Electrophotographic apparatus
By using polyaryl resin and an ether structure resin in an electrophotographic device, as well as a strontium titanate toner, the problem of deterioration of transfer properties under low temperature/low humidity conditions is solved, and higher durability and image quality are achieved.
Patent Information
- Application Number
- CN202410708796.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-05
- Filing Date
- 2024-06-03
- Publication Date
- 2024-12-06
AI Technical Summary
The problem of deterioration in transferability of existing electrophotographic equipment under low temperature/low humidity conditions leads to degradation of image quality and waste of toner.
An electrophotographic photosensitive member containing a polyaryl resin is used, and an ether structure is introduced into the resin to enhance the discharge deterioration resistance, and strontium titanate is used as an external additive for the toner to improve transferability and durability.
The transferability and durability of the electrophotographic equipment are significantly improved under low temperature/low humidity conditions, reducing toner residues, and improving image quality.
Smart Images

Figure BDA0004873403160000021 
Figure BDA0004873403160000081 
Figure BDA0004873403160000082
Abstract
Description
Technical Field
[0001] The present invention relates to an electrophotographic apparatus having an electrophotographic photosensitive member. Background Art
[0002] An organic electrophotographic photosensitive member (hereinafter also referred to simply as "electrophotographic photosensitive member" or "photosensitive member") containing an organic photoconductive material (charge generating material) is used as an electrophotographic photosensitive member installed in an electrophotographic apparatus and a process cartridge. In recent years, there has been a demand for electrophotographic apparatuses with longer lifespans, and thus there has been a demand for providing electrophotographic photosensitive members having enhanced image quality and wear resistance (mechanical durability).
[0003] In addition to the above-mentioned methods for longer life, recent electrophotographic apparatuses are also required to achieve enhanced image quality and reduced amount of waste toner by increasing the efficiency of the transfer process to prevent toner from scattering during transfer.
[0004] Polycarbonate resin is generally used as a binder resin for a charge transport layer of an electrophotographic photosensitive member. Strontium titanate is used as an external additive for a toner for electrostatic charge image development to control the chargeability of the toner. Japanese Patent Application Laid-Open No. 2021-131520 proposes an electrophotographic device in which a polycarbonate resin is used as a binder resin for a charge transport layer of a photosensitive member, and a toner having strontium titanate as an external additive is used.
[0005] It is proposed to enhance the durability of an electrophotographic photosensitive member by using a polyarylate resin having higher mechanical strength than a polycarbonate resin as a binder resin for a charge transport layer. The polyarylate resin is a polyester resin containing an aromatic dicarboxylic acid. Japanese Patent Application Laid-Open No. 2011-227486 proposes a photosensitive member having enhanced durability and electrical characteristics by including a polyarylate resin in a photosensitive layer.
[0006] Studies conducted by the present inventors have concluded that an image forming apparatus that replaces the polycarbonate resin of the electrophotographic photosensitive member described in Japanese Patent Application Laid-Open No. 2021-131520 with the polyarylate resin described in Japanese Patent Application Laid-Open No. 2011-227486 to impart enhanced durability to the photosensitive member has room for improving transferability under a low temperature / low humidity environment after durability.
[0007] Therefore, an object of the present invention is to provide an image forming apparatus having strontium titanate used as an external additive of a toner, wherein the image forming apparatus is an electrophotographic apparatus which maintains the durability of an electrophotographic photosensitive member and has excellent transferability even under low temperature / low humidity conditions. Summary of the invention
[0008] The above object is achieved by the present invention as follows. Specifically, the electronic photographic device according to the present invention is characterized by comprising:
[0009] An electrophotographic photosensitive member having a surface layer containing a resin X as a binder resin;
[0010] a charging unit that charges the surface of the electrophotographic photosensitive member;
[0011] an exposure unit that irradiates the charged surface of the electrophotographic photosensitive member with light to form an electrostatic latent image;
[0012] a developing unit that supplies toner to the electrostatic latent image to form a toner image; and
[0013] A transfer unit transfers the toner image to a transfer medium, wherein
[0014] The toner contains strontium titanate as an external additive, and
[0015] The resin X contains a structural unit represented by formula (1):
[0016]
[0017] Further features of the present invention will become apparent from the following description of exemplary embodiments with reference to the attached drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 is a diagram showing an example of a schematic configuration of an electrophotographic apparatus including a process cartridge having the electrophotographic photosensitive member according to the present invention. DETAILED DESCRIPTION
[0019] Preferred embodiments of the present invention will now be described in detail with reference to the accompanying drawings.
[0020] Hereinafter, the present invention will be described in detail with reference to preferred embodiments.
[0021] The image forming apparatus described in Japanese Patent Application Laid-Open No. 2021-131520, which includes an electrophotographic photosensitive member containing a polycarbonate resin and a toner having externally added strontium titanate, does not experience deterioration in transferability. However, in order to achieve enhanced durability, a combined image forming apparatus in which an electrophotographic photosensitive member containing a polycarbonate resin is converted into an electrophotographic photosensitive member containing a polyarylate resin experiences deterioration in transferability under low temperature / low humidity conditions. From this, the inventors speculate that the reason why the electrophotographic photosensitive member containing a polyarylate resin causes deterioration in transferability is as follows.
[0022] When the surface of the photosensitive member is charged, discharge is generated from the charging member to the photosensitive member. The energy of the discharge causes the material contained in the surface of the photosensitive member to discharge and degrade; specifically, the bonds in the binder resin in the surface of the photosensitive member may be broken. The polyarylate resin may undergo the generation of COOH groups through the ester bond part due to the breakage of the discharge. Especially under low temperature / low humidity conditions, the instability of the discharge leads to occasional strong discharge, and significant discharge degradation may occur. Therefore, through repeated use during long-term use, a large number of COOH groups tend to be generated in the surface of the photosensitive member. Strontium titanate has a perovskite-type crystal structure, and metallic titanium is easy to interact with functional groups and the like. In particular, COOH exhibits strong interaction through the coordination binding of non-shared electron pairs with metallic titanium orbitals. Therefore, through repeated use, it is expected that a strong adhesion will be generated between the toner with externally added strontium titanate and the photosensitive member containing the polyarylate resin, resulting in the occurrence of transferability degradation. Polycarbonate is less likely to undergo the generation of COOH groups and has a lower mechanical strength than polyarylate, so that the COOH groups are easily removed by rubbing on the surface of the photosensitive member. This is presumably the reason why the conventional combination of strontium titanate and polycarbonate does not cause transferability degradation, while the combination of strontium titanate and polyarylate causes transferability degradation.
[0023] Based on this assumption, methods involving the use of strontium titanate as an external additive of a toner to achieve enhanced durability in an electrophotographic photosensitive member without causing deterioration in transferability were studied in various ways, and the constitution of the present invention was arrived at.
[0024] The polyarylate resin has a structure in which a structure derived from a dicarboxylic acid containing an aromatic ring and a diol (bisphenol) containing an aromatic ring are combined. The inventors have found that if such a resin has an ether structure as a bond between aromatic rings, the resin is resistant to discharge degradation. In addition, as represented by the structure of formula (1), the resin X having an ether structure between aromatic rings in the structure derived from the dicarboxylic acid and also having an ether structure between aromatic rings in the structure derived from the bisphenol is particularly resistant to discharge degradation and is less likely to experience the generation of COOH groups. It is speculated that this prevents an increase in adhesion to a toner having externally added strontium titanate, and results in enhanced transferability even in durability under low temperature / low humidity conditions.
[0025] [Electrophotographic photosensitive member]
[0026] The electrophotographic photosensitive member of the present invention includes at least: a support; and a photosensitive layer formed on the support.
[0027] Examples of methods for producing the electrophotographic photosensitive member of the present invention include a method of preparing a coating solution for each layer described later, applying in the desired order of each layer, and drying. Examples of usable methods for applying the coating solution include dip coating, spray coating, inkjet coating, roll coating, die coating, blade coating, curtain coating, wire rod coating, and ring coating. Among them, dip coating is preferred from the viewpoint of efficiency and productivity.
[0028] Each layer will be described below.
[0029] <Support>
[0030] In the present invention, the electrophotographic photosensitive member includes a support. In the present invention, the support is preferably a conductive support having conductivity. Examples of the shape of the support include cylindrical, belt-shaped, and sheet-shaped. Among these shapes, the support preferably has a cylindrical shape. The surface of the support may be subjected to electrochemical treatment such as anodization, sandblasting, cutting treatment, and the like.
[0031] Preferably, the material of the support is, for example, metal, resin or glass.
[0032] Examples of the metal include aluminum, iron, nickel, copper, gold, stainless steel, and alloys thereof. Among these metals, the support is preferably an aluminum support using aluminum.
[0033] The resin or glass may be rendered conductive by treatment, such as by mixing with or coating with a conductive material.
[0034] <Conductive layer>
[0035] In the present invention, a conductive layer may be provided on the support. The provided conductive layer can mask unevenness and defects of the support and prevent interference fringes from being generated. The average thickness of the conductive layer is preferably 5 μm or more and 40 μm or less.
[0036] The conductive layer preferably contains conductive particles and a binder resin. Examples of conductive particles include carbon black, metal particles and metal oxide particles. Examples of metal oxides include zinc oxide, aluminum oxide, indium oxide, silicon oxide, zirconium oxide, tin oxide, titanium oxide, magnesium oxide, antimony oxide and bismuth oxide. Examples of metals include aluminum, nickel, iron, nickel-chromium alloy, copper, zinc and silver.
[0037] Among them, metal oxides are preferably used for the conductive particles; in particular, titanium oxide, tin oxide, or zinc oxide is more preferably used.
[0038] In the case where a metal oxide is used for the conductive particles, the surface of the metal oxide may be treated with a silane coupling agent or the like, and the metal oxide may be doped with an element such as phosphorus, aluminum, or an oxide thereof. Examples of the element and its oxide used for doping include phosphorus, aluminum, niobium, and tantalum.
[0039] The conductive particles may have a laminated structure including a core particle and a coating layer coating the core particle. Examples of the core particle include titanium oxide, barium sulfate, and zinc oxide. Examples of the coating layer include metal oxides such as tin oxide and titanium oxide.
[0040] When a metal oxide is used for the conductive particles, the volume average particle diameter thereof is preferably 1 nm or more and 500 nm or less.
[0041] Examples of the resin include polyester resins, polycarbonate resins, polyvinyl acetal resins, acrylic resins, silicone resins, epoxy resins, melamine resins, polyurethane resins, phenolic resins, and alkyd resins.
[0042] The conductive layer may also contain, for example, silicone oil, resin particles, or a masking agent such as titanium oxide.
[0043] The average thickness of the conductive layer is preferably 1 μm or more and 50 μm or less.
[0044] The conductive layer can be formed in such a manner that a conductive layer coating liquid containing the above-mentioned materials and a solvent is prepared, and a coating film is formed with the coating liquid, and dried. Examples of solvents used for the coating liquid include alcohol solvents, sulfoxide solvents, ketone solvents, ether solvents, ester solvents, and aromatic hydrocarbon solvents. Examples of a dispersion method for dispersing conductive particles in the conductive layer coating liquid include a method using a paint stirrer, a sand mill, a ball mill, or a liquid collision type high-speed disperser.
[0045] <Base Coating>
[0046] In the present invention, an undercoat layer may be provided on the support or the conductive layer. The provided undercoat layer can impart a high interlayer adhesion function and a function of suppressing charge injection.
[0047] The primer layer preferably contains a resin. The primer layer can be formed as a cured film by polymerizing a composition containing a monomer having a polymerizable functional group.
[0048] Examples of the resin include polyester resins, polycarbonate resins, polyvinyl acetal resins, acrylic resins, epoxy resins, melamine resins, polyurethane resins, phenolic resins, polyvinylphenolic resins, alkyd resins, polyvinyl alcohol resins, polyethylene oxide resins, polypropylene oxide resins, polyamide resins, polyamic acid resins, polyimide resins, polyamideimide resins, and cellulose resins.
[0049] Examples of the polymerizable functional group possessed by the monomer having a polymerizable functional group include an isocyanate group, a blocked isocyanate group, a methylol group, an alkylated methylol group, an epoxy group, a metal alkoxide group, a hydroxyl group, an amino group, a carboxyl group, a thiol group, a carboxylic acid anhydride group and a carbon-carbon double bond group.
[0050] The undercoat layer may further contain, for example, an electron transport material, a metal oxide, a metal or a conductive polymer to enhance the electrical characteristics. Among them, an electron transport material or a metal oxide is preferably used.
[0051] Examples of electron transport materials include quinone compounds, imide compounds, benzimidazole compounds, cyclopentadienyl compounds, fluorenone compounds, xanthone compounds, benzophenone compounds, cyanovinyl compounds, halogenated aryl compounds, silole compounds and fluorine-containing compounds. The undercoat layer can be formed as a cured film by copolymerizing an electron transport material having a polymerizable functional group and the above-mentioned monomer having a polymerizable functional group.
[0052] Examples of metal oxides include indium tin oxide, tin oxide, indium oxide, titanium oxide, zinc oxide, aluminum oxide, and silicon dioxide. Examples of metals include gold, silver, and aluminum.
[0053] The base coat may further contain additives.
[0054] The average thickness of the primer layer is preferably 0.1 μm or more and 50 μm or less, more preferably 0.2 μm or more and 40 μm or less, particularly preferably 0.3 μm or more and 30 μm or less.
[0055] The undercoat layer can be formed in such a manner that a coating liquid for the undercoat layer containing the above-mentioned materials and a solvent is prepared, and a coating film is formed with the coating liquid, and dried and / or cured. Examples of solvents for the coating liquid include alcohol solvents, ketone solvents, ether solvents, ester solvents, and aromatic hydrocarbon solvents.
[0056] <Photosensitive layer>
[0057] The photosensitive layer of the electrophotographic photosensitive member is mainly classified into (1) a laminated photosensitive layer and (2) a single-layer photosensitive layer. (1) The laminated photosensitive layer includes a charge generating layer containing a charge generating material and a charge transporting layer containing a charge transporting material. (2) The single-layer photosensitive layer includes a photosensitive layer containing both a charge generating material and a charge transporting material. The electrophotographic photosensitive member according to the present invention preferably includes a laminated photosensitive layer.
[0058] (1) Laminated photosensitive layer
[0059] The laminated photosensitive layer includes a charge generating layer and a charge transporting layer. In an embodiment of the present invention, the charge transporting layer is a surface layer.
[0060] (1-1) Charge Generation Layer
[0061] The charge generating layer preferably contains a charge generating material and a resin.
[0062] The charge generating material used for the charge generating layer is preferably a phthalocyanine pigment. Examples of phthalocyanine include oxytitanium phthalocyanine, hydroxygallium phthalocyanine, and chlorogallium phthalocyanine. Among phthalocyanines, oxytitanium phthalocyanine is more preferred.
[0063] Examples of binder resins for the charge generation layer include resins (insulating resins) including polyvinyl butyral resins, polyvinyl acetal resins, polyarylate resins, polycarbonate resins, polyester resins, polyvinyl acetate resins, polysulfone resins, polystyrene resins, phenoxy resins, acrylic resins, phenoxy resins, polyacrylamide resins, polyvinyl pyridine resins, polyurethane resins, agarose resins, cellulose resins, casein resins, polyvinyl alcohol resins, polyvinyl pyrrolidone resins, vinylidene chloride resins, acrylonitrile copolymers, and polyvinyl alcohol benzaldehyde resins. In addition, organic photoconductive polymers such as poly-N-vinyl carbazole, polyvinyl anthracene, and polyvinyl pyrene can be used. Only one binder resin can be used; alternatively, two or more binder resins can be used in combination as a mixture or a copolymer.
[0064] Examples of the solvent for the charge generating layer coating solution include toluene, xylene, tetralin, chlorobenzene, methylene chloride, chloroform, trichloroethylene, tetrachloroethylene, carbon tetrachloride, methyl acetate, ethyl acetate, propyl acetate, methyl formate, ethyl formate, acetone, methyl ethyl ketone, cyclohexanone, diethyl ether, dipropyl ether, propylene glycol monomethyl ether, dioxane, methylal, tetrahydrofuran, water, methanol, ethanol, n-propanol, isopropanol, butanol, methyl cellosolve, methoxypropanol, dimethylformamide, dimethylacetamide, and dimethyl sulfoxide. One or more of the solvents may be used alone or as a mixture.
[0065] The charge generating layer can be provided by dispersing a phthalocyanine pigment as a charge generating material and an optional binder resin in a solvent to prepare a charge generating layer coating liquid, and forming a coating film with the charge generating layer coating liquid, and drying.
[0066] The charge generating layer coating liquid can be prepared by dispersing only the charge generating material in a solvent and then adding the binder resin or by dispersing the charge generating material and the binder resin simultaneously in a solvent.
[0067] In the dispersion, a disperser including a media type disperser such as a sand mill and a ball mill, a liquid collision type disperser, and an ultrasonic disperser can be used.
[0068] (1-2) Charge transport layer
[0069] In the case where the surface layer of the present invention is a charge transport layer, the charge transport layer contains a binder resin. Preferably, the charge transport layer further contains a charge transport material.
[0070] [Binder resin]
[0071] The binder resin used in the charge transport layer comprises a resin X containing a structural unit represented by formula (1):
[0072]
[0073] Preferably, the resin X further contains a structural unit represented by formula (2):
[0074]
[0075] Where R 1 and R 2 Each represents a methyl group, R 3 and R 4 Combined with each other to represent a cycloalkylidene group having 5 or 6 carbon atoms; or R 1 and R 2 Each independently represents a hydrogen atom or a methyl group, R 3 Represents methyl, R 4 represents a hydrogen atom or an alkyl group having 2 or 3 carbon atoms.
[0076] The structural unit comprising formula (1) and formula (2) makes the charge transport layer have enhanced wear resistance and can better suppress discharge degradation. The reasons for the enhanced wear resistance and better suppression of discharge degradation are speculated as follows. Formula (2) includes a structure derived from a dicarboxylic acid and a structure derived from bisphenol. In addition, the structure derived from the dicarboxylic acid includes an ether structure that gives wear resistance and resistance to discharge degradation, and the structure derived from bisphenol gives a bulky skeleton on one side.
[0077] Including R 1 and R 2 The presence of molecules which are asymmetric in position and size with respect to the main chain tends to prevent the binder resin and the charge transport material in the charge transport layer from being localized.
[0078] As a result of preventing localization of the binder resin and the charge transport material in the charge transport layer, uniform distribution is achieved, the effect of suppressing discharge degradation of the structural units of formula (1) and formula (2) is fully exerted, and enhanced wear resistance and better suppression of discharge degradation are achieved.
[0079] In the charge transport layer, the value of n2 / n1 is preferably 1.0 or more, wherein the value is the ratio of the number n2 of the structural unit represented by formula (2) contained in the resin X to the number n1 of the structural unit represented by formula (1) contained in the resin X. If the value is 10.0 or more, it is less likely to obtain the effects of wear resistance and suppression of discharge degradation. More preferably, n2 / n1 is 1.0 or more and 3.0 or less.
[0080] Preferred examples of formula (2) include formula (2-1), formula (2-2), formula (2-3), formula (2-4) and formula (2-5):
[0081]
[0082] Among them, the resin X more preferably contains the formula (2-5).
[0083] The viscosity average molecular weight of the resin X is preferably 10,000 or more, more preferably 40,000 or more. The viscosity average molecular weight of the resin X of 10,000 or more allows the photosensitive member to have enhanced wear resistance. On the other hand, the viscosity average molecular weight of the resin X is preferably 80,000 or less, more preferably 70,000 or less. The viscosity average molecular weight of the resin X of 80,000 or less allows the resin X to be easily dissolved in a solvent used to form a photosensitive layer.
[0084] More preferably, the resin X further contains a structural unit represented by the formula (PE1-1) and a structural unit represented by (PE2-1):
[0085]
[0086] The charge transport layer may also contain a resin other than the resin X as a binder resin, wherein the resin A contains a structural unit represented by the formula (1) and a structural unit represented by the formula (2). Examples of other resins include another type of polyarylate resin, polyester resin, polycarbonate resin, styrene resin and acrylic resin. The polyarylate resin may be, for example, a random copolymer, an alternating copolymer, a periodic copolymer or a block copolymer.
[0087] Examples of structural units of another type of polyarylate resin include the following:
[0088]
[0089]
[0090] The resin X used as a binder resin for the surface layer of the electrophotographic photosensitive member of the present invention and containing the structural unit represented by formula (1) may contain another structural unit as long as the resin X contains the structural unit represented by formula (1), and the resin X may be a copolymer having a structural unit including a group derived from another type of divalent carboxylic acid different from formula (1) and a divalent organic residue.
[0091] The content of the resin X containing the structural unit represented by the formula (1) and the structural unit represented by the formula (2) in the binder resin in the charge transport layer is preferably 50% by mass or more and 100% by mass or less.
[0092] The production of the resin X is not limited to a specific method. One example is a method of polycondensing bisphenol for constituting a bisphenol-derived structure and dicarboxylic acid for constituting a dicarboxylic acid-derived structure. Known synthesis methods including polycondensation can be used.
[0093] Derivatives of bisphenol and dicarboxylic acid can be used. Aromatic diacetates can be used as derivatives of bisphenol. Examples of derivatives of dicarboxylic acid include dicarboxylic acid dichlorides, dimethyl dicarboxylate, diethyl dicarboxylate, and dicarboxylic acid anhydrides.
[0094] When producing resin X, the ratio n2 / n1 can be adjusted by varying the type and amount of bisphenol and dicarboxylic acid.
[0095] The ratio n2 / n1 can be calculated by analysis of NMR analysis and pyrolysis GS-MS analysis.
[0096] [Charge transport material]
[0097] Any compound represented by the following formula (20), formula (21), formula (22), formula (23), formula (24) and formula (25) is preferably used for the charge transport material:
[0098]
[0099]
[0100]
[0101] In formula (20), R 11 , R 12 , R 13 and R 14 Each independently represents an alkyl group having 1 or more and 6 or less carbon atoms or an alkoxy group having 1 or more and 6 or less carbon atoms. a1, a2, a3, and a4 each independently represent an integer of 0 or more and 5 or less. In formula (20), when a1 represents an integer of 2 or more and 5 or less, a plurality of R 11 The groups may represent the same group or different groups. When a2 represents an integer of 2 or more and 5 or less, a plurality of R 12 The groups may represent the same group or different groups. When a3 represents an integer of 2 or more and 5 or less, a plurality of R 13 The groups may represent the same group or different groups. When a4 represents an integer of 2 or more and 5 or less, a plurality of R 14 The groups may represent the same group or different groups. 11 , R 12 , R 13 and R 14Preferably, each independently represents an alkyl group having 1 to 3 carbon atoms, and more preferably each independently represents a methyl group or an ethyl group. a1, a2, a3, and a4 preferably each independently represent an integer of 1 to 3, and more preferably each independently represent 1.
[0102] In formula (21), R 21 , R 22 and R 23 Each independently represents an alkyl group having 1 or more and 6 or less carbon atoms. 24 , R 25 and R 26 Each independently represents a hydrogen atom or an alkyl group having 1 or more and 6 or less carbon atoms. b1, b2 and b3 each independently represent 0 or 1. In formula (21), R 21 , R 22 and R 23 Preferably, each independently represents an alkyl group having 1 or more and 3 or less carbon atoms, and more preferably each independently represents a methyl group. 21 , R 22 and R 23 It is preferably bonded to the meta position of the corresponding phenyl group relative to the vinyl or butadienyl group. 24 , R 25 and R 26 Preferably, each of b1, b2 and b3 represents 0 or 1.
[0103] In formula (22), R 31 , R 32 and R 33 Each independently represents an alkyl group having 1 or more and 6 or less carbon atoms. 34 represents an alkyl group having 1 or more and 6 or less carbon atoms or a hydrogen atom. d1, d2 and d3 each independently represent an integer of 0 or more and 5 or less. In formula (22), when d1 represents an integer of 2 or more and 5 or less, a plurality of R 31 The groups may represent the same group or different groups. When d2 represents an integer of 2 or more and 5 or less, a plurality of R 32 The groups may represent the same group or different groups. When d3 represents an integer of 2 or more and 5 or less, a plurality of R 33 The groups may represent the same group or different groups. 34 Preferably, d1, d2 and d3 each represent 0.
[0104] In formula (23), R 41 , R 42 , R 43 , R 44 , R 45and R 46 Each independently represents an alkyl group or a phenyl group having 1 to 6 carbon atoms. 47 and R 48 Each independently represents a hydrogen atom, an alkyl group having 1 to 6 carbon atoms, or a phenyl group. e1, e2, e3, and e4 each independently represent an integer of 0 to 5. e5 and e6 each independently represent an integer of 0 to 4. e7 and e8 each independently represent 0 or 1. In formula (23), when e1 represents an integer of 2 to 5, multiple R 41 The groups may represent the same group or different groups. When e2 represents an integer of 2 or more and 5 or less, a plurality of R 42 The groups may represent the same group or different groups. When e3 represents an integer of 2 or more and 5 or less, a plurality of R 43 The groups may represent the same group or different groups. When e4 represents an integer of 2 or more and 5 or less, a plurality of R 44 The groups may represent the same group or different groups. When e5 represents an integer of 2 or more and 4 or less, a plurality of R 45 The groups may represent the same group or different groups. When e6 represents an integer of 2 or more and 4 or less, a plurality of R 46 The groups may represent the same group or different groups. 41 To R 46 Preferably, each independently represents an alkyl group having 1 or more and 6 or less carbon atoms, more preferably each independently represents an alkyl group having 1 or more and 3 or less carbon atoms, and even more preferably each independently represents a methyl group or an ethyl group. 47 and R 48 Preferably, each of e1, e2, e3 and e4 independently represents an integer of 0 or more and 2 or less, and more preferably, e1 and e2 each represent 0, and e3 and e4 each represent 2. Preferably, e5 and e6 each represent 0. Preferably, e7 and e8 each represent 0 or 1.
[0105] In formula (24), R 50 and R 51 Each independently represents an alkyl group having 1 to 6 carbon atoms, an alkoxy group having 1 to 6 carbon atoms, or a phenyl group. 52 , R 53 , R 54 , R 55 , R 56 , R 57 and R 58Each independently represents a hydrogen atom, an alkyl group having 1 to 6 carbon atoms, an alkoxy group having 1 to 6 carbon atoms, or a phenyl group optionally substituted by an alkyl group having 1 to 6 carbon atoms. f1 and f2 each independently represent an integer of 0 to 2. f3 and f4 each independently represent an integer of 0 to 5. In formula (24), when f3 represents an integer of 2 to 5, multiple R 50 The groups may represent the same group or different groups. When f4 represents an integer of 2 or more and 5 or less, a plurality of R 51 The groups may represent the same group or different groups. 50 and R 51 Preferably, each independently represents an alkyl group having 1 or more and 6 or less carbon atoms. 52 and R 53 Preferably, each represents a hydrogen atom or a phenyl group optionally substituted by an alkyl group having 1 to 6 carbon atoms. 54 To R 58 Preferably, each independently represents a hydrogen atom, an alkyl group having 1 to 6 carbon atoms, or an alkoxy group having 1 to 6 carbon atoms. Preferably, f1 and f2 each represent 0, or each represent 1, or each represent 2. Preferably, f3 and f4 each independently represent 0 or 1. 50 and R 51 The alkyl group having 1 or more and 6 or less carbon atoms represented by is preferably an alkyl group having 1 or more and 3 or less carbon atoms, and more preferably a methyl group. 52 and R 53 The phenyl group optionally substituted by an alkyl group having 1 to 6 carbon atoms represented by is preferably a phenyl group or a phenyl group substituted by an alkyl group having 1 to 3 carbon atoms at 1 to 5 positions. The phenyl group substituted by an alkyl group having 1 to 3 carbon atoms is preferably a methylphenyl group, more preferably a 4-methylphenyl group. 54 To R 58 The alkyl group having 1 or more and 6 or less carbon atoms represented by is preferably an alkyl group having 1 or more and 4 or less carbon atoms, and is preferably a methyl group, an ethyl group or an n-butyl group. 54 To R 58 The alkoxy group having 1 to 6 carbon atoms represented by is preferably an alkoxy group having 1 to 3 carbon atoms, and more preferably an ethoxy group.
[0106] In formula (25), R 61 , R 62 , R 63 , R 64 , R 65 and R 66Each independently represents an alkyl group having 1 or more and 8 or less carbon atoms, a phenyl group or an alkoxy group having 1 or more and 8 or less carbon atoms, h1, h2, h4 and h5 each independently represent an integer of 0 or more and 5 or less, and h3 and h6 each independently represent an integer of 0 or more and 4 or less.
[0107] Preferred examples of the charge transport compound (20) include compounds represented by formula (H-11). Preferred examples of the charge transport compound (21) include compounds represented by formulas (H-7) and (H-8). Preferred examples of the charge transport compound (22) include compounds represented by formula (H-6). Preferred examples of the charge transport compound (23) include compounds represented by formulas (H-9) and (H-10). Preferred examples of the charge transport compound (24) include compounds represented by formulas (H-1), (H-2), (H-3) and (H-5). Preferred examples of the charge transport compound (25) include compounds represented by formula (H-4). In the following, compounds represented by formulas (H-1) to (H-11) are sometimes referred to as charge transport compounds (H-1) to (H-11).
[0108]
[0109]
[0110]
[0111]
[0112] The content of the charge transport material is preferably 10 parts by mass or more and 200 parts by mass or less, more preferably 30 parts by mass or more and 120 parts by mass or less, and even more preferably 50 parts by mass or more and 100 parts by mass or less, based on 100 parts by mass of the binder resin. The photosensitive layer may contain only one charge transport compound, or may contain two or more charge transport compounds. The photosensitive layer may also contain a charge transport compound other than the charge transport compounds (20), (21), (22), (23), (24) and (25) (hereinafter, sometimes referred to as other electron transport compounds or electron transport materials). Examples of other charge transport compounds include triphenylamine derivatives, diamine derivatives (e.g., N,N,N',N'-tetraphenylbenzidine derivatives, N,N,N',N'-tetraphenylphenylenediamine derivatives, N,N,N',N'-tetraphenylnaphthylenediamine derivatives, N,N,N',N'-tetraphenylphenanthrylenediamine derivatives and di(aminophenylvinyl)benzene derivatives), oxadiazole compounds (e.g., 2,5-bis(4-methylaminophenyl)-1,3,4-oxadiazole), styryl compounds (e.g., 9-(4-diethylaminostyryl)anthracene), carbazole compounds (e.g., polyvinylcarbazole), organic polysilane compounds, pyrazoline compounds (e.g., 1-phenyl-3-(p-dimethylaminophenyl)pyrazoline), hydrazone compounds, indole compounds, oxazole compounds, isoxazole compounds, thiazole compounds, thiadiazole compounds, imidazole compounds, pyrazole compounds and triazole compounds.
[0113] The charge transport layer may contain additives such as antioxidants, ultraviolet absorbers, plasticizers, leveling agents, lubricants and wear resistance enhancers. Specific examples include hindered phenol compounds, hindered amine compounds, sulfur compounds, phosphorus compounds, benzophenone compounds, siloxane modified resins, silicone oils, fluorine resin particles, polystyrene resin particles, polyethylene resin particles, silica particles, aluminum oxide particles and boron nitride particles.
[0114] The average thickness of the charge transport layer is preferably 5 μm or more and 50 μm or less, and more preferably 8 μm or more and 40 μm or less.
[0115] The charge transport layer can be formed in such a manner that a charge transport layer coating liquid containing the above-mentioned materials and a solvent is prepared, and a coating film is formed with the coating liquid, and dried. Examples of solvents for the coating liquid include alcohol solvents, ketone solvents, ether solvents, ester solvents, and aromatic hydrocarbon solvents. Among these solvents, ether solvents or aromatic hydrocarbon solvents are preferred.
[0116] (2) Single-layer photosensitive layer
[0117] The single-layer photosensitive layer can be formed in such a manner that a photosensitive layer coating liquid containing a charge generating material, a charge transporting material, a resin and a solvent is prepared, and a coating film is formed with the coating liquid, and dried. Examples of the charge generating material, the charge transporting material and the resin are the same as the examples of the materials shown in the above "(1) Laminated photosensitive layer".
[0118] [Toner]
[0119] The toner according to the present invention contains: toner particles containing a binder resin; and an external additive, and the toner contains strontium titanate as such an external additive. Strontium titanate can adjust the chargeability and fluidity of the toner. The content of strontium titanate is 0.05 to 5.0 parts by mass based on 100.0 parts by mass of the toner particles. The content is preferably 0.1 to 1.0% by mass.
[0120] <Binder Resin>
[0121] The binder resin contained in the toner particles according to the present invention is not limited to a specific binder resin, and a known binder resin can be used; however, vinyl resins, polyester resins, etc. are preferred. Examples of the vinyl resins, polyester resins, and other binder resins include the following resins or polymers.
[0122] Homopolymers of styrene and substituted forms thereof, such as polystyrene and polyvinyltoluene; styrene copolymers, such as styrene-propylene copolymers, styrene-vinyltoluene copolymers, styrene-vinylnaphthalene copolymers, styrene-methyl acrylate copolymers, styrene-ethyl acrylate copolymers, styrene-butyl acrylate copolymers, styrene-octyl acrylate copolymers, styrene-dimethylaminoethyl acrylate copolymers, styrene-methyl methacrylate copolymers, styrene-ethyl methacrylate copolymers, styrene-butyl methacrylate copolymers, styrene-dimethylaminoethyl methacrylate copolymers, styrene-vinyl methyl ether copolymers, styrene-vinyl ethyl ether copolymers, styrene-vinyl methyl ketone copolymers, styrene-butadiene copolymers, styrene-isoprene copolymers, styrene-maleic acid copolymers and styrene-maleic acid ester copolymers; polymethyl methacrylate, polybutyl methacrylate, polyvinyl acetate, polyethylene, polypropylene, polyvinyl butyral, silicone resins, polyamide resins, epoxy resins, polyacrylic resins, rosin, modified rosin, terpene resins, phenolic resins, aliphatic or alicyclic hydrocarbon resins and aromatic petroleum resins. These binder resins may be used alone or as a mixture. The binder resin is preferably a styrene-based copolymer.
[0123] The binder resin preferably contains a carboxyl group, and the binder resin is preferably a resin produced using a polymerizable monomer containing a carboxyl group.
[0124] Examples of polymerizable monomers containing a carboxyl group include acrylic acid, methacrylic acid; α-alkyl derivatives or β-alkyl derivatives of acrylic acid or methacrylic acid, such as α-ethylacrylic acid and crotonic acid; unsaturated dicarboxylic acids, such as fumaric acid, maleic acid, citraconic acid and itaconic acid; unsaturated dicarboxylic acid monoester derivatives, such as monoacryloxyethyl succinate, monoacryloxyethylene succinate, monoacryloxyethyl phthalate and monomethacryloxyethyl phthalate.
[0125] A polycondensation product of a carboxylic acid component and an alcohol component as shown below can be used as the polyester resin.
[0126] Examples of the carboxylic acid component include terephthalic acid, isophthalic acid, phthalic acid, fumaric acid, maleic acid, cyclohexanedicarboxylic acid and trimellitic acid. Examples of the alcohol component include bisphenol A, hydrogenated bisphenol, ethylene oxide adduct of bisphenol A, propylene oxide adduct of bisphenol A, glycerol, trimethylolpropane and pentaerythritol.
[0127] The polyester resin may be a resin containing a urea group. The carboxyl groups in the polyester resin, such as the carboxyl groups at the terminals, are preferably not capped.
[0128] <Wax>
[0129] The toner according to the present invention may contain wax. The wax preferably used is as described above. The content of the wax is preferably 5.0 parts by mass or more and 20.0 parts by mass or less based on 100.0 parts by mass of the binder resin or the polymerizable monomer used to produce the binder resin.
[0130] <Colorant>
[0131] Known colorants can be used without any particular limitation.
[0132] Examples of usable yellow pigments include yellow iron oxide, Napels Yellow, naphthol yellow S, condensed azo compounds such as Hansa Yellow G, Hansa Yellow 10G, benzidine yellow G, benzidine yellow GR, quinoline yellow lake, permanent yellow NCG and lemon yellow lake, isoindolinone compounds, anthraquinone compounds, azo metal complexes, methine compounds and allylamide compounds. Specific examples include the following.
[0133] CI Pigment Yellow 12, 13, 14, 15, 17, 62, 74, 83, 93, 94, 95, 109, 110, 111, 128, 129, 147, 155, 168, 180, 185, 193.
[0134] Examples of red pigments include red ochre, condensed azo compounds such as Permanent Red 4R, Litho Red, Pyrazolone Red, Watchung Red calcium salt, Watchung Red C, Watchung Red D, Brilliant Carmine 6B, Brilliant Carmine 3B, Eoxin Lake, Rhodamine Lake B and Alizarin Red Lake, diketopyrrolopyrrole compounds, anthraquinone compounds, quinacridone compounds, basic lake dye compounds, naphthol compounds, benzimidazolone compounds, thioindigo compounds and perylene compounds. Specific examples include the following. CI Pigment Red 2, 3, 5, 6, 7, 23, 48:2, 48:3, 48:4, 57:1, 81:1, 122, 144, 146, 150, 166, 169, 177, 184, 185, 202, 206, 220, 221, 254.
[0135] Examples of blue pigments include copper phthalocyanine compounds and derivatives thereof such as basic blue lake, Victoria blue lake, phthalocyanine blue, metal-free phthalocyanine blue, phthalocyanine blue partial chloride, First Sky Blue and Indanthrene Blue BG, anthraquinone compounds and basic lake dye compounds. Specific examples include the following. CI Pigment Blue 1, 7, 15, 15:1, 15:2, 15:3, 15:4, 60, 62, 66.
[0136] Examples of black pigments include carbon black, aniline black, non-magnetic ferrite, magnetite, and pigments obtained by toning the above-mentioned yellow colorant, red colorant, and blue colorant to black. These colorants may be used alone, as a mixture, or even in the state of a solid solution.
[0137] If necessary, the colorant may be surface treated with a substance that does not cause polymerization inhibition.The content of the colorant is preferably 3.0 parts by mass or more and 15.0 parts by mass or less based on 100.0 parts by mass of the binder resin or the polymerizable monomer used to produce the binder resin.
[0138] <Charge Control Agent>
[0139] The toner according to the present invention may contain a charge control agent. Known charge control agents can be used. In particular, a charge control agent having a high charging speed and capable of stably maintaining a constant charge amount is preferred. In addition, in the case of producing toner particles by a direct polymerization method, a charge control agent having a low polymerization inhibition activity and having substantially no dissolved product in an aqueous medium is preferred.
[0140] Examples of the charge control agent that controls toner particles to have negative charges include the following.
[0141] Organometallic compounds and chelate compounds, including monoazo metal compounds and acetylacetonate metal compounds, and metal compounds of hydroxycarboxylic acids and dicarboxylic acids such as aromatic oxycarboxylic acids and aromatic dicarboxylic acids. Other examples include aromatic oxycarboxylic acids and aromatic monocarboxylic acids / aromatic polycarboxylic acids and their metal salts, their anhydrides or their esters, and phenol derivatives such as bisphenol. Other examples include urea derivatives, metal-containing salicylic acid compounds, metal-containing naphthoic acid compounds, boron compounds, quaternary ammonium salts, and calixarene.
[0142] These charge control agents may be contained alone; alternatively, two or more charge control agents may be contained in combination. The added amount of the charge control agent is preferably 0.01 parts by mass or more and 10.0 parts by mass or less relative to 100.0 parts by mass of the binder resin.
[0143] <Toner External Additives>
[0144] The toner according to the present invention may contain an external additive other than strontium titanate in order to enhance fluidity, chargeability, and adhesion.
[0145] Examples of external additives include inorganic fine particles, such as silica fine particles, alumina fine particles, and titanium oxide fine particles. One of these external additives can be used alone; alternatively, two or more external additives can be used in combination. Such inorganic fine particles are preferably surface treated with a silane coupling agent, a titanium coupling agent, a higher fatty acid or silicone oil to enhance storage properties at high temperatures and enhance environmental stability.
[0146] The total content of these various external additives is preferably 0.05 to 5.0 parts by mass based on 100.0 parts by mass of the toner particles. The content of strontium titanate is preferably 0.1 to 1.0 part by mass based on 100.0 parts by mass of the toner particles.
[0147] Known production methods can be used for toner particles, and kneading pulverization and wet production methods can be used. For uniform particle size and shape controllability, wet production methods are preferred. Wet production methods include suspension polymerization, dissolution / suspension, emulsion polymerization / aggregation, and emulsion aggregation, and emulsion aggregation is more preferred. That is, the toner particles are preferably emulsion-aggregated toner particles.
[0148] In the emulsion aggregation method, a dispersion of a material including fine particles of a binder resin and a colorant is first prepared. The dispersion of the obtained material is dispersed and mixed with the addition of a dispersion stabilizer as necessary. Then, the resultant is aggregated to a desired toner particle size with the addition of a flocculant, and after or while the aggregation, the resin fine particles are fused together. Furthermore, shape control by heating is performed as necessary to form toner particles.
[0149] The following dispersion stabilizers can be used.
[0150] Surfactants such as known cationic surfactants, anionic surfactants and nonionic surfactants can be used.
[0151] Examples of the inorganic dispersion stabilizer include tricalcium phosphate, magnesium phosphate, zinc phosphate, aluminum phosphate, calcium carbonate, magnesium carbonate, calcium hydroxide, magnesium hydroxide, aluminum hydroxide, calcium metasilicate, calcium sulfate, barium sulfate, bentonite, silicon dioxide, and aluminum oxide.
[0152] Examples of the organic dispersion stabilizer include polyvinyl alcohol, gelatin, methyl cellulose, methyl hydroxypropyl cellulose, ethyl cellulose, sodium salt of carboxymethyl cellulose, and starch.
[0153] As a flocculant, not only a surfactant having the opposite polarity to the surfactant used as a dispersion stabilizer as described above can be preferably used, but also an inorganic salt and a divalent or higher valent inorganic metal salt can be preferably used. In particular, an inorganic metal salt is preferred because the inorganic metal salt makes it easy to control the aggregation and the toner chargeability by ionizing the multivalent metal element in the aqueous medium. Specific examples of preferred inorganic metal salts include metal salts such as calcium chloride, calcium nitrate, barium chloride, magnesium chloride, zinc chloride, ferric chloride, aluminum chloride and aluminum sulfate, and polymers of inorganic metal salts such as polyferric chloride, polysilicon iron, polyaluminum chloride, polyaluminum hydroxide and calcium polysulfide. Among them, aluminum salts and polymers thereof and polysilicon iron are particularly preferred. Generally, in order to obtain a sharper particle size distribution, for inorganic metal salts, divalent is more preferred relative to monovalent, trivalent or higher is more preferred relative to divalent, and for the same valence, inorganic metal salt polymers are more suitable than inorganic metal salts.
[0154] As the external adding device, for example, a double cone mixer, a V-shaped mixer, a drum mixer, a super mixer, an FM mixer (manufactured by NIPPON COKE & ENGINEERING CO., LTD.), a Nauta mixer, or a MECHANOHYBRID can be used. In the preparation of the toner, the rotation frequency of the external adding device, the processing time, and / or the water temperature in the jacket can be adjusted to control the coverage state of the external additive.
[0155] For high-definition and high-resolution images, the weight average particle diameter of the toner particles is preferably 3.0 μm or more and 10.0 μm or less.
[0156] <Processing cartridge and electrophotographic apparatus>
[0157] Figure 1 An example of a schematic configuration of an electrophotographic apparatus having a process cartridge including an electrophotographic photosensitive member is shown. Figure 11 , reference numeral 1 denotes a cylindrical (drum-shaped) electrophotographic photosensitive member, which is rotationally driven about an axis 2 in the direction of an arrow at a predetermined peripheral speed (process speed).
[0158] During the rotation, the surface of the electrophotographic photosensitive member 1 is charged to a predetermined positive or negative potential by the charging unit 3. Subsequently, the charged surface of the electrophotographic photosensitive member 1 is irradiated with exposure light 4 from an exposure unit (not shown), and an electrostatic latent image corresponding to target image information is formed. The image exposure light 4 is light output from an exposure unit such as slit exposure and laser beam scanning exposure, and has been intensity modulated according to a time series electrical digital image signal of the target image information.
[0159] The toner contained in the developing unit 5 is supplied to the electrostatic latent image formed on the surface of the electrophotographic photosensitive member 1 and the electrostatic latent image is developed (normal development or reverse development), so that a toner image is formed on the surface of the electrophotographic photosensitive member 1. The toner image formed on the surface of the electrophotographic photosensitive member 1 is then transferred to the transfer medium 7 by the transfer unit 6. At this time, a bias having a polarity opposite to the charge of the toner is applied to the transfer unit 6 from a bias power supply (not shown). In the case where the transfer medium 7 is a paper, the transfer medium 7 is taken out from a paper supply portion (not shown) and sent between the electrophotographic photosensitive member 1 and the transfer unit 6 in synchronization with the rotation of the electrophotographic photosensitive member 1.
[0160] The transfer medium 7 to which the toner image has been transferred from the electrophotographic photosensitive member 1 is separated from the surface of the electrophotographic photosensitive member 1, then conveyed to the fixing unit 8, and the fixing process of the toner image is performed, and the image is printed out of the electrophotographic device as an image formation (print, copy). The surface of the electrophotographic photosensitive member 1 after the toner image is transferred to the transfer medium 7 is cleaned by removing attachments such as toner (residual toner) by the cleaning unit 9. The recently developed cleaner-free system allows the residual toner to be directly removed in the developer or another unit. The surface of the electrophotographic photosensitive member 1 is electrically neutralized with the front exposure light 10 further from the front exposure unit (not shown), and then used again for image formation. In the case where the charging unit 3 is a contact charging unit using a charging roller or the like, the front exposure unit is not necessarily required. In the present invention, a plurality of constituent elements among the aforementioned constituent elements including the electrophotographic photosensitive member 1, the charging unit 3, the developing unit 5 and the cleaning unit 9 are accommodated in a container and integrally supported to form a process cartridge. The processing box can be installed in a detachable manner to the main body of the electronic photographic device. For example, at least one selected from the charging unit 3, the developing unit 5 and the cleaning unit 9 is integrally supported together with the electronic photographic photosensitive member 1 to form a processing box. With a guide unit 12 such as a guide rail of the main body of the electronic photographic device, a processing box 11 that can be installed to the main body of the electronic photographic device or detachable from the main body of the electronic photographic device is obtained. In the case where the electronic photographic device is a copier or a printer, the exposure light 4 can be reflected light or transmitted light from the original image. Alternatively, the exposure light 4 can be light radiated by scanning with a laser beam, driving an LED array, or driving a liquid crystal shutter array according to a signal, and the signal is given by reading the original image with a sensor and signalizing it.
[0161] The electrophotographic photosensitive member 1 can also be widely used in electrophotographic application fields such as laser beam printers, CRT printers, LED printers, facsimiles, liquid crystal printers, and laser plate making.
[0162] [Example]
[0163] Hereinafter, the present invention will be described in more detail by examples and comparative examples. The present invention is not limited to the following examples in any way unless any deviation from the scope is caused. In the description of the following examples, "parts" are based on mass, unless otherwise indicated.
[0164] [Resin X]
[0165] (Resin X(P1))
[0166] As a synthesis example, a method for synthesizing a resin X represented by (P1) shown below will be described below.
[0167] A dicarboxylic acid chloride having a structure represented by the following formula (DC-1) is dissolved in dichloromethane to prepare an acidic chloride solution.
[0168] Separately from the acidic chloride solution, bisphenols having structures represented by the following formula (BP-1) and the following formula (BP-2) were mixed in a molar ratio of 27:23 and dissolved in a 10% sodium hydroxide aqueous solution, tributylbenzylammonium chloride was added thereto as a polymerization catalyst, and the resultant was stirred to prepare a bisphenol solution.
[0169] Subsequently, the acid chloride solution was added to the bisphenol solution under stirring to initiate polymerization. The polymerization was carried out for 3 hours under stirring while maintaining the reaction temperature at 25° C. or less.
[0170] Then, acetic acid was added to terminate the polymerization reaction, and washing with water was repeated until the water layer became neutral.
[0171] After washing, methanol was added dropwise to the resultant under stirring to precipitate a polymerization product, which was vacuum dried to obtain a resin X represented by (P1). The viscosity average molecular weight of the obtained (P1) was found to be 46,000. The subscripts in the formula (for example, the two numerical values 54.0 and 46.0 in formula P1) represent the molar ratio (copolymerization ratio) between the corresponding units. .
[0172]
[0173] (Resin X (P2) to (P15), (P26))
[0174] Resins X (P2) to (P15) and (P26) were produced in the same manner as resin X (P1) except that the bisphenol used was changed and the ratio was adjusted as shown in Table 1. Table 1 also shows the viscosity average molecular weight of each resin X.
[0175] [Table 1]
[0176] Polyarylate resin The structural unit of formula (1) The structural unit of formula (2) n2 / n1 Viscosity average molecular weight P1 (1) (2-0) - 46000 P2 (1) (2-0) - 46600 P3 (1) (2-1) 0.85 44000 P4 (1) (2-1) 1.00 45300 P5 (1) (2-2) 1.00 48100 P6 (1) (2-3) 1.00 45200 P7 (1) (2-4) 1.00 49200 P8 (1) (2-5) 1.00 45800 P9 (1) (2-5) 0.85 41300 P10 (1) (2-1) 3.00 43500 P11 (1) (2-2) 3.00 42600 P12 (1) (2-3) 3.00 43300 P13 (1) (2-4) 3.00 45900 P14 (1) (2-5) 3.00 43200 P15 (1) (2-1) 4.00 42500 P26 (1) (2-5) 4.00 42900
[0177] The structures of resins X (P2) to (P15) and (P26) are shown below.
[0178]
[0179]
[0180]
[0181] <Production of Electrophotographic Photosensitive Member>
[0182] The thickness of each layer of the electrophotographic photosensitive member except the charge generating layer is determined by a method using an eddy current thickness meter (Fischerscope, manufactured by FISCHER INSTRUMENTS KK) or a method of converting the mass per unit area into specific gravity. The thickness of the charge generating layer is measured in such a manner that a spectroscopic densitometer (product name: X-Rite504 / 508, manufactured by X-Rite, Inc.) is pressed against the surface of the photosensitive member to measure the Macbeth density value of the photosensitive member, and the Macbeth density value is converted using a calibration curve obtained in advance from the thickness measurement obtained by cross-sectional SEM image observation.
[0183] [Photosensitive member 1]
[0184] <Conductive layer>
[0185] An aluminum cylinder (JIS-A3003, aluminum alloy) having a diameter of 24 mm and a length of 257.5 mm was used as a support (conductive support).
[0186] Then, prepare the following materials.
[0187] - Titanium oxide (TiO2) particles covered with oxygen-deficient tin oxide (SnO2) as metal oxide particles (average primary particle size: 230 nm): 214 parts
[0188] - Phenolic resin (monomer / oligomer of phenolic resin) as a binder material (product name: Plyophen J-325, manufactured by DIC Corporation, resin solid content: 60 mass %): 132 parts - 1-methoxy-2-propanol as a solvent: 98 parts
[0189] These and 450 parts of glass beads with a diameter of 0.8 mm are placed in a sand mill and dispersed under the conditions of a rotation frequency of 2000 rpm, a dispersion time of 4.5 hours, and a preset temperature of cooling water of 18°C to obtain a dispersion. The glass beads of the dispersion are removed by a sieve (sieve size: 150 μm). Silicone resin particles (product name: TOSPEARL 120, manufactured by Momentive Performance Materials, Inc., average particle size: 2 μm) are added to the obtained dispersion as a surface roughening material. The amount of silicone resin particles added is 10% by mass relative to the total mass of the metal oxide particles and the binder material in the dispersion from which the glass beads are removed. In addition, silicone oil (product name: SH28PA, manufactured by Dow Toray Co., Ltd.) in an amount of 0.01% by mass relative to the total mass of the metal oxide particles and the binder material in the dispersion is added as a leveling agent for the dispersion. Subsequently, a mixed solvent of methanol and 1-methoxy-2-propanol (mass ratio: 1:1) was added to the dispersion in such a manner that the total mass of the metal oxide particles, the binder material and the surface roughening material in the dispersion (i.e., the mass of the solid content) reached 67% by mass relative to the mass of the dispersion. Then, the resultant was stirred to prepare a conductive layer coating liquid. The conductive layer coating liquid was applied to the support by dip coating, and the resultant was heated at 140°C for 1 hour to form a conductive layer with a thickness of 30 μm.
[0190] <Base Coating>
[0191] Prepare surface treated titanium oxide (number average primary particle size: 10nm). Titanium oxide is surface treated with aluminum oxide and silicon dioxide, and surface treated titanium oxide is further surface treated with methyl hydrogen polysiloxane, while wet dispersion. Subsequently, 2 parts by mass of surface treated titanium oxide, 1 part by mass of polyamide resin ("AmilanCM8000", manufactured by TORAY INDUSTRIES, INC., as a polyamide resin of a tetrapolymer of polyamide 6, polyamide 12, polyamide 66 and polyamide 610), 10 parts by mass of methanol, 1 part by mass of butanol and 1 part by mass of toluene are mixed with a bead mill for 5 hours to obtain a primer coating liquid. Then, the primer coating liquid obtained is applied to the conductive substrate prepared as above to form a coating film by dip coating, which is dried at 130°C for 30 minutes to form a primer having a thickness of 1.5 μm. The conductive substrate used is a drum-shaped support made of aluminum.
[0192] <Charge Generation Layer>
[0193] Y-type oxytitanium phthalocyanine (1.5 parts by mass) and polyvinyl acetal resin ("S-LECBX-5", manufactured by SEKISUI CHEMICAL CO., LTD.) (1 part by mass) as a charge generating material were added to a solvent containing propylene glycol monomethyl ether (40 parts by mass) and tetrahydrofuran (40 parts by mass). These materials and the solvent were mixed for 12 hours with a bead mill to disperse the materials in the solvent to obtain a coating liquid for a charge generating layer. The obtained coating liquid for a charge generating layer was applied to the undercoat layer by dip coating to form a coating film, which was dried by heating at a temperature of 100°C for 10 minutes to form a charge generating layer having a thickness of 0.25 μm.
[0194] <Charge Transport Layer>
[0195] A charge transport layer coating liquid was produced by mixing 6 parts by mass of (HTM-1) as a charge transport material, 4.5 parts by mass of resin X (P1) as a binder resin, 5.5 parts by mass of a polyarylate resin (P16) containing a structural unit represented by the following formula, 67.5 parts by mass of tetrahydrofuran, and 22.5 parts by mass of toluene. The resulting charge transport layer coating liquid was applied to the charge generating layer by dip coating to form a coating film, which was dried by heating at 120° C. for 30 minutes to form a charge transport layer having a thickness of 18 μm.
[0196]
[0197] (Viscosity average molecular weight: 40000)
[0198] [Photosensitive members 2 to 29, photosensitive members A to M]
[0199] An electrophotographic photosensitive member was produced according to the above-mentioned [Photosensitive member 1] except that the charge transporting material in the charge transporting layer, ie, the surface layer, the binder resin and the content of the charge transporting material based on the content of the binder resin were changed as shown in Table 2.
[0200] [Table 2]
[0201]
[0202]
[0203] The polyarylate resins (P17) to (P22), (P24) and (P25) contain a structural unit represented by the following formula:
[0204] (Viscosity average molecular weight: 42000)
[0205]
[0206] (Viscosity average molecular weight: 42500)
[0207]
[0208] (Viscosity average molecular weight: 42300)
[0209]
[0210] (Viscosity average molecular weight: 43300)
[0211]
[0212] (Viscosity average molecular weight: 41600)
[0213]
[0214] (Viscosity average molecular weight: 42900)
[0215]
[0216] (Viscosity average molecular weight: 45000)
[0217]
[0218] (Viscosity average molecular weight: 46200)
[0219] (Polycarbonate resin)
[0220] Prepare the following polycarbonate resin.
[0221] "Iupilon Z400" manufactured by MITSUBISHI GAS CHEMICAL COMPANY, INC. (viscosity average molecular weight: 40,000)
[0222] An example of production of toner will be described below.
[0223] <Preparation Example of Binder Resin Particle Dispersion>
[0224] 78.0 parts of styrene, 20.7 parts of butyl acrylate, 1.3 parts of acrylic acid as a carboxyl group-imparting monomer and 3.2 parts of n-lauryl mercaptan were mixed and dissolved. To this solution, an aqueous solution of 1.5 parts of NEOGEN RK (manufactured by DKS Co. Ltd.) in 150 parts of ion-exchanged water was added to disperse.
[0225] Furthermore, while slowly stirring the solution for 10 minutes, an aqueous solution of 0.3 parts of potassium persulfate in 10 parts of ion exchange water was added. After purging with nitrogen, emulsion polymerization was performed at 70° C. for 6 hours. After the polymerization was completed, the reaction solution was cooled to room temperature, and ion exchange water was added; thereby, a resin particle dispersion 1 having a solid content concentration of 12.5% by mass and a median particle diameter of 0.2 μm based on volume was obtained.
[0226] To measure the acid value, part of the obtained resin particles was washed with pure water and dried under reduced pressure to remove the surfactant. The acid value of the resin was measured and found to be 9.5 mgKOH / g.
[0227] <Preparation Example of Release Agent Dispersion Liquid>
[0228] 100 parts of behenyl behenate (melting point: 72.1° C.) and 15 parts of NEOGENRK were mixed in 385 parts of ion exchange water and dispersed for about 1 hour using a wet jet mill JN100 (manufactured by JOKOH CO., LTD.) to obtain a release agent dispersion having a concentration of 20% by mass.
[0229] <Preparation Example of Colorant Dispersion Liquid>
[0230] 100 parts of carbon black Nipex35 (manufactured by Orion Engineered Carbons S.A.) and 15 parts of NEOGEN RK were mixed in 885 parts of ion-exchanged water and dispersed with a wet jet mill JN100 for about 1 hour to obtain a colorant dispersion.
[0231] <Preparation Example of Toner 1>
[0232] Using a homogenizer (manufactured by IKA: ULTRA-TURRAX T50), 265 parts of the resin particle dispersion, 1:10 parts of the wax dispersion and 10 parts of the colorant dispersion were dispersed. The temperature of the container was adjusted to 30°C under stirring, and the pH was adjusted to 8.0 by adding a 1 mol / L sodium hydroxide aqueous solution.
[0233] An aqueous solution of 0.25 parts of aluminum chloride dissolved in 10 parts of ion exchange water was added as a flocculant under stirring at 30°C for 10 minutes. After standing for 3 minutes, the temperature began to rise, and the temperature was raised to 50°C to produce associated particles. While maintaining this state, the particle size of the associated particles was measured using a "Coulter Counter Multisizer 3" (registered trademark, manufactured by Beckman Coulter, Inc.). When the weight-average particle size reached 6.0 μm, 0.9 parts of sodium chloride and 5.0 parts of NEOGEN RK were added to stop the particle growth.
[0234] The pH was adjusted to 9.0 by adding 1 mol / L of sodium hydroxide aqueous solution, and then the temperature was raised to 95° C. to sphericalize the aggregated particles. The temperature was started to drop when the average circularity reached 0.980, and the temperature was lowered to room temperature; thereby, a toner particle dispersion was obtained.
[0235] Hydrochloric acid was added to the obtained toner particle dispersion to adjust the pH to 1.5 or less, the toner particle dispersion was stirred for 1 hour and allowed to stand, and then solid-liquid separation was performed with a pressure filter to obtain a toner cake. It was re-pulped into a dispersion with ion exchange water, and then solid-liquid separation was performed with the aforementioned filtering device. Re-pulping and solid-liquid separation were repeated until the conductivity of the filtrate reached 5.0 μS / cm or less, and then a final solid-liquid separation was performed to obtain a toner cake. The obtained toner cake was dried and further classified with a classifier to reach a weight average particle size (D4) of 6.0 μm to obtain toner particles.
[0236] The thus obtained toner particles (100 parts) were mixed with externally added strontium titanate particles (0.7 parts) (number average primary particle size: 70 nm) and silica particles (2.5 parts) (number average primary particle size: 12 nm) surface-treated with dimethyl silicone oil as external additives using FM10C (manufactured by NIPPON COKE & ENGINEERING CO., LTD.). The conditions for external addition were as follows. Lower blade: A0 blade; Interval setting between deflector and wall: 20 mm; Supply amount of toner particles: 2.0 kg; Rotation frequency: 66.6 s -1 ; External addition time: 10 minutes; Cooling water temperature and flow rate: 20℃, 10L / min.
[0237] Then, the resultant was sieved through a sieve having a mesh size of 200 μm to obtain a toner.
[0238] <Production Example of Toner 2>
[0239] Toner 2 is produced in the same manner as Toner 1, except that the flocculant aluminum chloride is replaced with polysilicon ferrosilicon PSI-100 (manufactured by SUIDO KIKO KAISHA, LTD.).
[0240] <Production Example of Toner 3>
[0241] Toner 3 was produced in the same manner as Toner 1 except that aluminum chloride, a flocculant, was replaced with magnesium chloride.
[0242] <Example 1>
[0243] <Evaluation>
[0244] Evaluation was performed using the electrophotographic photosensitive member and toner produced as described above. Table 3 shows the evaluation results.
[0245] A laser beam printer manufactured by Hewlett-Packard Company (product name: HP LaserJet Enterprise Color M553dn) was modified and the modified model was used. The modification enables the device to control and measure the voltage applied to the charging roller, to control and measure the image exposure light amount, and to control and measure the voltage applied during the transfer process.
[0246] The toner is removed from the black toner cartridge, and in place of the toner, the produced toner 1 is put in. The photosensitive member 1 is mounted to the black toner cartridge.
[0247] Subsequently, an image of a test chart with a coverage of 1% was output on 10,000 sheets of A4 plain paper under a low temperature / low humidity environment of 15°C and 10% RH. For charging conditions, the dark area potential was adjusted to -500 V; for exposure conditions, the image exposure light amount was adjusted to 0.25 μJ / cm 2 The paper used is ordinary paper CS-680 (68g / m 2 )(Canon Marketing Japan Inc.).
[0248] [Evaluation of wear resistance]
[0249] The amount of wear of the charge transport layer was determined from the difference between the thicknesses of the photosensitive member before and after the repeated output of 10,000 images.
[0250] [Evaluation of transferability]
[0251] After repeatedly outputting 10,000 images, a full solid image with a width of 30 mm was output in the longitudinal direction on plain paper CS-680, the output when the solid image was formed was stopped, and the residual toner on the electrophotographic photosensitive member was collected using a transparent belt made of transparent polyester (Polyester Belt 5511 Nichiban Co., Ltd.).
[0252] The measurement of the residual toner concentration was performed by the following procedure. A transparent tape having collected residual toner peeled off from the surface of the electrophotographic photosensitive member and an unused transparent tape were each attached to a high-grade white paper (GFC081 CANON INC.). The concentration D1 of the portion having the transparent tape loaded with the collected residual toner and the concentration D0 of the portion having the unused transparent tape were respectively measured with an X-Rite color reflection densitometer (X-rite 500 Series, manufactured by X-Rite, Inc.).
[0253] The difference value "D1-D0" obtained in the measurement is defined as the concentration of the residual toner. A lower residual toner concentration value indicates a smaller amount of residual toner.
[0254] (Evaluation Criteria)
[0255] A: Residual concentration is less than 0.02
[0256] B: Residual concentration is 0.02 or more and less than 0.06
[0257] C: Residual concentration is 0.06 or more and less than 0.10
[0258] D: Residual concentration is 0.10 or more
[0259] The results are shown in Table 3.
[0260] [Table 3]
[0261]
[0262]
[0263]
[0264] <Examples 2 to 35>
[0265] In Examples 2 to 35, process cartridges were produced using photosensitive members 2 to 29 and toners 1 to 3 as shown in Table 3, and the same image output test as in Example 1 was conducted.
[0266] <Comparative Examples 1 to 13>
[0267] In Comparative Examples 1 to 13, process cartridges were produced using photosensitive members A to M and toner 1 as shown in Table 3, and the same image output test as in Example 1 was performed. The evaluation results are shown in FIG.
[0268] According to the present invention, an image forming apparatus having strontium titanate used as an external additive for a toner can be provided, wherein the image forming apparatus maintains the durability of an electrophotographic photosensitive member and has excellent transferability even under low temperature / low humidity conditions.
[0269] While the present invention has been described with reference to exemplary embodiments, it is to be understood that the invention is not limited to the disclosed exemplary embodiments.The scope of the following claims is to be accorded the broadest interpretation so as to encompass all such modifications and equivalent structures and functions.
Claims
1. An electronic photographic device, comprising: An electrophotographic photosensitive member comprising a surface layer containing a resin X as a binder resin; a charging unit that charges the surface of the electrophotographic photosensitive member; an exposure unit that irradiates the charged surface of the electrophotographic photosensitive member with light to form an electrostatic latent image; a developing unit that supplies toner to the electrostatic latent image to form a toner image; and a transfer unit that transfers the toner image to a transfer medium, wherein The toner contains strontium titanate as an external additive, and The resin X comprises a structural unit represented by formula (1):
2. The electrophotographic apparatus according to claim 1, wherein the resin X further comprises a structural unit represented by formula (2): Where R 1 and R 2 Each represents a methyl group, R 3 and R 4 Combined with each other to represent a cycloalkylidene group having 5 or 6 carbon atoms; or R 1 and R 2 Each independently represents a hydrogen atom or a methyl group, R 3 Represents methyl, R 4 represents a hydrogen atom or an alkyl group having 2 or 3 carbon atoms.
3. An electrophotographic apparatus according to claim 2, wherein the value of n2 / n1 is 1.0 or more, wherein the value is the ratio of the number n2 of the structural units represented by formula (2) contained in the resin X to the number n1 of the structural units represented by formula (1) contained in the resin X.
4. The electrophotographic apparatus according to claim 2, wherein the content of the resin X containing the structural unit represented by the formula (1) and the structural unit represented by the formula (2) in the binder resin in the surface layer is 50% by mass or more and 100% by mass or less.
5. The electrophotographic apparatus according to claim 2, wherein the structural unit represented by formula (2) is a structural unit represented by formula (2-1), (2-2), (2-3), (2-4) or (2-5):
6. The electrophotographic apparatus according to claim 2, wherein the structural unit represented by formula (2) is a structural unit represented by formula (2-5):
7. The electrophotographic apparatus according to claim 1 or 2, wherein the resin X further comprises a structural unit represented by formula (PE1-1) and a structural unit represented by formula (PE2-1): 8 . The electrophotographic apparatus according to claim 1 , wherein the strontium titanate is in an amount of 0.1 to 1.0% by mass based on the mass percentage of toner particles in the toner.