 7) forming a third ITO film layer on the structure after step 6);
[0054] Step 8) providing a third HM layer on the surface of the third ITO film layer;
[0055] Step 9) performing multiple coating, exposure and etching on the third HM layer to form a third mask pattern 3 with a semicircular lens morphology at a position corresponding to the third filter;
[0056] Step 10) etching is performed on the structure after step 9) to form the anode structure for increasing light polymerization.
[0057] Because the transmittance of ITO film layers of different thicknesses under different colors is different, an ITO film layer of corresponding thickness is set according to the corresponding color selection to obtain a higher transmittance. The film layer with the smallest thickness is used as the first ITO film layer, and the second ITO film layer and the third ITO film layer are set in order from small to large film layer thickness. In the present invention, the first ITO film layer is a blue light ITO film layer, the second ITO film layer is a green light ITO film layer, and the third ITO film layer is a red light ITO film layer.
[0058] Specifically, the present invention provides a method for preparing an anode structure, and the specific steps are as follows:
[0059] Before step 1), clean the dirt and foreign matter on the surface for the first time;
[0060] In step 1), PVD is used to form the anode (TI / TIN / AL / TIN) and the blue light ITO film (B-ITO), such as Figure 1 As shown in;
[0061] In step 2), a first HM layer (Hard Mask) hard mask is set on the B-ITO surface, and the mask is used for photolithography pattern, such as Figure 2 as shown in .
[0062] In step 3), multiple coating, exposure and etching are performed on the first HM layer to form a first mask pattern 1 with a semicircular lens morphology at a position corresponding to the B filter;
[0063] A photoresist (PR glue) is coated on the first HM layer. In the present invention, a negative photoresist is used, and the UV-irradiated part of the negative photoresist is retained. If a negative photoresist is used, the area to be retained is exposed and then baked. The photoresist corresponding to the first filter is retained for the first time, and the rest is completely removed. Figure 3 As shown in; the entire surface is etched so that the photoresist retains part of the morphology and is transferred to the first HM layer, retaining the first HM layer at the corresponding position of the first filter, as shown in Figure 4 As shown in ; perform photoresist coating again, continue to expose the part that needs to be retained, remove the PR glue in the area that needs to be etched, and then perform post-baking; the second time of coating, the exposed first ITO film layer is completely coated with glue, and the width of the PR glue set in the middle of the first HM layer corresponding to the position of the first filter is smaller than the width of the straight section of the first HM layer, as shown in Figure 5 shown in; Figure 5 The entire surface is etched on the structure, so that the retained part of the PR morphology is transferred to the first HM layer, and the arc structure is etched on both sides, such as Figure 6As shown in ; Continue PR coating to keep part of the exposure, remove the PR in the area that needs to be etched, and then perform post-baking. Apply glue for the third time, and apply glue all over the exposed first ITO film layer. The width of the PR glue set in the middle of the first HM layer at the corresponding position of the first filter is smaller than the width of the straight section on the first HM layer. The two sides have been etched and coated with glue on the curved surface, as shown Figure 7 shown in; Figure 7 The entire surface is etched on the structure, so that the retained part of the PR morphology is transferred to the first HM layer, and the two sides are further etched to form an arc structure, such as Figure 8 As shown in ; continuing PR coating will require retaining part of the exposure, removing the PR in the area that needs to be etched, and then post-baking, such as Fig. 9 As shown in , the operation is repeated many times until the first HM layer obtains a semicircular lens morphology to form a first mask pattern 1, as shown in Fig.10 As shown in;
[0064] In step 3), except for the first coating, the exposed first ITO film layer is coated with glue in all the coatings, the width of the photoresist in the middle is gradually reduced compared with the width of the straight section of the first HM layer retained in the previous coating, and the two sides of the etched curved surface are retained in the next coating;
[0065] In step 4), PVD is used to form a green ITO film (G-ITO), such as Fig.11 As shown in;
[0066] In step 5), a second HM layer (Hard Mask) hard mask template is set on the G-ITO surface, such as Fig.12 As shown in;
[0067] In step 6), multiple coating, exposure and etching are performed on the second HM layer to form a second mask pattern 2 with a semicircular lens morphology at a position corresponding to the G filter;
[0068] The photoresist (PR glue) is coated on the second HM layer, and the area to be retained is exposed and then baked. The photoresist corresponding to the second filter is retained for the first time, and the rest is removed. Fig.13 As shown in; the entire surface is etched so that the photoresist retains part of the morphology and is transferred to the second HM layer, retaining the second HM layer at the corresponding position of the second filter, as shown in Fig.14 As shown in ; perform photoresist coating again, continue to expose the part that needs to be retained, remove the PR glue in the area that needs to be etched, and then perform post-baking; the second time of coating, all the exposed second ITO film layer is coated with glue, and the width of the PR glue set in the middle of the second HM layer corresponding to the position of the second filter is smaller than the width of the straight section of the second HM layer, as shown in Fig.15 shown in; Fig.15The entire surface is etched on the structure, so that the retained part of the PR morphology is transferred to the second HM layer, and the arc structure is etched on both sides, such as Fig.16 As shown in ; Continue PR coating to keep part of the exposure, remove the PR in the area that needs to be etched, and then perform post-baking. Apply glue for the third time, and apply glue all over the exposed second ITO film layer. The width of the PR glue set in the middle of the second HM layer at the corresponding position of the second filter is smaller than the width of the straight section on the second HM layer. The two sides have been etched and coated with glue on the curved surface, as shown Fig.17 shown in; Fig.17 The entire surface is etched on the structure, so that the retained part of the PR morphology is transferred to the second HM layer, and the two sides are further etched to form an arc structure, such as Fig.18 As shown in ; continuing PR coating will require retaining part of the exposure, removing the PR in the area that needs to be etched, and then post-baking, such as Fig.19 As shown in , the operation is repeated several times until the second HM layer obtains a semicircular lens morphology to form a second mask pattern 2, as shown in Fig. 20 As shown in;
[0069] In step 6), each time the photoresist is applied, the width of the photoresist in the middle is gradually reduced compared with the width of the straight section of the second HM layer retained in the previous time, and the photoresist on both sides that have been etched into curved surfaces are retained in the next application of the photoresist;
[0070] In step 7), PVD is used to form a red ITO film (R-ITO), such as Fig.21 As shown in;
[0071] In step 8), a third HM layer (Hard Mask) hard mask template is set on the R-ITO surface, such as Fig. 22 As shown in;
[0072] In step 9), multiple times of coating, exposure and etching are performed on the third HM layer to form a third mask pattern 3 with a semicircular lens morphology at a position corresponding to the R filter;
[0073] The photoresist (PR glue) is coated on the third HM layer, and the area to be retained is exposed and then baked. The photoresist corresponding to the third filter is retained for the first time, and the rest is removed. Fig.23 As shown in; the entire surface is etched so that the photoresist retains part of the morphology and is transferred to the third HM layer, retaining the third HM layer at the corresponding position of the third filter, as shown in Fig.24 As shown in ; perform photoresist coating again, continue to expose the part that needs to be retained, remove the PR glue in the area that needs to be etched, and then perform post-baking; the second time of coating, all the exposed third ITO film layer is coated with glue, and the width of the PR glue set in the middle of the third HM layer corresponding to the position of the third filter is smaller than the width of the straight section of the third HM layer, as shown in Fig.25 shown in; Fig.25The entire surface is etched on the structure, so that the PR retains part of the morphology and is transferred to the third HM layer, and the two sides are etched to form an arc structure, such as Fig.26 As shown in ; Continue PR coating to keep part of the exposure, remove the PR in the area that needs to be etched, and then perform post-baking. Apply glue for the third time, and apply glue all over the exposed third ITO film layer. The width of the PR glue set in the middle of the third HM layer at the corresponding position of the third filter is smaller than the width of the straight section on the third HM layer. The two sides have been etched and coated with glue on the curved surface, as shown in Fig. 27 shown in; Fig. 27 The entire surface is etched on the structure, so that the retained part of the PR morphology is transferred to the third HM layer, and the two sides are further etched to form an arc structure, such as Fig.28 As shown in ; continuing PR coating will require retaining part of the exposure, removing the PR in the area that needs to be etched, and then post-baking, such as Fig.29 As shown in , the operation is repeated several times until the third HM layer obtains a semicircular lens morphology to form a third mask pattern 3, as shown in Fig.30 As shown in;
[0074] In step 9), each time the photoresist is applied, the width of the photoresist in the middle is gradually reduced compared with the width of the straight section of the third HM layer retained in the previous time, and the photoresist on both sides that have been etched into curved surfaces are retained in the next application of the photoresist;
[0075] Step 10) etching the structure after step 9) to form the anode structure for increasing light polymerization, such as Fig.31 In step 10), etching is performed under the action of the first mask pattern 1, the second mask pattern 2 and the third mask pattern 3 to form a corresponding semicircular lens ITO film layer at the corresponding position of each filter.
[0076] The present invention adds an anode structure for light polymerization and a preparation method thereof. Based on the existing structure, ITO (indium tin oxide conductive film) is transformed into a convex lens form by dry etching, and the material refractive index condition is satisfied, which can reduce light loss to a certain extent. The anode structure is simple in structure, can effectively reduce light loss, achieve high brightness display, and is formed through reasonable manufacturing steps, and has strong practicality and good application prospects.
[0077] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0078] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings, but it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principles of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.
Claims
1. An anode structure for increasing light polymerization, comprising a CMOS substrate, a pixel anode layer provided on the CMOS substrate, and an ITO film layer provided on the pixel anode layer, characterized in that: The ITO film layer corresponding to the color filter is a semicircular lens structure.
2. The anode structure for increasing light polymerization according to claim 1, characterized in that: The thickness of the ITO film layer corresponding to red light is greater than the thickness of the ITO film layer corresponding to green light, and the thickness of the ITO film layer corresponding to green light is greater than the thickness of the ITO film layer corresponding to blue light.
3. A method for preparing an anode structure for increasing light polymerization as claimed in any one of claims 1 to 2, characterized in that: The method comprises the following steps: step 1) forming a pixel anode layer (Anode) and a first ITO film layer on a CMOS substrate; Step 2) providing a first HM layer on the surface of the first ITO film layer; Step 3) performing multiple coating, exposure and etching on the first HM layer to form a first mask pattern with a semicircular lens morphology at a position corresponding to the first filter; Step 4) forming a second ITO film layer on the structure after step 3); Step 5) providing a second HM layer on the surface of the second ITO film layer; Step 6) performing multiple coating, exposure and etching on the second HM layer to form a second mask pattern with a semicircular lens morphology at a position corresponding to the second filter; Step 7) forming a third ITO film layer on the structure after step 6); Step 8) providing a third HM layer on the surface of the third ITO film layer; Step 9) performing multiple coating, exposure and etching on the third HM layer to form a third mask pattern with a semicircular lens morphology at a position corresponding to the third filter; Step 10) etching is performed on the structure after step 9) to form the anode structure for increasing light polymerization.
4. The method for preparing an anode structure for increasing light polymerization according to claim 3, characterized in that: The first ITO film layer is a blue light ITO film layer, the second ITO film layer is a green light ITO film layer, and the third ITO film layer is a red light ITO film layer.
5. The method for preparing an anode structure for increasing light polymerization according to claim 3, characterized in that: In step 3), step 6) and step 9), negative photoresist is used for coating.
6. The method for preparing an anode structure for increasing light polymerization according to claim 5, characterized in that: In step 3), the photoresist at the position corresponding to the first filter is retained during the first coating, and the rest is removed; the entire surface is etched, and the morphology of the retained portion of the photoresist is transferred to the first HM layer.
7. The method for preparing an anode structure for increasing light polymerization according to claim 6, characterized in that: In step 3), except for the first time, glue is applied on the exposed first ITO film layer each time, and the width of the photoresist in the middle is gradually reduced compared with the width of the straight section of the first HM layer retained in the previous time. The two sides that have been etched into curved surfaces are retained in the next glue application.
8. The method for preparing an anode structure for increasing light polymerization according to claim 5, characterized in that: In step 6), the photoresist at the position corresponding to the second filter is retained during the first coating, and the rest is removed; the entire surface is etched, and the morphology of the retained portion of the photoresist is transferred to the second HM layer.
9. The method for preparing an anode structure for increasing light polymerization according to claim 8, characterized in that: In step 6), except for the first time, glue is applied on the exposed second ITO film layer each time, and the width of the photoresist in the middle is gradually reduced compared with the width of the straight section of the second HM layer retained in the previous time. The two sides that have been etched into curved surfaces are retained in the next glue application.
10. The method for preparing an anode structure for increasing light polymerization according to claim 5, characterized in that: In step 9), the photoresist at the position corresponding to the third filter is retained during the first glue coating, and the rest is removed; the entire surface is etched, and the photoresist retains the morphology of the part to be transferred to the third HM layer; except for the first glue coating, glue is applied on the exposed third ITO film layer for each glue coating, and the width of the photoresist in the middle is gradually reduced compared with the straight section width of the third HM layer retained in the previous time, and the two sides that have been etched into curved surfaces are retained during the next glue coating.