Mask, mask preparation method and display panel
By setting a compensation area with preset compensation structure parameters in the mask of the display panel, the problem of poor film thickness uniformity of large-size display panels is solved, and optical uniformity and viewing angle yield are improved.
Patent Information
- Application Number
- CN202411197031.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-12-06
AI Technical Summary
The overall film thickness of large-size display panels is not uniform, resulting in poor in-plane optical discreteness, affecting the viewing angle yield of the display panel.
Design a mask to set a compensation area with preset compensation structure parameters in the vapor deposition area so as to make the top surface of the pixel film layer formed by the vapor deposition material after the compensation area and the top surface of the pixel film layer formed by other regions. The difference is less than or equal to the preset value, ensuring the uniformity of the overall film thickness of the display panel and reducing optical differences.
By optimizing the compensation structural parameters of the mask, the optical uniformity of the display panel is improved, the optical difference between the inner edge column and the middle column is reduced, and the viewing angle yield is improved.
Smart Images

Figure CN119082664A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display technology, and in particular to a mask, a method for preparing the mask, and a display panel. Background Art
[0002] With the development of technology, display panels are not only used in small devices such as smartphones and tablets, but also in large devices such as televisions, monitors, and public displays. When preparing large-size display panels, in order to ensure optical uniformity, there are high requirements for the uniformity of the overall film thickness of the display panel.
[0003] However, the overall film thickness uniformity of current large-size display panels is not high, which easily leads to poor in-plane optical discreteness and affects the visual color deviation yield of the display panel. Summary of the invention
[0004] Based on this, the present invention aims to provide an improved mask, a method for preparing the mask and a display panel to solve at least one of the above problems.
[0005] In a first aspect, the present application provides a mask for evaporation of a pixel film layer, wherein the mask includes an evaporation area, the evaporation area includes at least one compensation area, the mask structure of the compensation area has preset compensation structure parameters, and the compensation structure parameters are configured to make the height difference between the top surface of the pixel film layer formed on the substrate after the evaporation material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporation material passes through other areas in the evaporation area is less than or equal to a preset value.
[0006] The above-mentioned mask is used for the evaporation of the pixel film layer in the display panel, and by setting a compensation area with preset compensation structural parameters in the evaporation area, the height difference between the top surface of the pixel film layer formed on the substrate after the evaporation material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporation material passes through other areas in the evaporation area is less than or equal to a preset value, which is beneficial to ensure the uniformity of the overall film thickness of the display panel, reduce the optical difference between the edge column and the middle column within the display panel, and improve the optical uniformity of the display panel.
[0007] In one embodiment, the compensation structure parameters are configured so that the top surface of the pixel film layer formed on the substrate after the evaporated material passes through the compensation area is flush with the top surface of the pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporated area.
[0008] In one embodiment, the compensation region includes a first compensation region located at an edge of the mask and extending along a width direction of the mask.
[0009] In one of the embodiments, the first compensation region includes a plurality of first compensation sub-regions arranged along the width direction of the mask, and mask structures of different first compensation sub-regions have the same or different compensation structure parameters.
[0010] In one embodiment, the compensation region includes a second compensation region located on a side of the first compensation region close to the center of the mask.
[0011] In one embodiment, the second compensation region includes a plurality of second compensation sub-regions, and mask structures of different second compensation sub-regions have the same or different compensation structure parameters.
[0012] In one embodiment, the evaporation area includes a first surface and a second surface relative to each other, the first surface is provided with a plurality of first holes, the second surface is provided with a plurality of second holes connected to the first holes, the first holes and the second holes correspond one to one, and the opening area of the second holes is larger than the opening area of the first holes; the compensation structure parameters include the hole depth of the first hole located in the compensation area, wherein the hole depth of the first hole located in the compensation area is less than or equal to a preset depth.
[0013] In one embodiment, the hole depth of the first hole located in the compensation area is less than or equal to 5 μm.
[0014] In one embodiment, the depth of the first hole located in the compensation area is greater than or equal to 3 μm.
[0015] In one embodiment, the first hole includes a first inner surface extending from the first surface to the second surface and arranged at an angle to the first surface, and the compensation structure parameters include the length of the first inner surface of the first hole located in the compensation area and / or the angle formed by the first inner surface and the first surface; wherein the length of the first inner surface is less than or equal to a preset length, and the angle formed by the first inner surface and the first surface is less than or equal to a preset angle.
[0016] In a second aspect, the present application provides a method for preparing a mask, wherein the mask is used for evaporation of a pixel film layer and includes an evaporation region, wherein the preparation method includes:
[0017] determining at least one compensation region in the evaporation region;
[0018] Determine the compensation structure parameters of the mask structure in the compensation area, and apply the compensation structure parameters to the mask structure in the compensation area to obtain the mask; wherein the compensation structure parameters are configured so that the height difference between the top surface of the pixel film layer formed on the substrate after the evaporated material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporated area is less than or equal to a preset value.
[0019] The preparation method of the above-mentioned mask determines the compensation area in the mask evaporation area and determines the compensation structure parameters of the mask structure in the compensation area, and applies the compensation structure parameters to the mask structure in the compensation area, so that the height difference between the top surface of the pixel film layer formed on the substrate after the evaporation material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporation material passes through other areas in the evaporation area is less than or equal to a preset value, so as to ensure the uniformity of the overall film thickness of the display panel, thereby reducing the optical difference between the edge column and the middle column within the display panel, and improving the optical uniformity of the display panel.
[0020] In one of the embodiments, obtaining at least one preset compensation area of the mask includes: obtaining the thickness distribution of the substrate; determining a first target area to be compensated based on the thickness distribution of the substrate; wherein the substrate thickness of the first target area is greater than or equal to a first standard thickness; and determining at least one compensation area of the mask based on the first target area.
[0021] In one embodiment, obtaining at least one preset compensation area of the mask includes: obtaining the superimposed thickness distribution of the pixel film layer formed on the substrate after the evaporated material passes through the original mask and the substrate; wherein the original mask is a mask to which the compensation structural parameters are not applied; determining a second target area to be compensated according to the superimposed thickness distribution; wherein the substrate thickness of the second target area is greater than or equal to a second standard thickness; and determining at least one compensation area of the mask according to the second target area.
[0022] In one embodiment, the compensation structure parameters of the mask structure in the compensation area are determined, and the compensation structure parameters are applied to the mask structure in the compensation area to obtain the mask, including: determining the initial compensation parameters of the mask structure in the compensation area, and applying the initial compensation parameters to the mask structure in the compensation area to obtain a first new version mask; using the first new version mask to evaporate the pixel film layer, and obtaining the height difference between the top surface of the pixel film layer formed on the substrate after the evaporated material passes through the compensation area, and the top surface of the pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporation area; if the height difference is greater than the preset value, adjusting the initial compensation parameters according to the height difference to obtain optimized compensation parameters, and applying the optimized compensation parameters to the mask structure in the compensation area to obtain a second new version mask, and then using the second new version mask to evaporate the pixel film layer and obtain the height difference again, until the height difference is less than or equal to the preset value, to obtain the mask; wherein the latest version of the optimized compensation parameters applied on the mask are the compensation structure parameters.
[0023] In one embodiment, the evaporation area includes a first surface and a second surface relative to each other, the first surface is provided with a plurality of first holes, the second surface is provided with a plurality of second holes connected to the first holes, the opening area of the second holes is larger than the opening area of the first holes, and the compensation structure parameters include the hole depth of the first holes located in the compensation area.
[0024] In a third aspect, the present application provides a display panel, comprising: a substrate; and a plurality of pixel film layers formed on the substrate by evaporating a material through a mask as described above.
[0025] In the above-mentioned display panel, the height difference of the top surface of the pixel film layer at different positions is less than or equal to a preset value, which ensures the uniformity of the overall film thickness of the display panel, is beneficial to reducing the optical difference between the edge column and the middle column within the display panel, and improves the optical uniformity of the display panel.
[0026] In a fourth aspect, the present application provides a display device, comprising a housing and a display panel as described above and disposed on the housing.
[0027] The above display device, by providing a display panel with better optical uniformity, is helpful to improve the user's viewing experience and usage experience. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] In order to more clearly illustrate the implementation methods of this specification or the technical solutions in the prior art, the drawings required for use in the implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some implementation methods recorded in this specification. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0029] Figure 1 Schematic diagram of the evaporation of pixel film layer in traditional technology
[0030] Figure 2 Schematic diagram of film thickness distribution of anode substrate in conventional technology;
[0031] Figure 3 This is a schematic diagram of the structure of an embodiment of the present application;
[0032] Figure 4 for Figure 3 Schematic cross-sectional view of section AA;
[0033] Figure 5 It is a structural schematic diagram of forming a pixel film layer on a substrate using a mask according to an embodiment of the present application;
[0034] Figure 6 for Figure 5 The enlarged schematic diagram of the P1 part;
[0035] Figure 7 for Figure 5 An enlarged schematic diagram of the P2 portion;
[0036] Figure 8 It is a structural schematic diagram of forming a pixel film layer on a substrate using a mask according to another embodiment of the present application;
[0037] Fig. 9 for Figure 8 An enlarged schematic diagram of the P3 portion;
[0038] Fig.10 A schematic diagram of mask structure adjustment according to a specific embodiment of the present application;
[0039] Fig.11 for Fig.10 A schematic diagram of color point comparison between the specific embodiment and the original mask;
[0040] Fig.12 for Fig.10 A schematic diagram comparing the optical effects of the display panel formed by the specific embodiment and the original mask;
[0041] Fig.13 A flowchart of a method for preparing a mask according to an embodiment of the present application;
[0042] Fig.14 A schematic diagram of a first compensation area according to an embodiment of the present application;
[0043] Fig.15 A schematic diagram of a second compensation area according to an embodiment of the present application;
[0044] Fig.16 FIG. 4 is a schematic diagram of vapor deposition of a pixel film layer using a mask according to an embodiment of the present application.
[0045] Component number description:
[0046] 100', a mask in conventional technology, 300', a pixel film layer obtained by evaporation using a conventional mask, 100, a mask, 200, a substrate, 300, a pixel film layer, 400, a source of evaporation material;
[0047] 110, evaporation region, 120, non-evaporation region, 111, compensation region, 111A, first compensation region, 111A1-111A5, first compensation sub-region, 111B, second compensation region, 111B1-111B3, second compensation sub-region, 112, other regions in the evaporation region, 113, first surface, 114, second surface, 1130, first hole, 1140, second hole, 1131, first inner surface, 1141, second inner surface;
[0048] 310~360, pixel film layer. DETAILED DESCRIPTION
[0049] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific embodiments disclosed below.
[0050] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0051] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0052] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used herein are for illustrative purposes only and are not intended to be the only implementation method.
[0053] In the process of implementing the present invention, the inventors found that the related art has the following problems:
[0054] In an organic light-emitting diode (OLED) device, the organic matter contained in the light-emitting layer can be evaporated on a substrate by an evaporation mask called a fine metal mask (FMM), and the evaporated organic matter can be formed into a pattern corresponding to the pattern formed on the evaporation mask 100' to play the role of a pixel.
[0055] like Figure 1 As shown, the conventional evaporation device includes a mask 100', a substrate 200 and an evaporation material source 400, and the entire evaporation device is arranged in a vacuum chamber. During evaporation, the evaporation material emitted by the evaporation material source 400 can be incident on the substrate 200 through the through hole in the mask 100', thereby forming a pixel film layer 300 on the substrate 200. Among them, the pixel film layer 300 may include a red (Red) pixel film layer, a green (Green) pixel film layer, and a blue (Blue) pixel film layer. Each color pixel film layer can emit a light beam of a corresponding color wavelength. The light beam will be transmitted and reflected at different interfaces in the OLED device, resulting in a complex interference phenomenon. In order to produce constructive interference of the light beam, the superimposed film thickness of the pixel film layer 300 and the substrate 200 can be controlled to form a resonant microcavity inside the OLED device to maximize the brightness of the light beam emitted from the display panel.
[0056] However, the inventors found that Figure 1 and Figure 2As shown, since the anode substrate (i.e., base 200) has a thickness distribution shape with high edges (shaded part) and low middle in the length direction (i.e., aa direction), it is easy to cause the top surface flatness of the pixel film layer formed on the anode substrate to be poor, and the microcavity length on both sides of the device is higher than expected, which in turn causes the overall optical uniformity of the display panel to be low, affecting the color deviation yield of the product. Among them, the anode substrate may include an indium tin oxide layer (ITO), the pixel film layer 300 may be formed on the ITO layer, and the microcavity length is approximately the superimposed thickness of the ITO layer and the pixel film layer.
[0057] In view of this, an embodiment of the present application provides an improved mask, which, by setting a compensation area with preset compensation structural parameters in the evaporation area, makes the height difference between the top surface of the pixel film layer formed on the substrate after the evaporation material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporation material passes through other areas in the evaporation area is less than or equal to a preset value, thereby ensuring the uniformity of the overall film thickness of the display panel, reducing the optical difference between the edge column and the middle column within the display panel, and improving the optical uniformity of the display panel.
[0058] like Figure 3 and Figure 4 As shown, an embodiment of the present application provides a mask 100, including a vapor deposition area 110, the vapor deposition area 110 includes at least one compensation area 111, and the mask structure of the compensation area 111 has preset compensation structure parameters; wherein the compensation structure parameters are configured to: make the height difference between the top surface of the pixel film layer formed on the substrate after the vapor deposition material passes through the compensation area 111 and the top surface of the pixel film layer formed on the substrate after the vapor deposition material passes through other areas 112 in the vapor deposition area 110 is less than or equal to a preset value.
[0059] For example, see Figure 3 , the mask 100 may include an evaporation region 110 and non-evaporation regions 120 located on both sides of the length direction (i.e., aa direction) of the mask 100. Among them, the evaporation region 110 may be a region for forming a pixel film layer, that is, the evaporation material may form a pixel film layer on the substrate through the evaporation region 110; the non-evaporation region 120 may be a region that does not participate in evaporation, and optionally, the non-evaporation region 120 may include a frame fixing region for fixing the mask 100 to the frame. Further, the evaporation region 110 includes at least one compensation region 111 and other regions 112 located outside the compensation region 111, so that the evaporation material can form a corresponding pixel film layer on the substrate after passing through the compensation region 111 and other regions 112 in the evaporation region 110.
[0060] Optionally, the evaporation area 110 may include a plurality of effective evaporation areas spaced apart along the length direction (i.e., the aa direction) of the mask 100 and non-effective evaporation areas outside the effective evaporation areas, wherein through holes are formed in the effective evaporation areas for the evaporation material to pass through, and through holes may or may not be provided in the non-effective evaporation areas (for example, the spacing area between two adjacent effective evaporation areas and the outer edge area of the effective evaporation areas), and the present application does not impose any restrictions on this. Furthermore, the evaporation area 110 includes at least one compensation area 111 and other areas 112 located outside the compensation area 111, so that the compensation area 111 is located in the above-mentioned effective evaporation area, part of the other areas 112 may be located in the above-mentioned effective evaporation area, and part of the other areas 112 may be located in the above-mentioned non-effective evaporation area. Therefore, during evaporation, the evaporation material can form a pixel film layer on the substrate after passing through other areas 112 located in the effective evaporation area, and the evaporation material does not form a pixel film layer on the substrate without passing through other areas 112 located in the non-effective evaporation area or even after passing through other areas 112 located in the non-effective evaporation area.
[0061] Optionally, the compensation region 111 may be located on both sides of the length direction of the mask 100 (i.e., the aa direction), thereby corresponding to the region with a higher layer thickness of the anode substrate (i.e., the base 200). It can be understood that when the layer thickness of the anode substrate on both sides along its width direction is higher, the compensation region 111 may also be formed on both sides of the width direction of the mask (i.e., the bb direction). Therefore, when the compensation region 111 is actually set, it can be determined according to the thickness distribution of the base 200.
[0062] Optional, such as Figure 4 As shown, the compensation structure parameters may include one or more of the through hole size, the depth of the through hole, the inclination degree, the length, and the angle of the hole wall on the mask structure in the compensation area 111. By reasonably setting the above compensation structure parameters, the height difference between the top surface of the pixel film layer formed on the substrate after the evaporation material passes through the compensation area 111 and the top surface of the pixel film layer formed on the substrate after the evaporation material passes through other areas 112 in the evaporation area 110 can be less than or equal to a preset value, which is beneficial to ensure the uniformity of the overall film thickness of the display panel, reduce the optical difference between the edge column and the middle column in the display panel, and improve the optical uniformity of the display panel.
[0063] Optionally, the preset value can be set according to different design schemes of the RGB pixel film layer, and at least one of the optical requirements and specification requirements of different display panels. In general, when the optical uniformity requirements of the display panel are high, the preset value can be set to be smaller to improve the alignment accuracy of the top surfaces of different pixel film layers; when the optical uniformity requirements of the display panel are not high, the preset value can be set to be larger to reduce the difficulty of mask design and preparation, and reduce the preparation cost of the display panel. Optionally, when the two top surfaces used for comparison are both planes, the height difference between the two top surfaces can be expressed as the absolute value of the difference in the vertical distance of the two top surfaces relative to the same reference plane, wherein the two top surfaces are parallel to the reference plane. Optionally, when at least one of the two top surfaces used for comparison is a curved surface, the height difference between the two top surfaces can be expressed as the height difference between the two cut surfaces at the bottom or top of the two top surfaces, and the height difference between the two cut surfaces can be expressed as the absolute value of the difference in the vertical distance of the two cut surfaces relative to the same reference plane, wherein the two cut surfaces are parallel to the reference plane.
[0064] by Figures 5 to 7 As shown in the figure, after the evaporation material passes through the evaporation area 110, a pixel film layer 310, a pixel film layer 320, and a pixel film layer 330 are formed on the substrate 200. The thickness of the substrate 200 is high on both sides and low in the middle. The pixel film layer 310 and the pixel film layer 330 are formed on both sides of the substrate 200 by the evaporation material passing through the compensation area 111, and the pixel film layer 320 is formed in the middle of the substrate 200 by the evaporation material passing through the other area 112 located in the effective evaporation area. Figure 6 and Figure 7 It can be seen that the top surface of the pixel film layer 320 is higher than the top surface of the pixel film layer 310 by ΔH1, and the top surface of the pixel film layer 330 is higher than the top surface of the pixel film layer 320 by ΔH2, wherein ΔH1 and ΔH2 are both less than or equal to the preset value, indicating that the superimposed film thickness of the pixel film layer formed by the mask 100 and the substrate 200 meets the preset uniformity requirement, which is beneficial to improving the optical uniformity of the display panel.
[0065] In some embodiments of the present application, the compensation structure parameters are configured to make the top surface of the pixel film layer formed on the substrate after the evaporated material passes through the compensation area flush with the top surface of the pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporation area. By controlling the compensation structure parameters to meet the above settings, it is helpful to better make the superimposed film thickness of the pixel film layer and the substrate meet the preset uniformity requirements, thereby helping to further improve the optical uniformity of the display panel.
[0066] In some embodiments of the present application, Figure 3As shown, the compensation region 110 includes a first compensation region 111A located at the edge of the mask 100 and extending along the width direction of the mask (i.e., the bb direction). Since the anode substrate (ITO) has a relatively obvious thickness distribution shape of high on both sides and low in the middle, the edge regions on both sides of the mask 100 can be set as the first compensation region 111A along the width direction of the mask 100 corresponding to the thickness distribution of the anode substrate, so as to reversely compensate for the region of the substrate 200 with obviously poor uniformity, thereby improving the uniformity of the overall film thickness of the display panel.
[0067] Optional, such as Fig.14 As shown, the first compensation region 111A may include a plurality of first compensation sub-regions 111A1, 111A2, 111A3, 111A4, and 111A5 arranged along the width direction (bb direction) of the mask 100. Optionally, the first compensation sub-regions 111A1 and 111A2 may be arranged continuously, and the first compensation sub-regions 111A3, 111A4, and 111A5 may be arranged at intervals. In addition, the mask structures of different first compensation sub-regions may have the same or different compensation structure parameters. For example, if the substrate thickness corresponding to the first compensation sub-region 111A1 is thicker than the substrate thickness corresponding to the first compensation sub-region 111A2, the compensation structure parameters of the first compensation region 111A1 may be different from the compensation structure parameters of the first compensation sub-region 111A2.
[0068] For further information, see Figure 3 , the compensation area 111 also includes a second compensation area 111B located on one side of the first compensation area 111A1 close to the center of the mask 100. Since the optical uniformity of the display panel is the optical uniformity within the entire surface, in addition to compensating the thickness on both sides of the substrate 200, the uniformity of the superimposed film thickness of other areas on the substrate 200 and the pixel film layer must also be considered. When the superimposed film thickness of other areas on the substrate 200 and the pixel film layer does not meet the preset uniformity condition (for example, the height difference between the top surfaces of the two pixel film layers is greater than the preset value), the corresponding area on the mask 100 can be set as the second compensation area 111B to reversely compensate for the part of the substrate 200. Therefore, by setting the second compensation area 111B, it is more conducive to ensuring the uniformity of the overall film thickness of the display panel, thereby improving the optical uniformity of the display panel. Optionally, the length of the second compensation area 111B along the width direction of the mask 100 (i.e., the bb direction) is less than or equal to the length of the first compensation area 111A along the width direction of the mask 100.
[0069] Optional, such as Fig.15As shown, the second compensation region 111B may include a plurality of arranged second compensation sub-regions 111B1, 1111B2, and 111B3, and each second compensation sub-region is discretely arranged. In addition, the mask structures of different second compensation sub-regions have the same or different compensation structure parameters. For example, if the substrate thickness corresponding to the second compensation sub-region 111B1 is thicker than the substrate thickness corresponding to the second compensation sub-region 111B2, the compensation structure parameters of the second compensation region 111B1 may be different from the compensation structure parameters of the second compensation sub-region 111B2.
[0070] In some embodiments of the present application, the compensation structure parameters are configured to make the height difference between the bottom of the top surface of the pixel film layer formed on the substrate after the vapor deposition material passes through the compensation area and the bottom of the top surface of the pixel film layer formed on the substrate after the vapor deposition material passes through other areas in the vapor deposition area is less than or equal to a preset value. Depending on the selection of the compensation structure parameters, the top surface morphology of the pixel film layer formed on the substrate will also be different. Figure 8 As shown, the evaporation material forms pixel film layers 340, 350, and 360 on the substrate 200 after passing through the evaporation area 110, wherein the pixel film layers 340 and 360 are formed on both sides of the substrate 200 by the evaporation material passing through the compensation area 111, and the top surfaces of the pixel film layers 340 and 360 are concave curved surfaces, and the pixel film layer 350 is formed in the middle of the substrate 200 by the evaporation material passing through the other area 112 located in the effective evaporation area, and the top surface of the pixel film layer 350 is a plane. Fig. 9 As shown, the bottommost section through the top surface of the pixel film layer 340 is lower than the top surface of the pixel film layer 350 by ΔH3, where ΔH3 is less than or equal to a preset value. On the other hand, the bottommost section through the top surface of the pixel film layer 340 is flush with the top surface of the pixel film layer 350, thereby meeting the uniformity requirement of the overall film thickness of the display panel. If the top surfaces of the pixel film layer 340 and the pixel film layer 360 are convex curved surfaces, the corresponding height difference value can be obtained by taking the section through the topmost part of the top surface, and then judging whether the overall film thickness of the display panel meets the uniformity requirement. For details, please refer to the judgment method of the above-mentioned concave curved surface, which will not be repeated here.
[0071] Further, such as Figure 4As shown, the evaporation region 110 includes a first surface 113 and a second surface 114 that are opposite to each other, the first surface 113 is provided with a plurality of first holes 1130, the second surface 114 is provided with a plurality of second holes 1140 that are connected to the first holes 1130, the first holes 1130 and the second holes 1140 correspond to each other one by one, and the opening area of the second holes 1140 is greater than the opening area of the first holes 1130; the compensation structure parameter includes the hole depth of the first hole 1130 located in the compensation region 111, wherein the hole depth of the first hole 1130 located in the compensation region 111 is less than or equal to the preset depth. Exemplarily, since the opening area of the second hole 1140 is greater than the opening area of the first hole 1130, the second hole 1140 may face the incident side of the evaporation material of the mask 100, and the first hole 1130 may face the evaporation material exit side of the mask 100. Optionally, a hole depth h of the first holes 1130 located in the compensation area 111 is smaller than a hole depth h′ of the first holes 1130 located in other areas 112 in the evaporation area 110 .
[0072] By making the hole depth of the first hole 1130 located in the compensation area 111 less than or equal to the preset depth, the evaporated material emitted through the first hole 1130 can form a pixel film layer 300 with more convergent shadows on both sides of the substrate, thereby facilitating the reduction of the middle film thickness of the pixel film layer, so that it can reversely compensate for the thickness of the corresponding substrate, and improve the uniformity of the overall film thickness of the display panel. Fig.16 As shown, after the evaporated material is emitted through the large-hole deep mask structure (dashed line portion), a pixel film layer 300' will be formed on the substrate 200. When the hole depth of the first hole 1130 is reduced to be less than or equal to the preset depth, the evaporated material is emitted through the small-hole deep mask structure (solid line portion) to form a pixel film layer 300 on the substrate 200. It can be seen that the shadow areas on both sides of the pixel film layer 300 are more convergent than the pixel film layer 300', which is beneficial to reduce the thickness of the middle area of the pixel film layer 300 and realize reverse compensation for the thicker substrate portion.
[0073] Optionally, the hole depth of the first hole 1130 located in the compensation area 111 is less than or equal to 5μm, for example, it can be 2μm, 3μm, 4μm, 5μm. By controlling the hole depth of the first hole 1130 located in the compensation area 111 to meet the above range, it is helpful to fully reduce the intermediate film thickness of the pixel film layer, thereby effectively reversely compensating the substrate. Optionally, the hole depth of the first hole 1130 located in the compensation area 111 is greater than or equal to 3μm, for example, it can be 3μm, 3.5μm, 4μm, 4.5μm, 5μm. By controlling the hole depth of the first hole 1130 located in the compensation area 111 to meet the above range, it is helpful to avoid excessive reverse compensation and cause the height difference between the top surfaces of the pixel film layer to increase.
[0074] Optional, continue to see Figure 4 , the first hole 1130 includes a first inner surface 1131 extending from the first surface 113 to the second surface 114 and arranged at an angle with the first surface 113, and the compensation structural parameters include the length L of the first inner surface 1131 of the first hole 1130 located in the compensation area 111 and / or the angle formed by the first inner surface 1131 and the first surface 113; wherein, the length of the first inner surface 1131 is less than or equal to the preset length, and the angle formed by the first inner surface 1131 and the first surface 113 is less than or equal to the preset angle. In this way, it is beneficial to adjust the hole depth of the first hole 1130 through multiple degrees of freedom. Optionally, the second hole 114 also has a second inner surface 1141 arranged at an angle with the second surface 114. Since the second inner surface 1141 is connected to the first inner surface 1131, the hole depth of the first hole 1130 can also be adjusted by setting the length L and / or the inclination angle of the second inner surface 1141.
[0075] The mask and effects of the embodiment of the present application will be further described below through a specific embodiment.
[0076] like Fig.10 As shown, both mask 100' and mask 100 can divide the effective evaporation area into multiple sub-areas. According to the thickness distribution of the anode substrate (i.e., substrate 200), the colored areas AA, AB, BA, CA, CB, DA, EA, EB, AT, AU, BU, CT, CU, DU, ET, and EU on mask 100 correspond to the thicker areas on substrate 200. Since mask 100' does not perform compensation design on these areas, it is difficult to ensure the uniformity of the overall film thickness of the display panel; on mask 100, AA, BA, CA, DA, EA, AU, BU, CU, DU, and EU located at the edge are set as the first compensation area, and AB, CB, EB, AT, CT, and ET close to the first compensation area are set as the second compensation area for compensation design (reducing the hole depth of the first hole located in the compensation area), thereby greatly improving the uniformity of the overall film thickness of the display panel, reducing the optical difference between the edge column and the middle column in the display panel, and greatly improving the optical uniformity of the display panel.
[0077] in,
[0078] Fig.11A schematic diagram of the color point comparison formed by mask 100 and mask 100' is shown, wherein the color point represents the position of the color in a specific color space (such as CIE1931 color space, CIE1976 color space, etc.), usually represented by color coordinates (x, y), which define the specific position of the color in the color space, thereby allowing accurate replication and comparison of colors. It can be seen that the red light color point of the pixel film layer formed by the optimized mask 100 is significantly reduced, that is, the value of the red light color point color coordinate X direction is significantly reduced (from 0.681 to 0.68). It can be seen that the pixel film layer formed by the mask 100 can complement the anode ITO to reduce the microcavity thickness, so that the optical color point of the display panel is close to the normal level and the optical uniformity of the display panel is improved, wherein the microcavity thickness represents the thickness of the resonant cavity formed between the fully reflective anode and the semi-reflective cathode in the display panel, mainly including the thickness of the ITO layer and the thickness of the organic light-emitting layer (pixel film layer). Further, Fig.12 A schematic diagram comparing the optical effects of the display panels formed by the mask 100 and the mask 100' is shown. It can be seen that the optimized mask 100 can significantly improve the problem of high optical quality at the edge columns of the display panel, thereby improving the uniformity of the monochrome color points within the display panel surface. The estimated improvement compared to the traditional mask is greater than or equal to 30% (for example, the estimated improvement may be 40%, 50%, 60%, etc.), thereby reducing the discreteness of JNCD (just Noticeable Color Difference, JNCD). For example, it is estimated that the monochromatic discreteness within the optical surface can be reduced from 0.23% to 0.15% (a reduction of about 0.08%); and for the chromatic aberration dispersion, the value of θJNCDσ can be used as an evaluation parameter (where θ represents the angle between the human eye's line of sight and the normal of the display panel, σ represents the discreteness, for example, 0°JNCDσ represents the chromatic aberration dispersion value when the human eye vertically observes the display panel). If 0°JNCDσ is taken as 0 as the evaluation standard (the closer the discrete value is to 0, the lower the degree of discreteness and the better the display effect), the display panel made by the mask of the present application can reduce the 30°JNCDσ from 0.45 to 0.34, the 45°JNCDσ can be reduced from 0.62 to 0.49, and the 60°JNCDσ can be reduced from 0.48 to 0.35 compared to the display panel made by the traditional mask; in addition, the defective rate can also be reduced by about 0.5%.
[0079] An embodiment of the present application also provides a method for preparing a mask, by determining a compensation area in the mask evaporation area and determining the compensation structure parameters of the mask structure in the compensation area, and applying the compensation structure parameters to the mask structure in the compensation area, so that the height difference between the top surface of the pixel film layer formed on the substrate after the evaporation material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporation material passes through other areas in the evaporation area is less than or equal to a preset value, so as to ensure the uniformity of the overall film thickness of the display panel, thereby reducing the optical difference between the edge column and the middle column within the display panel, and improving the optical uniformity of the display panel.
[0080] like Fig.11 As shown, the above preparation method comprises:
[0081] S100: Determine at least one compensation area in a vapor deposition area.
[0082] S200, determining compensation structure parameters of the mask structure in the compensation area, and applying the compensation structure parameters to the mask structure in the compensation area to obtain a mask; wherein the compensation structure parameters are configured so that the height difference between the top surface of the pixel film layer formed on the substrate after the evaporated material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporated area is less than or equal to a preset value.
[0083] The evaporation area, compensation area, compensation structure parameters and preset values may refer to the relevant description of the mask 100 in the aforementioned embodiment, and will not be repeated here.
[0084] In some embodiments of the present application, step S100 may include:
[0085] S110, obtaining thickness distribution of the substrate;
[0086] S120, determining a first target area to be compensated according to the thickness distribution of the substrate; wherein the substrate thickness of the first target area is greater than or equal to the first standard thickness;
[0087] S130. Determine at least one compensation area of the mask according to the first target area.
[0088] Exemplarily, due to the manufacturing process error of the substrate, its thickness may present a distribution form with high sides and low middle. By obtaining the thickness distribution of the substrate, the position of the compensation area on the mask can be determined according to the thickness distribution. Optionally, when the thickness of the area on the substrate is greater than or equal to the first standard thickness, the part of the substrate area can be determined as the area that needs to be reversely compensated, and then at least one compensation area on the mask can be determined according to the part of the substrate area.
[0089] It should be noted that the present application does not limit the order of steps S110-S130. As long as the purpose of the present invention can be achieved, even if the order of the steps is changed, it still falls within the protection scope of the present invention.
[0090] In some embodiments of the present application, step S100 may include:
[0091] S110', obtaining the superimposed thickness distribution of the pixel film layer formed on the substrate by the evaporation material after passing through the original mask and the substrate; wherein the original mask is a mask to which no compensation structural parameters are applied;
[0092] S120', determining a second target area to be compensated according to the stacked thickness distribution; wherein the substrate thickness of the second target area is greater than or equal to the second standard thickness;
[0093] S130', determining at least one compensation area of the mask according to the second target area.
[0094] Exemplarily, the area requiring reverse compensation can be determined by obtaining the distribution of the superimposed thickness of the anode substrate and the originally formed pixel film layer. Optionally, when it is observed that the superimposed thickness of the anode substrate and the originally formed pixel film layer is greater than or equal to the second standard thickness, the partial substrate area can be determined as the area requiring reverse compensation, and then at least one compensation area on the mask can be determined based on the partial substrate area.
[0095] It should be noted that the present application does not limit the order of steps S110'-S130'. As long as the purpose of the present invention can be achieved, even if the order of the steps is changed, it still falls within the protection scope of the present invention.
[0096] In some embodiments of the present application, step S200 may include the following steps:
[0097] S210, determining initial compensation parameters of the mask structure in the compensation area, and applying the initial compensation parameters to the mask structure in the compensation area to obtain a first new version mask;
[0098] S220, performing vapor deposition of a pixel film layer using a first new mask, and obtaining a height difference between a top surface of the pixel film layer formed on the substrate after the vapor deposition material passes through the compensation area and a top surface of the pixel film layer formed on the substrate after the vapor deposition material passes through other areas in the vapor deposition area;
[0099] S230. If the height difference is greater than the preset value, the initial compensation parameters are adjusted according to the height difference to obtain optimized compensation parameters, and the optimized compensation parameters are applied to the mask structure in the compensation area to obtain a second new version of the mask, and then the second new version of the mask is used to evaporate the pixel film layer and obtain the height difference again until the height difference is less than or equal to the preset value to obtain a mask; wherein the latest version of the optimized compensation parameters applied on the mask are the compensation structure parameters of the mask structure in the compensation area on the mask.
[0100] Optionally, the initial compensation parameters can be determined based on the thickness distribution of the substrate, or based on the superimposed thickness distribution of the pixel film layer formed on the substrate after the vapor deposition material passes through the original mask and the substrate, wherein the original mask is a mask to which the compensation structural parameters are not applied. It should be noted that the mask to which the initial compensation parameters determined in the above manner are applied can improve the optical uniformity of the display panel to a certain extent, but affected by the process, equipment and other external factors, such a preliminary improved mask may not be able to achieve the desired optical uniformity display effect in one step, so the initial compensation parameters can be adjusted and optimized according to the actual vapor deposition situation, and then the preliminary improved mask is iteratively optimized, and finally a mask that makes the display panel meet the optical uniformity display requirements is obtained.
[0101] Optionally, the evaporation area includes a first surface and a second surface relative to each other, the first surface is provided with a plurality of first holes, the second surface is provided with a plurality of second holes connected to the first holes, the opening area of the second holes is larger than the opening area of the first holes, and the compensation structure parameters include the hole depth of the first holes located in the compensation area.
[0102] Since reducing the hole depth of the first hole can correspondingly reduce the intermediate film thickness of the pixel film layer formed on the substrate, the intermediate film thickness of the pixel film layer formed on the substrate through the compensation area can be reduced by reducing the hole depth of the first hole located in the compensation area, thereby reversely compensating the thick area of the anode substrate, reducing the microcavity length, lowering the color point coordinates, and improving the optical uniformity of the display panel.
[0103] The embodiment of the present application further provides a display panel, comprising: a substrate; and a plurality of pixel film layers formed on the substrate by evaporating a material through a mask as described above.
[0104] In the above-mentioned display panel, the height difference of the top surface of the pixel film layer at different positions is less than or equal to a preset value, which ensures the uniformity of the overall film thickness of the display panel, is beneficial to reducing the optical difference between the edge column and the middle column within the display panel, and improves the optical uniformity of the display panel.
[0105] An embodiment of the present application further provides a display device, comprising a housing and a display panel as described above and disposed on the housing.
[0106] The above display device, by providing a display panel with better optical uniformity, is helpful to improve the user's viewing experience and usage experience.
[0107] For example, the display device can be any product or component with a display function, such as a mobile phone, a tablet computer, a television, a monitor, a laptop computer, a digital photo frame, a navigator, a smart wearable device, etc. Other essential components of the display device should be understood by ordinary technicians in the field, and will not be described in detail here, nor should they be used as limitations to the present application.
[0108] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0109] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A mask for evaporation of pixel film layer, It is characterized in that The mask comprises an evaporation region, the evaporation region comprises at least one compensation region, and the mask structure of the compensation region has preset compensation structure parameters; in, The compensation structure parameters are configured so that the height difference between the top surface of the pixel film layer formed on the substrate after the evaporated material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporated area is less than or equal to a preset value.
2. The mask according to claim 1, It is characterized in that The compensation structure parameters are configured so that a top surface of a pixel film layer formed on the substrate after the evaporated material passes through the compensation area is flush with a top surface of a pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporated area.
3. The mask according to claim 1, It is characterized in that The compensation region includes a first compensation region located at an edge of the mask and extending along a width direction of the mask; Preferably, the first compensation region includes a plurality of first compensation sub-regions arranged along the width direction of the mask, and mask structures of different first compensation sub-regions have the same or different compensation structure parameters; Preferably, the compensation region includes a second compensation region located on one side of the first compensation region close to the center of the mask; Preferably, the second compensation region includes a plurality of second compensation sub-regions, and mask structures of different second compensation sub-regions have the same or different compensation structure parameters.
4. The mask according to any one of claims 1 to 3, It is characterized in that The evaporation region includes a first surface and a second surface opposite to each other, the first surface is provided with a plurality of first holes, the second surface is provided with a plurality of second holes connected to the first holes, the first holes correspond to the second holes one by one, and the opening area of the second holes is larger than the opening area of the first holes; The compensation structure parameter includes a hole depth of the first hole located in the compensation area, wherein the hole depth of the first hole located in the compensation area is less than or equal to a preset depth; Preferably, the depth of the first hole located in the compensation area is less than or equal to 5 μm; Preferably, the depth of the first hole located in the compensation area is greater than or equal to 3 μm; Preferably, the first hole includes a first inner surface extending from the first surface to the second surface and arranged at an angle to the first surface, and the compensation structure parameters include the length of the first inner surface of the first hole located in the compensation area and / or the angle formed by the first inner surface and the first surface; wherein, the length of the first inner surface is less than or equal to a preset length, and the angle formed by the first inner surface and the first surface is less than or equal to a preset angle.
5. A method for preparing a mask, wherein the mask is used for evaporation of a pixel film layer and comprises an evaporation region, It is characterized in that The preparation method comprises: determining at least one compensation region in the evaporation region; Determine the compensation structure parameters of the mask structure in the compensation area, and apply the compensation structure parameters to the mask structure in the compensation area to obtain the mask; wherein the compensation structure parameters are configured so that the height difference between the top surface of the pixel film layer formed on the substrate after the evaporated material passes through the compensation area and the top surface of the pixel film layer formed on the substrate after the evaporated material passes through other areas in the evaporated area is less than or equal to a preset value.
6. The preparation method according to claim 5, It is characterized in that The acquiring at least one preset compensation area of the mask comprises: Obtaining a thickness distribution of the substrate; Determining a first target area to be compensated according to the thickness distribution of the substrate; wherein the substrate thickness of the first target area is greater than or equal to a first standard thickness; At least one compensation region of the mask is determined based on the first target region.
7. The preparation method according to claim 5, It is characterized in that The acquiring at least one preset compensation area of the mask comprises: Obtaining the superimposed thickness distribution of the pixel film layer formed on the substrate by the evaporated material after passing through the original mask and the substrate; wherein the original mask is a mask to which the compensation structure parameters are not applied; Determine a second target area to be compensated according to the stacked thickness distribution; wherein the substrate thickness of the second target area is greater than or equal to a second standard thickness; At least one compensation region of the mask is determined based on the second target region.
8. The preparation method according to any one of claims 5 to 7, It is characterized in that The step of determining compensation structure parameters of the mask structure of the compensation area and applying the compensation structure parameters to the mask structure of the compensation area to obtain the mask comprises: Determining initial compensation parameters of the mask structure of the compensation area, and applying the initial compensation parameters to the mask structure of the compensation area to obtain a first new version of the mask; Using the first new mask to perform evaporation of a pixel film layer, and obtaining a height difference between a top surface of the pixel film layer formed on the substrate after the evaporation material passes through the compensation area and a top surface of the pixel film layer formed on the substrate after the evaporation material passes through other areas in the evaporation area; If the height difference is greater than the preset value, the initial compensation parameter is adjusted according to the height difference to obtain an optimized compensation parameter, and the optimized compensation parameter is applied to the mask structure of the compensation area to obtain a second new version of the mask, and then the second new version of the mask is used to evaporate the pixel film layer and obtain the height difference again until the height difference is less than or equal to the preset value to obtain the mask; wherein the latest version of the optimized compensation parameter applied on the mask is the compensation structure parameter; Preferably, the evaporation area includes a first surface and a second surface relative to each other, the first surface is provided with a plurality of first holes, the second surface is provided with a plurality of second holes connected to the first holes, the opening area of the second holes is larger than the opening area of the first holes, and the compensation structure parameters include the hole depth of the first holes located in the compensation area.
9. A display panel, It is characterized in that include: substrate; as well as, A plurality of pixel film layers are formed on the substrate after the evaporation material passes through a mask as described in any one of claims 1 to 4 or a mask prepared by the method for preparing a mask as described in any one of claims 5 to 8.
10. A display device, It is characterized in that The invention comprises a housing and the display panel as claimed in claim 9 arranged on the housing.