Method for removing water from functional ingredient composition and composition containing resulting product

By mixing solid alkali and polyester solvent with aqueous functional ingredient composition at room temperature, the water is removed through hydrolysis reaction, which solves the problem that high water content functional ingredient is difficult to convert into tableting, and effectively removes water and ingredients are achieved. The retention of functions reduces energy consumption and component losses.

CN119096106APending Publication Date: 2024-12-06KEMLINK LABORATORIES GMBH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202380036342.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-05-24
Filing Date
2023-05-22
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Prior Art When removing water from functional ingredient compositions, conventional methods such as heating or distillation can lead to loss of components and high energy consumption, and high water content functional ingredients are difficult to convert into tablet form, affecting the stability of the formulation. and use.

Method used

The solid base and polyester solvent are mixed with the aqueous functional component composition at room temperature, and the water is removed by hydrolysis reaction. The resulting dehydrated product can be a flowable powder, a viscous fluid or a gel, and then mixed with a fluid additive. to form a flowable powder to ensure the retention of the ingredient function.

Benefits of technology

The effective removal of water is achieved, the functionality of functional components is maintained, energy consumption and component loss is reduced, and functional components with high water content is allowed to be converted into suitable tableting forms, which improves the stability and economicality of the formulation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119096106A_ABST
    Figure CN119096106A_ABST
Patent Text Reader

Abstract

A method for removing water from a functional ingredient composition containing 10% by weight or more of water is provided that does not require the input of thermal energy. The amount of water in the resulting dehydrated product does not exceed 33% of the starting amount of the water in the functional component, and the process produces a dehydrated product having a weight loss of 2% or less based on the total weight of the starting component.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Related Applications

[0002] Priority is claimed to U.S. Provisional Application No. 63 / 345,188, filed on May 24, 2022, entitled “PROCESS FOR REMOVING WATER FROM A FUNCTIONAL INGREDIENT COMPOSITION. AND COMPOSITIONS CONTAINING THE RESULTING PRODUCT.”

[0003] Where permitted, the subject matter of the above-identified applications is incorporated herein by reference in its entirety. Technical Field

[0004] The present invention as a whole relates to a method for removing water from a functional ingredient composition containing 10% by weight or more of water, which method does not require the input of thermal energy. The amount of water that can be detected in the dehydrated product produced by the method does not exceed 33% of the starting amount of water in the functional ingredient composition, or 25% of the starting amount of water in the functional ingredient composition, or 15% of the starting amount of water in the functional ingredient composition. The method can produce a dehydrated product with a weight loss of 2% or less based on the difference between the total weight of the starting ingredients and the final weight of the final product. A composition comprising a dehydrated functional ingredient product produced by the method herein is also provided. Background Art

[0005] Functional ingredients such as surfactants, dispersants, anti-redeposition agents, solubility regulators, rinse aids, odor counteractants, conditioners, antistatic agents, soil screening agents, detergents, and color protectants are sometimes provided by their manufacturers as compositions containing 10% by weight or more of water. However, the presence of such relatively large amounts of water may prevent the use of these functional ingredient compositions in some formulations, such as in compositions provided in tablet form.

[0006] Compositions in tablet form are known in the art. For example, detergent tablets are described in U.S. Pat. No. 3,953,350 (Fujino et al., 1976). Such tablet compositions are becoming more popular and desirable among consumers. Tablet compositions have several advantages over liquid and powder products because they do not require measurement, are therefore easier to handle and distribute by consumers, and are more compact, and are therefore more economical to ship and store. Compositions in tablet form are generally prepared by compacting or pressing a certain amount of a composition, usually in granular form. Functional ingredients containing water, particularly functional ingredient compositions containing 10% by weight or more of water, may be difficult (if not impossible) to incorporate as is into a typical formulation to be pressed into tablets. A relatively high water content may react with other ingredients in a tablet composition, or may make it impossible to release the compression or tablet. Even if tablets can be prepared, a relatively high water content may also lead to storage stability problems, or may adversely affect tablet hardness, friability, and physical integrity.

[0007] Conventional methods for removing water from functional ingredient compositions include applying thermal energy, such as evaporation or thermal distillation. Both methods result in a loss of functionality of the ingredient, or a portion of the ingredient is lost during the water removal process. Functionality loss defeats the entire purpose of efforts to remove water from the delivered functional ingredient composition, while ingredient loss during the water removal process and the cost of energy and equipment required to remove water using conventional methods increase the cost of the final formulation.

[0008] Therefore, there is a need for methods of removing water from functional ingredient compositions that do not adversely affect ingredient functionality or result in product loss and that can allow functional ingredient compositions having 10 wt % or more water to be used as a component of a composition in tablet form. Summary of the invention

[0009] Provided is a method for removing water from a functional ingredient composition containing 10% by weight or more of water, the method does not require input of thermal energy. The resulting dehydrated product can be in the form of a flowable powder, or the resulting product can be mixed with a flow aid to produce a flowable powder. The amount of water that can be detected in the dehydrated product produced by the method provided herein is no more than 33% of the initial amount of water in the functional ingredient, or 25% of the initial amount of water in the functional ingredient, or 15% of the initial amount of water in the functional ingredient. Based on the gross weight of the starting ingredient, the method provided herein can produce a dehydrated product with a weight loss of 2% or less, or a weight loss of 1% or less. The dehydrated product retains the functionality of the functional ingredient, and allows the functional ingredient composition originally containing 10% by weight or more of water provided by its manufacturer to be converted into a form that can be used for inclusion in a composition (such as tableting) in tablet form.

[0010] Provided herein are eco-friendly, environmentally acceptable, economical and efficient methods for modifying functional ingredient compositions containing 10 wt % or more water so that the product can be converted into a dehydrated form that retains the functionality of the functional ingredient and makes the functional ingredient composition suitable for inclusion in a tableting composition.

[0011] A method for removing water from an aqueous functional ingredient composition containing more than 10% by weight of water is provided, the method comprising mixing a solid base, a polyester solvent and the aqueous functional ingredient composition in a mixer at room temperature to produce a dehydrated product, wherein the amount of water in the dehydrated product does not exceed 33% of the initial amount of water in the aqueous functional ingredient composition, and the difference between the total weight of the solid base, polyester solvent and aqueous functional ingredient composition added to the mixer and the final weight of the dehydrated product is 2% or less. The functional ingredient in the aqueous functional ingredient composition can be or include a surfactant, a dispersant, an anti-redeposition agent, a solubility regulator, a rinse aid, an odor counteractant, a chelating agent, a conditioner, an antistatic agent, a soil shielding agent, a detergent, a color protectant or a combination thereof. The initial amount of water in the aqueous functional ingredient composition can be in the range of 10% to 98% by weight.

[0012] Solid alkali can include alkaline materials that are solid at room temperature and have a pH in the range of about 8 to 13.5. Solid alkali can include alkali metal salts, alkaline earth metal salts, chelating agents based on amino polycarboxylates, tetrasodium iminodisuccinate complexing agents or their combinations. Solid alkali can include one or more selected from the group consisting of: sodium acetate, potassium acetate, sodium carbonate, potassium carbonate, calcium carbonate, magnesium carbonate, sodium bicarbonate, potassium bicarbonate, sodium sesquicarbonate, sodium silicate, potassium silicate, sodium metasilicate, potassium metasilicate, methylglycine N, N-diacetic acid trisodium salt (MGDA), glutamic acid diacetic acid tetrasodium salt (GLDA) and tetrasodium iminodisuccinate. Solid alkali can include sodium carbonate, sodium bicarbonate, potassium carbonate, potassium bicarbonate, MGDA, GLDA or their combinations.

[0013] In the methods provided herein, the polyester solvent may include an ester compound comprising three or more Part. The polyester solvent can be or include a citrate, a lactate, a glyceride or a combination thereof. The polyester solvent can include triethyl citrate, acetyl triethyl citrate, tributyl citrate, acetyl tributyl citrate, trihexyl citrate, n-butyryl-tri(n-hexyl)-citrate, trioctyl citrate, tributyl aconitate, triacetin (glyceryl triacetate), tripropionin (glyceryl tripropionate), tributyrin (glyceryl tributyrate), tricaprin (glyceryl tricaprate), triolein (glyceryl trioleate), tristearin (stearin), tripalmitin (glyceryl tripalmitate), pentaerythritol tetraethylhexanoate or a combination thereof. The polyester solvent may be selected from triethyl citrate, acetyl triethyl citrate, tributyl citrate, acetyl tributyl citrate, triacetin (glyceryl triacetate), tripropionin (glyceryl tripropionate), tributyrin (glyceryl tributyrate), and combinations thereof.

[0014] In the methods provided herein, when the ratio of the solid base to the functional ingredient composition is in the range of about 5:1 to 15:1, the dehydration product is in the form of a flowable powder. When the ratio of the solid base to the functional ingredient composition is in the range of about 5:1 to 15:1, the ratio of the solid base to the polyester solvent can be in the range of about 3:1 to 8.5:1. When the ratio of the solid base to the functional ingredient composition is in the range of about 5:1 to 15:1, the ratio of the polyester solvent to the functional ingredient composition can be in the range of about 1:1 to 3:1.

[0015] In the methods provided herein, when the ratio of the solid base to the functional ingredient composition is in the range of about 3:1 to 1:5, the dehydration product is in the form of a viscous fluid. When the ratio of the solid base to the functional ingredient composition is in the range of about 3:1 to 1:5, the ratio of the solid base to the polyester solvent is in the range of about 3.5:1 to 1:11. When the ratio of the solid base to the functional ingredient composition is in the range of about 3:1 to 1:5, the ratio of the polyester solvent to the functional ingredient composition is in the range of about 4:1 to 1:4.

[0016] In the methods provided herein, when the ratio of the solid base to the functional ingredient composition is in the range of about 3:1 to 1:5, the dehydrated product can be allowed to age for a period of 3 to 8 hours to obtain a dehydrated product in the form of a gel. The dehydrated product can be aged for a period of 18 to 24 hours to obtain a dehydrated product in the form of a putty.

[0017] The dehydrated product in the form of a viscous fluid, or a gel, or a putty can be blended with a flow aid to produce a flowable product. The flow aid may include: a) sodium chloride, potassium chloride sodium sulfate, potassium sulfate, or a combination thereof; b) a sodium and / or potassium salt of at least one of acetate, carbonate, bicarbonate, citrate, phosphate, silicate, aluminate, or a combination thereof; or c) a combination of these materials. The ratio of the flow aid to the dehydrated product can be about 1:1 to 5:1. The blending of the dehydrated product in the form of a viscous fluid or gel with the flow aid can be performed for a period of about 10 minutes or longer. The time period can be 10 minutes to 120 minutes, or 10 minutes to 60 minutes. In some methods, the dehydrated product is allowed to age for a period of 1 hour to 24 hours before blending with the flow aid.

[0018] In some methods provided herein, when the dehydrated product is aged for 18 to 24 hours and the resulting dehydrated product has the consistency of hard putty, the dehydrated product can be converted into a flowable powder by simply applying energy to crush the aged product into microparticles without adding a flowability aid.

[0019] In the methods provided herein, the mixer used to mix the solid base, the polyester solvent, and the aqueous functional ingredient composition can be any mixer known in the art. The mixer can be Countertop stand mixer, Planetary mixers, V-blenders, V-conical blenders, rotary batch mixers, ribbon blenders, paddle blenders, plow blenders, screw mixers, turbulence enhancers, The mixture may be mixed in a mixing process, for example, by mixing the mixture in a mixer, a double-arm kneader mixer or a combination thereof. The mixing may be carried out at room temperature and atmospheric pressure. The mixing may be carried out for a period of at least 10 minutes. The mixing may be carried out for a period of 10 to 120 minutes or for a period of 10 to 60 minutes. The amount of water in the dehydrated product does not exceed 33% of the initial amount of water in the aqueous functional ingredient composition.

[0020] Also provided are dehydrated products produced by the methods provided herein. Also provided are compositions comprising the dehydrated products produced by the methods provided herein. The compositions may be in the form of compressed tablets.

[0021] Based on the gross weight of composition or compressed tablet, the amount of dehydrated product in composition or compressed tablet can be in the scope of about 5 % by weight to 95 % by weight.Based on the gross weight of composition, composition or compressed tablet can also comprise the additional component in the scope of about 0.05 % by weight to 75 % by weight.Additional component can be selected from organic solvent, additional surfactant, buffer salt, lubricant, aromatic, coloring agent, chelating agent, enzyme, acid, carbonate, bicarbonate, phosphate, wetting agent, dispersant, hydrotrope, effervescent generator, rheology control agent, defoamer and their combination.Composition or compressed tablet can be formulated as sterilization product, disinfection product, surface cleaner, hand washing product, bath product, hair washing product, hair conditioning product, skin softening product, dish soap or detergent product, laundry detergent, clothing softening product, clothing antistatic product or pet odor removal product.

[0022] Also provided are unit dosage forms comprising the dehydrated products produced by the methods provided herein. The unit dosage form can be in the form of compressed tablets, capsules, pellets, pucks, bricks, briquettes, blocks, soluble pouches, soluble sachets. When dissolved in a solvent, one or more unit dosage forms can produce a germicidal solution, a disinfecting solution, a surface cleaner, a hand washing product, a bath product, a hair washing product, a hair conditioning product, a skin softening product, a dishwashing soap or detergent product, a laundry detergent, a laundry softening product, a laundry antistatic product, or a pet odor removal product. DETAILED DESCRIPTION

[0023] A. Definition

[0024] Unless otherwise defined, all technical terms and scientific terms used herein have the same meaning as the meaning generally understood by those skilled in the art to which the present invention belongs. Unless otherwise specified, all patents, patent applications, published patent applications and publications, websites and other published materials mentioned throughout the entire disclosure of this article are incorporated herein by reference as a whole. In the case where there are multiple definitions for the terms herein, the definition in this section shall prevail. In the case of quoting URLs or other such identifiers or addresses, it should be understood that such identifiers can change and specific information on the Internet can come and go, but equivalent information can be found by searching the Internet. Reference to it proves the availability and public dissemination of such information.

[0025] As used herein, the singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise.

[0026] As used herein, all ranges include upper and lower limits. As used herein, the expression of a numerical range for a variable is intended to convey that the variable can be equal to any value within the range and any and all subranges covered by a wider range. Therefore, the variable can be equal to any integer value within the numerical range, including the endpoints of the range. For example, a variable described as having a value between 0 and 10 can be 0, 3, 4-8, 2.15, 6.8-9.1, etc.

[0027] As used herein, "about" is a term of approximation, and is intended to include slight variations from the literally stated amount, as understood by those skilled in the art. Such variations include, for example, standard deviations associated with techniques commonly used to measure the amounts of constituent elements or components of an alloy or composite material, or other properties and characteristics. All values ​​characterized by the above modifier "about" are also intended to include the exact value associated therewith. Thus, "about 5%" means "about 5%" as well as "5%".

[0028] As used herein, "optional" or "optionally" means that the subsequently described event or circumstance does or does not occur, and that the description includes instances where the event or circumstance occurs and instances where the event or circumstance does not occur. For example, an optional component in a system means that the component may or may not be present in the system.

[0029] As used herein, the terms "comprises" and "comprising" are inclusive and can be interpreted broadly rather than exclusively. When used in the specification and claims, the terms "comprises" and "comprising" and variations thereof mean the inclusion of specified features, steps or components but not the exclusion of other features, steps or components.

[0030] Unless expressly stated to the contrary, any composition described herein is intended to encompass compositions consisting of, consisting essentially of, and comprising the various components identified herein.

[0031] In the specification and claims, the singular includes plural referents unless the context clearly dictates otherwise. As used herein, unless otherwise specifically indicated, the word "or" is used in the "inclusive" sense of "and / or" and not in the "exclusive" sense of "either / or".

[0032] As used herein, the term "exemplary" means "serving as an example or illustration," and should not be construed as preferred or advantageous over other configurations disclosed herein.

[0033] Unless otherwise stated, each individual feature or embodiment of this specification may be combined with any other individual feature or embodiment described herein without limitation. Such combinations are specifically contemplated to be within the scope of the present invention, regardless of whether they are explicitly described as a combination herein.

[0034] As used herein, "weight percent" or "wt%" refers to the concentration of a substance when the weight of the substance is divided by the total weight of the composition and multiplied by 100.

[0035] As used herein, "functional ingredient composition" refers to a composition that includes compounds or ingredients that perform or achieve a specific function within a product to deliver or produce a beneficial effect. Exemplary functional ingredient compositions include surfactants, dispersants, anti-redeposition agents, solubility modifiers, rinse aids, odor counteractants, chelating agents, conditioning agents, antistatic agents, soil screening agents, detergents, and color protection agents.

[0036] As used herein, "water removal" means converting at least a portion of the water in a composition into other more desirable products, and thereby resulting in a negligible total weight loss of the total weight of the starting ingredients.

[0037] As used herein, "compressed tablets" refers to dosage forms comprising compressed powders. For example, compressed tablets can be formed using a rotary tablet press or other similar machines known to those skilled in the art.

[0038] As used herein, "surfactant" refers to a surface active molecule that absorbs at the air / water, oil / water and / or oil / water interface, thereby substantially reducing its surface energy. Surfactants are generally classified according to the charge of the surface active portion, and can be classified as cationic surfactants, anionic surfactants, nonionic surfactants, and amphoteric surfactants.

[0039] As used herein, a "biosurfactant" is a surfactant of biological origin.

[0040] As used herein, "composite material" refers to a mixture of two or more different components where the components are not completely dissolved or combined, but which form a substantially homogeneous material (ie, a material that does not have a layered structure or compositional gradients).

[0041] As used herein, "eco-friendly" means not harmful to the environment or having minimal negative impact on the environment.

[0042] As used herein, "solid" refers to a composition that is not a fluid or liquid and that substantially retains its shape under moderate stress, pressure, or gravity.

[0043] As used herein, "flowable" refers to the ability of a material to flow under its own weight at a given temperature, or a material that can move in a flow in response to external forces applied thereto.

[0044] As used herein, "granule" refers to an aggregate of particles.

[0045] As used herein, "powder" refers to a solid that consists of particulate material, such as particles or granules, or a combination thereof, and that flows freely under moderate stress (such as mixing) or gravity.

[0046] As used herein, "dehydration product" refers to a resulting material that contains less water than the starting material used.

[0047] As used herein, "flow aid" refers to a substance that, when blended with the dehydrated product, aids in dispersing the dehydrated product into free-flowing particles.

[0048] As used herein, "viscous liquid" refers to a material that exhibits relatively high viscosity while maintaining fluidity and has a consistency between water and gel, which have low viscosity.

[0049] As used herein, "gel" refers to a flowable jelly-like material, typically having the consistency of petroleum jelly or toothpaste.

[0050] As used herein, "putty" refers to a composition having a dough-like or clay-like texture, which may have varying degrees of firmness (resistance to deformation). "Very soft putty" is easily deformable and has a consistency similar to bread dough. "Soft putty" requires minimal force to deform and has the composition of a pomade or balm. "Regular putty" has the consistency of "Silly Putty" (an "elastic solid" that is a mixture containing dimethicone, silica, polydimethylsiloxane, glycerin, decamethylcyclopentasiloxane, and a castor oil derivative) or Play-Doh (a soft, pliable modeling compound) and can be deformed with moderate force. "Hard putty" does not deform easily and requires a moderately high force to deform. "Very hard putty" requires a high degree of force to deform and has the consistency of a waxy solid, such as carnauba wax, such as Turtle Wax.

[0051] As used herein, "room temperature" means an ambient temperature in the range of about 20°C to about 25°C (typically with an average of about 21°C).

[0052] As used herein, "room temperature process" means that the process is performed at ambient temperature and without the addition of thermal energy, although frictional heating due to mixing or temperature increases due to chemical reactions such as hydrolysis may occur. BRIEF DESCRIPTION OF THE DRAWINGS

[0053] Figure 1 is the second derivative near infrared spectrum of the dehydration product produced by the method provided herein. The dehydration product was scanned on a Metrohm / Foss near infrared spectroscopy system.

[0054] FIG. 2A to FIG. 6B is a graph of a bivariate fit showing the decrease in the intensity ("Y") of the water peaks (1400 nm and 1900 nm) alone, which correlates to the decrease in the amount of water molecules in the blend. The X-axis shows the measurement time. Figure 2A and Figure 2B The results for mixture 1 ( Results obtained at 1400 nm and 1900 nm for LGC Sorb surfactant). Figure 3A and Figure 3B The results for mixture 2 ( LS30 surfactant) at 1400 nm and 1900 nm. Figure 4A and Figure 4B The results obtained for mixture 3 (Hostapon CGN surfactant) at 1400 nm and 1900 nm, respectively, are shown. Figure 5A and Figure 5B The results for mixture 4 ( BOB surfactant and soda ash) at 1400nm and 1900nm. Fig. 6A and Figure 6B The results for mixture 5 ( BOB surfactants and M) Results obtained at 1400 nm and 1900 nm.

[0055] C. Description of the Methods Provided Herein

[0056] Many functional ingredients with desired attributes, such as surfactants, deodorants, etc., cannot be obtained in anhydrous form. For example, many surfactant compositions can contain 30% to 70% by weight provided by their manufacturers, and can not be obtained in dry form. These aqueous surfactant compositions account for approximately 30% to 40% of currently available surfactant composition options. The presence of water may hinder their use in some preparations, such as solid granular or tabletted products, unless the water present in the functional ingredient composition delivered is removed. Some other functional ingredients can be provided by their manufacturers in the form that can comprise 98% to 99% by weight water. With such high water content, these functional ingredient compositions can not be included in preparations usually, such as solid granular or tabletted products, unless the water present in the functional ingredient composition delivered is removed.

[0057] Provided herein are eco-friendly, environmentally acceptable, economical and effective methods for modifying a functional ingredient composition containing 10 wt % or more of water so that the functional ingredient composition can be converted into a stable dehydrated product form that retains the functionality of the functional ingredient and makes the functional ingredient composition suitable for inclusion in a tableting composition.

[0058] The method provided herein does not require a long period of time to achieve water reduction, does not require a large energy input to reduce the amount of water present, does not require a heating unit, and does not require any specialized equipment to perform the method. The method can be performed using mixing equipment that is typically present at the production site of the formulation manufacturer.

[0059] In addition, unlike conventional heating or distillation methods commonly used to remove water from ingredient compositions, the methods provided herein do not result in loss of active ingredients during processing. Conventional methods depend on the use of energy-intensive methods to remove water, typically by heating or distillation, and thus reduce the total weight of the product obtained at the end of the water removal process. In contrast, the methods provided herein convert at least a portion of the water present in the aqueous active ingredient composition into a beneficial ingredient, and thus the weight change of the final product is minimal compared to the weight of the starting material.

[0060] In the methods provided herein, the functional ingredients in the functional ingredient compositions provided are not subjected to high temperatures to evaporate or distill off water. Instead, a method is provided that is performed under ambient conditions, typically room temperature and pressure (about 1 atmosphere, or about 1 bar, or about 14.7 psi). The method includes a chemical reaction that allows water to be converted under thermodynamically favorable conditions, so that no heat energy input is required to drive the reaction. Frictional heating during mixing or chemical reactions during the method, or both, can result in a temperature increase, but the method does not require additional heat energy input. For example, adding water from the functional ingredient composition to sodium carbonate or potassium carbonate can result in a temperature increase, such as up to 40°C to 70°C.

[0061] The method provided herein can remove water from a functional ingredient composition containing 10 wt % or more (such as 10 wt % to 98 wt %) water, thereby obtaining a dehydrated product. The method includes mixing a solid base, a polyester solvent and a functional ingredient composition in a pH range of 8 to 13 in a mixer. Mixing can be performed at room temperature and ambient pressure. Mixing can be performed for a period of 10 minutes to 60 minutes. In some methods, the resulting dehydrated product is in the form of a flowable powder. In some methods, the resulting dehydrated product is in the form of a viscous fluid or gel, which can be converted into a flowable powder by mixing with a salt. In some embodiments, the salt can be or contain a neutral salt, such as sodium chloride, potassium chloride sodium sulfate or potassium sulfate or a combination thereof. In some embodiments, the salt can be or contain a sodium salt and / or potassium salt of at least one of acetate, carbonate, bicarbonate, citrate, phosphate, silicate or aluminate or a combination thereof.

[0062] In the provided methods, the ester hydrolysis reaction consumes at least a portion of the water present in the active ingredient and produces safe byproducts, such as glycerol or ethanol, which can be beneficial, particularly for tableting production.

[0063] An exemplary reaction scheme for the methods provided herein is shown in Reaction Scheme 1 below.

[0064] <Reaction Scheme 1> - Using triacetin as polyester solvent

[0065]

[0066] In the reaction shown in Reaction Scheme 1, an aqueous surfactant composition (Crodasinic TM LS30, an aqueous composition containing sodium lauroyl sarcosinate) is mixed with triacetin (triacetin) as a polyester solvent and soda ash (sodium carbonate (Na2CO3)) as a solid base. A hydrolysis reaction occurs, so that diacetin, monoacetin, glycerol and acetic acid are produced, which undergo ion exchange between sodium lauroyl sarcosinate, soda ash and acetic acid to produce, in particular, N-lauryl sarcosinate, sodium bicarbonate, sodium acetate and glycerol. Almost no water remains.

[0067] Any technology known in the art can be used to assess the reduction or disappearance of water. For example, near infrared spectroscopy (NIRS) can be used. The peak of water appears in the near infrared spectrum at about 1400nm to 1450nm and 1900nm to 1950nm. The dehydrated product produced using the method provided herein is scanned on the Metrohm / Foss near infrared spectroscopy system immediately after mixing and after 24 hours of storage. As shown in Figure 2, the amount of water present in the dehydrated product at the end of the reaction of the method provided herein is significantly reduced. The spectrum shown in Figure 2 is a second derivative spectrum for characterizing the dehydrated product.

[0068] The method using different polyester solvents is shown in Reaction Scheme 2. In Reaction Scheme 2, triethyl citrate ( A1) as polyester solvent.

[0069] <Reaction Scheme 2> - Using Citrofol as a polyester solvent

[0070]

[0071] In the reaction shown in Reaction Scheme 2, an aqueous surfactant composition (Crodasinic TM LS30, an aqueous composition containing sodium lauroyl sarcosinate) and a polyester solvent Al (triethyl 2-hydroxypropane-1,2,3-tricarboxylate or triethyl citrate) and pure ash (sodium carbonate (Na2CO3)) as a solid base are mixed. A hydrolysis reaction occurs, so that sodium 4-ethoxy-2-(2-ethoxy-oxoethyl)-2-hydroxy-4-oxobutyrate, sodium (2S)-2-(2-oxoethyl)-2-hydroxy-succinate, sodium 2-hydroxypropane-1,2,3-tricarboxylate, sodium bicarbonate and ethanol are produced, which undergo ion exchange to produce, in particular, N-sarcosine lauryl ester, sodium bicarbonate, sodium citrate and ethanol. There is almost no water remaining.

[0072] In the methods provided herein, safe starting materials are used, and the reactions result in the production of safe products.

[0073] Solid Base

[0074] The method provided herein includes mixing a solid base with a polyester solvent and a functional ingredient composition. The solid base used in the method can be any alkaline material that is solid at room temperature and has a pH in the range of about 8 to 13.5. In some embodiments, the solid base can have a pH in the range of about 8.3 to 12.5. In some embodiments, the solid base can have a pH in the range of about 9 to 12. In some embodiments, the solid base can have a pH in the range of about 10.5 to 12.

[0075] Solid base can comprise alkali metal salt, alkaline earth metal salt, amino polycarboxylate based chelating agent, iminodisuccinic acid tetrasodium complexing agent or their combination. Some examples of alkali metal salt include alkali metal acetate, bicarbonate, carbonate, citrate, silicate, metasilicate and their mixture. Some examples of alkaline earth metal salt include alkaline earth metal acetate, bicarbonate, carbonate, citrate, silicate, metasilicate and their mixture. Exemplary solid base includes but is not limited to potassium acetate, sodium acetate, sodium carbonate, potassium carbonate, calcium carbonate, magnesium carbonate, sodium bicarbonate, potassium bicarbonate, sodium sesquicarbonate, sodium citrate, potassium citrate, sodium silicate, potassium silicate, sodium metasilicate, potassium metasilicate, methylglycine N, N-diacetic acid trisodium salt (MGDA, such as MS, Nouryon, Arnhem, The Netherlands), glutamic acid diacetate tetrasodium salt (N,N-dicarboxymethylglutamate tetrasodium salt (GLDA, such as GL-PD-S, Nouryon, Arnhem, The Netherlands), tetrasodium iminodisuccinate such as CX100 solid G (RheinChemie Additives, Cologne, Germany) and combinations thereof. In some embodiments, the solid base is sodium carbonate, sodium bicarbonate, potassium carbonate, potassium bicarbonate, MGDA, GLDA, or combinations thereof.

[0076] Polyester solvent

[0077] The polyester solvent may be a polyester containing three or more In some embodiments, the polyester solvent may include a glyceride, a citrate, or a combination thereof. In some embodiments, the polyester solvent may include a glyceride, a citrate, or a combination thereof.

[0078] Exemplary polyester solvents include, but are not limited to, triethyl citrate ( Al, Jungbunzlauer), acetyl triethyl citrate ( Al1), tributyl citrate ( Bl, Jungbunzlauer), acetyl tributyl citrate ( In some embodiments, the polyester solvent may be selected from triethyl citrate, acetyl triethyl citrate, tributyl citrate, triacetin (glyceryl triacetate), tripropionin (glyceryl tripropionate), tributyrin (glyceryl tributyrate), tricaprin (glyceryl tricaprylate), triolein (glyceryl trioleate), tristearin (stearin), tripalmitin (glyceryl tripalmitate), pentaerythritol tetraethylhexanoate and combinations thereof. In some embodiments, the polyester solvent may be selected from triethyl citrate, acetyl triethyl citrate, tributyl citrate, acetyl tributyl citrate, triacetin (glyceryl triacetate), tripropionin (glyceryl tripropionate), tributyrin (glyceryl tributyrate) and combinations thereof.

[0079] Functional ingredient composition

[0080] Any functional ingredient composition containing 10% by weight or more water can be selected to remove water from the functional ingredient composition using the methods provided herein. Exemplary functional ingredient compositions include, but are not limited to, surfactants, dispersants, anti-redeposition agents, solubility regulators, rinse aids, odor counteractants, chelating agents, conditioners, antistatic agents, soil shielding agents, detergents, and color protectants.

[0081] When the functional ingredient composition comprises a surfactant, the surfactant may be selected from cationic surfactants, anionic surfactants, nonionic surfactants, zwitterionic surfactants, silicone surfactants, biosurfactants, and combinations thereof.

[0082] Exemplary nonionic surfactants include nonylphenol ethoxylate surfactants, nonylphenoxy poly(ethyleneoxy)ethanol; nonionic nonylphenyl polyglycol ethers; polyoxyethylene (10) nonylphenol; polyoxyethylene (14) nonylphenol; polyoxyethylene (1.5) nonylphenol; polyoxyethylene (20) nonylphenol; polyoxyethylene (30) nonylphenol; polyoxyethylene (4) nonylphenol; polyoxyethylene (5) nonylphenol; polyoxyethylene (6) nonylphenol; polyoxyethylene (8) nonylphenol; polyoxyethylene (9) nonylphenyl ether; Protachem 630; Sterox; Surfionic N; T-DET-N; Tergitol NP; Tergitol NP-14; Tergitol NP-27; Tergitol NP-33; Tergitol NP-35; Tergitol NP-40; Tergitol NPX; Tergitol TP-9; Triton N; Triton X; Dowfax 9N; ethoxylated nonylphenol; Igepal CO; Igepal CO-630; polyethylene glycol nonylphenyl ether; Makon; Neutronyx 600; Nonipol NO; nonionic surfactants having an alkylene oxide polymer as part of the surfactant molecule, such as polyglycol ethers of chloro-terminated, benzyl-terminated, methyl-terminated, ethyl-terminated, propyl-terminated, butyl-terminated and other similar alkyl-terminated fatty alcohols; nonionic materials without alkylene oxides, such as alkyl polyglycosides; sorbitan and sucrose esters and their ethoxylates; alkoxylated ethylenediamines; alcohol alkoxylates such as alcohol ethoxylate propoxylates, alcohol propoxylates, alcohol propoxylate ethoxylate propoxylates, alcohol ethoxylate butoxylates; nonylphenol ethoxylates, polyoxyethylene glycol ethers; carboxylates such as glycerol esters of fatty acids, polyoxyethylene esters, ethoxylated and ethylene glycol esters; carboxylic acid amides such as diethanolamine condensates, monoalkanolamine condensates, polyoxyethylene fatty acid amides; and alkylene oxide block copolymers, including ethylene oxide / propylene oxide block copolymers, such as those available under the trademark Those commercially available from BASF-Wyandotte.

[0083] Exemplary silicone surfactants that may be present in the functional ingredient composition include, but are not limited to, dimethicone copolyols and alkyl dimethicone copolyols and blends thereof; polyalkyl polyether polysiloxane copolymers having alkyl radicals containing from 5 to 22 carbon atoms, such as cetyl dimethicone copolyol, such as those manufactured by Evonik Industries AG (Essen, Germany) under the name EM-90; a mixture of dimethicone copolyol and cyclopentasiloxane (85 / 15), such as sold by Goldschmidt under the name EM-97; linear polyether-modified silicone emulsifiers, including methyl ether dimethicone, such as PEG-3 methyl ether dimethicone, PEG-9 methyl ether dimethicone, PEG-10 methyl ether dimethicone, PEG-11 methyl ether dimethicone, and butyl ether dimethicone (available from Shin-Etsu, Akron, Ohio); branched polyether-modified silicone emulsifiers, such as PEG-9 polydimethylsiloxyethyl dimethicone (Shin-Etsu); alkyl co-modified branched polyether silicones, such as lauryl PEG-9 polydimethyl-siloxyethyl dimethicone (Shin-Etsu); alkylene oxide-containing silicone emulsifiers, such as commercially available 7001, manufactured by Momentive Performance Materials (Albany, NY); Dow Corning FG-10, L-77 (alkylene oxide-modified heptamethyl trisiloxane containing methyl end groups and 1 side group and having an average molecular weight of 645) and L-7608 (alkylene oxide-modified heptamethyltrisiloxane containing hydrogen terminal groups and one pendant group and having an average molecular weight of 630), available from Momentive Performance Materials; Lambent TM MFF-199-SW (containing hydrogen end groups and one pendant polyethylene oxide group and having an average molecular weight between 600 and 1000), available from Lambent Technologies Inc. (Gurnee, IL); carboxylic acid esters based on silicone copolyols, such as SW-CP-K (containing phthalate end groups and one polyethylene oxide pendant group and having an average molecular weight between 800 and 1100) and Lube CPI (containing phthalate end groups and 3 to 5 pendant groups and having an average molecular weight between 2900 and 5300) available from Lambent Technologies Inc.; alkyl-dimethicone copolyol type surfactants, such as those described in U.S. Pat. No. 7,083,800 (Terren et al., 2006), including those marketed under the name " WE09″、″ WS 08″ and″ Such silicone emulsifiers are commercially available as ELECTRONICS EM 90" (Evonik Industries AG, Essen, Germany), as well as cationic silicone emulsifiers such as those described in U.S. Pat. No. 5,124,466 (Azechi et al., 1992).

[0084] Exemplary cationic surfactants include, but are not limited to, homopolymers and copolymers derived from free radical polymerizable acrylate or methacrylate or amide monomers. Copolymers may contain one or more units derived from acrylamide, methacrylamide, diethyl ketone acrylamide, acrylic acid or methacrylic acid or their esters, vinyl lactams (such as vinyl pyrrolidone or vinyl caprolactam), and vinyl esters. Exemplary polymers include copolymers containing acrylamide and dimethylaminoethyl methacrylate quaternized with dimethyl sulfate or with alkyl halides; copolymers of acrylamide and methacryloyloxyethyltrimethylammonium chloride; copolymers of acrylamide and methacryloyloxyethyltrimethylammonium methylsulfate; copolymers of vinyl pyrrolidone / dialkylaminoalkyl acrylate or methacrylate, optionally quaternized, such as those sold by International Specialty Products under the name GAFQUAT TM Products marketed as dimethylaminoethyl dimethacrylate / vinyl caprolactam / vinyl pyrrolidone terpolymers, such as those marketed under the name GAFFIX by International Specialty Products TM Products sold under the name STYLEZE by International Specialty Products; Vinyl pyrrolidone / methacrylamidopropyl dimethylamine copolymer; TM CC 10; and a copolymer of vinyl pyrrolidone and quaternized dimethylaminopropyl methacrylamide, such as that sold under the name GAFQUAT by International Specialty Products TM HS100; quaternary ammonium polymers of vinylpyrrolidone and vinylimidazole, such as those sold by BASF under the trade name (Products marked FC 905, FC 550 and FC 370) sold; Acetamidopropyl trimonium chloride, Behenamidopropyl dimethylamine, Behenamidopropyl ethyl dimethyl ammonium ethosulfate, Behentrimonium chloride, Cetyl ethyl morpholinium ethosulfate, Cetyl trimonium chloride, Cocoamidopropyl ethyl-dimethyl ammonium ethosulfate, Dicetyl dimethyl ammonium chloride, Polydimethicone hydroxypropyl trimonium chloride, Hydroxyethyl behenamidopropyl diammonium chloride, Quaternium-26, Quaternium-27, Quaternium-53, Quaternium-63, Quaternium-70, Quaternium-72, Quaternium-76 hydrolyzed collagen, PPG-9 diethyl ammonium chloride, PPG-25 Diethylammonium chloride, PPG-40 diethylammonium chloride, stearyl dimethyl benzyl ammonium chloride, stearamidopropyl ethyl dimethyl ethosulfate, stearyl dimethyl hydroxypropyl hydrolyzed wheat protein, stearyl dimethyl hydroxypropyl hydrolyzed collagen, wheat germ oil amido-propyl ammonium chloride, wheat germ oil amidopropyl ethyl dimethyl ethosulfate, polymers and copolymers of diallyl dimethyl ammonium chloride, such as polyquaternium-4, polyquaternium-6, polyquaternium-7, polyquaternium-10, polyquaternium-11, polyquaternium-16, polyquaternium-22, polyquaternium-24, polyquaternium-28, polyquaternium-29, polyquaternium-32, polyquaternium-3 3. Polyquaternium-35, Polyquaternium-37, Polyquaternium-39, Polyquaternium-44, Polyquaternium-46, Polyquaternium-47, Polyquaternium-52, Polyquaternium-53, Polyquaternium-55, Polyquaternium-59, Polyquaternium-61, Polyquaternium-64, Polyquaternium-65, Polyquaternium-67, Polyquaternium-69, Polyquaternium-70, Polyquaternium-71, Polyquaternium-72, Polyquaternium-73, Polyquaternium-74, Polyquaternium-76, Polyquaternium-77, Polyquaternium-78, Polyquaternium-79, Polyquaternium-80, Polyquaternium-81, Polyquaternium-82, Polyquaternium- 84, polyquaternium-85, polyquaternium-87, PEG-2-cocoyl ammonium chloride and mixtures thereof; polyalkylene imines, such as polyethylene imine, polymers containing vinyl pyridine or vinyl pyridinium units, condensates of polyamines and epichlorohydrin; quaternary polyurethanes; salts of optionally polyoxyalkylened primary, secondary or tertiary fatty amines; quaternary ammonium derivatives or amine oxides of imidazoline; monoalkyl quaternary ammonium compounds, dialkyl quaternary ammonium compounds or trialkyl quaternary ammonium compounds with counterions (such as chloride, methyl sulfate, toluene sulfonate), including but not limited to hexadecyl trimethyl ammonium chloride, dihexadecyl dimethyl ammonium chloride and behenyl trimethyl ammonium methyl sulfate.

[0085] Exemplary anionic surfactants include, but are not limited to, one or more of the following: carboxylates, such as, but not limited to, alkyl carboxylates (e.g., carboxylic acids and / or salts thereof), polyalkoxy carboxylates (e.g., polycarboxylic acids and / or salts thereof), alcohol ethoxylate carboxylates, nonylphenol ethoxylate carboxylates, or combinations thereof; sulfonates, such as, but not limited to, alkyl sulfonates, alkyl benzene sulfonates (e.g., dodecyl benzene sulfonic acid and / or salts thereof), alkyl aryl sulfonates, sulfonated fatty acid esters, or combinations thereof; sulfates, such as, but not limited to, sulfated alcohols, sulfated alcohol ethoxylates, sulfated alkylphenols, alkyl sulfates, sulfosuccinates, alkyl ether sulfates, or combinations thereof; phosphates, such as, but not limited to, alkyl phosphates; or combinations thereof. Exemplary anionic surfactants include sodium alkyl aryl sulfonates, α-olefin sulfonates, fatty alcohol sulfates, and combinations thereof. Exemplary sulfosuccinates include alkyl sulfosuccinates and amido sulfosuccinates, such as disodium lauryl sulfosuccinate (CAS 26838-05-1), disodium lauryl polyoxyethylene ether sulfosuccinate (CAS No. 39354-45-5), disodium oleamide MIPA sulfosuccinate (CAS No. 67815-88-7), and combinations thereof.

[0086] Exemplary amphoteric surfactants (or zwitterionic surfactants) include, but are not limited to, imidazoline derivatives, betaines, imidazolines, sulfobetaines, propionates, amine oxides, or combinations thereof, including imidazoline betaines, dimethyl alkyl lauryl betaines, alkyl glycine, and alkyl di(aminoethyl) glycine. Betaines may be alkyl betaines, alkyl amido betaines, or mixtures thereof, such as cetyl betaine (CAS No. 693-33-4), lauryl betaine (CAS No. 683-10-3), cocoamidopropyl betaine (CAS No. 61789-40-0), lauroamidopropyl betaine (CAS No. 4292-10-8), or any one of their combinations.

[0087] The functional ingredient composition may include a surfactant including a linear alcohol ethoxylate (e.g., 25-7, available from Evonik Industries AG, Essen, Germany) or C11 alcohol ethoxylate 5E.O. (e.g. 1-5, Evonik), or C11 alcohol ethoxylate 7E.O. (e.g., 1-7, Evonik), or C11 alcohol ethoxylate 9E.O. (e.g., 1-9, Evonik), or sodium lauryl sulfate, or sodium dodecylbenzene sulfonate (e.g., available from Stepan Company, Northfield, IL), or C9-C11 alcohol ethoxylate (e.g., 91-6, Evonik), or C12-C18 alcohol ethoxylate (e.g., available from Croda Inc., Mill Hall, Pennsylvania, USA), or PEG 7 cocoyl glyceride, or sodium lauroyl sarcosinate (e.g., L30, available from Schill and Seilacher GmbH, Berningen, Germany) or any combination thereof. The surfactant may include 1-dodecyl 2-butene dioate (CAS No. 2424-61-5), sodium 2-sulfosuccinate (CAS No. 13419-59-5), sodium lauroyl sarcosinate (CAS No. 137-16-6), sodium cocoyl sarcosinate (CAS No. 61791-59-1) or a combination thereof.

[0088] Functional ingredient compositions can include biosurfactants. Biosurfactants can be polymeric biosurfactants, glycolipids, lipopeptides, lipoproteins, phospholipids, flavonoids or combinations thereof. Biosurfactants can be lecithin, saponin, rhamnolipid, sophorolipid, mannosylerythritol lipid, trehalose lipid, glucolipid, cellulose lipid, trehalose lipid, glucoside, alkyl glucoside, alkyl polyglucoside, cellobiose lipid, polyhydroxy lipid, protein polyamine, lipopolysaccharide, fengycin, iturin, lichenin, surfactin or combinations thereof.

[0089] Exemplary functional ingredient compositions include, but are not limited to, Crodateric TM CAB30 (cocamidopropyl betaine and water, Croda Inc., Chino Hills, CA), Crodasinic TM LS30 (sodium lauroyl sarcosinate and water, Croda Inc., Chino Hills, CA), Crodasinic TM CS30 (sodium cocoyl sarcosinate and water, Croda Inc., Chino Hills, CA), 818UP (coco-glucoside and water, BASF CareCreaions, San Bruno, CA), PC48 (sodium methyl 2-sulfolaurate, disodium 2-sulfolaurate, and water, Stepan Company, Northbrook, IL), reric BOB (babassuamidopropyl betaine, Colonial Chemical Inc., Pittsburgh, TN, USA), 420UP (C8-C16 alkyl polyglycosides (caprylyl / myristyl glucoside) and water, BASF Care Creations, San Bruno, California), Amphi TM M (sophorolipid lactone CAS No. 1573124-58-9 and water, Locus Performance Ingredients, Richmond, VA), MultiTrope TM 810 (anionic surfactant and water, Croda Inc., Chino Hills, CA), Zinador TM 22L (poly-zinc itaconate complex odor neutralizer and water, Croda Inc., Chino Hills, CA), Zinador TM 35L (polyzinc itaconate complex odor neutralizer and water, Croda Inc., Chino Hills, CA) and 25-40D (sodium carboxymethylinulin and water, Cosun Beet Company, San Jose, CA).

[0090] In the methods provided herein, the starting amount of water in the functional ingredient composition can be in the range of 10 wt % to 98 wt %, or 15 wt % to 95 wt %, or 20 wt % to 85 wt %, or 25 wt % to 75 wt %, or 30 wt % to 70 wt %, or 10 wt % to 40 wt %, or 35 wt % to 60 wt %, based on the total weight of the functional ingredient composition.

[0091] 1. Direct formation of the dehydrated product in the form of a flowable powder

[0092] In some methods, the resulting dehydrated product is in the form of a flowable powder. The flowable powder form of the product can be achieved by controlling the ratio of the solid base to the functional ingredient composition. In the method provided herein, when the ratio of the solid base to the functional ingredient composition used in the method is in the range of about 5:1 to 15:1, a dehydrated product in the form of a flowable powder can be produced. The ratio of the solid base to the functional ingredient composition used in the method can be 5:1, 5.5:1, 6:1, 6.5:1, 7:1, 7.5:1, 8:1, 8.5:1, 9:1, 9.5:1, 10:1, 10.5:1, 11:1, 11.5:1, 12:1, 12.5:1, 13:1, 13.5:1, 14:1, 14.5:1 or 15:1.

[0093] When the ratio of the solid base used in the method to the functional ingredient composition is in the range of about 5:1 to 15:1, the ratio of the solid base used in the method to the polyester solvent may be in the range of about 3:1 to 8.5:1. The ratio of the solid base used in the method to the polyester solvent may be in the range of about 3.5:1 to 8:1. The ratio of the solid base used in the method to the polyester solvent may be 3:1, 3.25:1, 3.5:1, 3.75:1, 4:1, 4.25:1, 4.5:1, 4.75:1, 5:1, 5.25:1, 5.5:1, 5.75:1, 6:1, 6.25:1, 6.5:1, 6.75:1, 7:1, 7.25:1, 7.5:1, 7.75:1, 8:1, 8.25:1 or 8.5:1.

[0094] When the ratio of the solid base to the functional ingredient composition used in the method is in the range of about 5:1 to 15:1, the ratio of the polyester solvent to the functional ingredient composition used in the method may be in the range of about 1:1 to 3:1. The ratio of the polyester solvent to the functional ingredient composition used in the method may be in the range of about 1.1:1 to 2.75:1. The ratio of the polyester solvent to the functional ingredient composition used in the method may be 1:1, 1.1:1, 1.25:1, 1.5:1, 1.75:1, 2:1, 2.25:1, 2.5:1, 2.75:1 or 3:1.

[0095] Any mixing equipment known in the art that can mix and combine components can be used in the methods provided herein. Known devices such as Countertop stand mixer, Planetary mixers, V-blenders, V-conical blenders, rotary batch mixers, ribbon blenders, paddle blenders, plow blenders, screw mixers, turbulence enhancers, A mixer, a double-arm kneader mixer, or a combination thereof can be used to mix the components in the methods provided herein. The mixing can be performed at room temperature and atmospheric pressure and is not adversely affected by temperature or pressure conditions.

[0096] Mixing can be performed for 10 minutes or longer. The amount of time required may depend on the amount of material to be mixed and the size and type of mixing equipment selected. In some methods, mixing is performed for about 10 minutes to 60 minutes.

[0097] After the reaction has been completed, the dehydrated product in the mixer is in the form of a flowable powder. The dehydrated product can be taken out of the mixer and packaged, or can be aged for 1 to 24 hours before use, or can be directly taken out of the mixer as a component in a formulation for a granular or tableted product.

[0098] 2. Dehydration products in the form of viscous fluids, gels or putties

[0099] In the methods provided herein, when the ratio of the solid base to the functional ingredient composition used in the method is in the range of about 5:1 to 15:1, the resulting dehydrated product is in the form of a viscous fluid. When aged for about 3 to 8 hours without mixing, the dehydrated product forms a gel consistency. When further aged, about 18 to 24 hours after initial mixing, the dehydrated product forms a putty consistency.

[0100] The viscous fluid form of the product can be achieved by controlling the ratio of the solid base to the functional ingredient composition. In the method provided herein, when the ratio of the solid base to the functional ingredient composition used in the method is in the range of about 3:1 to 1:5, a dehydrated product in the form of a viscous fluid can be produced. The ratio of the solid base to the functional ingredient composition used in the method can be 3:1, 2.5:1, 2:1, 1.5:1, 1:1, 1:1.5, 1:2, 1:2.5, 1:3, 1:3.5, 1:4, 1:4.5 or 1:5.

[0101] When the ratio of the solid base used in the method to the functional ingredient composition is in the range of about 3:1 to 1:5, the ratio of the solid base used in the method to the polyester solvent may be in the range of about 3.5:1 to 1:11. The ratio of the solid base used in the method to the polyester solvent may be 3:5, 3:1, 2.5:1, 2:1, 1.5:1, 1:1, 1:1.5, 1:2, 1:2.5, 1:3, 1:3.5, 1:4, 1:4.5, 1:5, 1:5.5, 1:6, 1:6.5, 1:7, 1:7.5, 1:8, 1:8.5, 1:9, 1:9.5, 1:10, 1:10.5 or 1:11.

[0102] When the ratio of the solid base to the functional ingredient composition used in the method is in the range of about 3:1 to 1:5, the ratio of the polyester solvent to the functional ingredient composition used in the method may be in the range of about 4:1 to 1:4. The ratio of the polyester solvent to the functional ingredient composition used in the method may be in the range of about 3:1 to 1:3. The ratio of the polyester solvent to the functional ingredient composition used in the method may be 4:1, 3.5:1, 3:1, 2.5:1, 2:1, 1.5:1, 1.1, 1:1.5, 1:2, 1:2.5, 1:3, 1:3.5 or 1:4.

[0103] Any mixing equipment known in the art that can mix and combine components can be used in the methods provided herein. Known devices such as Countertop stand mixer, Planetary mixers, V-blenders, V-conical blenders, rotary batch mixers, ribbon blenders, paddle blenders, plow blenders, screw mixers, turbulence enhancers, A mixer, a double-arm kneader mixer, or a combination thereof can be used to mix the components in the methods provided herein. The mixing can be performed at room temperature and atmospheric pressure and is not adversely affected by temperature or pressure conditions.

[0104] Mixing can be performed for more than 10 minutes. The amount of time required may depend on the amount of material to be mixed and the size and type of mixing equipment selected. In some methods, mixing is performed for about 10 minutes to 60 minutes.

[0105] After the reaction has ended, the dehydrated product in the mixer is in the form of a viscous liquid. The viscous liquid can be aged for a period of about 3 hours to 8 hours without mixing to obtain a dehydrated product with a gel consistency. Upon further aging, about 18 hours to 24 hours after initial mixing, the dehydrated product forms a putty consistency.

[0106] The dehydrated product, whether in the form of a viscous liquid, gel or putty, can be converted into a flowable powder by mixing with a flow aid. Any flow aid known in the art can be used. In some embodiments, the flow aid includes a neutral salt, such as sodium chloride, potassium chloride, sodium sulfate or potassium sulfate or a combination thereof. In some embodiments, the flow aid includes a Na salt and / or a K salt of at least one of acetate, carbonate, bicarbonate, citrate, phosphate, silicate or aluminate or a combination thereof. In some embodiments, the flow aid may include a low bulk density carbonate or bicarbonate or a combination thereof. In some embodiments, the flow aid may include an expanded percarbonate, such as U.S. Pat. No. 8,652,434 (US Pat. No. 5,652,434). oo The amount of the added flow aid can be a ratio of the flow aid to the dehydrated product of 1:1 to 5:1. For example, 8 parts of the flow aid can be added to 2 parts of the dehydrated product, or 6 parts of the flow aid can be added to 4 parts of the dehydrated product.

[0107] The flowability aid can be added directly to the dehydrated product in the mixer after the initial mixing cycle, or the dehydrated product can be allowed to age for 1 to 24 hours before adding the flowability aid. Mixing can be performed for more than 10 minutes. The amount of time required can depend on the amount of material to be mixed, the size and type of the selected mixing equipment, and the form of the dehydrated product (viscous liquid, gel or putty). In some methods, mixing is performed for about 10 to 60 minutes. Mixing can be continued until a flowable powder is produced.

[0108] The resulting flowable powder can be removed from the mixer and packaged, or it can be used directly from the mixer as a component in the formulation of a granulated or tableted product.

[0109] In some processes where the resulting dehydrated product after aging has the consistency of hard putty, the dehydrated product can be converted into a flowable powder by simply applying energy to pulverize the aged product into microparticles without adding a flow aid. Any device known in the art for pulverization can be used to produce particles of the dehydrated product. Examples include impact mills, Pulverizers and coffee grinders.

[0110] In some embodiments, instead of using a flow aid, the components of the preparation can be added directly to the dehydrated product in the mixer, wherein one or more of the components of the preparation substantially serve as a flow aid material. Alternatively, the components of the preparation can be mixed together in the mixer, and the dehydrated product (as a viscous liquid, gel or putty) can be added to the mixed components. The mixing of the components of the preparation and the dehydrated product can be performed until a flowable powder is produced. The resulting flowable powder can then be processed into a granular product, or pressed into a tablet form.

[0111] D. Dehydrated product

[0112] In some embodiments, the amount of water that can be detected in the dehydrated product produced by the methods provided herein, whether directly produced in the form of a flowable powder or a viscous liquid of a gel, does not exceed 33% of the starting amount of water in the functional ingredient composition. For example, if the starting amount of water in the functional ingredient composition is 50% by weight, the amount of water in the dehydrated product produced by the method will not exceed about 16.5% by weight.

[0113] In some embodiments, the amount of water that can be detected in the dehydrated product produced by the methods provided herein does not exceed 25% of the starting amount of water in the functional ingredient composition. For example, if the starting amount of water in the functional ingredient composition is 50% by weight, the amount of water in the dehydrated product produced by the method will not exceed about 12.5% ​​by weight.

[0114] In some embodiments, the amount of water that can be detected in the dehydrated product produced by the methods provided herein does not exceed 15% of the starting amount of water in the functional ingredient composition. For example, if the starting amount of water in the functional ingredient composition is 50% by weight, the amount of water in the dehydrated product produced by the method will not exceed about 7.5% by weight.

[0115] In some embodiments, the amount of water that can be detected in the dehydrated product produced by the methods provided herein does not exceed 10% of the starting amount of water in the functional ingredient composition. For example, if the starting amount of water in the functional ingredient composition is 50% by weight, the amount of water in the dehydrated product produced by the method will not exceed about 5% by weight.

[0116] In some embodiments, the amount of water detectable in the dehydrated product may be no more than 20%, no more than 19%, no more than 18%, no more than 17%, no more than 16%, no more than 15%, no more than 14%, no more than 13%, no more than 12%, no more than 10%, no more than 9%, no more than 8%, no more than 7%, no more than 6%, no more than 5%, no more than 4%, no more than 3%, no more than 2%, or no more than 1% of the starting amount of water in the functional ingredient composition.

[0117] The method provided herein "removes" at least a portion of the water present in the starting functional ingredient composition by converting at least a portion of the water into other more desirable products (such as glycerol, ethanol or sodium acetate), so there is a minimum total weight loss compared to the total weight of the solid base, polyester solvent and functional ingredient composition added to the mixer at the beginning of the method. In the method provided herein, the difference between the total weight of the solid base, polyester solvent and functional ingredient added to the mixer and the final weight of the dehydrated product produced by the method is 2% or less. In some embodiments, the weight loss is 1.5 weight % or less, or 1 weight % or less, 0.75 weight % or less. In some embodiments, the weight loss is 0.6 weight % or less. In some embodiments, the weight loss is 0.5 weight % or less.

[0118] The dehydrated product produced by this method is substantially stable for one year or more at room temperature. When dissolved in a solvent, the dehydrated product functional ingredient composition provided herein exhibits the same or substantially similar activity or functionality as the equivalent amount of the functional ingredient in its original aqueous formulation.

[0119] E. Use in preparations

[0120] The dehydrated product produced by the method provided herein can be provided as a flowable powder, or can be converted into a flowable powder by mixing with a flow aid, or can be directly mixed into the other components of the formulation to form a flowable powder. The dehydrated product can be used as a component in a formulation, particularly a formulation provided in the form of a flowable powder, an agglomerate or a tablet.

[0121] Preparations containing the dehydrated products produced by the methods herein may be converted into any desired form using techniques known in the art.

[0122] For example, the preparation containing the dehydrated product produced by the method provided herein can be provided as a powder, an agglomerate, a tablet, a capsule, a granule, a spring disk, a brick, a briquette, a block or a composite material. The preparation containing the dehydrated product produced by the method provided herein can be mixed with a solvent or dissolved in a solvent to provide a composition in liquid form.

[0123] In some applications, the preparation containing the dehydrated product produced by the method provided herein can be provided in the form of a tablet. In some embodiments, the tablet is a compressed tablet. The preparation to be made into a tablet form can include the dehydrated product produced by the method provided herein in an amount in the range of about 5 wt % to 95 wt % based on the total weight of the compressed tablet. In some embodiments, the compressed tablet can include the dehydrated product in an amount in the range of about 10 wt % to 75 wt % based on the total weight of the compressed tablet.

[0124] Tablet compositions may contain one or more additional components. Exemplary additional components include, for example, organic solvents, one or more additional surfactants, buffer salts, tablet lubricants, fragrances, colorants, chelating agents (e.g., iminodisuccinate (as CX 100 was purchased from Lanxess Deutschland GmbH, Leverkusen, Germany) and methylglycine-diacetic acid ( M, available from BASF, Florham Park, NJ), enzymes, acids, additional carbonates or bicarbonates, phosphates, wetting agents, dispersants, hydrotropes, effervescent agents, rheology control agents, defoamers, and other functional additives.

[0125] In some applications, the formulation for tablet compositions may include expanded percarbonate as described in U.S. Patent No. 8,652,434 (Moore et al., 2014) as an additional component. In some applications, the formulation for tablet compositions may include an acid selected from acetic acid, adipic acid, azelaic acid, citric acid, fumaric acid, glutaric acid, maleic acid, malonic acid, oxalic acid, pimelic acid, suberic acid, sebacic acid, succinic acid and combinations thereof as an additional component. In some applications, the formulation for tablet compositions may include solid acetic acid such as described in U.S. Patent No. 8,859,482 (Moore et al., 2014). In some applications, the formulation for tablet compositions may include an enzyme selected from lipase, protease, peroxidase, oxidase, amylolytic enzyme, cellulase, polyesterase, glucanase, amylase, glucoamylase, glycosidase, hemicellulase, mannanase, xylanase, xyloglucanase, pectinase, β-glucosidase or any combination thereof.

[0126] When present in a tablet composition having a dehydrated product produced by the methods provided herein, the additional components can be present in an amount in the range of about 0.05% to 75%, or in the range of about 0.25% to 60%, or in the range of about 0.5% to 50%, or in the range of about 0.75% to 40%, based on the total weight of the tablet.

[0127] Tablets have several advantages over powder products: they do not need to measure and are therefore easier to handle and distribute, and they are more compact, thereby facilitating more economical shipment and reducing shipping costs. Tablets containing the dehydrated products produced by the method provided herein can have any geometric shape. Exemplary shapes include spheres, cubes, disks, rods, triangles, squares, rectangles, pentagons, hexagons, lozenges, modified balls, mandrel types (with holes in the center), capsules, ellipses, bullets, arrows, composite cups, arcuate triangles, arcuate squares (pillows), rhombuses, half-moons, and almonds. Tablets can be convex or concave. Tablets can be plane flat tablets, plane bevel edge types, plane radius edge types, concave bevel edges, or any combination thereof. In some embodiments, tablets can have a generally axially symmetrical form, and can have a circular, square, or rectangular cross section.

[0128] Tablets containing the dehydrated products produced by the methods provided herein can be prepared using any method known in the art, including compression, casting, briquetting, injection molding, and extrusion. In some embodiments, tablets can be prepared by compression (e.g., in a tablet press). Direct compression is generally considered to be the simplest and most economical method for producing tablets. Direct compression requires only two main steps: mixing all the ingredients and pressing the mixture into tablets. Any method known in the art for forming tablets can be used to prepare tablets containing the dehydrated products produced by the methods provided herein. For example, the components of the preparations containing the dehydrated products provided herein can be prepared by mixing the components together to achieve uniform mixing. Any powder blending, mixing, or shaking techniques that result in a uniform final product can be used. Known devices, such as Planetary mixers, V-blenders, V-cone blenders, rotary batch mixers, fluidized bed mixers, ribbon blenders, paddle blenders and plow blenders or combinations thereof can be used to mix the components. The homogeneous blend can be blended with a lubricant or other excipients known in the art prior to tableting.

[0129] The resulting homogeneous mixture can then be placed in a mold of desired geometry in a conventional tablet press (such as a single stroke press or a rotary press). The press includes a punch suitable for forming a tablet. The homogeneous mixture is then subjected to a compression force sufficient to produce a tablet, and the tablet containing the dehydrated product produced by the method provided herein is discharged from the tablet press. Agglomerates and particles can also be used to form tablets. Agglomerates or particles can be blended with lubricants or other excipients before tableting.

[0130] Any tableting equipment known in the art can be used for tablet formation. Suitable equipment includes a standard single stroke press or a rotary press. Such presses are commercially available and are purchased from, for example, Carver, Inc. (Wabash, Indiana), Compression Components & Service, LLC (Wharton, Pennsylvania), Specialty Measurements Inc. (Lebanon, New Jersey), GEA Pharma Systems (Wommelheim, Belgium), Korsch America Inc. (South Easton, Massachusetts) or Bosch Packaging Technology (Minneapolis, Minnesota). Tableting can be carried out at room temperature and atmospheric pressure, and is not adversely affected by temperature or pressure conditions.

[0131] The dehydrated product produced by the method provided herein can be included in a unit dosage form. The unit dosage form can be dissolved in a solvent to produce a functional solution. The functional solution can be, for example, a solution for cleaning or disinfecting a surface. In addition to the dehydrated product produced by the method provided herein, the unit dosage form can also include one or more than one additional components. Additional components can be selected from organic solvents, additional surfactants, buffer salts, lubricants, fragrances, colorants, chelating agents, enzymes, acids, carbonates, bicarbonates, phosphates, wetting agents, dispersants, hydrotropes, effervescent generators, rheology control agents, defoamers and combinations thereof.

[0132] F. Packaging system

[0133] The dehydrated product produced by the method provided herein can be packaged with packaging materials to form a packaging system. The compressed tablets or unit dosage forms containing the dehydrated product produced by the method provided herein can be packaged with packaging materials to form a packaging system. The packaging material can be rigid or flexible and can be made of any material suitable for accommodating the flowable powder produced by the method provided herein. The example of suitable packaging material includes glass, metal foil, treated metal foil, metal foil pouch, plastic, plastic film, plastic sheet, blister pack, cardboard, cardboard composite, paper and treated paper and any combination thereof.

[0134] G. Products

[0135] The dehydrated product produced by the method provided herein can be a part of goods, and the goods can include a container suitable for accommodating (such as for shipping and / or storage) composition. The dehydrated product produced by the method provided herein can be stored or shipped in a variety of containers, and the container can be made by any one of a variety of container materials or include any one of a variety of container materials, such as glass, acrylonitrile butadiene styrene (ABS), high-impact polystyrene, polycarbonate, high-density polyethylene, low-density polyethylene, high-density polypropylene, low-density polypropylene, polyethylene terephthalate, polyethylene terephthalate and polyvinyl chloride and their combination. The container can include a barrier film to increase storage stability. Suitable barrier films can include nylon, polyethylene terephthalate, fluorinated polyethylene and the copolymer of acrylonitrile and methyl methacrylate.

[0136] An article of manufacture can include a dehydrated product produced by the methods provided herein and a set of instructions (such as for using the dehydrated product produced by the methods provided herein), or storage instructions, or a material safety data sheet, or any combination thereof.

[0137] H. Application

[0138] The dehydrated products produced by the methods provided herein can be provided alone or in combination with additional components in unit dosage forms such as compressed tablets, capsules, granules, spring discs, bricks, briquettes, blocks or as dissolvable pouches or sachets that can be used to produce the desired formulations. Exemplary formulations include germicidal solutions, disinfecting solutions, surface cleaners, hand washing products, bath products, hair washing products, hair conditioning products, skin softening products, dishwashing soaps or detergent products, laundry detergents, laundry softening products, clothing antistatic products, and pet odor removal products.

[0139] For example, the dehydrated products produced by the methods provided herein can be combined with additional components into unit dosage forms of preparations for cleaning or disinfecting surfaces. Exemplary surfaces include, but are not limited to, bathroom surfaces (e.g., floors, drains, tubs, showers, mirrors, wash basins, toilets, toilet seats, urinals, bidets, toilets, countertops, shower doors or curtains, shower stalls, laundry tubs, bathroom fixtures, windows, fans, walls, lamps, and tiles); appliance surfaces (e.g., coffee makers, stoves, ovens, ranges, wash basins, waste disposal units, dishwashers, refrigerators, freezers, microwave ovens, toasters, mixers, washers, dryers, broilers); kitchen surfaces (e.g., appliances, floors, fixtures, lamps, fans, countertops, crockery, cupboards, cutlery, doors, door handles, walls, tables, chairs, cabinets, drawers, food processing equipment, flatware, utensils, floors, glassware, telephones, clocks, cutlery, shelves, cabinets, pantries, sinks, dishwashers, windows, and work surfaces); transportation devices (e.g., automobiles, bicycles, snowmobiles, motorcycles, off-road vehicles, tractors, recreational vehicles, boats, and airplanes); yard equipment; farm equipment; laboratory surfaces (e.g., autoclaves, work surfaces, hoods, clean rooms, storage rooms, freezers, countertops, centrifuges, and floors); computer surfaces (keyboards, monitors, cases, towers, laptops, and cables); handrails; railings; dental equipment or devices; medical equipment or devices; patient care equipment; patient monitoring equipment; surgical equipment or devices or instruments; veterinary equipment; tools; and utility devices (e.g., telephones, radios, televisions, entertainment centers, stereo equipment, CD and DVD players, game consoles, and analog and digital audio devices). Countertops may include tile surfaces, granite, marble or other stone surfaces, or other artificial hard surfaces, engineered quartz such as Quartz stone surface (LG Hausys), wood surface, glass surface, acrylic or polyester resin surface, concrete surface and stainless steel surface.

[0140] I. Embodiment

[0141] The following examples are included for illustrative purposes only and are not intended to limit the scope of the embodiments provided herein.

[0142] Examples 1-12

[0143] Small scale preparation of the dehydrated product as a flowable powder

[0144] exist 500 gram batches were prepared in an Ultra Power Stand Mixer (300 Watt Stand Mixer - Whirlpool Corporation, Benton Harbor, Michigan) using a platen tamper attachment. The types and amounts of components used as starting materials are provided in Table 1.

[0145] Table 1. Exemplary small-scale production formulations

[0146]

[0147]

[0148] 1 Soda ash-sodium carbonate (FMC Corporation, Philadelphia, Pennsylvania, USA)

[0149] 2 MGDA-methylglycine N,N-diacetate trisodium salt (Nouryon Chemicals, Amsterdam, The Netherlands)

[0150] 3 GLDA - Tetrasodium Glutamate Diacetate (Nouryon Chemicals, Amsterdam, The Netherlands)

[0151] 4 Baypure CX100 - Tetrasodium iminodisuccinate (RheinChemie Additives, Cologne, Germany)

[0152] 5 Glyceryl triacetate-triacetin (Jiangsu Ruijia, Jiangsu Province, China)

[0153] 6 AI-triethyl citrate (Jungbunzlauer, Basel, Switzerland)

[0154] 7 Crodasinic TM LS30 - Sodium lauroyl sarcosinate (Croda Personal Care, New Castle, DE, USA)

[0155] 8 PC48 - sodium methyl 2-sulfolaurate, disodium 2-sulfolaurate, and water (Stepan Company, Northbrook, IL, USA)

[0156] 9 BOB-babassuamidopropyl betaine (Colonial Chemical, Pittsburgh, Pennsylvania, USA)

[0157] 10 CS30 - Sodium cocoyl sarcosinate (Croda Personal Care, New Castle, DE, USA)

[0158] 11 420UP-C8-C16 Alkyl Polyglucoside (Capryl / Myristyl Glucoside) and Water (BASF Care Creations, San Bruno, CA, USA)

[0159] 12 Amphi TM M-lactone sophorolipid CAS No. 1573124-58-9 and water (Locus Performance Ingredients, Richmond, VA, USA)

[0160] 13 MultiTrope TM 810 - anionic surfactant and water (Croda Inc., Chino Hills, CA, USA)

[0161] 14 Zinador TM 22L-Polymeric zinc itaconate complex odor neutralizer and water (Croda Inc., Chino Hills, CA, USA)

[0162] First, solid alkali is loaded into the stainless steel bowl of the mixer. Then polyester solvent is added, and the aqueous functional ingredient composition is added subsequently. Then the vertical mixer is started to stir the components together using the lowest rpm setting. The initial mixing is performed for about 1 minute to 5 minutes and stops so that the initial test sample can be taken out from the mixture. Then, under the same lowest rpm setting, the mixing operation is restarted, and the time of about 30 minutes is continued again. The dehydrated product is in the form of a flowable powder. Once the mixing operation is completed, the final flowable powder is transferred to a holding container and closed with a lid. After the mixing is completed, the final test sample is taken in 1 hour and 24 hours. The test sample is analyzed on a near infrared spectrometer (NIRS XDS Rapid Content Analyzer-model Xm-1100 series-Metrohm, Riverview, Florida), to analyze the change in the amount of water that can be detected.

[0163] Examples 13-24

[0164] Tablet formulation

[0165] The dehydrated product flowable powder produced in Examples 1-12 is added to form a compressed tablet. The tablet formulation is provided in Table 2. For Examples 13-24, the components of the tablet formulation are blended together in a laboratory-scale V-blender for 5 minutes to obtain a uniform blend. An aliquot of the uniform blend of about 9 g to 20 g is weighed and a compressed tablet is made using a mold (such as a mold with a diameter of about 27 mm to 38.1 mm). Using a CARVER Press at a pressure of about 4 metric tons to 8 metric tons, each aliquot of the uniform blend is pressed into a tablet using a mold with a diameter of 38.1 mm.

[0166] Table 2. Exemplary tablet compositions

[0167]

[0168]

[0169] 15 When the tablet is dissolved in a suitable solvent (such as water)

[0170] 16 Citric acid (SACitrique Belge NV, Tienen, Belgium)

[0171] 17 Sodium bicarbonate (Solvay USA Inc., Albright, WV, USA)

[0172] 18 Glycerox TM HE (Croda Personal Care, East Yorkshire, UK)

[0173] 19 Glucono-δ-lactone (Jungbunzlauer Suisse AG, Basel, Switzerland)

[0174] 20 Sodium benzoate (Emerald Kalama Chemical, Kalama, USA)

[0175] 21 Sodium lauryl sulfate (Stepan Company, Northfield, IL, USA)

[0176] 22 Dextrose( dextrose A, ADM, Chicago, IL, USA)

[0177] 23Potassium sorbate (APAC Chem Corp., Nantong, China)

[0178] 24 Fumaric acid (Bartek Ingredients, Inc., Ontario, Canada)

[0179] 25 Expanded sodium percarbonate (see U.S. Pat. No. 8,652,434)

[0180] 26 C9-11 ethoxylated alcohol EO6 (Tomadol 91-6, Air Products, Allentown, Pennsylvania, USA)

[0181] 27 Sodium acetate (Niacet Corporation, Niagara Falls, New York, USA)

[0182] 28 Polyacrylic acid (Sokalan PA25CL BASF, Florham Park, NJ, USA)

[0183] 29 Enzyme blend (BioCat, Troy, VA, USA)

[0184] 30 1,3-Propanediol( Propylene glycol, DuPont Tate & Lyle Bio Products, LLC, Loudon, TN, USA)

[0185] 31 Sodium gluconate (PMP Fermentation Products, Inc., Peoria, IL, USA)

[0186] Embodiment 25

[0187] Large-scale preparation of flowable powders

[0188] A 1041.67 lb batch was prepared in a 36 cu. ft. Ross ribbon blender (Model 42B-36 - Charles Ross & Son Company, Hauppauge, NY).

[0189] First, the solid base is loaded into the blender. Then the polyester solvent is added together with the water-containing functional ingredients. Then the blender is set to operate at 30Hz. The initial mixing operation is carried out for about 1 minute to 5 minutes and stops, so the initial test sample can be taken out from the powder. Then the mixing operation is continued for an additional 60 minutes. Once the mixing operation is completed, the final flowable powder is transferred to a bulk powder bag and tied. The final test sample is taken 1 hour and 24 hours after the mixing is completed. The test sample is analyzed on a near infrared spectrometer (NIRS XDS Rapid Content Analyzer-Model Xm-1100 Series-Metrohm, Riverview, Florida) for analyzing the water peak of the change.

[0190] Examples 26-29

[0191] Assessment of water loss

[0192] A small-scale production run was performed to analyze the weight loss that occurs during the process. 500 g batches were prepared in an UltraPower Stand Mixer (300 Watt Stand Mixer - Whirlpool Corporation, Benton Harbor, Michigan) using a platen tamper attachment as described above for Examples 1-12. The types and amounts of components used as starting materials are provided in Table 3. Weight loss data are also provided in Table 3.

[0193] Table 3. Weight loss

[0194]

[0195] 1 Soda ash-sodium carbonate (FMC Corporation, Philadelphia, Pennsylvania, USA)

[0196] 5 Glyceryl triacetate-triacetin (Jiangsu Ruijia, Jiangsu Province, China)

[0197] 6 AI-triethyl citrate (Jungbunzlauer, Basel, Switzerland)

[0198] 7 LS30 - Sodium lauroyl sarcosinate (Croda Personal Care, New Castle, DE, USA)

[0199] 32 CAB30-cocamidopropyl betaine (Croda Personal Care, New Castle, DE, USA)

[0200] 33 818UP-Coco-Glucoside (BASF Care Creations, Florham Park, NJ, USA)

[0201] From the data in Table 3, it can be seen that the weight loss after 24 hours from the completion of mixing was less than 1%, ranging from 0.26% to 0.60%.

[0202] Examples 30-45

[0203] Small-scale preparation of dehydration products as viscous fluids / gels

[0204] exist 200 gram batches were prepared in an Ultra Power Stand Mixer (300 Watt Stand Mixer - Whirlpool Corporation, Benton Harbor, Michigan) using a platen tamper attachment and mixed for 30 minutes. The types and amounts of components used as starting materials are provided in Table 4.

[0205] Table 4. Exemplary small-scale production formulations

[0206]

[0207]

[0208] 1 Soda ash-sodium carbonate (FMC Corporation, Philadelphia, Pennsylvania, USA)

[0209] 5 Glyceryl triacetate-triacetin (Jiangsu Ruijia, Jiangsu Province, China)

[0210] 7 LS30 - Sodium lauroyl sarcosinate (Croda Personal Care, New Castle, DE, USA)

[0211] After mixing for 30 minutes, the resulting product was a viscous liquid. Some of the dehydrated products were aged. After aging for 3 hours without mixing, the aged dehydrated product had a gel consistency. After aging for 24 hours without mixing, the aged dehydrated product had a putty consistency. The results of exemplary aged dehydrated products are listed in Table 5.

[0212] Table 5. Exemplary aged small-scale production formulations

[0213]

[0214] After aging for 24 hours without mixing, Examples 30 and 42 had the consistency of very soft putties that could be easily deformed and had a consistency similar to bread dough. After aging for 24 hours without mixing, Example 39 had the consistency of a soft putty that required minimal force to deform, similar to a soft pomade or balm. After aging for 24 hours without mixing, Example 36 had the consistency of a regular putty similar to Silly Putty or Play-Doh that could be deformed with moderate force. After aging for 24 hours without mixing, Example 35 had the consistency of a hard putty, like carnauba wax paste car wax, that required the application of moderately high force to deform.

[0215] Examples 46-48

[0216] Conversion of aged dehydrated products into flowable powders

[0217] The formulation of Example 42 (10% soda ash, 51.43% triacetin, 38.57% LS30) to prepare the dehydrated product. Three 200-gram batches were prepared by mixing the components for 30 minutes using a flat beater attachment in an Ultra Power Stand Mixer (300-watt stand mixer—Whirlpool Corporation, Benton Harbor, Michigan). The dehydrated product was aged for 24 hours without mixing before conversion to a flowable powder. The aged product had the consistency of bread dough and could be easily deformed.

[0218] An aliquot of each preparation was converted into a flowable powder. The amount of dehydrated product and the type and amount of flow aid are provided in Table 6.

[0219] Table 6. Conversion of viscous fluid / gel dehydration products to flowable powders

[0220] Example Example 42 (weight %) Flowability aids Flowability aid amount (weight %) 46 20 <![CDATA[Sodium chloride 34 > 80 47 33.33 <![CDATA[Sodium chloride 34 > 66.67 48 20 <![CDATA[Sodium sulfate 35 > 80

[0221] 34 Sodium chloride (Morton Salt, Inc., Chicago, IL, USA)

[0222] 35 Sodium sulfate (Saltex, LLC, Fort Worth, Texas, USA)

[0223] An aliquot of the dehydrated product of Example 42 was placed The flow aid was added to the bowl of an Ultra Power Stand Mixer (300 Watt Stand Mixer - Whirlpool Corporation, Benton Harbor, Michigan) and the mixture was mixed for 30 minutes using a flat beater attachment. Each resulting product was a flowable powder.

[0224] Examples 49-51

[0225] Tablet composition

[0226] The dehydrated products in the form of flowable powders provided in Examples 46 to 48 were used to prepare tablet forms of the neutral surface cleaner formulations. The components and amounts are provided in Table 7.

[0227] Table 7. Exemplary Neutral Surface Cleaner Formulations

[0228] Element Embodiment 49 Embodiment 50 Embodiment 51 Powder - Example 46 10 - - Powder - Example 47 - 20 - Powder - Example 48 - - 10 <![CDATA[Citric acid 16 > 38 35 40 <![CDATA[Sodium bicarbonate 17 > 40 32 40 <![CDATA[Sodium acetate 27 > 7 8 5 <![CDATA[PEG 8000 36 ]]> 5 5 5

[0229] 16 Citric acid (SACitrique Belge NV, Tienen, Belgium)

[0230] 17 Sodium bicarbonate (Solvay USA Inc., Albright, WV, USA)

[0231] 27 Sodium acetate (Niacet Corporation, Niagara Falls, New York, USA)

[0232] 36 E8000 (BASF Personal Care, San Bruno, California, USA)

[0233] For Examples 49 to 51, the components of the tablet formulations were mixed together in a laboratory scale V-blender for 5 minutes to obtain a homogenous blend. Aliquots of the homogenous blend in amounts of about 8 to 10 grams were weighed and pressed using a 1 inch (2.54 cm) die. Each aliquot of the homogenous blend was separately compressed into tablets using a CARVER Press at a pressure of about 4 to 8 metric tons.

[0234] Examples 52-56

[0235] Experiments were performed using the methods described herein to demonstrate that water decreases over time. The water peaks at 1400 nm and 1900 nm were monitored over time using NIR. Five different mixtures of 12 g batches were prepared directly in the tumbler using a glass tumbler machine from Metrohm ((Part No. 6.7400.010, Metrohm AG, Riverview, Florida)) to obtain an initial water peak reading as close to time zero as possible. The formulations for the mixtures are shown in Table 8.

[0236] Table 8. Formulations used for water reduction measurements

[0237]

[0238] 1 Soda ash-sodium carbonate (FMC Corporation, Philadelphia, Pennsylvania, USA)

[0239] 37 M-Methylglycine diacetic acid, trisodium salt (MDGA-Na3), purchased from BASF, Florham Park, NJ

[0240] 5 Glyceryl triacetate-triacetin (Jiangsu Ruijia, Jiangsu Province, China)

[0241] 9 BOB-babassuamidopropyl betaine (Colonial Chemical, Pittsburgh, Pennsylvania, USA)

[0242] 7 Crodasinic TM LS30 - Sodium lauroyl sarcosinate (Croda Personal Care, New Castle, DE, USA)

[0243] 38 LGC Sorb - Sodium Lauryl Glucose Carboxylate (and) Lauryl Glucoside, (BASF, Florham Park, NJ)

[0244] 39 CGN-sodium cocoyl glutamate (Clariant Produkte (Deutschland) GmbH, Frankfurt, Germany)

[0245] process

[0246] Soda ash or M and surfactant were dispensed into a tumbler, then triacetin was added, the contents were mixed with a glass rod for about 30 seconds, and immediately measured using a near infrared spectrometer (NIRS XDS Rapid Content Analyzer - Model Xm-1100 Series - Metrohm, Riverview, Florida). The focus of the measurement was on the two water band peaks found at 1400nm and 1900nm. Each sample was covered and left on the NIR overnight. The NIR automatically took readings at regular intervals over a period of up to 900 minutes (15 hours). The results are shown in FIG. 2A to FIG. 6B Each graph in the accompanying drawings shows separately a graph of the decrease in the intensity ("Y") of the water peaks (1400 nm and 1900 nm), which decrease in intensity is correlated to the decrease in the amount of water molecules in the blend. The X-axis shows the measurement time. Figure 2A and Figure 2B The results obtained for mixture 1 are shown. Figure 3A and Figure 3B The results obtained for mixture 2 are shown. Figure 4A and Figure 4B The results obtained for mixture 3 are shown. Figure 5A and Figure 5B The results obtained for mixture 4 are shown. Fig. 6A and Figure 6B Results obtained for Mix 5 are shown. As can be seen in all figures, the methods provided herein result in a significant reduction in water over time. No sample had a weight loss of more than 0.2 g from the overnight NIR readings.

[0247] Embodiment 57

[0248] Preparations incorporating the dehydrated product of the above mixture 1 were prepared. After 900 minutes of reaction time, mixture 1 (75% by weight of soda ash, 17% by weight of triacetin and 8% by weight of LGC) was used to prepare a foaming hand soap formulation.

[0249] Table 9. Foaming Hand Soap Formulations

[0250]

[0251]

[0252] 16 Citric acid (SACitrique Belge NV, Tienen, Belgium)

[0253] 17 Sodium bicarbonate (Solvay USA Inc., Albright, WV, USA)

[0254] 19 Glucono-δ-lactone (Jungbunzlauer Suisse AG, Basel, Switzerland)

[0255] 20 Sodium benzoate (Emerald Kalama Chemical, Kalama, USA)

[0256] 21 Sodium lauryl sulfate (Stepan Company, Northfield, IL, USA)

[0257] The components shown in Table 9 were blended together to prepare a final blend weighing 200 g. A 15 gram aliquot was then taken from the blend and compressed into tablets on a CARVER PRESS using a 1.25" diameter die size at approximately 8 metric tons. One tablet was added to 240 mL of water (255 mL total) to form a foaming hand soap formulation. When the final solution was used in a foaming pump, the foam was thicker and had good glide (silky feel) compared to formulations that did not contain the dehydrated surfactant blend in combination with SLS. When the dehydrated surfactant blend of Mix 1 was combined with a sulfate-free powdered surfactant such as Lathanol 2000 shown in Table 9.1, the foaming properties of the hand soap formulation were better. Even better skin feel and thicker foam buildup were achieved when used with Amisoft CS-11.

[0258] Table 9.1. Foaming Hand Soap Formulations (Sulfate-Free)

[0259] Components Amount (weight %) Amount (weight %) Dehydration mixture 1 18 18 <![CDATA[Citric acid 16 > 36.5 36.5 <![CDATA[Sodium bicarbonate 17 > 12.5 12.5 Fragrance 2 2 <![CDATA[GDL (Glucono-δ-lactone) 19 > 13.5 13.5 <![CDATA[Sodium benzoate 20 > 9.5 9.5 <![CDATA[Surfactant - Lathanol LAL 40 > 8.0 -- <![CDATA[Surfactant - Amisoft CS-11 41 > -- 8.0

[0260] 16 Citric acid (SACitrique Belge NV, Tienen, Belgium)

[0261] 17 Sodium bicarbonate (Solvay USA Inc., Albright, WV, USA)

[0262] 19 Glucono-6-lactone (Jungbunzlauer Suisse AG, Basel, Switzerland)

[0263] 20 Sodium benzoate (Emerald Kalama Chemical, Kalama, USA)

[0264] 40 Lathanol LAL - Sodium lauryl sulfonate (Stepan Company, Northfield, IL, USA)

[0265] 41 Amisoft CS-11 - Sodium Cocoyl Glutamate (Ajinomoto, Tokyo, Japan)

[0266] Embodiment 58

[0267] Preparations incorporating the dehydrated product of the above mixture 3 were prepared. After 900 minutes of reaction time, mixture 3 (75% by weight of soda ash, 17% by weight of triacetin and 8% by weight of CGN) was used to prepare a multi-surface cleaner. The formulation is shown in Table 10.

[0268] Table 10. Multi-Surface Cleaner Formulations

[0269] Components Amount (weight %) Dehydration mixture 3 40 <![CDATA[Citric acid 16 > 48 <![CDATA[Sodium lauryl sulfate (SLS)]]> 21 > 2 <![CDATA[Sodium acetate 27 > 8 <![CDATA[Sodium gluconate 31 > 2

[0270] 16 Citric acid (SACitrique Belge NV, Tienen, Belgium)

[0271] 21 Sodium lauryl sulfate (Stepan Company, Northfield, IL, USA)

[0272] 27 Sodium acetate (Niacet Corporation, Niagara Falls, New York, USA)

[0273] 31 Sodium gluconate (PMP Fermentation Products, Inc., Peoria, IL, USA)

[0274] The components shown in Table 10 were blended together to prepare a final blend weighing 200 g. 10 grams of this blend was then compressed into tablets on a CARVERPRESS using a die size of 1.063″ in diameter at approximately 8 metric tons. The tablets were added to 690 mL of water to prepare a multi-surface cleaner. The tablets showed excellent visible foam, very good dissolution rate, and the resulting solution had good clarity.

Claims

1. A method for removing water from an aqueous functional ingredient composition containing more than 10% by weight of water, the method comprising: mixing a solid base, a polyester solvent and the aqueous functional ingredient composition in a mixer at room temperature to produce a dehydrated product, in: The amount of water in the dehydrated product does not exceed 33% of the initial amount of water in the aqueous functional ingredient composition, and The difference between the total weight of the solid base, the polyester solvent and the aqueous functional ingredient composition added to the mixer and the final weight of the dehydrated product is 2% or less.

2. The method of claim 1, wherein the functional ingredient in the aqueous functional ingredient composition comprises a surfactant, a dispersant, an anti-redeposition agent, a solubility regulator, a rinse aid, an odor counteractant, a chelating agent, a conditioning agent, an antistatic agent, a soil shielding agent, a detergent, a color protection agent, or a combination thereof.

3. The method according to claim 1 or 2, wherein the starting amount of water in the aqueous functional ingredient composition is in the range of 10 wt% to 98 wt%.

4. The method of any one of claims 1 to 3, wherein the solid base comprises an alkaline material that is solid at room temperature and has a pH in the range of about 8 to 13.

5.

5. The method according to any one of claims 1 to 4, wherein the solid base comprises an alkali metal salt, an alkaline earth metal salt, an aminopolycarboxylate-based chelating agent, a tetrasodium iminodisuccinate complexing agent, or a combination thereof.

6. The method according to any one of claims 1 to 5, wherein the solid base comprises one or more selected from the group consisting of sodium acetate, potassium acetate, sodium carbonate, potassium carbonate, calcium carbonate, magnesium carbonate, sodium bicarbonate, potassium bicarbonate, sodium sesquicarbonate, sodium silicate, potassium silicate, sodium metasilicate, potassium metasilicate, methylglycine N,N-diacetic acid trisodium salt (MGDA), glutamic acid diacetic acid tetrasodium salt (GLDA) and tetrasodium iminodisuccinate.

7. The method of any one of claims 1 to 6, wherein the solid base comprises sodium carbonate, sodium bicarbonate, potassium carbonate, potassium bicarbonate, MGDA, GLDA, or a combination thereof.

8. The method according to any one of claims 1 to 7, wherein the polyester solvent comprises an ester compound comprising three or more part.

9. The method of any one of claims 1 to 8, wherein the polyester solvent comprises a citrate ester, a lactate ester, a glyceride, or a combination thereof.

10. The method according to any one of claims 1 to 9, wherein the polyester solvent comprises triethyl citrate, acetyl triethyl citrate, tributyl citrate, acetyl tributyl citrate, trihexyl citrate, n-butyryl-tri(n-hexyl)-citrate, trioctyl citrate, tributyl aconitate, glyceryl triacetate (glyceryl triacetate), glyceryl tripropionate (glyceryl tripropionate), glyceryl tributyrate (glyceryl tributyrate), glyceryl tricaprate (glyceryl tricaprate), glyceryl trioleate (glyceryl trioleate), glyceryl tristearate (stearin), glyceryl tripalmitate (glyceryl tripalmitate), pentaerythritol tetraethylhexanoate, or a combination thereof.

11. The method according to any one of claims 1 to 10, wherein the polyester solvent is selected from triethyl citrate, acetyl triethyl citrate, tributyl citrate, acetyl tributyl citrate, triacetin (glyceryl triacetate), tripropionin (glyceryl tripropionate), tributyrin (glyceryl tributyrate), and combinations thereof.

12. The method according to any one of claims 1 to 11, wherein the ratio of the solid base to the functional ingredient composition is in the range of about 5:1 to 15:1, and the dehydration product is in the form of a flowable powder.

13. The method of claim 12, wherein the ratio of the solid base to the polyester solvent is in the range of about 3:1 to 8.5:

1.

14. The method of claim 12 or 13, wherein the ratio of the polyester solvent to the functional ingredient composition is in the range of about 1:1 to 3:

1.

15. The method according to any one of claims 1 to 11, wherein the ratio of the solid base to the functional ingredient composition is in the range of about 3:1 to 1:5, and the dehydration product is in the form of a viscous fluid.

16. The method of claim 15, wherein the ratio of the solid base to the polyester solvent is in the range of about 3.5:1 to 1:

11.

17. The method of claim 15 or 16, wherein the ratio of the polyester solvent to the functional ingredient composition is in the range of about 4:1 to 1:

4.

18. The method according to any one of claims 13 to 17, wherein the dehydrated product is aged for a period of 3 to 8 hours to obtain the dehydrated product in the form of a gel.

19. The method according to any one of claims 13 to 17, wherein the dehydrated product is aged for a period of 18 to 24 hours, thereby obtaining the dehydrated product in the form of putty.

20. The method of any one of claims 13 to 19, further comprising blending the dehydrated product with a flowability aid to produce a flowable product.

21. The method of claim 20, wherein the flow aid comprises: a) sodium chloride, potassium chloride, sodium sulfate, potassium sulfate or a combination thereof; b) a sodium and / or potassium salt of at least one of acetate, carbonate, bicarbonate, citrate, phosphate, silicate, aluminate, or a combination thereof; or c) A combination of a) and b).

22. The method of claim 20 or 21, wherein the ratio of the flow aid to the dehydration product is about 1:1 to 5:

1.

23. The method of any one of claims 20 to 22, wherein the blending is performed for about 10 minutes or longer.

24. The method according to any one of claims 1 to 23, wherein the mixer is Countertop stand mixer, Planetary mixers, V-blenders, V-conical blenders, rotary batch mixers, ribbon blenders, paddle blenders, plow blenders, screw mixers, turbulence enhancers, mixer, double arm kneader mixer or a combination thereof.

25. The method according to any one of claims 1 to 24, wherein the mixing is carried out at room temperature and atmospheric pressure.

26. The method of any one of claims 1 to 25, wherein the amount of water in the dehydration product does not exceed about 33% of the initial amount of water in the aqueous functional ingredient composition.

27. The method of any one of claims 1 to 26, wherein the mixing is performed for a period of 10 minutes to 60 minutes.

28. A dehydrated product produced by the method according to any one of claims 1 to 27.

29. A composition comprising the dehydration product according to claim 28.

30. The composition of claim 29 in the form of a compressed tablet.

31. The composition of claim 30, wherein the amount of the dehydration product is in the range of about 5 wt% to 95 wt% based on the total weight of the compressed tablet.

32. The composition according to claim 30 or 31, further comprising an additional component in the range of about 0.05 wt% to 75 wt% based on the total weight of the tablet.

33. The composition of claim 29, further comprising an additional component in the range of about 0.05 wt% to 75 wt% based on the total weight of the composition.

34. A composition according to any one of claims 29 to 33, wherein the additional components are selected from organic solvents, additional surfactants, buffer salts, lubricants, fragrances, colorants, chelating agents, enzymes, acids, carbonates, bicarbonates, phosphates, wetting agents, dispersants, hydrotropes, effervescent agents, rheology control agents, defoamers and combinations thereof.

35. A composition according to any one of claims 29 to 34, formulated as a germicidal product, a disinfecting product, a surface cleaner, a hand washing product, a bath product, a hair washing product, a hair conditioning product, a skin softening product, a dishwashing soap or detergent product, a laundry detergent, a laundry softening product, a laundry antistatic product or a pet odor removal product.

36. A unit dosage form comprising the dehydration product of claim 28.

37. The unit dosage form according to claim 36, which is in the form of a compressed tablet, capsule, pellet, puck, brick, briquette, block, dissolvable pouch, dissolvable sachet.

38. The unit dosage form of claim 36 or 37, which dissolves in a solvent to produce a germicidal solution, a disinfecting solution, a surface cleaner, a hand washing product, a bath product, a hair washing product, a hair conditioning product, a skin softening product, a dishwashing soap or detergent product, a laundry detergent, a laundry softening product, a laundry antistatic product, or a pet odor removal product.

Citation Information

Patent Citations

  • Alkaline liquid laundry detergent compositions comprising polyesters

    CN104508000A

  • Recycled sulfopolyesters

    CN114222652A

  • method for removing a volatile component from a detergent composition

    FR2328767A1

  • Builder particle for detergent and detergent composition

    JP2004238529A

  • Process for making non-particulate detergent product readily dispersible in water

    US6495509B1