Liquefied gas electrolyte with reduced vapor pressure using high concentration salt
The combination of high-concentration salt and liquefied gas solvents is reduced, and the problem of difficult treatment of liquefied gas electrolytes under high pressure is solved, thus achieving thinner-walled battery shell and higher battery performance.
Patent Information
- Application Number
- CN202380035876.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-07-21
- Filing Date
- 2023-04-06
- Publication Date
- 2024-12-03
AI Technical Summary
Existing liquefied gas electrolytes at high vapor pressures cause difficulties in handling and manufacturing of electrochemical devices and require thicker housing walls, increasing mass, volume and cost.
Using a combination of high-concentration salt and liquefied gas solvent, the vapor pressure is significantly reduced by adjusting the ratio of salt to solvent, so that it is lower than atmospheric pressure, allowing the electrolyte to be treated as a liquid, and forming a stable electrode-electrolyte interface to improve cycle life and power capability.
Reduces the structural requirements of the battery case, allows for a thinner wall design, reduces quality and cost, while improving the performance and safety of the battery pack.
Smart Images

Figure CN119072761A_ABST
Abstract
Description
[0001] 1.0 Cross-reference to related applications
[0002] This application is also related to the following filed applications, the entire contents of each of which are incorporated herein by reference: PCT / US20 / 048660, filed on August 30, 2020; PCT / US20 / 020547, filed on February 29, 2020; PCT / US20 / 048661, filed on August 30, 2020; PCT / US19 / 032413, filed on May 15, 2019; PCT / US19 / 032414, filed on May 15, 2019; PCT / US14 / 066015, filed on November 17, 2014; PCT / US20 / 048661, filed on April 1, 2020 / 026086; PCT / US17 / 029821 filed on April 27, 2017; PCT / US22 / 031594 filed on May 31, 2022; PCT / US23 / 11864 filed on January 30, 2023; Provisional Application 63 / 328480 filed on July 7, 2022; Provisional Application 63 / 391224 filed on July 21, 2022; Provisional Application 63 / 418703 filed on October 24, 2022; Provisional Application 63 / 418704 filed on October 24, 2022; and Provisional Application 63 / 306393 filed on February 3, 2022.
[0003] This application claims priority to U.S. Provisional Application No. 63 / 328,480 filed on April 7, 2022, U.S. Provisional Application No. 63 / 391,220 filed on July 21, 2022, and U.S. Application No. 18 / 131,616 filed on April 6, 2023. The contents of these applications are incorporated herein by reference. Technical Field
[0004] Various embodiments of the present invention are directed to compositions and chemical formulations for use as electrolytes in electrochemical energy devices such as batteries and electrochemical capacitors. Devices using the compositions and methods of using the compositions are also provided. Background Art
[0005] Electrochemical devices, such as batteries or capacitors, use ion-conducting, electrically insulating electrolytes to carry charge between negative and positive electrodes. These electrolytes are typically liquid at room temperature and atmospheric pressure (293.15K and 100kPa) or standard conditions, and consist of about 1.0M salt and optional additives in a solvent mixture, which can be solid, liquid or gas under standard conditions. The salt and solvent molecules exist in so-called "solvation shells", in which positive and negative ions are usually surrounded by solvents, additives and other positive and negative ions. These solvation shells affect various aspects of the device, from cyclability to safety, and depend on the concentration and composition of the electrolyte formulation.
[0006] Liquefied gas electrolytes are known to improve the performance of electrochemical devices in terms of higher power, higher energy, temperature performance or safety. However, most liquefied gas solvents, additives and salt mixtures suffer from vapor pressures far above atmospheric pressure (>100 kPa), which makes handling and device construction more difficult.
[0007] Therefore, an electrolyte with reduced vapor pressure is needed to overcome these deficiencies. Summary of the invention
[0008] A novel electrolyte based on liquefied gas and high concentration salt in liquefied gas electrolyte is disclosed. Unlike ordinary electrolytes, liquefied gas electrolytes use solvents that are gaseous under standard conditions. The present disclosure describes an electrolyte composed of a solvent and a salt or a combination of salts, the solvent comprising one or more solvents, one or more of which are liquefied gas solvents, and the concentration of the salt or the combination of salts is high enough so that the combination of solid salt and liquefied gas solvent causes the vapor pressure of the electrolyte to be reduced compared to the base solvent alone. The vapor pressure can be significantly reduced, and even a liquid electrolyte mixture with a vapor pressure lower than atmospheric pressure at a temperature of 293.15K is produced, thereby allowing the electrolyte mixture to be treated as a liquid. A large amount of salt helps to form a stable electrode-electrolyte interface (SEI), which can improve the battery cycle life performance or reduce the impedance of the electrode-electrolyte interface, thereby achieving high power capabilities. Improved SEI formation is believed to be due to more contact ion pairs (CIPs) and aggregates in the solvation shell, where salt cations and anions are still in contact, not separated by the solvent, and may cause the anions to be reduced before the solvent. This generally results in a more compact inorganic SEI, compared to the less compact organic SEI formed by solvent reduction. In addition, reducing the amount of solvent in the device can reduce costs, and the lower vapor pressure simplifies the manufacturability of the electrolyte and the electrochemical devices using the electrolyte by allowing thinner-walled battery housings, thereby reducing mass, volume, and cost.
[0009] However, unlike conventional liquefied gas electrolytes, these electrolytes can achieve lower vapor pressures when mixed with large amounts of salts, e.g. Figure 1 This allows the use of liquefied gases in the electrolyte without the mechanical or manufacturing limitations imposed by high vapor pressure solvents, which can simplify manufacturing, reduce the mass of the battery cell housing, and reduce costs.
[0010] Other aspects, alternatives and variations that are obvious to those skilled in the art are also disclosed herein and are specifically contemplated as part of the present invention. The present invention is set forth only in the claims allowed by the patent office in this or related applications, and the following brief description of certain examples does not in any way limit, define or establish the scope of legal protection. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The present invention may be better understood with reference to the following drawings. The components in the drawings are not necessarily to scale, with emphasis placed on clearly illustrating exemplary aspects of the present invention. In the drawings, the same reference numerals represent corresponding parts throughout the different views and / or embodiments. In addition, various features of the different disclosed embodiments may be combined to form additional embodiments, which are a part of the present disclosure. It should be understood that certain components and details may not appear in the drawings to help more clearly describe the present invention.
[0012] Figure 1 The electrolyte pressure at room temperature of each liquefied gas electrolyte containing lithium salts (lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) and lithium bis(fluorosulfonyl)imide (LiFeI)) with increasing molar concentrations is shown compared to the pure solvent dimethyl ether (Me2O) showing a salt concentration of 0 M.
[0013] Figure 2 The performance of a battery coin cell at room temperature using a lithium metal counter electrode and reference electrode while electrochemically plating and stripping lithium metal onto a stainless steel cathode in 15.0 M LiFSI in Me2O is shown. The coin cell is constructed in a housing enclosing an ionically conductive electrolyte under pressurized conditions to maintain the electrolyte in a liquid phase.
[0014] Figure 3 The performance of a battery coin cell using a lithium metal anode at room temperature is shown while linearly sweeping the potential of a carbon cathode in a 15.0 M LiFSI electrolyte in Me2O. The coin cell is constructed in a housing enclosing an ion-conducting electrolyte under pressurized conditions to maintain the electrolyte in a liquid phase, with the anode and cathode in contact with the ion-conducting electrolyte.
[0015] Figure 4The performance of a battery coin cell at room temperature using a lithium metal anode and a lithium nickel cobalt manganese oxide (NMC 622) cathode and a 15.0 M LiFSI electrolyte in Me2 O is shown. The coin cell is constructed in a housing that encloses an ion-conducting electrolyte under pressurized conditions to maintain the electrolyte in a liquid phase.
[0016] Figure 5 Dimethyl ether (C2H6O) was compared to the two closest linear ethers that are liquid at room temperature, diethyl ether (C4H10O) and 1,2-dimethoxyethane (C4H10O2). The electronic properties of dimethyl ether (ionization potential of about 9.9 eV and electron affinity of about -1.55 eV) were calculated to be superior to these solvents and tetrahydrofuran (a cyclic ether).
[0017] Figure 6 The binding energies of four different liquefied gas solvent types were compared: fluoromethane (CH3F), formaldehyde (H2CO), dimethyl ether ((CH3)2O), and trimethylamine ((CH3)3N). The calculated results of a single solvent molecule binding to a single lithium cation were compared. The results showed that the binding energies of formaldehyde (1.6eV), dimethyl ether (1.72eV), and trimethylamine (1.82eV) were significantly higher than those of fluoromethane (1.31eV).
[0018] Figure 7 is a diagram showing the solvation shell of solvent molecules around a single cation (anions are not included for clarity). Various salt to solvent ratios are shown as 3:1, 2:1, 1:1, 1:2, 1:3, 1:4, 1:5, 1:6. Because the solvation sphere is essentially complete at a ratio of 1:4, any additional solvent has less binding energy for the cation at a ratio of 1:5 or 1:6, which results in a higher vapor pressure.
[0019] Figure 8 is a block diagram showing an embodiment of an apparatus for dispensing a liquefied gas electrolyte mixture to a secondary container. DETAILED DESCRIPTION
[0020] Reference is made herein to some specific embodiments of the present invention, including any best mode contemplated by the inventor for carrying out the present invention. Examples of these specific embodiments are shown in the accompanying drawings. Although the present invention has been described in conjunction with these specific embodiments, it should be understood that they are not intended to limit the present invention to the embodiments described or shown. On the contrary, they are intended to cover alternatives, modifications and equivalents that may be included in the spirit and scope of the present invention as defined by the appended claims.
[0021] In the following description, many specific details are set forth in order to provide a thorough understanding of the present invention. Specific exemplary embodiments of the present invention can be implemented without some or all of these specific details. In other cases, process operations well known to those skilled in the art are not described in detail so as not to unnecessarily obscure the present invention. For the sake of clarity, various techniques and mechanisms of the present invention are sometimes described in singular form. However, it should be noted that, unless otherwise stated, some embodiments include multiple iterations of techniques or multiple mechanisms. Similarly, in certain embodiments, the various steps of the methods shown and described herein are not necessarily performed in the order indicated, or not performed at all. Therefore, some implementations of the methods discussed herein may include more or fewer steps than the steps shown or described. In addition, the techniques and mechanisms of the present invention sometimes describe connections, relationships, or communications between two or more entities. It should be noted that a connection or relationship between entities does not necessarily mean a direct, unimpeded connection, because various other entities or processes may exist or occur between any two entities. Therefore, unless otherwise stated, the indicated connection does not necessarily mean a direct, unimpeded connection.
[0022] Liquefied gas electrolytes are known to improve the performance of electrochemical devices in terms of higher power, higher energy, temperature performance or safety. However, most liquefied gas solvents, additives and salt mixtures suffer from vapor pressures well above atmospheric pressure (>100 kPa), which makes handling and device construction more difficult and requires thicker enclosure walls, which can increase mass, volume and cost.
[0023] A novel electrolyte based on liquefied gas and high concentration of salt in liquefied gas electrolyte is disclosed. Unlike ordinary electrolytes, liquefied gas electrolytes use solvents that are gaseous under standard conditions. The present disclosure describes an electrolyte consisting of a solvent and a salt or a combination of salts, the solvent consisting of one or more solvents, one or more of which are liquefied gas solvents, and the concentration of the salt or salt combination is high enough so that the combination of solid salt and liquefied gas solvent causes the vapor pressure of the electrolyte to be reduced compared to the base solvent alone. The vapor pressure can be significantly reduced, and even a liquid electrolyte mixture with a vapor pressure lower than atmospheric pressure at a temperature of 293.15K is produced, so that the solid-gas mixture can be treated as a liquid. A large amount of salt helps to form a stable electrode-electrolyte interface (SEI), reduces the amount of solvent in the device, and simplifies the manufacturability of the electrolyte and the electrochemical device in which the electrolyte is used. The formation of improved SEI is believed to be due to more contact ion pairs (CIPs) and aggregates in the solvation shell, where salt cations and anions are still in contact, not separated by the solvent, and may cause the anions to be reduced before the solvent. This generally results in a denser inorganic SEI compared to the less dense organic SEI formed by solvent reduction.
[0024] Through a large number of experiments, it was found that, unlike traditional liquefied gas electrolytes, certain liquefied gas electrolyte preparations containing a large amount of salt can obtain a vapor pressure below atmospheric pressure at room temperature, while using liquefied gas solvents whose vapor pressure is higher than atmospheric pressure at room temperature, such as Figure 1 This is believed to be due to the tight binding of the solvent to the lithium ions and salt anions, as shown in Figure 7 As shown. An example of a liquefied gas solvent that exhibits this phenomenon is dimethyl ether. At sufficiently high salt concentrations above about 7M, the resulting lower vapor pressure allows the liquefied gas electrolyte to be handled as a liquid at room temperature and pressure. It was not previously obvious to those skilled in the art that increasing the molar concentration of lithium salts in a liquefied gas solvent such as dimethyl ether would maintain these highly desirable qualities without conducting experiments, formation, and studies of these electrolyte compositions within a battery device. As a comparison, a salt to solvent molar ratio of 1 mole of LiTFSI to 2 moles of dimethyl ether salt produces a concentration of 3.65M, which shows a vapor pressure reduction from 86psi for pure dimethyl ether solvent to about 40psi, i.e., a 53% reduction in vapor pressure. The significant reduction in vapor pressure will reduce the structural requirements for the battery housing, thereby allowing thinner battery housing walls, reduced mass, and reduced volume.
[0025] Figure 7 is a diagram showing the solvation shell of solvent molecules around a single cation (anions are not included for clarity). Various salt to solvent ratios are shown as 3:1, 2:1, 1:1, 1:2, 1:3, 1:4, 1:5, 1:6. If the solvent molecule is within the first solvation sphere of the salt (where the solvent molecule is tightly bound to the cation), then the solvent molecule will generally be tightly bound to the salt cation. The solvent in the second solvation sphere may also show some binding to the salt cation, but at a reduced energy compared to the first solvation sphere. This tight binding reduces the free energy of the molecule, thereby reducing its kinetic energy and, in turn, its effective vapor pressure. Therefore, with too much solvent, the vapor pressure is more determined by free solvent molecules that have little attraction to the cation, which produces an electrolyte with a higher vapor pressure.
[0026] Electrolyte salt concentration can be described as molar concentration (moles of salt per unit volume of mixed electrolyte) or the ratio of salt to solvent. For example, an electrolyte with 1 part LiTFSI and 2 parts dimethyl ether corresponds to a molar concentration of about 3.65 mol / liter (M). This concentration produces an electrolyte with a reduced vapor pressure of about 40 psi, which is about 53% lower than the pure solvent vapor pressure of 86 psi at room temperature. It has also been shown that when the molar concentration of the salt is 10 M, the vapor pressure is significantly reduced, making the electrolyte vapor pressure below atmospheric pressure, effectively providing a liquid electrolyte.
[0027] It can be seen that for gaseous solvents that have a strong attraction for salt cations, high concentrations of salt will produce lower vapor pressures. Figure 6 The binding energies of four different liquefied gas solvent types were compared: fluoromethane (CH3F), formaldehyde (H2CO), dimethyl ether ((CH3)2O), and trimethylamine ((CH3)3N). The calculated results for the binding of a single solvent molecule to a single lithium cation were compared. The results show that the binding energies of formaldehyde (1.6eV), dimethyl ether (1.72eV), and trimethylamine (1.82eV) are significantly higher than that of fluoromethane (1.31eV). It was observed that fluoromethane only weakly coordinates to lithium salts, and it is difficult to increase the salt concentration in the pure solvent without precipitating the salt from the solution. In contrast, formaldehyde, dimethyl ether, and trimethylamine show excellent solubility for high concentrations of salt. It is known that carbonyl oxygens, ether oxygens, and amine nitrogens show a high degree of binding to salt cations, but it is surprising that this binding is so strong as to allow high salt concentrations in the liquefied gas solvents and a significant reduction in the gas vapor pressure of the mixed electrolyte. This behavior is due to the increased binding energy of these solvents to lithium cations. Furthermore, this effect can be extended to any liquefied gas with carbonyl oxygen, ether oxygen, and amine nitrogen.
[0028] It is usually seen that the reduction in vapor pressure is large enough to make the vapor pressure below atmospheric pressure at room temperature, making the electrolyte liquid under standard conditions. Therefore, any liquefied gas electrolyte can be handled as a liquid under standard conditions if a high enough concentration of salt is dissolved in the electrolyte mixture to make the vapor pressure of the liquefied gas solvent below atmospheric pressure.
[0029] The benefits of reducing the vapor pressure of liquefied gas electrolytes include allowing liquefied gas electrolytes to directly replace traditional liquid electrolytes in common equipment and liquid handling processes, including production lines and existing battery and electrochemical device structures such as pouch cells and prismatic cells, products, and housings. Liquefied gas electrolytes are preferred over traditional liquid electrolytes because gas molecules are generally chemically simpler than common liquid electrolytes. An example is dimethyl ether (C2H6O), compared to the two closest other linear ethers that are liquids at room temperature: diethyl ether (C4H10O) and 1,2-dimethoxyethane (C4H10O2). As Figure 5As shown, the electronic properties of dimethyl ether (ionization potential of about 9.9 eV and electron affinity of about -1.55 eV) are calculated to be superior to these solvents and tetrahydrofuran (a cyclic ether). This translates into improved oxidation and reduction potentials. These larger liquid molecules generally have lower electrochemical stability and can decompose at high oxidation or reduction potentials within the battery cell. Typically, the carbon-carbon bond in these larger liquid molecules is a weak point in the molecule, which is conducive to this undesirable chemical instability. Smaller molecules with smaller sizes are beneficial to the research and production of electrolytes in terms of reducing the chemical complexity of understanding phenomena, the computational requirements and costs of simulations. In addition, smaller molecular sizes benefit from lower viscosity in the electrolyte, resulting in higher salt mobility and, in turn, higher overall electrolyte conductivity. This higher electrolyte conductivity provides a higher power battery. In addition, liquid solvents freeze at low temperatures, rendering the battery cell inoperable. In contrast, the freezing point of smaller molecule liquefied gas solvents is much lower than that of liquid solvents, which allows the electrolyte to operate at significantly lower temperatures. For example, fluoromethane has a freezing point of -138° C., dimethyl ether has a freezing point of -141° C., and ammonia has a freezing point of -77° C. This is in contrast to conventional liquid solvents such as ethylene carbonate (-48° C.) and dimethyl carbonate (+2° C.) which have higher freezing points.
[0030] like Figure 2 As shown, the disclosed formulations were found to facilitate low overpotentials for lithium plating and stripping. In addition, although ethers are generally unstable at higher potentials common in battery devices, Figure 3 The disclosed formulations were shown to be stable at 5.0 V with no deleterious side reactions. Figure 4 This is also shown in , where the disclosed formulation was used in a battery coin cell with NMC 622 cathode, showing higher first cycle efficiency.
[0031] like Figure 1As shown, the vapor pressure of pure Me2O solvent at zero salt molar concentration is about 80 psia at room temperature, which exceeds normal atmospheric pressure (15 psia or 100 kPa). As more salt is added, at 5M salt concentration, the vapor pressure drops to about 60%, although the vapor pressure of 5M electrolyte (35 psia) is still above atmospheric pressure. However, the vapor pressure of 10M or higher electrolytes is about 5 psia or 94% lower than that of no salt, which is much lower than atmospheric pressure. Different salt addition amounts can be used to reduce the pressure of the electrolyte, such as a salt to solvent ratio of 3:1, 2:1, 1:1, 1:2, 1:3, 1:4, 1:5 or 1:6, and an electrolyte with a reduced vapor pressure of about 1%, 5%, 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, up to 99% can be obtained. The reduction in pressure depends of course on the solvent, salt, the ratio of salt to solvent, and the temperature of the mixture. Where two or more solvents are used, the solvents described in the salt to solvent ratio may be only those solvents that exhibit high binding energies for lithium cations. In general, any liquefied gas solvent that exhibits a reduction in vapor pressure at sufficiently high salt concentrations in the pure solvent may be mixed together to combine multiple solvents and an overall lower vapor pressure electrolyte. These solvents may also be mixed with solvents that bind more weakly to the salt cation. The cation may be any salt cation, but preferably lithium, sodium, calcium, magnesium or potassium.
[0032] This reduction in vapor pressure can be so great that it effectively makes the electrolyte a liquid at atmospheric pressure. Any reduction in electrolyte vapor pressure will benefit from ease of handling, use of common liquid dispensing techniques and equipment, cell housings and structures (including pouch cells and prismatic cells), and improved safety due to lower electrolyte pressure.
[0033] In some cases, it may be desirable to maintain the vapor pressure of the liquefied gas electrolyte at a level above atmospheric pressure but below the vapor pressure of the liquefied gas solvent. For example, to improve the safety of a battery cell in the event of a crush or puncture, it is desirable that the electrolyte can evaporate quickly from the cell to prevent any short circuits and subsequent thermal runaway reactions in the battery. Electrolytes that can evaporate quickly from a punctured or crushed cell are of high safety importance. The electrolyte can evaporate completely along with the salt, or it can evaporate partially, evaporating only the solvent. The increase in cell impedance after electrolyte evaporation can prevent further cell short circuits and thermal runaway reactions. Therefore, for safety reasons, it may be desirable to optimize the vapor pressure to be above atmospheric pressure, but below the vapor pressure of the pure liquefied gas solvent to improve handling. By having a lower vapor pressure, the electrolyte within the electrochemical device does not have to be subjected to such severe pressures. This allows the housing and various device components to be less robust and therefore easier and more efficiently manufactured. For example, the housing wall thickness can be smaller, but still maintain the same structural integrity with a lower pressure electrolyte. This reduces housing mass, volume, and cost, which is beneficial from a performance and cost perspective.
[0034] like Figure 2 As shown, the 15M LiFSI electrolyte is able to effectively promote the plating and stripping of lithium metal at room temperature with low overpotential and no evidence of additional reactions of salts or solvents. The smooth voltage trace indicates that the electrolyte does not produce uneven growth or harmful electrolyte side reactions.
[0035] like Figure 3 As shown, the 15M LiFSI electrolyte also has an impressively high potential stability at room temperature, as can be seen from the linear swear voltagram (LSV) from the open circuit potential to 5 V vs Li / Li+. The electrolyte is stable up to 4.5 V vs Li / Li+. It is known that typical ether-based electrolytes have relatively low potential oxidation, 3-4 V vs Li / Li+.
[0036] Figure 4 The 15M LiFSI electrolyte was shown to be compatible with transition metal oxide cathodes in lithium-ion batteries. The electrolyte was able to reversibly charge and discharge the lithium nickel manganese cobalt oxide cathode from an open circuit potential of 4.2 V to 2.5 V.
[0037] like Figure 5As shown, based on DFT calculations, the ionization potential of dimethyl ether solvent molecules (about 9.9 eV) is higher than other ether solvents, such as diethyl ether (about 9.4 eV), dimethoxyethane (about 9.2 eV), and tetrahydrofuran (about 9.2 eV). Ionization potential is the energy required for a molecule to lose electrons or be oxidized, which is related to the solvent's resistance to oxidation. Similarly, dimethyl ether also has a lower electron affinity (about -1.55 eV) compared to diethyl ether (about -1.45 eV), dimethoxyethane (about 1.35 eV), and tetrahydrofuran (about -1.4 eV). Electron affinity is the energy required for a molecule to gain electrons or be reduced, which is related to the solvent's resistance to reduction.
[0038] like Figure 6 As shown, based on DFT calculations, the binding energies of four different liquefied gas solvent types are compared: fluoromethane (CH3F), formaldehyde (H2CO), dimethyl ether ((CH3)2O), and trimethylamine ((CH3)3N). The calculation results of a single solvent molecule binding to a single lithium cation are compared. The results show that the binding energies of formaldehyde (1.6eV), dimethyl ether (1.72eV), and trimethylamine (1.82eV) are significantly higher than those of fluoromethane (1.31eV).
[0039] One embodiment is an electrochemical device comprising an ion-conducting electrolyte. The ion-conducting electrolyte may include one or more salts, and optionally one or more additives. The one or more additives may be liquid, solid or gas at standard room temperature and standard pressure (about 100 kPa) of 293.15 K. The one or more salts may be liquid, solid or gas at standard room temperature and standard pressure (about 100 kPa) of 293.15 K.
[0040] Some such embodiments of the electrochemical device may further include a housing surrounding the ionically conductive electrolyte and a pair of electrodes in contact with the ionically conductive electrolyte and configured to provide sealing conditions for a solution of the one or more salts and the one or more solvents (eg, liquefied gas solvents).
[0041] Those skilled in the art will understand that the terms "one or more salts", "one or more solvents" (including "liquefied gas solvents" and "liquid solvents") and "one or more additives" used herein in conjunction with "ion-conducting electrolyte" refer to one or more electrolyte components.
[0042] In one embodiment, the liquefied gas electrolyte includes a liquefied gas solvent comprising dimethyl ether and one or more lithium-based salts, wherein the ratio of salt to solvent is 3: 1, 2: 1, 1: 1, 1: 2, 1: 3, 1: 4, 1: 5 or 1: 6. In another embodiment, the liquefied gas solvent includes other gas solvents having an ether oxygen structure, such as methyl ethyl ether, methyl vinyl ether, ethylene oxide, desflurane, 1, 1, 2, 2-tetrafluoro-1- (trifluoromethoxy) ethane, bis (difluoromethyl) ether, methyl pentafluoroethyl ether or perfluoroethyl methyl ether. In another embodiment, the liquefied gas solvent includes any other gas solvent having a carbonyl oxygen, such as formaldehyde, ethylene ketone, carbonyl sulfide, carbon monoxide, tris (difluoroamine) fluoromethane, or ethylamine or trifluoroacetyl fluoride. In another embodiment, the liquefied gas solvent includes any other gas solvent having an amine structure, such as ammonia, methylamine, dimethylamine or trimethylamine.
[0043] These vapor pressure-reduced solvents with high salt concentrations can also be mixed with other liquefied gas solvents to enhance the performance of electrochemical devices, such as fluoromethane, difluoromethane, trifluoromethane, fluoroethane, tetrafluoroethane, pentafluoroethane, 1,1-difluoroethane, 1,2-difluoroethane, 1,1,1-trifluoroethane, 1,1,2-trifluoroethane, 1,1,1,2-tetrafluoroethane, 1,1,2,2-tetrafluoroethane, pentafluoroethane, chloromethane, chloroethane, thionyl fluoride, thionyl chloride, phosphoryl fluoride, phosphoryl chloride, sulfuryl fluoride, sulfuryl chloride, 1-fluoropropane, 2- Fluoropropane, 1,1-difluoropropane, 1,2-difluoropropane, 2,2-fluoropropane, 1,1,1-trifluoropropane, 1,1,2-trifluoropropane, 1,2,2-trifluoropropane, vinyl fluoride, cis-1,2-fluoroethylene, 1,1-fluoroethylene, 1-fluoropropylene, 2-propylene, chlorine, methyl chloride, bromine, iodine, ammonia, methylamine, dimethylamine, trimethylamine, molecular oxygen, molecular nitrogen, carbon monoxide, carbon dioxide, sulfur dioxide, methyl vinyl ether, difluoroethylene, nitrous oxide, nitrogen dioxide, nitrogen monoxide, carbon disulfide, hydrogen fluoride, hydrogen chloride or any combination thereof. In some embodiments, the liquefied gas electrolyte includes a single liquefied gas solvent or a liquefied gas solvent in combination with one or more additives and / or one or more salts. These additives can be gas, liquid or solid at standard room temperature and standard pressure (about 100 kPa) of 293.15K. In addition, any gas additive can also be used as the main solvent.
[0044] In an exemplary electrochemical device using a liquefied gas electrolyte composed of any combination of one or more liquefied gas components and one or more liquid components, one or more solid components, or one or more salt components, the electrode is composed of any combination of two electrodes, intercalation type such as graphite, carbon, activated carbon, vanadium oxide, lithium titanate, titanium disulfide, molybdenum disulfide, lithium iron phosphate, lithium cobalt phosphate, lithium nickel phosphate, lithium cobalt oxide, lithium nickel manganese oxide, lithium nickel manganese cobalt oxide, lithium nickel cobalt aluminum oxide, carbon, or chemical reaction electrode such as with chemical sulfur, oxygen, carbon dioxide, nitrogen, nitrous oxide, sulfur dioxide, thionyl fluoride, thionyl chloride fluoride, sulfuryl fluoride, sulfuryl chloride fluoride or metal electrode with lithium, sodium, magnesium, tin, aluminum, calcium, titanium, zinc or any combination thereof. These components can be combined with various binder polymer components (including polyvinylidene fluoride, carboxymethyl cellulose, styrene butadiene rubber or polytetrafluoroethylene) to maintain the structural integrity of the electrode.
[0045] In some embodiments, additives are used in combination with liquefied gas solvents and lithium, sodium, zinc, calcium, magnesium, aluminum, or titanium based salts. In addition, the one or more liquefied gas solvent solutions or electrolytes can be combined with one or more salts, including lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), lithium hexafluorophosphate (LiPF6), lithium perchlorate (LiClO4), lithium hexafluoroarsenate (LiAsF6), lithium tetrachloroaluminate (LiAlCl4), lithium tetragaliumaluminate, lithium bis(oxalato)borate (LiBOB), lithium hexafluorostannate, lithium difluoro(oxalato)borate (LiDFOB), lithium bis(fluorosulfonyl)imide (LiFSI), lithium aluminum fluoride (LiAlF3), lithium nitrate (LiNO3), lithium chloroaluminate, lithium tetrafluoroborate (LiBF4), lithium tetrachloroaluminate, lithium difluorophosphate, lithium tetrafluoro(oxalato) phosphate, lithium difluorobis(oxalato) phosphate, lithium borate, lithium oxalate (lithium The invention can be selected from the group consisting of lithium oxolate, lithium thiocyanate, lithium tetrachlorogallate, lithium chloride, lithium bromide, lithium iodide, lithium carbonate, lithium fluoride, lithium oxide, lithium hydroxide, lithium nitride, lithium super oxide, lithium azide, lithium deltate, di-lithium squarate, lithium croconate dihydrate, dilithium rhodizonate, lithium oxalate, di-lithium ketomalonate, lithium di-ketosuccinate, or any corresponding salts thereof, wherein the positively charged lithium cation replaces the sodium or magnesium, or any combination thereof.Other useful salts include those in which a positively charged cation is paired with a negatively charged anion, such as tetramethylammonium, tetraethylammonium, tetrapropylammonium, tetrabutylammonium, triethylmethylammonium, spiro-(1,1′)-bipyrrolidinium, 1,1-dimethylpyrrolidinium and 1,1-diethylpyrrolidinium, N,N-diethyl-N-methyl-N(2-methoxyethyl)ammonium, N,N-diethyl-N-methyl-N-propylammonium, N,N-dimethyl-N-ethyl- N-(3-methoxypropyl)ammonium, N,N-dimethyl-N-ethyl-N-benzylammonium, N,N-dimethyl-N-ethyl-N-phenylethylammonium, N-ethyl-N,N-dimethyl-N-(2-methoxyethyl)ammonium, N-tributyl-N-methylammonium, N-trimethyl-N-hexylammonium, N-trimethyl-N-butylammonium, N-trimethyl-N-propylammonium, 1,3-dimethylimidazolium, 1-(4-sulfobutyl)-3-methylimidazolium, 1-allyl- 3H-imidazolium, 1-butyl-3-methylimidazolium, 1-ethyl-3-methylimidazolium, 1-hexyl-3-methylimidazolium, 1-octyl-3-methylimidazolium, 3-methyl-1-propylimidazolium, H-3-methylimidazolium, trihexyl (tetradecyl) phosphonium, N-butyl-N-methylpiperidinium, N-propyl-N-methylpiperidinium, 1-butyl-1-methylpyrrolidinium, 1-methyl-1-(2-methoxyethyl)pyrrolidinium, 1-methyl-1 -(3-methoxypropyl)pyrrolidinium, 1-methyl-1-octylpyrrolidinium, 1-methyl-1-pentylpyrrolidinium or N-methylpyrrolidinium, negatively charged anions such as acetate, bis(fluorosulfonyl)imide, bis(oxalato)borate, bis(trifluoromethanesulfonyl)imide, bromide, chloride, dicyandiamide, diethylphosphate, hexafluorophosphate, hydrogen sulfate, iodide, methanesulfonate, methylphosphate, tetrachloroaluminate, tetrafluoroborate and trifluoromethanesulfonate.
[0046] As described above, the reduction in electrolyte vapor pressure simplifies the manufacturability of electrochemical devices by allowing battery housings with thinner walls, thereby reducing mass, volume, and cost. For example, in co-pending U.S. patent application 63 / 391,220, filed on July 21, 22, an apparatus for premixing an electrolyte mixture for subsequent dispensing into an electrochemical device is described. Figure 8 Taken from the application. A liquefied gas solvent having a vapor pressure greater than 100 kPa at a temperature of 293.15 K is mixed with a suitable salt such that the ratio of salt to solvent is sufficient to reduce the vapor pressure of the electrolyte mixture to at least 90% of the vapor pressure of the pure liquefied gas solvent at a temperature of 293.15 K. The mixture may be made in a container 4, wherein the container is configured to contain the pressure of the liquefied gas solvent. Figure 8The device shown also includes a container isolation valve 12, a liquefied gas electrolyte mixture 6 (including salt 5) and a temperature sensor 7 for dispensing the liquefied gas electrolyte mixture 6 into a secondary container 24. The secondary container 24 can be any suitable metal, ceramic or plastic device capable of containing a liquefied gas electrolyte mixture having a vapor pressure greater than 100 kPa atmospheric pressure at a temperature of 293.15K. If the ratio of salt to solvent of the liquefied gas electrolyte mixture contained in the container is sufficient to reduce the vapor pressure at a temperature of 293.15K to less than 100 kPa, then the container 4 does not need to be strong enough to withstand high pressure. The secondary container 24 can be an electrochemical device such as a battery or a capacitor. Other filling devices are disclosed in co-pending U.S. patent application 63 / 391,220, the entire contents of which are incorporated herein by reference.
[0047] use Figure 8 In the arrangement in, the secondary container 24 can be a housing having an anode and a cathode. The premixed mixture is then dispensed into the housing so that the anode and cathode are in contact with the mixture. The housing can then be sealed and electrical contacts are connected to the anode and cathode and can be touched from outside the housing. If the electrolyte mixture is above 100 kPa at a temperature of 293.15 K, the dispensing step should be performed at a pressure above 100 kPa and the housing structure should be selected so that the electrolyte mixture is maintained above 100 kPa at a temperature of 293.15 K after the housing is sealed. However, the housing does not need to be as strong as the higher pressures of a pure liquefied gas solvent or a liquefied gas electrolyte having a salt-to-salt ratio that hardly reduces the vapor pressure, thereby simplifying the manufacturability of the electrochemical device by allowing a battery housing with thinner walls, thereby reducing mass, volume and cost.
[0048] Alternatively, if the electrolyte mixture is below 100 kPa at 293.15 K, the dispensing step should be performed at atmospheric pressure or lower. In the latter case, the housing does not need to be as strong because the electrolyte mixture is not under pressure, even further simplifying manufacturability and reducing costs.
[0049] Similarly, although operations are depicted in a particular order in the accompanying drawings, this should not be understood as requiring that the operations be performed in the particular order shown or in a sequential order, or that all of the operations shown be performed to achieve a desired result. In addition, the separation of various system components in the embodiments described in this patent document should not be understood as requiring such separation in all embodiments. Only a few implementations and examples are described, and other implementations, improvements, and variations may be made based on what is described and shown in this patent document without departing from the scope and spirit of the invention.
[0050] Although this patent document contains many details, these details should not be construed as limitations on any invention or on the scope of what may be claimed, but rather as descriptions of features that may be specific to a particular embodiment of a particular invention. Certain features described in this patent document in the context of separate embodiments may also be implemented in combination in a single embodiment. Conversely, various features described in the context of a single embodiment may also be implemented separately in multiple embodiments or in any suitable subcombination. In addition, although the above-mentioned features may be described as working in certain combinations or even initially claimed, in some cases one or more features in the claimed combination may be deleted from that combination, and the claimed combination may be directed to a subcombination or a variation of a subcombination.
Claims
1. An ion-conductive electrolyte mixture comprising: Liquefied gaseous solvents having a vapour pressure above 100 kPa at a temperature of 293.15 K; and Salt; The ratio of salt to solvent is sufficient to reduce the vapor pressure of the electrolyte mixture to at least 90% of the vapor pressure of the pure liquefied gas solvent at a temperature of 293.15 K.
2. The mixture of claim 1, wherein the ratio of salt to solvent is about 3:1 to 1:
6.
3. The mixture of claim 1, wherein the ratio of salt to solvent is sufficient to reduce the vapor pressure of the electrolyte mixture to less than 100 kPa at a temperature of 293.15 K.
4. The mixture according to claim 1, wherein the salt consists of LiTFSI, LiFSI, LiPF6, LiBOB, LiBF4, LiDFOB, LiNO3 or any combination thereof.
5. The mixture according to claim 1, wherein the liquefied gas solvent comprises a solvent having a carbonyl oxygen group.
6. A mixture according to claim 5, wherein the carbonyl oxygen group is in the form of formaldehyde, ketene, carbonyl sulfide, carbon monoxide or trifluoroacetyl fluoride.
7. The mixture of claim 1, wherein the liquefied gas solvent comprises a solvent having ether oxygen groups.
8. The mixture according to claim 7, wherein the ether oxygen groups are in the form of dimethyl ether, ethyl methyl ether, methyl vinyl ether, desflurane, 1,1,2,2-tetrafluoro-1-(trifluoromethoxy)ethane, bis(difluoromethyl)ether, methyl pentafluoroethyl ether, perfluoroethyl methyl ether or ethylene oxide.
9. The mixture of claim 1, wherein the liquefied gas solvent comprises a solvent having an amine nitrogen group.
10. A mixture according to claim 9, wherein the amine nitrogen groups are in the form of ammonia, methylamine, dimethylamine, trimethylamine, tris(difluoroammonium)fluoromethane or ethylamine.
11. The mixture according to claim 1, wherein the liquefied gas solvent further comprises: Fluoromethane, difluoromethane, trifluoromethane, fluoroethane, tetrafluoroethane, pentafluoroethane, 1,1-difluoroethane, 1,2-difluoroethane, 1,1,1-trifluoroethane, 1,1,2-trifluoroethane, 1,1,1,2-tetrafluoroethane, 1,1,2,2-tetrafluoroethane, pentafluoroethane, chloromethane, chloroethane, thionyl fluoride, thionyl chloride fluoride, phosphoryl fluoride, phosphoryl chloride fluoride, sulfuryl fluoride, sulfuryl chloride fluoride, 1-fluoropropane, 2-fluoropropane, 1,1-difluoropropane , 1,2-difluoropropane, 2,2-fluoropropane, 1,1,1-trifluoropropane, 1,1,2-trifluoropropane and 1,2,2-trifluoropropane, vinyl fluoride, cis-1,2-fluoroethylene, 1,1-fluoroethylene, 1-fluoropropylene, 2-propylene, chlorine, methyl chloride, bromine, iodine, molecular oxygen, molecular nitrogen, carbon monoxide, carbon dioxide, sulfur dioxide, difluoroethylene, nitrous oxide, nitrogen dioxide, nitric oxide, carbon disulfide, hydrogen fluoride, hydrogen chloride or any combination thereof.
12. An electrochemical device comprising: The mixture of claim 1; an anode in contact with the mixture; a cathode in contact with the mixture; and The casing surrounding the mixture, anode and cathode.
13. The electrochemical device of claim 12, wherein the cathode is selected from the group consisting of graphite, carbon, activated carbon, vanadium oxide and lithium titanate, titanium disulfide, molybdenum disulfide, lithium iron phosphate, lithium cobalt phosphate, lithium nickel phosphate, lithium cobalt oxide, lithium nickel manganese oxide, lithium nickel manganese cobalt oxide and lithium nickel cobalt aluminum oxide.
14. The electrochemical device of claim 12, wherein the anode comprises one or more of lithium metal, sodium metal, calcium metal, magnesium metal, aluminum metal, and zinc metal.
15. The electrochemical device of claim 12, wherein the ratio of salt to solvent of the mixture is about 3:1 to 1:
6.
16. The electrochemical device of claim 12, wherein the salt to solvent ratio of the mixture is sufficient to reduce the vapor pressure of the electrolyte mixture to less than 100 kPa at a temperature of 293.15 K.
17. The electrochemical device according to claim 12, wherein the salt of the mixture consists of LiTFSI, LiFSI, LiPF6, LiBOB, LiBF4, LiDFOB, LiNO3 or any combination thereof.
18. The electrochemical device of claim 12, wherein the liquefied gas solvent of the mixture includes a solvent having a carbonyl oxygen group.
19. The electrochemical device of claim 18, wherein the carbonyl oxygen group is in the form of formaldehyde, ketene, carbonyl sulfide, carbon monoxide or trifluoroacetyl fluoride.
20. The electrochemical device of claim 12, wherein the liquefied gas solvent of the mixture comprises a solvent having an ether oxygen group.
21. The electrochemical device of claim 20, wherein the ether oxygen group is in the form of dimethyl ether, ethyl methyl ether, methyl vinyl ether, or ethylene oxide, desflurane, 1,1,2,2-tetrafluoro-1-(trifluoromethoxy)ethane, bis(difluoromethyl)ether, methyl pentafluoroethyl ether, or perfluoroethyl methyl ether.
22. The electrochemical device of claim 12, wherein the liquefied gas solvent of the mixture comprises a solvent having an amine nitrogen group.
23. The electrochemical device of claim 22, wherein the amine nitrogen group is in the form of ammonia, methylamine, dimethylamine, trimethylamine, tris(difluoroammonium)fluoromethane, or ethylamine.
24. The electrochemical device of claim 12, wherein the liquefied gas solvent of the mixture further comprises: Fluoromethane, difluoromethane, trifluoromethane, fluoroethane, tetrafluoroethane, pentafluoroethane, 1,1-difluoroethane, 1,2-difluoroethane, 1,1,1-trifluoroethane, 1,1,2-trifluoroethane, 1,1,1,2-tetrafluoroethane, 1,1,2,2-tetrafluoroethane, pentafluoroethane, chloromethane, chloroethane, thionyl fluoride, thionyl chloride fluoride, phosphoryl fluoride, phosphoryl chloride fluoride, sulfuryl fluoride, sulfuryl chloride fluoride, 1- Fluoropropane, 2-fluoropropane, 1,1-difluoropropane, 1,2-difluoropropane, 2,2-fluoropropane, 1,1,1-trifluoropropane, 1,1,2-trifluoropropane, 1,2,2-trifluoropropane; vinyl fluoride; cis-1,2-fluoroethylene; 1,1-fluoroethylene; 1-fluoropropene; 2-propene; chlorine; methyl chloride; bromine; iodine; molecular oxygen; molecular nitrogen; carbon monoxide; carbon dioxide; sulfur dioxide; difluoride.
25. The electrochemical device of claim 12, wherein the device is a capacitor or a battery.
26. A method of constructing an electrochemical device, the method comprising: In a container, mixing an electrolyte mixture consisting of a liquefied gas solvent having a vapor pressure of more than 100 kPa at a temperature of 293.15 K and a salt, wherein the ratio of the salt to the solvent is sufficient to reduce the vapor pressure of the electrolyte mixture to at least 90% of the vapor pressure of the pure liquefied gas solvent at a temperature of 293.15 K; providing a housing having an anode and a cathode; dispensing a sufficient amount of the electrolyte mixture from the container into the housing to allow the anode and cathode to contact the electrolyte mixture; Seal the housing.
27. The method of claim 26, wherein the ratio of salt to solvent of the electrolyte mixture is sufficient to reduce the vapor pressure of the electrolyte mixture to less than 100 kPa at a temperature of 293.15 K, and the dispensing step is performed at or below atmospheric pressure.
28. The method of claim 26, wherein the vapor pressure of the electrolyte mixture at a temperature of 293.15 K is above 100 kPa, and the dispensing step is performed above atmospheric pressure.
29. The method of claim 28, wherein the enclosure structure is selected to maintain the electrolyte mixture above 100 kPa at a temperature of 293.15 K after the enclosure is sealed.